Sample records for al mn zn

  1. Elastocaloric effect in CuAlZn and CuAlMn shape memory alloys under compression

    PubMed Central

    Qian, Suxin; Wang, Yi; Pillsbury, Thomas E.; Hada, Yoshiharu; Yamaguchi, Yuki; Fujimoto, Kenjiro; Hwang, Yunho; Radermacher, Reinhard; Cui, Jun; Yuki, Yoji; Toyotake, Koutaro; Takeuchi, Ichiro

    2016-01-01

    This paper reports the elastocaloric effect of two Cu-based shape memory alloys: Cu68Al16Zn16 (CuAlZn) and Cu73Al15Mn12 (CuAlMn), under compression at ambient temperature. The compression tests were conducted at two different rates to approach isothermal and adiabatic conditions. Upon unloading at a strain rate of 0.1 s−1 (adiabatic condition) from 4% strain, the highest adiabatic temperature changes (ΔTad) of 4.0 K for CuAlZn and 3.9 K for CuAlMn were obtained. The maximum stress and hysteresis at each strain were compared. The stress at the maximum recoverable strain of 4.0% for CuAlMn was 120 MPa, which is 70% smaller than that of CuAlZn. A smaller hysteresis for the CuAlMn alloy was also obtained, about 70% less compared with the CuAlZn alloy. The latent heat, determined by differential scanning calorimetry, was 4.3 J g−1 for the CuAlZn alloy and 5.0 J g−1 for the CuAlMn alloy. Potential coefficients of performance (COPmat) for these two alloys were calculated based on their physical properties of measured latent heat and hysteresis, and a COPmat of approximately 13.3 for CuAlMn was obtained. This article is part of the themed issue ‘Taking the temperature of phase transitions in cool materials’. PMID:27402936

  2. Thouless length and valley degeneracy factor of ZnMnO thin films with anisotropic, highly conductive surface layers

    NASA Astrophysics Data System (ADS)

    Vegesna, Sahitya V.; Bürger, Danilo; Patra, Rajkumar; Abendroth, Barbara; Skorupa, Ilona; Schmidt, Oliver G.; Schmidt, Heidemarie

    2017-06-01

    Isothermal magnetoresistance (MR) of n-type conducting Zn1-xMnxO thin films on a sapphire substrate with a Mn content of 5 at. % has been studied in in-plane and out-of-plane magnetic fields up to 6 T in the temperature range of 5 K to 300 K. During pulsed laser deposition of the ZnMnO thin films, we controlled the thickness and roughness of a highly conductive ZnMnO surface layer. The measured MR has been modeled with constant s-d exchange (0.2 eV in ZnMnO) and electron spin (S = 5/2 for Mn2+) for samples with a single two dimensional (2D) ZnMnO layer, a single three dimensional (3D) ZnMnO layer, or a 2D and 3D (2D + 3D) ZnMnO layer in parallel. The temperature dependence of modeled Thouless length LTh (LTh ˜ T-0.5) is in good agreement with the theory [Andrearczyk et al., Phys. Rev. B 72, 121309(R) (2005)]. The superimposed positive and negative MR model for ZnCoO thin films [Xu et al., Phys. Rev. B 76, 134417 (2007)] has been extended in order to account for the increase in the density of states close to the Fermi level of n-ZnMnO due to substitutional Mn2+ ions and their effect on the negative MR in ZnMnO.

  3. Wettability of MnxSiyOz by Liquid Zn-Al Alloys

    NASA Astrophysics Data System (ADS)

    Kim, Yunkyum; Shin, Minsoo; Tang, Chengying; Lee, Joonho

    2010-08-01

    The wettability of MnxSiyOz by liquid Zn-Al alloys was investigated to obtain basic information on the coating properties of high-strength steels with surface oxides in the hot-dip galvanizing process. In this study, the contact angles of liquid Zn-Al alloys (Al concentrations were 0.12 and 0.23 wt pct) on four different MnxSiyOz oxides, namely MnO, MnSiO3, Mn2SiO4, and SiO2, were measured with the dispensed drop method. The contact angle did not change across time. With an increasing Al concentration, the contact angle was slightly decreased for MnO and Mn2SiO4, but there was no change for MnSiO3 and SiO2. With an increasing SiO2 content, the contact angle gradually increased by 54 wt pct to form MnSiO3, and for pure SiO2 substrate, the contact angle decreased again. Consequently, the MnSiO3 substrate showed the worst wettability among the four tested oxide substrates.

  4. Silicic Acid and Beer Consumption Reverses the Metal Imbalance and the Prooxidant Status Induced by Aluminum Nitrate in Mouse Brain.

    PubMed

    González-Muñoz, María José; Garcimartán, Alba; Meseguer, Isabel; Mateos-Vega, Carmen José; Orellana, José María; Peña-Fernández, Antonio; Benedí, Juana; Sánchez-Muniz, Francisco J

    2017-01-01

    Emerging evidence suggests that by affecting mineral balance, aluminum (Al) may enhance some events associated with neurodegenerative diseases. To examine the effect of Al(NO3)3 exposure on brain Al, cooper (Cu), iron (Fe), magnesium (Mg), manganese (Mn), silicon (Si), and zinc (Zn) levels, and the metal-change implication in brain oxidant and inflammatory status. Four groups of six-week-old male NMRI mice were treated for three months: i) controls, administrated with deionized water; ii) Al, which received Al(NO3)3; iii) Al+silicic acid, which were given Al(NO3)3 plus silicic acid; and iv) Al+beer, which received Al(NO3)3 plus beer. Brain Al and TBARS levels and TNFα and GPx expressions increased, while Cu, Mn, and Zn levels, and catalase and CuZn-SOD expression decreased (at least, p < 0.05) in Al versus control animals. Al, Si, and TBARS levels and TNFα expression decreased (p < 0.05) in Al+silicic acid and Al+beer specimens while Cu, Mn, and Zn levels and antioxidant expression increased versus the Al group. Brain Al levels correlated negatively with those of Cu, Fe, Mn, and Zn, and catalase, CuZn-SOD, and GPx enzyme expressions but positively with Si and TBARS levels and TNFα expression. Two components of the principal component analysis (PCA) explained 71.2% of total data variance (p < 0.001). PCA connected the pro-oxidant markers with brain Al content, while brain Zn and Cu levels were closer to antioxidant enzyme expression. Administration of Al(NO3)3 induced metal imbalance, inflammation, and antioxidant status impairment in the brain. Those effects were blocked to a significant extent by silicic acid and beer administration.

  5. Role of Al in Zn bath on the formation of the inhibition layer during hot-dip galvanizing for a 1.2Si-1.5Mn transformation-induced plasticity steel

    NASA Astrophysics Data System (ADS)

    Wang, Kuang-Kuo; Hsu, Chiung-Wen; Chang, Liuwen; Gan, Dershin; Yang, Kuo-Cheng

    2013-11-01

    This study investigated the interaction between the Al in the Zn bath and the surface oxides formed by selective oxidation on a 1.2Si-1.5Mn TRIP steel during hot-dip galvanizing. XPS and TEM were employed for characterization. The results indicated that the amorphous xMnO·SiO2 oxide could react with Al to form a Si-Mn-Al-containing oxide. The crystalline MnSiO3 and Mn2SiO4 oxides could be largely reduced by Al to form holes in the oxide film. Consequently, the steel covered by a layer of mixed xMnO·SiO2 and MnSiO3 could form a continuous Fe2Al5 inhibition layer and showed the highest galvanizability among the three samples examined.

  6. Evidence from x-ray and neutron powder diffraction patterns that the so-called icosahedral and decagonal quasicrystals of MnAl(6) and other alloys are twinned cubic crystals.

    PubMed

    Pauling, L

    1987-06-01

    It is shown that the x-ray powder diffraction patterns of rapidly quenched MnAl(6) and Mg(32)(Al,Zn)(49) and the neutron powder diffraction pattern of MnAl(6) are compatible with the proposed 820-atom primitive cubic structure [Pauling, L. (1987) Phys. Rev. Lett. 58, 365-368]. The values found for the edge of the unit cube are 23.365 A (x-ray) and 23.416 A (neutron) for MnAl(6) and 24.313 A (x-ray) for Mg(32)(Al,Zn)(49).

  7. Evidence from x-ray and neutron powder diffraction patterns that the so-called icosahedral and decagonal quasicrystals of MnAl6 and other alloys are twinned cubic crystals

    PubMed Central

    Pauling, Linus

    1987-01-01

    It is shown that the x-ray powder diffraction patterns of rapidly quenched MnAl6 and Mg32(Al,Zn)49 and the neutron powder diffraction pattern of MnAl6 are compatible with the proposed 820-atom primitive cubic structure [Pauling, L. (1987) Phys. Rev. Lett. 58, 365-368]. The values found for the edge of the unit cube are 23.365 Å (x-ray) and 23.416 Å (neutron) for MnAl6 and 24.313 Å (x-ray) for Mg32(Al,Zn)49. PMID:16593841

  8. Performance of Al-0.5 Mg-0.02 Ga-0.1 Sn-0.5 Mn as anode for Al-air battery in NaCl solutions

    NASA Astrophysics Data System (ADS)

    Ma, Jingling; Wen, Jiuba; Gao, Junwei; Li, Quanan

    2014-05-01

    In this research, metal-air battery based on Al, Zn, Al-0.5 Mg-0.02 Ga-0.1 Sn and Al-0.5 Mg-0.02 Ga-0.1 Sn-0.5 Mn (wt%) is prepared and the battery performance is investigated by constant current discharge test in 2 mol L-1 NaCl solutions. The characteristics of the anodes after discharge are investigated by electrochemical impedance spectroscopy (EIS), scanning electron microscopy (SEM). The corrosion behavior of the anodes is studied by self-corrosion rate measurement and potentiodynamic polarization measurement. The results show that Al-Mg-Ga-Sn-Mn is more active than Al, Zn and Al-Mg-Ga-Sn anodes. The self-corrosion rate is found to be in the order: Al < Al-Mg-Ga-Sn-Mn < Al-Mg-Ga-Sn < Zn. It has been observed that the Al-air battery based on Al-Mg-Ga-Sn-Mn offers higher operating voltage and anodic utilization than those with others. SEM and EIS results of the alloy are in good agreement with corrosion characteristics.

  9. Effect of Al and Mg Contents on Wettability and Reactivity of Molten Zn-Al-Mg Alloys on Steel Sheets Covered with MnO and SiO2 Layers

    NASA Astrophysics Data System (ADS)

    Huh, Joo-Youl; Hwang, Min-Je; Shim, Seung-Woo; Kim, Tae-Chul; Kim, Jong-Sang

    2018-05-01

    The reactive wetting behaviors of molten Zn-Al-Mg alloys on MnO- and amorphous (a-) SiO2-covered steel sheets were investigated by the sessile drop method, as a function of the Al and Mg contents in the alloys. The sessile drop tests were carried out at 460 °C and the variation in the contact angles (θc) of alloys containing 0.2-2.5 wt% Al and 0-3.0 wt% Mg was monitored for 20 s. For all the alloys, the MnO-covered steel substrate exhibited reactive wetting whereas the a-SiO2-covered steel exhibited nonreactive, nonwetting (θc > 90°) behavior. The MnO layer was rapidly removed by Al and Mg contained in the alloys. The wetting of the MnO-covered steel sheet significantly improved upon increasing the Mg content but decreased upon increasing the Al content, indicating that the surface tension of the alloy droplet is the main factor controlling its wettability. Although the reactions of Al and Mg in molten alloys with the a-SiO2 layer were found to be sluggish, the wettability of Zn-Al-Mg alloys on the a-SiO2 layer improved upon increasing the Al and Mg contents. These results suggest that the wetting of advanced high-strength steel sheets, the surface oxide layer of which consists of a mixture of MnO and SiO2, with Zn-Al-Mg alloys could be most effectively improved by increasing the Mg content of the alloys.

  10. Toxicity of Metals to a Freshwater Ostracod: Stenocypris major

    PubMed Central

    Shuhaimi-Othman, Mohammad; Yakub, Nadzifah; Ramle, Nur-Amalina; Abas, Ahmad

    2011-01-01

    Adults of freshwater ostracod Stenocypris major (Crustacea, Candonidae) were exposed for a four-day period in laboratory conditions to a range of copper (Cu), cadmium (Cd), zinc (Zn), lead (Pb), nickel (Ni), iron (Fe), aluminium (Al), and manganese (Mn) concentrations. Mortality was assessed, and median lethal times (LT50) and concentrations (LC50) were calculated. LT50 and LC50 increased with the decrease in mean exposure concentrations and times, respectively, for all metals. LC50s for 96 hours for Cu, Cd, Zn, Pb, Ni, Fe, Al, and Mn were 25.2, 13.1, 1189.8, 526.2, 19743.7, 278.9, 3101.9, and 510.2 μg/L, respectively. Metals bioconcentration in S. major increases with exposure to increasing concentrations, and Cd was the most toxic to S. major, followed by Cu, Fe, Mn, Pb, Zn, Al, and Ni (Cd>Cu>Fe>Mn>Pb>Zn>Al>Ni). Comparison of LC50 values for metals for this species with those for other freshwater crustacean reveals that S. major is equally or more sensitive to metals than most other tested crustacean. PMID:21559091

  11. Syntheses and applications of manganese-doped II-VI semiconductor nanocrystals

    NASA Astrophysics Data System (ADS)

    Yang, Heesun

    Syntheses, characterizations, and applications of two different Mn-doped semiconductor nanocrystals, ZnS:Mn and CdS:Mn/ZnS core/shell, were investigated. ZnS:Mn nanocrystals with sizes between 3 and 4 nm were synthesized via a competitive reaction chemistry. A direct current (dc) electroluminescent (EL) device having a hybrid organic/inorganic multilayer structure of an indium tin oxide (ITO) transparent conducting electrode, a (poly(3,4-ethylenedioxythiophene)/poly(styrenesulfonate) (PEDOT-PSS) and a poly(N-vinylcarbazole) (PVK) bilayer hole transport film, a ZnS:Mn nanocrystal layer, and Al dot contacts was demonstrated to emit blue (˜445 and ˜495 nm) from PVK and yellow (˜600 nm) light from Mn activator in ZnS. The EL emission spectrum was dependent upon both the voltage and Mn concentration, showing a decreasing nanocrystal to PVK emission ratio from 10 at 20 V to 4 at 28 V, and an increasing ratio from 1.3 at 0.40 mol % to 4.3 at 2.14 mol %. Mn-doped CdS core nanocrystals were produced ranging from 1.5 to 2.3 nm in diameter with a ZnS shell via a reverse micelle process. In contrast to CdS:Mn nanocrystals passivated by n-dodecanethiol, ZnS-passivated CdS:Mn (CdS:Mn/ZnS core/shell) nanocrystals were efficient and photostable. CdS:Mn/ZnS core/shell nanocrystals exhibited a quantum yield of ˜18%, and the photoluminescence (PL) intensity increased by 40% after 400 nm UV irradiation in air. X-ray photoelectron spectroscopy (XPS) data showed that UV irradiation of CdS:Mn/ZnS nanocrystals induces the photooxidation of the ZnS shell surface to ZnSO4. This photooxidation product is presumably responsible for the increased PL emission by serving as a passivating surface layer. Luminescent lifetime data from the core/shell nanocrystals could be fit with two exponential functions, with a time constant of ˜170 nsec for the defect-related centers and of ˜1 msec for the Mn centers. The CdS:Mn/ZnS nanocrystals with a core crystal diameter of 2.3 nm and a 0.4 nm thick ZnS shell were used as an electroluminescent material. EL devices were tested having a hybrid organic/inorganic multilayer structure of ITO//PEDOT-PSS//conjugated polymer//CdS:Mn/ZnS nanocrystal//Al. Orange from PVK device and green EL emission from poly(p-phenylene vinylene) (PPV) device were observed, respectively. These observations are shown to be consistent with the energy level diagrams of the EL devices. The CdS:Mn/ZnS core/shell quantum dots are not water-soluble because of their hydrophobicity. Silica-overcoated CdS:Mn/ZnS quantum dots were synthesized to create water-soluble quantum dots. The amorphous and porous silica layer did not significantly modify the optical and photophysical properties of CdS:Mn/ZnS quantum dots.

  12. The potential of selected macroalgal species for treatment of AMD at different pH ranges in temperate regions.

    PubMed

    Oberholster, Paul J; Cheng, Po-Hsun; Botha, Anna-Maria; Genthe, Bettina

    2014-09-01

    The metal bioaccumulation potential of selected macroalgae species at different pH ranges was study for usage as part of a possible secondary passive acid mine drainage (AMD) treatment technology in algae ponds. Two separate studies were conducted to determine the suitability of macroalgae for passive treatment when metabolic processes in macrophytes and microorganisms in constructed wetlands decrease during winter months. In the field study, the bioconcentration of metals (mg/kg dry weight) measured in the benthic macroalgae mats was in the following order: site 1. Oedogonium crassum Al > Fe > Mn > Zn; site 2. Klebsormidium klebsii, Al > Fe > Mn > Zn; site 3. Microspora tumidula, Fe > Al > Mn > Zn and site 4. M. tumidula, Fe > Mn > Al > Zn. In the laboratory study, cultured macroalgae K. klebsii, O. crassum and M. tumidula isolated from the field sampling sites were exposed to three different pH values (3, 5 and 7), while bioaccumulation of the metals, Al, Fe, Mn and Zn and glutathione S-transferase (GST) activity were measured in the different selected algae species at a constant water temperature of 14 °C. Bioaccumulation of Al was the highest for O. crassum followed by K. klebsii and M. tumidula (p < 0.0001). From the study it was evident that the highest metal bioaccumulation occurred in the macroalgae O. crassum at all three tested pH values under constant low water temperature. Copyright © 2014 Elsevier Ltd. All rights reserved.

  13. Toxicity of Metals to a Freshwater Snail, Melanoides tuberculata

    PubMed Central

    Shuhaimi-Othman, M.; Nur-Amalina, R.; Nadzifah, Y.

    2012-01-01

    Adult freshwater snails Melanoides tuberculata (Gastropod, Thiaridae) were exposed for a four-day period in laboratory conditions to a range of copper (Cu), cadmium (Cd), zinc (Zn), lead (Pb), nickel (Ni), iron (Fe), aluminium (Al), and manganese (Mn) concentrations. Mortality was assessed and median lethal times (LT50) and concentrations (LC50) were calculated. LT50 and LC50 increased with the decrease in mean exposure concentrations and times, respectively, for all metals. The LC50 values for the 96-hour exposures to Cu, Cd, Zn, Pb, Ni, Fe, Al, and Mn were 0.14, 1.49, 3.90, 6.82, 8.46, 8.49, 68.23, and 45.59 mg L−1, respectively. Cu was the most toxic metal to M. tuberculata, followed by Cd, Zn, Pb, Ni, Fe, Mn, and Al (Cu > Cd > Zn > Pb > Ni > Fe > Mn > Al). Metals bioconcentration in M. tuberculata increases with exposure to increasing concentrations and Cu has the highest accumulation (concentration factor) in the soft tissues. A comparison of LC50 values for metals for this species with those for other freshwater gastropods reveals that M. tuberculata is equally sensitive to metals. PMID:22666089

  14. Threshold pressure for mechanoluminescence of macrocrystals, microcrystals and nanocrystals of doped zinc sulphide

    NASA Astrophysics Data System (ADS)

    Chandra, B. P.; Chandra, V. K.; Jha, Piyush; Sonwane, V. D.

    2016-06-01

    The threshold pressure for elastico-mechanoluminescence (EML) of ZnS:Mn macrocrystals is 20 MPa, and ZnS:Cu,Al macrocrystals do not show ML during elastic deformation. However, the threshold pressure for EML of ZnS:Mn and ZnS:Cu,Cl microcrystals and nanocrystals is nearly 1 MPa. Thus, it seems that high concentration of defects in microcrystalline and nanocrystalline ZnS:Mn and ZnS:Cu,Cl produces disorder and distortion in lattice and changes the local crystal-structure near impurities, and consequently, the enhanced piezoelectric constant of local region produces EML for low value of applied pressure. The threshold pressure for the ML of ZnS:Mn and ZnS:Cu,Al single macrocrystals is higher because such crystals possess comparatively less number of defects near the impurities where the phase-transition is not possible and their ML is caused for high value of stress because the bulk piezoelectric constant is less. Thus, size-dependent threshold pressure for ML supports the origin of EML from piezoelectricity in local region of the crystals. The finding of present investigation may be useful in tailoring phosphors emitting intense EML of different colours.

  15. A Generic Metallographic Preparation Method for Magnesium Alloys

    DTIC Science & Technology

    2013-05-01

    treated castings or wrought alloys. Stains solid solution, leaves compound white. 9: 100-ml water 0.2–2-g oxalic acid For pure Mg and most alloys. Swab...water 2-g oxalic acid Pure Mg Mg-Mn Mg-Al, Mg-Al-Zn (Al+Znɝ%) Mg-Al, Mg-Al-Zn (Al+Zn>5%) Mg-Zn-Zr Mg-Th-Zr Swab...using a 100-ml ethanol, 10-ml distilled water, 10-ml acetic acid , and 5-g picric acid etchant. Immersed and using gentle agitation 5–20 s. Though not

  16. Geochemical studies of Fe, Mn, Co, As, Cr, Sb, Zn, Sc and V in surface sediments from Jiaozhou Bay

    NASA Astrophysics Data System (ADS)

    Wu, Run; Li, Pei-Quan; Miao, Lu-Tian; Zhang, Shu-Xin; Tian, Wei-Zhi

    1994-12-01

    The contents of nearly forty-elements in surface sediments in Jiaozhou Bay were determined using a Neutron Activation Analysis Technique (Grancini, et al., 1976; Li Peiquan et al., 1985, 1986; Li Xiuxia et al., 1986). This paper's detailed discussion on only nine elements (Fe, Mn, Co, Cr, Sc, As, Sb, Zn and V) includes their distributions, concentrations, correlationships, material sources, background, etc. Based on Zavaristski's classification method, Fe, Mn, Co, Cr and V belong to the second group; As and Sb to the eighth groups: Sc and Zn to the third and sixth groups. It was found that their notably good correlationship is mainly due to the similarity of their ionic structures and that their variation is controlled by the Fe content (except Mn). The source of sediments is mainly terristrial material, and the composition of sediment is similar to that of shale and shale+clay. The contents for a large number of elements are within the scope of the background level, but there still is pollution of Zn and Cr, at least in a few stations.

  17. PSEUDO-BINARY SYSTEMS INVOLVING RARE EARTH LAVES PHASES

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Wernick, J.H.; Haszko, S.E.; Dorsi, D.

    1962-06-01

    The phase relations in a number of pseudo-binary systems involving rare earth Laves phases were determined. Complete series of cubic solid-solutions occur in the DyMn/sub 2/HoMn/sub 2/, HoMn/sub 2/-HoFe/sub 2/, DyMn/sub 2/-DyFe/ sub 2/, HoMn/sub 2/-HoAl/ sub 2/, TbMn/sub 2/TbAl/sub 2/, and DyMn/sub 2/-DyAl/ sub 2/ pseudobinary systems. Deviations from linearity in the lattice constants with composition occur in all these systems. Complete series of cubic solidsolutions also exist in the GdAl/sub 2/-ErAl/sub 2/, GdAl/sub 2/-PrAl/sub 2/ , GdAl/sub 2/-NdAl/sub 2/, GdAl/sub 2/-DyAl/sub 2/, TbAl/sub 2/-NdAl/sub 2/, and T bAl/sub 2/-DyAl/sub 2/ systems. For these systems, no deviation from linearitymore » occurs in the lattice constants. For the DyFe/sub 2/-DyAl/sub 2/ and DyCo/sub 2/- DyAl/sub 2/ systems, two new ternary phases, DyFeAl and DyCoAl, form and have the MgZn/sub 2/ structure. Their structures were determined from x-ray powder data only. The electronic state giving rise to the formation of these ternary phases is discussed qualitatively. For the DyMn/sub 2/TmMn/sub 2/ system, the range of composition in which the cubic MgCu/sub 2/ and hexagonal MgZn/sub 2/ structures exist are reported. No complete series of solid solutions or intermediate phases are formed in the DyNi/sub 2/-DyAl/sub 2/ system. (auth)« less

  18. Grain Refinement of Al-Si-Fe-Cu-Zn-Mn Based Alloy by Al-Ti-B Alloy and Its Effect on Mechanical Properties.

    PubMed

    Yoo, Hyo-Sang; Kim, Yong-Ho; Jung, Chang-Gi; Lee, Sang-Chan; Lee, Seong-Hee; Son, Hyeon-Taek

    2018-03-01

    We investigated the effects of Al-5.0wt%Ti-1.0wt%B addition on the microstructure and mechanical properties of the as-extruded Al-0.15wt%Si-0.2wt%Fe-0.3wt%Cu-0.15wt%Zn-0.9wt%Mn based alloys. The Aluminum alloy melt was held at 800 °C and then poured into a mould at 200 °C. Aluminum alloys were hot-extruded into a rod that was 12 mm in thickness with a reduction ratio of 38:1. AlTiB addition to Al-0.15Si-0.2Fe-0.3Cu-0.15Zn-0.9Mn based alloys resulted in the formation of Al3Ti and TiB2 intermetallic compounds and grain refinement. With increasing of addition AlTiB, ultimate tensile strength increased from 93.38 to 99.02 to 100.01 MPa. The tensile strength of the as-extruded alloys was improved due to the formation of intermetallic compounds and grain refinement.

  19. Laser Surface Alloying of Aluminum for Improving Acid Corrosion Resistance

    NASA Astrophysics Data System (ADS)

    Jiru, Woldetinsay Gutu; Sankar, Mamilla Ravi; Dixit, Uday Shanker

    2018-04-01

    In the present study, laser surface alloying of aluminum with magnesium, manganese, titanium and zinc, respectively, was carried out to improve acid corrosion resistance. Laser surface alloying was conducted using 1600 and 1800 W power source using CO2 laser. Acid corrosion resistance was tested by dipping the samples in a solution of 2.5% H2SO4 for 200 h. The weight loss due to acid corrosion was reduced by 55% for AlTi, 41% for AlMg alloy, 36% for AlZn and 22% for AlMn alloy. Laser surface alloyed samples offered greater corrosion resistance than the aluminum substrate. It was observed that localized pitting corrosion was the major factor to damage the surface when exposed for a long time. The hardness after laser surface alloying was increased by a factor of 8.7, 3.4, 2.7 and 2 by alloying with Mn, Mg, Ti and Zn, respectively. After corrosion test, hardness was reduced by 51% for AlTi sample, 40% for AlMg sample, 41.4% for AlMn sample and 33% for AlZn sample.

  20. Phase composition and corrosion resistance of magnesium alloys

    NASA Astrophysics Data System (ADS)

    Morozova, G. I.

    2008-03-01

    The effects of phase composition of castable experimental and commercial alloys based on the Mg-Al, Mg-Al-Mn, Mg-Al-Zn-Mn, and Mg-Zn-Zr systems and of the form of existence of iron and hydrogen admixtures on the rate of corrosion of the alloys in 3% solution of NaCl are studied. The roles of heat treatment in the processes of hydrogen charging and phase formation in alloy ML5pch and of hydrogen in the process of formation of zirconium hydrides and zinc zirconides in alloys of the Mg-Zn-Zr system and their effect on the corrosion and mechanical properties of alloy ML12 are discussed.

  1. Molecular structure of Mg-Al, Mn-Al and Zn-Al halotrichites-type double sulfates--an infrared spectroscopic study.

    PubMed

    Palmer, Sara J; Frost, Ray L

    2011-05-01

    Near infrared (NIR), X-ray diffraction (XRD) and infrared (IR) spectroscopy have been applied to halotrichites of the formula MgAl(2)(SO(4))(4)·22H(2)O, MnAl(2)(SO(4))(4)·22H(2)O and ZnAl(2)(SO(4))(4)·22H(2)O. Comparison of the halotrichites in different spectral regions has shown that the incorporation of a divalent transition metal into the halotrichite structure causes a shift in OH stretching band positions to lower wavenumbers. Therefore, an increase of the hydrogen bond strength of the bonded water is observed for divalent cations with a larger molecular mass. XRD has confirmed the formation of halotrichite for all three samples and characteristic peaks of halotrichite have been identified for each halotrichite-type compound. It has been observed that Mg-Al and Mn-Al halotrichite are very similar in structure, while Zn-Al showed several differences particularly in the NIR spectra. This work has shown that compounds with halotrichite structures can be synthesised and characterised by infrared and NIR spectroscopy. Copyright © 2011 Elsevier B.V. All rights reserved.

  2. Spinel, YbFe2O4, and Yb2Fe3O7 types of structure for compounds in the In2O3 and Sc2O3-A2O3-BO systems (A: Fe, Ga, or Al; B: Mg, Mn, Fe, Ni, Cu, or Zn) at temperatures over 1000C

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Kimizuka, N.; Mohri, T.

    In the Sc2O3-Ga2O3-CuO, Sc2O3-Ga2O3-ZnO, and Sc2O3-Al2O3-CuO systems, ScGaCuO4, ScGaZnO4, and ScAlCuO4 with the YbFe2O4-type structure and Sc2Ga2CuO7 with the Yb2Fe3O7-type structure were obtained. In the In2O3-A2O3-BO systems (A: Fe, Ga, or Al; B: Mg, Mn, Fe, Ni, or Zn), InGaFeO4, InGaNiO4, and InFeT MgO4 with the spinel structure, InGaZnO4, InGaMgO4, and InAl-CuO4 with the YbFe2O4-type structure, and In2Ga2MnO7 and In2Ga2ZnO7 with the Yb2Fe3O7-type structure were obtained. InGaMnO4 and InFe2O4 had both the YbFe2O4-type and spinel-type structures. The revised classification for the crystal structures of AB2O4 compounds is presented, based upon the coordination numbers of constituent A and B cations. 5more » references, 2 tables.« less

  3. White LED based on CaAl2Si2O8:Eu2+ Mn2+ phosphor and CdS/ZnS quantum dots

    NASA Astrophysics Data System (ADS)

    Shen, Changyu; Zhong, Chuan; Hou, Qianglong; Li, Ke

    2011-02-01

    Core/shell CdS/ZnS quantum dots (QDs) with the emission wavelength of 610nm, was synthesized by thermal deposition using cadmium oxide and selenium as precursors in a hot lauric acid and hexadecylamine trioctylphosphine oxide hybrid. CaAl2Si2O8:Eu2+ Mn2+ phosphor was synthesized by high-temperature solid state reaction at 1290 °C for 2 hours under the H2 reducing atmosphere, and X-ray powder diffraction analysis confirmed the formation of it. It has two emission bands peaking at 420 nm and 580nm originated from the transition 5d to 4f of Eu2+ and 4T1-6A1 of Mn2+, respectively. Blends of CaAl2Si2O8:Eu2+,Mn2+ phosphor and CdS/ZnS QDs exhibited the prominent spectral evolution with an increasing content of QDs. A hybrid white LED, which combines a blue LED with the blend of CaAl2Si2O8:Eu2+ Mn2+ phosphor and QDs with a weight ratio of 2:1, with the CIE coordinate of (0.3183, 0.3036) and CRI of 85 was obtained.

  4. Alkali-deficient tourmaline from the Sullivan Pb-Zn-Ag deposit, British Columbia

    USGS Publications Warehouse

    Jiang, S.-Y.; Palmer, M.R.; Slack, J.F.

    1997-01-01

    Alkali-deficient tourmalines are found in albitized rocks from the hanging-wall of the Sullivan Pb-Zn-Ag deposit (British Columbia, Canada). They approximate the Mg-equivalent of foitite with an idealized formula D???(Mg2Al)Al6Si6O18(BO 3)3(OH)4. Major chemical substitutions in the tourmalines are the alkali-defect type [Na*(x) + Mg*(Y) = ???(X) + Al(Y)] and the uvite type [Na*(X) + Al(Y) = Ca(X) + Mg*(Y)], where Na* = Na + K, Mg* = Mg + Fe + Mn. The occurrence of these alkali-deficient tourmalines reflects a unique geochemical environment that is either alkali-depleted overall or one in which the alkalis preferentially partitioned into coexisting minerals (e.g. albite). Some of the alkali-deficient tourmalines have unusually high Mn contents (up to 1.5 wt.% MnO) compared to other Sullivan tourmalines. Manganese has a strong preference for incorporation into coexisting garnet and carbonate at Sullivan, thus many tourmalines in Mn-rich rocks are poor in Mn (<0.2 wt.% MnO). It appears that the dominant controls over the occurrence of Mn-rich tourmalines at Sullivan are the local availability of Mn and the lack of other coexisting minerals that may preferentially incorporate Mn into their structures.

  5. Crystal structure of hexagonal MnAl(4).

    PubMed

    Pauling, L

    1987-06-01

    A structure is proposed for the hexagonal form of MnAl(4), with a(H) = 28.4 A and c(H) = 12.43 A, on the basis of a high-resolution electron micrograph and comparison with crystals of known structures. The proposed structure involves seven 104-atom complexes of 20 Friauf polyhedra, sharing some atoms with one another. It is closely related to the 23.36-A cubic structure of MnAl(4) and to the 14.19-A cubic structure of Mg(32)(Al,Zn)(49).

  6. Manganese containing layer for magnetic recording media

    DOEpatents

    Lambeth, David N.; Lee, Li-Lien; Laughlin, David E.

    1999-01-01

    The present invention provides for a magnetic recording media incorporating Mn-containing layers between a substrate and a magnetic layer to provide media having increased coercivity and lower noise. The Mn-containing layer can be incorporated in a rotating, translating or stationary recording media to operate in conjunction with magnetic transducing heads for recording and reading of magnetic data, as well as other applications. The magnetic recording medium of the invention preferably includes a Co or Co alloy film magnetic layer, and Mn-containing layer, preferably comprised of VMn, TiMn, MnZn, CrMnMo, CrMnW, CrMnV, and CrMnTi, and most preferably a CrMn alloy, disposed between the substrate and the magnetic layer to promote an epitaxial crystalline structure in the magnetic layer. The medium can further include seed layers, preferably polycrystalline MgO for longitudinal media, underlayers, and intermediate layers. Underlayers and intermediate layers are comprised of materials having either an A2 structure or a B2-ordered crystalline structure disposed between the seed layer and the magnetic layer. Materials having an A2 structure are preferably Cr or Cr alloys, such as CrV, CrMo, CrW and CrTi. Materials having a B2-ordered structure having a lattice constant that is substantially comparable to that of Cr, such as those preferably selected from the group consisting of NiAl, AILCo, FeAl, FeTi, CoFe, CoTi, CoHf, CoZr, NiTi, CuBe, CuZn, A-LMn, AlRe, AgMg, and Al.sub.2 FeMn.sub.2, and is most preferably FeAl or NiAl.

  7. Trace elements in muscle of three fish species from Todos os Santos Bay, Bahia State, Brazil.

    PubMed

    de Santana, Carolina Oliveira; de Jesus, Taíse Bomfim; de Aguiar, William Moura; de Jesus Sant'anna Franca-Rocha, Washington; Soares, Carlos Alberto Caroso

    2017-03-01

    In this study, an analysis was performed on the concentrations of the trace elements Al, As, Ba, Cd, Co, Cr, Cu, Fe, Mn, Ni, Pb, V, and Zn in muscle of two carnivorous and one planktivorous fish species collected at Todos os Santos Bay (BTS). The accumulation order of the trace elements in Lutjanus analis was Al >Zn >Fe >Cr >Ba >Ni. In Cetengraulis edentulus, the order was Al >Fe >Zn >Cr >Ni >Mn >As. In the species Diapterus rhombeus, the order was Al >Fe >Zn >Cr >Ni >Mn >Cd. To determine the risk related to the consumption of fish, toxicity guidelines were used as standard references. It was observed that the species C. edentulus contained concentrations of As exceeding WHO limits, but these concentrations were acceptable according to the Agência Nacional de Vigilância Sanitária (ANVISA) guidelines. Cd levels were found only in D. rhombeus and in low concentrations according to the determinations of WHO and ANVISA. Pb levels were not detected in any of the three fish species. The analyzed elements did not differ statistically according to the species and feeding habits. The results point to possible risks of human contamination by As related to the consumption of the fish species C. edentulus from the BTS.

  8. ONR Tokyo Scientific Bulletin. Volume 5, Number 1, January-March 1980,

    DTIC Science & Technology

    1980-03-01

    alloys studied are in die AI-Zn, Al -Mg, Al -Si. Al - Cu . Cu - Al . and Cu -Fe... alloys Digital processing Measuring N 20. Abstract (cont.) with certain reports also being contributed by visiting stateside scientist. Occasionally a...atomic absorption spectrophotometer with tubes for the determination of Zn, Cu , Pb, Cr, Fe, Mg, Mn, Al , Co, Cd, Si, Ti, Zr, Ga, Au, Ag, Ni, Na, and

  9. Crystal structure of hexagonal MnAl4

    PubMed Central

    Pauling, Linus

    1987-01-01

    A structure is proposed for the hexagonal form of MnAl4, with aH = 28.4 Å and cH = 12.43 Å, on the basis of a high-resolution electron micrograph and comparison with crystals of known structures. The proposed structure involves seven 104-atom complexes of 20 Friauf polyhedra, sharing some atoms with one another. It is closely related to the 23.36-Å cubic structure of MnAl4 and to the 14.19-Å cubic structure of Mg32(Al,Zn)49. Images PMID:16593837

  10. High strength cast aluminum alloy development

    NASA Astrophysics Data System (ADS)

    Druschitz, Edward A.

    The goal of this research was to understand how chemistry and processing affect the resulting microstructure and mechanical properties of high strength cast aluminum alloys. Two alloy systems were investigated including the Al-Cu-Ag and the Al-Zn-Mg-Cu systems. Processing variables included solidification under pressure (SUP) and heat treatment. This research determined the range in properties that can be achieved in BAC 100(TM) (Al-Cu micro-alloyed with Ag, Mn, Zr, and V) and generated sufficient property data for design purposes. Tensile, stress corrosion cracking, and fatigue testing were performed. CuAl2 and Al-Cu-Fe-Mn intermetallics were identified as the ductility limiting flaws. A solution treatment of 75 hours or longer was needed to dissolve most of the intermetallic CuAl 2. The Al-Cu-Fe-Mn intermetallic was unaffected by heat treatment. These results indicate that faster cooling rates, a reduction in copper concentration and a reduction in iron concentration might increase the ductility of the alloy by decreasing the size and amount of the intermetallics that form during solidification. Six experimental Al-Zn-Mg-Cu series alloys were produced. Zinc concentrations of 8 and 12wt% and Zn/Mg ratios of 1.5 to 5.5 were tested. Copper was held constant at 0.9%. Heat treating of the alloys was optimized for maximum hardness. Al-Zn-Mg-Cu samples were solution treated at 441°C (826°F) for 4 hours before ramping to 460°C (860°F) for 75 hours and then aged at 120°C (248°F) for 75 hours. X-ray diffraction showed that the age hardening precipitates in most of these alloys was the T phase (Mg32Zn 31.9Al17.1). Tensile testing of the alloys showed that the best mechanical properties were obtained in the lowest alloy condition. Chilled Al-8.2Zn-1.4Mg-0.9Cu solidified under pressure resulted in an alloy with a yield strength of 468MPa (68ksi), tensile strength of 525MPa (76ksi) and an elongation of 9%.

  11. Spatial distribution and metal contamination in the coastal sediments of Al-Khafji area, Arabian Gulf, Saudi Arabia.

    PubMed

    Alharbi, Talal; Alfaifi, Hussain; Almadani, Sattam A; El-Sorogy, Abdelbaset

    2017-11-13

    To document the spatial distribution and metal contamination in the coastal sediments of the Al-Khafji area in the northern part of the Saudi Arabian Gulf, 27 samples were collected for Al, V, Cr, Mn, Cu, Zn, Cd, Pb, Hg, Sr, As, Fe, Co, and Ni analysis using inductively coupled plasma-mass spectrometer (ICP-MS). The results revealed the following descending order of the metal concentrations: Sr > Fe > Al > As > Mn > Ni > V > Zn > Cr > Cu > Pb > Co > Hg > Cd. Average levels of enrichment factor of Sr, As, Hg, Cd, Ni, V, Cu, Co, and Pb were higher than 2 (218.10, 128.50, 80.94, 41.50, 12.31, 5.66, 2.95, 2.90, and 2.85, respectively) and that means the anthropogenic sources of these metals, while Al, Zn, Cr and Mn have enrichment factor less than 2, which implies natural sources. Average values of Sr, Hg, Cd, Cr, Ni, and As in the coastal sediments of Al-Khafji area were mostly higher than the values recorded from the background shale and earth crust and from those results along coasts of the Caspian Sea and the Mediterranean Sea. The highest levels of Cu in the northern part of the studied coastline might be due to Al-Khafji desalination plant, while levels of Al, Ni, Cr, Fe, Mn, Pb, and Zn in the central part may be a result of landfilling and industrial sewage. The highest levels of As, Cd, Co, Cu, Hg, and V in the southern part seem to be due to oil pollutants from Khafji Joint Operations (KJO). The higher values of Sr in the studied sediments in general and particularly in locality 7 could relate to the hypersalinity and aragonitic composition of the scleractinian corals abundant in that area.

  12. A new mineral species ferricoronadite, Pb[Mn6 4+(Fe3+, Mn3+)2]O16: mineralogical characterization, crystal chemistry and physical properties

    NASA Astrophysics Data System (ADS)

    Chukanov, Nikita V.; Aksenov, Sergey M.; Jančev, Simeon; Pekov, Igor V.; Göttlicher, Jörg; Polekhovsky, Yury S.; Rusakov, Vyacheslav S.; Nelyubina, Yuliya V.; Van, Konstantin V.

    2016-07-01

    A new mineral ferricoronadite with the simplified formula Pb(Mn6 4+Fe2 3+)O16 was discovered in the orogenetic zone related to the "Mixed Series" metamorphic complex near the Nežilovo village, Pelagonian massif, Republic of Macedonia. Associated minerals are franklinite, gahnite, hetaerolite, roméite, almeidaite, Mn-analogue of plumboferrite, zincohögbomite analogue with Fe3+ > Al, zincochromite, Zn-bearing talc, Zn-bearing muscovite, baryte, quartz and zircon. Ferricoronadite is a late hydrothermal mineral forming veinlets up to 8 mm thick in granular aggregate predominantly composed by zinc-dominant spinels. The new mineral is opaque, black, with brownish black streak. The luster is strong submetallic to metallic. The micro-indentation hardness is 819 kg/mm2. Distinct cleavage is observed on (100). Ferricoronadite is brittle, with uneven fracture. The density calculated from the empirical formula is 5.538 g/cm3. In reflected light, ferricoronadite is light gray. The reflectance values [ R max/ R min, % ( λ, nm)] are: 28.7/27.8 (470), 27.6/26.6 (546), 27.2/26.1 (589), 26.5/25.5 (650). The IR spectrum shows the absence of H2O and OH groups. According to the Mössbauer spectrum, all iron is trivalent. The Mn K-edge XANES spectroscopy shows that Mn is predominantly tetravalent, with subordinate Mn3+. The chemical composition is (wt%; electron microprobe, Mn apportioned between MnO2 and Mn2O3 based on the charge-balance requirement): BaO 5.16, PbO 24.50, ZnO 0.33, Al2O3 0.50, Mn2O3 9.90, Fe2O3 11.45, TiO2 4.19, MnO2 44.81, total 100.84. The empirical formula based on 8 cations Mn + Fe + Ti + Al + Zn pfu is Pb1.03Ba0.32(Mn 4.85 4+ Fe 1.35 3+ Mn 1.18 3+ Ti0.49Al0.09Zn0.04)Σ8.00O16. The crystal structure was determined using single-crystal X-ray diffraction data. The new mineral is tetragonal, space group I4/ m, a = 9.9043(7), c = 2.8986(9) Å, V = 284.34(9) Å3, Z = 1. In ferricoronadite, double chains of edge-sharing (Mn, Fe, Ti)-centered octahedra are connected via common vertices to form a pseudo-framework with tunnels containing large cations Pb and Ba. The strongest lines of the powder X-ray diffraction pattern [ d, Å ( I, %) ( hkl)] are: 3.497 (33) (220), 3.128 (100) (-130, 130), 2.424 (27) (-121, 121), 2.214 (23) (240, -240), 2.178 (17) (031), 1.850 (15) (141, -141), 1.651 (16) (060), 1.554 (18) (-251, 251). Ferricoronadite is named as an analogue of coronadite Pb(Mn6 4+Mn2 3+)O16 with the major charge-compensating octahedral cation Fe3+ instead of Mn3+.

  13. Evaluation of elemental enrichments in surface sediments off southwestern Taiwan

    NASA Astrophysics Data System (ADS)

    Chen, Chen-Tung; Kandasamy, Selvaraj

    2008-05-01

    Surface slices of 20 sediment cores, off southwestern Taiwan, and bed sediment of River Kaoping were measured for major and trace elements (Al, As, Ca, Cd, Cl, Cr, Cu, Fe, K, Mg, Mn, Na, Ni, P, Pb, S, Si, Ti, V, and Zn) to evaluate the geochemical processes responsible for their distribution, including elemental contamination. Major element/Al ratio and mean grain size indicate quartz-dominated, coarse grained sediments that likely derived from sedimentary rocks of Taiwan and upper crust of Yangtze Craton. Bi-plot of SiO2 versus Fe2O{3/T} suggests the possible iron enrichment in sediments of slag dumping sites. Highest concentrations of Cr, Mn, P, S, and Zn found in sediments of dumping sites support this. Correlation analysis shows dual associations, detrital and organic carbon, for Cr, P, S, and V with the latter association typical for sediments in dumping sites. Normalization of trace elements to Al indicates high enrichment factors (>2) for As, Cd, Pb, and Zn, revealing contamination. Factor analysis extracted four geochemical associations with the principal factor accounted for 25.1% of the total variance and identifies the combined effects of dumped iron and steel slag-induced C-S-Fe relationship owing to authigenic precipitation of Fe-Mn oxyhydroxides and/or metal sulfides, and organic matter complexation of Fe, Mn, Ca, Cr, P, and V. Factors 2, 3, and 4 reveal detrital association (Ti, Al, Ni, Pb, Cu, and V), effect of sea salt (Cl, Mg, Na, and K) and anthropogenic component (As and Zn)-carbonate link, respectively, in the investigated sediments.

  14. Comparison of the Microstructure and Flux Pinning Properties of Polycrystalline YBa2Cu3O7-d Containing Zn0.95Mn0.05O or Al2O3 Nanoparticles

    NASA Astrophysics Data System (ADS)

    Al-Mohsin, R. A.; Al-Otaibi, A. L.; Almessiere, M. A.; Al-badairy, H.; Slimani, Y.; Ben Azzouz, F.

    2018-07-01

    Here we compare the microstructure and flux pinning properties of polycrystalline YBa2Cu3O7-d (Y-123 or YBCO) containing either Al2O3 or Zn0.95Mn0.05O nanoparticles. Samples were prepared using a standard solid-state reaction process, and nanoparticles were added up to a concentration of 0.1 wt%. The crystal structure, microstructure, electrical and magnetic properties were analyzed using X-ray diffraction, scanning electron microscopy and transmission electron microscopy (TEM), and electrical resistivity and DC magnetization measurements, respectively. TEM observations showed that the addition of Zn0.95Mn0.05O resulted in a high density of fine twins and a variety of interacting microstructures, while Al2O3 addition resulted in a high density of Al-rich nanoscale inhomogeneities embedded in the Y-123 matrix. Flux pinning forces were determined, and predominant pinning mechanisms in the prepared samples were proposed. We evaluated the superconducting properties of YBCO considering the effects of adding insulating or magnetic nanoparticles.

  15. Comparison of the Microstructure and Flux Pinning Properties of Polycrystalline YBa2Cu3O7-d Containing Zn0.95Mn0.05O or Al2O3 Nanoparticles

    NASA Astrophysics Data System (ADS)

    Al-Mohsin, R. A.; Al-Otaibi, A. L.; Almessiere, M. A.; Al-badairy, H.; Slimani, Y.; Ben Azzouz, F.

    2018-03-01

    Here we compare the microstructure and flux pinning properties of polycrystalline YBa2Cu3O7-d (Y-123 or YBCO) containing either Al2O3 or Zn0.95Mn0.05O nanoparticles. Samples were prepared using a standard solid-state reaction process, and nanoparticles were added up to a concentration of 0.1 wt%. The crystal structure, microstructure, electrical and magnetic properties were analyzed using X-ray diffraction, scanning electron microscopy and transmission electron microscopy (TEM), and electrical resistivity and DC magnetization measurements, respectively. TEM observations showed that the addition of Zn0.95Mn0.05O resulted in a high density of fine twins and a variety of interacting microstructures, while Al2O3 addition resulted in a high density of Al-rich nanoscale inhomogeneities embedded in the Y-123 matrix. Flux pinning forces were determined, and predominant pinning mechanisms in the prepared samples were proposed. We evaluated the superconducting properties of YBCO considering the effects of adding insulating or magnetic nanoparticles.

  16. ``Amarna blue'' painted on ancient Egyptian pottery

    NASA Astrophysics Data System (ADS)

    Uda, M.; Nakamura, M.; Yoshimura, S.; Kondo, J.; Saito, M.; Shirai, Y.; Hasegawa, S.; Baba, Y.; Ikeda, K.; Ban, Y.; Matsuo, A.; Tamada, M.; Sunaga, H.; Oshio, H.; Yamashita, D.; Nakajima, Y.; Utaka, T.

    2002-04-01

    "Amarna blue" pigments (18 Dynasty, c. 1400 BC) painted on pottery fragments were investigated using the PIXE, XRF and XRD methods in laboratories and also using a portable type of X-ray spectrometer at the sites of excavation. On the blue-colored part enrichment of Na, Al, S, Cl, Ca, Mn, Co, Ni and Zn was found using X-ray spectroscopy, and CaSO 4, NaCl and Co(M)Al 2O 4, M denoting Mn, Fe, Ni and Zn, were found by the help of X-ray diffraction. This means that Amarna blue is a mixture of CaSO 4 and Co(M)Al 2O 4, at least in part.

  17. Formation of the structure and properties of an Mg-Al-Zn-Mn alloy during plastic deformation by rolling

    NASA Astrophysics Data System (ADS)

    Bozhko, S. A.; Betsofen, S. Ya.; Kolobov, Yu. R.; Vershinina, T. N.

    2015-03-01

    The laws of formation of an ultrafine structure in an Mg-Al-Zn-Mn alloy (MA5 alloy) under severe plastic deformation have been studied during lengthwise section rolling at a strain e = 1.59. The deformation behavior and the physical factors of anisotropy of yield strength during compression tests in various directions with respect to axis of rolling are analyzed. The role of crystallographic texture and twinning processes in the generation of strength processes and the development of plastic deformation of the alloy is analyzed.

  18. Removal of metals from landfill leachate by sorption to activated carbon, bone meal and iron fines.

    PubMed

    Modin, Hanna; Persson, Kenneth M; Andersson, Anna; van Praagh, Martijn

    2011-05-30

    Sorption filters based on granular activated carbon, bone meal and iron fines were tested for their efficiency of removing metals from landfill leachate. Removal of Al, As, Ca, Cd, Co, Cr, Cu, Fe, Hg, Mg, Mn, Mo, Ni, Pb, Sr and Zn were studied in a laboratory scale setup. Activated carbon removed more than 90% of Co, Cr, Cu, Fe, Mn and Ni. Ca, Pb, Sr and Zn were removed but less efficiently. Bone meal removed over 80% of Cr, Fe, Hg, Mn and Sr and 20-80% of Al, Ca, Cu, Mo, Ni, Pb and Zn. Iron fines removed most metals (As, Ca, Co, Cr, Cu, Fe, Mg, Mn, Pb, Sr and Zn) to some extent but less efficiently. All materials released unwanted substances (metals, TOC or nutrients), highlighting the need to study the uptake and release of a large number of compounds, not only the target metals. To remove a wide range of metals using these materials two or more filter materials may need to be combined. Sorption mechanisms for all materials include ion exchange, sorption and precipitation. For iron fines oxidation of Fe(0) seems to be important for metal immobilisation. Copyright © 2011 Elsevier B.V. All rights reserved.

  19. Effect of adsorbed metals ions on the transport of Zn- and Ni-EDTA complexes in a sand and gravel aquifer

    USGS Publications Warehouse

    Kent, D.B.; Davis, J.A.; Anderson, L.C.D.; Rea, B.A.; Coston, J.A.

    2002-01-01

    Adsorption, complexation, and dissolution reactions strongly influenced the transport of metal ions complexed with ethylenediaminetetraacetic acid (EDTA) in a predominantly quartz-sand aquifer during two tracer tests conducted under mildly reducing conditions at pH 5.8 to 6.1. In tracer test M89, EDTA complexes of zinc (Zn) and nickel (Ni), along with excess free EDTA, were injected such that the lower portion of the tracer cloud traveled through a region with adsorbed manganese (Mn) and the upper portion of the tracer cloud traveled through a region with adsorbed Zn. In tracer test S89, Ni- and Zn-EDTA complexes, along with excess EDTA complexed with calcium (Ca), were injected into a region with adsorbed Mn. The only discernable chemical reaction between Ni-EDTA and the sediments was a small degree of reversible adsorption leading to minor retardation. In the absence of adsorbed Zn, the injected Zn was displaced from EDTA complexes by iron(III) [Fe(III)] dissolved from the sediments. Displacement of Zn by Fe(III) on EDTA became increasingly thermodynamically favorable with decreasing total EDTA concentration. The reaction was slow compared to the time-scale of transport. Free EDTA rapidly dissolved aluminum (Al) from the sediments, which was subsequently displaced slowly by Fe. In the portion of tracer cloud M89 that traveled through the region contaminated with adsorbed Zn, little displacement of Zn complexed with EDTA was observed, and Al was rapidly displaced from EDTA by Zn desorbed from the sediments, in agreement with equilibrium calculations. In tracer test S89, desorption of Mn dominated over the more thermodynamically favorable dissolution of Al oxyhydroxides. Comparison with results from M89 suggests that dissolution of Al oxyhydroxides in coatings on these sediment grains by Ca-EDTA was rate-limited whereas that by free EDTA reached equilibrium on the time-scale of transport. Rates of desorption are much faster than rates of dissolution of Fe oxyhydroxides from sediment-grain surfaces and, therefore, adsorbed metal ions can strongly influence the speciation of ligands like EDTA in soils and sediments, especially over small temporal and spatial scales. Copyright ?? 2002 Elsevier Science Ltd.

  20. [Spatial variations of heavy metals in precipitation at Mount Taishan region].

    PubMed

    Wang, Yan; Liu, Xiao-Huan; Jin, Ling-Ren; Yue, Tai-Xing; Wang, De-Zhong; Wang, Wen-Xing

    2007-11-01

    Zn, Al, Mn, Fe, Pb, Cu, Ni, Cr, As, Cd in rain samples collected from two sites at Mount Taishan region were determined by ICP-MS, to evaluate the spatial variation characteristics of heavy metals in precipitation. Individual rain events were sampled for one whole year from Jan. to Dec. 2006. High concentrations of heavy metals were found at both sites, indicating serious heavy metal pollution. Zn was the most abundant element, accounting for 54% - 57% of the total metals concentrations. Its volume-weighted mean concentrations of precipitation at Mt-top and Mt-foot sites were 92.94 microg/L and 70.41 microg/L respectively. The following elements were Fe, Al and Mn and their concentrations were much higher than toxic heavy metals (As, Cd and Cd) except Pb (8.04 microg/L and 7.79 microg/L at two sites respectively). Comparison results between two sites suggested that heavy metal characteristics of precipitation at two sites were different, due to the influences of different ambient air conditions. Correlation analysis between two sites showed that Al, Mn, Fe, As, Cd, Pb influenced by air mass origin greatly, while Ni, Cu, Zn affected by other different factors.

  1. Combining cross flow ultrafiltration and diffusion gradients in thin-films approaches to determine trace metal speciation in freshwaters

    NASA Astrophysics Data System (ADS)

    Liu, Ruixia; Lead, Jamie R.; Zhang, Hao

    2013-05-01

    Cross flow ultrafiltration (CFUF) and diffusive gradients in thin films (DGT) with open pore gel (OP) and restricted pore gel (RP) were used to measure trace metal speciation in selected UK freshwaters. The proportions of metals present in particulate forms (>1 μm) varied widely between 40-85% Pb, 60-80% Al, 7-56% Mn, 10-49% Cu, 0-55% Zn, 20-38% Cr, 20-30% Fe, 6-25% Co, 5-22% Cd and <7% Ni. In the colloidal fraction (2 kDa-1 μm) values varied between 53-91% Pb, 33-55% Al, 21-55% Cu, 20-44% Fe, 34-36% Cr, 20-40% Cd, 7-28% Co and Ni, 2-32% Zn and <8% Mn. Wide variations were also observed in the ultrafiltered fraction (<2 kDa). These results indicated that colloids indeed influenced the occurrence and transport of Al, Fe, Cr, Co, Ni, Cu, Zn, Cr and Pb metals in rivers, while inorganic or organic colloids did not exert an important control on Mn transport in the selected freshwaters. Of total species, total labile metal measured by DGT-OP accounted for 1.4-50% for Al, Fe, Co, Ni, Cu, Cd and Pb in all selected waters. Of these metals total labile Pb concentration was the lowest with value less than 1.4% although this value slightly increased after deducting particulate fractions. In some waters, a majority of total Mn, Zn and Cr is DGT labile, in which the DGT labile Mn fraction accounted for 98-118% of the total dissolved phase. In most cases, the inorganic labile concentration measured by DGT-RP was lower than the total labile metal concentration. By the combination of CFUF and DGT techniques, the concentrations of total labile and inorganic labile metal species in CFUF-derived truly dissolved phase were measured in four water samples. 100% of ultrafiltered Mn species was found to be total DGT labile. The proportions of total labile metal species were lower than those of ultrafiltered fraction for Al, Fe, Co, Ni, Cu, Cd and Pb in all selected waters, and Cr and Zn in some cases, indicating a large amount of natural complexing ligands with smaller size for the metals to form kinetically inert species or thermodynamically stable complexes. Observed discrepancies in metal speciation between metals and within sampling sites were related to the differences in the characteristics of the metals and the nature of water sources.

  2. Survey on composition and bioconcentration potential of 12 metallic elements in King Bolete (Boletus edulis) mushroom that emerged at 11 spatially distant sites.

    PubMed

    Falandysz, Jerzy; Frankowska, Aneta; Jarzynska, Grazyna; Dryzałowska, Anna; Kojta, Anna K; Zhang, Dan

    2011-01-01

    This paper provides data on baseline concentrations, interrelationships and bioconcentration potential of 12 metallic elements by King Bolete collected from 11 spatially distant sites across Poland. There are significant differences in concentrations of metals (Al, Ba, Ca, Cd, Cu, Fe, K, Mg, Mn, Na, Sr, Zn) and their bioconcentration potential in King Bolete Boletus edulis at 11 spatially distant sites surveyed across Poland. These have resulted from significant geographical differences in trace metal concentrations in a layer (0-10 cm) of organic and mineral soil underneath to fruiting bodies and possible local bioavailabilities of macro- (Ca, K, Mg, Na) and trace metals (Al, Ba, Cd, Cu, Fe, Mn, Sr, Zn) to King Bolete. The use of highly appreciated wild-grown edible King Bolete mushroom has established a baseline measure of regional minerals status, heavy metals pollution and assessment of intake rates for wild mushroom dish fanciers against which future changes can be compared. Data on Cd, Cu and Zn from this study and from literature search can be useful to set the maximum limit of these metals in King Bolete collected from uncontaminated (background) areas. In this report also reviewed are data on Al, Ba, Ca, Cd, Cu, Fe, K, Mg, Mn, Na, Sr and Zn accumulation in King Bolete.

  3. [The eye and nutrition].

    PubMed

    Amemiya, T

    1999-12-01

    To examine the effect of vitamins and trace elements on ocular tissue. Rats or mice were fed diets deficient in the trace elements Zn, Cu, Mn, Se, Mg, and Cr or in vitamins A, B12, C, and E. In some rats Al and vitamin A were injected in excessive amounts. We studied the conjunctiva, cornea, retina, and optic nerve with a light microscope, transmission and scanning electron microscopes, an energy dispersive X-ray analyser, and an ion microscope. Histochemical, cytochemical, and immunohistochemical techniques were applied to the pathological specimens. Deficiencies of Zn, Cu, Mn, and vitamins A, C and E caused a loss of goblet cells in the conjunctiva and a prominent decrease of microvilli and microplicae in the conjunctiva and cornea. The elements in the goblet cells were changed in these conditions. In addition, epithelial cells showed poor fibrous development and abnormal distribution of chromatin in the nucleus. Zn, Cu, Mn, and vitamins A and E deficiencies caused photoreceptor cells to degenerate and disappear. Se deficiency reduced the horizontal and amacrine cells. Vitamin B12 deficiency reduced nerve fibers in the nerve fiber layer of the retina. Mg deficiency induced multifocal necrosis in the retinal pigment epithelium and apoptotic nuclear changes in the photoreceptor cells. Cr deficiency showed abnormal phagocytosis of the photoreceptor outer segment discs in the retinal pigment epithelium. Vitamin B12 was found to be related to the circadian rhythm in the retina. Deficiencies of Zn, Cu, Mn, and vitamins A, B12, and E induced degeneration and disappearance of myelin lamellae in the myelinated optic nerve fibers. In hypervitaminosis A, lipid droplets appeared in the retinal pigment epithelium and alcohol dehydrogenase disappeared in the retinal pigment epithelium and photoreceptor outer segments. Excessive Al was toxic to the retina, which showed disappearance of photoreceptor cells. Al deposits were seen in dendrites and neurons in the outer plexiform layer. Zn seemed to be necessary for corneal epithelial cell wound healing. Trace elements usually are contained in enzymes, which have many metabolic functions. They are related to synthesis and breakdown of many substances. Some trace elements such as Zn, Cu, Mn, and Se and vitamins including vitamins A, C, and E prevent peroxidation of lipids. Some vitamins have an affinity for specific tissues such as epithelial cells, nerve fibers, and neuronal cells and are needed for cell differentiation, development, and maintenance. Cu, Zn, Mn, Se, Mg, and Cr and vitamins A, B12, C, and E are necessary for maintenance of cellular structure and metabolism.

  4. The eye and nutrition

    PubMed

    Amemiya

    2000-05-01

    Purpose: To examine the effect of vitamins and trace elements on ocular tissue.Materials and Methods: Rats or mice were fed diets deficient in the trace elements Zn, Cu, Mn, Se, Mg, and Cr or in vitamins A, B(12), C, and E. In some rats Al and vitamin A were injected in excessive amounts. We studied the conjunctiva, cornea, retina, and optic nerve with a light microscope, transmission and scanning electron microscopes, an energy dispersive X-ray analyzer, and an ion microscope. Histochemical, cytochemical, and immunohistochemical techniques were applied to the pathological specimens.Results: Deficiencies of Zn, Cu, Mn, and vitamins A, C and E caused a loss of goblet cells in the conjunctiva and a prominent decrease of microvilli and microplicae in the conjunctiva and cornea. The elements in the goblet cells were changed in these conditions. In addition, epithelial cells showed poor fibrous development and abnormal distribution of chromatin in the nucleus.Zn, Cu, Mn, and vitamins A and E deficiencies caused photoreceptor cells to degenerate and disappear. Se deficiency reduced the horizontal and amacrine cells. Vitamin B(12) deficiency reduced nerve fibers in the nerve fiber layer of the retina. Mg deficiency induced multifocal necrosis in the retinal pigment epithelium and apoptotic nuclear changes in the photoreceptor cells. Cr deficiency showed abnormal phagocytosis of the photoreceptor outer segment discs in the retinal pigment epithelium. Vitamin B(12) was found to be related to the circadian rhythm in the retina.Deficiencies of Zn, Cu, Mn, and vitamins A, B(12), and E induced degeneration and disappearance of myelin lamellae in the myelinated optic nerve fibers.In hypervitaminosis A, lipid droplets appeared in the retinal pigment epithelium and alcohol dehydrogenase disappeared in the retinal pigment epithelium and photoreceptor outer segments. Excessive Al was toxic to the retina, which showed disappearance of photoreceptor cells. Al deposits were seen in dendrites and neurons in the outer plexiform layer.Zn seemed to be necessary for corneal epithelial cell wound healing.Discussion: Trace elements usually are contained in enzymes, which have many metabolic functions. They are related to synthesis and breakdown of many substances. Some trace elements such as Zn, Cu, Mn, and Se and vitamins including vitamins A, C, and E prevent peroxidation of lipids. Some vitamins have an affinity for specific tissues such as epithelial cells, nerve fibers, and neuronal cells and are needed for cell differentiation, development, and maintenance.Conclusion: Cu, Zn, Mn, Se, Mg, and Cr and vitamins A, B(12), C, and E are necessary for maintenance of cellular structure and metabolism.

  5. Colloid formation and metal transport through two mixing zones affected by acid mine drainage near Silverton, Colorado

    USGS Publications Warehouse

    Schemel, L.E.; Kimball, B.A.; Bencala, K.E.

    2000-01-01

    Stream discharges and concentrations of dissolved and colloidal metals (Al, Ca, Cu, Fe, Mg, Mn, Pb, and Zn), SO4, and dissolved silica were measured to identify chemical transformations and determine mass transports through two mixing zones in the Animas River that receive the inflows from Cement and Mineral Creeks. The creeks were the dominant sources of Al, Cu, Fe, and Pb, whereas the upstream Animas River supplied about half of the Zn. With the exception of Fe, which was present in dissolved and colloidal forms, the metals were dissolved in the acidic, high-SO4 waters of Cement Creek (pH 3.8). Mixing of Cement Creek with the Animas River increased pH to near-neutral values and transformed Al and some additional Fe into colloids which also contained Cu and Pb. Aluminium and Fe colloids had already formed in the mildly acidic conditions in Mineral Creek (pH 6.6) upstream of the confluence with the Animas River. Colloidal Fe continued to form downstream of both mixing zones. The Fe- and Al-rich colloids were important for transport of Cu, Pb, and Zn, which appeared to have sorbed to them. Partitioning of Zn between dissolved and colloidal phases was dependent on pH and colloid concentration. Mass balances showed conservative transports for Ca, Mg, Mn, SO4, and dissolved silica through the two mixing zones and small losses (< 10%) of colloidal Al, Fe and Zn from the water column.

  6. Distribution and chemistry of suspended particles from an active hydrothermal vent site on the Mid-Atlantic Ridge at 26°N

    NASA Astrophysics Data System (ADS)

    Trocine, Robert P.; Trefry, John H.

    1988-04-01

    Suspended particles were collected from an area of active hydrothermal venting at the Trans-Atlantic Geotraverse (TAG) Hydrothermal Field on the Mid-Atlantic Ridge and analyzed for Fe, Mn, Cd, Zn, Cu, V, Ni, Cr, Pb, Mg, Ca, Al and Si. Rapid advection of vent-derived precipitates produced a lens with total suspended matter (TSM) loadings of 14-60 μg/l at 200-700 m above the seafloor; TSM concentrations > 60 μg/l were observed only at near-vent sites. The distribution of suspended particles correlated well with increased dissolved Mn concentrations and particulate Fe values near the vent source. Particulate Fe values decreased linearly relative to TSM concentrations as hydrothermal precipitates mixed with background suspended matter. Near-vent precipitates were characterized by up to 35% Fe, 2% Zn, 0.6% Cu and > 100 μg/g Cd. In comparison to Fe, particulate Cd, Zn and Cu values decreased dramatically away from the vent source. This trend supports differential settling and/or dissolution of Cd-, Zn- and Cu-bearing phases. Particulate Mn and Fe values were inversely related with only 50 μg Mn/g in the near-vent particles. At near-vent sites, > 99% of the total Mn was in solution; this fraction decreased to 75-80% at background TSM values. In contrast to Cd, Zn and Cu, particulate V levels show a continuous, linear decrease with particulate Fe values. This trend is explained by adsorption of V on Fe-oxides in the vent plume. Scavenging of Cr, Pb and Mg by hydrothermal precipitates is also suggested by the data. Nickel and Al values were low in near-vent particles at < 100 and < 3 μg/g, respectively. The complementary behavior of dissolved Mn and particulate trace metals provides a useful framework for studying broad aspects of hydrothermal plume processes.

  7. Layered double hydroxide stability. 1. Relative stabilities of layered double hydroxides and their simple counterparts

    NASA Technical Reports Server (NTRS)

    Boclair, J. W.; Braterman, P. S.

    1999-01-01

    Solutions containing di- and trivalent metal chlorides [M(II) = Mg2+, Zn2+, Co2+, Ni2+, Mn2+; M(III) = Al3+, Fe3+] were titrated with NaOH to yield hydrotalcite-like layered double hydroxides (LDH), [[M(II)]1-x[M(III)]x(OH)2][Cl]x yH2O, by way of M(III) hydroxide/hydrous oxide intermediates. Analysis of the resultant titration curves yields nominal solubility constants for the LDH. The corresponding LDH stabilities are in the order Mg < Mn < Co approximately Ni < Zn for M(II) and Al < Fe for M(III). The stability of LDH relative to the separate metal hydroxides/hydrous oxides is discussed.

  8. [Heavy metals pollution and analysis of seasonal variation runoff in Xi'an].

    PubMed

    Yuan, Hong-Lin; Li, Xing-Yu; Wang, Xiao-Chang

    2014-11-01

    In order to explore heavy metals pollution situation,changes in characteristics, the correlation between each heavy mental and pollution source analysis of Xi'an various regions in different season in one year. This study collected several samples of Xi'an rainfall typical urban trunk roads throughout the year in 2013 and used inductively coupled plasma mass spectrometry (ICP-MS) to determine the level of Fe, Mn, Pb, Zn, Al, Cd of the samples, then, analyzed the seasonal change of heavy mental. Studies have shown that: the heavy metal of Xi'an road runoff pollutes seriously, the concentration of Fe over three times of the national standard and maintain the higher levels throughout the year, meanwhile the concentration with the intensity of human activities increases. The concentration of Mn and Zn in one year show a trends: winter > autumn > summer> spring. Pb concentration increases with the increase in traffic volume, while showing: winter > spring > summer > autumn. Factor analysis shows: Fe and Al was affected by the same sources-natural sources; Zn, Cd affected by anthropogenic sources of large; Mn, Pb affected by the larger traffic sources.

  9. Determination of elements in ayurvedic medicinal plants by AAS

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Teerthe, Santoshkumar S.; Kerur, B. R., E-mail: kerurbrk@yahoo.com

    India has a rich country for the uses of Ayurvedic medicinal plants for treatment and also the north- Karnataka boasts an unparallel diversity of medicinal plants. The present study attempts to estimate and compare the level of trace and heavy metals in some selected leaves and root samples of Ayurvedic medicinal plants such as Mg, Al, K, Cr, Mn, Fe, Cu, Zn, and Cd. The samples are collected from different places of North-Karnataka regions and sample solutions prepared as the ratio of 1:25:25+950ml=1000ppm.the trace and heavy elemental concentration was estimated using Atomic Absorption Spectrometric (AAS) Method. The average concentrations ofmore » Mg, Mn, Fe and Zn, are ranging from 2ppm to 5250.2ppm and potassium (K) has more concentration as compare to all other. The other elements likes Al, Cr, Cu, and Cd were also estimed and presented in the table. Therefore, these medicinal plants are rich in some essential minerals, especially K, Mg, Mn, Fe and Zn which are essential for human health.« less

  10. Spatio-Temporal Variability of Dissolved Metals in the Surface Waters of an Agroforestry Catchment with Low Levels of Anthropogenic Activity

    NASA Astrophysics Data System (ADS)

    Soto-Varela, Fátima; Rodríguez-Blanco, M. Luz; Mercedes Taboada-Castro, M.; Taboada-Castro, M. Teresa

    2017-12-01

    Evaluation of levels and spatial variations of metals in surface waters within a catchment are critical to understanding the extent of land-use impact on the river system. The aims of this study were to investigate the spatial and temporal variations of five dissolved metals (Al, Fe, Mn, Cu and Zn) in surface waters of a small agroforestry catchment (16 km2) in NW Spain. The land uses include mainly forests (65%) and agriculture (pastures: 26%, cultivation: 4%). Stream water samples were collected at four sampling sites distributed along the main course of the Corbeira stream (Galicia, NW Spain) between the headwaters and the catchment outlet. The headwater point can be considered as pristine environment with natural metal concentrations in waters because of the absence of any agricultural activity and limited accessibility. Metal concentrations were determined by ICP-MS. The results showed that metal concentrations were relatively low (Fe > Al > Mn > Zn > Cu), suggesting little influence from agricultural activities in the area. Mn and Zn did not show significant differences between sampling points along main stream, while for Fe and Cu significant differences were found between the headwaters and all other points. Al tended to decrease from the headwaters to the catchment outlet.

  11. Rice seed toxicity tests for organic and inorganic substances

    USGS Publications Warehouse

    Wang, W.

    1994-01-01

    Plant seed toxicity tests can be used to evaluate hazardous waste sites and to assess toxicity of complex effluents and industrial chemicals. Conventional plant seed toxicity tests are performed using culture dishes containing filter paper. Some reports indicate that filter papers might interfere with the toxicity of inorganic substances. In this study, a plastic seed tray was used. Rice was used as the test species. A comparison of results in the literature and this study revealed that variation of test species, methods, exposure duration, and other factors may affect the test results. The results of this study showed that the order of decreasing toxicity of metal ions was Cu>Ag>Ni>Cd>Cr(VI)>Pb>Zn>Mn>NaF for rice. The test results were similar to those reported in the literature for lettuce Ag>Ni>Cd,Cu>Cr (VI)>Zn>Mn, millet Cu,Ni>Cd>Cr(VI)>Zn>Mn, and ryegrass Cu>Ni>Mn>>Pb>Cd>Zn> Al>Hg>Cr>Fe. The order of decreasing toxicity of organic herbicides was paraquat, 2,4-D>>glyphosate>bromacil.

  12. Determining baseline element composition of lichens. I. Parmelia sulcata at Theodore Roosevelt national park, North Dakota

    USGS Publications Warehouse

    Gough, L.P.; Severson, R.C.; Jackson, L.L.

    1988-01-01

    Element-concentration baselines are given for Parmelia sulcata and associated soils. Parmelia chlorochroa was found sporadically and therefore only representative concentration ranges are reported for this species. Element data include (1) for lichens; Al, As, Ba, B, Ca, Cr, Cu, Fe, Hg, Mn, Ni, P, Sr, S, Ti, V, Y, and Zn; and (2) for soils: Al, Ba, Be, Ca, Cs, Cr, Cu, Fe, Hg, Mg, Mn, Ni, Nb, P, Pb, Sr, S, Ti, V, Y, and Zn. Very little (usually 7.2 km); thus, P sulcata is, in general, chemically similar throughout the park. This same uniformity was found for soil geochemistry. Numerous samples collected at close intervals would be required, therefore, to produce detailed element-concentration maps for P. sulcata and soils. No instances of elemental phytotoxic conditions were found; however, P. sulcata apparently possesses large concentrations of Ba, Cu, Fe, Pb, S, V, and possibly Zn.

  13. Literature Survey on Decorporation of Radionuclides from the Human Body

    DTIC Science & Technology

    2002-04-01

    66 8. Adverse Health Effects Associated with... effects ........................................... 66 Table 11- Common foods with chelating effects ...Mn Tetracycline Fe, MR, Mn, Mo, Al, Ca Table 11- Common foods with chelating effects Foodstuff Chelate Cq hhPe 1314 99 M. 75’s Eggs 59Fe Soybean 65Zn

  14. Determination of the spinel group end-members based on electron microprobe analyses

    NASA Astrophysics Data System (ADS)

    Ferracutti, Gabriela R.; Gargiulo, M. Florencia; Ganuza, M. Luján; Bjerg, Ernesto A.; Castro, Silvia M.

    2015-04-01

    The spinel group minerals have been the focus of many studies, not only because of their economic interest, but also due to the fact that they are very useful as petrogenetic indicators. The application End-Members Generator (EMG) allows to establish, based on electron microprobe analyses (EMPA), the 19 end-members of the spinel group: MgAl2O4 (Spinel sensu stricto, s.s.), FeAl2O4 (Hercynite), MnAl2O4 (Galaxite), ZnAl2O4 (Gahnite), MgFe2O4 (Magnesioferrite), Fe3O4 (Magnetite), MnFe2O4 (Jacobsite), ZnFe2O4 (Franklinite), NiFe2O4 (Trevorite), MgCr2O4 (Magnesiochromite), FeCr2O4 (Chromite), MnCr2O4 (Manganochromite), ZnCr2O4 (Zincochromite), NiCr2O4 (Nichromite), MgV2O4 (Magnesiocoulsonite), FeV2O4 (Coulsonite), MnV2O4 (Vuorelainenite), Mg2TiO4 (Qandilite) and Fe2TiO4 (Ulvöspinel). EMG is an application that does not require an installation process and was created with the purpose of performing calculations to obtain: cation proportions (per formula unit, p.f.u.), end-members of the spinel group, redistribution proportions for the corresponding end-members in the Magnetite prism or Ulvöspinel prism and a data validation section to check the results. EMG accepts .csv data files and the results obtained can be used to represent a given dataset with the SpinelViz program or any other 2D and/or 3D graph plotting software.

  15. Enhancement of Mechanical Properties of Extruded Mg-9Al-1Zn-1MM-0.7CaO-0.3Mn Alloy Through Pre-aging Treatment

    NASA Astrophysics Data System (ADS)

    Jeong, Seok Hoan; Kim, Yong Joo; Kong, Kyung Ho; Cho, Tae Hee; Kim, Young Kyun; Lim, Hyun Kyu; Kim, Won Tae; Kim, Do Hyang

    2018-03-01

    The effect of pre-aging treatment before extrusion has been investigated in Mg-9.0Al-1.0Zn-1MM-0.7CaO-0.3Mn alloy. The as-cast microstructure consists of α-Mg dendrite with secondary solidification phase particles, (Mg, Al)2Ca, β-Mg17Al12 and Al11RE3 at the inter-dendritic region. After extrusion, β-Mg17Al12 precipitates are present, but higher density and more homogeneous distribution in pre-aged alloy. In addition, μm-scale banded bulk β-Mg17Al12 particles are generated during extrusion. Al11RE3 particles are broken into small particles, and are aligned along the extrusion direction. (Mg, Al)2Ca particles are only slightly elongated along the extrusion direction, providing stronger particle stimulated nucleation (PSN) effect by severe deformation during extrusion. The mechanical properties can be significantly enhanced by introducing pre-aging treatment, i.e. β-Mg17Al12 precipitates provide grain refining and strengthening effects and (Mg, Al)2Ca particles provide PSN effect.

  16. Texture and structure contribution to low-temperature plasticity enhancement of Mg-Al-Zn-Mn Alloy MA2-1hp after ECAP and annealing

    NASA Astrophysics Data System (ADS)

    Serebryany, V. N.; D'yakonov, G. S.; Kopylov, V. I.; Salishchev, G. A.; Dobatkin, S. V.

    2013-05-01

    Equal channel angular pressing (ECAP) in magnesium alloys due to severe plastic shear deformations provides both grain refinement and the slope of the initial basal texture at 40°-50° to the pressing direction. These changes in microstructure and texture contribute to the improvement of low-temperature plasticity of the alloys. Quantitative texture X-ray diffraction analysis and diffraction of backscattered electrons are used to study the main textural and structural factors responsible for enhanced low-temperature plasticity based on the example of magnesium alloy MA2-1hp of the Mg-Al-Zn-Mn system. The possible mechanisms of deformation that lead to this positive effect are discussed.

  17. Effect of Iron Impurity on the Phase Composition, Structure and Properties of Magnesium Alloys Containing Manganese and Aluminum

    NASA Astrophysics Data System (ADS)

    Volkova, E. F.

    2017-07-01

    Results of a study of the interaction between iron impurity and manganese and aluminum alloying elements during formation of phase composition in alloys of the Mg - Mn, Mg - Al, Mg - Al - Mn, and Mg - Al - Zn - Mn systems are presented. It is proved that this interaction results in introduction of Fe into the intermetallic phase. The phase compositions of model magnesium alloys and commercial alloys MA2-1 and MA5 are studied. It is shown that both manganese and aluminum may bind the iron impurity into phases. Composite Fe-containing intermetallic phases of different compositions influence differently the corrosion resistance of magnesium alloys.

  18. Syntheses and characterizations of transition-metal-substituted aluminophosphate molecular sieves |(C3N2H5) 8|[M8Al16P24O96] (M = Co, Mn, Zn) with zeotype LAU topology.

    PubMed

    Song, Xiaowei; Li, Jiyang; Guo, Yanan; Pan, Qinhe; Gan, Lin; Yu, Jihong; Xu, Ruren

    2009-01-05

    Three transitional-metal-substituted aluminophosphate molecular sieves, |(C3N2H5)8|[M8Al16P24O96] (denoted MAPO-LAU, M = Co, Mn, Zn), have been synthesized under solvothermal conditions in the presence of imidazole as the structure-directing agent. Their structures are determined by single-crystal X-ray diffraction and further characterized by powder X-ray diffraction, inductively coupled plasma, thermogravimetric, and diffuse reflectance spectroscopy (UV-vis) analyses. The structure of MAPO-LAU is based on the strict alternation of MO4/AlO4 tetrahedra and PO4 tetrahedra through vertex oxygen atoms. Their frameworks are analogous to the zeotype LAU structure in which 33% of the aluminum sites are replaced by transitional-metal ions. The protonated imidazole cations resided in the 10-ring channels. These compounds show photoluminescent properties due to the existence of imidazole molecules in the structures. Magnetic measurements reveal that there is very weak antiferromagnetic interaction among the metal centers of MnAPO-LAU.

  19. [Distribution characteristics of heavy metals along an elevation gradient of montane forest].

    PubMed

    Wan, Jia-rong; Nie, Ming; Zou, Qin; Hu, Shao-chang; Chen, Jia-kuan

    2011-12-01

    In the present paper, the concentrations of fourteen heavy metals (Fe, Al, Ti, Cu, Cr, Mn, V, Zn, Ni, Co, Pb, Se, Cd and As) were determined by ICP-AES and atomic absorption spectroscopy along an elevation gradient of montane forest. The results show that the elevation gradient had significant effects on the concentrations of Fe, Al, Ti, V, Pb and As. And the concentrations of Cu, Cr, Mn, Zn, Ni, Co, Se and Cd were not significantly affected by the elevation gradient. Because the studying area is red soil, the elevation gradient had significant effects on the concentrations of Fe, Al and Ti which are characteristic heavy metals of red soil, suggesting that the red soil at different elevations has different intensities of weathering desilication and bioaccumulation. Other heavy metals have different relationships with the elevation gradient, such as the concentrations of Cr, Zn and Cd were high at relatively high elevation and Pb and As were high at relatively low elevation. These results suggest that the different elevations of montane forest soils were polluted by differently types of heavy metals.

  20. Cation hydrolysis and the regulation of trace metal composition in seawater

    NASA Astrophysics Data System (ADS)

    Kumar, M. Dileep

    1987-08-01

    Thermodynamic calculations have been performed for cation hydrolysis, including temperatures from 2°C to the high values of significance near Mid-Oceanic Ridge Systems (MORS). Eighteen elements with wide range of residence times ( t) in seawater (Mn, Th, Al, Bi, Ce, Co, Cr(III), Fe, Nd, Pb, Sc, Sm, Ag, Cd, Cu, Hg, Ni and Zn) have been considered. A model for the regulation of trace metal composition in seawater by cation hydrolytic processes, including those at MORS, is presented. Results show an increase in the abundance of neutral metal hydroxyl species with increase in temperature. During hydrothermal mixing, as the temperature increases, transformation from lower positive hydroxyl complexes to higher or neutral complexes would occur for Cd, Ce, Co, Cr(III), Cu, Mn, Nd, Ni, Pb, Sm and Zn. pH values for adsorption of the metal ion onto solid surfaces have direct relation with pH values of hydrolysis. Co, Mn and Pb could be oxidized to higher states (at Mn-oxide surfaces) that would occur even at MORS. Ce can also be oxidized at 25°C. Solubility calculations show that Al, Bi, Cr(III), Sc, Fe and Th are saturated while Ce, Nd and Sm are not with respect to their oxyhydroxide solids at their concentrations in seawater at 25°C. Cu, Hg, Ni and Zn reach saturation equilibrium at 250°C, whereas Co, Mn and Pb exhibit unsaturation. The results suggest an increase in scavenging capacity of a cation with rise in temperature.

  1. Occupational and environmental exposure of automobile mechanics and nonautomotive workers to airborne manganese arising from the combustion of methylcyclopentadienyl manganese tricarbonyl (MMT).

    PubMed

    Sierra, P; Loranger, S; Kennedy, G; Zayed, J

    1995-07-01

    Inhalation exposure to manganese (Mn) was measured for a group of garage mechanics and a control group of nonautomotive workers. The airborne Mn exposure of 35 garage mechanics suspected of being relatively highly exposed to Mn from MMT was measured at the workplace over one-week period. It also was measured for 30 nonautomotive workers at the University of Montreal. The environmental exposure also was measured for the two groups, as was the exposure to three other metals, aluminum (Al), iron (Fe), and zinc (Zn). At work the mechanics were exposed to Mn concentrations varying from 0.010 to 6.673 micrograms m-3 with a mean of 0.45 microgram m-5, while the control group was exposed to concentrations varying from 0.011 to 1.862 microgram m-3 with a mean of 0.04 microgram m-3. The mean environmental exposure for the two groups was similar to the Mn concentrations gathered in Montreal in 1992. Workplace concentrations of Al, Fe, and Zn also were higher for the garage mechanics. The results suggest that less than 10% of the Mn exposure of the garage mechanics was due to MMT. The levels of the metals measured were below the established limits for industrial and even environmental exposure.

  2. Metal pollution in Al-Khobar seawater, Arabian Gulf, Saudi Arabia.

    PubMed

    Alharbi, Talal; Alfaifi, Hussain; El-Sorogy, Abdelbaset

    2017-06-15

    In order to assess heavy metals pollution along the Al-Khobar coastline, 30 seawater samples and 15 sediment ones were collected for Al, V, Cr, Mn, Fe, Co, Ni, Cu, Zn, As, Se, Sr, Mo, Cd, Hg and Pb analysis by Inductively Coupled Plasma-Mass Spectrometer (ICP-MS). The analysis indicated a southward decreasing pattern in most heavy metal concentrations and the average values of Zn, Fe, Mn, Cu, As and Cr were higher than the ones reported from some worldwide seas and gulfs. Most of the highest levels were recorded within the bays and were related with in situ under sediments especially that composed of clays and very fine sands, and in localities characterized with anthropogenic activities like landfilling, desalination plants, fishing boats, oil spills and solid rubbish. The results of the present study provide useful background for further marine investigation and management in the Arabian Gulf region. Copyright © 2017 Elsevier Ltd. All rights reserved.

  3. High potential of Mn-doped ZnS nanoparticles with different dopant concentrations as novel MRI contrast agents: synthesis and in vitro relaxivity studies

    NASA Astrophysics Data System (ADS)

    Jahanbin, Tania; Gaceur, Meriem; Gros-Dagnac, Hélène; Benderbous, Soraya; Merah, Souad Ammar

    2015-06-01

    Over several decades, metal-doped quantum dots (QDs) with core-shell structure have been studied as dual probes: fluorescence and magnetic resonance imaging (MRI) probes (Dixit et al., Mater Lett 63(30):2669-2671, 2009). However, metal-doped nanoparticles, in which the majority of metal ions are close to the surface, can affect their efficacy as MRI contrast agents (CAs). In this context, herein the high potential of synthesized Mn-doped ZnS QDs via polyol method as imaging probe is demonstrated. The mean diameters of QDs were measured via transmission electron microscopy (TEM) and X-ray diffraction (XRD). Optical and magnetic properties of MnZnS nanoparticles were characterized using fluorescence spectroscopy and super quanducting interference devices magnetometer and electron paramagnetic resonance system, respectively. T1- and T2-weighted images of nanoparticles in aqueous solution were acquired from spin-echo sequences at 3 T. From TEM images and XRD spectra of the prepared nanoparticles, it is observed that the average diameter of particles does not significantly change with Mn dopant content ( 1.6-1.9 nm). All three samples exhibit broad blue emission under UV light excitation. According to the MRI studies, MnZnS nanoparticles generate strong T1 contrast enhancement (bright T1-weighted images) at the low concentration (<0.1 mM). The MnZnS nanoparticles exhibit the high longitudinal ( r 1) relaxivity that increases from 20.34 to 75.5 mM-1 s-1 with the Mn dopant contents varying between 10 and 30 %. Strong signal intensity on T1-weighted images and high r 1 with {r2 }/{r_{1 }} ≈ 1 can demonstrate the high potential of the synthesized Mn:ZnS nanoparticles, which can serve as an effective T1 CA.

  4. Anthropogenic metal enrichment of snow and soil in north-eastern European Russia.

    PubMed

    Walker, T R; Young, S D; Crittenden, P D; Zhang, H

    2003-01-01

    Trace metal composition of winter snowpack, snow-melt filter residues and top-soil samples were determined along three transects through industrial towns in the Usa basin, North-East Russia: Inta, Usinsk and Vorkuta. Snow was analysed for Ag, Al, As, Ba, Cd, Co, Cr, Cu, Mn, Ni, Pb, Sr and Zn using ICP-MS (Ca and K by F-AAS for Vorkuta only), pH and acidity/alkalinity. Filter residues were analysed for: Al, Ba, Ca, Cd, Cu, K, Mg, Mn, Ni, Pb, Sr and Zn using F-AAS and GF-AAS; top-soil samples were analysed for Ba, Cu, Mg, Mn, Na, Ni, Pb, Sr, Zn using F-AAS. Results indicate elevated concentrations of elements associated with alkaline combustion ash around the coal mining towns of Vorkuta and Inta. There is little evidence of deposition around the gas and oil town of Usinsk. Atmospheric deposition in the vicinity of Vorkuta, and to a lesser extent Inta, added significantly to the soil contaminant loading as a result of ash fallout. Acid deposition was associated with pristine areas whereas alkaline combustion ash near to emission sources more than compensated for the acidity caused by SO2.

  5. Zn-Mn alloy coatings from acidic chloride bath: Effect of deposition conditions on the Zn-Mn electrodeposition-morphological and structural characterization

    NASA Astrophysics Data System (ADS)

    Loukil, N.; Feki, M.

    2017-07-01

    Zn-Mn alloy electrodeposition on steel electrode in chloride bath was investigated using cyclic voltammetric, chronopotentiometric and chronoamperometric techniques. Cyclic voltammetries (CV) reveal a deep understanding of electrochemical behaviors of each metal Zn, Mn, proton discharge and Zn-Mn co-deposition. The electrochemical results show that with increasing Mn2+ ions concentration in the electrolytic bath, Mn2+ reduction occurs at lower over-potential leading to an enhancement of Mn content into the Zn-Mn deposits. A dimensionless graph model was used to analyze the effect of Mn2+ ions concentration on Zn-Mn nucleation process. It was found that the nucleation process is not extremely affected by Mn2+ concentration. Nevertheless, it significantly depends on the applied potential. Several parameters such as Mn2+ ions concentration, current density and stirring were investigated with regard to the Mn content into the final Zn-Mn coatings. It was found that the Mn content increases with increasing the applied current density jimp and Mn2+ ions concentration in the electrolytic bath. However, stirring of the solution decreases the Mn content in the Zn-Mn coatings. The phase structure and surface morphology of Zn-Mn deposits are characterized by means of X-ray diffraction analysis and Scanning Electron Microscopy (SEM), respectively. The Zn-Mn deposited at low current density is tri-phasic and consisting of η-Zn, ζ-MnZn13 and hexagonal close packed ε-Zn-Mn. An increase in current density leads to a transition from crystalline to amorphous structure, arising from the hydroxide inclusions in the Zn-Mn coating at high current density.

  6. Properties of self-assembled diluted magnetic semiconductor nanostructures =

    NASA Astrophysics Data System (ADS)

    Ankiewicz, Amelia Olga Goncalves

    Este trabalho centra-se na investigacao da possibilidade de se conseguir um semicondutor magnetico diluido (SMD) baseado em ZnO. Foi levado a cabo um estudo detalhado das propriedades magneticas e estruturais de estruturas de ZnO, nomeadamente nanofios (NFs), nanocristais (NCs) e filmes finos, dopadas com metais de transicao (MTs). Foram usadas varias tecnicas experimentais para caracterizar estas estruturas, designadamente difraccao de raios-X, microscopia electronica de varrimento, ressonancia magnetica, SQUID, e medidas de transporte. Foram incorporados substitucionalmente nos sitios do Zn ioes de Mn2+ e Co2+ em ambos os NFs e NCs de ZnO. Revelou-se para ambos os ioes dopantes, que a incorporacao e heterogenea, uma vez que parte do sinal de ressonancia paramagnetica electronica (RPE) vem de ioes de MTs em ambientes distorcidos ou enriquecidos com MTs. A partir das intensidades relativas dos espectros de RPE e de modificacoes da superficie, demonstra-se ainda que os NCs exibem uma estrutura core-shell. Os resultados, evidenciam que, com o aumento da concentracao de MTs, a dimensao dos NCs diminui e aumentam as distorcoes da rede. Finalmente, no caso dos NCs dopados com Mn, obteve-se o resultado singular de que a espessura da shell e da ordem de 0.3 nm e de que existe uma acumulacao de Mn na mesma. Com o objectivo de esclarecer o papel dos portadores de carga na medicao das interaccoes ferromagneticas, foram co-dopados filmes de ZnO com Mn e Al ou com Co e Al. Os filmes dopados com Mn, revelaram-se simplesmente paramagneticos, com os ioes de Mn substitucionais nos sitios do Zn. Por outro lado, os filmes dopados com Co exibem ferromagnetismo fraco nao intrinseco, provavelmente devido a decomposicao spinodal. Foram ainda efectuados estudos comparativos com filmes de ligas de Zn1-xFexO. Como era de esperar, detectaram-se segundas fases de espinela e de oxido de ferro nestas ligas; todas as amostras exibiam curvas de histerese a 300 K. Estes resultados suportam a hipotese de que as segundas fases sao responsaveis pelo comportamento magnetico observado em muitos sistemas baseados em ZnO. Nao se observou nenhuma evidencia de ferromagnetismo mediado por portadores de carga. As experiencias mostram que a analise de RPE permite demonstrar directamente se e onde estao incorporados os ioes de MTs e evidenciam a importancia dos efeitos de superficie para dimensoes menores que 15 nm, para as quais se formam estruturas core-shell. As investigacoes realizadas no ambito desta tese demonstram que nenhuma das amostras de ZnO estudadas exibiram propriedades de um SMD intrinseco e que, no futuro, sao necessarios estudos teoricos e experimentais detalhados das interaccoes de troca entre os ioes de MTs e os atomos do ZnO para determinar a origem das propriedades magneticas observadas.

  7. Variation of the coordination environment and its effect on the white light emission properties in a Mn-doped ZnO-ZnS complex structure.

    PubMed

    Cheng, Yan; Chen, Rui; Feng, Haifeng; Hao, Weichang; Xu, Huaizhe; Wang, Yu; Li, Jiong

    2014-03-14

    Mn-doped ZnO-ZnS complex nanocrystals were fabricated through coating of dodecanethiol on Mn-doped ZnO nanocrystals. The relationship between the component of white light emission and the coordination environments of Mn-dopants were experimentally investigated. It was shown that Mn ions mainly formed Mn(3+)O6 octahedra in as prepared Mn-doped ZnO, while the Mn(3+) ions on the surface of ZnO transferred into Mn(2+) ions at the interface between ZnO and ZnS after dodecanethiol coating. The Mn(2+)S4 tetrahedron density and the orange emission intensity increased upon enhancing the dodecanethiol content. These results provide an alternative way to optimize the white emission spectrum from nanocrystals of Mn-doped ZnS-ZnO complex structures through modulation of the coordination environment of Mn ions.

  8. Geochemistry of magnetite from porphyry Cu and skarn deposits in the southwestern United States

    USGS Publications Warehouse

    Nadoll, Patrick; Mauk, Jeffrey L.; LeVeille, Richard A.; Koenig, Alan E.

    2015-01-01

    A combination of petrographic observations, laser ablation inductively coupled plasma mass spectrometry (LA-ICP-MS), and statistical data exploration was used in this study to determine compositional variations in hydrothermal and igneous magnetite from five porphyry Cu–Mo and skarn deposits in the southwestern United States, and igneous magnetite from the unmineralized, granodioritic Inner Zone Batholith, Japan. The most important overall discriminators for the minor and trace element chemistry of magnetite from the investigated porphyry and skarn deposits are Mg, Al, Ti, V, Mn, Co, Zn, and Ga—of these the elements with the highest variance for (I) igneous magnetite are Mg, Al, Ti, V, Mn, Zn, for (II) hydrothermal porphyry magnetite are Mg, Ti, V, Mn, Co, Zn, and for (III) hydrothermal skarn magnetite are Mg, Ti, Mn, Zn, and Ga. Nickel could only be detected at levels above the limit of reporting (LOR) in two igneous magnetites. Equally, Cr could only be detected in one igneous occurrence. Copper, As, Mo, Ag, Au, and Pb have been reported in magnetite by other authors but could not be detected at levels greater than their respective LORs in our samples. Comparison with the chemical signature of igneous magnetite from the barren Inner Zone Batholith, Japan, suggests that V, Mn, Co, and Ga concentrations are relatively depleted in magnetite from the porphyry and skarn deposits. Higher formation conditions in combination with distinct differences between melt and hydrothermal fluid compositions are reflected in Al, Ti, V, and Ga concentrations that are, on average, higher in igneous magnetite than in hydrothermal magnetite (including porphyry and skarn magnetite). Low Ti and V concentrations in combination with high Mn concentrations are characteristic features of magnetite from skarn deposits. High Mg concentrations (<1,000 ppm) are characteristic for magnetite from magnesian skarn and likely reflect extensive fluid/rock interaction. In porphyry deposits, hydrothermal magnetite from different vein types can be distinguished by varying Ti, V, Mn, and Zn contents. Titanium and V concentrations are highly variable among hydrothermal and igneous magnetites, but Ti concentrations above 3,560 ppm could only be detected in igneous magnetite, and V concentrations are on average lower in hydrothermal magnetite. The highest Ti concentrations are present in igneous magnetite from gabbro and monzonite. The lowest Ti concentrations were recorded in igneous magnetite from granodiorite and granodiorite breccia and largely overlap with Ti concentrations found in hydrothermal porphyry magnetite. Magnesium and Mn concentrations vary between magnetite from different skarn deposits but are generally greater than in hydrothermal magnetite from the porphyry deposits. High Mg, and low Ti and V concentrations characterize hydrothermal magnetite from magnesian skarn deposits and follow a trend that indicates that magnetite from skarn (calcic and magnesian) commonly has low Ti and V concentrations.

  9. Trace elements distribution in hawksbill turtle (Eretmochelys imbricata) and green turtle (Chelonia mydas) tissues on the northern coast of Bahia, Brazil.

    PubMed

    de Macêdo, Gustavo R; Tarantino, Taiana B; Barbosa, Isa S; Pires, Thaís T; Rostan, Gonzalo; Goldberg, Daphne W; Pinto, Luis Fernando B; Korn, Maria Graças A; Franke, Carlos Roberto

    2015-05-15

    Concentrations of elements (As, Al, Ba, Ca, Cd, Co, Cr, Cu, Fe, Hg, K, Mg, Mn, Mo, Na, Ni, Pb, Sb, Se, Sr, V, Zn) were determined in liver, kidneys and bones of Eretmochelys imbricata and Chelonia mydas specimens found stranded along the northern coast of Bahia, Brazil. Results showed that the concentrations of Cd, Cu, Ni and Zn in the liver and kidneys of juvenile C. mydas were the highest found in Brazil. We also observed a significant difference (p<0.05) on the bioaccumulation of trace elements between the two species: Al, Co, Mo, Na and Se in the liver; Al, Cr, Cu, K, Mo, Ni, Pb, Sr and V in the kidneys; and Al, Ba, Ca, Cd, Mn, Ni, Pb, Se, Sr and V in the bones. This study represents the first report on the distribution and concentration of trace elements in E. imbricata in the Brazilian coast. Copyright © 2015 Elsevier Ltd. All rights reserved.

  10. Effects of frit addition on the surface morphology and structural properties of ZnO-Bi2O3-Mn2O3 discs

    NASA Astrophysics Data System (ADS)

    Shahardin, Ahmad Hajidi; Mahmud, Shahrom; Sendi, Rabab Khalid

    2015-04-01

    ZnO-Bi2O3-Mn2O3 discs were prepared using conventional ceramic processing method and sintered at 1000°C. The different percentages of frit on the ZnO-Bi2O3-Mn2O3 discs were 0.0%, 0.5%, 1.0% and 3.0%. From FESEM observation, the grain structure and grain growth were more uniformly constructed and well distributed. Frit addition was found to cause a big drop in the average grain size from 4.59 µm to 2.76 µm even with an addition of 0.5 mol%. The Si and Al content in the frit recipe might have played a role as inhibiting agents in grain growth during sintering. RAMAN intensity and phase shifting were not affected by frit addition except at 3 mol%. Frit addition did not affect the formation of secondary phases. Frit addition below 3 mol% in ZnO-Bi2O3-Mn2O3 varistor discs can be used as a method in controlling grain size without affecting other properties.

  11. A novel method for vanadium slag comprehensive utilization to synthesize Zn-Mn ferrite and Fe-V-Cr alloy.

    PubMed

    Liu, Shi-Yuan; Li, Shu-Jin; Wu, Shun; Wang, Li-Jun; Chou, Kuo-Chih

    2018-07-15

    Vanadium slag is a by-product from steelmaking process of vanadium-titanium magnetite, which mainly contains FeO, MnO, V 2 O 3 , and Cr 2 O 3 , The elements Fe and Mn are major components of Mn-Zn ferrite. The elements V and Cr are major components of V-Cr alloy. In view of the potential application in these study, a Mn 0.8 Zn 0.2 Fe 2 O 4 of high saturation magnetization (Ms = 68.6 emu/g) and low coercivity (Hc = 3.3 Oe) was successfully synthesized from the leaching solutions of vanadium slag by adding appropriate chemical reagents, ZnCl 2 and MnCl 2 ·4H 2 O, via roasting at 1300 °C for 1 h. The minor components (CaO and SiO 2 ) in the leaching solution of vanadium slag segregated to the grain boundaries resulting in increasing the resistivity of ferrite. The value of DC resistivity of Mn 0.8 Zn 0.2 Fe 2 O 4 at 25 °C reached 1230.7Ω m. The residue containing Fe, V and Cr was chlorinated by AlCl 3 and the Fe 3+ , V 3+ , and Cr 3+ ions were released into the NaCl-KCl eutectic. The current-time curve for the electrolysis of molten salt was investigated. Alloy (Fe, V, and Cr) of granular shape was obtained. The residue can be used to produce the mulite. This process provided a new approach to utilize slag from steelmaking. Copyright © 2018 Elsevier B.V. All rights reserved.

  12. Structural classification of RAO3( MO) n compounds ( R =Sc, In, Y, or lanthanides; A =Fe(III), Ga, Cr, or Al; M =divalent cation; n = 1-11)

    NASA Astrophysics Data System (ADS)

    Kimizuka, Noboru; Mohri, Takahiko

    1989-01-01

    A series of new compounds RAO3( MO) n ( n = 1-11) having spinel, YbFe 2O 4, or InFeO 3(ZnO) n types of structures were newly synthesized ( R =Sc, In, Y, Lu, Yb, Tm, or Er; A =Fe(III), Ga, Cr, or Al; M =Mg, Mn, Fe(II), Co, Ni, Zn, or Cd) at elevated temperatures. The conditions of synthesis and the lattice constants for these compounds are reported. The stacking sequences of the InO 1.5, (FeZn)O 2.5, and ZnO layers for InFeO 3(ZnO) 10 and the TmO 1.5, (AlZn)O 2.5, and ZnO layers for TmAlO 3(ZnO) 11 are presented, respectively. The crystal structures of the( RAO3) m( MO) n phases ( R =Sc, In, Y, or lanthanide elements; A =Fe(III), Ga, Cr, or Al; M =divalent cation elements; m and n =integer) are classified into four crystal structure types (K 2NiF 4, CaFe 2O 4, YbFe 2O 4, and spinel), based upon the constituent cations R, A, and M

  13. Highly efficient and selective adsorption of In{sup 3+} on pristine Zn/Al layered double hydroxide (Zn/Al-LDH) from aqueous solutions

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Barnabas, Mary Jenisha; Parambadath, Surendran; Mathew, Aneesh

    2016-01-15

    A pristine Zn/Al-layered double hydroxide (Zn/Al-LDH) showed excellent adsorption ability and selectivity towards In{sup 3+} ions from aqueous solutions. The adsorption behaviour as a function of the contact time, solution pH, ionic strength, and amount of adsorbent under ambient conditions revealed a strong dependency on the pH and ionic strength over In{sup 3+} intake. The structure and properties of Zn/Al-LDH and In{sup 3+} adsorbed Zn/Al-LDH (In–Zn/Al-LDH) were examined carefully by X-ray diffraction, Fourier transform infrared spectroscopy, N{sub 2}-sorption/desorption, UV–vis spectroscopy, and X-ray photoelectron spectroscopy. The adsorbent had a sufficient number of active sites that were responsible for the In{sup 3+}more » adsorption and quite stable even after the adsorption process. The selective adsorption of In{sup 3+} on Zn/Al-LDH was also observed even from a mixture containing competing ions, such as Mn{sup 2+}, Co{sup 2+}, Ni{sup 2+}, Cd{sup 2+}, Pb{sup 2+}, and Cu{sup 2+}. The adsorption experiments showed that Zn/Al-LDH is a promising material for the pre-concentration and selective removal of In{sup 3+} from large volumes of aqueous solutions. - Highlights: • A pristine Zn/Al-layered double hydroxide showed good selectivity for In{sup 3+} ions. • The material exhibited a maximum In{sup 3+} intake of 205 mg g{sup −1} at pH 6. • The materials showed good affinity of In{sup 3+} over Cu{sup 2+} and Pb{sup 2+} from ion mixtures.« less

  14. The chemistry of hydrothermal magnetite: a review

    USGS Publications Warehouse

    Nadoll, Patrick; Angerer, Thomas; Mauk, Jeffrey L.; French, David; Walshe, John

    2014-01-01

    Magnetite (Fe3O4) is a well-recognized petrogenetic indicator and is a common accessory mineral in many ore deposits and their host rocks. Recent years have seen an increased interest in the use of hydrothermal magnetite for provenance studies and as a pathfinder for mineral exploration. A number of studies have investigated how specific formation conditions are reflected in the composition of the respective magnetite. Two fundamental questions underlie these efforts — (i) How can the composition of igneous and, more importantly, hydrothermal magnetite be used to discriminate mineralized areas from barren host rocks, and (ii) how can this assist exploration geologists to target ore deposits at greater and greater distances from the main mineralization? Similar to igneous magnetite, the most important factors that govern compositional variations in hydrothermal magnetite are (A) temperature, (B) fluid composition — element availability, (C) oxygen and sulfur fugacity, (D) silicate and sulfide activity, (E) host rock buffering, (F) re-equilibration processes, and (G) intrinsic crystallographic controls such as ionic radius and charge balance. We discuss how specific formation conditions are reflected in the composition of magnetite and review studies that investigate the chemistry of hydrothermal and igneous magnetite from various mineral deposits and their host rocks. Furthermore, we discuss the redox-related alteration of magnetite (martitization and mushketovitization) and mineral inclusions in magnetite and their effect on chemical analyses. Our database includes published and previously unpublished magnetite minor and trace element data for magnetite from (1) banded iron formations (BIF) and related high-grade iron ore deposits in Western Australia, India, and Brazil, (2) Ag–Pb–Zn veins of the Coeur d'Alene district, United States, (3) porphyry Cu–(Au)–(Mo) deposits and associated (4) calcic and magnesian skarn deposits in the southwestern United States and Indonesia, and (5) plutonic igneous rocks from the Henderson Climax-type Mo deposit, United States, and the un-mineralized Inner Zone Batholith granodiorite, Japan. These five settings represent a diverse suite of geological settings and cover a wide range of formation conditions. The main discriminator elements for magnetite are Mg, Al, Ti, V, Cr, Mn, Co, Ni, Zn, and Ga. These elements are commonly present at detectable levels (10 to > 1000 ppm) and display systematic variations. We propose a combination of Ni/(Cr + Mn) vs. Ti + V, Al + Mn vs. Ti + V, Ti/V and Sn/Ga discriminant plots and upper threshold concentrations to discriminate hydrothermal from igneous magnetite and to fingerprint different hydrothermal ore deposits. The overall trends in upper threshold values for the different settings can be summarized as follows: (I) BIF (hydrothermal) — low Al, Ti, V, Cr, Mn, Co, Ni, Zn, Ga and Sn; (II) Ag–Pb–Zn veins (hydrothermal) — high Mn and low Ga and Sn; (III) Mg-skarn (hydrothermal) — high Mg and Mn and low Al, Ti, Cr, Co, Ni and Ga; (IV) skarn (hydrothermal) — high Mg, Al, Cr, Mn, Co, Ni and Zn and low Sn; (V) porphyry (hydrothermal) — high Ti and V and low Sn; (VI) porphyry (igneous) — high Ti, V and Cr and low Mg; and (VII) Climax-Mo (igneous) — high Al, Ga and Sn and low Mg and Cr.

  15. Tululite, Ca14(Fe3+,Al)(Al,Zn,Fe3+,Si,P,Mn,Mg)15O36: a new Ca zincate-aluminate from combustion metamorphic marbles, central Jordan

    NASA Astrophysics Data System (ADS)

    Khoury, Hani N.; Sokol, Ella V.; Kokh, Svetlana N.; Seryotkin, Yurii V.; Nigmatulina, Elena N.; Goryainov, Sergei V.; Belogub, Elena V.; Clark, Ian D.

    2016-02-01

    Tululite (Ca14(Fe3+,Al)(Al,Zn,Fe3+,Si,P,Mn,Mg)15O36 (the hypothetical end-member formula Ca14{Fe3+O6}[SiO4][Zn5Al9]O26) (IMA2014-065) is a new natural Ca zincate-aluminate, identified in medium-temperature (800-850 °C) combustion metamorphic (CM) spurrite-fluorellestadite marbles from central Jordan. The type locality (Tulul Al Hammam area) is situated in the northern part of the Siwaqa complex, the largest area of the "Mottled Zone" Formation in the Dead Sea region. The marbles originated from bitumen-rich chalky marine sediments of the Maastrichtian-Paleogene Muwaqqar Chalk Marl Formation, which have low clay content (and, consequently, low Al) and high Zn, Cd, and U enrichments. The bulk CM rocks derived from the low-Al protolith have unusually high (Zn + Cd)/Al ratios ( 0.2) and, as a result, a mineralogy with negligibly small percentages of Ca aluminates having low Ca:Al molar ratios (minerals of mayenite supergroup, Ca:Al = 6:7) common to most of calcareous CM rocks in the Mottled Zone. Instead, the mineral assemblage of the Zn-rich marbles contains tululite, with high Ca:Al = 2.55 molar ratios and Zn substituting for a large portion of Al (Zn:Al = 1.1). Tululite occurs in thin clusters as irregular grains with indented outlines (20-100 μm in size), having typical open-work textures associated with rock-forming calcite, fluorellestadite, spurrite, and accessory Zn-rich periclase, lime-monteponite solid solutions, calcium uranates, and zincite. Marbles also bear brownmillerite, dorrite, fluormayenite, high-fluorine Ca aluminate, and lakargiite. Secondary phases are brucite, gel-like calcium silicate hydrates and calcium silicate aluminate hydrates, including Zn- and U-bearing and Cd-rich compounds, Si-bearing hydrated compounds after calcium uranates, and basic Cd chlorides. The empirical formula of the holotype tululite (a mean of 32 analyses) is (Ca13.29Cd0.75)Σ14.04(Al5.46Zn5.20Fe3+ 2.23Si0.95Mn3+ 1.01Mg0.78P0.41)Σ16.04O36. Tululite is cubic, space group F23; a = 14.9346(4) Å; V = 3331.07(15) Å3, Z = 4. The strongest lines of the X-ray powder-diffraction pattern [ d, Å - ( I obs )] are: 2.874(57), 2.640 (100), 2.524(42), 2.278(41), 1.760(54), 1.725(25), 1.524(33), 1.500(33). The crystal structure was solved from single-crystal X-ray diffraction data and refined to wR2 = 0.0672 on the basis of 913 unique reflections with I 0 > 2σ( I). Tululite belongs to a group of compounds with the general formula Ca14 MT 15O35+ x (0 ≤ x ≤ 1), and is a new structure type. The tetrahedral framework of tululite structure is formed by T7O13 secondary building units (SBU), which consist of four corner-linked tetrahedra sharing a common oxygen atom and three tetrahedra sharing two O atoms with the neighbor SBU. Ca2+ cations occupy three positions; two of them also contain a minor amount of Cd2+. The Ca sites surround an island (Fe3+,Al)O6 octahedron and a (Si,P)O4 tetrahedron in the centers of framework cages at the junction of eight SBUs. The (Fe3+,Al)O6 octahedron is coordinated by fourteen Ca positions into a 6-capped cube, whereas the (Si,P)O4 tetrahedron is coordinated by six Ca positions into a regular octahedron. The structural formula of tululite is Ca14{Fe3+O6}M1[(Si,P)O4]T1[(Al,Zn)7O13]2 T2-T4. The mineral is yellow with greenish tint, transparent with vitreous luster, non-fluorescent under ultraviolet light, and showing neither parting nor cleavage; Mohs hardness is 6.5. The density calculated on the basis of the empirical formula is 3.826 g/cm3. Its Raman spectrum shows strong bands at 522, 550 and 636 cm-1 and weak bands at 199, 260, 295, 456, and 754 cm-1.

  16. iMAST Quarterly, Number 2, 2000

    DTIC Science & Technology

    2000-01-01

    Metal Iron N2 Metal Niobium N2 Metal Al12Si N2 Metal Al6061 N2 Metal CCC (Al 9Ce 5Cr 2.8 Co) N2 Metal Pech 1 (Al 12 Zn 3Mg 1 Cu 0.25Mn N2 Metal...Cu 38Ni N2 Metal Nichrome (80/20) N2 Metal Ni 5Al N2 Metal Cr3 C2 –25Ni Cr N2 Metal Co 29Cr 6Al 1Y (Amdry 920) N2 Metal Co 32Ni 20Cr 8Al N2 Metal 316...St. Steel N2 Metal Ancorsteel 1000 N2 Metal Ti 35Zr 10Nl N2 Metal Al Alloys + SiC (15%) (No. 12-17) N2 Metal Al, Zn + 10-15% HA N2 Metal (HA

  17. Effect of (Mn,Cr) co-doping on structural, electronic and magnetic properties of zinc oxide by first-principles studies

    NASA Astrophysics Data System (ADS)

    Aimouch, D. E.; Meskine, S.; Boukortt, A.; Zaoui, A.

    2018-04-01

    In this study, structural, electronic and magnetic properties of Mn doped (ZnO:Mn) and (Mn,Cr) co-doped zinc oxide (ZnO:(Mn,Cr)) have been calculated with the FP-LAPW method by using the LSDA and LSDA+U approximations. Going through three configurations of Mn,Cr co-doped ZnO corresponding to three different distances between manganese and chromium, we have analyzed that ZnO:(Mn,Cr) system is more stable in its preferred configuration2. The lattice constant of undoped ZnO that has been calculated in this study is in a good agreement with the experimental and theoretical values. It was found to be increased by doping with Mn or (Mn,Cr) impurities. The band structure calculations showed the metallic character of Mn doped and Mn,Cr co-doped ZnO. As results, by using LSDA+U (U = 6eV), we show the half-metallic character of ZnO:Mn and ZnO:Mn,Cr. We present the calculated exchange couplings d-d of Mn doped ZnO which is in a good agreement with the former FPLO calculation data and the magnetization step measurement of the experimental work. The magnetic coupling between neighboring Mn impurities in ZnO is found to be antiferromagnetic. In the case of (Mn,Cr) co-doped ZnO, the magnetic coupling between Mn and Cr impurities is found to be antiferromagnetic for configuration1 and 3, and ferromagnetic for configuration2. Thus, the ferromagnetic coupling is weak in ZnO:Mn. Chromium co-doping greatly enhance the ferromagnetism, especially when using configuration2. At last, we present the 2D and 3D spin-density distribution of ZnO:Mn and ZnO:(Mn,Cr) where the ferromagnetic state in ZnO:(Mn,Cr) comes from the strong p-d and d-d interactions between 2p-O, 3d-Mn and 3d-Cr electrons. The results of our calculations suggest that the co-doping ZnO(Mn, Cr) can be among DMS behavior for spintronic applications.

  18. Effects of the ZnO layer on the structure and white light emission properties of a ZnS:Mn/GaN nanocomposite system.

    PubMed

    Wang, Cai-Feng; Hu, Bo

    2017-10-01

    ZnO films were inserted between the ZnS:Mn films and GaN substrates by pulsed laser deposition (PLD). The structure, morphology, and optical properties of the ZnS:Mn/ZnO/GaN nanocomposite systems have been investigated. X-ray diffraction results show that there are three diffraction peaks located at 28.4°, 34.4°, and 34.1°, which correspond to the β-ZnS(111), ZnO(002), and GaN(002) planes, respectively. Due to the insertion of ZnO films, the diffraction peak intensity of ZnS:Mn in ZnS:Mn/ZnO/GaN is stronger than that of ZnS:Mn in ZnS:Mn/GaN, and the full width at half-maximum is smaller. Though the transmittance of ZnS:Mn/ZnO films is slightly lower than that of ZnS:Mn films, the transmittance is still higher than 80%. Compared with ZnS:Mn/GaN, an ultraviolet (UV) emission at 387 nm (originated from the near-band emission of ZnO) and a green light emission at about 520 nm appeared in the photoluminescence (PL) spectra of ZnS:Mn/ZnO/GaN, in addition to the blue emission at 435 nm and the orange-red emission at 580 nm. The emission at 520 nm may be related to the deep-level emission from ZnO and the interface of ZnS:Mn/ZnO. The PL spectrum of ZnS:Mn/ZnO/GaN covers the visible region from the blue light to the red light (400-700 nm), and its color coordinate and color temperature are (0.3103,0.3063) and 6869 K, respectively, presenting strong white light emission.

  19. Trace element biomonitoring using mosses in urban areas affected by mud volcanoes around Mt. Etna. The case of the Salinelle, Italy.

    PubMed

    Bonanno, Giuseppe; Lo Giudice, Rosa; Pavone, Pietro

    2012-08-01

    Trace element impact was assessed using mosses in a densely inhabited area affected by mud volcanoes. Such volcanoes, locally called Salinelle, are phenomena that occur around Mt. Etna (Sicily, Italy) and are interpreted as the surface outflow of a hydrothermal system located below Mt. Etna, releasing sedimentary fluids (hydrocarbons and NaCl brines) along with magmatic gases (mainly CO(2) and He). To date, scarce data are available about the presence of trace elements, and no biomonitoring campaigns are reported about the cumulative effects of such emissions. In this study, concentrations of Al, As, Cd, Cr, Cu, Hg, Mn, Ni, Pb, V, and Zn were detected in the moss Bryum argenteum, in soil and water. Results showed that the trace element contribution of the Salinelle to the general pollution was significant for Al, Mn, Ni, and Zn. The comparison of trace concentrations in mosses from Salinelle and Etna showed that the mud volcanoes release a greater amount of Al and Mn, whereas similar values of Ni were found. Natural emissions of trace elements could be hazardous in human settlements, in particular, the Salinelle seem to play an important role in environmental pollution.

  20. EPR and FTIR spectroscopic studies of MO-Al2O3-Bi2O3-B2O3-MnO2(M = Pb, Zn and Cd) glasses

    NASA Astrophysics Data System (ADS)

    Lalitha Phani, A. V.; Sekhar, K. Chandra; Chakradhar, R. P. S.; Narasimha Chary, M.; Shareefuddin, Md

    2018-03-01

    Glasses of the system (30-x)MO-xAl2O3-15Bi2O3-54.5B2O3-0.5MnO2 [M = Pb, Zn & Cd] (x = 0, 5, 10 & 15 mol%) were prepared by the normal melt quenching method. The amorphous nature of the prepared glasses was confirmed by the XRD studies. The EPR and FTIR studies were carried out at room temperature (RT). The EPR spectra exhibited three resonance signals at g ≈ 2.0 with a hyperfine structure, an absorption around g = 4.3 and a distinct shoulder at g = 3.3. Deconvoluted spectra were drawn for g ≈ 2.0 to resolve the six hyperfine lines. The electron paramagnetic resonance signal at g ≈ 2.0 indicates that the Mn2+ ions are in nearly perfectly octahedral symmetry. The low field signals at g = 3.3 and g = 4.3 are attributed to the Mn2+ ion which are in distorted rhombic symmetries. The hyperfine (HF) splitting constant (A) values suggested that the bonding between Mn2+ ions and its ligands is ionic in nature. The presence of BO3 and BO4 borate units, metal oxide cation units, Mn2+ and Bi-O bond vibrations in BiO3 units were noticed from the FTIR spectra.

  1. Improvement on the magnetic and dielectric behavior of hard/soft ferrite nanocomposites

    NASA Astrophysics Data System (ADS)

    Mansour, S. F.; Hemeda, O. M.; Abdo, M. A.; Nada, W. A.

    2018-01-01

    Nanocomposites from M-type hexaferrite BaFe11.7Al0.15Zn0.15O19 and spinel ferrite Mn0.8Mg0.2Fe2O4 nanoparticles according to the formula [(x)(Ba Fe11.7Al0.15 Zn0.15O19) + (1 - x)(Mn0.8 Mg0.2Fe2O4); x = 0.3, 0.4 and 0.5] have been manufactured by the citrate combustion method. The structure and morphology of the nanocomposites were appointed by X-ray diffraction (XRD) analysis and field emission scanning electron microscopy (FESEM). The remanent magnetization and coercivity of the nanocomposites became 2 and 2.5 times higher, respectively by adding BaFe11.7Al0.15 Zn0.15O19 phase. The Cole-Cole plots of the nanocomposite x = 0.4 at the selected temperatures shows two successive semicircles at all the selected temperatures. The first low frequencies semicircle elucidates the contribution of the grain boundary and the second one, at high frequencies, gives the contribution of grain to conduction process. Multilateral applications for exchange spring magnets can be manufactured using those nanocomposites.

  2. Synthesis, structural, optical and dielectric properties of transition metal doped ZnMnO nanoparticles by sol-gel combustion technique

    NASA Astrophysics Data System (ADS)

    Dar, M. A.; Varshney, Dinesh

    2018-02-01

    Nanocrystalline samples of Zn0.94Mn0.06O and transition metal (TM) doped Zn0.94Mn0.01TM0.05O (TM = Co, Ni, and Cu) were prepared by sol-gel auto combustion method. X-ray diffraction (XRD) pattern infers that all synthesized samples except Zn0.94Mn0.01Ni0.05O and Zn0.94Mn0.01Cu0.05O with secondary phases of NiO and CuO are in single phase with hexagonal wurtzite structure (P63mc space group). Raman spectroscopy reveals four vibrational phonon modes are centered at 331, 380, 410, and 438 cm-1, assigned as E2 (H)-E2(L), A1(TO), E1(TO), and E1(LO) modes, respectively. A Raman spectrum of Zn0.94Mn0.01TM0.05O is entirely different from undoped Zn0.94Mn0.06O sample. Also, the infrared spectrum of transition metal doped samples is completely different from undoped Zn0.94Mn0.06O. Similar spectra are observed for Zn0.94Mn0.01Co0.05O, Zn0.94Mn0.01NiO, Zn0.94Mn0.01Cu0.05O and Zn0.94Mn0.01Zn0.05O samples. It was found that the band gap of Zn0.94Mn0.06O increased from 3.19 to 3.25eV by doping 5% transition metal oxide. Improved dielectric constant and reduced dielectric loss is measured for Zn0.94Mn0.01Ni/Cu0.05O as compared to Zn0.94Mn0.06O.

  3. Cuprian fraipontite and sauconite from the Defiance-Silver Bill mines, Gleeson, Arizona.

    USGS Publications Warehouse

    Foord, E.E.; Taggart, J.E.; Conklin, N.M.

    1983-01-01

    XRD studies have shown the fine-grained, light blue-green mineral previously identified as turquoise or chrysocolla to be the rare species fraipontite + or - admixed sauconite. Composite microprobe and XRF analyses gave SiO2 24.8, Al2O3 17.3, CaO 0.34, CuO 5.2, ZnO 40.95, H2O (ign. loss, 900oC) 12.8, = 101.39, yielding the formula (Zn1.84Al0.77Cu0.24box 0.13- Ca0.02)3.00(Si1.51Al0.49)2.00O5(OH)4. Semiquantitative emission spectrographic analysis showed Fe 0.007, Mg 0.01, Ca 0.07, Si 10, Al major, Na 0.015, Zn major, Cu 5%; Mn 15, B 150, Be 7, Ni 50, Pb 15, Sc 15, Ga 70 and Ag 1 ppm. It has a 5.331(8), b 9.23(1), c 7.275(6) A, beta 104.15o; H. 3.5-4; Dcalc 3.44, Dobs. 3.08- 3.10; mean refr. ind. approx 1.61. Much of the fraipontite is admixed with sauconite, which may be forming from the fraipontite. XRF analysis of this material gave SiO2 32.8, Al2O3 10.9, MgO < 0.1, CaO 1.51, Na2O < 0.2, K2O < 0.02, TiO2 < 0.02, P2O5 < 0.02, MnO < 0.02, CuO 4.65, ZnO 39.9, ign. loss 13.9, = 103.7.-G.W.R.

  4. Trace metals in bulk precipitation and throughfall in a suburban area of Japan

    NASA Astrophysics Data System (ADS)

    Hou, H.; Takamatsu, T.; Koshikawa, M. K.; Hosomi, M.

    Throughfall and bulk precipitation samples were collected monthly for 1.5 years over bare land and under canopies of Japanese cedar ( Cryptomeria japonica), Japanese red pine ( Pinus densiflora), Japanese cypress ( Chamaecyparis obtusa), and bamboo-leafed oak ( Quercus myrsinaefolia) in a suburban area of Japan. Samples were analyzed for dissolved Al, Mn, Fe, Cu, Zn, Ag, In, Sn, Sb and Bi by ICP-AES and ICP-MS. The metal concentrations were higher in throughfall, especially that of C. japonica, than bulk precipitation. Enrichment ratios (ERs: ratios of metal concentrations in throughfall to those in bulk precipitation) ranged from 2.5 (Zn) to 5.3 (Ag) (3.9 on average), and ERs for slightly soluble metals were generally higher than those for easily soluble metals. Concentrations of Mn, Fe, Cu, and Zn accounted for 99% of the total concentration of heavy metals in rainwater, whereas those of rare metals such as Ag, In, Sn, and Bi totaled <0.23%. Average concentrations of rare metals were 0.002 and 0.010 μg l -1 for Ag, 0.001 and 0.005 μg l -1 for In, 0.062 and 0.21 μg l -1 for Sn, and 0.006 and 0.023 μg l -1 for Bi in bulk precipitation and throughfall, respectively. The metal concentrations in rainwater were negatively correlated to the volume of rainwater, indicating that washout is the main mechanism that incorporates metals into rainwater. From the enrichment factors, that is, (X/Al) rain/(X/Al) crust, metals other than Fe were shown to be more enriched in rainwater than in the Earth's crust, including those present as a result of leaching from soil dust (Mn) and from anthropogenic sources (Cu, Zn, Ag, In, Sn, Sb, and Bi).

  5. Chemistry of impact events on Mercury

    NASA Astrophysics Data System (ADS)

    Berezhnoy, Alexey A.

    2018-01-01

    Based on the equilibrium thermochemical approach and quenching theory, formation of molecules and dust grains in impact-produced clouds formed after collisions between meteoroids and Mercury is considered. Based on observations of Al, Fe, and Mn atoms in the exosphere of Mercury and new results of studies of the elemental composition of the surface of Mercury, quenching temperatures and pressures of main chemical reactions and condensation of dust particles were estimated. The behavior of the main Na-, K-, Ca-, Fe-, Al-, Mn-, Mg-, Si-, Ti, Ni-, Cr-, Co, Zn-, O-, H-, S-, C-, Cl-, N-, and P-containing species delivered to the Hermean exosphere during meteoroid impacts was studied. The importance of meteoroid bombardment as a source of Na, K, Ca, Fe, Al, Mn, Mg, and O atoms in the exosphere of Mercury is discussed.

  6. Resistivity Changes Due to Precipitation Effects in Fibre Reinforced Mg-Al-Zn-Mn Alloy

    NASA Astrophysics Data System (ADS)

    Kiehn, J.; Kainer, K. U.; Vostrý, P.; Stulíková, I.

    1997-05-01

    The change of electrical properties of alumina short fibre reinforced Mg-Al-Zn-Mn alloy AZ91D during isochronal annealing up to 300 °C is discussed. The Saffil® fibres were incorporated into the magnesium alloy by direct squeeze casting. The fibre distribution is random planar parallel to the flat faces of the dc four-point resistivity specimens machined from the solution treated castings. A sharp drop of resistivity between 140 and 260 °C is explained by the formation of incoherent -phase particles. Some practical recommendations concerning the use of alumina short fibre reinforced AZ91 alloy are made on the basis of the results obtained. Es werden die Änderungen der elektrischen Eigenschaften der aluminiumoxid-kurzfaserverstärkten Mg-Al-Zn-Mn Legierung AZ91D während isochroner Wärmebehandlungen bis 300 °C diskutiert. Das direkte Preßgießverfahren diente zur Herstellung der Saffil®-Faser Magnesium Verbundwerkstoffe. Die Proben zur Widerstandsmessung nach der Vier-Punkt Methode wurden durch spanende Bearbeitung aus den lösungsgeglühten Preßgußstücken herausgearbeitet, so daß sie regellose Faserverteilung in den Ebenen parallel zu den flachen Probenseiten aufwiesen. Ein starker Abfall des elektrischen Widerstands im Temperaturbereich zwischen 140 und 260 °C wird durch die Bildung inkohärenter β-Phase erklärt. Auf Grundlage der Ergebnisse werden einige Empfehlungen zur Anwendung der kurzfaserverstärkten Legierung AZ91 gegeben.

  7. Diurnal variations in, and influences on, concentrations of particulate and dissolved arsenic and metals in the mildly alkaline Wallkill River, New Jersey, USA

    NASA Astrophysics Data System (ADS)

    Barringer, Julia L.; Wilson, Timothy P.; Szabo, Zoltan; Bonin, Jennifer L.; Fischer, Jeffrey M.; Smith, Nicholas P.

    2008-01-01

    Diurnal variations in particulate and dissolved As and metal concentrations were observed in mildly alkaline water from a wetlands site on the Wallkill River in northwestern New Jersey. The site, underlain by glacial sediments over dolomite bedrock, is 10 km downstream from a mined area of the Franklin Marble, host to Zn ores, also As and Mn minerals. In mid-September 2005, maxima and minima in dissolved-oxygen-concentration and pH, typically caused by photosynthesis and respiration, occurred at 2000 and 0800 hours. Concentrations of dissolved As (1.52-1.95 μg/L) peaked at dusk (2000 hours), whereas dissolved Mn and Zn concentrations (76.5-96.9 and 8.55-12.8 μg/L, respectively) were lowest at dusk and peaked at 1000 hours. These opposing cycles probably reflect sorption and desorption of As (an anion), and Mn and Zn (cations) as pH varied throughout the 24-h period. Doubly-peaked cycles of B, Cl, SO4, and nutrients also were observed; these may result from upstream discharges of septic-system effluent. Both recoverable amd particulate Al, Fe, Mn, and Zn concentrations peaked between 0200 and 0600 hours. The particulate metals cycle, with perturbations at 0400 hours, may be influenced by biological activity.

  8. Recent advances in nanosized Mn-Zn ferrite magnetic fluid hyperthermia for cancer treatment.

    PubMed

    Lin, Mei; Huang, Junxing; Sha, Min

    2014-01-01

    This paper reviews the recent research and development of nanosized manganese zinc (Mn-Zn) ferrite magnetic fluid hyperthermia (MFH) for cancer treatment. Mn-Zn ferrite MFH, which has a targeted positioning function that only the temperature of tumor tissue with magnetic nanoparticles can rise, while normal tissue without magnetic nanoparticles is not subject to thermal damage, is a promising therapy for cancer. We introduce briefly the composition and properties of magnetic fluid, the concept of MFH, and features of Mn-Zn ferrite magnetic nanoparticles for MFH such as thermal bystander effect, universality, high specific absorption rate, the targeting effect of small size, uniformity of hyperthermia temperature, and automatic temperature control and constant temperature effect. Next, preparation methods of Mn-Zn ferrite magnetic fluid are discussed, and biocompatibility and biosecurity of Mn-Zn ferrite magnetic fluid are analyzed. Then the applications of nanosized Mn-Zn ferrite MFH in cancer are highlighted, including nanosized Mn-Zn ferrite MFH alone, nanosized Mn-Zn ferrite MFH combined with As2O3 chemotherapy, and nanosized Mn-Zn ferrite MFH combined with radiotherapy. Finally, the combination application of nanosized Mn-Zn ferrite MFH and gene-therapy is conceived, and the challenges and perspectives for the future of nanosized Mn-Zn ferrite MFH for oncotherapy are discussed.

  9. Synthesis and characterization of three-dimensional transition metal ions doped zinc oxide based dilute magnetic semiconductor thin films

    NASA Astrophysics Data System (ADS)

    Samanta, Kousik

    Dilute magnetic semiconductors (DMS), especially 3d-transition metal (TM) doped ZnO based DMS materials are the most promising candidates for optoelectronics and spintronics applications; e.g. in spin light emitting diode (SLED), spin transistors, and spin field effect transistors (SFET), etc. In the present dissertation, thin films of Zn1-xTMxO (TM = Co2+, Cu2+, and Mn2+) were grown on (0001) oriented Al2O3 substrates by pulsed laser deposition (PLD) technique. The films were highly c-axis oriented, nearly single crystalline, and defects free for a limited concentration of the dilution of transition metal ions. In particular, we have obtained single crystalline phases of Zn1-xTMxO thin films for up to 10, 3, and 5 stoichiometric percentages of Co2+, Cu2+, and Mn2+ respectively. Raman micro-probe system was used to understand the structural and lattice dynamical properties at different physical conditions. The confinement of optical phonons in the disorder lattice was explained by alloy potential fluctuation (APF) using a spatial correlation (SC) model. The detailed analysis of the optical phonon behavior in disorder lattice confirmed the substitution of the transition metal ions in Zn 2+ site of the ZnO host lattice. The secondary phases of ZnCo 2O4, CuO, and ZnMn2O4 were detected in higher Co, Cu, and Mn doped ZnO thin films respectively; where as, XRD did not detect these secondary phases in the same samples. Room temperature ferromagnetism was observed in Co2+ and Cu2+ ions doped ZnO thin films with maximum saturation magnetization (Ms) of 1.0 and 0.76 muB respectively. The origin of the observed ferromagnetism in Zn1-xCoxO thin films was tested by the controlled introduction of shallow donors (Al) in Zn0.9-x Co0.1O:Alx (x = 0.005 and 0.01) thin films. The saturation magnetization for the 10% Co-doped ZnO (1.0 muB /Co) at 300K reduced (˜0.25 muB/Co) due to Al doping. The observed ferromagnetism and the reduction due to Al doping can be explained by the Bound Magnetic Polaron (BMP) model. The Resistivity of ZCO sample (˜ 103 O-cm) dropped by 5 orders of magnitude (0.02 O-cm) in Co, Al co-doped samples and the carrier concentrations increases 4 orders of magnitude (˜ 1019/cm3). The Cu2+ doped ZnO thin films showed the ferromagnetic property at 300K. The p-d orbital mixing of high spin Cu2+ (d9) state with the nearest neighbor oxygen p-orbital can explain the origin of RTFM in Zn 1-xCuxO thin films. The optical transmission spectroscopy and the photoluminescence spectroscopy analysis were used to understand the electronic band structure, near band edge (NBE) transition, and the excitonic behavior in ZnO and Zn1-xTMxO thin films. We have found the reduction of NBE transition at 300K due to the substitution of Co and Cu in ZnO host lattice. This narrowing of the optical band gap (NBE) is due to the sp-d exchange interaction between the d electrons of transition metal ions and the band electrons of ZnO; the strength of this interaction strongly depends on the number of d electrons. The s-d and p-d exchanges give rise to negative and positive corrections to the conduction and valance band edges respectively, leading to the NBE narrowing. We have observed the characteristic inter atomic d-d transitions in Co doped samples; thus confirming the substitution of Co2+ in the tetrahedral site in ZnO. The low temperature (77K) PL spectrum showed the basic excitonic characteristics of pure ZnO in Zn1-xTMxO thin films. The X-ray photoelectron spectroscopy (XPS) showed that the Co and Cu are normally in 2+ oxidation state, but in the case of higher Cu concentrations (>3%), the mixed state of Cu2+ and Cu1+ were detected.

  10. Determination of bioavailable macro- and microelements from agricultural soil using different extractants

    NASA Astrophysics Data System (ADS)

    Milićević, Tijana; Relić, Dubravka; Popović, Aleksandar

    2015-04-01

    Translocation of elements from soil to plant has a major impact on the growing plants and on their quality in any agricultural field. In this study, soil samples were collected from agricultural area Radmilovac, Serbia during grapevine season in 2013. Bioavailable elements from soil to plant (grapevine) were isolated by five different extractants: 0.11 mol L-1 CH3COOH, 0.05 mol L-1 Na-EDTA, 0.01 mol L-1 CaCl2, 1 mol L-1 NH4NO3 and distilled water during 2 and 16 h. Concentrations of 22 bioavailable macroelements: Al, Ca, Fe, K, Mg, Mn, Na, P, S, Si and microelements: B, Be, Cd, Co, Cr, Cu, Mo, Ni, Pb, Sb, V, Zn were determined by ICP-OES. The best extractant for Al, B, Be, Mg, Mo, Si and Zn was CH3COOH, Na-EDTA for Ca, Cd, Co, Cu, Fe, K, Mn, Ni, P, Pb, V, and distilled water for Na and S. Acetic acid has been proven to be an aggressive extractant and it can be used for isolation of higher concentrations of plant bioavailable elements from soil, rather than distilled water, CaCl2 and NH4NO3. The acidity of CH3COOH enhances the extraction of bioavailable fraction of microelements from various substrates and destruction of carbonates as well. However, it can be concluded that there is no unique extractant for isolation of the most bioavailable fraction for all elements from the soil. It can be noticed that the most common concentrations of macroelements, K and Mn, are in correlation with concentrations of microelements, Cd, Co, Ni and Zn. This indicates that the most of their concentrations in soils are followed by microelements, whose concentrations are much lower than concentrations of macroelements. However, as these correlations are the most common, it can be concluded that the pairs of macro- and microelements (e.g. Mn-Cd, Mn-Co, Ni-Cd, Ni-Co, Ni-Mn, Zn-Cd, Zn-Co, Zn-Mn, Zn-Ni) have the same source in soil and can be isolated by the same extractant. It is interesting to note that the concentrations of Ca and Mg extracted from soil using CH3COOH are in correlation and that neither of these macroelements is in correlation with the concentration of microelements isolated with the same extractant. The concentrations of Cu and S extracted from soil by distilled water during 16 h are in correlation. These elements could have entered only through the soil surface layer while grapevines were primarily treated by fungicide copper(II)-sulphate. In addition, the concentration of S is correlated with the concentrations of Mn, P and Na. It can be assumed that the correlation between these elements points to their origin from the pesticides used in agriculture production.

  11. From Serendipity to Rational Design: Tuning the Blue Trigonal Bipyramidal Mn3+ Chromophore to Violet and Purple through Application of Chemical Pressure.

    PubMed

    Li, Jun; Lorger, Simon; Stalick, Judith K; Sleight, Arthur W; Subramanian, M A

    2016-10-03

    We recently reported that an allowed d-d transition of trigonal bipyramidal (TBP) Mn 3+ is responsible for the bright blue color in the YIn 1-x Mn x O 3 solid solution. The crystal field splitting between a'(d z 2 ) and e'(d x 2 -y 2 , d xy ) energy levels is very sensitive to the apical Mn-O distance. We therefore applied chemical pressure to compress the apical Mn-O distance in YIn 1-x Mn x O 3 , move the allowed d-d transition to higher energy, and thereby tune the color from blue to violet/purple. This was accomplished by substituting smaller cations such as Ti 4+ /Zn 2+ and Al 3+ onto the TBP In/Mn site, which yielded novel violet/purple phases. The general formula is YIn 1-x-2y-z Mn x Ti y Zn y Al z O 3 (x = 0.005-0.2, y = 0.1-0.4, and z ≤ 0.1), where the color darkens with the increasing amount of Mn. Higher y or small additions of Al provide a more reddish hue to the resulting purple colors. Substituting other rare earth cations for Y has little impact on color. Crystal structure analysis by neutron powder diffraction confirms a shorter apical Mn-O distance compared with that in the blue YIn 1-x Mn x O 3 . Magnetic susceptibility measurements verify the 3+ oxidation state for Mn. Diffuse reflection spectra were obtained over the wavelength region 200-2500 nm. All samples show excellent near-infrared reflectance comparable to that of commercial TiO 2 , making them ideal for cool pigment applications such as energy efficient roofs of buildings and cars where reducing solar heat to save energy is desired. In a comparison with commercial purple pigments, such as Co 3 (PO 4 ) 2 , our pigments are much more thermally stable and chemically inert, and are neither toxic nor carcinogenic.

  12. Distinct effects of Al3+ doping on the structure and properties of hexagonal turbostratic birnessite: A comparison with Fe3+ doping

    NASA Astrophysics Data System (ADS)

    Yin, Hui; Kwon, Kideok D.; Lee, Jin-Yong; Shen, Yi; Zhao, Huaiyan; Wang, Xiaoming; Liu, Fan; Zhang, Jing; Feng, Xionghan

    2017-07-01

    Hexagonal turbostratic birnessite, one of the most reactive Mn oxide minerals, is ubiquitous throughout the ocean floor to the surface environment. During its crystallization, birnessite may coexist with Al3+, which is the third most abundant crustal element. However, interactions of Al3+ with birnessite compared to the transition metal (TM) ions have rarely been explored thus far. This study examines the structure and properties of Al3+-doped hexagonal turbostratic birnessite to obtain insights into the interaction of metal cations with birnessite-like minerals in natural environments. For Al3+-incorporated birnessite, the crystal chemistry of Al3+, as well as alteration in the mineral structure, physicochemical properties, and reactivity toward the sorption of Pb2+/Zn2+ is investigated by powder X-ray diffraction, chemical analysis, Fourier transform infrared spectroscopy, X-ray photoelectron spectroscopy, and X-ray absorption spectroscopy. Electronic structure calculations based on density functional theory (DFT) are further combined to aid in the experimental interpretation of Al3+ incorporation. As a comparative system, Fe3+-coprecipitated birnessite is also examined. Under the experimental conditions used, only a small amount of Al3+ is incorporated into birnessite, with a final Al/(Al + Mn) molar ratio of ∼0.07, whereas Fe3+ is incorporated into birnessite with a final Fe/(Fe + Mn) molar ratio of up to ∼0.21. Irrespective of metal type, the incorporation of a metal cation significantly alters the physicochemical properties of birnessite, such as decrease in the thickness of crystals along the c∗ axis and coherent scattering domain sizes in the a-b plane and the Mn average oxidation state, increase in the specific surface area and the total amount of hydroxyl groups, in which the contents of hydroxyl groups around vacancies are decreased. The lattice parameters in the a-b plane tend to decrease in Al-incorporated birnessites but first significantly decrease and then increase in Fe-incorporated birnessites. In Fe-incorporated birnessites, ∼32-50% of the total Fe3+ is located inside the Mn octahedral sheets (INC species). In Al-incorporated birnessites, the edge- and corner-sharing Mn-Mn distances gradually decrease. Density function theory (DFT) computation results support that the dominant species in Al-birnessite is a triple-corner-sharing complex on vacancies. The DFT geometry optimization further demonstrates that the in-plane cell size experimentally observed for these birnessites depends on not only the metal type but also its position in the mineral. The Al- or Fe-birnessites exhibit significantly increased adsorption capacities for Pb2+ but reduced capacities for Zn2+. The metal incorporation effects on the chemical reactivity are discussed with the observed changes in the particle size and available vacancy sites.

  13. Zincovelesite-6N6S, Zn3(Fe3+,Mn3+,Al,Ti)8O15(OH), a new högbomite-supergroup mineral from Jacupica mountains, Republic of Macedonia

    NASA Astrophysics Data System (ADS)

    Chukanov, Nikita V.; Krzhizhanovskaya, Maria G.; Jančev, Simeon; Pekov, Igor V.; Varlamov, Dmitry A.; Göttlicher, Jörg; Rusakov, Vyacheslav S.; Polekhovsky, Yury S.; Chervonnyi, Alexandr D.; Ermolaeva, Vera N.

    2018-02-01

    A new mineral species zincovelesite-6N6S with the simplified formula Zn3(Fe3+,Mn3+,Al,Ti)8O15(OH) was discovered in the orogenetic zone related to the "Mixed Series" metamorphic complex near the Nežilovo village, Jacupica Mountains, Pelagonia mountain range, Republic of Macedonia. In oxide Zn-Fe-Mn ore, zincovelesite-6N6S forms lenticular aggregates up to 2 × 2 × 0.5 mm consisting of thin near-coplanar platelets up to 70 × 70 × 1 µm3 and associated with franklinite, gahnite, hetaerolite, zincochromite, ferricoronadite, baryte, As-rich fluorapatite, dolomite, Zn-bearing talc, almeidaite, hydroxycalcioroméite, zircon, quartz, and scheelite. In silicate-baryte zones of the metasomatic rock, uniaxial intergrowths of zincovelesite-6N6S with nežilovite are observed. The new mineral is opaque, black, with brownish-black streak. The lustre is strong submetallic to metallic. The micro-indentation hardness is 1118 kg/mm2 which corresponds to Mohs' hardness ca. 6½. Zincovelesite-6N6S is brittle, with uneven fracture. No cleavage or parting is observed. The density calculated from the empirical formula is 5.158 g/cm3. In reflected light zincovelesite-6N6S is light grey. The reflectance values [R max/R min, % (λ, nm)] are: 17.1/13.4 (470), 16.5/12.8 (546), 16.2/12.6 (589), 15.6/12.2 (650). The IR spectrum shows the presence of OH groups. According to the Mössbauer spectrum, all iron is trivalent. The Mn K-edge XANES spectroscopy shows that Mn is predominantly or completely trivalent. The average chemical composition is (wt%; electron microprobe, H2O determined by gas chromatography of ignition products): MgO 0.97, CuO 0.50, ZnO 30.80, Al2O3 8.17, Mn2O3 21.31, Fe2O3 29.44, TiO2 5.28, Sb2O5 3.74, H2O 1.1, total 101.31. The empirical formula based on 16 O atoms is H1.05Zn3.26Mg0.21Cu0.05Fe3+ 3.18Mn3+ 2.32Al1.38Ti0.57Sb0.20O16. Zincovelesite-6N6S is trigonal, probable space group P-3m1, a = 5.902(2) Å, c = 55.86(1) Å, V = 1684.8(9) Å3, Z = 6. The strongest lines of the powder X-ray diffraction pattern [d, Å (I, %) (hkl)] are: 2.952 (62) (110), 2.881 (61) (1.0.16), 2.515 (100) (204), 2.493 (88) (1.1.12), 2.451 (39) (1.0.20), 1.690 (19) (304, 2.1.16), 1.572 (19) (2.0.28), 1.475 (29) (221). Zincovelesite-6N6S is the first Fe3+-dominant member of the högbomite supergroup and, thus, can be considered as a parent species of a new mineral group. The rootname velesite is given for the discovery locality near the city of Veles.

  14. Compositional dependence of elastic moduli for transition-metal oxide spinels

    NASA Astrophysics Data System (ADS)

    Reichmann, H. J.; Jacobsen, S. D.; Boffa Ballaran, T.

    2012-12-01

    Spinel phases (AB2O4) are common non-silicate oxides in the Earth's crust and upper mantle. A characteristic of this mineral group is the ability to host a wide range of transition metals. Here we summarize the influence of transition metals (Fe, Zn, and Mn) on the pressure dependence of elastic moduli of related spinels (magnetite, gahnite, and franklinite) using GHz-ultrasonic interferometry. Measurements were carried out up to 10 GPa in diamond-anvil cells using hydrostatic pressure media. Transition metals with unfilled 3d orbitals strongly influence the elastic properties of spinels. Franklinite (Zn,Mn)Fe2O4 and magnetite Fe3O4 with transition metals on both A and B cation sites exhibit pressure-induced mode softening of C44, whereas C44 of gahnite(ZnAl2O4) and spinel (MgAl2O4) exhibit positive pressure derivatives of the shear moduli. Spinels with two transition elements tend to undergo phase changes at a lower pressure than those with none or only one transition metal. Along the Mn-Zn solid solution, the variation of moduli with composition is non-linear, and a mid-range franklinite composition studied here shows a minimum in C44 compared with either end-member: MnFe2O 4 or ZnFe2O4. In general, the linear variation of sound velocity with density (Birch's Law) is followed by spinels, however spinels containing only one or no transition metals follow a distinct slope from those containing transition metals on both A and B sites. The Cauchy relation, 0.5(C12 - C44) = P is fulfilled by spinels with only one or no transition metals, suggesting that that Coulomb interactions dominate. Spinels with two transition metals fail to meet the Cauchy relation, indicating strong directional dependence and covalent character of bonding. The bonding character of transition metals is crucial to understanding the elastic behavior of natural and synthetic spinel solid solutions containing transition metals.

  15. Production and Isomeric Distribution of Xanthylium Cation Pigments and Their Precursors in Wine-like Conditions: Impact of Cu(II), Fe(II), Fe(III), Mn(II), Zn(II), and Al(III).

    PubMed

    Guo, Anque; Kontoudakis, Nikolaos; Scollary, Geoffrey R; Clark, Andrew C

    2017-03-22

    This study establishes the influence of Cu(II), Fe(II), Fe(III), Zn(II), Al(III), and Mn(II) on the oxidative production of xanthylium cations from (+)-catechin and either tartaric acid or glyoxylic acid in model wine systems. The reaction was studied at 25 °C using UHPLC and LC-HRMS for the analysis of phenolic products and their isomeric distribution. In addition to the expected products, a colorless product, tentatively assigned as a lactone, was detected for the first time. The results show the importance of Fe ions and a synergistic influence of Mn(II) in degrading tartaric acid to glyoxylic acid, whereas the other metal ions had minimal activity in this mechanistic step. Fe(II) and Fe(III) were shown to mediate the (+)-catechin-glyoxylic acid addition reaction, a role previously attributed to only Cu(II). Importantly, the study demonstrates that C-8 addition products of (+)-catechin are promoted by Cu(II), whereas C-6 addition products are promoted by Fe ions.

  16. [Comparison of heavy metal elements between natural and plantation forests in a subtropical Montane forest].

    PubMed

    Nie, Ming; Wan, Jia-Rong; Chen, Xiao-Feng; Wang, Li; Li, Bo; Chen, Jia-Kuan

    2011-11-01

    Heavy metals as one of major pollutants is harmful to the health of forest ecosystems. In the present paper, the concentrations of thirteen heavy metals (Fe, Al, Ti, Cr, Cu, Mn, V, Zn, Ni, Co, Pb, Se and Cd) were compared between natural and plantation forests in the Mt. Lushan by ICP-AES and atomic absorption spectroscopy. The results suggest that the soil of natural forest had higher concentrations of Fe, Al, Ti, Cu, Mn, V, Zn, Ni, Co, Pb, Se, and Cd than the plantation forest except for Cr. The soil of natural forest had a higher level of heavy metals than that of the plantation forest as a whole. This might be due to that the natural forest has longer age than the plantation forest, and fixed soil heavy metals take a longer period of time than the plantation forest.

  17. Implementation of an MgO-based metal removal step in the passive treatment system of Shilbottle, UK: column experiments.

    PubMed

    Caraballo, Manuel A; Rötting, Tobias S; Silva, Verónica

    2010-09-15

    Three laboratory column experiments were performed to test the suitability of two different MgO-rich reagents for removal of Mn and Al from the out-flowing waters of Shilbottle passive treatment system (Northumberland, UK). The input water was doped with 100 mg/L Zn in order to extrapolate results to waters in sulphide mining districts. One column was filled with a Dispersed Alkaline Substrate (DAS) containing 12.5% (v/v) caustic magnesia precipitator dust (CMPD) from Spain mixed with wood shavings, two columns were filled with DAS containing wood shavings and 12.5% or 25% (v/v), respectively, of dolomitic lime precipitator dust (DLPD) from Thrislington, UK. The two columns containing 12.5% of CMPD or DLPD completely removed the contaminants from the inflow water during the first 6 weeks of the experiment (mean removal of 88 mg/L Al, 96 mg/L Zn and 37 mg/L Mn), operating at an acidity load of 140 g acidity/m(2)day. At this moment, a substantial increase of the Al and Mn water concentration in the out-flowing waters of Shilbottle occurred (430 g acidity/m(2)day), leading to passivation of the reactive material and to the development of preferential flow paths within less than another 6 weeks, probably mainly due to Al precipitates. Al should be removed prior to MgO treatment. Copyright 2010 Elsevier B.V. All rights reserved.

  18. Constructing MnO{sub 2}/single crystalline ZnO nanorod hybrids with enhanced photocatalytic and antibacterial activity

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Yu, Weiwei; Liu, Tiangui, E-mail: tianguiliu@gmail.com; Cao, Shiyi

    In order to improve the photocatalytic and antibacterial activity of ZnO nanorods, ZnO nanorods decorated with MnO{sub 2} nanoparticles (MnO{sub 2}/ZnO nanorod hybrids) were prepared by using microwave assisted coprecipitation method under the influence of hydrogen peroxide, and the structure, photocatalytic activity and antibacterial property of the products were studied. Experimental results indicated that MnO{sub 2} nanoparticles are decorated on the surface of single crystalline ZnO nanorods. Moreover, the resultant MnO{sub 2}/ZnO nanorod hybrids have been proven to possess good photocatalytic and antibacterial activity, which their degradated efficiency for Rhodamin B (RhB) is twice as the pure ZnO nanorods. Enhancementmore » for photocatalytic and antibacterial activity is mainly attributed to the low band gap energy and excellent electrochemical properties of MnO{sub 2} nanoparticles. - Graphical abstract: The MnO{sub 2}/single crystalline ZnO nanorods hybrids, which MnO{sub 2} nanoparticles are loaded on the surface of ZnO nanorods, were prepared by the step-by-step precipitation method under the assistance of ammonia and hydrogen peroxide. Display Omitted - Highlights: • MnO{sub 2}/ZnO nanorod hybrids were prepared by the step-by-step assembly method. • Single crystalline ZnO nanorods can be decorated by MnO{sub 2} nanoparticles. • MnO{sub 2}/ZnO nanorod hybrids possess good photocatalytic and antibacterial activity. • MnO{sub 2} can improve the photocatalytic activity of ZnO nanorods under visible light.« less

  19. Super-bright and short-lived photoluminescence of textured Zn2SiO4:Mn2+ phosphor film on quartz glass

    NASA Astrophysics Data System (ADS)

    Park, Jehong; Park, Kwangwon; Lee, Jaebum; Kim, Jongsu; Seo, Kwangil; Kwon, Kevin; Kung, Patrick; Kim, Seongsin M.

    2010-02-01

    Green-emissive textured Zn2SiO4:Mn2+ phosphor film was fabricated by a thermal diffusion of ZnO:Mn on quartz glass. The characterization has been performed in terms of Mn2+ ions concentration (Mn/Zn=1~9 mol %). As an increase of Mn2+ ions concentration in the Zn2SiO4:Mn2+ phosphor film, the emission peak was red shifted from 519 nm to 526 nm, and the decay time to 10% of the maximum intensity was shorter from 20 ms to 0.5 ms. All annealed Zn2SiO4:Mn2+ phosphor films became textured along some hexagonal directions on the amorphous quartz glass. The brightest Zn2SiO4:Mn2+ film at optimal Mn2+ concentration of 5 % showed the photoluminescence brightness of 65 % and the shortened decay time of 4.4 ms in comparison with a commercially Zn2SiO4: Mn2+ powder phosphor screen. The excellencies can be attributed to a unique textured structure.

  20. Health risk assessment of heavy metal variability in sachet water sold in Ado-Odo Ota, South-Western Nigeria.

    PubMed

    Emenike, PraiseGod Chidozie; Tenebe, Theophilus Imokhai; Omeje, Maxwell; Osinubi, Damilare Samuel

    2017-08-31

    The sales of sachet water (SW), also known as "pure water" (PW), in Nigeria is a lucrative business. It serves many people, especially low-income earners, by providing a more affordable access to safe drinking water when compared with table water. However, some of the producers of SW do not effectively treat raw water before packaging them for sale. This study investigates the presence and concentrations of heavy metals, such as chromium (Cr), iron (Fe), manganese (Mn), copper (Cu), aluminum (Al), and zinc (Zn) in some samples of SW sold within Ota, Ogun State, Nigeria. Samples of SW from nine different producers were purchased for four consecutive weeks and analyzed to determine the concentrations of these heavy metals in them. Furthermore, health risk indicators, such as chronic daily intake (CDI) and health risk indices (HRI) for children and adults, were calculated separately. The metal concentrations were compared with allowable limits set by the World Health Organization (WHO), Nigerian Industrial Standard (NIS), and the United States Environmental Protection Agency (US EPA). High concentrations of Cr, Fe, and Al were found in all the nine samples and exceeded the maximum allowable limits (MAL) of all the standards considered. However, the concentrations of Zn, Mn, and Cu were within permissible limits. The HRIs of heavy metals were in the order of Cu > Fe > Zn > Mn > Al > Cr, but since the standard limits set for some metals were exceeded, proper and effective treatment is required to safeguard the health of consumers.

  1. Heavy metal distribution in blood, liver and kidneys of Loggerhead (Caretta caretta) and Green (Chelonia mydas) sea turtles from the Northeast Mediterranean Sea.

    PubMed

    Yipel, Mustafa; Tekeli, İbrahim Ozan; İşler, Cafer Tayer; Altuğ, Muhammed Enes

    2017-12-15

    The aim of the present study was to determine the concentrations of the most investigated environmentally relevant heavy metals in two highly endangered sea turtle species (Caretta caretta and Chelonia mydas) from the important nesting area on the Northeast Mediterranean Sea. The highest mean concentration was of Fe, while Hg and Pb were lowest. All tissue concentrations of Al, As, Fe and Mn were significantly different between the species. In particular, As, Cd, Cu, Mn, Ni, Se, Zn concentrations were lower in Caretta caretta and Cd, Hg, Mn, Zn concentrations were lower in Chelonia mydas than those reported in other parts of the world. Compared to studies conductud in other parts of the Mediterranean, Cd was lower. Copyright © 2017 Elsevier Ltd. All rights reserved.

  2. [Distribution Characteristics, Sources and Pollution Assessment of Trace Elements in Surficial Sediments of the Coastal Wetlands, Northeastern Hainan Island].

    PubMed

    Zhang, Wei-kun; Gan, Hua-yang; Bi, Xiang-yang; Wang, Jia-sheng

    2016-04-15

    Totally 128 surficial sediments samples were collected from the coastal wetlands, northeastern Hainan Island and analyzed for their concentrations of 14 elements including Al2O3, Fe2O3, MnO, Cu, Ni, Sr, Zn, V, Pb, Cr, Zr, As, Cd and Hg, TOC and grain sizes. The mean concentrations of trace metals V, Cr, Ni, Cu, Zn, As, Pb, Cd and Hg were (40.13 +/- 32.65), (35.92 +/- 26.90), (13.03 +/- 11.46), (11.56 +/- 10.27)-, (48.75 +/- 27.00), (5.48 +/- 1.60), ( 18.70 +/- 8.66), (0.054 +/- 0.045 ), (0.050 +/- 0.050) microg x g(-1), respectively, which were much lower than those in Pearl River Estuary, Yangzi River Estuary, Bohai Bay, upper crust and average shale. The average concentrations of Sr and Zr were much higher, reaching up to (1253.60 +/- 1649.58) microg x g(-1) and (372.40 +/- 516.49) microg x g(-1), respectively. The spatial distribution patterns of Al2O3, Fe2O3, MnO, Cu, Ni, Zn, V, Pb, Cr, Cd and Hg concentrations were the same as each other except for those of As, Sr and Zr. Generally, relatively high concentrations of these elements only appeared in the Haikou Bay, Nandu estuary, Dongzhai Harbor, Qinglan Harbor and Xiaohai in study area. The factor analysis revealed that the trace elements Al2O3 Fe2O3, MnO, Cu, Ni, Zn, V, Pb, Cr and part of Hg were mainly originated from the rock material by natural weathering processes, while the Cd and a part of Hg were from the biological source controlled by TOC. As and part of MnO were influenced by anthropogenic source, especially by aquacultures. Zr and some MnO were derived from heavy minerals dominated by the coarse grain of sediments. In contrast to the ERL, ERM and the results of enrichment factors (EF) , the environment of study area was good in general and the degree of contamination by trace elements was low on the whole. However, there are still some places where anthropogenic input have caused serious enrichments of trace elements and the occasional adverse effect on benthic organism induced by Ni could probably occur in 22% areas of all the sampling stations.

  3. Potentially toxic elements (PTEs) in soils from the surroundings of the Trans-Amazonian Highway, Brazil.

    PubMed

    de Souza, Edna Santos; Fernandes, Antonio Rodrigues; de Souza Braz, Anderson Martins; Sabino, Lorena Lira Leite; Alleoni, Luís Reynaldo Ferracciú

    2015-01-01

    The Trans-Amazonian Highway (TAH) is located in the northern region of Brazil, comprising a border region where agricultural, mining, and logging activities are the main activities responsible for fostering economic development, in addition to large hydroelectric plants. Such activities lead to environmental contamination by potentially toxic elements (PTEs). Environmental monitoring is only possible through the determination of element contents under natural conditions. Many extraction methods have been proposed to determine PTEs' bioavailability in the soil; however, there is no consensus about which extractor is most suitable. In this study, we determined the contents of PTEs in soils in the surroundings of TAH after mineral extraction with diethylenetriaminepentaacetic acid-triethanolamine (DTPA-TEA), Mehlich I, and Mehlich III solutions. Soil samples were collected in areas of natural vegetation in the vicinity of TAH in the state of Pará, Brazil. Chemical attributes and particle size were determined, besides concentrations of Fe, Al, Mn, and Ti by sulfuric acid digestion, Si after alkaline solution attack, and poorly crystalline Fe, Al, and "free" Fe oxides. Mehlich III solution extracted greater contents from Fe, Al, and Pb as compared to Mehlich I and DTPA-TEA and similar contents from Cd, Mn, Zn, and Cu. Significant correlations were found between concentrations of PTEs and the contents of Fe and Mn oxides as well as organic carbon and soil cation exchange capacity. Contents of Cu, Mn, Fe, and Zn by the three methods were positively correlated.

  4. Structural classification of RAO/sub 3/(MO)/sub n/ compounds (R = Sc, In, Y, or lanthanides; A = Fe(III), Ga, Cr, or Al; M = divalent cation; n = 1-11)

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Kimizuka, N.; Mohri, T.

    A series of new compounds (RAO/sub 3/MO)/sub n/ (n = 1-11) having spinel, YbFe/sub 2/O/sub 4/, or InFeO/sub 3/(ZnO)/sub n/ types of structures were newly synthesized (R = Sc, In, Y, Lu, Yb, Tm, or Er; A = Fe(III), Ga, Cr, or Al; M = Mg, Mn, Fe(II), Co, Ni, Zn, or Cd) at elevated temperatures. The conditions of synthesis and the lattice constants for these compounds are reported. The stacking sequences of the InO/sub 1.5/, (FeZn)O/sub 2.5/, and ZnO layers for InFeO/sub 3/(ZnO)/sub 10/ and the TmO/sub 1.5/, (AlZn)O/sub 2.5/, and ZnO layers for TmAlO/sub 3/(ZnO)/sub 11/ are presented,more » respectively. The crystal structures of the (RAO/sub 3/)/sub m/(MO)/sub n/ phases R = Sc, In, Y, or lanthanide elements; A = Fe(III), Ga, Cr, or Al; M = divalent cation elements; m and n = integer are classified into four crystal structure types (K/sub 2/NiF/sub 4/, CaFe/sub 2/O/sub 4/, YbFe/sub 2/O/sub 4/, and spinel), based upon the constituent cations R, A, and M.« less

  5. Accumulation of Heavy Metals in Tea Leaves and Potential Health Risk Assessment: A Case Study from Puan County, Guizhou Province, China

    PubMed Central

    Yang, Ruidong; Chen, Rong; Peng, Yishu; Wen, Xuefeng; Gao, Lei

    2018-01-01

    This study features a survey of the concentrations of aluminum (Al) and heavy metals (Mn, Pb, Cd, Hg, As, Cr, Ni, Cu, and Zn) in tea leaves and the corresponding cultivation soils (0–30 cm), carried out in Puan County (Guizhou Province, China). The average concentrations of Al, Mn, Pb, Cd, Hg, As, Cr, Ni, Cu, and Zn in the soil were 106 × 103, 214, 20.9, 0.09, 0.12, 17.5, 121, 27.8, 131.2, and 64 mg·kg−1, respectively. The heavy metals’ pollution indexes in the soil can be ranked as follows: Cu > Cr > Hg > As > Ni > Zn > Pb > Mn > Cd. The soil was moderately polluted by Cu because of the high geochemical background value of Cu in the area. The potential environment risk index (RI) showed that 7.69% out of the total sample sites were within the moderate level. Moreover, the ranges of Al, Mn, Pb, Cd, Hg, As, Cr, Ni, Cu, and Zn concentrations in young tea leaves were 250–660, 194–1130, 0.107–0.400, 0.012–0.092, 0.014–0.085, 0.073–0.456, 0.33–1.26, 6.33–14.90, 14.90–26.10, and 35.8–50.3 mg·kg−1, respectively. While in mature tea leaves, they were 4300–10,400, 536–4610, 0.560–1.265, 0.040–0.087, 0.043–0.089, 0.189–0.453, 0.69–2.91, 3.43–14.20, 6.17–16.25, and 9.1–20.0 mg·kg−1, respectively. Furthermore, the concentrations of Pb, Cu, As, Hg, Cd, and Cr in young tea leaves and mature tea leaves were all lower than the standard limit values (5.0, 30, 2.0, 0.3, 1.0, and 5.0 mg·kg−1 for Pb, Cu, As, Hg, Cd, and Cr, respectively) in China. Besides, the accumulation ability of tea leaves to Mn was the strongest, and the average bioconcentration factor (BCF) of Mn in mature tea leaves was 12.5. In addition, the average target hazard quotients (THQ) were all less than one for the young tea leaves and the average aggregate risk hazard index (HI) to adults was 0.272, indicating that there was not a potential health risk for adults through the consumption of the infusions brewed by young tea leaves. However, for mature tea leaves, the percentage which HI values were above one was 38.46%, and the risk to adults via the consumption of mature tea infusions were mainly contributed by Mn and Al. PMID:29342877

  6. Geochemistry of ferromanganese nodule-sediment pairs from Central Indian Ocean Basin

    NASA Astrophysics Data System (ADS)

    Pattan, J. N.; Parthiban, G.

    2011-01-01

    Fourteen ferromanganese nodule-sediment pairs from different sedimentary environments such as siliceous ooze (11), calcareous ooze (two) and red clay (one) from Central Indian Ocean Basin (CIOB) were analysed for major, trace and rare earth elements (REE) to understand the possible elemental relationship between them. Nodules from siliceous and calcareous ooze are diagenetic to early diagenetic whereas, nodule from red clay is of hydrogenetic origin. Si, Al and Ba are enriched in the sediments compared to associated nodules; K and Na are almost in the similar range in nodule-sediment pairs and Mn, Fe, Ti, Mg, P, Ni, Cu, Mo, Zn, Co, Pb, Sr, V, Y, Li and REEs are all enriched in nodules compared to associated sediments (siliceous and calcareous). Major portion of Si, Al and K in both nodules and sediments appear to be of terrigenous nature. The elements which are highly enriched in the nodules compared to associated sediments from both siliceous and calcareous ooze are Mo - (307, 273), Ni - (71, 125), Mn - (64, 87), Cu - (43, 80), Co - (23, 75), Pb - (15, 24), Zn - (9, 11) and V - (8, 19) respectively. These high enrichment ratios of elements could be due to effective diagenetic supply of metals from the underlying sediment to the nodule. Enrichment ratios of transition metals and REEs in the nodule to sediment are higher in CIOB compared to Pacific and Atlantic Ocean. Nodule from red clay, exhibit very small enrichment ratio of four with Mn and Ce while, Al, Fe, Ti, Ca, Na, K, Mg, P, Zn, Co, V, Y and REE are all enriched in red clay compared to associated nodule. This is probably due to presence of abundant smectite, fish teeth, micronodules and phillipsite in the red clay. The strong positive correlation ( r ⩾ 0.8) of Mn with Ni, Cu, Zn and Mo and a convex pattern of shale-normalized REE pattern with positive Ce-anomaly of siliceous ooze could be due to presence of abundant manganese micronodules. None of the major trace and REE exhibits any type of inter-elemental relationship between nodule and sediment pairs. Therefore, it may not be appropriate to correlate elemental behaviour between these pairs.

  7. Diurnal variations in, and influences on, concentrations of particulate and dissolved arsenic and metals in the mildly alkaline Wallkill River, New Jersey, USA

    USGS Publications Warehouse

    Barringer, J.L.; Wilson, T.P.; Szabo, Z.; Bonin, J.L.; Fischer, J.M.; Smith, N.P.

    2008-01-01

    Diurnal variations in particulate and dissolved As and metal concentrations were observed in mildly alkaline water from a wetlands site on the Wallkill River in northwestern New Jersey. The site, underlain by glacial sediments over dolomite bedrock, is 10 km downstream from a mined area of the Franklin Marble, host to Zn ores, also As and Mn minerals. In mid-September 2005, maxima and minima in dissolved-oxygen-concentration and pH, typically caused by photosynthesis and respiration, occurred at 2000 and 0800 hours. Concentrations of dissolved As (1.52-1.95 ??g/L) peaked at dusk (2000 hours), whereas dissolved Mn and Zn concentrations (76.5-96.9 and 8.55-12.8 ??g/L, respectively) were lowest at dusk and peaked at 1000 hours. These opposing cycles probably reflect sorption and desorption of As (an anion), and Mn and Zn (cations) as pH varied throughout the 24-h period. Doubly-peaked cycles of B, Cl, SO4, and nutrients also were observed; these may result from upstream discharges of septic-system effluent. Both recoverable amd particulate Al, Fe, Mn, and Zn concentrations peaked between 0200 and 0600 hours. The particulate metals cycle, with perturbations at 0400 hours, may be influenced by biological activity. ?? 2007 Springer-Verlag.

  8. Enhanced electrochemical performance of a ZnO-MnO composite as an anode material for lithium ion batteries.

    PubMed

    Song, Min Seob; Nahm, Sahn; Cho, Won Il; Lee, Chongmok

    2015-09-28

    A ZnO-MnO composite was synthesized using a simple solvothermal method combined with a high-temperature treatment. To observe the phase change during the heating process, in situ high-temperature XRD analysis was performed under vacuum conditions. The results indicated that ZnMn2O4 transformed into the ZnO-MnO composite phase starting from 500 °C and that this composite structure was retained until 700 °C. The electrochemical performances of the ZnO-MnO composite electrode were evaluated through galvanostatic discharge-charge tests and cyclic voltammetry analysis. Its initial coulombic efficiency was significantly improved to 68.3% compared to that of ZnMn2O4 at 54.7%. Furthermore, the ZnO-MnO composite exhibited improved cycling performance and enhanced rate capability compared with untreated ZnMn2O4. To clarify the discharge-charge mechanism of the ZnO-MnO composite electrode, the structural changes during the charge and discharge processes were also investigated using ex situ XRD and TEM.

  9. Adsorption of multi-heavy metals Zn and Cu onto surficial sediments: modeling and adsorption capacity analysis.

    PubMed

    Li, Shanshan; Zhang, Chen; Wang, Meng; Li, Yu

    2014-01-01

    Improved multiple regression adsorption models (IMRAMs) was developed to estimate the adsorption capacity of the components [Fe oxides (Fe), Mn oxides (Mn), organic materials (OMs), residuals] in surficial sediments for multi-heavy metal Zn and Cu. IMRAM is an improved version over MRAM, which introduces a computer program in the model developing process. As MRAM, Zn(Cu) IMRAM, and Cu(Zn) IMRAM again confirmed that there is significant interaction effects that control the adsorption of compounded Zn and Cu, which was neglected by additional adsorption model. The verification experiment shows that the relative deviation of the IMRAMs is less than 13%. It is revealed by the IMRAMs that Mn, which has the greatest adsorption capability for compounded Zn and Cu (54.889 and 161.180 mg/l, respectively), follows by interference adsorption capacity of Fe/Mn (-1.072 and -24.591 mg/l respectively). Zn and Cu influence each other through different mechanisms. When Zn is the adsorbate, compounded Cu mainly affects the adsorption capacities of Fe/Mn and Fe/Mn/OMs; while when Cu is the adsorbate, compounded Zn mainly exerts its effect on Mn, Fe/Mn, and Mn/OMs. It also shows that the compounded Zn or Cu weakened the interference adsorption of Fe/Mn, and meanwhile, strengthened the interference adsorption of Mn/OMs.

  10. Trace Metals Derived from Electronic Cigarette (ECIG) Generated Aerosol: Potential Problem of ECIG Devices That Contain Nickel

    PubMed Central

    Palazzolo, Dominic L.; Crow, Andrew P.; Nelson, John M.; Johnson, Robert A.

    2017-01-01

    Introduction: ECIGs are currently under scrutiny concerning their safety, particularly in reference to the impact ECIG liquids (E-liquids) have on human health. One concern is that aerosolized E-liquids contain trace metals that could become trapped in respiratory tissues and induce pathology. Methods: To mimic this trapping, peristaltic pumps were used to generate and transport aerosol onto mixed cellulose ester (MCE) membranes where aluminum (Al), arsenic (As), cadmium (Cd), copper (Cu), iron (Fe), manganese (Mn), nickel (Ni), lead (Pb), and zinc (Zn) were subsequently captured and quantified. The presence of trace metals on unexposed MCE membranes and on MCE membranes exposed to mainstream smoke served as control and comparison, respectively. The presence of these metals was also determined from the E-liquid before aerosolization and untouched by the ECIG device. All metals were quantified using ICP-MS. The ECIG core assembly was analyzed using scanning electron microscopy with elemental analysis capability. Results: The contents (μg) of Al, As, Cd, Cu, Fe, Mn, Ni, Pb, and Zn on control MCE membranes were 1.2 ± 0.2, 0.050 ± 0.002, 0.047 ± 0.003, 0.05 ± 0.01, 0.001 ± 0.001, 0.16 ± 0.04, 0.005 ± 0.003, 0.014 ± 0.006, and 0.09 ± 0.02, respectively. The contents of all trace metals on MCE membranes exposed to aerosol were similar to controls, except Ni which was significantly (p < 0.01) higher (0.024 ± 0.004 μg). In contrast, contents of Al, As, Fe, Mn, and Zn on MCE membranes exposed to smoke were significantly higher (p < 0.05) than controls. The contents of Al, As, Cu, Fe, and Mn on smoke-exposed MCE membranes were also significantly higher (p < 0.05) than their content on aerosol-exposed membranes. The contents per cigarette equivalent of metals in E-liquid before aerosolization were negligible compared to amounts of aerosolized E-liquid, except for Fe (0.002 μg before and 0.001 μg after). Elemental analysis of the core assembly reveals the presence of several of these trace metals, especially Al, Fe, Ni, and Zn. Conclusions: In general, from the single ECIG-device/E-liquid combination used, the amount of trace metals from ECIG-generated aerosol are lower than in traditional mainstream smoke, Only Ni in the ECIG-generated aerosol was higher than control. The most probable source of Ni in this aerosol is the core assembly. PMID:28119618

  11. Cryogenic and elevated temperature strengths of an Al-Zn-Mg-Cu alloy modified with Sc and Zr

    NASA Astrophysics Data System (ADS)

    Senkova, S. V.; Senkov, O. N.; Miracle, D. B.

    2006-12-01

    The effect of minor additions of Sc and Zr on tensile properties of two developmental Al-Zn-Mg-Cu alloys was studied in the temperature range -196°C to 300°C. Due to the presence of Sc and Zr in a fine dispersoid form, both low-temperature and elevated temperature strengths of these alloys are much higher than those of similar 7000 series alloys that do not contain these elements. After short holding times (up to 10 hours) at 205°C, the strength of these alloys is higher than those of high-temperature Al alloys 2219-T6 and 2618-T6; however, the latter alloys show better strength after longer holding times. It is suggested that additional alloying of the Sc-containing Al-Zn-Mg-Cu alloys with other dispersoid-forming elements, such as Ni, Fe, Mn, and Si, with a respective decrease in the amounts of Zn and Mg may further improve the elevated temperature strength and decrease the loss of strength with extended elevated temperature exposure.

  12. Synthesis and Luminescence Properties of Core/Shell ZnS:Mn/ZnO Nanoparticles.

    PubMed

    Jiang, Daixun; Cao, Lixin; Liu, Wei; Su, Ge; Qu, Hua; Sun, Yuanguang; Dong, Bohua

    2009-01-01

    In this paper the influence of ZnO shell thickness on the luminescence properties of Mn-doped ZnS nanoparticles is studied. Transmission electron microscopy (TEM) images showed that the average diameter of ZnS:Mn nanoparticles is around 14 nm. The formation of ZnO shells on the surface of ZnS:Mn nanoparticles was confirmed by X-ray diffraction (XRD) patterns, high-resolution TEM (HRTEM) images, and X-ray photoelectron spectroscopy (XPS) measurements. A strong increase followed by a gradual decline was observed in the room temperature photoluminescence (PL) spectra with the thickening of the ZnO shell. The photoluminescence excitation (PLE) spectra exhibited a blue shift in ZnO-coated ZnS:Mn nanoparticles compared with the uncoated ones. It is shown that the PL enhancement and the blue shift of optimum excitation wavelength are led by the ZnO-induced surface passivation and compressive stress on the ZnS:Mn cores.

  13. AMELIORATION OF ETHANOL-INDUCED DYSMORPHOGENESIS IN RODENT EMBRYOS IN VITRO USING ADENOVIRAL-MEDIATED EXPRESSION OF CU,ZN-SUPEROXIDE DISMUTASE (SOD1) OR MN-SUPEROXIDE DISMUTASE (SOD2)

    EPA Science Inventory

    Ethanol produces dysmorphogenesis in offspring when pregnant animals are exposed in vivo (Chaudhuri 2000; Hannigan and Armant, 2000) and by direct exposure of neurulation staged embryos to ethanol in vitro (Kotch et al., 1995; Hunter et al., 1994 ; Thompson and Folb, 1982). The a...

  14. Uptake of Al, As, Cr, Cd, Cu, Fe, Mn, Ni, Pb, Sr, and Zn in native wheatgrasses, wildryes, and bluegrass on three metal-contaminated soils from Montana

    USDA-ARS?s Scientific Manuscript database

    One of the biggest challenges to successfully phytoremediate contaminated mineland soils is the identification of native plants that possess a broad adaptation to ecological sites and either exclude or uptake heavy metals of interest. This study evaluated forage concentrations of aluminum (Al), ars...

  15. [Effects of thiourea on pH and availability of metal ions in acid red soil].

    PubMed

    Yang, Bo; Wang, Wen; Zeng, Qing-Ru; Zhou, Xi-Hong

    2014-03-01

    Through the simulation research, the effects of application of thiourea and urea on pH and availability of metal ions in acid red soil were studied, and the results showed that after applying urea, the soil pH increased in the first experimental stage and then reduced gradually to a low level, however, decreased trends of soil pH values were inhibited by the application of thiourea, especially when the concentration of thiourea reached to 5.0 mmol x kg(-1) dry soil, the soil pH was stable at high level, which exceeded to 6.0. It proved that the application of thiourea could inhibit the soil acidification due to urea application. After applying urea with different concentrations of thiourea, the available contents of Zn and Al decreased with the increasing concentration of thiourea, nevertheless, when the concentration of thiourea reached to 5.0 mmol x kg(-1), the available content of Mn was stable at high level which was over 110 mg x kg(-1). In addition, the results showed a highly significant negative correlation between the soil pH and the available content of Cu, Zn and Al, but for Mn, no discipline was found between the soil pH and the availability after applying thiourea. Moreover, the soil pH became higher after applying urea with thiourea compared to add urea only, which led to the decreasing of available content of Al, and it was benefited for the control of the phytotoxic effect of Al. The available content of Mn in the soil not only depended on soil pH but also the content of thiourea due to its redox and complexing reaction with Mn.

  16. Tolerance and growth kinetics of bacteria isolated from gold and gemstone mining sites in response to heavy metal concentrations.

    PubMed

    Oladipo, Oluwatosin Gbemisola; Ezeokoli, Obinna Tobechukwu; Maboeta, Mark Steve; Bezuidenhout, Jacobus Johannes; Tiedt, Louwrens R; Jordaan, Anine; Bezuidenhout, Cornelius Carlos

    2018-04-15

    Response and growth kinetics of microbes in contaminated medium are useful indices for the screening and selection of tolerant species for eco-friendly bio-augmentative remediation of polluted environments. In this study, the heavy metal (HM) tolerance, bioaccumulation and growth kinetics of seven bacterial strains isolated from mining sites to 10 HMs (Cd, Hg, Ni, Al, Cr, Pb, Cu, Fe, Mn and Zn) at varied concentrations (25-600 mgL -1 ) were investigated. The isolates were phylogenetically (16S rRNA gene) related to Lysinibacillus macroides, Achromobacter spanius, Bacillus kochii, B. cereus, Klebsiella pneumoniae, Pseudomonas mosselii and P. nitroreducens. Metal tolerance, effects on lag phase duration and growth rates were assessed using the 96-well micro-titre method. Furthermore, metal bioaccumulation and quantities within cells were determined by transmission electron microscopy and electron dispersive x-ray analyses. Tolerance to Ni, Pb, Fe and Mn occurred at highest concentrations tested. Growth rates increased with increasing Fe concentrations, but reduced significantly (p < .05) with increasing Zn, Cu, Hg, Cd and Al. Significantly higher (p < .05) growth rates (compared to controls) was found with some isolates in Hg (25 mgL -1 ), Ni (100 mgL -1 ), Cr (150 mgL -1 ), Mn (600 mgL -1 ), Pb (100 mgL -1 ), Fe (600 mgL -1 ) and Al (50 mgL -1 ). Lag phase urations were isolate- and heavy metal-specific, in direct proportion to concentrations. A. spanius accumulated the most Mn and Zn, while B. cereus accumulated the most Cu. Metals accumulated intra-cellularly without cell morphology distortions. The isolates' multi-metal tolerance, intra-cellular metal bioaccumulation and growth kinetics suggest potentials for application in the synergetic biodegradation and bioremediation of polluted environments, especially HM-rich sites. Copyright © 2018 Elsevier Ltd. All rights reserved.

  17. Control of conduction type in ferromagnetic (Zn,Sn,Mn)As2 thin films by changing Mn content and effect of annealing on thin films with n-type conduction

    NASA Astrophysics Data System (ADS)

    Minamizawa, Yuto; Kitazawa, Tomohiro; Hidaka, Shiro; Toyota, Hideyuki; Nakamura, Shin-ichi; Uchitomi, Naotaka

    2018-04-01

    The conduction type in (Zn,Sn,Mn)As2 thin films grown by molecular beam epitaxy (MBE) on InP substrates was found to be controllable from p-type to n-type as a function of Mn content. n-type (Zn,Sn,Mn)As2 thin films were obtained by Mn doping of more than approximately 11 cat.%. It is likely that Mn interstitials (MnI) incorporated by excess Mn doping are located at tetrahedral hollow spaces surrounded by Zn and Sn cation atoms and four As atoms, which are expected to act as donors in (Zn,Sn,Mn)As2, resulting in n-type conduction. The effect of annealing on the structural, electrical and magnetic properties of n-type (Zn,Sn,Mn)As2 thin films was investigated as functions of annealing temperature and time. It was revealed that even if the annealing temperature is considerably higher than the growth temperature of 320 °C, the magnetic properties of the thin films remain stable. This suggests that a MnI complex surrounded by Zn and Sn atoms is thermally stable during high-temperature annealing. The n-type (Zn,Sn,Mn)As2 thin films may be suitable for application as n-type spin-polarized injectors.

  18. Effect of sintering temperature on the microstructure, electrical and magnetic properties of Zn0.98 Mn0.02O material

    NASA Astrophysics Data System (ADS)

    Sebayang, K.; Aryanto, D.; Simbolon, S.; Kurniawan, C.; Hulu, S. F.; Sudiro, T.; Ginting, M.; Sebayang, P.

    2018-02-01

    Zn0.98Mn0.02O material was synthesized from ZnO and MnO2 powders using solid state reaction method. The microstructure, electrical and magnetic properties of Zn0.98Mn0.02O were studied as a function of sintering temperature. The X-ray diffraction analysis indicates that the main phase of synthesized sample is composed of hexagonal wurtzite ZnO phase. While the secondary phase of ZnMnO3 were found at the sintering temperature of 700°C and 900°C. The electrical properties measurement of Zn0.98Mn0.02O sample revealed that the resistivity and the dielectric constant of samples increase with the increase of sintering temperature. The ferromagnetic properties at room temperature were observed in the Zn0.98Mn0.02O samples sintered at 500°C and 700°C. It also found that the increase in sintering temperature leads to a tendency toward the changes in the magnetic properties into paramagnetic. The presence of ZnMnO3 secondary phases in Zn0.98Mn0.02O system is believed to be a factor that affects the decrease of the electrical and magnetic properties of the sample.

  19. Template-free fabrication of graphene-wrapped mesoporous ZnMn2O4 nanorings as anode materials for lithium-ion batteries.

    PubMed

    Zhou, Weiwei; Wang, Dong; Zhao, Limin; Ding, Chunyan; Jia, Xingtao; Du, Yu; Wen, Guangwu; Wang, Huatao

    2017-06-16

    We rationally designed a facile two-step approach to synthesize ZnMn 2 O 4 @G composite anode material for lithium-ion batteries (LIBs), involving a template-free fabrication of ZnMn 2 O 4 nanorings and subsequent coating of graphene sheets. Notably, it is the first time that ring-like ZnMn 2 O 4 nanostructure is reported. Moreover, our system has been demonstrated to be quite powerful in producing ZnMn 2 O 4 nanorings regardless of the types of Zn and Mn-containing metal salts reactants. The well-known inside-out Ostwald ripening process is tentatively proposed to clarify the formation mechanism of the hollow nanorings. When evaluated as anode material for LIBs, the resulting ZnMn 2 O 4 @G hybrid displays significantly improved lithium-storage performance with high specific capacity, good rate capability, and excellent cyclability. After 500 cycles, the ZnMn 2 O 4 @G hybrid can still deliver a reversible capacity of 958 mAh g -1 at a current density of 200 mA g -1 , much higher than the theoretical capacity of 784 mAh g -1 for pure ZnMn 2 O 4 . The outstanding electrochemical performance should be reasonably ascribed to the synergistic interaction between hollow and porous ZnMn 2 O 4 nanorings and the three-dimensional interconnected graphene sheets.

  20. Surface characterization of ZnO/ZnMn{sub 2}O{sub 4} and Cu/Mn{sub 3}O{sub 4} powders obtained by thermal degradation of heterobimetallic complexes

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Barrault, Joeel, E-mail: joel.barrault@univ-poitiers.fr; Makhankova, Valeriya G., E-mail: leram@univ.kiev.ua; Khavryuchenko, Oleksiy V.

    2012-03-15

    From the selective transformation of the heterometallic (Zn-Mn or Cu-Mn) carboxylate complexes with 2,2 Prime -bipyridyl by thermal degradation at relatively low (350 Degree-Sign C) temperature, it was possible to get either well defined spinel ZnMn{sub 2}O{sub 4} over zinc oxide or well dispersed copper particles surrounded by a manganese oxide (Mn{sub 3}O{sub 4}) in a core-shell like structure. Morphology of the powder surface was examined by scanning electron microscopy with energy dispersive X-ray microanalysis (SEM/EDX). Surface composition was determined by X-ray photoelectron spectroscopy (XPS). Specific surface of the powders by nitrogen adsorption was found to be 33{+-}0.2 and 9{+-}0.06more » m{sup 2} g{sup -1} for Zn-Mn and Cu-Mn samples, respectively, which is comparable to those of commercial products. - Graphical abstract: From the selective transformation of heterometallic (Zn-Mn or Cu-Mn) carboxylate complexes, it was possible to get either well defined spinel ZnMn{sub 2}O{sub 4} over zinc oxide or well dispersed copper particles surrounded by a manganese oxide (Mn{sub 3}O{sub 4}) in a core-shell like structure. Highlights: Black-Right-Pointing-Pointer Thermal degradation of heterometallic complexes results in fine disperse particles. Black-Right-Pointing-Pointer Core-shell Cu/Mn{sub 3}O{sub 4} particles are obtained. Black-Right-Pointing-Pointer ZnMn{sub 2}O{sub 4} spinel layer covers ZnO particles.« less

  1. Synthesis of metal-doped Mn-Zn ferrite from the leaching solutions of vanadium slag using hydrothermal method

    NASA Astrophysics Data System (ADS)

    Liu, Shiyuan; Wang, Lijun; Chou, Kuochih

    2018-03-01

    Using vanadium slag as raw material, Metal-doped Mn-Zn ferrites were synthesized by multi-step processes including chlorination of iron and manganese by NH4Cl, selective oxidation of Fe cation, and hydrothermal synthesis. The phase composition and magnetic properties of synthesized metal-doped Mn-Zn ferrite were characterized by X-ray powder diffraction, Raman spectroscopy, transmission electron microscopy (TEM), X-ray photon spectra (XPS) and physical property measurement. It was found that Mn/Zn mole ratio significantly affected the magnetic properties and ZnCl2 content significantly influenced the purity of the phase of ferrite. Synthesized metal-doped Mn-Zn ferrite, exhibiting a larger saturation magnetization (Ms = 60.01 emu/g) and lower coercivity (Hc = 8.9 Oe), was obtained when the hydrothermal temperature was controlled at 200 °C for 12 h with a Mn/Zn mole ratio of 4. The effect of ZnCl2 content, Mn/Zn mole ratio and temperature on magnetic properties of the synthesized metal-doped Mn-Zn ferrite were systemically investigated. This process provided a new insight to utilize resources in the aim of obtaining functional materials.

  2. Magnetic properties and photovoltaic applications of ZnO:Mn nanocrystals.

    PubMed

    Zhang, Ying; Han, Fengxiang; Dai, Qilin; Tang, Jinke

    2018-05-01

    A simple and large-scale synthetic method of Mn doped ZnO (ZnO:Mn) was developed in this work. ZnO:Mn nanocrystals with hexagonal structure were prepared by thermal decomposition of zinc acetate and manganese acetate in the presence of oleylamine and oleic acid with different temperatures, ligand ratios, and Mn doping concentrations. The particle size (47-375 nm) and morphology (hexagonal nanopyramid, hexagonal nanodisk and irregular nanospheres) of ZnO:Mn nanocrystals can be controlled by the ratio of capping ligand, reaction temperature, reaction time and Mn doping concentration. The corresponding optical and magnetic properties were systemically studied and compared. All samples were found to be paramagnetic with antiferromagnetic (AFM) exchange interactions between the Mn moments in the ZnO lattice, which can be affected by the reaction conditions. The quantum dot sensitized solar cells (QDSSCs) were fabricated based on ZnO:Mn nanocrystals and CdS quantum dots, and the device performance affected by Mn doping concentration was also studied and compared. Copyright © 2018 Elsevier Inc. All rights reserved.

  3. Efficient photocatalytic degradation of malachite green dye under visible irradiation by water soluble ZnS:Mn/ZnS core/shell nanoparticles

    NASA Astrophysics Data System (ADS)

    Khaparde, Rohini A.; Acharya, Smita A.

    2018-05-01

    ZnS:Mn/ ZnS core/shell nanoparticles was prepared by two step synthesis method. In first step, oleic acid - coated Mn doped ZnS core nanoparticles were prepared which were charged through ligand exchange. Shell of ZnS NPs was finally deposited upon the surface of charged Mn doped ZnS core. Scanning electron microscopy (SEM) image exhibit morphological confirmation of ZnS:Mn/ZnS core/shell. As Nano ZnS are the most suitable candidates for photocatalyst that extensively involved in degradation and complete mineralization of various toxic organic pollutants owing to its high efficiency, strong oxidizing power, non-toxicity, high photochemical and biological stability, corrosive resistance and low cost. Photodegradation of malachite green is systematically investigated by adding different molar proportional of ZnS:Mn/ZnS core/shell in the dye. The rate of de-coloration of dye is detected by UV-VIS absorption spectroscopy. Efficient detoriation in the colour of dye is attributed to the core /shell morphology of the particles.

  4. Excellent Brightness with Shortening Lifetime of Textured Zn2SiO4:Mn2+ Phosphor Films on Quartz Glass

    NASA Astrophysics Data System (ADS)

    Park, Jehong; Park, Kwangwon; Lee, Jaebum; Kim, Jongsu; Kim, Seongsin Margaret; Kung, Patrick

    2010-04-01

    Green-emissive textured Zn2SiO4:Mn2+ phosphor films were fabricated by the thermal diffusion of ZnO:Mn on quartz glass. The Zn2SiO4:Mn2+ phosphor films became textured along several hexagonal directions and their chemical composition was continuously graded at the interface. The decay time of Mn2+ was as short as 4.4 ms, and the optical transition probability of the films defined as the inverse of decay time showed a strong correlation with film texture degree as a function of annealing temperature. The brightest Zn2SiO4:Mn2+ film showed a photoluminescent brightness as high as 65% compared with a commercial Zn2SiO4:Mn2+ phosphor powder screen and a maximum absolute transparency of 70%. These excellent optical properties are explained by the combination of the unique textured structure and continuous grading of the Zn2SiO4:Mn2+ chemical composition at the interface.

  5. Contributions of phase and structural transformations in multicomponent Al-Mg alloys to the linear and nonlinear mechanisms of anelasticity

    NASA Astrophysics Data System (ADS)

    Golovin, I. S.; Bychkov, A. S.; Mikhailovskaya, A. V.; Dobatkin, S. V.

    2014-02-01

    The effects of the processes of severe plastic deformation (SPD), recrystallization, and precipitation of the β phase in multicomponent alloys of the Al-5Mg-Mn-Cr and Al-(4-5%)Mg-Mn-Zn-Sc systems on the mechanisms of grain-boundary relaxation and dislocation-induced microplasticity have been studied in some detail. To stabilize the ultrafine-grained structure and prevent grain growth, dispersed Al-transition-metal particles, such as Al3Zr, Al6Mn, Al7Cr, Al6(Mn,Cr), Al18Cr2Mg3 have been used. We have special interest in alloys with additions of scandium, which forms compounds of the Al3Sc type and favors the precipitation of finer particles compared to the aluminides of other transition metals. After SPD, Al-(4-5%)Mg-Mn-Zr-Sc alloys exhibit an enhanced recrystallization temperature. The general features of the dislocation and grain-boundary anelasticity that have been established for the binary Al-Mg alloys are retained; i.e., (1) the decrease in the dislocation density in the process of recrystallization of cold-worked alloys leads to the formation of a pseudo-peak in the curves of the temperature dependences of internal friction (TDIF) and to a decrease in the critical amplitude of deformation corresponding to the onset of dislocation motion in a stress field; (2) the precipitation of the β phase suppresses the grain-boundary relaxation; (3) the dissolution of the β phase, the passage of the magnesium atoms into the solid solution, and the precipitation of the β' phase upon heating hinder the motion of dislocations; (4) the coarsening of the highly dispersed particles containing Zr and Sc increases the dislocation mobility. The grain-boundary relaxation and dislocation-impurity interaction and their temperature dependences, as well as processes of the additional alloying of the binary alloys by Mn, Cr, Zr, and Sc, have been estimated quantitatively.

  6. Optical properties and toxicity of undoped and Mn-doped ZnS semiconductor nanoparticles synthesized through the aqueous route

    NASA Astrophysics Data System (ADS)

    Labiadh, Houcine; Sellami, Badreddine; Khazri, Abdelhafidh; Saidani, Wiem; Khemais, Said

    2017-02-01

    Undoped and Mn-doped ZnS nanoparticles were synthesized at 95 °C in basic aqueous solution using the nucleation-doping strategy. Various samples of the Mn:ZnS NPs with 5, 10 and 20% of Mn dopant have been prepared and characterized using X-ray diffraction, energy-dispersive X-ray analysis, high resolution electron microscopy and photoluminescence (PL) measurements. When increasing the concentration of manganese Mn, the photoluminescence intensity gradually decreases. The PL spectra of the Mn-doped ZnS nanoparticles at room temperature exhibit both, the 450 nm blue defect-related emission and the 592 nm orange Mn2+ emission. It is vital to obtain NPs that meet the application requirements, however their environmental toxicity needs to be investigated. In this study, the induction of oxidative stress within the digestive gland of the Ruditapes decussatus organism (clam) is described. Antioxidant enzyme activities (superoxide dismutase (SOD) and catalase (CAT)) as well as malondialdehyde (MDA) levels have been determined in the digestive gland after exposure to 100 μg/L of ZnS, ZnS:Mn (5%), ZnS:Mn (10%) and ZnS:Mn (20%). The nanomaterials studied exhibit different responses in the digestive gland. Undoped Mn-ZnS has no effect on the markers considered, showing the limited interaction between this nanoparticle and the cells of the test organisms. In contrast, Mn-doped ZnS increases the activities of SOD and CAT and the level of MDA species, although this toxicity is highly dependent on the chemical properties of the material. These findings provide ideas for future considerations of ZnS nanoparticles, as well as information on the interaction between these materials and an aquatic environment. These data are the first evidence available of the formation of ZnS NPs using aqueous method and are an indication of the importance of knowing the biological target of the NPs when testing their potential impact on environmental model organisms.

  7. Phosphorescence detection of manganese(VII) based on Mn-doped ZnS quantum dots

    NASA Astrophysics Data System (ADS)

    Deng, Pan; Lu, Li-Qiang; Cao, Wei-Cheng; Tian, Xi-Ke

    2017-02-01

    The phosphorescent L-cysteine modified manganese-doped zinc sulfide quantum dots (L-cys-MnZnS QDs) was developed for a highly sensitive detection of permanganate anions (MnO4-). L-cys-MnZnS QDs, which were easily synthesized in aqueous media using safe and low-cost materials, can emit intense phosphorescence even though the solution was not deoxygenated. However, the phosphorescence of L-cys-Mn-ZnS QDs was strongly quenched by MnO4- ascribed to the oxidation of L-cys and the increase of surface defects on L-cys-MnZnS QDs. Under the optimal conditions, L-cys-MnZnS QDs offer high selectivity over other anions for MnO4- determination, and good linear Stern-Volmer equation was obtained for MnO4- in the range of 0.5-100 μM with a detection limit down to 0.24 μM. The developed method was finally applied to the detection of MnO4- in water samples, and the spike-recoveries fell in the range of 95-106%.

  8. Evidence for Different Reaction Pathways for Liquid and Granular Micronutrients in a Calcareous Soil

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Hettiarachchi, Ganga M.; McLaughlin, Mike J.; Scheckel, Kirk G.

    2008-06-16

    The benefits of Mn and Zn fluid fertilizers over conventional granular products in calcareous sandy loam soils have been agronomically demonstrated. We hypothesized that the differences in the effectiveness between granular and fluid Mn and Zn fertilizers is due to different Mn and Zn reaction processes in and around fertilizer granules and fluid fertilizer bands. We used a combination of several synchrotron-based x-ray techniques, namely, spatially resolved micro-x-ray fluorescence (?-XRF), micro-x-ray absorption near edge structure spectroscopy (?-XANES), and bulk-XANES and -extended x-ray absorption fine structure (EXAFS) spectroscopy, along with several laboratory-based x-ray techniques to speciate different fertilizer-derived Mn and Znmore » species in highly calcareous soils to understand the chemistry underlying the observed differential behavior of fluid and granular micronutrient forms. Micro-XRF mapping of soil-fertilizer reactions zones indicated that the mobility of Mn and Zn from liquid fertilizer was greater than that observed for equivalent granular sources of these micronutrients in soil. After application of these micronutrient fertilizers to soil, Mn and Zn from liquid fertilizers were found to remain in comparatively more soluble solid forms, such as hydrated Mn phosphate-like, Mn calcite-like, adsorbed Zn-like, and Zn silicate-like phases, whereas Mn and Zn from equivalent granular sources tended to transform into comparatively less soluble solid forms such as Mn oxide-like, Mn carbonate-like, and Zn phosphate-like phases.« less

  9. The Ti-Mn system revisited: experimental investigation and thermodynamic modelling.

    PubMed

    Khan, A U; Brož, P; Premović, M; Pavlů, J; Vřeštál, J; Yan, X; Maccio, D; Saccone, A; Giester, G; Rogl, P

    2016-08-17

    As the Ti-Mn phase diagram is part of numerous ternary and higher order systems of technological importance, the present paper defines phase relations which have been experimentally established throughout this work from 800 °C to the melting range based on Differential Thermal Analyses (DTA), X-ray powder diffraction, metallography and Electron Probe Micro Analysis (EPMA) techniques on ∼50 alloys, which were prepared by arc melting or high frequency melting under high purity argon starting from freshly cleaned metal ingots. Novel compounds were identified and reaction isotherms were redefined accordingly. In the Ti-rich region a novel compound TiMn was detected, sandwiched between the known phases: TiMn1-x (∼45 at% Mn) and TiMn1+x (∼55 at% Mn). In the Mn-rich region the hitherto unknown crystal structure of TiMn∼3 was solved from X-ray single crystal diffraction data and found to be of a unique structure type Ti6(Ti1-xMnx)6Mn25 (x = 0.462; space group Pbam (#55); a = 0.79081(3) nm, b = 2.58557(9) nm, c = 0.47931(2) nm), which consists of two consecutive layers of the hexagonal MgZn2-type Laves phase (TiMn2) and a combined layer of alternate structure blocks of MgZn2 type and Zr4Al3 type. Whereas TiMn can be considered as a line compound (solubility range <∼1 at%), the homogeneity regions of the Ti-Mn compounds are significant (determined by EPMA): TiMn1-x (44.0 to 46.6 at% Mn), TiMn1+x (54.6 to 56.3 at% Mn), Ti1+xMn2-x (MgZn2-type, 59 to 69 at% Mn at 1000 °C: -0.08 < x < 0.23), TiMn∼3 (unique type; 74 to 76.5 at% Mn) and TiMn∼4 (R-phase: Ti8(TixMn1-x)6Mn39, 80 to 84 at% Ti). Supported by ab initio calculations of the ground state energy for the Laves phase, the new experimental results enabled thermodynamic modelling of the entire Ti-Mn phase diagram providing a complete and novel set of thermodynamic data thus providing a sound basis for future thermodynamic predictions of higher order Ti-Mn-X-Y systems.

  10. Influence of heavy metal leaf contaminants on the in vitro growth of urban-tree phylloplane-fungi

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Smith, W.H.

    1977-01-01

    The surfaces of urban woody vegetation are contaminated with varying amounts of numerous metallic compounds, including Cd, Cu, Mn, Al, Cr, Ni, Fe, Pb, Na, and Zn. To examine the possibility that these metals may affect phylloplane fungi, the above cations were tested in vitro for their ability to influence the growth of numerous saprophytic and parasitic fungi isolated from the leaves of London plane trees. Considerable variation in growth inhibition by the metals was observed. Generally Aureobasidium pullulans, Epicoccum sp., and Phialophora verrucosa were relatively tolerant; Gnomonia platani, Cladsporium sp., and Pleurophomella sp. were intermediate; and Pestalotiopsis and Chaetomiummore » sp. were relatively sensitive to the incorporation of certain metals into solid and liquid media. If similar growth inhibitions occur in nature, competitive abilities or population structures of plant surface microbes may be altered by surface metal contamination. Metals causing the greatest and broadest spectrum growth suppression included Ni, Zn, Pb, Al, Fe, and Mn. 25 references, 4 figures.« less

  11. Tracking Metal Pollution in Lake Chapala: Concentrations in Water, Sediments, and Fish.

    PubMed

    Torres, Zaria; Mora, Miguel A; Taylor, Robert J; Alvarez-Bernal, Dioselina

    2016-09-01

    We measured concentrations of selected metals (Al, Ba, Cu, Mn, Hg, Sr, V, and Zn) in water, sediments, and fish from Lake Chapala and a reference site to evaluate potential negative effects on wildlife, particularly fish-eating birds. Fish metal concentrations ranged from 0.05 µg/g wet weight (ww) for Al and Cu to 64.70 µg/g ww for Sr. There was a positive and significant correlation between fish length and metals particularly for Ba, Cu, Mn, and Zn in Lake Chapala (p < 0.05). However, there were no significant correlations between metal concentrations and δ(15)N values in fish indicating no biomagnification through the food web. Overall, metal concentrations in water, sediments, and fish were similar to and in some cases below those reported for Lake Chapala over the last 20 years. Also, metal concentrations were below those that could be of concern for negative effects on fish and wildlife of Lake Chapala.

  12. Trace elements in urban and suburban rainfall, Mersin, Northeastern Mediterranean

    NASA Astrophysics Data System (ADS)

    Özsoy, Türkan; Örnektekin, Sermin

    2009-10-01

    Spatial/temporal variabilities of rainwater constituents are examined based on soluble/insoluble trace elements, pH and electrical conductivity measurements in rainfall sampled during December 2003-May 2005 at two urban and two suburban sites in Mersin, an industrialized city of 850,000 inhabitants on the southern coast of Turkey. In the analyses, backward air mass trajectories for rainy days were used in addition to factor analyses, enrichment factors, phase distributions and correlations between trace elements. The pH varied from 4.8 to 8.5 with an average value of 6.2, reflecting a mainly alkaline regime. Mean concentrations of trace elements collected from urban and suburban sites are spatially variable. Based on the overall data, total concentrations of trace elements were ordered as Ca > Na > Fe > Al > Mg > K > Zn > Mn > Sr > Pb > Ni > Cr > Ba > Cu > Co > Cd. Mainly terrigeneous (Ca, Fe, Al) and, to a lesser extent, sea salt particles (Na, Mg) were shown to be the major source of trace elements. Excluding major cations, the solubilities of trace elements were found to be ordered as Sr > Zn > Ba > Mn > Cu > Ni > Cr > Fe > Al, confirming the lower solubility of crustal elements. Cd, Co and Pb were excluded from the above evaluation because of the low numbers of soluble samples allowing quantitative measurements. The solubilities of Al, Fe, Mn and particularly of Ni were found to be considerably lower than those reported for various sites around the world, most likely due to the effect of pH. During the entire sampling period, a total of 28 dust transport episodes associated with 31 red rain events were identified. Extremely high mean concentration ratios of Al (8.2), Fe (14.4) and Mn (13.1) were observed in red rain, compared to normal rain. The degree of this enhancement displayed a decrease from crustal to anthropogenic origin elements and the lowest enhancements were found for anthropogenic origin elements of Zn and Cd (both having a ratio of 1.1). Aerosol dust was found to be the main source of almost all analyzed elements in Mersin precipitation, regardless that they are crustal or anthropic derived elements. The magnitude of crustal source contribution to trace element budget of precipitation was at its highest levels for crustal originated elements, most probably due to much higher scavenging ratios of crustal elements compared to anthropogenic ones.

  13. Distribution and metal contamination in the coastal sediments of Dammam Al-Jubail area, Arabian Gulf, Saudi Arabia.

    PubMed

    El-Sorogy, Abdelbaset; Al-Kahtany, Khaled; Youssef, Mohamed; Al-Kahtany, Fahd; Al-Malky, Mazen

    2018-03-01

    Present work aims to document the distribution and metal contamination in the coastal sediments of the Dammam Al-Jubail area, Saudi Arabian Gulf. Twenty-six samples were collected for Al, V, Cr, Mn, Cu, Zn, Cd, Pb, Hg, Sr, As, Fe, Co and Ni analysis. Results of enrichment factor indicated that Sr, Cd, Cu, Hg, V, As, Ni, Cr and Zn gave enrichment factors higher than 2 (98.87, 40.28, 33.20, 27.87, 26.11, 14.10, 6.15, 3.72 and 2.62 respectively) implying anthropogenic sources, while Pb, Mn and Al have very low background level (1.37, 0.71, 0.124 respectively), probably originated from natural sources. Average concentrations of Sr, V, Hg, Cd and As were mostly higher than those from the background shale and the earth crust, the Caspian Sea, the Mediterranean Sea, the sediment quality guidelines, the Red Sea, the Gulf of Aqaba and the Gulf of Oman. The higher levels of the studied metals are mostly related samples with high Al and TOM content, as well as the visible anthropogenic pollutants along the studied coastline. The most recorded anthropogenic pollutants were sewage effluent, landfilling due to coastal infrastructure development, oil spills, petrochemical industries and desalination plants in Al-Jubail industrial city. Copyright © 2018 Elsevier Ltd. All rights reserved.

  14. ``Flash'' synthesis of ``giant'' Mn-doped CdS/ZnSe/ZnS nanocrystals with ZnSe layer as hole quantum-well

    NASA Astrophysics Data System (ADS)

    Xu, Ruilin; Zhang, Jiayu

    Usually, exciton-Mn energy transfer in Mn-doped CdS/ZnS nanocrystals (NCs) can readily outcompete the exciton trapping by an order of magnitude. However, with the accumulation of non-radiative defects in the giant shell during the rapid growth of the thick shell (up to ~20 monolayers in no more than 10 minutes), the photoluminescence (PL) quantum yield of this kind of ``giant'' NCs is significantly reduced by the accumulation of non-radiative defects during the rapid growth of thick shell. That is because the exciton-Mn energy transfer in Mn-doped CdS/ZnS NCs is significantly inhibited by the hole trapping as the major competing process, resulting from the insufficient hole-confinement in CdS/ZnS NCs. Accordingly ``flash'' synthesis of giant Mn-doped CdS/ZnSe/ZnS NCs with ZnSe layer as hole quantum-well is developed to suppress the inhibition. Meanwhile Mn2+ PL peak changes profoundly from ~620 nm to ~540 nm after addition of ZnSe layer. Studies are under the way to explore the relevant mechanisms.

  15. Assessment of heavy metals in agricultural soils and their source apportionment: a Turkish district survey.

    PubMed

    Dartan, Güler; Taşpınar, Fatih; Toröz, İsmail

    2015-03-01

    This study aimed at investigating the impact of industrialization on the quality of agricultural soils in the district of Bandırma, Turkey, in terms of soil heavy metal contamination. Many soil and phosphogypsum samples were analyzed, and enrichment factors (EFs) were calculated. The average concentration gradient of metals in the soil (mg/kg) was As < Se < Sb < Pb < Co < Cd < V < Cu < Ni < Zn < Cr < P < Mn < Na < K < Mg < Fe < Ca < Al. According to the Pearson cross-correlation results for the element pairs of Fe-Mg (0.635), Fe-Cu (0.863), Fe-Cd (0.545), Cu-Cd (0.630), Mn-Cr (0.698), Mn-Al (0.523), Cr-Mg (0.543), Al-P (0.508), Na-K (0.616), and C-Zn (0.703), the metal enrichments in the soil were found to be moderately high and significant. In the majority of soil samples, Ni, Cu, Co, Zn, Se, Pb, and Cr were moderately enriched whereas Sb and Cd were extremely highly enriched. A factor analysis (FA) was applied to the cross-correlations of the elements to identify their sources. Six significant factors were extracted with the help of FA, explaining 77.22 % of the total variance, and the elements loaded on these factors were interpreted. The evaluations of the factors showed that the study area has been exposed to heavy metal pollution from anthropogenic sources considering the high levels of Cr, Cd, Cu, P, V, Zn, Ni, Sb, and Pb in the soil and the higher EFs falling in the range of 2.54-372.87. Moreover, the soil concentrations of Mn, Mg, Co, Al, K, and Ca were also high, but they were of lithogenic in origin according to the FA.

  16. (Zn, Mg)2GeO4:Mn2+ submicrorods as promising green phosphors for field emission displays: hydrothermal synthesis and luminescence properties.

    PubMed

    Shang, Mengmeng; Li, Guogang; Yang, Dongmei; Kang, Xiaojiao; Peng, Chong; Cheng, Ziyong; Lin, Jun

    2011-10-07

    (Zn(1-x-y)Mg(y))(2)GeO(4): xMn(2+) (y = 0-0.30; x = 0-0.035) phosphors with uniform submicrorod morphology were synthesized through a facile hydrothermal process. X-Ray diffraction (XRD), field emission scanning electron microscopy (FE-SEM), photoluminescence (PL), and cathodoluminescence (CL) spectroscopy were utilized to characterize the samples. SEM and TEM images indicate that Zn(2)GeO(4):Mn(2+) samples consist of submicrorods with lengths around 1-2 μm and diameters around 200-250 nm, respectively. The possible formation mechanism for Zn(2)GeO(4) submicrorods has been presented. PL and CL spectroscopic characterizations show that pure Zn(2)GeO(4) sample shows a blue emission due to defects, while Zn(2)GeO(4):Mn(2+) phosphors exhibit a green emission corresponding to the characteristic transition of Mn(2+) ((4)T(1)→(6)A(1)) under the excitation of UV and low-voltage electron beam. Compared with Zn(2)GeO(4):Mn(2+) sample prepared by solid-state reaction, Zn(2)GeO(4):Mn(2+) phosphors obtained by hydrothermal process followed by high temperature annealing show better luminescence properties. In addition, codoping Mg(2+) ions into the lattice to substitute for Zn(2+) ions can enhance both the PL and CL intensity of Zn(2)GeO(4):Mn(2+) phosphors. Furthermore, Zn(2)GeO(4):Mn(2+) phosphors exhibit more saturated green emission than the commercial FEDs phosphor ZnO:Zn, and it is expected that these phosphors are promising for application in field-emission displays.

  17. Monitoring and assessment of the groundwater quality in wadi Al-Arish downstream area, North Sinai (Egypt)

    NASA Astrophysics Data System (ADS)

    Masoud, Alaa A.; Meswara, Ebtesam A.; El Bouraie, Mohamed M.; Kamh, Samir Z.

    2018-04-01

    At a rate of 3 samples a year over 7 years (2008-2014), groundwater quality indicators for 294 samples from 14 groundwater supply wells located on the delta of Wadi Al-Arish, North Sinai (Egypt) were measured and analyzed. The prime objective was to characterize significant and sustained trends in the concentrations of the pH, TDS, Total Alkalinity, Fe2+, Mn2+, Zn2+, NO3-, K+, Pb2+, Al3+, and fecal coliform (FC). Detection and estimation of trends and magnitude were carried out applying the nonparametric Mann-Kendall and Thiel-Sen trend statistical tests, respectively. Geostatistical kriging implemented in ArcGIS 10× was appraised for the spatial distribution of the indicators and their sustained trends. Factor analysis was applied to identify significant sources of quality variation and their loads. Average contents of all indicators exceeded the permissible limits except for Mn. Violation of groundwater quality standards clarified emergence of FC (99.6%), Pb2+ (76.8%), TDS (60.2%), Al3+ (56.6%), NO3- (46.5%), Fe2+ (37.5%), and Mn2+ (14%). Out of the 14 wells, notable upward trends (deterioration) were significant (>95% level) for Mg2+ (100%), TDS (78.5%), NO3- (71.42%), Zn2+ (42.85%), pH (14.28%), K+ (14.28%), and 7.14% for Al3+ and FC. Ranges of attenuation rates (mg/l/year) varied for TDS (52.61-37.59), Mg2+ hardness (3.81-0.14), K+ (0.58-1), pH (0.004-0.027), total alkalinity (-1.89-13.18), NO3- (1.47-0.69), Al3+ (0.002-0.011), Fe2+ (-0.001-0.016), Mn2+ (-0.00004-0.01), Pb2+ (-0.00001-0.002), Zn2+ (0.049-0.018), and FC (5.25-22) in cfu/100 ml. Out of the 14 wells, well no. 9 showed the largest increasing attenuation rates (mg/l/year) that marked NO3- (1.47), K+ (0.58), pH (0.004), and Al3+ (0.002). TDS showed the largest rates of increase of 52.61, and 28.26 for well nos. 5 and 9, respectively. FC showed the highest rate of deterioration of 5.25 in well no. 10. Zn2+ recorded strong deterioration rates of 0.049, and 0.046 for well nos. 12 and 9, respectively. Four factors were found to explain 60.48% of the total variance of the quality variables and in particular, a significant load of TDS, Cl-, EC, SO42-, Na+, Ca2+, Mg2+, NO3-, K+, Pb2+ and Total Alkalinity in decreasing order of influence were identified. Variation in quality parameters originated from anthropogenic sources due to improper well head protection in the urban centers or from the agricultural wastes and the flash floodwater stagnation and intense evaporation in low relief areas.

  18. Intrinsic ferromagnetism in nanocrystalline Mn-doped ZnO depending on Mn concentration.

    PubMed

    Subramanian, Munisamy; Tanemura, Masaki; Hihara, Takehiko; Soga, Tetsuo; Jimbo, Takashi

    2011-04-01

    The physical properties of Zn(1-x)Mn(x)O nanoparticles synthesized by thermal decomposition are extensively investigated by X-ray diffraction (XRD), Transmission Electron Microscopy (TEM), X-ray photoelectron spectroscopy (XPS), Raman light scattering and Hysteresis measurements. XRD and XPS spectra reveal the absence of secondary phase in nanocrystalline ZnO doped with 5% or less Mn; and, later confirms that the valance state of Mn to be 2+ for all the samples. Raman spectra exhibit a peak at 660 cm(-1) which we attribute to the intrinsic lattice defects of ZnO with increasing Mn concentration. Overall, our results demonstrate that ferromagnetic properties can be realized while Mn-doped ZnO obtained in the nanocrystalline form.

  19. UV Light-Driven Photodegradation of Methylene Blue by Using Mn0.5Zn0.5Fe2O4/SiO2 Nanocomposites

    NASA Astrophysics Data System (ADS)

    Indrayana, I. P. T.; Julian, T.; Suharyadi, E.

    2018-04-01

    The photodegradation activity of nanocomposites for 20 ppm methylene blue solution has been investigated in this work. Nanocomposites Mn0.5Zn0.5Fe2O4/SiO2 have been synthesized using coprecipitation method. The X-ray diffraction (XRD) pattern confirmed the formation of three phases in sample Mn0.5Zn0.5Fe2O4/SiO2 i.e., Mn0.5Zn0.5Fe2O4, Zn(OH)2, and SiO2. The appearance of SiO2 phase showed that the encapsulation process has been carried out. The calculated particles size of Mn0.5Zn0.5Fe2O4/SiO2 is greater than Mn0.5Zn0.5Fe2O4. Bonding analysis via vibrational spectra for Mn0.5Zn0.5Fe2O4/SiO2 confirmed the formation of bonds Me-O-Si stretching (2854.65 cm-1) and Si-O-Si asymmetric stretching (1026.13 cm-1). The optical gap energy of Mn0.5Zn0.5Fe2O4/SiO2 was smaller (2.70 eV) than Mn0.5Zn0.5Fe2O4 (3.04 eV) due to smaller lattice dislocation and microstrain that affect their electronic structure. The Mn0.5Zn0.5Fe2O4/SiO2 showed high photodegradation ability due to smaller optical gap energy and the appearance of SiO2 ligand that can easily attract dye molecules. The Mn0.5Zn0.5Fe2O4/SiO2 also showed high degradation activity even without UV light radiation. The result showed that photodegradation reaction doesn’t follow pseudo-first order kinetics.

  20. A Hollow-Structured Manganese Oxide Cathode for Stable Zn-MnO₂ Batteries.

    PubMed

    Guo, Xiaotong; Li, Jianming; Jin, Xu; Han, Yehu; Lin, Yue; Lei, Zhanwu; Wang, Shiyang; Qin, Lianjie; Jiao, Shuhong; Cao, Ruiguo

    2018-05-05

    Aqueous rechargeable zinc-manganese dioxide (Zn-MnO₂) batteries are considered as one of the most promising energy storage devices for large scale-energy storage systems due to their low cost, high safety, and environmental friendliness. However, only a few cathode materials have been demonstrated to achieve stable cycling for aqueous rechargeable Zn-MnO₂ batteries. Here, we report a new material consisting of hollow MnO₂ nanospheres, which can be used for aqueous Zn-MnO₂ batteries. The hollow MnO₂ nanospheres can achieve high specific capacity up to ~405 mAh g −1 at 0.5 C. More importantly, the hollow structure of birnessite-type MnO₂ enables long-term cycling stability for the aqueous Zn-MnO₂ batteries. The excellent performance of the hollow MnO₂ nanospheres should be due to their unique structural properties that enable the easy intercalation of zinc ions.

  1. Polycrystalline ZnO and Mn-doped ZnO nanorod arrays with variable dopant content via a template based synthesis from Zn(II) and Mn(II) Schiff base type single source molecular precursors

    NASA Astrophysics Data System (ADS)

    Pashchanka, Mikhail; Hoffmann, Rudolf C.; Burghaus, Olaf; Corzilius, Björn; Cherkashinin, Gennady; Schneider, Jörg J.

    2011-01-01

    The synthesis and full characterisation of pure and Mn-doped polycrystalline zinc oxide nanorods with tailored dopant content are obtained via a single source molecular precursor approach using two Schiff base type coordination compounds is reported. The infiltration of precursor solutions into the cylindrical pores of a polycarbonate template and their thermal conversion into a ceramic green body followed by dissolution of the template gives the desired ZnO and Mn-doped ZnO nanomaterial as compact rods. The ZnO nanorods have a mean diameter between 170 and 180 nm or 60-70 nm, depending on the template pore size employed, comprising a length of 5-6 μm. These nanorods are composed of individual sub-5 nm ZnO nanocrystals. Exact doping of these hierarchically structured ZnO nanorods was achieved by introducing Mn(II) into the ZnO host lattice with the precursor complex Diaquo-bis[2-(meth-oxyimino)-propanoato]manganese, which allows to tailor the exact Mn(II) doping content of the ZnO rods. Investigation of the Mn-doped ZnO samples by XRD, TEM, XPS, PL and EPR, reveals that manganese occurs exclusively in its oxidation state + II and is distributed within the volume as well as on the surface of the ZnO host.

  2. Bioleaching of zinc and manganese from spent Zn-Mn batteries and mechanism exploration.

    PubMed

    Xin, Baoping; Jiang, Wenfeng; Aslam, Hina; Zhang, Kai; Liu, Changhao; Wang, Renqing; Wang, Yutao

    2012-02-01

    In this work, bioleaching was used to extract valuable Zn and Mn from spent Zn-Mn batteries. The results showed that 96% of Zn extraction was achieved within 24h regardless of energy source types and bioleaching bacteria species. However, initial pH had a remarkable influence on Zn release, extraction dose sharply decreased from 2200 to 500mg/l when the initial pH value increased from 1.5 to 3.0 or higher. In contrast to Zn, all the tested factors evidently affected Mn extraction; the maximum released dose of 3020mg/l was obtained under the optimum conditions. The acidic dissolution by biogenic H(2)SO(4) by the non-contact mechanism was responsible for Zn extraction, while Mn extraction was owed to both contact/biological and non-contact mechanisms. The combined action of acidic dissolution of soluble Mn(2+) by biogenic H(2)SO(4) and reductive dissolution of insoluble Mn(4+) by Fe(2+) resulted in 60% of Mn extraction, while contact of microbial cells with the spent battery material and incubation for more than 7days was required to achieve the maximum extraction of Mn. Copyright © 2011 Elsevier Ltd. All rights reserved.

  3. Magnetically engineered Cd-free quantum dots as dual-modality probes for fluorescence/magnetic resonance imaging of tumors.

    PubMed

    Ding, Ke; Jing, Lihong; Liu, Chunyan; Hou, Yi; Gao, Mingyuan

    2014-02-01

    Magnetically engineered Cd-free CuInS2@ZnS:Mn quantum dots (QDs) were designed, synthesized, and evaluated as potential dual-modality probes for fluorescence and magnetic resonance imaging (MRI) of tumors in vivo. The synthesis of Mn-doped core-shell structured CuInS2@ZnS mainly comprised three steps, i.e., the preparation of fluorescent CuInS2 seeds, the particle surface coating of ZnS, and the Mn-doping of the ZnS shells. Systematic spectroscopy studies were carried out to illustrate the impacts of ZnS coating and the following Mn-doping on the optical properties of the QDs. In combination with conventional fluorescence, fluorescence excitation, and time-resolved fluorescence measurements, the structure of CuInS2@ZnS:Mn QDs prepared under optimized conditions presented a Zn gradient CuInS2 core and a ZnS outer shell, while Mn ions were mainly located in the ZnS shell, which well balanced the optical and magnetic properties of the resultant QDs. For the following in vivo imaging experiments, the hydrophobic CuInS2@ZnS:Mn QDs were transferred into water upon ligand exchange reactions by replacing the 1-dodecanethiol ligand with dihydrolipoic acid-poly(ethylene glycol) (DHLA-PEG) ligand. The MTT assays based on HeLa cells were carried out to evaluate the cytotoxicity of the current Cd-free CuInS2@ZnS:Mn QDs for comparing with that of water soluble CdTe QDs. Further in vivo fluorescence and MR imaging experiments suggested that the PEGylated CuInS2@ZnS:Mn QDs could well target both subcutaneous and intraperitoneal tumors in vivo. Copyright © 2013 Elsevier Ltd. All rights reserved.

  4. Apxs Chemical Composition of the Kimberley Sandstone in Gale Crater

    NASA Astrophysics Data System (ADS)

    Gellert, R.; Boyd, N.; Campbell, J. L.; VanBommel, S.; Thompson, L. M.; Schmidt, M. E.; Berger, J. A.; Clark, B. C.; Grotzinger, J. P.; Yen, A. S.; Fisk, M. R.

    2014-12-01

    Kimberley was chosen as a major waypoint of the MSL rover Curiosity on its way to Mount Sharp. APXS data before drilling showed interestingly high K, Fe and Zn. This warranted drilling of the fine-grained sandstone for detailed investigations with SAM and Chemin. With significantly lower Na, Al and higher K, Mg and Fe, the composition of the drill target Windjana is very distinct from the previous ones in the mudstones at Yellowknife Bay. Up to 2000 ppm Br and 4000 ppm Zn post-brush were among the highest measured values in Gale Crater. The excavated fines, stemming from about 6cm, showed lower Br, but even higher Zn. Preliminary Chemin results indicate K-feldspar and magnetite being major mineral phases in Windjana, which is consistent with the pre drill APXS result and derived CIPW norms. Inside the accessible work volume of the arm at the drill site ChemCam exposed a greyish, shinier patch of rock underneath the dust, dubbed Stephen. ChemCam sees a high Mn signal in most of the spots. An APXS integration revealed high MnO as well (~4%), in addition to high Mg, Cl,K,Ni,Zn,Br,Cu,Ge and for the first time an APXS detectable amount of ~300 ppm Co. The surface might reflect a thin surface layer and may underestimate the higher Z elemental concentration since the APXS analysis assumes an infinite sample. Important elemental correlations are likely not impacted. A four spot daytime raster of Stephen before leaving the drill site showed a good correlation of Mn with Zn, Cu and Ni. All spots have 3-3.5% Cl, the highest values measured on Mars so far. While the stratigraphic setting of the Stephen sample is discussed elsewhere, the similarity with Mn deep-sea nodules is striking, e.g. the APXS calibration sample GBW07296. Whatever process formed Stephen, the process of Mn scavenging high Z trace metals from solutions seems to have happened similarly at this site on Mars.

  5. Competition of the self-activated and Mn-related luminescence in ZnS single crystals

    NASA Astrophysics Data System (ADS)

    Bacherikov, Yu. Yu.; Vorona, I. P.; Markevich, I. V.; Korsunska, N. O.; Kurichka, R. V.

    2018-06-01

    The photoluminescence (PL) and photoluminescence excitation (PLE) spectra of ZnS single crystals thermally doped from ZnS/MnS mixture were studied at 300 and 77 K. PL spectra exhibit bands caused by Mn-related centers and centers of self-activated (SA) emission. Besides intrinsic maximum, a number of narrow peaks corresponded to Mn-related absorption are found in the PLE spectra of both SA and Mn-related emission. A redistribution of SA and Mn-related emission intensities is observed with temperature change. The mechanism of this phenomenon involving free hole trapping by MnZn and the possible position of a ground energy level of substitutional Mn are discussed.

  6. Processes of zinc attenuation by biogenic manganese oxides forming in the hyporheic zone of Pinal Creek, Arizona

    USGS Publications Warehouse

    Fuller, Christopher C.; Bargar, John R.

    2014-01-01

    The distribution and speciation of Zn sorbed to biogenic Mn oxides forming in the hyporheic zone of Pinal Creek, AZ, was investigated using extended X-ray absorption fine structure (EXAFS) and microfocused synchrotron X-ray fluorescence (μSXRF) mapping, and chemical extraction. μSXRF and chemical extractions show that contaminant Zn co-varied with Mn in streambed sediment grain coatings. Bulk and microfocused EXAFS spectra of Zn in the biogenic Mn oxide coating are indicative of Zn forming triple-corner-sharing inner-sphere complexes over octahedral vacancies in the Mn oxide sheet structure. Zn desorbed in response to the decrease in pH in batch experiments and resulted in near-equal dissolved Zn at each pH over a 10-fold range in the solid/solution ratio. The geometry of sorbed Zn was unchanged after 50% desorption at pH 5, indicating that desorption is not controlled by dissolution of secondary Zn phases. In summary, these findings support the idea that Zn attenuation in Pinal Creek is largely controlled by sorption to microbial Mn oxides forming in the streambed during hyporheic exchange. Sorption to biogenic Mn oxides is likely an important process of Zn attenuation in circum-neutral pH reaches of many acid-mine drainage contaminated streams when dissolved Mn is present.

  7. Magnetic phase change in Mn-doped ZnSnAs2 thin films depending on Mn concentration

    NASA Astrophysics Data System (ADS)

    Uchitomi, Naotaka; Hidaka, Shiro; Saito, Shin; Asubar, Joel T.; Toyota, Hideyuki

    2018-04-01

    The relationship between Mn concentration and Curie temperature (TC) is studied for Mn-doped ZnSnAs2 ferromagnetic semiconductors, epitaxially grown on InP substrates by molecular beam epitaxy. In the ferromagnetic phase, Mn distributions in a (Zn,Mn,Sn)As2 thin film with 7.2 cation percent (cat. %) Mn are investigated using three-dimensional atom probe tomography. The results indicate an inhomogeneous distribution which spreads to a relatively high Mn concentration of 9.0 at. % (at. %). In the paramagnetic phase, it is found that the paramagnetic to ferromagnetic transition takes place sharply with a TC of 334 K when the Mn doping concentration increases to about 4 cat. % Mn, which corresponds to a magnetic percolation threshold for ferromagnetism in (Zn,Mn,Sn)As2. An effective Curie temperature ⟨TC⟩ is considered to bridge the Curie temperatures obtained experimentally to those calculated theoretically in inhomogeneous magnetic semiconductors. The behavior of magnetism in Mn-doped ZnSnAs2 can be explained by three different phases within the present framework.

  8. A novel metallogel based approach to synthesize (Mn, Cu) doped ZnS quantum dots and labeling of MCF-7 cancer cells.

    PubMed

    Bhowal, Soumya; Ghosh, Arijit; Chowdhuri, Srijita Paul; Mondal, Raju; Das, Benu Brata

    2018-05-08

    The present study aims to formulate a common synthetic strategy for preparing quantum dots (QDs) in a greener way by using combination of popular methods, viz. a colloidal method with suitable capping agent and low molecular weight gel based synthesis. Pyridine dicarboxylic acid (PDC) in presence of AlCl3 forms a stable metallogel, which serves as an excellent medium for selective ZnS QD synthesis. The aromatic pyridine moiety, well known for being a capping agent, indeed plays its part in the run up to QD synthesis. To the best of our knowledge, this is the first example of a metallogel based doped ZnS QD synthesis. Altering the doping material and its composition changes the properties of the QDs, but herein we also tried to establish how these changes affect the gel morphology and stability of both gel and QDs. We further demonstrate, by using live cell confocal microscopy, the delivery of QDs Cu ZnS and MnZnS nanomaterials in the nucleus and the cytoplasm of human breast cancer cells (MCF7), implicating the use of metallogel based QDs for bio-imaging and bio-labeling.

  9. Ab initio Study of Transition metal binding to the Prion Protein

    NASA Astrophysics Data System (ADS)

    Cox, Daniel L.; Singh, Rajiv R. P.; Pan, Jianping

    2004-03-01

    Fundamental understanding of the prion protein (PrP) is of critical public health importance in view of mad cow and chronic wasting diseases. In recent years, it has been shown that the normal form (PrP^c) binds copper^1), and the structure of the copper binding domain has been elaborated. Hypotheses about toxicity associated with binding of other metals (notably manganese) have been put forward, Accordingly, using the ab initio SIESTA density functional theory code^2), we calculated the binding energy E_B(M) of M-(PrP) complexes relative to initially uncomplexed M ions, with M=Cu,Ni,Zn,Mn and (PrP)^* the minimal binding domain. The binding energy trend is E_B(Ni)>E_B(Cu)>E_B(Zn)>E_B(Mn), consistent with recent experiments apart from the surprising stability of Ni. We will also present preliminary results for binding of initially complexed M ions. *-Supported by U.S. DOE, Office of Basic Energy Sciences, Division of Materials Research 1) G.S. Jackson et al., Proc. Nat. Acad. Sci. (USA) 98, 8531 (2001). 2) P. Ordejón, et al., Phys. Rev. B53, R10441 (1996); J.M. Soler et al., J. Phys. Cond. Matt. 14, 2745 (2002).

  10. Distribution of rare-earth (Y, La, Ce) and other heavy metals in the profiles of the podzolic soil group

    NASA Astrophysics Data System (ADS)

    Vodyanitskii, Yu. N.; Goryachkin, S. V.; Savichev, A. T.

    2011-05-01

    Along with Fe and Al, many heavy metals (Mn, Cr, Zn, Cu, and Ni) show a markedly pronounced eluvial-illuvial redistribution in the profiles of soils of the podzolic group. The intensity of the redistribution of the bulk forms of these metals is comparable with that of Fe and exceeds that of Al. Although the podzolic soils are depleted of rare-earth metals, the latter respond readily to soil podzolization. The inactive participation of Al is explained by an insignificant portion of the active reaction-capable fraction. Podzolization does not influence the profile distribution of Sr and Ba. The leaching degree of heavy metals such as Mn, Cr, Zn, Ni, and Zr is noticeably higher in the sandy podzols than in the loamy podzolic soils. Leaching of heavy metals from the podzolic horizons is of geochemical importance, whereas the depletion of metals participating in plant nutrition and biota development is of ecological importance. The leaching of heavy metals is related to the destruction of clay particles in the heavy-textured podzolic soils; the effect of the soil acidity on the leaching of heavy metals is less significant.

  11. Toxic and essential elements in five tree nuts from Hangzhou market, China.

    PubMed

    Ni, Zhanglin; Tang, Fubin; Yu, Qing; Liu, Yihua

    2016-12-01

    In this study, a total of 35 tree nut samples of walnut, pecan, pine seed, hickory nut and torreya were obtained from 5 farm product markets in Hangzhou, China, and investigated for essential (Cr, Mn, Fe, Mo, Cu, Zn, Se and Sr) and toxic (Al, As, Cd and Pb) elements by inductively coupled plasma-mass spectroscopy. Mean elemental concentrations of different tree nuts were in the following ranges: Cr 0.26-0.78 mg kg -1 , Mn 42.1-174 mg kg -1 , Fe 33.7-43.9 mg kg -1 , Mo 0.11-0.48 mg kg -1 , Cu 10.3-17.6 mg kg -1 , Zn 21.6-56.1 mg kg -1 , Se 0.015-0.051 mg kg -1 , Al 1.44-37.6 mg kg -1 , As 0.0062-0.047 mg kg -1 , Cd 0.016-0.18 mg kg -1 and Pb 0.0069-0.029 mg kg -1 . The estimated provisional tolerable daily intake of Al, As, Cd and Pb was much lower than the provisional tolerable daily intake.

  12. Preparation of a nanosized as(2)o(3)/mn(0.5)zn(0.5)fe(2)o(4) complex and its anti-tumor effect on hepatocellular carcinoma cells.

    PubMed

    Zhang, Jia; Zhang, Dongsheng

    2009-01-01

    Manganese-zinc-ferrite nanoparticles (Mn(0.5)Zn(0.5)Fe(2)O(4), MZF-NPs) prepared by an improved co-precipitation method and were characterized by transmission electron microscopy (TEM), X-ray diffraction (XRD) and energy dispersive spectrometry (EDS). Then thermodynamic testing of various doses of MZF-NPs was performed in vitro. The cytotoxicity of the Mn(0.5)Zn(0.5)Fe(2)O(4) nanoparticles in vitro was tested by the MTT assay. A nanosized As(2)O(3)/Mn(0.5)Zn(0.5)Fe(2)O(4) complex was made by an impregnation process. The complex's shape, component, envelop rate and release rate of As(2)O(3) were measured by SEM, EDS and atom fluorescence spectrometry, respectively. The therapeutic effect of nanosized As(2)O(3)/Mn(0.5)Zn(0.5)Fe(2)O(4) complex combined with magnetic fluid hyperthermia (MFH) on human hepatocelluar cells were evaluated in vitro by an MTT assay and flow cytometry. The results indicated that Mn(0.5)Zn(0.5)Fe(2)O(4) and nanosized As(2)O(3)/Mn(0.5)Zn(0.5)Fe(2)O(4) complex were both prepared successfully. The Mn(0.5)Zn(0.5)Fe(2)O(4) nanoparticles had powerful absorption capabilities in a high-frequency alternating electromagnetic field, and had strong magnetic responsiveness. Moreover, Mn(0.5)Zn(0.5)Fe(2)O(4) didn't show cytotoxicity in vitro. The therapeutic result reveals that the nanosized As(2)O(3)/Mn(0.5)Zn(0.5)Fe(2)O(4) complex can significantly inhibit the growth of hepatoma carcinoma cells.

  13. Surface characterization of ZnO/ZnMn2O4 and Cu/Mn3O4 powders obtained by thermal degradation of heterobimetallic complexes

    NASA Astrophysics Data System (ADS)

    Barrault, Joël; Makhankova, Valeriya G.; Khavryuchenko, Oleksiy V.; Kokozay, Vladimir N.; Ayrault, Philippe

    2012-03-01

    From the selective transformation of the heterometallic (Zn-Mn or Cu-Mn) carboxylate complexes with 2,2'-bipyridyl by thermal degradation at relatively low (350 °C) temperature, it was possible to get either well defined spinel ZnMn2O4 over zinc oxide or well dispersed copper particles surrounded by a manganese oxide (Mn3O4) in a core-shell like structure. Morphology of the powder surface was examined by scanning electron microscopy with energy dispersive X-ray microanalysis (SEM/EDX). Surface composition was determined by X-ray photoelectron spectroscopy (XPS). Specific surface of the powders by nitrogen adsorption was found to be 33±0.2 and 9±0.06 m2 g-1 for Zn-Mn and Cu-Mn samples, respectively, which is comparable to those of commercial products.

  14. Detection of DNA via the fluorescence quenching of Mn-doped ZnSe D-dots/doxorubicin/DNA ternary complexes system.

    PubMed

    Gao, Xue; Niu, Lu; Su, Xingguang

    2012-01-01

    This manuscript reports a method for the detection of double-stranded DNA, based on Mn:ZnSe d-dots and intercalating agent doxorubicin (DOX). DOX can quench the photoluminescence (PL) of Mn:ZnSe d-dots through photoinduced electron transfer process, after binding with Mn:ZnSe d-dots. The addition of DNA can result in the formation of the Mn:ZnSe d-dots-DOX-DNA ternary complexes, the fluorescence of the Mn:ZnSe d-dots-DOX complexes would be further quenched by the addition of DNA, thus allowing the detection of DNA. The formation mechanism of the Mn:ZnSe d-dots-DOX-DNA ternary complexes was studied in detail in this paper. Under optimal conditions, the quenched fluorescence intensity of Mn:ZnSe d-dots-DOX system are perfectly described by Stern-Volmer equation with the concentration of hsDNA ranging from 0.006 μg mL(-1) to 6.4 μg mL(-1). The detection limit (S/N = 3) for hsDNA is 0.5 ng mL(-1). The proposed method was successfully applied to the detection of DNA in synthetic samples and the results were satisfactory.

  15. Resonantly enhanced spin-lattice relaxation of Mn2 + ions in diluted magnetic (Zn,Mn)Se/(Zn,Be)Se quantum wells

    NASA Astrophysics Data System (ADS)

    Debus, J.; Ivanov, V. Yu.; Ryabchenko, S. M.; Yakovlev, D. R.; Maksimov, A. A.; Semenov, Yu. G.; Braukmann, D.; Rautert, J.; Löw, U.; Godlewski, M.; Waag, A.; Bayer, M.

    2016-05-01

    The dynamics of spin-lattice relaxation in the magnetic Mn2 + ion system of (Zn,Mn)Se/(Zn,Be)Se quantum-well structures are studied using optical methods. Pronounced cusps are found in the giant Zeeman shift of the quantum-well exciton photoluminescence at specific magnetic fields below 10 T, when the Mn spin system is heated by photogenerated carriers. The spin-lattice relaxation time of the Mn ions is resonantly accelerated at the cusp magnetic fields. Our theoretical analysis demonstrates that a cusp occurs at a spin-level mixing of single Mn2 + ions and a quick-relaxing cluster of nearest-neighbor Mn ions, which can be described as intrinsic cross-relaxation resonance within the Mn spin system.

  16. Micro-spatial variation of elemental distribution in estuarine sediment and their accumulation in mangroves of Indian Sundarban.

    PubMed

    Bakshi, Madhurima; Ram, S S; Ghosh, Somdeep; Chakraborty, Anindita; Sudarshan, M; Chaudhuri, Punarbasu

    2017-05-01

    This work describes the micro-spatial variation of elemental distribution in estuarine sediment and bioaccumulation of those elements in different mangrove species of the Indian Sundarbans. The potential ecological risk due to such elemental load on this mangrove-dominated habitat is also discussed. The concentrations of elements in mangrove leaves and sediments were determined using energy-dispersive X-ray fluorescence spectroscopy. Sediment quality and potential ecological risks were assessed from the calculated indices. Our data reflects higher concentration of elements, e.g., Al, K, Ca, Ti, V, Cr, Mn, Fe, Ni, Cu, Zn, and Pb, in the sediment, as compared to that reported by earlier workers. Biological concentration factors for K, Ca, Mn, Fe, Cu, and Zn in different mangroves indicated gradual elemental bioaccumulation in leaf tissues (0.002-1.442). Significant variation was observed for elements, e.g., Ni, Mn, and Ca, in the sediments of all the sites, whereas in the plants, significant variation was found for P, S, Cl, K, Ca, Mn, Fe, Cu, and Zn. This was mostly due to the differences in uptake and accumulation potential of the plants. Various sediment quality indices suggested the surface sediments to be moderately contaminated and suffering from progressive deterioration. Cu, Cr, Zn, Mn, and Ni showed higher enrichment factors (0.658-1.469), contamination factors (1.02-2.7), and geo-accumulation index (0.043-0.846) values. The potential ecological risk index values considering Cu, Cr, Pb, and Zn were found to be within "low ecological risk" category (20.04-24.01). However, Cr and Ni in the Sundarban mangroves exceeded the effect range low and probable effect level limits. Strong correlation of Zn with Fe and K was observed, reflecting their similar transportation and accumulation process in both sediment and plant systems. The plant-sediment elemental correlation was found to be highly non-linear, suggesting role of some physiological and edaphic factors in the accumulation process. Overall, the study of micro-spatial distribution of elements can act as a useful tool for determining health of estuarine ecosystem.

  17. Giant spin splitting in optically active ZnMnTe/ZnMgTe core/shell nanowires.

    PubMed

    Wojnar, Piotr; Janik, Elżbieta; Baczewski, Lech T; Kret, Sławomir; Dynowska, Elżbieta; Wojciechowski, Tomasz; Suffczyński, Jan; Papierska, Joanna; Kossacki, Piotr; Karczewski, Grzegorz; Kossut, Jacek; Wojtowicz, Tomasz

    2012-07-11

    An enhancement of the Zeeman splitting as a result of the incorporation of paramagnetic Mn ions in ZnMnTe/ZnMgTe core/shell nanowires is reported. The studied structures are grown by gold-catalyst assisted molecular beam epitaxy. The near band edge emission of these structures, conspicuously absent in the case of uncoated ZnMnTe nanowires, is activated by the presence of ZnMgTe coating. Giant Zeeman splitting of this emission is studied in ensembles of nanowires with various average Mn concentrations of the order of a few percent, as well as in individual nanowires. Thus, we show convincingly that a strong spin sp-d coupling is indeed present in these structures.

  18. Contaminants in surface water and sediments near the Tynagh silver mine site, County Galway, Ireland.

    PubMed

    O'Neill, A; Phillips, D H; Bowen, J; Sen Gupta, B

    2015-04-15

    A former silver mine in Tynagh, Co. Galway, Ireland is one of the most contaminated mine sites in Europe with maximum concentrations of Zn, As, Pb, Mn, Ni, Cu, and Cd far exceeding guideline values for water and sediment. The aims of this research were to 1) further assess the contamination, particularly metals, in surface water and sediment around the site, and 2) determine if the contamination has increased 10 years after the Environmental Protection Agency Ireland (EPAI) identified off-site contamination. Site pH is alkaline to neutral because CaCO3-rich sediment and rock material buffer the exposed acid generating sulphide-rich ore. When this study was compared to the previous EPAI study conducted 10 years earlier, it appeared that further weathering of exposed surface sediment had increased concentrations of As and other potentially toxic elements. Water samples from the tailings ponds and adjacent Barnacullia Stream had concentrations of Al, Cd, Mn, Zn and Pb above guideline values. Lead and Zn concentrations from the tailings pond sediment were 16 and 5 times higher, respectively, than concentrations reported 10 years earlier. Pb and Zn levels in most sediment samples exceeded the Expert Group (EGS) guidelines of 1000 and 5000 mg/kg, respectively. Arsenic concentrations were as high as 6238 mg/kg in the tailings ponds sediment, which is 62 and 862 times greater than the EGS and Canadian Soil Quality Guidelines (CSQG), respectively. Cadmium, Cu, Fe, Mn, Pb and Zn concentrations in water and sediment were above guideline values downstream of the site. Additionally, Fe, Mn and organic matter (OM) were strongly correlated and correlated to Zn, Pb, As, Cd, Cu and Ni in stream sediment. Therefore, the nearby Barnacullia Stream is also a significant pathway for contaminant transport to downstream areas. Further rehabilitation of the site may decrease the contamination around the area. Copyright © 2015 Elsevier B.V. All rights reserved.

  19. On the state of Mn in Mn{sub x}Zn{sub 1−x}O nanoparticles and their surface modification with isonipecotic acid

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Jiménez-Hernández, L.; Estévez-Hernández, O.; Instituto de Ciencia y Tecnología de Materiales

    Mn-doped ZnO (Mn{sub x}Zn{sub 1−x}O) nanoparticles were synthesized by the co-precipitation method and coated with isonipecotic acid as capping ligand. The structure, composition and morphology of the resulting nanomaterial were investigated by energy disperse X-ray analysis, X-ray diffraction, and transmission electron microscopy data. Such measurements showed that the solid obtained contains 6 at% of Mn and it is formed by a highly crystalline material with 3–5 nm range of crystallite size, and only a small elongation of its cell parameter with respect to undoped ZnO wurtzite unit cell. Information on the state of manganese atom in the Mn{sub x}Zn{sub 1−x}Omore » nanostructures formed was obtained from X-ray photoelectron (XPS) and electron energy loss (EELS) spectroscopies. XPS and EELS spectra are composed of four peaks, corresponding to two species of Mn(II) and signals from Mn(III) and Mn(IV). Such spectral data on the state of Mn in the material studied is consistent with the mapping of Mn distribution observed in recorded transmission electron microscopy images, which reveal presence of clusters of Mn atoms. Only a fraction of doping Mn atoms were found forming a solid solution with the host ZnO structure. The functionalization of the nanoparticles system with Isonipecotic acid shows that this molecule remains anchored to the nanoparticles surface mainly through its N basic site. The availability of free carboxylate groups in the capping molecule was tested by conjugation to type IV horseradish peroxidase. - Graphical abstract: State of Mn atoms in Mn-doped ZnO nanostructures prepared by the precipitation method, their capping with isonipecotic acid and subsequent conjugation to peroxidase. - Highlights: • State of manganese in manganese-doped zinc oxide nanoparticles. • Isonipecotic acid as surface modifier of ZnO nanoparticles. • Peroxidase conjugation to ZnO nanoparticles modified with isonipecotic acid.« less

  20. Processes of zinc attenuation by biogenic manganese oxides forming in the hyporheic zone of Pinal Creek, Arizona

    PubMed Central

    Fuller, Christopher C.; Bargar, John R.

    2014-01-01

    The distribution and speciation of Zn sorbed to biogenic Mn oxides forming in the hyporheic zone of Pinal Creek, AZ, was investigated using micro-focused Extended X-ray Absorption Fine Structure (EXAFS) and X-ray fluorescence (μSXRF) mapping , bulk EXAFS, and chemical extraction. μSXRF and chemical extractions show that contaminant Zn co-varied with Mn in streambed sediment grain coatings. Bulk and micro-focused EXAFS spectra of Zn in the biogenic Mn oxides coating are indicative of Zn forming triple corner sharing inner-sphere complexes over octahedral vacancies in the Mn oxide sheet structure. Zn desorbed in response to decreasing in pH in batch experiments and resulted in near-equal dissolved Zn at each pH over a 10-fold range in solid to solution ratio. The geometry of sorbed Zn was unchanged after 50% desorption at pH 5, indicating desorption is not controlled by dissolution of secondary Zn phases. In sum, these findings support the idea that Zn attenuation in Pinal Creek is largely controlled by sorption to microbial Mn oxides forming in the streambed during hyporheic exchange. Sorption to biogenic Mn oxides is likely an important process in Zn attenuation in circum-neutral pH reaches of many acid-mine drainage contaminated streams when dissolved Mn is present. PMID:24460038

  1. Out-of-plane easy-axis in thin films of diluted magnetic semiconductor Ba1-xKx(Zn1-yMny)2As2

    NASA Astrophysics Data System (ADS)

    Wang, R.; Huang, Z. X.; Zhao, G. Q.; Yu, S.; Deng, Z.; Jin, C. Q.; Jia, Q. J.; Chen, Y.; Yang, T. Y.; Jiang, X. M.; Cao, L. X.

    2017-04-01

    Single-phased, single-oriented thin films of Mn-doped ZnAs-based diluted magnetic semiconductor (DMS) Ba1-xKx(Zn1-yMny)2As2 (x = 0.03, 0.08; y = 0.15) have been deposited on Si, SrTiO3, LaAlO3, (La,Sr)(Al,Ta)O3, and MgAl2O4 substrates, respectively. Utilizing a combined synthesis and characterization system excluding the air and further optimizing the deposition parameters, high-quality thin films could be obtained and be measured showing that they can keep inactive-in-air up to more than 90 hours characterized by electrical transport measurements. In comparison with films of x = 0.03 which possess relatively higher resistivity, weaker magnetic performances, and larger energy gap, thin films of x = 0.08 show better electrical and magnetic performances. Strong magnetic anisotropy was found in films of x = 0.08 grown on (La,Sr)(Al,Ta)O3 substrate with their magnetic polarization aligned almost solely on the film growth direction.

  2. Metal transport and remobilisation in a basin affected by acid mine drainage: the role of ochreous amorphous precipitates.

    PubMed

    Consani, Sirio; Carbone, Cristina; Dinelli, Enrico; Balić-Žunić, Tonci; Cutroneo, Laura; Capello, Marco; Salviulo, Gabriella; Lucchetti, Gabriella

    2017-06-01

    Metal-polluted mine waters represent a major threat to the quality of waters and sediments in a downstream basin. At the confluence between acidic mine waters and the unpolluted waters of the Gromolo Torrent (Liguria, North-West Italy), the massive formation of an ochreous amorphous precipitate takes place. This precipitate forms a soft blanket that covers the torrent bed and can be observed down to its mouth in the sea. The aim of this work is to evaluate the dispersion of metals in the Gromolo Torrent basin from the abandoned Cu-Fe sulphide mine of Libiola to the Ligurian Sea and to assess the metal remobilisation from the amorphous precipitates. The mineralogy of the superficial sediments collected in the torrent bed and the concentrations of different elements of environmental concern (Cu, Zn, Cd, Co, Cr, Mn, Ni, Pb, As, and Sb) were therefore analysed. The results showed that the precipitates contain high concentration of Fe, Al, Cu, and Zn, significantly modifying the bulk chemistry of the Gromolo Torrent sediments. In order to evaluate the possible remobilisation of ecotoxic elements from the amorphous precipitates, bulk leaching tests were performed with both deionised and seawater. Bulk leaching tests with deionised water mobilised primarily high Pb amounts, but also relatively high concentrations of Fe, Al, Cu, and Zn are released in the leachate. In seawater tests, Fe, Al, Cu, and Zn were released in smaller amounts, while other elements like Mn, Cd, Co, and Ni increased in the released fraction. Pb was still strongly released as in deionised water experiments. The results show that the interaction of precipitates and seawater can remobilise high concentrations of metals, thus affecting the surrounding environment.

  3. Effect of 50 MeV Li3+ irradiation on structural and electrical properties of Mn-doped ZnO.

    PubMed

    Neogi, S K; Chattopadhyay, S; Banerjee, Aritra; Bandyopadhyay, S; Sarkar, A; Kumar, Ravi

    2011-05-25

    The present work aims to study the effect of ion irradiation on structural and electrical properties and their correlation with the defects in the Zn(1 - x)Mn(x)O-type system. Zn(1 - x)Mn(x)O (x = 0.02, 0.04) samples have been synthesized by the solid-state reaction method and have been irradiated with 50 MeV Li(3+) ions. The concomitant changes have been probed by x-ray diffraction (XRD), temperature-dependent electrical resistivity and positron annihilation lifetime (PAL) spectroscopy. The XRD result shows a single-phase wurtzite structure for Zn(0.98)Mn(0.02)O, whereas for the Zn(0.96)Mn(0.04)O sample an impurity phase has been found, apart from the usual peaks of ZnO. Ion irradiation removes this impurity peak. The grain size of the samples is found to be uniform. For Zn(0.98)Mn(0.02)O, the observed sharp decrease in room temperature resistivity (ρ(RT)) with irradiation is consistent with the lowering of the full width at half maximum of the XRD peaks. However, for Zn(0.96)Mn(0.04)O, ρ(RT) decreases for the initial fluence but increases for a further increase in fluence. All the irradiated Zn(0.98)Mn(0.02)O samples show a metal-semiconductor transition in temperature-dependent resistivity measurements at low temperature. But all the irradiated Zn(0.96)Mn(0.04)O samples show a semiconducting nature in the whole range of temperatures. Results of room temperature resistivity, XRD and PAL measurements are consistent with each other.

  4. Synthesis and characterization of Mn-ZnFe2O4 and Mn-ZnFe2O4/rGO nanocomposites from waste batteries for photocatalytic, electrochemical and thermal studies

    NASA Astrophysics Data System (ADS)

    Mylarappa, M.; Venkata Lakshmi, V.; Vishnu Mahesh, K. R.; Nagaswarupa, H. P.; Raghavendra, N.

    2017-11-01

    In the present paper, Mn-ZnFe2O4 and Mn-ZnFe2O4/rGO composites recovered from waste batteries using acid dissolution and ferrite processing were studied. The recovered Mn-ZnFe2O4 nanocomposites were decorated onto rGO using the facile hydrothermal method. The recovered material was characterized using x-ray powder diffraction to study the particle size and crystallinity. The morphology of the composites was analyzed using scanning electron microscopy, and elements present in the materials were studied using energy dispersive x-ray analysis. The functional groups attached were observed using a Fourier transform infrared spectrometer. Furthermore, the recovered composites were evaluated in thermal studies using thermal gravimetric analysis, differential scanning calorimetry and dynamic thermal analysis. The material was used as a photocatalyst for the removal of acid orange 88 dye, and as an electrocatalyst. The decreased band gap energy for the Mn-ZnFe2O4/rGO composite was displayed in better photocatalytic activity for a given reaction. The electrochemical properties of Mn-ZnFe2O4 and Mn-ZnFe2O4/rGO have been investigated using cyclic voltammetry (CV) and electrochemical impedance spectroscopy (EIS) with a paste-type electrode. The CV indicated the reversibility of the electrode reaction, and the EIS revealed that a decrease in the charge transfer resistance increases the double layer capacitance of the rGO/Mn-ZnFe2O4 electrode.

  5. Narrowing the gap: from semiconductor to semimetal in the homologous series of rare-earth zinc arsenides RE(2-y)Zn4As4·n(REAs) and Mn-substituted derivatives RE(2-y)Mn(x)Zn(4-x)As4·n(REAs) (RE = La-Nd, Sm, Gd).

    PubMed

    Lin, Xinsong; Tabassum, Danisa; Mar, Arthur

    2015-12-14

    A homologous series of ternary rare-earth zinc arsenides, prepared by reactions of the elements at 750 °C, has been identified with the formula RE(2-y)Zn4As4·n(REAs) (n = 2, 3, 4) for various RE members. They adopt trigonal structures: RE(4-y)Zn4As6 (RE = La-Nd), space group R3̄m1, Z = 3; RE(5-y)Zn4As7 (RE = Pr, Nd, Sm, Gd), space group P3̄m1, Z = 1; RE(6-y)Zn4As8 (RE = La-Nd, Sm, Gd), space group R3̄m1, Z = 3. The Zn atoms can be partially substituted by Mn atoms, resulting in quaternary derivatives RE(2-y)Mn(x)Zn(4-x)As4·n(REAs). Single-crystal structures were determined for nine ternary and quaternary arsenides RE(2-y)M4As4·n(REAs) (M = Mn, Zn) as representative examples of these series. The structures are built by stacking close-packed nets of As atoms, sometimes in very long sequences, with RE atoms occupying octahedral sites and M atoms occupying tetrahedral sites, resulting in an intergrowth of [REAs] and [M2As2] slabs. The recurring feature of all members of the homologous series is a sandwich of [M2As2]-[REAs]-[M2As2] slabs, while rocksalt-type blocks of [REAs] increase in thickness between these sandwiches with higher n. Similar to the previously known related homologous series REM(2-x)As2·n(REAs) which is deficient in M, this new series RE(2-y)M4As4·n(REAs) exhibits deficiencies in RE to reduce the electron excess that would be present in the fully stoichiometric formulas. Enthalpic and entropic factors are considered to account for the differences in site deficiencies in these two homologous series. Band structure calculations indicate that the semiconducting behaviour of the parent n = 0 member (with CaAl2Si2-type structure) gradually evolves, through a narrowing of the gap between valence and conduction bands, to semimetallic behaviour as the number of [REAs] blocks increases, to the limit of n = ∞ for rocksalt-type REAs.

  6. Improved photovoltaic performance and stability of quantum dot sensitized solar cells using Mn-ZnSe shell structure with enhanced light absorption and recombination control.

    PubMed

    Gopi, Chandu V V M; Venkata-Haritha, M; Kim, Soo-Kyoung; Kim, Hee-Je

    2015-08-07

    To make quantum-dot-sensitized solar cells (QDSSCs) competitive, photovoltaic parameters comparable to those of other emerging solar cell technologies are necessary. In the present study, ZnSe was used as an alternative to ZnS, one of the most widely used passivation materials in QDSSCs. ZnSe was deposited on a TiO2-CdS-CdSe photoanode to form a core-shell structure, which was more efficient in terms of reducing the electron recombination in QDSSCs. The development of an efficient passivation layer is a requirement for preventing recombination processes in order to attain high-performance and stable QDSSCs. A layer of inorganic Mn-ZnSe was applied to a QD-sensitized photoanode to enhance the adsorption and strongly inhibit interfacial recombination processes in QDSSCs, which greatly improved the power conversion efficiency. Impedance spectroscopy revealed that the combined Mn doping with ZnSe treatment reduces interfacial recombination and increases charge collection efficiency compared with Mn-ZnS, ZnS, and ZnSe. A solar cell based on the CdS-CdSe-Mn-ZnSe photoanode yielded excellent performance with a solar power conversion efficiency of 5.67%, Voc of 0.584 V, and Jsc of 17.59 mA cm(-2). Enhanced electron transport and reduced electron recombination are responsible for the improved Jsc and Voc of the QDSSCs. The effective electron lifetime of the device with Mn-ZnSe was higher than those with Mn-ZnS, ZnSe, and ZnS, leading to more efficient electron-hole separation and slower electron recombination.

  7. Switchable Schottky diode characteristics induced by electroforming process in Mn-doped ZnO thin films

    NASA Astrophysics Data System (ADS)

    Nam, Yoonseung; Hwang, Inrok; Oh, Sungtaek; Lee, Sangik; Lee, Keundong; Hong, Sahwan; Kim, Jinsoo; Choi, Taekjib; Ho Park, Bae

    2013-04-01

    We investigated the asymmetric current-voltage (I-V) characteristics and accompanying unipolar resistive switching of pure ZnO and Mn(1%)-doped ZnO (Mn:ZnO) films sandwiched between Pt electrodes. After electroforming, a high resistance state of the Mn:ZnO capacitor revealed switchable diode characteristics whose forward direction was determined by the polarity of the electroforming voltage. Linear fitting of the I-V curves highlighted that the rectifying behavior was influenced by a Schottky barrier at the Pt/Mn:ZnO interface. Our results suggest that formation of conducting filaments from the cathode during the electroforming process resulted in a collapse of the Schottky barrier (near the cathode), and rectifying behaviors dominated by a remnant Schottky barrier near the anode.

  8. Periodic table of 3d-metal dimers and their ions.

    PubMed

    Gutsev, G L; Mochena, M D; Jena, P; Bauschlicher, C W; Partridge, H

    2004-10-08

    The ground states of the mixed 3d-metal dimers TiV, TiCr, TiMn, TiFe, TiCo, TiNi, TiCu, TiZn, VCr, VMn, VFe, VCo, VNi, VCu, VZn, CrMn, CrFe, CrCo, CrNi, CrCu, CrZn, MnFe, MnCo, MnNi, MnCu, MnZn, FeCo, FeNi, FeCu, FeZn, CoNi, CoCu, CoZn, NiCu, NiZn, and CuZn along with their singly negatively and positively charged ions are assigned based on the results of computations using density functional theory with generalized gradient approximation for the exchange-correlation functional. Except for TiCo and CrMn, our assignment agrees with experiment. Computed spectroscopic constants (r(e),omega(e),D(o)) are in fair agreement with experiment. The ground-state spin multiplicities of all the ions are found to differ from the spin multiplicities of the corresponding neutral parents by +/-1. Except for TiV, MnFe, and MnCu, the number of unpaired electrons, N, in a neutral ground-state dimer is either N(1)+N(2) or mid R:N(1)-N(2)mid R:, where N(1) and N(2) are the numbers of unpaired 3d electrons in the 3d(n)4s(1) occupation of the constituent atoms. Combining the present and previous results obtained at the same level of theory for homonuclear 3d-metal and ScX (X=Ti-Zn) dimers allows one to construct "periodic" tables of all 3d-metal dimers along with their singly charged ions.

  9. Application of multivariate statistical analysis in the pollution and health risk of traffic-related heavy metals.

    PubMed

    Ebqa'ai, Mohammad; Ibrahim, Bashar

    2017-12-01

    This study aims to analyse the heavy metal pollutants in Jeddah, the second largest city in the Gulf Cooperation Council with a population exceeding 3.5 million, and many vehicles. Ninety-eight street dust samples were collected seasonally from the six major roads as well as the Jeddah Beach, and subsequently digested using modified Leeds Public Analyst method. The heavy metals (Fe, Zn, Mn, Cu, Cd, and Pb) were extracted from the ash using methyl isobutyl ketone as solvent extraction and eventually analysed by atomic absorption spectroscopy. Multivariate statistical techniques, principal component analysis (PCA), and hierarchical cluster analysis were applied to these data. Heavy metal concentrations were ranked according to the following descending order: Fe > Zn > Mn > Cu > Pb > Cd. In order to study the pollution and health risk from these heavy metals as well as estimating their effect on the environment, pollution indices, integrated pollution index, enrichment factor, daily dose average, hazard quotient, and hazard index were all analysed. The PCA showed high levels of Zn, Fe, and Cd in Al Kurnish road, while these elements were consistently detected on King Abdulaziz and Al Madina roads. The study indicates that high levels of Zn and Pb pollution were recorded for major roads in Jeddah. Six out of seven roads had high pollution indices. This study is the first step towards further investigations into current health problems in Jeddah, such as anaemia and asthma.

  10. Volatilization, transport and sublimation of metallic and non-metallic elements in high temperature gases at Merapi Volcano, Indonesia

    USGS Publications Warehouse

    Symonds, R.B.; Rose, William I.; Reed, M.H.; Lichte, F.E.; Finnegan, David L.

    1987-01-01

    Condensates, silica tube sublimates and incrustations were sampled from 500-800??C fumaroles and lava samples were collected at Merapi Volcano, Indonesia in Jan.-Feb., 1984. With respect to the magma, Merapi gases are enriched by factors greater than 105 in Se, Re, Bi and Cd; 104-105 in Au, Br, In, Pb and W; 103-104 in Mo, Cl, Cs, S, Sn and Ag; 102-103 in As, Zn, F and Rb; and 1-102 in Cu, K, Na, Sb, Ni, Ga, V, Fe, Mn and Li. The fumaroles are transporting more than 106 grams/day ( g d) of S, Cl and F; 104-106 g/d of Al, Br, Zn, Fe, K and Mg; 103-104 g d of Pb, As, Mo, Mn, V, W and Sr; and less than 103 g d of Ni, Cu, Cr, Ga, Sb, Bi, Cd, Li, Co and U. With decreasing temperature (800-500??C) there were five sublimate zones found in silica tubes: 1) cristobalite and magnetite (first deposition of Si, Fe and Al); 2) K-Ca sulfate, acmite, halite, sylvite and pyrite (maximum deposition of Cl, Na, K, Si, S, Fe, Mo, Br, Al, Rb, Cs, Mn, W, P, Ca, Re, Ag, Au and Co); 3) aphthitalite (K-Na sulfate), sphalerite, galena and Cs-K. sulfate (maximum deposition of Zn, Bi, Cd, Se and In; higher deposition of Pb and Sn); 4) Pb-K chloride and Na-K-Fe sulfate (maximum deposition of Pb, Sn and Cu); and 5) Zn, Cu and K-Pb sulfates (maximum deposition of Pb, Sn, Ti, As and Sb). The incrustations surrounding the fumaroles are also chemically zoned. Bi, Cd, Pb, W, Mo, Zn, Cu, K, Na, V, Fe and Mn are concentrated most in or very close to the vent as expected with cooling, atmospheric contamination and dispersion. The highly volatile elements Br, Cl, As and Sb are transported primarily away from high temperature vents. Ba, Si, P, Al, Ca and Cr are derived from wall rock reactions. Incomplete degassing of shallow magma at 915??C is the origin of most of the elements in the Merapi volcanic gas, although it is partly contaminated by particles or wall rock reactions. The metals are transported predominantly as chloride species. As the gas cools in the fumarolic environment, it becomes saturated with sublimate phases that fractionate from the gas in the order of their equilibrium saturation temperatures. Devolatilization of a cooling batholith could transport enough acids and metals to a hydrothermal system to play a significant role in forming an ore deposit. However, sublimation from a high temperature, high velocity carrier gas is not efficient enough to form a large ore deposit. Re, Se, Cd and Bi could be used as supporting evidence for magmatic fluid transport in an ore deposit. ?? 1987.

  11. Sulfide and Oxide Heterostructures For the SrTiO3 Thin Film Growth on Si and Their Structural and Interfacial Stabilities

    NASA Astrophysics Data System (ADS)

    Yoo, Young‑Zo; Song, Jeong‑Hwan; Konishi, Yoshinori; Kawasaki, Masashi; Koinuma, Hideomi; Chikyow, Toyohiro

    2006-03-01

    Epitaxial SrTiO3 (STO) thin films with high electrical properties were grown on Si using ZnS single- and SrS/MnS hetero-buffer layers. STO films on both ZnS-buffered and SrS/MnS-buffered Si showed two growth orientations, (100) and (110). The temperature dependence of the growth orientation for STO films was different for the ZnS single-buffer layer in comparison with the SrS/MnS heterobuffer layers. (100) growth of STO films on SrS/MnS-buffered Si became dominant at high temperatures about 700 °C, while (100) growth of STO films on ZnS-buffered Si became dominant at a relatively low growth temperature of 550 °C. STO(100) films on ZnS-buffered and SrS/MnS-buffered Si showed lattice and domain matches for epitaxial relationships with [001]ZnS\\parallel[011]STO and SrS[001]\\parallel[011]STO, respectively via 45° in-plane rotation of STO films relative to both ZnS and SrS layers. The ZnS buffer layer contained many stacking faults because of the mismatch between ZnS and Si, however, those defects were terminated at the ZnS/STO interface. In contrast, the MnS buffer was very stable against stacking defect formation. Transmission electron microscopy measurements revealed the presence of a disordered region at the ZnS/Si and MnS/Si interfaces. Auger electron spectroscopy and transmission electron microscopy results showed that a good MnS/Si interface at the initial growth stage degraded to a SiS2-x-rich phase during MnS deposition and again into a SiO2-x-rich phase during STO deposition at the high growth temperature of 700 °C. It was also observed that STO on SrS/MnS-buffered Si showed a markedly high dielectric constant compared with that of STO on ZnS-buffered Si.

  12. LABORATORY EVALUATION OF ZERO-VALENT IRON TO TREAT WATER IMPACTED BY ACID MINE DRAINAGE

    EPA Science Inventory

    This study examines the applicability and limitations of granular zero-valent iron for the treatment of water impacted by mine wastes. Rates of acid neutralization and of metal (Cu, Cd, Ni, Zn, Hg, Al, and Mn) and metalloid (As) uptake were determined in batch systems using simu...

  13. Mineral Analysis of Pine Nuts (Pinus spp.) Grown in New Zealand

    PubMed Central

    Vanhanen, Leo P.; Savage, Geoffrey P.

    2013-01-01

    Mineral analysis of seven Pinus species grown in different regions of New Zealand; Armand pine (Pinus armandii Franch), Swiss stone pine (Pinus cembra L.), Mexican pinyon (Pinus cembroides Zucc. var. bicolor Little), Coulter pine (Pinus coulteri D. Don), Johann’s pine (Pinus johannis M.F. Robert), Italian stone pine (Pinus pinea L.) and Torrey pine (Pinus torreyana Parry ex Carrière), was carried out using an inductively coupled plasma optical emission spectrophotometer (ICP-OES) analysis. Fourteen different minerals (Al, B, Ca, Cr, Cu, Fe, K, Mg, Mn, Na, Ni, P, S and Zn) were identified in all seven varieties, except that no Al or Na was found in Pinus coulteri D. Don. New Zealand grown pine nuts are a good source of Cu, Mg, Mn, P and Zn, meeting or exceeding the recommended RDI for these minerals (based on an intake of 50 g nuts/day) while they supplied between 39%–89% of the New Zealand RDI for Fe. Compared to other commonly eaten tree-nuts New Zealand grown pine nuts are an excellent source of essential minerals. PMID:28239104

  14. Mineral Analysis of Pine Nuts (Pinus spp.) Grown in New Zealand.

    PubMed

    Vanhanen, Leo P; Savage, Geoffrey P

    2013-04-03

    Mineral analysis of seven Pinus species grown in different regions of New Zealand; Armand pine ( Pinus armandii Franch), Swiss stone pine ( Pinus cembra L.), Mexican pinyon ( Pinus cembroides Zucc. var. bicolor Little), Coulter pine ( Pinus coulteri D. Don), Johann's pine ( Pinus johannis M.F. Robert), Italian stone pine ( Pinus pinea L.) and Torrey pine ( Pinus torreyana Parry ex Carrière), was carried out using an inductively coupled plasma optical emission spectrophotometer (ICP-OES) analysis. Fourteen different minerals (Al, B, Ca, Cr, Cu, Fe, K, Mg, Mn, Na, Ni, P, S and Zn) were identified in all seven varieties, except that no Al or Na was found in Pinus coulteri D. Don. New Zealand grown pine nuts are a good source of Cu, Mg, Mn, P and Zn, meeting or exceeding the recommended RDI for these minerals (based on an intake of 50 g nuts/day) while they supplied between 39%-89% of the New Zealand RDI for Fe. Compared to other commonly eaten tree-nuts New Zealand grown pine nuts are an excellent source of essential minerals.

  15. Anode materials for lithium ion batteries

    DOEpatents

    Abouimrane, Ali; Amine, Khalil

    2017-04-11

    An electrochemical device includes a composite material of general Formula (1-x)J-(x)Q wherein: J is a metal carbon alloy of formula Sn.sub.zSi.sub.z'Met.sub.wMet'.sub.w'C.sub.t; Q is a metal oxide of formula A.sub..gamma.M.sub..alpha.M'.sub..alpha.'O.sub..beta.; and wherein: A is Li, Na, or K; M and M' are individually Ge, Mo, Al, Ga, As, Sb, Te, Ti, Ta, Zr, Ca, Mg, Sr, Ba, Li, Na, K, V, Cr, Mn, Fe, Co, Ni, Cu, Zn, Nb, Rt, Ru or Cd; Met and Met' are individually Ge, Mo, Al, Ga, As, Sb, Te, Ti, Ta, Zr, Ca, Mg, Sr, Ba, Li, Na, K, V, Cr, Mn, Fe, Co, Ni, Cu, Zn, Nb, Rt, Ru or Cd; 0

  16. The effects of copper, manganese and zinc on plant growth and elemental accumulation in the manganese-hyperaccumulator Phytolacca americana.

    PubMed

    Zhao, Huijun; Wu, Liangqi; Chai, Tuanyao; Zhang, Yuxiu; Tan, Jinjuan; Ma, Shengwen

    2012-09-01

    Synchrotron radiation X-ray fluorescence (SRXRF) and inductively coupled plasma mass spectrometry were used to estimate major, minor and trace elements in Cu-, Zn- and Mn-treated Phytolacca americana. The effects of the addition of Cu, Zn and Mn on morphological parameters, such as root length, shoot height, and fresh and dry weights of shoots and roots, were also examined. In addition, the activities of superoxide dismutase (SOD), ascorbate peroxidase (APX), guaiacol peroxidases (GPX) and catalase (CAT) and the expression of Fe-SOD, Cu/Zn-SOD, metallothionein-2 and glutathione S-transferase (GST) exposed to the highest amounts of Cu, Zn or Mn were detected. Our results confirmed the following: (1) Zn supplementation leads to chlorosis, disturbed elemental homeostasis and decreased concentrations of micro- and macroelements such as Fe, Mg, Mn, Ca and K. Cu competed with Fe, Mn and Zn uptake in plants supplemented with 25 μM Cu. However, no antagonistic interactions took place between Cu, Zn, Mn and Fe uptake in plants supplemented with 100 μM Cu. Mn supplementation at various concentrations had no negative effects on elemental deficits. Mn was co-located with high concentrations of Fe and Zn in mature leaves and the concentrations of macro elements were unchanged. (2) P. americana supplemented with increased concentrations of Zn and Cu exhibited lower biomass production and reduced plant growth. (3) When plants were supplemented with the highest Zn and Cu concentrations, symptoms of toxicity corresponded to decreased SOD or CAT activities and increased APX and GPX activities. However, Mn tolerance corresponded to increased SOD and CAT activities and decreased POD and APX activities. Our study revealed that heavy metals partially exert toxicity by disturbing the nutrient balance and modifying enzyme activities that induce damage in plants. However, P. americana has evolved hyper accumulating mechanisms to maintain elemental balance and redox homeostasis under excess Mn. Copyright © 2012 Elsevier GmbH. All rights reserved.

  17. Heavy metals and metalloids in the surface sediments of the Xiangjiang River, Hunan, China: distribution, contamination, and ecological risk assessment.

    PubMed

    Chai, Liyuan; Li, Huan; Yang, Zhihui; Min, Xiaobo; Liao, Qi; Liu, Yi; Men, Shuhui; Yan, Yanan; Xu, Jixin

    2017-01-01

    Here, we aim to determine the distribution, ecological risk and sources of heavy metals and metalloids in the surface sediments of the Xiangjiang River, Hunan Province, China. Sixty-four surface sediment samples were collected in 16 sites of the Xiangjiang River, and the concentrations of ten heavy metals and metalloids (Mn, Zn, Cr, V, Pb, Cu, As, Ni, Co, and Cd) in the sediment samples were investigated using an inductively coupled plasma mass spectrometer (ICP-MS) and an atomic fluorescence spectrophotometer (AFS), respectively. The results showed that the mean concentrations of the ten heavy metals and metalloids in the sediment samples followed the order Mn > Zn > Cr > V > Pb > Cu > As ≈ Ni >Co > Cd. The geoaccumulation index (I geo ), enrichment factor (EF), modified degree of contamination (mC d ), and potential ecological risk index (RI) revealed that Cd, followed by Pb, Zn, and Cu, caused severely contaminated and posed very highly potential ecological risk in the Xiangjiang River, especially in Shuikoushan of Hengyang, Xiawan of Zhuzhou, and Yijiawan of Xiangtan. The Pearson's correlation coefficient (PCC) analysis, principal component analysis (PCA), and hierarchical cluster analysis (HCA) indicated that the ten heavy metals and metalloids in the sampling sediments of the Xiangjiang River were classified into three groups: (1) Cd, Pb, Zn, and Cu which possibly originated from Shuikoushan, Xiawan, and Yijiawan clustering Pb-Zn mining and smelting industries; (2) Co, V, Ni, Cr, and Al from natural resources; and (3) Mn and As. Therefore, our results suggest that anthropogenic activities, especially mining and smelting, have caused severe contamination of Cd, Pb, Zn, and Cu and posed very high potential ecological risk in the Xiangjiang River.

  18. Performance of Zn-Fe-Mn/MCM-48 sorbents for high temperature H2S removal and analysis of regeneration process

    NASA Astrophysics Data System (ADS)

    Huang, Z. B.; Liu, B. S.; Wang, F.; Amin, R.

    2015-10-01

    MCM-48 was synthesized using a rapid and facile process at room temperature. A series of 50%Zn-Fe-Mn/MCM-48 sorbents were prepared and their performance of hot coal gas desulfurization was investigated. High breakthrough sulfur capacity (13.2 g-S/100 g sorbent) and utilization (66.1%) of 50%1Zn2Fe2Mn/MCM-48 sorbent at 550 °C was achieved. The characterization results of XRD, BET, TPR and FT-IR revealed that MCM-48 had excellent thermal stability at less than 700 °C, ZnMn2O4 and (Mn, Zn)Fe2O4 were mainly active particles in fresh sorbents which were highly dispersed on support. The MCM-48 mesoporous structure remained intact after eight successive desulfurization/regeneration cycles. The regeneration process of 50%1Zn2Fe2Mn/MCM-48 sorbent was analyzed, it indicated that the breakthrough sulfur capacity decline of sorbent was due to the migration of Zn onto the sorbent surface and Zn accumulated on the surface and vaporized to the exterior from the surface. In the TPO test, the oxidation of Zn was different for 50%Zn/MCM-48 at 700 °C. It revealed that the temperature of regeneration for ZnO sorbent should be higher than 700 °C.

  19. Metals geochemistry and mass export from the Mississippi-Atchafalaya River system to the Northern Gulf of Mexico.

    PubMed

    Reiman, Jeremy H; Xu, Y Jun; He, Songjie; DelDuco, Emily M

    2018-08-01

    Discharging 680 km 3 of freshwater annually to the Northern Gulf of Mexico (NGOM), the Mississippi-Atchafalaya River System (MARS) plays a significant role in transporting major and trace elements to the ocean. In this study, we analyzed total recoverable concentrations of thirty-one metals from water samples collected at five locations along the MARS during 2013-2016 to quantify their seasonal mass exports. The Atchafalaya River flows through a large swamp floodplain, allowing us to also test the hypothesis that floodplains function as a sink for metals. We found that the seven major elements (Ca, Na, Mg, Si, K, Al, and Fe) constituted 99% of the total annual mass load of metals (7.38 × 10 7 tons) from the MARS. Higher concentrations of Al, Ba, B, Ca, Fe, Mg, Mn, Ag, and Ti were found in the Mississippi River, while significantly higher Si and Na concentrations were found in the Atchafalaya River. Significant relationships were found between daily discharge and daily loads of Ba, Ca, Fe, K, Sr, and Ti in both rivers, while significant relationships were also found for Al, Mg, Mn, V, and Zn in the Atchafalaya River and B in the Mississippi River. Overall, the Mississippi River contributed 64-76% of the total annual loading of metals from the MARS to the NGOM. Daily loads of Al, Ba, B, Fe, Li, Mn, P, K, Si, Ag, Ti, V, and Zn regularly decreased upstream to downstream in the Atchafalaya River, partially accepting the initial hypothesis on metals transport in river floodplains. Copyright © 2018 Elsevier Ltd. All rights reserved.

  20. Ferromagnetism induced by oxygen-vacancy complex in (Mn, in) codoped ZnO

    NASA Astrophysics Data System (ADS)

    Wu, Kongping; Gu, Shulin; Tang, Kun; Zhu, Shunming; Zhou, Mengran; Huang, Yourui; Xu, Mingxiang; Zhang, Rong; Zheng, Youdou

    2012-07-01

    Mn doped Zinc oxide (ZnO) thin films were prepared by metal organic chemical vapor deposition (MOCVD) technique. Structural characterizations by X-ray diffraction technique (XRD) and photoluminescence (PL) indicate the crystal quality of ZnO films. PL and Raman show a large fraction of oxygen vacancies (VO2+) are generated by vacuum annealed the film. The enhancement of ferromagnetism in post-annealed (Mn, In) codoped ZnO could result from VO2+ incorporation. The effect of VO2+ on the magnetic properties of (Mn, In) codoped ZnO has been studied by first-principles calculations. It is found that only In donor cannot induce ferromagnetism (FM) in Mn-doped ZnO. Besides, the presence of VO2+ makes the Mn empty 3d-t2g minority state broadened, and a t2g-VO2+ hybrid level at the conduction band minimum forms. The presence of VO2+ can lead to strong ferromagnetic coupling with the nearest neighboring Mn cation by BMP model based on defects reveal that the ferromagnetic exchange is mediated by the donor impurity state, which mainly consists of Mn 3d electrons trapped in oxygen vacancies.

  1. Study of the preparation of NI-Mn-Zn ferrite using spent NI-MH and alkaline Zn-Mn batteries

    NASA Astrophysics Data System (ADS)

    Xi, Guoxi; Xi, Yuebin; Xu, Huidao; Wang, Lu

    2016-01-01

    Magnetic nanoparticles of Ni-Mn-Zn ferrite have been prepared by a sol-gel method making use of spent Ni-MH and Zn-Mn batteries as source materials. Characterization by X-ray diffraction was carried out to study the particle size. The presence of functional groups was identified by Fourier transform infrared spectroscopy. From studies by thermogravimetry and differential scanning calorimetry, crystallization occurred at temperatures above 560 °C. The magnetic properties of the final products were found to be directly influenced by the average particle size of the product. The Ms values increase and the Hc values decrease as the size of the Ni-Mn-Zn ferrite particles increases.

  2. Mn distribution in natural sphalerites: a micronalytical and EPR study

    NASA Astrophysics Data System (ADS)

    di Benedetto, F.; Bernardini, G. P.; Cipriani, C.; Plant, D.; Romanelli, M.; Vaughan, D. J.

    2003-04-01

    Electron Paramagnetic Resonance (EPR) has been successfully applied to determine the local coordination and distribution of transition metal cations in sulphides and sulphosalts (Di Benedetto et al., 2002). Due to its enhanced sensitivity and element-specificity it is one of the best tools to monitor Mn(II) behaviour down to very low concentrations. In order to reach a fuller understanding of the spectroscopic results, a microanalytical study has also been undertaken by means of Electron Microprobe Analysis. Operating conditions were chosen to achieve the lowest possible detection limits, taking into account that Mn can replace Zn in the sphalerite lattice both as a minor and trace element, and that EPR can detect Mn(II) below the ppm range. Six natural samples from the Museo di Storia Naturale, Università di Firenze, were selected to have pure single crystals and avoid magnetically active phases associated with the sphalerite. The Mn concentration determined ranges between 30 and 14300 ppm and Mn content varies considerably within the same sample, leading to differences up to the 50% as compared to the mean value. X-ray images confirm Mn to be distributed with an unusual pattern, unrelated to the other common Zn-replacing cations, Fe and Cd, present in the samples. Powder EPR spectra reveal at least three different Mn(II) signals: two sextets, overlapping in all samples containing Mn as trace element, and a single line, present only in the more concentrated samples. While the latter have been attributed to an inhomogeneous Mn distribution, due to an enhanced Mn-Mn superexchange interaction, the difference between the two sextets, observed by means of EEPR investigations in a synthetic sphalerite (Di Benedetto et al., 2002), appears unrelated to the Mn concentration and may be attributed to small differences in the local coordination of Mn(II) ions. This, in turn, may be explained by the segregation of small amounts of Mn into polytypic domains, features which usually characterise large sphalerite crystals. This study shows the distinctive behaviour of Mn in sphalerite, both at the micron and submicron scales. These features point to sphalerites "preserving" the out-of-equilibrium conditions of their genesis. Mn(II) magnetic interactions may play an important role in the stabilisation of polytypic hexagonal domains during the growth of sphalerite crystals. Di Benedetto, F., Bernardini, G.P., Caneschi, A., Cipriani, C., Danti, C., Pardi, L. and Romanelli, M. (2002): EPR and magnetic investigations on sulfides and sulfosalts. Eur. J. Mineral., 4(6), 1053.

  3. Fatigue Behavior of Long and Short Cracks in Wrought and Powder Aluminum Alloys.

    DTIC Science & Technology

    1984-05-01

    PROGRAM ELEMENT. PROJECT. TASK AREA & WORK UNIT NUMBERS Robert 0. Ritchie, Department of Materials Science and Mineral Engineering, University of 2306/ Al ...Chemical Compositions in wt% of Alloys Si Fe Cu Mn Mg Cr Zn Ti Zr Al 2024 0.50 0.50 4.50 0.50 1.50 0.10 0.25 0.15 -- balance 2124 0.20 0.30 4.50 0.50 1.50...been applied by Suresh et al .41 to rationalize the microstructural effects of precipitation hardening on fatigue crack growth in 7075 alloys. The

  4. One-step fabrication of biocompatible chitosan-coated ZnS and ZnS:Mn2+ quantum dots via a γ-radiation route

    NASA Astrophysics Data System (ADS)

    Chang, Shu-Quan; Kang, Bin; Dai, Yao-Dong; Zhang, Hong-Xu; Chen, Da

    2011-11-01

    Biocompatible chitosan-coated ZnS quantum dots [CS-ZnS QDs] and chitosan-coated ZnS:Mn2+ quantum dots [CS-ZnS:Mn2+ QDs] were successfully fabricated via a convenient one-step γ-radiation route. The as-obtained QDs were around 5 nm in diameter with excellent water-solubility. These QDs emitting strong visible blue or orange light under UV excitation were successfully used as labels for PANC-1 cells. The cell experiments revealed that CS-ZnS and CS-ZnS:Mn2+ QDs showed low cytotoxicity and good biocompatibility, which offered possibilities for further biomedical applications. Moreover, this convenient synthesis strategy could be extended to fabricate other nanoparticles coated with chitosan. PACS: 81.07.Ta; 78.67.Hc; 82.35.Np; 87.85.Rs.

  5. Exposure assessment models for elemental components of particulate matter in an urban environment: A comparison of regression and random forest approaches

    NASA Astrophysics Data System (ADS)

    Brokamp, Cole; Jandarov, Roman; Rao, M. B.; LeMasters, Grace; Ryan, Patrick

    2017-02-01

    Exposure assessment for elemental components of particulate matter (PM) using land use modeling is a complex problem due to the high spatial and temporal variations in pollutant concentrations at the local scale. Land use regression (LUR) models may fail to capture complex interactions and non-linear relationships between pollutant concentrations and land use variables. The increasing availability of big spatial data and machine learning methods present an opportunity for improvement in PM exposure assessment models. In this manuscript, our objective was to develop a novel land use random forest (LURF) model and compare its accuracy and precision to a LUR model for elemental components of PM in the urban city of Cincinnati, Ohio. PM smaller than 2.5 μm (PM2.5) and eleven elemental components were measured at 24 sampling stations from the Cincinnati Childhood Allergy and Air Pollution Study (CCAAPS). Over 50 different predictors associated with transportation, physical features, community socioeconomic characteristics, greenspace, land cover, and emission point sources were used to construct LUR and LURF models. Cross validation was used to quantify and compare model performance. LURF and LUR models were created for aluminum (Al), copper (Cu), iron (Fe), potassium (K), manganese (Mn), nickel (Ni), lead (Pb), sulfur (S), silicon (Si), vanadium (V), zinc (Zn), and total PM2.5 in the CCAAPS study area. LURF utilized a more diverse and greater number of predictors than LUR and LURF models for Al, K, Mn, Pb, Si, Zn, TRAP, and PM2.5 all showed a decrease in fractional predictive error of at least 5% compared to their LUR models. LURF models for Al, Cu, Fe, K, Mn, Pb, Si, Zn, TRAP, and PM2.5 all had a cross validated fractional predictive error less than 30%. Furthermore, LUR models showed a differential exposure assessment bias and had a higher prediction error variance. Random forest and other machine learning methods may provide more accurate exposure assessment.

  6. Exposure assessment models for elemental components of particulate matter in an urban environment: A comparison of regression and random forest approaches.

    PubMed

    Brokamp, Cole; Jandarov, Roman; Rao, M B; LeMasters, Grace; Ryan, Patrick

    2017-02-01

    Exposure assessment for elemental components of particulate matter (PM) using land use modeling is a complex problem due to the high spatial and temporal variations in pollutant concentrations at the local scale. Land use regression (LUR) models may fail to capture complex interactions and non-linear relationships between pollutant concentrations and land use variables. The increasing availability of big spatial data and machine learning methods present an opportunity for improvement in PM exposure assessment models. In this manuscript, our objective was to develop a novel land use random forest (LURF) model and compare its accuracy and precision to a LUR model for elemental components of PM in the urban city of Cincinnati, Ohio. PM smaller than 2.5 μm (PM2.5) and eleven elemental components were measured at 24 sampling stations from the Cincinnati Childhood Allergy and Air Pollution Study (CCAAPS). Over 50 different predictors associated with transportation, physical features, community socioeconomic characteristics, greenspace, land cover, and emission point sources were used to construct LUR and LURF models. Cross validation was used to quantify and compare model performance. LURF and LUR models were created for aluminum (Al), copper (Cu), iron (Fe), potassium (K), manganese (Mn), nickel (Ni), lead (Pb), sulfur (S), silicon (Si), vanadium (V), zinc (Zn), and total PM2.5 in the CCAAPS study area. LURF utilized a more diverse and greater number of predictors than LUR and LURF models for Al, K, Mn, Pb, Si, Zn, TRAP, and PM2.5 all showed a decrease in fractional predictive error of at least 5% compared to their LUR models. LURF models for Al, Cu, Fe, K, Mn, Pb, Si, Zn, TRAP, and PM2.5 all had a cross validated fractional predictive error less than 30%. Furthermore, LUR models showed a differential exposure assessment bias and had a higher prediction error variance. Random forest and other machine learning methods may provide more accurate exposure assessment.

  7. Exposure assessment models for elemental components of particulate matter in an urban environment: A comparison of regression and random forest approaches

    PubMed Central

    Brokamp, Cole; Jandarov, Roman; Rao, M.B.; LeMasters, Grace; Ryan, Patrick

    2017-01-01

    Exposure assessment for elemental components of particulate matter (PM) using land use modeling is a complex problem due to the high spatial and temporal variations in pollutant concentrations at the local scale. Land use regression (LUR) models may fail to capture complex interactions and non-linear relationships between pollutant concentrations and land use variables. The increasing availability of big spatial data and machine learning methods present an opportunity for improvement in PM exposure assessment models. In this manuscript, our objective was to develop a novel land use random forest (LURF) model and compare its accuracy and precision to a LUR model for elemental components of PM in the urban city of Cincinnati, Ohio. PM smaller than 2.5 μm (PM2.5) and eleven elemental components were measured at 24 sampling stations from the Cincinnati Childhood Allergy and Air Pollution Study (CCAAPS). Over 50 different predictors associated with transportation, physical features, community socioeconomic characteristics, greenspace, land cover, and emission point sources were used to construct LUR and LURF models. Cross validation was used to quantify and compare model performance. LURF and LUR models were created for aluminum (Al), copper (Cu), iron (Fe), potassium (K), manganese (Mn), nickel (Ni), lead (Pb), sulfur (S), silicon (Si), vanadium (V), zinc (Zn), and total PM2.5 in the CCAAPS study area. LURF utilized a more diverse and greater number of predictors than LUR and LURF models for Al, K, Mn, Pb, Si, Zn, TRAP, and PM2.5 all showed a decrease in fractional predictive error of at least 5% compared to their LUR models. LURF models for Al, Cu, Fe, K, Mn, Pb, Si, Zn, TRAP, and PM2.5 all had a cross validated fractional predictive error less than 30%. Furthermore, LUR models showed a differential exposure assessment bias and had a higher prediction error variance. Random forest and other machine learning methods may provide more accurate exposure assessment. PMID:28959135

  8. Hydrothermal synthesis of Mn-doped ZnCo2O4 electrode material for high-performance supercapacitor

    NASA Astrophysics Data System (ADS)

    Mary, A. Juliet Christina; Bose, A. Chandra

    2017-12-01

    Mn-doped ZnCo2O4 nanoparticle has been synthesized by hydrothermal method without adding any surfactants. Structural, morphological and electrochemical performances have been studied for the pure and various concentration of Mn-doped ZnCo2O4 nanoparticles. XRD and Raman studies demonstrate the crystalline structure of the material. Specific capacitance of the 10 wt% Mn doped ZnCo2O4 nanomaterial is analysed using the three-electrode system. 10 wt% Mn-doped ZnCo2O4 has a maximum capacitance of 707.4 F g-1 at a current density of 0.5 A g-1. Coulombic efficiency of the material is 96.3% for 500 cycles in the KOH electrolyte medium. A two-electrode device using 10 wt% Mn-doped ZnCo2O4 exhibits the highest specific capacitance of 6.5 F g-1 at a current density of 0.03 A g-1 which is the suitable material for supercapacitor application.

  9. Raman spectroscopy of ZnMnO thin films grown by pulsed laser deposition

    NASA Astrophysics Data System (ADS)

    Orozco, S.; Riascos, H.; Duque, S.

    2016-02-01

    ZnMnO thin films were grown by Pulsed Laser Deposition (PLD) technique onto Silicon (100) substrates at different growth conditions. Thin films were deposited varying Mn concentration, substrate temperature and oxygen pressure. ZnMnO samples were analysed by using Raman Spectroscopy that shows a red shift for all vibration modes. Raman spectra revealed that nanostructure of thin films was the same of ZnO bulk, wurzite hexagonal structure. The structural disorder was manifested in the line width and shape variations of E2(high) and E2(low) modes located in 99 and 434cm-1 respectively, which may be due to the incorporation of Mn ions inside the ZnO crystal lattice. Around 570cm-1 was found a peak associated to E1(LO) vibration mode of ZnO. 272cm-1 suggest intrinsic host lattice defects. Additional mode centred at about 520cm-1 can be overlap of Si and Mn modes.

  10. The enhancement of heavy metal removal from polluted river water treatment by integrated carbon-aluminium electrodes using electrochemical method

    NASA Astrophysics Data System (ADS)

    Yussuf, N. M.; Embong, Z.; Abdullah, S.; Masirin, M. I. M.; Tajudin, S. A. A.; Ahmad, S.; Sahari, S. K.; Anuar, A. A.; Maxwell, O.

    2018-01-01

    The heavy metal removal enhancement from polluted river water was investigated using two types of electrodes consist of integrated carbon-aluminium and a conventional aluminium plate electrode at laboratory-scale experiments. In the integrated electrode systems, the aluminium electrode surface was coated with carbon using mixed slurry containing carbon black, polyvinyl acetate and methanol. The electrochemical treatment was conducted on the parameter condition of 90V applied voltage, 3cm of electrode distance and 60 minutes of electrolysis operational time. Surface of both electrodes was investigated for pre and post electrolysis treatment by using SEM-EDX analytical technique. Comparison between both of the electrode configuration exhibits that more metals were accumulated on carbon integrated electrode surfaces for both anode and cathode, and more heavy metals were detected on the cathode. The atomic percentage of metals distributed on the cathode conventional electrode surface consist of Al (94.62%), Zn (1.19%), Mn (0.73%), Fe (2.81%) and Cu (0.64%), while on the anode contained O (12.08%), Al (87.63%) and Zn (0.29%). Meanwhile, cathode surface of integrated electrode was accumulated with more metals; O (75.40%), Al (21.06%), Zn (0.45%), Mn (0.22), Fe (0.29%), Cu (0.84%), Pb (0.47%), Na (0.94%), Cr (0.08%), Ni (0.02%) and Ag (0.22%), while on anode contain Al (3.48%), Fe (0.49 %), C (95.77%), and Pb (0.26%). According to this experiment, it was found that integrated carbon-aluminium electrodes have a great potential to accumulate more heavy metal species from polluted water compare to the conventional aluminium electrode. Here, heavy metal accumulation process obviously very significant on the cathode surface.

  11. Discriminating between pyroxenite and peridotite sources for continental flood basalts (CFB) in southern Africa using olivine chemistry

    NASA Astrophysics Data System (ADS)

    Howarth, Geoffrey H.; Harris, Chris

    2017-10-01

    Continental Flood Basalts (CFB) result from voluminous outpourings of magma that often precede continental break-up. Notwithstanding the petrogenetic importance of CFBs, the nature of the mantle source for such magmas is contentious, particularly with regard to picrites with Ni-rich olivine phenocrysts. Previous studies have suggested that Ni-rich olivines associated with plume volcanism in regions of thickened (>90 km) lithosphere are related to either source mineralogy differences (peridotite versus pyroxenite) or change in olivine-melt partitioning due to pressure increase. In order to evaluate these two hypotheses, we present trace element data for olivines from the Karoo CFB Tuli and Mwenezi picrites and the Etendeka CFB Horingbaai/LTZ-L type picrites, all of which erupted in regions of thickened (>90 km) lithosphere in southern Africa. Karoo picrite olivines are Ni-rich, Ca- and Mn-poor, and have low (<1.4) 100*Mn/Fe. These compositions are consistent with a pyroxenitic source. Etendeka Horingbaai/LTZ-L picrite olivines do not show Ni-enrichment, but are characterized by high Al and Cr, and high (>1.4) 100*Mn/Fe, which is more consistent with high temperature melting of a dominantly peridotitic source. We also show that the Karoo and Etendeka olivines are characterized by distinct Mn/Zn ratios of <13 and >15, respectively. In addition, bulk rock geochemical data compilations and previously reported olivine δ18O for Karoo and Etendeka CFBs are discussed in order to further constrain source components based on previously described pyroxenite melt geochemical indices such as MgO-CaO systematics, FeO/MnO, Zn/Fe, and FC3MS (FeO/CaO-3*MgO/SiO2). These geochemical indices suggest a pyroxenite-dominated source for Karoo CFBs as well as for Etendeka ferropicrites whereas a peridotite-dominated source is indicated for Etendeka Horingbaai/LTZ-L type picrites analyzed in this study. Based on our data, Ni-enrichment of olivine in plume-related magmas in regions of thickened lithosphere in southern Africa is not ubiquitous. We therefore suggest that mineralogical variation of the source is a more likely major control of olivine chemistry and parent melt variations for Karoo and Etendeka CFBs. We also show that olivine Mn-Zn correlations are a useful discriminator for source variation and recommend the use of olivine Mn /Zn < 13 for a pyroxenite-dominated source relative to olivine Mn /Zn > 15 for a peridotite-dominated source.

  12. Concentration and emission sources of airborne metals in particulate matter in the industrial district of Médio Paraíba, state of Rio de Janeiro, Brazil.

    PubMed

    Loyola, Josiane; de Almeida, Pierre Batista; Quiterio, Simone Lorena; Sousa, Célia Regina; Arbilla, Graciela; Escaleira, Viviane; de Carvalho, Maria Isabel; dos Santos Amaral Gomes da Silva, Alzira

    2006-11-01

    Total suspended particles and 12 airborne metals were determined in 4 sampling sites in the industrial region of Médio Paraíba, Brazil. The geometrical means for the four sampling locals were (in units of microg/m3): 65.9 in Barra Mansa, 57.3 in Jardim Paraíba (Volta Redonda), 41.7 in Resende, and 48.9 in Volta Grande (Volta Redonda). These values are lower than levels previously determined in urban and industrial locals of the Metropolitan Area of Rio de Janeiro. For metals, the higher concentrations were obtained for Ca, Zn, Al, Fe, and Mg. Ca, Zn, and Al levels are higher than those determined in other industrial areas. These three metals are used in steel manufacturing, the main economical activity of the region. Enrichment factors for Zn, Cu, Cd, and Pb are higher than 10, suggesting an industrial input. Statistical analysis show a high correlation among Ca, Mg, Zn, Cr, Al, Mn, and Fe, all of them used as raw materials in steel manufacturing and/or accumulated as industrial blast furnace slag and steelworks slag.

  13. Assessment of metal contamination in coastal sediments of Al-Khobar area, Arabian Gulf, Saudi Arabia

    NASA Astrophysics Data System (ADS)

    Alharbi, Talal; El-Sorogy, Abdelbaset

    2017-05-01

    An assessment of marine pollution due to heavy metals was made to coastal sediments collected from Al-Khobar coastline, in the Arabian Gulf, Saudi Arabia by analyzing of Al, V, Cr, Mn, Cu, Zn, Cd, Pb, Hg, Mo, Sr, Se, As, Fe, Co and Ni using Inductively Coupled Plasma-Mass Spectrometer (ICP-MS). The results indicated that the distribution of most metals was largely controlled by inputs of terrigenous material and most strongly associated with distribution of Al in sediments. In general Sr, Cr, Zn, Cu, V, Hg, Mo and Se show severe enrichment factors. Average values of Cu and Hg highly exceed the ERL and the Canadian ISQG values. Average Ni was higher than the ERL and the ERM values. The severe enrichment of some metals in the studied sediment could be partially attributed to anthropogenic activities, notably oil spills from exploration, transportation and from saline water desalination plants in Al-Khobar coast, and other industrial activities in the region.

  14. Achieving Ultrahigh Energy Density and Long Durability in a Flexible Rechargeable Quasi-Solid-State Zn-MnO2 Battery.

    PubMed

    Zeng, Yinxiang; Zhang, Xiyue; Meng, Yue; Yu, Minghao; Yi, Jianan; Wu, Yiqiang; Lu, Xihong; Tong, Yexiang

    2017-07-01

    Advanced flexible batteries with high energy density and long cycle life are an important research target. Herein, the first paradigm of a high-performance and stable flexible rechargeable quasi-solid-state Zn-MnO 2 battery is constructed by engineering MnO 2 electrodes and gel electrolyte. Benefiting from a poly(3,4-ethylenedioxythiophene) (PEDOT) buffer layer and a Mn 2+ -based neutral electrolyte, the fabricated Zn-MnO 2 @PEDOT battery presents a remarkable capacity of 366.6 mA h g -1 and good cycling performance (83.7% after 300 cycles) in aqueous electrolyte. More importantly, when using PVA/ZnCl 2 /MnSO 4 gel as electrolyte, the as-fabricated quasi-solid-state Zn-MnO 2 @PEDOT battery remains highly rechargeable, maintaining more than 77.7% of its initial capacity and nearly 100% Coulombic efficiency after 300 cycles. Moreover, this flexible quasi-solid-state Zn-MnO 2 battery achieves an admirable energy density of 504.9 W h kg -1 (33.95 mW h cm -3 ), together with a peak power density of 8.6 kW kg -1 , substantially higher than most recently reported flexible energy-storage devices. With the merits of impressive energy density and durability, this highly flexible rechargeable Zn-MnO 2 battery opens new opportunities for powering portable and wearable electronics. © 2017 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.

  15. Mechanism of γ-irradiation induced phase transformations in nanocrystalline Mn{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4} ceramics

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Jagadeesha Angadi, V.; Anupama, A.V.; Choudhary, Harish K.

    The structural, infrared absorption and magnetic property transformations in nanocrystalline Mn{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4} samples irradiated with different doses (0, 15, 25 and 50 kGy) of γ-irradiation were investigated in this work and a mechanism of phase transformation/decomposition is provided based on the metastable nature of the Mn-atoms in the spinel lattice. The nano-powder sample was prepared by solution combustion route and the pellets of the sample were exposed to γ-radiation. Up to a dose of 25 kGy of γ-radiation, the sample retained the single phase cubic spinel (Fd-3m) structure, but the disorder in the sample increased. On irradiatingmore » the sample with 50 kGy γ-radiation, the spinel phase decomposed into new stable phases such as α-Fe{sub 2}O{sub 3} and ZnFe{sub 2}O{sub 4} phases along with amorphous MnO phase, leading to a change in the surface morphology of the sample. Along with the structural transformations the magnetic properties deteriorated due to breakage of the ferrimagnetic order with higher doses of γ-irradiation. Our results are important for the understanding of the stability, durability and performance of the Mn-Zn ferrite based devices used in space applications. - Graphical abstract: The nanocrystalline Mn{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4} ceramic sample transforms to crystalline α-Fe{sub 2}O{sub 3} and ZnFe{sub 2}O{sub 4} phases (and amorphous MnO phase) at a γ-irradiation dose of 50 kGy, as MnO goes out of the spinel lattice. The high energy γ-irradiation causes structural damage to the nanomaterials leading to change in morphology of the sample as seen in the SEM images. - Highlights: • Mn atoms are more unstable in the Mn-Zn ferrite spinel lattice than Zn-atoms. • Displacement of Mn atoms by γ-radiation from the lattice renders phase transformation. • In Mn{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4}, Mn-ferrite cell transforms to crystalline α-Fe{sub 2}O{sub 3} and amorphous MnO. • The stable ZnFe{sub 2}O{sub 4} phase retains its structure even after 50 KGy γ-irradiation. • The γ-irradiation degrades the magnetic properties of Mn{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4} ceramics.« less

  16. Mn-based ferromagnetic semiconductors

    NASA Astrophysics Data System (ADS)

    Dietl, Tomasz; Sawicki, Maciej

    2003-07-01

    The present status of research and prospects for device applications of ferromagnetic (diluted magnetic) semiconductors (DMS) is presented. We review the nature of the electronic states and the mechanisms of the carrier-mediated exchange interactions (mean-field Zener model) in p-type Mn-based III-V and II-VI compounds, highlighting a good correspondence of experimental findings and theoretical predictions. An account of the latest progress on the road of increasing the Currie point to above the room temperature is given for both families of compounds. We comment on a possibility of obtaining ferromagnetism in n-type materials, taking (Zn,Mn)O:Al as the example. Concerning technologically important issue of easy axis and domain engineering, we present theoretical predictions and experimental results on the temperature and carrier concentration driven change of magnetic anisotropy in (Ga,Mn)As.

  17. Hydrothermal synthesis and magnetic properties of Mn doped ZnS nanoparticles

    NASA Astrophysics Data System (ADS)

    Rashad, M. M.; Rayan, D. A.; El-Barawy, K.

    2010-01-01

    Nanocrystallite Mn doped Zn1-XS (X = 0 to 0.4) powders have been synthesized through a hydrothermal route. The effect of the hydrothermal temperature and Mn2+ ions substitution on the crystal structure, crystallite size, microstructure and magnetic properties were investigated using (XRD), (SEM) and (VSM). The results revealed that wurtzite zinc sulfide phase was formed using thiourea as a sulfur source at temperature 150- 200oC for 24 h. The crystallite size was (7.9-15.1 nm) was obtained at the same conditions. The doping of Mn2+ ions decreased the crystallite size of the formed ZnS wurtzite phase was in the range between 7.9 and 3.8 nm. SEM micrographs showed that the produced ZnS and Mn doped ZnS particles were appeared as spherical shape. The magnetic properties were improved by substitution of Mn2+ ions up to 0.2.

  18. The salen based chemosensors for highly selective recognition of Zn2+ ion.

    PubMed

    Zhu, Wenkai; Du, LongChao; Li, Wensheng; Zuo, Jinyan; Shan, Jingrui

    2018-06-03

    Two novel salen based chemosensors have been successfully synthesized. UV-vis absorption, fluorescence emission spectroscopy and cyclic voltammetry (CV) were exploited to investigate their recognition toward various metal ions, including Na + , K + , Mg 2+ , Al 3+ , Zn 2+ , Ag + , Pb 2+ , Co 2+ , Li + , Ba 2+ , Ca 2+ , Cd 2+ , La 3+ , Cu 2+ and Mn 2+ ions. The results indicated that the sensor L1 and L2 exhibited highly selective and sensitive recognition for Zn 2+ ions. The binding stoichiometry ratio of L1-Zn 2+ /L2-Zn 2+ were recognized as 4:1 by the method of Job's plot. Meanwhile, this investigation is confirmed by 1 H NMR. These results indicated that L1 and L2 can be applied as chemosensor for the detection of Zn 2+ ion. Copyright © 2018 Elsevier B.V. All rights reserved.

  19. Biocompatible ZnS:Mn quantum dots for reactive oxygen generation and detection in aqueous media

    NASA Astrophysics Data System (ADS)

    Diaz-Diestra, Daysi; Beltran-Huarac, Juan; Bracho-Rincon, Dina P.; González-Feliciano, José A.; González, Carlos I.; Weiner, Brad R.; Morell, Gerardo

    2015-12-01

    We report here the versatility of Mn-doped ZnS quantum dots (ZnS:Mn QDs) synthesized in aqueous medium for generating reactive oxygen species and for detecting cells. Our experiments provide evidence leading to the elimination of Cd-based cores in CdSe/ZnS systems by substitution of Mn-doped ZnS. Advanced electron microscopy, X-ray diffraction, and optical spectroscopy were applied to elucidate the formation, morphology, and dispersion of the products. We study for the first time the ability of ZnS:Mn QDs to act as immobilizing agents for Tyrosinase (Tyr) enzyme. It was found that ZnS:Mn QDs show no deactivation of Tyr enzyme, which efficiently catalyzed the hydrogen peroxide (H2O2) oxidation and its eventual reduction (-0.063 V vs. Ag/AgCl) on the biosensor surface. The biosensor showed a linear response in the range of 12 μmol/L-0.1 mmol/L at low operation potential. Our observations are explained in terms of a catalase-cycled kinetic mechanism based on the binding of H2O2 to the axial position of one of the active copper sites of the oxy-Tyr during the catalase cycle to produce deoxy-Tyr. A singlet oxygen quantum yield of 0.62 in buffer and 0.54 in water was found when ZnS:Mn QDs were employed as a photosensitizer in the presence of a chemical scavenger and a standard dye. These results are consistent with a chemical trapping energy transfer mechanism. Our results also indicate that ZnS:Mn QDs are well tolerated by HeLa Cells reaching cell viabilities as high as 88 % at 300 µg/mL of QDs for 24 h of incubation. The ability of ZnS:Mn QDs as luminescent nanoprobes for bioimaging is also discussed.

  20. Mn-doping-induced photocatalytic activity enhancement of ZnO nanorods prepared on glass substrates

    NASA Astrophysics Data System (ADS)

    Putri, Nur Ajrina; Fauzia, Vivi; Iwan, S.; Roza, Liszulfah; Umar, Akrajas Ali; Budi, Setia

    2018-05-01

    Mn-doped ZnO nanorods were synthesized on glass substrates via a two-steps process of ultrasonic spray pyrolysis and hydrothermal methods with four different concentrations Mn-doping (0, 1, 3, and 7 mol%). Introduction of Mn into ZnO is known could enhance the photocatalytic activity owing to the increase in the defect sites that effectively suppress the recombination of free electrons and holes. In this study, results show that Mn-doping has effectively modified the nucleations and crystal growth of ZnO, as evidenced by the increasing in the diameter, height, and the number of nanorods per unit area, besides slightly reduced the band gap and increased the oxygen vacancy concentrations in the ZnO lattice. This condition has successfully multiplied the photocatalytic performance of the ZnO nanorods in the degradation of methylene blue (MB) compared to the undoped-ZnO sample where in the typical process the MB can be degraded approximately 77% within only 35 min under a UV light irradiation.

  1. Distribution and Potential Toxicity of Trace Metals in the Surface Sediments of Sundarban Mangrove Ecosystem, Bangladesh

    NASA Astrophysics Data System (ADS)

    Kumar, A.; Ramanathan, A.; Mathukumalli, B. K. P.; Datta, D. K.

    2014-12-01

    The distribution, enrichment and ecotoxocity potential of Bangladesh part of Sundarban mangrove was investigated for eight trace metals (As, Cd, Cr, Cu, Fe, Mn, Pb and Zn) using sediment quality assessment indices. The average concentration of trace metals in the sediments exceeded the crustal abundance suggesting sources other than natural in origin. Additionally, the trace metals profile may be a reflection of socio-economic development in the vicinity of Sundarban which further attributes trace metals abundance to the anthropogenic inputs. Geoaccumulation index suggests moderately polluted sediment quality w.r.t. Ni and As and background concentrations for Al, Fe, Mn, Cu, Zn, Pb, Co, As and Cd. Contamination factor analysis suggested low contamination by Zn, Cr, Co and Cd, moderate by Fe, Mn, Cu and Pb while Ni and As show considerable and high contamination, respectively. Enrichment factors for Ni, Pb and As suggests high contamination from either biota or anthropogenic inputs besides natural enrichment. As per the three sediment quality guidelines, Fe, Mn, Cu, Ni, Co and As would be more of a concern with respect to ecotoxicological risk in the Sundarban mangroves. The correlation between various physiochemical variables and trace metals suggested significant role of fine grained particles (clay) in trace metal distribution whereas owing to low organic carbon content in the region the organic complexation may not be playing significant role in trace metal distribution in the Sundarban mangroves.

  2. μSR investigation of a new diluted magnetic semiconductor Li(Zn,Mn,Cu)As with Mn and Cu codoping at the same Zn sites

    NASA Astrophysics Data System (ADS)

    Guo, S. L.; Zhao, Y.; Man, H. Y.; Ding, C.; Gong, X.; Zhi, G. X.; Fu, L. C.; Gu, Y. L.; Frandsen, B. A.; Liu, L.; Cheung, S. C.; Munsie, T. J.; Wilson, M. N.; Cai, Y. P.; Luke, G. M.; Uemura, Y. J.; Ning, F. L.

    2016-09-01

    We report the successful synthesis and characterization of a new type I-II-V bulk form diluted magnetic semiconductor (DMS) Li(Zn,Mn,Cu)As, in which charge and spin doping are decoupled via (Cu,Zn) and (Mn,Zn) substitution at the same Zn sites. Ferromagnetic transition temperature up to  ˜33 K has been observed with a coercive field  ˜40 Oe for the 12.5% doping level. μSR measurements confirmed that the magnetic volume fraction reaches nearly 100% at 2 K, and the mechanism responsible for the ferromagnetic interaction in this system is the same as other bulk form DMSs.

  3. The development of a new optical sensor based on the Mn doped ZnS quantum dots modified with the molecularly imprinted polymers for sensitive recognition of florfenicol

    NASA Astrophysics Data System (ADS)

    Sadeghi, Susan; Jahani, Moslem; Belador, Foroogh

    2016-04-01

    The Mn doped ZnS quantum dots (Mn:ZnS QDs) capped with the florfenicol molecularly imprinted polymer (Mn:ZnS QDs@MIP) were prepared via the sol-gel surface imprinting approach using 3-aminopropyltriethoxysilane (APTES) as the functional monomer and tetraethoxysilane (TEOS) as the cross-linker for the optosensing of the florfenicol. Transmission electron microscopy (TEM), X-ray diffractometer, IR spectroscopy, UV-Vis absorption spectrophotometry, and spectrofluorometry were used to elucidate the formation, morphology, and identification of the products. To illustrate the usefulness of the new imprinted material, the non-imprinted coated Mn:ZnS QDs (Mn:ZnS QDs@NIP) were synthesized without the presence of the florfenicol. It was revealed that the fluorescence (FL) intensity of the Mn:ZnS QDs@MIP increased with increasing the FF concentration. Under the optimal conditions, changes in the FL intensity in the presence of the target molecule showed a linear response in the concentration range of 30-700 μmol L- 1 with a detection limit of 24 μmol L- 1. The developed method was finally applied successfully to the determination of FF in different meat samples with satisfactory recoveries.

  4. The development of a new optical sensor based on the Mn doped ZnS quantum dots modified with the molecularly imprinted polymers for sensitive recognition of florfenicol.

    PubMed

    Sadeghi, Susan; Jahani, Moslem; Belador, Foroogh

    2016-04-15

    The Mn doped ZnS quantum dots (Mn:ZnS QDs) capped with the florfenicol molecularly imprinted polymer (Mn:ZnS QDs@MIP) were prepared via the sol-gel surface imprinting approach using 3-aminopropyltriethoxysilane (APTES) as the functional monomer and tetraethoxysilane (TEOS) as the cross-linker for the optosensing of the florfenicol. Transmission electron microscopy (TEM), X-ray diffractometer, IR spectroscopy, UV-Vis absorption spectrophotometry, and spectrofluorometry were used to elucidate the formation, morphology, and identification of the products. To illustrate the usefulness of the new imprinted material, the non-imprinted coated Mn:ZnS QDs (Mn:ZnS QDs@NIP) were synthesized without the presence of the florfenicol. It was revealed that the fluorescence (FL) intensity of the Mn:ZnS QDs@MIP increased with increasing the FF concentration. Under the optimal conditions, changes in the FL intensity in the presence of the target molecule showed a linear response in the concentration range of 30-700 μmol L(-1) with a detection limit of 24 μmol L(-1). The developed method was finally applied successfully to the determination of FF in different meat samples with satisfactory recoveries. Copyright © 2016 Elsevier B.V. All rights reserved.

  5. MnZn-ferrites: Targeted Material Design for New Emerging Application Products

    NASA Astrophysics Data System (ADS)

    Zaspalis, V. T.; Tsakaloudi, V.; Kogias, G.

    2014-07-01

    In this article the main characteristics for emerging MnZn-ferrite applications are described on the basis of the new demands they possess on the ferrite material development. A number of recently developed MnZn-ferrite materials is presented together with the main scientific principles lying behind their development. These include: (i) high saturation flux density MnZn-ferrites (i.e. Bsat=550 mT at 10 kHz, 1200 A/m, 100°C), (ii) low power losses MnZn-ferrites (i.e. Pv~210 mW cm-3 at 100 kHz, 200mT, 100°C), (iii) MnZn-ferrites with broad temperature stability (i.e. PV<375 mW cm-3 for 25°C

  6. The Crystal Structure of Micro- and Nanopowders of ZnS Studied by EPR of Mn2+ and XRD.

    PubMed

    Nosenko, Valentyna; Vorona, Igor; Grachev, Valentyn; Ishchenko, Stanislav; Baran, Nikolai; Becherikov, Yurii; Zhuk, Anton; Polishchuk, Yuliya; Kladko, Vasyl; Selishchev, Alexander

    2016-12-01

    The crystal structure of micro- and nanopowders of ZnS doped with different impurities was analyzed by the electron paramagnetic resonance (EPR) of Mn 2+ and XRD methods. The powders of ZnS:Cu, ZnS:Mn, ZnS:Co, and ZnS:Eu with the particle sizes of 5-7 μm, 50-200 nm, 7-10 μm, and 5-7 nm, respectively, were studied. Manganese was incorporated in the crystal lattice of all the samples as uncontrolled impurity or by doping. The Mn 2+ ions were used as EPR structural probes. It is found that the ZnS:Cu has the cubic structure, the ZnS:Mn has the hexagonal structure with a rhombic distortion, the ZnS:Co is the mixture of the cubic and hexagonal phases in the ratio of 1:10, and the ZnS:Eu has the cubic structure and a distorted cubic structure with stacking defects in the ratio 3:1. The EPR technique is shown to be a powerful tool in the determination of the crystal structure for mixed-polytype ZnS powders and powders with small nanoparticles. It allows observation of the stacking defects, which is revealed in the XRD spectra.

  7. Size Dependent Elemental Composition of Road-Associated Particles

    PubMed Central

    McKenzie, Erica R.; Wong, Carol M.; Green, Peter G.; Kayhanian, Masoud; Young, Thomas M.

    2009-01-01

    Stormwater particles often provide transport for metals and other contaminants, however only larger particles are effectively removed by typical best management practices. Fine particles and their associated constituents are more likely to reach receiving waters; this merits further investigation regarding the metal contribution of fine (dp<10 μm) and very fine (dp <1.5 μm) particles. Road associated particles were collected by vacuuming a road surface and by collecting highway stormwater runoff. A cell sorter was employed to sort road associated particles into four size ranges: 0.1–0.3, 0.3–0.5, 0.5–1.0, and 1.0–1.5 μm. These very fine particles, along with six particle size ranges (total range <2–63 μm) separated using a settling column, were analyzed for Al, Mn, Fe, Cr, Ni, Cu, Zn, and Pb using Inductively Coupled Plasma Mass Spectrometry (ICP-MS). Enrichment factors (EFs), calculated using Al as a basis to represent crustal contributions, were similar for the vacuumed road dust and the stormwater runoff. Fe and Mn were minimally depleted (0.1x) or near unity for all size ranges (Fe EF range 0.01–3.7; Mn EF range 0.02–10.6). Cr, Ni, Cu, Zn, and Pb were moderately (10x) to considerably (>100x) enriched for most size ranges; these metals were most enriched in the very fine fractions (max EF~4900 in Zn, 0.1–0.3 μm). Based on this preliminary study, a cell sorter is an acceptable means of fractionating aqueous particles of diameter 0.1–1.5 μm. In spite of their minimal relative mass contribution, the very fine particles are environmentally relevant due to their mobility and enrichment in potentially toxic metals.. PMID:18433840

  8. Direct Electrothermal Atomic Absorption Determination of Trace Elements in Body Fluids (Review)

    NASA Astrophysics Data System (ADS)

    Zacharia, A. N.; Arabadji, M. V.; Chebotarev, A. N.

    2017-03-01

    This review is focused on the state and development of tendencies of electrothermal atomic absorption spectroscopy over the last 25 years (from 1990 to 2016) in the direct determination of Cu, Zn, Pb, Cd, Mn, Se, As, Cr, Co, Ni, Al, and Hg in body fluids such as blood, urine, saliva, and breast milk.

  9. Solvothermal synthesis of Zn{sub 2}GeO{sub 4}:Mn{sup 2+} nanophosphor in water/diethylene glycol system

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Takeshita, Satoru; Honda, Joji; Isobe, Tetsuhiko, E-mail: isobe@applc.keio.ac.jp

    2012-05-15

    The influence of aging of the suspension containing the amorphous precusors on structural, compositional and photoluminescent properties is studied to understand the mechanism on the formation of Zn{sub 2}GeO{sub 4}:Mn{sup 2+} nanoparticles during the solvothermal reaction in the water/diethylene glycol mixed solvent. Aging at 200 Degree-Sign C for 20 min forms the crystalline Zn{sub 2}GeO{sub 4} nanorods and then they grow up to {approx} 50 nm in mean length after aging for 240 min. Their interplanar spacing of (410) increases with increasing the aging time. The photoluminescence intensity corresponding to the d-d transition of Mn{sup 2+} increases with increasing themore » aging time up to 120 min, and then decreases after aging for 240 min. The photoluminescence lifetime decreases with increasing the aging time, indicating the locally concentrated Mn{sup 2+} ions. These results reveal that Mn{sup 2+} ions gradually replace Zn{sup 2+} ions near surface through repeating dissolusion and precipitation processes during prolonged aging after the complete crystallization of Zn{sub 2}GeO{sub 4}. - Graphical abstract: TEM images of Zn{sub 2}GeO{sub 4}:Mn{sup 2+} nanoparticles aged at 200 Degree-Sign C for different aging times in the mixed solvent of water and diethylene glycol. Highlights: Black-Right-Pointing-Pointer Mechanism on formation of Zn{sub 2}GeO{sub 4}:Mn{sup 2+} nanophosphor under solvothermal condition. Black-Right-Pointing-Pointer Zn{sub 2}GeO{sub 4} nanorods crystallize via amorphous precursors. Black-Right-Pointing-Pointer Gradual substitution of Mn{sup 2+} during prolonged aging. Black-Right-Pointing-Pointer Such an inhomogeneous Mn{sup 2+} doping process results in concentration quenching.« less

  10. Synthesis and stability of hetaerolite, ZnMn2O4, at 25°C

    USGS Publications Warehouse

    Hem, J.D.; Roberson, C.E.; Lind, C.J.

    1987-01-01

    A precipitate of nearly pure hetaerolite, ZnMn2O4, a spinel-structured analog of hausmannite, Mn3O4, was prepared by an irreversible wprecipitation of zinc with manganese at 25°C. The synthesis technique entailed constant slow addition of a dilute solution of Mn2+ and Zn2+ chlorides having a Mn/Zn ratio of 2:1 to a reaction vessel that initially contained distilled deionized water, maintained at a pH of 8.50 by addition of dilute NaOH by an automated pH stat, with continuous bubbling of CO2-free air. The solid was identified by means of X-ray diffraction and transmission electron microscopy and consisted of bipyramidal crystals generally less than 0.10 μm in diameter. Zn2+ ions are able to substitute extensively for Mn2+ ions that occupy tetrahedral sites in the hausmannite structure.Hetaerolite appears to be more stable than hausmannite with respect to spontaneous conversion to γMnOOH. The value of the standard free energy of formation of hetaerolite was estimated from the experimental data to be −289.4 ± 0.8 kcal per mole. Solids intermediate in composition between hetaerolite and hausmannite can be prepared by altering the Mn/Zn ratio in the feed solution.

  11. Crystal structure, energy transfer and tunable luminescence properties of Ca8ZnCe(PO4)7:Eu2+,Mn2+ phosphor

    NASA Astrophysics Data System (ADS)

    Ding, Chong; Tang, Wanjun

    2018-02-01

    Single-phased Ca8ZnCe(PO4)7:Eu2+,Mn2+ phosphors with whitlockite-type structure have been prepared via the combustion-assisted synthesis technique. The XRD pattern show that the as-obtained phosphors crystallize in a trigonal phase with space group of R-3c (161). Ca8ZnCe(PO4)7 host is full of sensitizers (Ce3+) and the Ce3+ emission at different lattice sites has been discussed. The efficient energy transfers from Ce3+ ions to Eu2+/Mn2+ ions and from Eu2+ to Mn2+ have been validated. Under UV excitation, the emitting color of Ca8ZnCe(PO4)7:Eu2+/Mn2+ samples can be modulated from violet blue to green and from violet blue to red-orange by the energy transfers of Ce3+→Eu2+ and Ce3+→Mn2+, respectively. Additionally, white emission has been obtained through adjusting the relative concentrations of Eu2+ and Mn2+ ions in the Ca8ZnCe(PO4)7 host under UV excitation. These results indicate that as-prepared Ca8ZnCe(PO4)7:Eu2+,Mn2+ may be a potential candidate as color-tunable white light-emitting phosphors.

  12. Long-term impact of primary domestic sewage on metal/loid accumulation in drainage ditch sediments, plants and water: Implications for phytoremediation and restoration.

    PubMed

    Kumwimba, Mathieu Nsenga; Zhu, Bo; Suanon, Fidèle; Muyembe, Diana Kavidia; Dzakpasu, Mawuli

    2017-03-01

    We evaluate the long-term performance of a vegetated drainage ditch (VDD) treating domestic sewage with respect to heavy metal/metalloid (HM/M) accumulation in sediments, plants and water. VDD sediment contained significantly higher macro and trace elements compared to an agricultural ditch (AD) sediment. However, concentrations of HM/Ms in VDD sediment were below the ranges considered toxic to plants. Most HM/Ms were efficiently removed in the VDD, whereby removal efficiencies varied between 11% for Al and 89% for K. Accumulation of HM/Ms varied among species and plant parts, although sequestration by plants represents only a small proportion (<1%) of the inflow load. Accumulation of Al, As, Cd, Pb, Cr, Fe and Ni in VDD plants were mostly distributed in the roots, indicating an exclusive strategy for metal tolerance. The opposite was found for Zn, Cu, K, Ca, P, K, Na, N and Mg, which were accumulated either in the stems or leaves. Overall, concentrations of metals in sediment showed significant positive correlations with those in ditch plants. None of the studied species were identified as metal hyper-accumulators (i.e. >10,000mgkg -1 of Zn or Mn). Nevertheless, the high translocation factor (TF) values for Mn, Ni, Cu, Zn, Na, Mg, P, K and Ca in the ditch plants make them suitable for phytoextraction from water/soil, while the low TF values for Pb, Cd, As, Fe, Cr and Al make them suitable for their phytostabilization. Copyright © 2017 Elsevier B.V. All rights reserved.

  13. Iron-based soft magnetic composites with Mn-Zn ferrite nanoparticles coating obtained by sol-gel method

    NASA Astrophysics Data System (ADS)

    Wu, Shen; Sun, Aizhi; Xu, Wenhuan; Zhang, Qian; Zhai, Fuqiang; Logan, Philip; Volinsky, Alex A.

    2012-11-01

    This paper focuses on iron-based soft magnetic composites which were synthesized by utilizing Mn-Zn ferrite nanoparticles to coat iron powder. The nanocrystalline iron powders, with an average particle diameter of 20 nm, were obtained via the sol-gel method. Scanning electron microscopy, energy dispersive X-ray spectroscopy and distribution maps show that the iron particle surface is covered with a thin layer of Mn-Zn ferrites. Mn-Zn ferrite uniformly coated the surface of the powder particles, resulting in a reduced imaginary permeability, increased electrical resistivity and a higher operating frequency of the synthesized magnets. Mn-Zn ferrite coated samples have higher permeability and lower magnetic loss when compared with the non-magnetic epoxy resin coated compacts. The real part of permeability increases by 33.5% when compared with the epoxy resin coated samples at 10 kHz. The effects of heat treatment temperature on crystalline phase formation and on the magnetic properties of the Mn-Zn ferrite were investigated via X-ray diffraction and a vibrating sample magnetometer. Ferrites decomposed to FeO and MnO after annealing above 400 °C in nitrogen; thus it is the optimum annealing temperature to attain the desired permeability.

  14. Convenient synthesis of Mn-doped Zn (O,S) nanoparticle photocatalyst for 4-nitrophenol reduction

    NASA Astrophysics Data System (ADS)

    Susanto Gultom, Noto; Abdullah, Hairus; Kuo, Dong-Hau

    2018-04-01

    The conversion of 4-nitrophenol as a toxic and waste pollutant to 4-aminophenol as a non-toxic and useful compound by photocatalytic reduction is highly important. In this work, the solid-solution concept by doping was involved to synthesis earth-abundant and green material of Mn-doped Zn(O,S). Zn(O,S) with different Mn doping contents was easily synthesized at low temperature 90°C for 4-NP reduction without using the reducing agent of NaBH4. The Mn-doped Zn(O,S) catalyst exhibited the enhancements in optical and electrochemical properties compared to un-doped Zn(O,S).It was found that 10% Mn-doped Zn(O,S) had the best properties and it could totally reduce 4-NP after 2h photoreactions under low UV illumination. The hydrogen ion was proposed to involve the 4-NP reduction to 4-AP, which is hydrogen ion and electron replaced the oxygen in amino (NO2) group of 4-NP to form the nitro (NH2) group. We alsoproposed the incorporation of Mn in Zn site in the Zn(O,S) host lattice could make the oxygen surface bonding weak for easily forming the oxygen vacancy. The more oxygen vacancy for more hydrogen ion would be generated to consume for 4-NP reduction.

  15. Investigation of spatial and temporal metal atmospheric deposition in France through lichen and moss bioaccumulation over one century.

    PubMed

    Agnan, Y; Séjalon-Delmas, N; Claustres, A; Probst, A

    2015-10-01

    Lichens and mosses were used as biomonitors to assess the atmospheric deposition of metals in forested ecosystems in various regions of France. The concentrations of 17 metals/metalloids (Al, As, Cd, Co, Cr, Cs, Cu, Fe, Mn, Ni, Pb, Sb, Sn, Sr, Ti, V, and Zn) indicated overall low atmospheric contamination in these forested environments, but a regionalism emerged from local contributions (anthropogenic activities, as well as local lithology). Taking into account the geochemical background and comparing to Italian data, the elements from both natural and anthropogenic activities, such as Cd, Pb, or Zn, did not show any obvious anomalies. However, elements mainly originating from lithogenic dust (e.g., Al, Fe, Ti) were more prevalent in sparse forests and in the Southern regions of France, whereas samples from dense forests showed an accumulation of elements from biological recycling (Mn and Zn). The combination of enrichment factors and Pb isotope ratios between current and herbarium samples indicated the historical evolution of metal atmospheric contamination: the high contribution of coal combustion beginning 150 years ago decreased at the end of the 20th century, and the influence of car traffic during the latter observed period decreased in the last few decades. In the South of France, obvious local influences were well preserved during the last century. Copyright © 2015 Elsevier B.V. All rights reserved.

  16. DENSITY FUNCTIONAL STUDY OF ELEMENTAL MERCURY ADSORPTION ON X (X=Mn, Si, Ti, Al, AND Zn)-DOPED CuO (110) SURFACE

    NASA Astrophysics Data System (ADS)

    He, Ping; Peng, Xiaolong; Zhang, Zhongzhi; Wu, Jiang; Chen, Naichao; Ren, Jianxing

    Copper oxide (CuO) is proved to be a potential adsorbent for elemental mercury in the flue gas emitted from coal-fired power plant. However, the O-terminated CuO(110) surface has relatively week adsorption capacity for Hg. In this work, the doped method is applied to enhance the mercury adsorption capacity of O-terminated CuO(110). Mn, Si, Ti, Al and Zn are selected as the doped atom. It is found that only Zn-doped CuO (110) surfaces have the higher adsorption energy than the pure O-terminated CuO(110) surface. The mercury adsorption capacity is a complex issue, which depends on a combination of oxygen and doped element. The results suggest that the lower electropositive doped element is favorable for the improvement of mercury adsorption capacity. However, the lower electronegativity of oxygen atoms does not facilitate the mercury capture, which is different from the organic material. Cu and doped metal element, rather than oxygen atom, mainly determine mercury adsorption capacity of O-terminated CuO(110) surface, which leads to the lower adsorption capacity of the O-terminated CuO(110) surface than the Cu-terminated CuO(110) surface. The conclusions can also offer a valuable reference for the other metal oxide regarding mercury capture.

  17. Diode-pumped Cr-doped ZnMnSe and ZnMgSe lasers

    NASA Astrophysics Data System (ADS)

    Říha, A.; Němec, M.; Jelínková, H.; Čech, M.; Vyhlídal, D.; Doroshenko, M. E.; Komar, V. K.; Gerasimenko, A. S.

    2017-12-01

    Chromium ions Cr2+ are known to have good fluorescence properties in the mid-infrared spectral region around the wavelength of 2.5 μm. The aim of this study was the investigation of new laser crystal materials - Zn0.95Mn0.05Se, Zn0.70Mn 0.30Se, and Zn0.75Mg0.25Se doped by Cr2+ ions and comparison of their spectral and laser characteristics. The spectroscopic parameters as absorption and fluorescence spectra as well as lifetimes were measured. As optical pumping the laser diode generating radiation at the wavelength of 1.69 μm (pulse repetition rate 10 Hz, pulse width 2 ms) was used. The longitudinal-pumped resonator was hemispherical with an output coupler radius of curvature 150 mm. The laser emission spectra were investigated and the highest intensity of emitted radiation was achieved at wavelengths 2451 nm, 2469 nm, and 2470 nm from the Cr:Zn0.95Mn0.05Se, Cr:Zn0.70Mn0.30Se, and Cr:Zn0.75Mg0.25Se laser systems, respectively. The input-output characteristics of laser systems were measured; the maximum output peak power 177 mW was obtained for Cr:Zn0.95Mn0.05Se laser system with slope efficiency of 6.3 % with respect to absorbed peak power. The output peak power as well as output beam spatial structure were stable during measurements. For the selection of the lasing wavelength, the single 1.5 mm thick quartz plate was placed at the Brewster angle inside the optical resonator between the output coupler and laser active medium. This element provided the tuning in the wavelength range 2290-2578 nm, 2353-2543 nm, and 2420-2551 nm for Cr:Zn0.95Mn0.05Se, Cr:Zn0.70Mn0.30Se, and Cr:Zn0.75Mg0.25Se, respectively. The obtained spectral FWHM linewidth of the individual output radiation was 10 nm. A comparison with previously measured Cr:ZnSe laser system was added in the end

  18. Mechanisms of EDDHA effects on the promotion of floral induction in the long-day plant Lemna minor (L.).

    PubMed

    Krajncic, Bozidar; Nemec, Joze

    2003-02-01

    EDDHA added in an optimal concentration (20.5 mumol.L-1) to a modified Pirson-Seidel nutrient solution induces flowering in some clones of the species Lemna minor, Lemna gibba and Spirodela polyrrhiza, which in the absence of EDDHA in the same nutrient solution do not flower. By adding EDDHA (20.5 mumol.L-1), floral induction under LD conditions is optimally promoted in the long-day (LD) species Lemna minor. After adding EDDHA to the nutrient solution, before floral induction and during flowering, Zn, Mn and Cu content is significantly increased in plants. Zn-EDDHA (0.86 mumol.L-1), Mn-EDDHA (1.51 mumol.L-1) and Cu-EDDHA (0.12 mumol.L-1), when used individually, greatly promote flowering under LD conditions as compared to flowering in the same nutrient solution with an equivalent quantity of Zn, Mn or Cu in the nonchelate form. If, on the other hand, Zn-EDDHA and Mn-EDDHA are added to the nutrient solution together (instead of Zn and Mn in nonchelate form), their effect on the promotion of flowering is less than in the case of their individual use. This shows that there is antagonism between Zn-EDDHA and Mn-EDDHA that is eliminated by adding EDDHA to the nutrient solution. We obtained the highest percentage of flowering plants (i.e. 74%) if we added EDDHA (20.5 mumol.L-1) to the nutrient solution containing Mn, Zn and Cu in chelate form. 74% of flowering plants actually means that flowering was achieved in all physiologically mature plants. Our results show that EDDHA promotes floral induction in Lemna minor under LD conditions, especially through chelating Zn, Mn and Cu, and, in addition, through eliminating the antagonism between Mn and Zn chelates EDDHA. Zn-EDDHA (0.86 mumol.L-1) also promote floral differentiation, especially cell division of microspore mother cells into dyads and those into microspore tetrads, which can be seen in microphotographs. When investigating possible pathways through which Mn-EDDHA, Zn-EDDHA and Cu-EDDHA promote flowering, we studied the effects of various concentrations of IAA and sucrose added to the nutrient solution as well. The results support the hypothesis that one of the possible pathways in which Mn-EDDHA promotes floral induction is through auxin oxidase, whereas Zn-EDDHA and Cu-EDDHA probably promote it through the enhancement of the photosynthesis and synthesis of sucrose.

  19. Magnetic properties and loss separation in iron-silicone-MnZn ferrite soft magnetic composites

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Wu, Shen; Sun, Aizhi; Xu, Wenhuan

    This paper investigates the magnetic and structural properties of iron-based soft magnetic composites coated with silicone-MnZn ferrite hybrid. The organic silicone resin was added to improve the flexibility of the insulated iron powder and causes better adhesion between particles to increase the mechanical properties. Scanning electron microscopy and distribution maps show that the iron particle surface is covered with a thin layer of silicone-MnZn ferrite. Silicone-MnZn ferrite coated samples have higher permeability when compared with the non-magnetic silicone resin coated compacts. The real part of permeability increases by 34.18% when compared with the silicone resin coated samples at 20 kHz.more » In this work, a formula for calculating the total loss component by loss separation method is presented and finally the different parts of total losses are calculated. The results show that the eddy current loss coefficient is close to each other for the silicone-MnZn ferrite, silicone resin and MnZn ferrite coated samples (0.0078« less

  20. Catalytic conversion of syngas to mixed alcohols over Zn-Mn promoted Cu-Fe based catalyst

    DOE PAGES

    Lu, Yongwu; Yu, Fei; Hu, Jin; ...

    2012-04-12

    Zn-Mn promoted Cu-Fe based catalyst was synthesized by the co-precipitation method. Mixed alcohols synthesis from syngas was studied in a half-inch tubular reactor system after the catalyst was reduced. Zn-Mn promoted Cu-Fe based catalyst was characterized by SEM-EDS, TEM, XRD, and XPS. The liquid phase products (alcohol phase and hydrocarbon phase) were analyzed by GC-MS and the gas phase products were analyzed by GC. The results showed that Zn-Mn promoted Cu-Fe based catalyst had high catalytic activity and high alcohol selectivity. The maximal CO conversion rate was 72%, and the yield of alcohol and hydrocarbons were also very high. Cumore » (111) was the active site for mixed alcohols synthesis, Fe 2C (101) was the active site for olefin and paraffin synthesis. The reaction mechanism of mixed alcohols synthesis from syngas over Zn-Mn promoted Cu-Fe based catalyst was proposed. Here, Zn-Mn promoted Cu-Fe based catalyst can be regarded as a potential candidate for catalytic conversion of biomass-derived syngas to mixed alcohols.« less

  1. Anisotropic Dirac Fermions in BaMnBi2 and BaZnBi2

    NASA Astrophysics Data System (ADS)

    Ryu, Hyejin; Park, Se Young; Li, Lijun; Ren, Weijun; Petrovic, Cedomir; Hwang, Choonkyu; Mo, Sung-Kwan

    We report electronic structures of BaMnBi2 and BaZnBi2 sharing similar structural properties but having different valence configuration of the Mn/Zn-Bi complex. Our angle-resolved photoemission measurements found a strong anisotropic Dirac dispersion in BaMnBi2 and a complete departure from the Dirac dispersion in BaZnBi2. Our findings, substantiated by the first principle calculations, allow us to understand role of Mn/Zn-Bi tetrahedra in the changes of the electronic structures as well as the effect of varying band filling of Bi-square net. Work at BNL was supported by the U.S. Dept of Energy-BES, Division of Materials Science and Engineering, under Contract No. DE-SC0012704 and Chinese Academy of Sciences under Grant No. KJZD-EW-M05.

  2. Structure, morphology and optical properties of undoped and MN-doped ZnO(1-x)Sx nano-powders prepared by precipitation method

    NASA Astrophysics Data System (ADS)

    Dejene, F. B.; Onani, M. O.; Koao, L. F.; Wako, A. H.; Motloung, S. V.; Yihunie, M. T.

    2016-01-01

    The undoped and Mn-doped ZnO(1-x)Sx nano-powders were successfully synthesized by precipitation method without using any capping agent. Its structure, morphology, elemental analysis, optical and luminescence properties were determined by scanning electron microscopy (SEM), energy-dispersive X-ray spectroscopy (EDS), UV-vis spectroscopy (UV) and photoluminescence spectroscopy (PL). A typical SEM image of the un-doped ZnO(1-x)Sx nanoparticles exhibit flake like structures that changes to nearly spherical particles with Mn-doping. The XRD of undoped and Mn doped ZnO(1-x)Sx pattern reveals the formation of a product indexed to the hexagonal wurtzite phase of ZnS. The nanopowders have crystallite sizes estimated from XRD measurements were in the range of 10-20 nm. All the samples showed absorption maximum of ZnO(1-x)Sx at 271 nm and high transmittance in UV and visible region, respectively. The undoped ZnO(1-x)Sx nanoparticles show strong room-temperature photoluminescence with four emission bands centering at 338 nm, 384 nm, 448 nm and 705 nm that may originate to the impurity of ZnO(1-x)Sx, existence of oxide related defects. The calculated bandgap of the nanocrystalline ZnO(1-x)Sx showed a blue-shift with respect to the Mn-doping. The PL spectra of the Mn-doped samples exhibit a strong orange emission at around 594 nm attributed to the 4T1-6A1 transition of the Mn2+ ions.

  3. Facile hydrothermal synthesis of mn doped ZnO nanopencils for development of amperometric glucose biosensors

    NASA Astrophysics Data System (ADS)

    Shukla, Mayoorika; Pramila; Agrawal, Jitesh; Dixit, Tejendra; Palani, I. A.; Singh, Vipul

    2018-05-01

    Mn doped ZnO nanopencils were synthesized via low temperature hydrothermal process for fabrication of enzymatic electrochemical glucose biosensor. The KMnO4 was found to play a dual role in modifying morphology and inducing Mn doping. Interestingly, two different types of morphologies viz nanorods and nanopencils along with Mn doping in the later were obtained. Incorporation of Mn has shown a tremendous effect on the morphological variations, repression of defects and electrochemical charge transfer at electrode electrolyte interface. The possible reason behind obtained morphological changes has been proposed which in turn were responsible for the improvement in the different figure of merits of as fabricated enzymatic electrochemical biosensor. There has been a 17 fold enhancement in the sensitivity of the as fabricated glucose biosensor from ZnO nanorods to Mn doped ZnO nanopencils which can be attributed to morphological variation and Mn doping.

  4. Facile synthesis of highly uniform Mn/Co-codoped ZnO nanowires: optical, electrical, and magnetic properties.

    PubMed

    Li, Huifeng; Huang, Yunhua; Zhang, Qi; Qiao, Yi; Gu, Yousong; Liu, Jing; Zhang, Yue

    2011-02-01

    In this article, Co/Mn-codoped ZnO nanowires (NWs) were successfully synthesized on a silicon substrate by the thermal evaporation method with Au catalyst. The X-ray diffraction pattern indicated that the Co/Mn-codoped ZnO NWs are a hexagonal wurtzite structure without a second phase, and energy dispersive X-ray spectroscopy revealed that the Co and Mn ions were introduced into the ZnO NWs with the content of ∼0.8 at% and ∼1.2 at%, respectively. Photoluminescence spectra and Raman spectra showed that the Co/Mn were doped into the NWs and resulted in the shift of the near-band-edge emission. Moreover, the novel Raman peak at 519.3 cm(-1) has suggested that the two kinds of cations via doping could affect the local polarizability. Compared with the undoped ZnO NW, the electrical measurement showed that the Co/Mn-codoping enhanced the conductivity by an order of magnitude due to the presence of Co, Mn cations. The electron mobility and carrier concentration of a fabricated field effect transistor (FET) device is 679 cm2 V(-1) s(-1) and 2×10(18) cm(-3), respectively. Furthermore, the M-H curve demonstrated that the Co/Mn-codoped ZnO NWs have obvious ferromagnetic characteristics at room temperature. Our study enhances the understanding of the novel performances of transition-metal codoped ZnO NWs and also provides a potential way to fabricate optoelectronic devices.

  5. Effect of 50 MeV Li3 + irradiation on structural and electrical properties of Mn-doped ZnO

    NASA Astrophysics Data System (ADS)

    Neogi, S. K.; Chattopadhyay, S.; Banerjee, Aritra; Bandyopadhyay, S.; Sarkar, A.; Kumar, Ravi

    2011-05-01

    The present work aims to study the effect of ion irradiation on structural and electrical properties and their correlation with the defects in the Zn1 - xMnxO-type system. Zn1 - xMnxO (x = 0.02, 0.04) samples have been synthesized by the solid-state reaction method and have been irradiated with 50 MeV Li3 + ions. The concomitant changes have been probed by x-ray diffraction (XRD), temperature-dependent electrical resistivity and positron annihilation lifetime (PAL) spectroscopy. The XRD result shows a single-phase wurtzite structure for Zn0.98Mn0.02O, whereas for the Zn0.96Mn0.04O sample an impurity phase has been found, apart from the usual peaks of ZnO. Ion irradiation removes this impurity peak. The grain size of the samples is found to be uniform. For Zn0.98Mn0.02O, the observed sharp decrease in room temperature resistivity (ρRT) with irradiation is consistent with the lowering of the full width at half maximum of the XRD peaks. However, for Zn0.96Mn0.04O, ρRT decreases for the initial fluence but increases for a further increase in fluence. All the irradiated Zn0.98Mn0.02O samples show a metal-semiconductor transition in temperature-dependent resistivity measurements at low temperature. But all the irradiated Zn0.96Mn0.04O samples show a semiconducting nature in the whole range of temperatures. Results of room temperature resistivity, XRD and PAL measurements are consistent with each other.

  6. Preparation of Superparamagnetic Zn0.5Mn0.5Fe2O4 Particle by Coprecipitation-Sonochemical Method for Radar Absorbing Material

    NASA Astrophysics Data System (ADS)

    Taufiq, A.; Bahtiar, S.; Sunaryono; Hidayat, N.; Hidayat, A.; Mufti, N.; Diantoro, M.; Fuad, A.; Munasir; Rahmawati, R.; Adi, W. A.; Pratapa, S.; Darminto

    2017-05-01

    One of many applications of spinel ferrite nanoparticles is related to their performance as radar absorbing materials. In this work, we report developing synthesis method through combined coprecipitation-sonochemical routes in preparing Zn0.5Mn0.5Fe2O4 nanoparticle from iron sand in Indonesia as a vital raw material. The structure, size, morphology, and elements of the Zn0.5Mn0.5Fe2O4 nanoparticle were investigated via X-Ray diffractometry and Transmission/Scanning Electron Microscopy (TEM/SEM) combining Energy Dispersive Spectroscopy (EDS). The magnetic properties of the Zn0.5Mn0.5Fe2O4 nanoparticle were characterized by using Vibrating Sample Magnetometer (VSM). Furthermore, the reflection loss character of the Zn0.5Mn0.5Fe2O4 nanoparticle was determined via Vector Network Analyzer (VNA). From the qualitative and quantitative analysis of the XRD data, it can be identified that the Zn0.5Mn0.5Fe2O4 particle formed a spinel cubic structure in a single phase with the lattice parameter of approximately 8.401 Å. It is known from the TEM image that the Zn0.5Mn0.5Fe2O4 particle had a size of about 9.7 nm and tended to agglomerate. Furthermore, the data analysis of the M(H) curve presented that the Zn0.5Mn0.5Fe2O4 nanoparticle has a superparamagnetic behavior with the saturation magnetization of approximately 43 emu/g. Finally, the data analysis of the reflection loss as a function of frequency showed that the Zn0.5Mn0.5Fe2O4 nanoparticle performs as a radar absorbing material with the absorption performance of approximately -11.0 dB at the frequency of 10.8 GHz

  7. Chemically Tunable, All-Inorganic-Based White-Light Emitting 0D-1D Heterostructures

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Yue, Shiyu; Zhou, Yuchen; Zou, Shihui

    In this study, we initially created one-dimensional (1D) Mn2+-doped ZnS (ZnS: Mn) nanowires (NWs) with a unique optical signature. Specifically, these nanostructures coupled (i) ZnS defect-related self-activated emission spanning from wavelengths of 400 nm to 500 nm with (ii) Mn2+ dopant-induced emission centered at ~580 nm. These doped ZnS nanostructures were initially fabricated for the first time via a template-based co-precipitation approach followed by a post-synthesis annealing process. We subsequently formed novel 1D - zero-dimensional (0D) heterostructures incorporating ZnS: Mn NWs and AET (2-amino-ethanethiol) - CdSe quantum dots (QDs) by assembling annealed ZnS: Mn NWs with AET- capped CdSe QDsmore » as building blocks via a simple technique, involving physical sonication and stirring. Optical analyses of our heterostructures were consistent with charge (hole) and energy transfer-induced quenching of ZnS self-activated emission coupled with hole transfer-related quenching of Mn2+ emission by the QDs. The CdSe QD emission itself was impacted by competing charge (electron) and energy transfer processes occurring between the underlying ZnS host and the immobilized CdSe QDs. Chromaticity analysis revealed the significance of controlling both QD coverage density and Mn2+ dopant ratios in predictably influencing the observed color of our all-inorganic heterostructures. For example, white-light emitting behavior was especially prominent in composites, simultaneously characterized by (i) a 2.22% Mn2+ doping level and (ii) a molar compositional ratio of [ZnS: Mn2+]: [AET-capped CdSe QDs]) of 1: 1.5. Moreover, using these independent chemical ‘knobs’, we have been able to reliably tune for a significant shift within our composites from ‘cold-white’ (9604 K) to ‘warm-white’ (4383 K) light emission.« less

  8. Chemically Tunable, All-Inorganic-Based White-Light Emitting 0D-1D Heterostructures

    DOE PAGES

    Yue, Shiyu; Zhou, Yuchen; Zou, Shihui; ...

    2017-08-21

    In this study, we initially created one-dimensional (1D) Mn2+-doped ZnS (ZnS: Mn) nanowires (NWs) with a unique optical signature. Specifically, these nanostructures coupled (i) ZnS defect-related self-activated emission spanning from wavelengths of 400 nm to 500 nm with (ii) Mn2+ dopant-induced emission centered at ~580 nm. These doped ZnS nanostructures were initially fabricated for the first time via a template-based co-precipitation approach followed by a post-synthesis annealing process. We subsequently formed novel 1D - zero-dimensional (0D) heterostructures incorporating ZnS: Mn NWs and AET (2-amino-ethanethiol) - CdSe quantum dots (QDs) by assembling annealed ZnS: Mn NWs with AET- capped CdSe QDsmore » as building blocks via a simple technique, involving physical sonication and stirring. Optical analyses of our heterostructures were consistent with charge (hole) and energy transfer-induced quenching of ZnS self-activated emission coupled with hole transfer-related quenching of Mn2+ emission by the QDs. The CdSe QD emission itself was impacted by competing charge (electron) and energy transfer processes occurring between the underlying ZnS host and the immobilized CdSe QDs. Chromaticity analysis revealed the significance of controlling both QD coverage density and Mn2+ dopant ratios in predictably influencing the observed color of our all-inorganic heterostructures. For example, white-light emitting behavior was especially prominent in composites, simultaneously characterized by (i) a 2.22% Mn2+ doping level and (ii) a molar compositional ratio of [ZnS: Mn2+]: [AET-capped CdSe QDs]) of 1: 1.5. Moreover, using these independent chemical ‘knobs’, we have been able to reliably tune for a significant shift within our composites from ‘cold-white’ (9604 K) to ‘warm-white’ (4383 K) light emission.« less

  9. Marked synergism between mutant SOD1 and glutamate transport inhibition in the induction of motor neuronal degeneration in spinal cord slice cultures.

    PubMed

    Yin, Hong Z; Weiss, John H

    2012-04-11

    Loss of astrocytic glutamate transport capacity in ALS spinal cord supports an excitotoxic contribution to motor neuron (MN) damage in the disease, and dominant gain of function mutations in Cu/Zn superoxide dismutase (SOD1) cause certain familial forms of ALS. We have used organotypic slice cultures from wild type and G93A SOD1 mutant rat spinal cords to examine interactions between excitotoxicity and the presence of mutant SOD1 in the induction of MN degeneration. Slice cultures were prepared from 1 week old pups, and after an additional week in vitro, some were exposed to either a low level (30 μM) of the glutamate uptake inhibitor, trans-pyrrolidine-2,4-dicarboxylic acid (PDC) for 3 weeks, or a higher level (50 μM) for 48 h, followed by histochemical labeling to assess MN injury. In wild type animals these exposures caused relatively little MN degeneration. Similarly, little MN degeneration was seen in slices from SOD1 mutant animals that were not exposed to PDC. However, addition of PDC to SOD1 mutant slices resulted in substantial MN injury, which was markedly attenuated by a Ca2+ permeable AMPA-type (Ca-AMPA) glutamate channel blocker, or by a nitric oxide synthase antagonist. These observations illustrate the utility of the organotypic culture model for the investigation of intracellular interactions underlying MN degeneration in ALS, and support the hypothesis that activation of Ca-AMPA channels on MNs provides a metabolic burden that synergizes with deleterious effects of mutant SOD1 in the induction of MN injury. Copyright © 2012 Elsevier B.V. All rights reserved.

  10. Preliminary Study of ZnS:Mn2+ Quantum Dots Response Under UV and X-Ray Irradiation

    NASA Astrophysics Data System (ADS)

    Saatsakis, G.; Valais, I.; Michail, C.; Fountzoula, C.; Fountos, G.; Koukou, V.; Martini, N.; Kalyvas, N.; Bakas, A.; Sianoudis, I.; Kandarakis, I.; Panayiotakis, G. S.

    2017-11-01

    Quantum Dots are semiconductor nanocrystals, with their optical properties controlled by their size, shape and material composition. The aim of the present study is to examine the scintillation properties of Manganese Doped Zinc Sulfide (ZnS:Mn 2+) Quantum Dot (QDs) nanocrystals under UV and X-ray irradiation. ZnS:Mn 2+ Quantum Dots, with typical diameter of ZnS dots of 13-20nm (also called scintillation QDs, stQDs), were developed and acquired by Mesolight Inc. The initial stQD sample was a solution of 75mg of ZnS:Mn 2+ dissolved in 100μL of Toluene, having a concentration of 75% w/v. Emission characteristics under UV and X-Ray excitation were examined. Two ultraviolet sources were incorporated (315 nm and 365 nm) as well as a medical X-ray tube with tube voltage from 50 to 130 kVp. Parameters such as Energy Quantum Efficiency under UV excitation and Luminescence Efficiency-LE (light energy flux over exposure rate) under X-ray excitation were examined. Luminescence Efficiency (LE) of ZnS:Mn 2+ was higher than that exhibited by previously examined QDs, (ZnCdSeS:ZnS and ZnCuInS:ZnS). The ability of ZnS:Mn 2+ to transform UV photons energy into optical photons energy, tends to increase while the incident UV wavelength decreases. Energy Quantum Efficiency of the sample exhibited a 6% increase when exposed to 315nm UV light compared to 365 nm. The emission spectrum of the stQDs, exhibited a narrow peak (~585nm) in the yellow range.

  11. Accumulation of Metals and Boron in Phragmites australis Planted in Constructed Wetlands Polishing Real Electroplating Wastewater.

    PubMed

    Sochacki, Adam; Guy, Bernard; Faure, Olivier; Surmacz-Górska, Joanna

    2015-01-01

    The concentration of metals (Al, Cu, Fe, Mn, Ni, Zn) and B were determined in the above- and belowground biomass of Phragmites australis collected from the microcosm constructed wetland system used for the polishing of real electroplating wastewater. Translocation factor and bioconcentration factor were determined. Pearson correlation test was used to determine correlation between metal concentration in substrate and above- and belowground parts of Phragmites australis. The obtained results suggested that Phragmites australis did not play a major role as an accumulator of metals. It was observed also that the substrate could have exerted an effect on the translocation of Ni, Cu, Zn and Mn. The analysed concentrations of metals and B in biomass were in the range or even below the concentrations reported in the literature with the exception of Ni. The aboveground biomass was found suitable as a composting input in terms of metals concentrations.

  12. Geochemical distribution, fractionation and contamination assessment of heavy metals in marine sediments of the Asaluyeh port, Persian Gulf.

    PubMed

    Delshab, Hossein; Farshchi, Parvin; Keshavarzi, Behnam

    2017-02-15

    In this study, total concentration and speciation of heavy metals in sediments of the Asaluyeh, one of the Iran's largest commercial ports, are investigated. 48 sediment samples were collected and analyzed for trace and major elements. Sediment quality guidelines along with calculated enrichment factors and trace metal profiles indicate that Asaluyeh port is threated by contamination, especially with respect to Hg and Cu. Normalization to Sc indicated high enrichment factors in the sediments following the decreasing order of: Hg>Cu>As>Ni>Zn>Pb≈Cr≈Mn>Co≈V≈Fe≈Al. Hg displayed the greatest potential ecological risk factor among sampling stations. The results of sequential extraction procedure revealed that in some stations >50% of Mn, V, Cu and Zn occur in potentially mobile phases and therefore are more readily mobilized in the sediments of the study area. Copyright © 2016 Elsevier Ltd. All rights reserved.

  13. PIXE and ICP-MS Analysis of Andrographis Paniculata Medicinal Plant

    NASA Astrophysics Data System (ADS)

    Chandrasekhar Rao, J.; Naidu, B. G.; Sarita, P.; Srikanth, S.; Naga Raju, G. J.

    2017-08-01

    The concentrations of elements Li, Be, Al, Cl, K, Ca, Ti, V, Cr, Mn, Fe, Co, Ni, Cu, Zn, As, Se, Br, Rb, Sr, Ag, Cd, Ba, Pb and U in Andrographis Paniculata medicinal plant used in the treatment of Diabetes Mellitus were determined by using Particle Induced X-ray Emission (PIXE) and Inductively Coupled Plasma Mass Spectroscopy (ICP-MS) techniques. This plant was collected from four different geographical locations in Andhra Pradesh, India in order to assess the regional variation of elemental concentrations. Appreciable levels of K, Ca, Cr, Mn, Cu and Zn determined in this plant can be correlated to the antidiabetic property of Andrographis Paniculata since these elements are known to regulate and potentiate insulin action. Presence of toxic elements As, Cd and Pb necessitates the adoption of precautionary measures while prescribing dosage of the herbal medicine prepared from this plant for the treatment diabetes mellitus.

  14. Synthesis and property of spinel porous ZnMn2O4 microspheres

    NASA Astrophysics Data System (ADS)

    Guo, N.; Wei, X. Q.; Deng, X. L.; Xu, X. J.

    2015-11-01

    Mesoporous ternary zinc manganese oxides on the Ti sheet substrate are prepared by easy and fast hydrothermal method for the first time. The obtained ZnMn2O4 materials with homogenously distributed pores have been characterized by XRD, SEM and Raman spectra, which show the good crystal phase and particles for improving supercapacitive performance. XRD and SEM images show that the as-prepared samples have good crystallinity, and ZnMn2O4 microsphere has an average diameter of 10 μm. In addition, ZnMn2O4 are also characterized in 2 M KOH solution using three-electrode system. In the work, we study that different substrates (Ti, carbon and nickel foam) have an important effect on the electrochemical performance of the samples. The research of cyclic voltammogram (CV) indicates that the obtained specific capacitance (155 F g-1) values on nickel foam substrate for the ZnMn2O4 microspheres are higher than the values reported for some inexpensive oxides. However, the specific capacitance of all ZnMn2O4 samples has almost no change at two different scan rates which shows good long-term cycling stability. The electrochemical impedance spectroscopy with a small resistance reveals that the as-synthesized samples have good frequency response characteristics. These results indicate that the unique ZnMn2O4 electrode would be a promising electrode for high-performance supercapacitor applications.

  15. Synthesis and influence of ultrasonic treatment on luminescence of Mn incorporated ZnS nanoparticles

    NASA Astrophysics Data System (ADS)

    Cadis, A.-I.; Muresan, L. E.; Perhaita, I.; Munteanu, V.; Karabulut, Y.; Garcia Guinea, J.; Canimoglu, A.; Ayvacikli, M.; Can, N.

    2017-10-01

    Manganese (Mn) doping of ZnS phosphors was achieved by precipitation method using different ultrasound (US) maturation times. The structural and luminescence properties of the samples were carried out by means of X-ray diffraction (XRD), scanning electron microscope (SEM), energy dispersive spectroscopy (EDS), photoluminescence (PL), and cathodoluminescence (CL). The real amount of manganese incorporated in ZnS lattice was calculated based on ICP-OES results. According with XRD patterns, the phase structure of ZnS:Mn samples is cubic. EDS spectra reveal deviations of the Mn dopant concentration from the target composition. Both 300 K PL and CL emission spectra of the Mn doped ZnS phosphors display intense orange emission at 590 and 600 nm, respectively, which is characteristic emission of Mn ion corresponding to a 4T1→6A1 transition. Both PL and CL spectra confirmed manganese is substitutionally incorporated into the ZnS host as Mn2+. However, it is suggested that the origin of broad blue emission around 400 nm appeared in CL is due to the radiative recombination at deep level defect states in the ZnS. The ultrasound treatment at first enhances the luminescent intensity by ∼3 times in comparison with samples prepared by classical way. This study gives rise to an optimization guideline, which is extremely demanded for the development of new luminescent materials.

  16. Thermally stimulated properties in ZnSe:Tb and ZnSe:(Mn, Tb) phosphors

    NASA Astrophysics Data System (ADS)

    Mishra, A. K.; Mishra, S. K.; Pandey, S. P.; Lakshmi Mishra, Kshama

    2018-02-01

    Thermoluminescence studies were performed of ZnSe:Tb and ZnSe:(Mn, Tb) phosphors. A method of preparation for ZnSe phosphors doped with Tb and (Mn, Tb) has been discussed. The thermoluminescence (TL) properties of these phosphors have been studied from 100 to 370 K temperature after exciting by UV radiation (365 nm) at three uniform heating rates 0.4, 0.6 and 0.9 K/s. The trapping parameters like trap depth, lifetime of electrons and capture cross-section have also been determined using various methods.

  17. Functional manganese dioxide nanosheet for targeted photodynamic therapy and bioimaging in vitro and in vivo

    NASA Astrophysics Data System (ADS)

    Kim, Seongchan; Ahn, Seong Min; Lee, Ji-Seon; Kim, Tae Shik; Min, Dal-Hee

    2017-06-01

    Photodynamic therapy (PDT) has been widely studied as a promising non-invasive therapeutic strategy for the treatment of cancer. However, the poor solubility of photosensitizer (PS) in aqueous solution and inefficient cell-penetrating capability have limited the target-specific PDT. Herein, we develop a novel targeted photodynamic therapeutic and bioimaging system based on folic acid (FA)-conjugated MnO2 (FA-MnO2) nanosheet as a new carrier of PS, zinc phthalocyanine (ZnPc). ZnPc loaded FA-MnO2 nanosheet (FA-MnO2/ZnPc) complex is successfully formed by electrostatic interaction and coordination. We find that FA-MnO2/ZnPc complex exhibits excellent targeted delivery of ZnPc into folate receptor positive cancer cells and the ZnPc is released out from the complex via endogenous glutathione (GSH) stimulus, facilitating simultaneous bioimaging and targeted PDT by singlet oxygen (SO) generation upon light irradiation, showing high efficacy with only one tenth of conventional PS dosage in vitro and in vivo.

  18. Effects of Aging on the Evolution of Microstructure and Mechanical Properties of an Al - Li - Cu - Mg Alloy with Ag, Zr, Mn, and Zn Additives

    NASA Astrophysics Data System (ADS)

    Sun, Zhong-gang; Bao, Peng-li; Ma, Chao; Chen, Jie; Guo, Xuan; Li, Hua-guan; Ling, Juan

    2016-03-01

    The microstructure and the post-aging hardness of an Al - Li - Cu - Mg alloy is studied by the methods of transmission electron microscopy. Tensile tests are performed. The volume fraction and the size of the particles of the δ', S and T 1 phases are shown to be dependent on the aging temperature and time. The effect of the precipitates of the δ', S and T 1 phases on the hardening of the Al - Li - Cu - Mg alloy during aging is determined.

  19. Dependence of the magnetic properties of the dilute magnetic semiconductor Zn1-xMnxO nanorods on their Mn doping levels

    NASA Astrophysics Data System (ADS)

    Thongjamroon, S.; Ding, J.; Herng, T. S.; Tang, I. M.; Thongmee, S.

    2017-10-01

    The effects of Mn doping on the ferromagnetic properties of the dilute magnetic semiconductor Zn1-xMnxO nanorods (NR's) having the nominal composit-ions x = 0, 0.01, 0.03, 0.04 and 0.05 grown by a low temperature hydrothermal method are studied. Energy dispersive X-ray (EDX) is used to determine the actual amounts of the elements in each NR's. X-ray diffraction, scanning electron microscopy, photoluminescence and vibrating sample magnetometer measurements are used to observe the effects of the Mn substitution on the properties of the doped ZnO and to relate the changes in the properties to changes in the defect content. It is observed that the saturation magnetization of the Mn ions in the wurtzite structure varies from 0.0210 μB/Mn2+ to 0.0234 μB/Mn2+ reaching a high of 0.0251 μB/Mn2+ as the Mn concentrations is varied from 0.9 to 7.36 atomic%. It is argued that the changes in the saturation magnetization are due to the competition between the direct Mn-Mn exchange interaction and the indirect Mn-O-Mn exchange interaction in the doped Mn ZnO NP's.

  20. Multicolor tuning of manganese-doped ZnS colloidal nanocrystals.

    PubMed

    Quan, Zewei; Yang, Dongmei; Li, Chunxia; Kong, Deyan; Yang, Piaoping; Cheng, Ziyong; Lin, Jun

    2009-09-01

    In this paper, we report a facile route which is based on tuning doping concentration of Mn(2+) ions in ZnS nanocrystals, to achieve deliberate color modulation from blue to orange-yellow under single-wavelength excitation. X-ray diffraction (XRD), transmission electron microscopy (TEM), as well as photoluminescence (PL) spectra were employed to characterize the obtained samples. In this process, the relative emission intensities of both ZnS host (blue) and Mn(2+) dopant (orange-yellow) are sensitive to the Mn(2+) doping concentration, due to the energy transfer from ZnS host to Mn(2+) dopant. As a result of fine-tuning of these two emission components, white emission can be realized for Mn(2+)-doped ZnS nanocrystals. Furthermore, the as-synthesized doped nanocrystals possess extremely narrow size distribution and can be readily transferred into aqueous solution for the next potential applications.

  1. The effect of calcination temperature on the formation and magnetic properties of ZnMn2O4 spinel

    NASA Astrophysics Data System (ADS)

    Hermanto, B.; Ciswandi; Afriani, F.; Aryanto, D.; Sudiro, T.

    2018-03-01

    The spinel based on transition-metal oxides has a typical composition of AB2O4. In this study, the ZnMn2O4 spinel was synthesized using a powder metallurgy technique. The Zn and Mn metallic powders with an atomic ratio of 1:2 were mechanically alloyed for 3 hours in aqueous solution. The mixed powder was then calcined in a muffle furnace at elevated temperature of 400, 500 and 600 °C. The X-ray Diffractometer (XRD) was used to evaluate the formation of a ZnMn2O4 spinel structure. The magnetic properties of the sample at varying calcination temperatures were characterized by a Vibrating Sample Magnetometer (VSM). The results show that the fraction of ZnMn2O4 spinel formation increases with the increase of calcination temperature. The calcination temperature also affects the magnetic properties of the samples.

  2. Excitons and photoluminescence in ZnO and Zn0.99Mn0.01O nanocrystals

    NASA Astrophysics Data System (ADS)

    Gruzdev, N. B.; Sokolov, V. I.; Ermakov, A. E.; Uimin, M. A.; Mysik, A. A.; Pustovarov, V. A.

    2010-08-01

    The photoluminescence and photoluminescence excitation spectra for Zn1- x Mn x O nanocrystals are presented. After annealing of powders in air, the intensity of the bands attributable to manganese decreases noticeably. This suggests that the oxygen vacancies affect the Zhang-Rice-like states appearing due to strong d- p-hybridization, which is confirmed by an increase in the band gap of Zn1- x Mn x O for low x. The origin of the 2.9-eV peak and the shape of its excitation spectrum are discussed qualitatively. For Zn1- x Mn x O nanocrystals, the shape of the excitation spectrum is as unusual as the intense absorption in the range (2.2-3.0) eV.

  3. Bioaccumulation of Zn, Cu and Mn in the caviar and muscle of Persian sturgeon (Acipenser persicus) from the Caspian Sea, Iran.

    PubMed

    Mashroofeh, Abdulreza; Bakhtiari, Alireza Riyahi; Pourkazemi, Mohammad

    2012-12-01

    Concentrations of Zn, Cu and Mn were examined in caviar and muscle of the Persian sturgeon (Acipenser persicus) collected from coastal waters of south Caspian Sea during March and April, 2011. Mean Zn, Cu and Mn concentrations in caviar samples were 21.48, 2.05 and 1.66 μg g(-1) wet weight basis, respectively. The mean Zn, Cu and Mn concentrations in muscle tissues were 7.49, 1.00 and 0.34 μg g(-1) wet weight basis, respectively. The mean concentrations of Zn and Cu in caviar and muscle samples were under the permissible limits proposed by the United Kingdom's Ministry of Agriculture, Fisheries and Food (2000).

  4. Single-layer ZnMN2 (M = Si, Ge, Sn) zinc nitrides as promising photocatalysts.

    PubMed

    Bai, Yujie; Luo, Gaixia; Meng, Lijuan; Zhang, Qinfang; Xu, Ning; Zhang, Haiyang; Wu, Xiuqiang; Kong, Fanjie; Wang, Baolin

    2018-05-30

    Searching for two-dimensional semiconductor materials that are suitable for visible-light photocatalytic water splitting provides a sustainable solution to deal with the future energy crisis and environmental problems. Herein, based on first-principles calculations, single-layer ZnMN2 (M = Si, Ge, Sn) zinc nitrides are proposed as efficient photocatalysts for water splitting. Stability analyses show that the single-layer ZnMN2 zinc nitrides exhibit energetic and dynamical stability. The electronic properties reveal that all of the single-layer ZnMN2 zinc nitrides are semiconductors. Interestingly, single-layer ZnSnN2 is a direct band gap semiconductor with a desirable band gap (1.74 eV), and the optical adsorption spectrum confirms its optical absorption in the visible light region. The hydrogen evolution reaction (HER) calculations show that the catalytic activity for single-layer ZnMN2 (M = Ge, Sn) is better than that of single-layer ZnSiN2. Furthermore, the band gaps and band edge positions for the single-layer ZnMN2 zinc nitrides can be effectively tuned by biaxial strain. Especially, single-layer ZnGeN2 can be effectively tuned to match better with the redox potentials of water and enhance the light absorption in the visible light region at a tensile strain of 5%, which is confirmed by the corresponding optical absorption spectrum. Our results provide guidance for experimental synthesis efforts and future searches for single-layer materials suitable for photocatalytic water splitting.

  5. Photoluminescence study of Mn doped ZnS nanoparticles prepared by co-precipitation method

    NASA Astrophysics Data System (ADS)

    Deshpande, M. P.; Patel, Kamakshi; Gujarati, Vivek P.; Chaki, S. H.

    2016-05-01

    ZnS nanoparticles co-doped with different concentration (5,10,15%) of Mn were synthesized using polyvinylpyrrolidone (PVP) as a capping agent under microwave irradiation. We confirmed doping of Mn in the host ZnS by EDAX whereas powder X-ray diffractogram showed the cubic zinc blende structure of all these samples. TEM images did showed agglomeration of particles and SAED pattern obtained indicated polycrystalline nature. From SAED pattern we calculated lattice parameter of the samples which have close resemblance from that obtained from XRD pattern. The band gap values of pure and doped ZnS nanoparticles were calculated from UV-Visible absorption spectra. ZnS itself is a luminescence material but when we dope it with transition metal ion such as Mn, Co, and Cu they exhibits strong and intense luminescence in the particular region. The photoluminescence spectra of pure ZnS nanoparticles showed an emission at 421 and 485nm which is blue emission which was originated from the defect sites of ZnS itself and also sulfur deficiency and when doped with Mn2+ an extra peak with high intensity was observed at 530nm which is nearly yellow-orange emission which isrelated to the presence of Mn in the host lattice.

  6. Exploring the Cr{sup 2+} doping effect on structural, vibrational and dielectric properties of Mn-Zn ferrites

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Choudhary, Pankaj; Dar, M. A.; Varshney, Dinesh, E-mail: vdinesh33@rediffmail.com, E-mail: ty.ru123@gmail.com

    2016-05-23

    A series of Cr doped Mn-Zn ferrites with compositional formula Mn{sub 0.5}Zn{sub 0.5-x}Cr{sub x}Fe{sub 2}O{sub 4} (x = 0, 0.3, 0.5) were prepared by solid-state reaction route. X-ray diffraction (XRD) analysis reveals that the samples prepared are polycrystalline cubic spinel in structure (Fd3m) with some secondary phase of α–Fe{sub 2}O{sub 3}. Slight variation in the lattice parameter of Cr doped Mn{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4} has been observed due to difference in ionic radii of cations. Small shift in Raman modes towards higher wave number has been observed. Further the line width decreases with the doping ions. A giant dielectricmore » constant ~10{sup 4} is observed for parent Mn{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4} which is found to decrease with increase in Cr{sup 2+} doping. Low dielectric loss is observed for Mn{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4} and improves with Cr{sup 2+} doping at Zn{sup 2+} site.« less

  7. Novel magneto-luminescent effect in LSMO/ZnS:Mn nanocomposites at near-room temperature

    NASA Astrophysics Data System (ADS)

    Beltran-Huarac, Juan; Diaz-Diestra, Daysi; Bsatee, Mohammed; Wang, Jingzhou; Jadwisienczak, Wojciech M.; Weiner, Brad R.; Morell, Gerardo

    2016-02-01

    We report the tuning of the internal Mn photoluminescence (PL) transition of magnetically-ordered Sr-doped lanthanum manganite (LSMO)/Mn-doped zinc sulfide (ZnS:Mn) nanocomposites (NCs) by applying a static magnetic field in the range of 0-1 T below the critical temperature of ˜225 K. To do that, we have systematically fabricated LSMO/ZnS:Mn at different concentrations (1:1, 1:3, 1:5 and 1:10 wt%) via a straightforward solid-state reaction. X-ray diffraction and Raman analyses reveal that both phases coexist with a high degree of crystallinity and purity. Electron microscopy indicates that the NCs are almost spherical with an average crystal size of ˜6 nm, and that their surfaces are clean and smooth. The bifunctional character of LSMO/ZnS:Mn was evidenced by vibrating sample magnetometry and PL spectroscopy analyses, which show a marked ferromagnetic behavior and a broad, intense Mn orange emission band at room temperature. Moreover, the LSMO/ZnS:Mn at 1:3 wt% exhibits magneto-luminescent (ML) coupling below 225 K, and reaches the largest suppression of Mn-band PL intensity (up to ˜10%) at 150 K, when a magnetic field of 1.0 T is applied. The ML effect persists at magnetic fields as low as 0.2 T at 8 K, which can be explained by evoking a magnetic-ordering-induced spin-dependent restriction of the energy transfer to Mn states. No ML effect was observed in bare ZnS:Mn nanoparticles under the same experimental parameters. Our findings suggest that this NC can be considered as a new ML compound, similar to FeCo/InGaN-GaN and LSMO/ZnO NCs, useful as q-bits for quantum computation. The results presented here bring forth new avenues to better understand the interaction between semiconductors and perovskites, and exploit their synergistic effects in magneto-optics, spintronics and nanoelectronics.

  8. Enhanced magnetic fluid hyperthermia by micellar magnetic nanoclusters composed of Mn(x)Zn(1-x)Fe(2)O(4) nanoparticles for induced tumor cell apoptosis.

    PubMed

    Qu, Yang; Li, Jianbo; Ren, Jie; Leng, Junzhao; Lin, Chao; Shi, Donglu

    2014-10-08

    Monodispersed MnxZn1-xFe2O4 magnetic nanoparticles of 8 nm are synthesized and encapsulated in amphiphilic block copolymer for development of the hydrophilic magnetic nanoclusters (MNCs). These MNCs exhibit superparamagnetic characteristics, high specific absorption rate (SAR), large saturation magnetization (Ms), excellent stability, and good biocompatibility. MnFe2O4 and Mn0.6Zn0.4Fe2O4 are selected as optimum compositions for the MNCs (MnFe2O4/MNC and Mn0.6Zn0.4Fe2O4/MNC) and employed for magnetic fluid hyperthermia (MFH) in vitro. To ensure biosafety of MFH, the parameters of alternating magnetic field (AMF) and exposure time are optimized with low frequency, f, and strength of applied magnetic field, Happlied. Under optimized conditions, MFH of MnFe2O4/MNC and Mn0.6Zn0.4Fe2O4/MNC result in cancer cell death rate up to 90% within 15 min. The pathway of cancer cell death is identified as apoptosis, which occurs in mild hyperthermia near 43 °C. Both MnFe2O4/MNC and Mn0.6Zn0.4Fe2O4/MNC show similar efficiencies on drug-sensitive and drug-resistant cancer cells. On the basis of these findings, those MnxZn1-xFe2O4 nanoclusters can serve as a promising candidate for effective targeting, diagnosis, and therapy of cancers. The multimodal cancer treatment is also possible as amphiphilic block copolymer can encapsulate, in a similar fashion, different nanoparticles, hydrophobic drugs, and other functional molecules.

  9. Hydridable material for the negative electrode in a nickel-metal hydride storage battery

    DOEpatents

    Knosp, Bernard; Bouet, Jacques; Jordy, Christian; Mimoun, Michel; Gicquel, Daniel

    1997-01-01

    A monophase hydridable material for the negative electrode of a nickel-metal hydride storage battery with a "Lave's phase" structure of hexagonal C14 type (MgZn.sub.2) has the general formula: Zr.sub.1-x Ti.sub.x Ni.sub.a Mn.sub.b Al.sub.c Co.sub.d V.sub.e where ##EQU1##

  10. A preliminary study on identification of Thai rice samples by INAA and statistical analysis

    NASA Astrophysics Data System (ADS)

    Kongsri, S.; Kukusamude, C.

    2017-09-01

    This study aims to investigate the elemental compositions in 93 Thai rice samples using instrumental neutron activation analysis (INAA) and to identify rice according to their types and rice cultivars using statistical analysis. As, Mg, Cl, Al, Br, Mn, K, Rb and Zn in Thai jasmine rice and Sung Yod rice samples were successfully determined by INAA. The accuracy and precision of the INAA method were verified by SRM 1568a Rice Flour. All elements were found to be in a good agreement with the certified values. The precisions in term of %RSD were lower than 7%. The LODs were obtained in range of 0.01 to 29 mg kg-1. The concentration of 9 elements distributed in Thai rice samples was evaluated and used as chemical indicators to identify the type of rice samples. The result found that Mg, Cl, As, Br, Mn, K, Rb, and Zn concentrations in Thai jasmine rice samples are significantly different but there was no evidence that Al is significantly different from concentration in Sung Yod rice samples at 95% confidence interval. Our results may provide preliminary information for discrimination of rice samples and may be useful database of Thai rice.

  11. Investigation of the Influence of Selected Soil and Plant Properties from Sakarya, Turkey, on the Bioavailability of Trace Elements by Applying an In Vitro Digestion Model.

    PubMed

    Altundag, Huseyin; Albayrak, Sinem; Dundar, Mustafa S; Tuzen, Mustafa; Soylak, Mustafa

    2015-11-01

    The main aim of this study was an investigation of the influence of selected soil and plant properties on the bioaccessibility of trace elements and hence their potential impacts on human health in urban environments. Two artificial digestion models were used to determine trace element levels passing from soil and plants to man for bioavailability study. Soil and plant samples were collected from various regions of the province of Sakarya, Turkey. Digestive process is started by addition of soil and plant samples to an artificial digestion model based on human physiology. Bioavailability % values are obtained from the ratio of the amount of element passing to human digestion to element content of soil and plants. According to bioavailability % results, element levels passing from soil samples to human digestion were B = Cr = Cu = Fe = Pb = Li < Al < Ni < Co < Ba < Mn < Sr < Cd < Na < Zn < Tl, while element levels passing from plant samples to human digestion were Cu = Fe = Ni = Pb = Tl = Na = Li < Co < Al < Sr < Ba < Mn < Cd < Cr < Zn < B. It was checked whether the results obtained reached harmful levels to human health by examining the literature.

  12. Metal and hydrocarbon behavior in sediments from Brazilian shallow waters drilling activities using nonaqueous drilling fluids (NAFs).

    PubMed

    do Carmo R Peralba, Maria; Pozebon, Dirce; dos Santos, João H Z; Maia, Sandra M; Pizzolato, Tânia M; Cioccari, Giovani; Barrionuevo, Simone

    2010-08-01

    The impact of drilling oil activities in the Brazilian Bonito Field/Campos Basin (Rio de Janeiro) shell drilling (300 m) using nonaqueous fluids (NAFs) was investigated with respect to Al, Fe, Mn, Ba, Co, Pb, Cu, As, Hg, Cr, Ni, Zn, Cd, V, and aliphatic and polynuclear aromatic hydrocarbons concentrations in the sediment. Sampling took place in three different times during approximately 33 months. For the metals Al, As, Co, Cr, Cu, Cd, Fe, Ni, Mn, V, and Zn, no significant variation was observed after drilling activities in most of the stations. However, an increase was found in Ba concentration--due to the drilling activity--without return to the levels found 22 months after drilling. High Ba contents was already detected prior to well drilling, probably due to drilling activities in other wells nearby. Hydrocarbon contents also suggest previous anthropogenic activities. Aliphatic hydrocarbon contents were in the range usually reported in other drilling sites. The same behavior was observed in the case of polyaromatic hydrocarbons. Nevertheless, the n-alkane concentration increased sharply after drilling, returning almost to predrilling levels 22 months after drilling activities.

  13. Mass-size distribution and concentration of metals from personal exposure to arc welding fume in pipeline construction: a case report.

    PubMed

    Yang, Show-Yi; Lin, Jia-Ming; Young, Li-Hao; Chang, Ching-Wen

    2018-04-07

    We investigate exposure to welding fume metals in pipeline construction, which are responsible for severe respiratory problems. We analyzed air samples obtained using size-fractioning cascade impactors that were attached to the welders performing shielded metal and gas tungsten arc welding outdoors. Iron, aluminum, zinc, chromium, manganese, copper, nickel, and lead concentrations in the water-soluble (WS) and water-insoluble (WI) portions were determined separately, using inductively coupled plasma mass spectrometry. The mass-size distribution of welding fume matches a log-normal distribution with two modes. The metal concentrations in the welding fume were ranked as follows: Fe > Al > Zn > Cr > Mn > Ni > Cu > Pb. In the WS portion, the capacities of metals dissolving in water are correlated with the metal species but particle sizes. Particularly, Zn, Mn, and Pb exhibit relatively higher capacities than Cu, Cr, Al, Fe, and Ni. Exposure of the gas-exchange region of the lungs to WS metals were in the range of 4.9% to 34.6% of the corresponding metals in air by considering the particle-size selection in lungs, metal composition by particle size, and the capacities of each metal dissolving in water.

  14. Status of metal levels and their potential sources of contamination in Southeast Asian rivers.

    PubMed

    Chanpiwat, Penradee; Sthiannopkao, Suthipong

    2014-01-01

    To assess the concentration and status of metal contaminants in four major Southeast Asian river systems, water were collected from the Tonle Sap-Bassac Rivers (Cambodia), Citarum River (Indonesia), lower Chao Phraya River (Thailand), and Saigon River (Vietnam) in both dry and wet seasons. The target elements were Be, Al, Ti, V, Cr, Mn, Fe, Co, Ni, Cu, Zn, As, Se, Mo, Ag, Cd, Ba, Tl, and Pb and the concentrations exceeded the background metal concentrations by 1- to 88-fold. This distinctly indicates enrichment by human urban area activities. The results of a normalization technique used to distinguish natural from enriched metal concentrations confirmed contamination by Al, Cd, Co, Mn, Ni, Pb, and Zn. Cluster analysis revealed the probable source of metals contamination in most sampling sites on all rivers studied to be anthropogenic, including industrial, commercial, and residential activities. Stable lead isotopes analyses applied to track the sources and pathways of anthropogenic lead furthermore confirmed that anthropogenic sources of metal contaminated these rivers. Discharges of wastewater from both industrial and household activities were major contributors of Pb into the rivers. Non-point sources, especially road runoff and street dust, also contributed contamination from Pb and other metals.

  15. Effect of foliar application of micronutrients on the yield and quality of sweet orange (Citrus Sinensis L.).

    PubMed

    Tariq, M; Sharif, M; Shah, Z; Khan, R

    2007-06-01

    An experiment was designed to study the effect of foliar application of micronutrients on the yield, quality and leaf composition of sweet orange, Blood red variety at Shabazgari, Mardan. The experiment was laid out in a randomized complete block design in 2) factorial arrangement. Zinc, manganese and boron were applied as foliar spray at the rate of 0.4, 0.2 and 0.04 kg ha(-1), respectively in the presence of 1.56 kg N ha(-1) as urea and 0.4 kg surfactance ha(-1) (as wetting agent) in 400 L of water. The maximum fruit yield was obtained, when 0.4 kg Zn ha(-1) and 0.2 kg Mn ha(-1) was sprayed along with 1.56 kg N ha(-1) and 0.4 kg surfactance ha(-1) in 400 L of water. The minimum % peel was obtained with B alone and minimum % rag with Zn + Mn, maximum fruit size with Zn + B and maximum fruit volume with Zn + Mn. Similarly, % juice in sweet oranges was increased significantly by B alone, reducing sugar by Mn alone and vitamin C contents by Zn + B through foliar spray, suggested that each micronutrient had different role on the quality of citrus fruit. Foliar spray of Zn, Mn and B along with urea significantly increased the concentration of Zn and Mn in citrus leaves, while the concentration of B was not affected with foliar spray, perhaps due to dilution within the citrus tissues. Therefore, it is suggested that either Zn+Mn or Zn+B may be applied as foliar spray in combination with urea and surfactance for getting the maximum yield and improved quality of citrus fruit under prevailing conditions.

  16. First-principles study of ZnSnAs2-based dilute magnetic semiconductors

    NASA Astrophysics Data System (ADS)

    Kizaki, Hidetoshi; Morikawa, Yoshitada

    2018-02-01

    The electronic structure and magnetic properties of chalcopyrite Zn(Sn,TM)As2 and (Zn,TM)SnAs2 have been investigated by the Korringa-Kohn-Rostoker method combined with the coherent potential approximation within the local spin density approximation, where TM denotes a 3d transition metal element. We find that the half-metallic and high-spin ferromagnetic state can be obtained in Zn(Sn,V)As2, Zn(Sn,Cr)As2, Zn(Sn,Mn)As2, (Zn,V)SnAs2, and (Zn,Cr)SnAs2. The calculated result of Zn(Sn,Mn)As2 is in good agreement with the experimentally observed room-temperature ferromagnetism if we can control selective Mn doping at Sn sites. In addition, (Zn,V)SnAs2 and (Zn,Cr)SnAs2 are predicted to exhibit high-Curie-temperature ferromagnetism.

  17. Magneto-optical studies of ensembles of semimagnetic self-organized Cd(Mn)Se/Zn(Mn)Se Quantum Dots

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Reshina, I. I.; Ivanov, S. V.; Toropov, A. A.

    2013-12-04

    Ensembles of Cd(Mn)Se/ZnSe and CdSe/Zn(Mn)Se semimagnetic self-organized quantum dots with different Mn content have been studied by photoluminescence and resonant Raman scattering under strong magnetic fields in Faraday and Voigt geometries and with spectral and polarization selective excitation. Electron spin-flip Raman scattering has been observed in Voigt geometry in the structures with large Mn content. Narrow exciton peaks completely σ{sup −}σ{sup +} polarized have been observed under selective excitation in Faraday geometry in the structures with medium and small Mn content. A number of specific effects manifested themselves in the structures with a smallest Mn content where no Zeeman shiftmore » of the photoluminescence bands was observed.« less

  18. Distribution and Phase Association of Some Major and Trace Elements in the Arabian Gulf Sediments

    NASA Astrophysics Data System (ADS)

    Basaham, A. S.; El-Sayed, M. A.

    1998-02-01

    Twenty-four sediment samples were collected from the Arabian Gulf (ROPME Sea) and analysed for their grain size distribution and carbonate contents as well as the major elements Ca, Mg, Fe and Al and macro and trace elements Mn, Sr, Ba, Zn, Cu, Cr, V, Ni and Hg. Concentration of trace elements are found comparable to previous data published for samples taken before and after the Gulf War, and reflect the natural background level. Grain size analyses, aluminium and carbonate measurements support the presence of two major sediment types: (1) a terrigenous, fine-grained and Al rich type predominating along the Iranian side; and (2) a coarse-grained and carbonate rich type predominating along the Arabian side of the Gulf. Investigation of the correlation of the elements analysed with the sediment type indicates that they could be grouped under two distinct associations: (1) carbonate association including Ca and Sr; and (2) terrigenous association comprising Al, Fe, Mg, Ba, Mn, Zn, Cu, Cr, V, Ni and Hg. Element/Al ratios calculated for the mud non-carbonate fraction indicate that the Euphrates and Tigris rivers have minor importance as sediment sources to the Gulf. Most of the elements have exceptionally high aluminium ratios in sediments containing more than 85-90% carbonate. These sediments are restricted to the southern and south-eastern part of the area where depth is shallow and temperature and salinity are high. Both biological accumulation and chemical and biochemical coprecipitation could be responsible for this anomaly.

  19. Digestibility and retention of zinc, copper, manganese, iron, calcium, and phosphorus in pigs fed diets containing inorganic or organic minerals.

    PubMed

    Liu, Y; Ma, Y L; Zhao, J M; Vazquez-Añón, M; Stein, H H

    2014-08-01

    The objective of this experiment was to measure the apparent total tract digestibility (ATTD) and the retention rate of Zn, Cu, Mn, and Fe in pigs fed either inorganic or organic sources of Zn, Cu, Mn, and Fe. The experimental design was a randomized complete block design with a 2 × 3 factorial arrangement of treatments. There were 2 types of diets (corn grits-based or corn-soybean meal [SBM]-based diets) and 3 micromineral treatments (basal micromineral premix [BMM], inorganic micromineral premix [IMM], and organic micromineral premix [OMM]). The BMM contained no added Zn, Cu, Mn, or Fe; the IMM microminerals were provided as sulfates of Zn, Cu, Mn, and Fe at 40, 50, 20, and 100 mg/kg, respectively. The OMM contained the same levels of the 4 microminerals as IMM, but Zn, Cu, Mn, and Fe in this premix were provided by Zn(2-hydroxy-4-methylthio butanoic acid [HMTBa])2, Cu(HMTBa)2, Mn(HMTBa)2, and FeGly, respectively. Forty-eight barrows (initial BW: 31.1 ± 4.2 kg) were housed individually and allowed ad libitum access to the corn grits diet with BMM for 2 wk. All pigs were then moved to metabolism cages and randomly assigned to 1 of the 6 treatment diets with 8 replicates per diet. Fecal and urine samples were collected for 5 d following a 5-d adaptation period. Compared with corn grits diets, pigs fed corn-SBM diets had greater (P < 0.05) absorption and retention of Zn, Cu, and Mn but less (P < 0.05) ATTD of Zn and Cu. Compared with BMM, supplementation of IMM or OMM increased (P < 0.05) absorption, retention, ATTD, and retention rate of Zn, Cu, Mn, and Fe. Compared with IMM, adding OMM to the corn-SBM diet improved (P < 0.05) the absorption and retention of Cu and Mn and the ATTD of Cu, but these differences were not observed in the corn grits diets (interaction, P < 0.05). In addition, adding OMM to the corn-SBM diet increased (P < 0.05) absorption and retention of Zn and Fe and ATTD of Zn, Mn, and Fe compared with adding IMM to the corn-SBM diet. Supplementation of OMM also increased (P < 0.05) the ATTD and retention rate of P in corn-SBM diets. Results indicate that Zn(HMTBa)2 has greater digestibility and Cu(HMTBa)2 and Mn(HMTBa)2 have greater digestibility and retention rates compared with their inorganic sulfates, if included in a corn-SBM diet. Supplementation of organic microminerals also improves the digestibility of P in a corn-SBM diet.

  20. [The quantitative changes of bioelements (Ca, Zn, Mg, Cu, Mn) in crystalline lenses under the influence of hypodynamic stress and zinc].

    PubMed

    Kusleika, Saulius

    2002-01-01

    The aim of the study was to investigate and estimate quantitative changes of bioelements (Ca, Zn, Mg, Cu, Mn) in the lenses on the influence of hypodynamic stress and zinc (Zn). Hypodynamic stress of 48 days duration was provoked for Chinchilla rabbits (n = 20) by placing them in metal hutches. Every day (48 days) 10 rabbits, which had intervention received 0.3 mg/kg body wt. doses of Zn (in form of Zn acetate). The rabbits (n = 10) of the control group, which had no intervention were kept in vivarium conditions. Concentration of bioelements in the lenses of rabbits was detected by atomic absorption spectrophotometry 503 "Perkin-Elmer" (USA). The investigation revealed that hypodynamic stress of 48 days duration caused the increase in amount of Ca, Zn, Mn in lenses as compared with that in control rabbits and in rabbits receiving Zn. The concentration of bioelements (Ca, Zn, Mg, Cu, Mn) in lenses of rabbits receiving Zn in case of hypodynamic stress did not change significantly.

  1. Synthesis of robust water-soluble ZnS:Mn/SiO2 core/shell nanoparticles

    NASA Astrophysics Data System (ADS)

    Sun, Jing; Zhuang, Jiaqi; Guan, Shaowei; Yang, Wensheng

    2008-04-01

    Water-soluble Mn doped ZnS (ZnS:Mn) nanocrystals synthesized by using 3-mercaptopropionic acid (MPA) as stabilizer were homogeneously coated with a dense silica shell through a multi-step procedure. First, 3-mercaptopropyl triethoxy silane (MPS) was used to replace MPA on the particle surface to form a vitreophilic layer for further silica deposition under optimal experimental conditions. Then a two-step silica deposition was performed to form the final water-soluble ZnS:Mn/SiO2 core/shell nanoparticles. The as-prepared core/shell nanoparticles show little change in fluorescence intensity in a wide range of pH value.

  2. Manipulating the magnetism and resistance state of Mn:ZnO/Pb(Zr0.52Ti0.48)O3 heterostructured films through electric fields

    NASA Astrophysics Data System (ADS)

    Li, Yong-Chao; Wu, Jun; Pan, Hai-Yang; Wang, Jue; Wang, Guang-Hou; Liu, Jun-Ming; Wan, Jian-Guo

    2018-05-01

    Mn:ZnO/Pb(Zr0.52Ti0.48)O3 (PZT) heterostructured films have been prepared on Pt/Ti/SiO2/Si wafers by a sol-gel process. Nonvolatile and reversible manipulation of the magnetism and resistance by electric fields has been realized. Compared with the saturation magnetic moment (Ms) in the +3.0 V case, the modulation gain of Ms can reach 270% in the -3.0 V case at room temperature. The resistance change is attributed to the interfacial potential barrier height variation and the formation of an accumulation (or depletion) layer at the Mn:ZnO/PZT interface, which can be regulated by the ferroelectric polarization direction. The magnetism of Mn:ZnO originates from bound magnetic polarons. The mobile carrier variation in Mn:ZnO, owing to interfacial polarization coupling and the ferroelectric field effect, enables the electric manipulation of the magnetism in the Mn:ZnO/PZT heterostructured films. This work presents an effective method for modulating the magnetism of magnetic semiconductors and provides a promising avenue for multifunctional devices with both electric and magnetic functionalities.

  3. Exposure of women to trace elements through the skin by direct contact with underwear clothing.

    PubMed

    Nguyen, Thao; Saleh, Mahmoud A

    2017-01-02

    Heavy metals pose a potential danger to human health when present in textile materials. In the present study, inductive coupled plasma mass spectrometry (ICPMS) was used to determine the concentrations and the identity of extractable inorganic elements from different brands of women undergarments. A total of 120 samples consisting of 63 cottons, 44 nylons and 13 polyesters manufactured in 14 different countries having different colors were analyzed for their extractable metals contents. Elements analyzed were Ag, Al, As, Ba, Be, Bi, Ca, Cd, Co, Cr, Cu, Fe, Hg, K, Li, Mg, Mn, Na, Ni, Pb, Sb, Se, Sr, Ti, V and Zn. Cotton undergarments were rich in Al, Fe and Zn, nylon undergarments had high levels of Cr, Cu and Al, while polyester fabrics contained higher levels of Ni and Fe compared to cotton or nylon. With respect to manufacturing countries, China, Egypt and India showed the highest concentrations of metals in all fabrics. With respect to the color, black garments were characteristic by high concentration of Fe, blue colors with Cu, brown garments with Fe and Cu, green garments with Cu and Fe, pink garments with Al, purple garments with Al and Cu and red garments with Cr, Zn and Al. The consumer should be made aware of the potential dangers of these metals in their clothing.

  4. Photo- and electroluminescence of sulfide and silicate phosphors embedded in synthetic opal

    NASA Astrophysics Data System (ADS)

    Kaplan, S. F.; Kartenko, N. F.; Kurdyukov, D. A.; Medvedev, A. V.; Badalyan, A. G.; Golubev, V. G.

    2007-02-01

    The sulfide (ZnS:Mn, Zn xCd 1 -xS:Mn, Zn xCd 1- xS:Ag) and silicate (Zn 2SiO 4:Mn) phosphors were synthesized directly inside the pores of synthetic opal by chemical bath deposition. These composites are perfect three-dimensional photonic crystals, which produce effective photo- and electroluminescence at room temperature. The emission spectra are considerably modified by the photonic crystal structure to become anisotropic in accordance with the photonic band gap angular dispersion.

  5. Electrodeposition and Characterization of Mn-Cu-Zn Alloys for Corrosion Protection Coating

    NASA Astrophysics Data System (ADS)

    Tsurtsumia, Gigla; Gogoli, David; Koiava, Nana; Kakhniashvili, Izolda; Jokhadze, Nunu; Lezhava, Tinatin; Nioradze, Nikoloz; Tatishvili, Dimitri

    2017-12-01

    Mn-Cu-Zn alloys were electrodeposited from sulphate bath, containing citrate or EDTA and their mixtures as complexing ligands. The influence of bath composition and deposition parameters on alloys composition, cathodic current efficiency and structural and electrochemical properties were studied. At a higher current density (≥ 37.5 A dm-2) a uniform surface deposit of Mn-Cu-Zn was obtained. Optimal pH of electrolyte (0.3 mol/dm3Mn2+ + 0.6 mol/dm3 (NH4)2SO4 +0.1 mol/dm3Zn2++0.005 mol/dm3 Cu2++ 0.05mol/dm3Na3Cit + 0.15mol/dm3 EDTA; t=300C; τ=20 min) for silvery, nonporous coating of Mn-Cu-Zn alloy was within 6.5-7.5; coating composition: 71-83% Mn, 6-7.8% Cu, 11.5-20% Zn, current efficiency up to 40%. XRD patterns revealed BCT (body centred tetragonal) γ-Mn solid phase solution (lattice constants a=2.68 Å c=3.59 Å). Corrosion measurements of deposited alloys were performed in aerated 3.5% NaCl solution. The corrosion current density (icorr) of the electrodeposited alloys on carbon steel was 10 times lower than corrosion rate of pure zinc and manganese coatings. Triple alloy coatings corrosion potential (Ecorr = -1140 mV vs. Ag/AgCl) preserved negative potential value longer (more than three months) compared to carbon steel substrate (Ecorr = -670 mV vs. Ag/AgCl). Tafel polarization curves taken on Mn-Cu-Zn alloy coating in aerated 3.5% NaCl solution did not show a typical passivation behaviour which can be explained by formation oflow solubility of adherent corrosion products on the alloy surface. Corrosion test of Mn-Cu-Zn electrocoating in chlorine environment shows that it is the best cathodic protective coating for a steel product.

  6. Influence of Minor Alloying Elements on Selective Oxidation and Reactive Wetting of CMnSi TRIP Steel during Hot Dip Galvanizing

    NASA Astrophysics Data System (ADS)

    Cho, Lawrence; Kim, Myung Soo; Kim, Young Ha; De Cooman, Bruno C.

    2014-09-01

    The influence of the addition of minor alloying elements on the selective oxidation and the reactive wetting of CMnSi transformation-induced plasticity (TRIP) steels was studied by means of galvanizing simulator tests. Five TRIP steels containing small alloying additions of Cr, Ni, Ti, Cu, and Sn were investigated. After intercritical annealing (IA) at 1093 K (820 °C) in a N2 + 5 pct H2 gas atmosphere with a dew point of 213 K (-60 °C), two types of oxides were formed on the strip surface: Mn-rich xMnO·SiO2 ( x > 1.5) and Si-rich xMnO·SiO2 ( x < 0.3) oxides. The addition of the minor alloying elements changed the morphology of the Si-rich oxides from a continuous film to discrete islands and this improved the wettability by molten Zn. The improved wetting effect of the minor alloying elements was attributed to an increased area fraction of the surface where the oxides were thinner, enabling a direct unhindered reaction between Fe and the Al in the liquid Zn and the formation of the inhibition layer during the hot dip galvanizing. The addition of a small amount of Sn is shown to significantly decrease the density of Zn-coating defects on CMnSi TRIP steels.

  7. The role of marine biotoxins on the trophic transfer of Mn and Zn in fish.

    PubMed

    Pouil, Simon; Clausing, Rachel J; Metian, Marc; Bustamante, Paco; Dechraoui Bottein, Marie-Yasmine

    2018-05-01

    Essential nutrients are critical for physiological processes of organisms. In fish, they are obtained primarily from the diet, and their transfer and accumulation are known to be impacted by environmental variables such as water temperature, pH and salinity, as well as by diet composition and matrices. Yet, prey items consumed by fish may also contain toxic compounds such as marine toxins associated with harmful algae. These biotoxins have the potential to affect essential trace element assimilation in fish through chemical interactions such as the formation of trace element-toxin complexes or by affecting general fish physiology as in the modification of ion-specific transport pathways. We assessed the influence of dietary exposure to brevetoxins (PbTxs), ichthyotoxic neurotoxins produced by the dinoflagellate Karenia brevis, on trophic transfer of two essential trace elements, Mn and Zn, in a fish model. Using ecologically relevant concentrations of PbTxs and trace elements in controlled laboratory conditions, juvenile turbots Scophthalmus maximus were given food containing PbTxs before or at the same time as a feeding with radiotracers of the chosen essential elements ( 54 Mn and 65 Zn). Treatments included simultaneous exposure (PbTxs +  54 Mn +  65 Zn) in a single-feeding, 3-week daily pre-exposure to dietary PbTx followed by a single feeding with 54 Mn and 65 Zn, and a control ( 54 Mn and 65 Zn only). After a 21-day depuration period, turbot tissue brevetoxin levels were quantified and assimilation efficiencies of 54 Mn and 65 Zn were assessed. PbTxs were found in turbot tissues in each exposure treatment, demonstrating dietary trophic transfer of these toxins; yet, no differences in assimilation efficiencies of Mn or Zn were found between treatments or the control (p > 0.05). These results indicate that, in our experimental conditions, PbTx exposure does not significantly affect the trophic transfer of Mn and Zn in fish. Copyright © 2018 Elsevier B.V. All rights reserved.

  8. New procedure of quantitative mapping of Ti and Al released from dental implant and Mg, Ca, Fe, Zn, Cu, Mn as physiological elements in oral mucosa by LA-ICP-MS.

    PubMed

    Sajnóg, Adam; Hanć, Anetta; Koczorowski, Ryszard; Barałkiewicz, Danuta

    2017-12-01

    A new procedure for determination of elements derived from titanium implants and physiological elements in soft tissues by laser ablation inductively coupled plasma mass spectrometry (LA-ICP-MS) is presented. The analytical procedure was developed which involved preparation of in-house matrix matched solid standards with analyte addition based on certified reference material (CRM) MODAS-4 Cormorant Tissue. Addition of gelatin, serving as a binding agent, essentially improved physical properties of standards. Performance of the analytical method was assayed and validated by calculating parameters like precision, detection limits, trueness and recovery of analyte addition using additional CRM - ERM-BB184 Bovine Muscle. Analyte addition was additionally confirmed by microwave digestion of solid standards and analysis by solution nebulization ICP-MS. The detection limits are in range 1.8μgg -1 to 450μgg -1 for Mn and Ca respectively. The precision values range from 7.3% to 42% for Al and Zn respectively. The estimated recoveries of analyte addition line within scope of 83%-153% for Mn and Cu respectively. Oral mucosa samples taken from patients treated with titanium dental implants were examined using developed analytical method. Standards and tissue samples were cryocut into 30µm thin sections. LA-ICP-MS allowed to obtain two-dimensional maps of distribution of elements in tested samples which revealed high content of Ti and Al derived from implants. Photographs from optical microscope displayed numerous particles with µm size in oral mucosa samples which suggests that they are residues from implantation procedure. Copyright © 2017 Elsevier B.V. All rights reserved.

  9. Assessment of selected metals in the ambient air PM10 in urban sites of Bangkok (Thailand).

    PubMed

    Pongpiachan, Siwatt; Iijima, Akihiro

    2016-02-01

    Estimating the atmospheric concentrations of PM10-bounded selected metals in urban air is crucial for evaluating adverse health impacts. In the current study, a combination of measurements and multivariate statistical tools was used to investigate the influence of anthropogenic activities on variations in the contents of 18 metals (i.e., Al, Sc, V, Cr, Mn, Fe, Co, Ni, Cu, Zn, As, Se, Cd, Sb, Ba, La, Ce and Pb) in ambient air. The concentrations of PM10-bounded metals were measured simultaneously at eight air quality observatory sites during a half-year period at heavily trafficked roads and in urban residential zones in Bangkok, Thailand. Although the daily average concentrations of Al, V, Cr, Mn and Fe were almost equivalent to those of other urban cities around the world, the contents of the majority of the selected metals were much lower than the existing ambient air quality guidelines and standard limit values. The sequence of average values of selected metals followed the order of Al > Fe > Zn > Cu > Pb > Mn > Ba > V > Sb > Ni > As > Cr > Cd > Se > Ce > La > Co > Sc. The probability distribution function (PDF) plots showed sharp symmetrical bell-shaped curves in V and Cr, indicating that crustal emissions are the predominant sources of these two elements in PM10. The comparatively low coefficients of divergence (COD) that were found in the majority of samples highlight that site-specific effects are of minor importance. A principal component analysis (PCA) revealed that 37.74, 13.51 and 11.32 % of the total variances represent crustal emissions, vehicular exhausts and the wear and tear of brakes and tires, respectively.

  10. The bioleaching feasibility for Pb/Zn smelting slag and community characteristics of indigenous moderate-thermophilic bacteria.

    PubMed

    Cheng, Yi; Guo, Zhaohui; Liu, Xueduan; Yin, Huaqun; Qiu, Guanzhou; Pan, Fengkai; Liu, Hongwei

    2009-05-01

    The feasibility of recovering metal values and removing hazardous elements from the Pb/Zn smelting slag using bioleaching technique were studied through a flask experiment, and the community characteristics of the indigenous moderate-thermophilic bacteria in this bioleaching system were also analyzed through a culture-independent restriction fragment length polymorphism (RFLP) of 16S rRNA genes approach. The results show that more than 80% of Al, As, Cu, Mn, Fe and Zn in the Pb/Zn smelting slag were leached at 65(o)C, pH 1.5, pulp density 5%, but only about 5% of Pb. Phylogenetic analysis revealed that the bacteria in the bioleaching system mainly fell among Firmicutes, Gammaproteobacteria and Betaproteobacteria, and the dominant bacteria are affiliated with Bacillus spp., Sporosarcina spp. and Pseudomonas spp.

  11. Aqueous synthesis of Ag and Mn co-doped In2S3/ZnS quantum dots with tunable emission for dual-modal targeted imaging.

    PubMed

    Lai, Pei-Yu; Huang, Chih-Ching; Chou, Tzung-Han; Ou, Keng-Liang; Chang, Jia-Yaw

    2017-03-01

    Here, we present the microwave-assisted synthesis of In 2 S 3 /ZnS core/shell quantum dots (QDs) co-doped with Ag + and Mn 2+ (referred to as AgMn:In 2 S 3 /ZnS). Ag + altered the optical properties of the host QDs, whereas the spin magnetic moment (S=5/2) of Mn 2+ efficiently induced the longitudinal relaxation of water protons. To the best of our knowledge, this is the first report of the aqueous synthesis of color-tunable AgMn:In 2 S 3 /ZnS core/shell QDs with magnetic properties. The synthetic procedure is rapid, facile, reproducible, and scalable. The obtained QDs offered a satisfactory quantum yield (45%), high longitudinal relaxivity (6.84s -1 mM -1 ), and robust photostability. In addition, they exhibited excellent stability over a wide pH range (5-12) and high ionic strength (0.15-2.0M NaCl). As seen by confocal microscopy and magnetic resonance imaging, AgMn:In 2 S 3 /ZnS conjugated to hyaluronic acid (referred to as AgMn:In 2 S 3 /ZnS@HA) efficiently and specifically targeted cluster determinant 44, a receptor overexpressed on cancer cells. Moreover, AgMn:In 2 S 3 /ZnS@HA showed negligible cytotoxicity in vitro and in vivo, rendering it a promising diagnostic probe for dual-modal imaging in clinical applications. In this manuscript, we reported a facial and rapid method to prepare In 2 S 3 /ZnS core/shell quantum dots (QDs) co-doped with Ag + and Mn 2+ (referred to as AgMn:In 2 S 3 /ZnS). Ag + dopants were used to alter the optical properties of the In 2 S 3 host, whereas Mn 2+ co-dopants with their unpaired electrons provided paramagnetic properties. The emission wavelength of the core/shell QDs could be tuned from 550 to 743nm with a maximum PL quantum yield of 45%. The resulting core/shell QDs also maintained a stable emission in aqueous solution at broad ranges of pH (5-12) and ionic strength (0.15-2.0M NaCl), as well as a high photostability under continuous irradiation. In vivo cytotoxicity experiments showed that up to 500μg/mL AgMn:In 2 S 3 /ZnS@HA did not cause obvious toxicity to zebrafish embryos. In vitro targeted cell luminescence and magnetic resonance imaging showed that AgMn:In 2 S 3 /ZnS conjugated to hyaluronic acid was selectively and efficiently internalized in CD44-expressing tumor cells, confirming that the resultant QDs could function as dual-modal imaging probes for accurate diagnosis. Copyright © 2016 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

  12. Synthesis, characterization and ferromagnetic properties of Zn1-xMnxO (x ≤ 0.05) nanoparticles

    NASA Astrophysics Data System (ADS)

    Phuruangrat, Anukorn; Thongtem, Titipun; Thongtem, Somchai

    2018-06-01

    Zn1-xMnxO (x ≤ 0.05) nanoparticles were synthesized by a combination of room temperature precipitation and high temperature calcination. Pure hexagonal wurtzite ZnO nanoparticles with the size of ≤100 nm and a dominant vibrational peak at 437 cm-1 of E2H non-polar optical phonon mode were detected. The present research was succeeded in doping of ZnO lattice by Mn2+ ions, including the detection of an additional peak at 528 cm-1 associated with lattice defects. Magnetic properties of Zn1-xMnxO (x ≤ 0.05) nanoparticles were controlled by correlated spin of Mn-O-Mn exchange couple and lattice disorder. The saturation magnetization of ferromagnetic Zn0.97Mn0.03O was the highest at 51.49 × 10-3 emu/g.

  13. Solubility of polyvalent cations in fogwater at an urban site in Strasbourg (France)

    NASA Astrophysics Data System (ADS)

    Millet, M.; Wortham, H.; Mirabel, Ph.

    The concentrations in the soluble and total (soluble + insoluble) fractions of Mg, Ca, Fe, Mn, Zn, Al, Cd and Pb have been analysed by "inductively coupled plasma (ICP)" in 14 fog events collected in 1992 at an urban site in France (Strasbourg). For each fog event, two droplet size categories (2-6 μm and 5-8 μm) have been collected separately. For the analysis of the polyvalent cations in the soluble and total fractions, an analytical procedure using ICP and filtration on cellulose/PVC filters has been developed. The study of the solubility of some polyvalent cations has shown that two of the most important factors controlling the partitioning between the soluble and insoluble fraction are the nature of the particles and the pH of the fogwater. The influence of pH depended on the element. The solubility of Pb, Cd, Al, Fe, Mg, and Ca were pH dependent whereas, Zn and Mn solubility varied but no relationship with pH existed, ranging between 25 and 100% and 10 and 100%, respectively. On the other hand, Mg, Pb and Ca were predominantly present in the soluble phase, whereas Al was prevalent in the insoluble fraction. In the case of Cd and Fe., the presence in the soluble or insoluble phase depended largely on the fogwater pH.

  14. Use of geostatistics for assessing the concentration of heavy metals in a stretch of the River Apodi-Mossoro (Rio Grande do Norte State, Brazil).

    NASA Astrophysics Data System (ADS)

    Bezerra, J. M.; Siqueira, G. M.; Montenegro, A. A. A.; Silva, P. C. M.; Batista, R. O.

    2012-04-01

    The objective of this study was to assess the environmental changes with respect to the concentration of heavy metals in the sediment contained a stretch of the River Apodi-Mossoró (Rio Grande do Norte State, Brazil), considering changes in land use and soil. The sediment samples were collected at 30 points in the bed Apodi- Mossoró River in a section with features urban-rural town of Mossoró. The concentration of heavy metals in the sediment was determined using composite samples of surface sediments from the bottom with a depth of 20 cm, according to the methodology of APHAAWWA-WPCF (1998), where he subsequently held to determine the presence and quantity of metal concentration total by the technique of atomic absorption spectrometry, and analyzed the following heavy metals: aluminum(Al), cádmium (Cd), chromium (Cr), copper (Cu), iron (Fe), manganese (Mn), nickel (Ni), lead (Pb) and zinc (Zn). Data were analyzed using statistical and geostatistical. The geostatistical analysiswas performed by the construction of experimental semivariogramas self-assessment and adjustment by using the technique of Jack-kinifing. The elemento Cd was absent in the samples, which reduces the possibility of environmental contamination events. The average concentrations of the elements under study are within the limits proposed by the environmental legislation (National Environmental Council). However, for the elements Fe, Al and Mn no threshold values, because these are associated with the rocky material of geochemical origin. The elemento Fe had the highest range of values than the other, and all elements except for Zn and Cd showed the presence of outliers, suggesting the possibility that these points are listed as points liable to contribution by human activities. It was verified the presence of human influence, because the elements undergo an increase of concentration values from the point 11, which is located downstream of the urban bus consolidated. The experimental semivariogramas of elements Cu and Zn adjusted to the spherical model, while the elemen Fe was adjusted to the exponential model. The concentration of Mn is set to the Gaussian model, while the other elements (Al, Cr, Ni and Pb) showed pure nugget effect. The spatial variability of heavy metals analyzed in the study area has high spatial discontinuity, being influenced by the presence of human action, leading to the existence of trend in the semivariogram of the data of Al, Ni, Pb and Cr. Being derived values range from 350 m for Cu and Mn, Fe and 400 m to 425 m for Zn. It is recommended that future studies adopt a sampling grid with spacing less than 350 mand is expected to get a better response to the behavior of the spatial variability of the elements.

  15. X-ray absorption fine structure and X-ray excited optical luminescence studies of II-VI semiconducting nanostructures

    NASA Astrophysics Data System (ADS)

    Murphy, Michael Wayne

    2010-06-01

    Various II-VI semiconducting nanomaterials such as ZnO-ZnS nanoribbons (NRs), CdSxSe1-x nanostructures, ZnS:Mn NRs, ZnS:Mn,Eu nanoprsims (NPs), ZnO:Mn nanopowders, and ZnO:Co nanopowders were synthesized for study. These materials were characterized by techniques such as scanning electron microscopy, transmission electron microscopy, element dispersive X-ray spectroscopy, selected area electron diffraction, and X-ray diffraction. The electronic and optical properties of these nanomaterials were studied by X-ray absorption fine structure (XAFS) spectroscopy and X-ray excited optical luminescence (XEOL) techniques, using tuneable soft X-rays from a synchrotron light source. The complementary nature ofthe XAFS and XEOL techniques give site, element and chemical specific measurements which allow a better understanding of the interplay and role of each element in the system. Chemical vapour deposition (CVD) of ZnS powder in a limited oxygen environment resulted in side-by-side biaxial ZnO-ZnS NR heterostructures. The resulting NRs contained distinct wurtzite ZnS and wurtzite ZnO components with widths of 10--100 nm and 20 --500 nm, respectively and a uniform interface region of 5-15 nm. XAFS and XEOL measurements revealed the luminescence of ZnO-ZnS NRs is from the ZnO component. The luminescence of CdSxSe1-x nanostructures is shown to be dependent on the S to Se ratio, with the band-gap emission being tunable between that of pure CdS and CdSe. Excitation of the CdSxSe 1-x nanostructures by X-ray in XEOL has revealed new de-excitation channels which show a defect emission band not seen by laser excitation. CVD of Mn2+ doped ZnS results in nanostructures with luminescence dominated by the yellow Mn2+ emission due to energy transfer from the ZnS host to the Mn dopant sites. The addition of EuCl3 to the reactants in the CVD process results in a change in morphology from NR to NP. Zn1-xMnxO and Zn1-xCOxO nanopowders were prepared by sol-gel methods at dopant concentrations of 0, 1,3, and 10% and annealed at 400, 600 and 800°C in air. XAFS spectra show that low dopant concentrations and low processing temperatures limit the amount of secondary phase formation. The nanopowders did not show roomtemperature ferromagnetism and increased secondary phase formation increases the paramagnetic character of the hysteresis curves at 5°K. Keywords: X-ray absorption fine structures (XAFS), X-ray absorption near-edge structures (XANES), extended X-ray absorption fine structure (EXAFS), X-ray absorption spectroscopy(XAS), X-ray excited optical luminescence (XEOL), time-resolved, II-VI semiconductors, nanostructure, nanomaterial, nanoribbon, nanowire, nanopartic1e, heterostructure, ZnO, ZnS, ZnO-ZnS, CdS, CdSe, CdSSe, ZnO:Mn, ZnO:Co, ZnS:Mn, dilute magnetic semiconductor (DMS), dilute magnetic oxide (DMO), spintronics, magnetism, paramagnetism, ferromagnetism.

  16. Process optimization and leaching kinetics of zinc and manganese metals from zinc-carbon and alkaline spent batteries using citric acid reagent

    NASA Astrophysics Data System (ADS)

    Yuliusman; Amiliana, R. A.; Wulandari, P. T.; Huda, M.; Kusumadewi, F. A.

    2018-03-01

    Zn-Carbon and Alkaline spent batteries contains heavy metals, such as zinc and manganese, which can causes environmental problem if not handled properly. Usually the recovery of these metals were done by leaching method using strong acid, but the use of strong acids as leaching reagents can be harmful to the environment. This paper concerns the recovery of Zn and Mn metals from Zn-C and alkaline spent batteries with leaching method using citric acid as the environmental friendly leaching reagent. The leaching conditions using citric acid were optimized and the leaching kinetics of Zn and Mn in citric acid solution was investigated. The leaching of 89.62% Zn and 63.26% Mn was achieved with 1.5 M citric acid, 90°C temperature, and 90 minutes stirring time. Kinetics data for the dissolution of Zn showed the best fit to chemical control shrinking core model, while the diffusion controlled model was suitable for the dissolution of Mn kinetics data. The activation energy of 6.12 and 1.73 kcal/mol was acquired for the leaching of Zn and Mn in the temperature range 60°C-90°C.

  17. Factors affecting the partitioning of Cu, Zn and Pb in boulder coatings and stream sediments in the vicinity of a polymetallic sulfide deposit

    USGS Publications Warehouse

    Filipek, L.H.; Chao, T.T.; Carpenter, R.H.

    1981-01-01

    A sequential extraction scheme is utilized to determine the geochemical partitioning of Cu, Zn and Pb among hydrous Mn- and Fe-oxides, organics and residual crystalline silicates and oxides in the minus-80-mesh ( Fe-oxides > Mn-oxides; Zn, Mn-oxides {reversed tilde equals} organics > Fe-oxides; Pb, Fe-oxides > organics > Mn-oxides. In the sediments, organics are the most efficient scavengers of all three ore metals. These results emphasize the importance of organics as sinks for the ore metals, even in environments with high concentrations of Mn- and Fe-oxides. Of the ore metals, Zn appears to be the most mobile, and is partitioned most strongly into the coatings. However, anomaly contrast for hydromorphic Zn, normalized to the MnFe-oxide or organic content, is similar in sediments and coatings. Cu shows the highest anomaly on the boulder coatings, probably due to precipitation of a secondary Cu mineral. In contrast, detrital Pb in the pan concentrates shows a better anomaly than any hydromorphic Pb component. ?? 1981.

  18. Mineral phases and metals in baghouse dust from secondary ...

    EPA Pesticide Factsheets

    Baghouse dust (BHD) is a solid waste generated by air pollution control systems during secondary aluminum processing (SAP). Management and disposal of BHD can be challenging in the U.S. and elsewhere. In this study, the mineral phases, metal content and metal leachability of 78 BHD samples collected from 13 different SAP facilities across the U.S. were investigated. The XRD semi-quantitative analysis of BHD samples suggests the presence of metallic aluminum, aluminum oxide, aluminum nitride and its oxides, spinel, elpasolite as well as diaspora. BHD also contains halite, sylvite and fluorite, which are used as fluxes in SAP activities. Total aluminum (Al) in the BHD samples averaged 18% by weight. Elevated concentrations of trace metals (>100 µgL-1 As; >1000 µgL-1 Cu, Mn, Se, Pb, Mn and Zn) were also detected in the leachate. The U.S. toxicity characteristic leaching procedure (TCLP) results showed that some samples leached above the toxicity limit for Cd, Pb and Se. Exceeding the TCLP limits in all sample is independent of facilities generating the BHD. From the metal content perspective only, it appears that BHD has a higher potential to exhibit toxicity characteristics than salt cake (the largest waste stream generated by SAP facilities). The objective of this study was to investigate BHD from SAP facilities in the U.S. by determining the mineral phases and the metal (Al, As, Ca, Cd, Cr, Cu, Fe, K, Mg, Mn, Na, Pb, Se and Zn) content of the sample

  19. Replacement of a cytosolic copper/zinc superoxide dismutase by a novel cytosolic manganese superoxide dismutase in crustaceans that use copper (haemocyanin) for oxygen transport.

    PubMed Central

    Brouwer, Marius; Hoexum Brouwer, Thea; Grater, Walter; Brown-Peterson, Nancy

    2003-01-01

    The blue crab, Callinectes sapidus, which uses the copper-dependent protein haemocyanin for oxygen transport, lacks the ubiquitous cytosolic copper-dependent enzyme copper/zinc superoxide dismutase (Cu,ZnSOD) as evidenced by undetectable levels of Cu,ZnSOD activity, protein and mRNA in the hepatopancreas (the site of haemocyanin synthesis) and gills. Instead, the crab has an unusual cytosolic manganese SOD (cytMnSOD), which is retained in the cytosol, because it lacks a mitochondrial transit peptide. A second familiar MnSOD is present in the mitochondria (mtMnSOD). This unique phenomenon occurs in all Crustacea that use haemocyanin for oxygen transport. Molecular phylogeny analysis suggests the MnSOD gene duplication is as old as the origin of the arthropod phylum. cytMnSOD activity in the hepatopancreas changes during the moulting cycle of the crab. Activity is high in intermoult crabs and non-detectable in postmoult papershell crabs. mtMnSOD is present in all stages of the moulting cycle. Despite the lack of cytCu,ZnSOD, crabs have an extracellular Cu,ZnSOD (ecCu,ZnSOD) that is produced by haemocytes, and is part of a large, approx. 160 kDa, covalently-linked protein complex. ecCu,ZnSOD is absent from the hepatopancreas of intermoult crabs, but appears in this tissue at premoult. However, no ecCu,ZnSOD mRNA can be detected, suggesting that the protein is recruited from the haemolymph. Screening of different taxa of the arthropod phylum for Cu,ZnSOD activity shows that those crustaceans that use haemoglobin for oxygen transport have retained cytCu,ZnSOD. It appears, therefore, that the replacement of cytCu,ZnSOD with cytMnSOD is part of an adaptive response to the dynamic, haemocyanin-linked, fluctuations in copper metabolism that occur during the moulting cycle of the crab. PMID:12769817

  20. Imaging of single magnetic dopants in III-V semiconductor hosts

    NASA Astrophysics Data System (ADS)

    Koenraad, Paul; Celebi, Cem; Silov, Andrei; Yakunin, Andrei; Tang, Jian-Ming; Flatte, Michael; Kaminska, Maria

    2007-03-01

    We present room-temperature cross-sectional scanning tunneling microscopy (STM) topographic measurements of the acceptor state wave function for Mn dopants in InP and compare with measurements for the nonmagnetic dopants Zn and Cd as well as with previous results for Mn in GaAs[1]. We find a strongly anisotropic ``bow-tie'' shape for the Mn acceptor state wave function in InP, similar to Mn in GaAs, which has a binding energy of 210 meV (compared to 113 meV for Mn in GaAs). The shape for Mn in InP is more symmetric with respect to the 001 plane than Mn in GaAs, which agrees with a general trend for the magnetic and nonmagnetic acceptor state symmetry as a function of acceptor binding energy. We present a new theoretical model based on the surface strain of GaAs (110) that explains why the 001-plane asymmetry of acceptor states seen in STM measurements is much larger than expected from bulk calculations. [1] A. M. Yakunin, et al., Phys. Rev. Lett. 92, 216806 (2004).

  1. Recovery of manganese and zinc from waste Zn-C cell powder: Characterization and leaching.

    PubMed

    Biswas, Ranjit K; Karmakar, Aneek K; Kumar, Sree L; Hossain, Mohammad N

    2015-12-01

    A large number of waste Zn-C cells (Haquebrand) were broken down and collected as agglomerated powder. This powder was sun-dried, dry-ground and sieved down to 300 mesh size and stored. The sample was analysed and found to contain (35.4 ± 0.2)% Mn, (11.0 ± 0.1)% Zn and ∼ 2.5% Fe as major metallic constituents. The phases, ZnMn2O4 and Zn(ClO4)2 · 2H2O or MnO(OH) were identified in the hot water washed sample. The material was found to be leached effectively by a 2 mol/L sulfuric acid solution containing glucose (2g/L). However, the dissolution was dependent on (S/L) ratio; and the stage-wise leaching was not fruitful for Mn-dissolution. On leaching 5 g of powder (<53 μm) with a 250 mL of 0.5 g glucose containing 2 mol/L sulfuric acid solution (S/L=20 g/L), at 100°C and 300 rpm for 1h, a solution containing (7.08 ± 0.10)g/L Mn(2+), (2.20 ± 0.06) Zn(2+) and ∼ 0.40 g/L Fe(3+) was recovered corresponding to cent percent dissolutions of Zn and Mn and 80% dissolution of Fe. Copyright © 2015 Elsevier Ltd. All rights reserved.

  2. [Spatial variability and evaluation of soil heavy metal contamination in the urban-transect of Shanghai].

    PubMed

    Liu, Yun-Long; Zhang, Li-Jia; Han, Xiao-Fei; Zhuang, Teng-Fei; Shi, Zhen-Xiang; Lu, Xiao-Zhe

    2012-02-01

    Soil heavy metal concentrations along the typical urban-transect in Shanghai were analyzed to indicate the effect of urbanization and industrialization on soil environment quality. Spatial variation structure and distribution of 5 heavy metals (Cu, Cr, Mn, Pb and Zn) in the top soil of urban-transect were analyzed. The single pollution index and the composite pollution index were used to evaluate the soil heavy metal pollution. The results showed that the average concentrations of the Cu, Pb, Zn, Cr, Mn were 27.80, 28.86, 99.36, 87.72, 556.97 mg x kg(-1), respectively. Cu, Cr, Mn, Pb and Zn were medium in variability, Mn was distributed lognormally, while Cu, Cr, Pb and Zn were distributed normally. The results of semivariance analysis showed that Mn was fit for the exponential model, Cr, Pb, Cu and Zn were fit for the linear model. The spatial distribution maps of heavy metal content of the topsoil in this city-transect were produced by means of the universal kriging interpolation. Cu was spatially distributed in ribbon, Cr and Mn were distributed in island, while the spatial distribution of Pb and Zn showed the mixed characteristic of ribbon and island. With the result of soil pollution evaluation, it showed that the pollution of Cr, Zn and Pb was relatively severe. Cr, Zn, Pb, Mn and Cu were significantly correlated, and heavy metal co-contamination existed in soil. Difference of soil heavy metals pollution along "Urban-suburban-rural" was obvious, the special variation of heavy metal concentrations in the soil closely related to the degree of industrialization and urbanization of the city.

  3. Phosphorescent quantum dots/ethidium bromide nanohybrids based on photoinduced electron transfer for DNA detection.

    PubMed

    Bi, Lin; Yu, Yuan-Hua

    2015-04-05

    Mercaptopropionic acid-capped Mn-doped ZnS quantum dots/ethidium bromide (EB) nanohybrids were constructed for photoinduced electron transfer (PIET) and then used as a room-temperature phosphorescence (RTP) probe for DNA detection. EB could quench the RTP of Mn-doped ZnS QDs by PIET, thereby forming Mn-doped ZnS QDs/EB nanohybrids and storing RTP. Meanwhile, EB could be inserted into DNA and EB could be competitively desorbed from the surface of Mn-doped ZnS QDs by DNA, thereby releasing the RTP of Mn-doped ZnS QDs. Based on this mechanism, a RTP sensor for DNA detection was developed. Under optimal conditions, the detection limit for DNA was 0.045 mg L(-1), the relative standard deviation was 1.7%, and the method linear ranged from 0.2 to 20 mg L(-1). The proposed method was applied to biological fluids, in which satisfactory results were obtained. Copyright © 2015 Elsevier B.V. All rights reserved.

  4. Dissociation kinetics of Mn2+ complexes of NOTA and DOTA.

    PubMed

    Drahoš, Bohuslav; Kubíček, Vojtěch; Bonnet, Célia S; Hermann, Petr; Lukeš, Ivan; Tóth, Éva

    2011-03-07

    The kinetics of transmetallation of [Mn(nota)](-) and [Mn(dota)](2-) was investigated in the presence of Zn(2+) (5-50-fold excess) at variable pH (3.5-5.6) by (1)H relaxometry. The dissociation is much faster for [Mn(nota)](-) than for [Mn(dota)](2-) under both experimental and physiologically relevant conditions (t(½) = 74 h and 1037 h for [Mn(nota)](-) and [Mn(dota)](2-), respectively, at pH 7.4, c(Zn(2+)) = 10(-5) M, 25 °C). The dissociation of the complexes proceeds mainly via spontaneous ([Mn(nota)](-)k(0) = (2.6 ± 0.5) × 10(-6) s(-1); [Mn(dota)](2-)k(0) = (1.8 ± 0.6) × 10(-7) s(-1)) and proton-assisted pathways ([Mn(nota)](-)k(1) = (7.8 ± 0.1) × 10(-1) M(-1) s(-1); [Mn(dota)](2-)k(1) = (4.0 ± 0.6) × 10(-2) M(-1) s(-1), k(2) = (1.6 ± 0.1) × 10(3) M(-2) s(-1)). The observed suppression of the reaction rates with increasing Zn(2+) concentration is explained by the formation of a dinuclear Mn(2+)-L-Zn(2+) complex which is about 20-times more stable for [Mn(dota)](2-) than for [Mn(nota)](-) (K(MnLZn) = 68 and 3.6, respectively), and which dissociates very slowly (k(3)∼10(-5) M(-1) s(-1)). These data provide the first experimental proof that not all Mn(2+) complexes are kinetically labile. The absence of coordinated water makes both [Mn(nota)](-) and [Mn(dota)](2-) complexes inefficient for MRI applications. Nevertheless, the higher kinetic inertness of [Mn(dota)](2-) indicates a promising direction in designing ligands for Mn(2+) complexation.

  5. Environmental exposures of trace elements assessed using keratinized matrices from patients with chronic kidney diseases of uncertain etiology (CKDu) in Sri Lanka.

    PubMed

    Diyabalanage, Saranga; Fonseka, Sanjeewani; Dasanayake, D M S N B; Chandrajith, Rohana

    2017-01-01

    An alarming increase in chronic kidney disease with unknown etiology (CKDu) has recently been reported in several provinces in Sri Lanka and chronic exposures to toxic trace elements were blamed for the etiology of this disease. Keratinized matrices such as hair and nails were investigated to determine the possible link between CKDu and toxic element exposures. Elements Li, B, Al, Cr, Mn, Fe, Co, Ni, Cu, Zn, As, Se, Sr, Mo, Cd, Ba, Hg and Pb of hair and nails of patients and age that matched healthy controls were determined with Inductively Coupled Plasma Mass Spectrometry (ICP-MS). The results showed that trace element contents in the hair of patients varies in the order of Zn>Fe>Al>Mn>Cu>Ba>Sr>Ni>Pb>Cr>B>Hg>Se>Mo>Co>As>Li>Cd while Fe>Al>Zn>Ni>Cu>Mn>Cr>Ba>Sr>B>Pb>Se>Mo>Co>Hg>Li>As>Cd in nail samples. The hair As levels of 0.007-0.165μgg -1 were found in CKDu subjects. However, no significant difference was observed between cases and controls. The total Se content in hair of CKDu subjects ranged from 0.043 to 0.513μgg -1 while it was varied from 0.031 to 1.15μgg -1 in controls. Selenium in nail samples varied from 0.037μgg -1 to 4.10μgg -1 in CKDu subjects and from 0.042μgg -1 to 2.19μgg -1 in controls. This study implies that substantial proportions of Sri Lankan population are Se deficient irrespective of gender, age and occupational exposure. Although some cutaneous manifestations were observed in patient subjects, chemical analyses of hair and nails indicated that patients were not exposed to toxic levels of arsenic or the other studied toxic elements. Therefore the early suggested causative factors such as exposure to environmental As and Cd, can be ruled out. Copyright © 2016 Elsevier GmbH. All rights reserved.

  6. Substrate temperature effects on the structure and properties of ZnMnO films prepared by pulsed laser deposition

    NASA Astrophysics Data System (ADS)

    Riascos, H.; Duque, J. S.; Orozco, S.

    2017-01-01

    ZnMnO thin films were grown on silicon substrates by pulsed laser deposition (PLD). Pulsed Nd:YAG laser was operated at a wavelength of 1064 nm and 100 mJ. ZnMnO thin films were deposited at the vacuum pressure of 10-5 Torr and with substrate temperature from room temperature to 600 °C. The effects of substrate temperature on the structural and Optical properties of ZnMnO thin films have been investigated by X-ray diffraction (XRD), Raman spectroscopy and Uv-vis spectroscopy. From XRD data of the samples, it can be showed that temperature substrate does not change the orientation of ZnMnO thin films. All the films prepared have a hexagonal wurtzite structure, with a dominant (002) peak around 2θ=34.44° and grow mainly along the c-axis orientation. The substrate temperature improved the crystallinity of the deposited films. Uv-vis analysis showed that, the thin films exhibit high transmittance and low absorbance in the visible region. It was found that the energy band to 300 ° C is 3.2 eV, whereas for other temperatures the values were lower. Raman reveals the crystal quality of ZnMnO thin films.

  7. Electronic structure and linear optical properties of ZnSe and ZnSe:Mn.

    PubMed

    Su, Kang; Wang, Yuhua

    2010-03-01

    As an important wide band-gap II-VI semiconductor, ZnSe has attracted much attention for its various applications in photo-electronic devices such as blue light-emitting diodes and blue-green diode lasers. Mn-doped ZnSe is an excellent quantum dot material. The electronic structures of the sphalerite ZnSe and ZnSe:Mn were calculated using the Vienna ab initio Simulation Package with ultra-soft pseudo potentials and Material Studio. The calculated equilibrium lattice constants agree well with the experimental values. Using the optimized equilibrium lattice constants, the densities of states and energy band structures were further calculated. By analyzing the partial densities of states, the contributions of different electron states in different atoms were estimated. The p states of Zn mostly contribute to the top of the valence band, and the s states of Zn and the s states of Se have major effects on the bottom of the conduction band. The calculated results of ZnSe:Mn show the band gap was changed from 2.48 to 1.1 eV. The calculated linear optical properties, such as refractive index and absorption spectrum, are in good agreement with experimental values.

  8. Triple-mixture of Zn, Mn, and Fe increases bioaccumulation and causes oxidative stress in freshwater neotropical fish.

    PubMed

    de Oliveira, Luciana Fernandes; Santos, Caroline; Risso, Wagner Ezequiel; Dos Reis Martinez, Claudia Bueno

    2018-06-01

    Metal bioaccumulation and oxidative stress biomarkers were determined in Prochilodus lineatus to understand the effects of short-term exposure to a triple-mixture of Zn, Mn, and Fe. Three independent tests were carried out, in which fish were exposed to 3 concentrations of Zn (0.18, 1.0, and 5.0 mg L -1 ), Mn (0.1, 0.5, and 5.0 mg L -1 ), and in the mix test to Fe (5.0 mg L -1 ) and a mixture of Zn (1.0 mg L -1 ) + Mn (0.5 mg L -1 ), with and without Fe. After exposure for 96 h, tissues were removed for metal bioaccumulation analysis and oxidative stress biomarkers were determined in liver, along with DNA damage in blood cells. Our results revealed that Zn and Mn were bioaccumulated in fish tissues after exposure to 5.0 mg L -1 , whereas Fe only bioaccumulated in muscle and gills after mixture exposure. Results indicated that 1 metal interfered with the other's bioaccumulation. In P. lineatus, 5 mg L -1 of both Mn and Fe were toxic, because damage was observed (lipid peroxidation [LPO] in liver and DNA damage in blood cells), whereas Zn induced liver responses (metallothionein [MT] and reduced glutathione [GSH] increases) to prevent damage. In terms of bioaccumulation and alterations of oxidative stress biomarkers, we showed that Zn, Mn, and Fe triple-mixture enhances individual metal toxicity in Neotropical fish P. lineatus. Environ Toxicol Chem 2018;37:1749-1756. © 2018 SETAC. © 2018 SETAC.

  9. Assessment of trace metals contamination in the coastal sediments of the Egyptian Mediterranean coast

    NASA Astrophysics Data System (ADS)

    El Baz, Sherif M.; Khalil, Mohamed M.

    2018-07-01

    Trace metals contamination has been recently increased in the Egyptian Mediterranean coast owing to the nearby anthropological activities. This investigation aimed to detect the concentrations of six different trace metals (Fe, Mn, Cu, Cd, Pb and Zn) in surface sediments from the central part of the Egyptian Mediterranean coast, and to assess their state of contamination from different indices and risk factor calculations. Mean concentrations of Cu, Pb and Zn were lower and the mean concentration of Cd was higher compared to the background values. The assessment of pollution was mainly based on the contamination indices. Based on the contamination factor, Pb was the most enriched element followed by Cd, Mn, Zn and Cu. Most of the sites show low contamination with respect to Pb, Mn, Cd, Fe, Zn and Cu. The pollution load index also suggests that all the coastal sediments are unpolluted. According to the geoaccumulation index, the sediments were classified into unpolluted with Mn, Cd, Fe and Pb, and unpolluted to moderately polluted with Pb. Risk evaluation revealed that Cd had the greatest ecological risk, followed by Pb, Cu, Mn, while Zn had the lowest risk. With the aid of statistical methods, the origin of metals is classified into two clusters (A and B). Group A consists of Fe, Mn and Cu, whereas group B contains Zn, Pb and Cd. In the first cluster Fe and Mn are joined to each other at a positive and significant similarity (0.68). Fe is recognized as an indicator of lithogenous origin, therefore, its higher similarity with Mn may be indicative of the similar origin for Manganese. In the second cluster Pb and Zn are joined to each other at a positive and significant similarity (0.80). Pb is recognized as an indicator of anthropogenic origin, therefore, its higher similarity with Zn may be indicative of the similar origin for Zinc.

  10. Efficacy of heat generation in CTAB coated Mn doped ZnFe2O4 nanoparticles for magnetic hyperthermia

    NASA Astrophysics Data System (ADS)

    Raland, R. D.; Borah, J. P.

    2017-01-01

    Manganese doped Zinc ferrite (Mn-ZnFe2O4, where Mn  =  0%, 3%, 5% and 7%) nanoparticles were synthesized by a simple co-precipitation method. CTAB (cetyltrimethylammonium bromide) was used as a surfactant to inhibitgrowth and agglomeration. In this work, we have discussed on the influence of CTAB and Mn doping in tailoring the structural and magnetic properties of Mn-ZnFe2O4 nanoparticles for the effective application of magnetic hyperthermia. X-ray diffraction (XRD) pattern confirmed the formation of cubic spinel structure of Mn-ZnFe2O4 nanoparticles. Lattice parameter and x-ray densities were obtained from the Rietveld refinement of the XRD pattern. The presence of CTAB as a stabilizing layer adsorbed on the surface of the nanoparticles were confirmed by transmission electron microscope (TEM) and Raman vibrational spectrum. The saturation magnetization showsan increasing trend with Mn addition owing to cationic re-distribution and an increase super-exchange interaction between the two sub-lattices. Superparamagnetic behaviorof Mn-ZnFe2O4 nanoparticles were confirmed by temperature-dependent zero-field-cooling (ZFC) and field-cooling (FC) magnetization curves. The efficiency of induction heating measured by its specific absorption rate (SAR) and intrinsic loss power (ILP) value varies as a function of saturation magnetization. It has been hypothesized that the maximum generation of heat arises from Neel relaxation mechanism. The optimum generation of heat of Mn-ZnFe2O4 nanoparticle is determined by the higher frequency (f  =  337 kHz) range and maximum concentration of Mn doping.

  11. Merely two mutations switch a DNA-hydrolyzing deoxyribozyme from heterobimetallic (Zn2+/Mn2+) to monometallic (Zn2+-only) behavior

    PubMed Central

    Xiao, Ying; Allen, Emily C.

    2012-01-01

    A deoxyribozyme that hydrolyzes DNA phosphodiester linkages with a requirement for both Zn2+ and Mn2+ is switched by only two nucleotide mutations to require Zn2+ alone, demonstrating that DNA-catalyzed DNA hydrolysis can be achieved using only one metal ion cofactor. PMID:21125108

  12. New diluted ferromagnetic semiconductor with Curie temperature up to 180 K and isostructural to the '122' iron-based superconductors.

    PubMed

    Zhao, K; Deng, Z; Wang, X C; Han, W; Zhu, J L; Li, X; Liu, Q Q; Yu, R C; Goko, T; Frandsen, B; Liu, Lian; Ning, Fanlong; Uemura, Y J; Dabkowska, H; Luke, G M; Luetkens, H; Morenzoni, E; Dunsiger, S R; Senyshyn, A; Böni, P; Jin, C Q

    2013-01-01

    Diluted magnetic semiconductors have received much attention due to their potential applications for spintronics devices. A prototypical system (Ga,Mn)As has been widely studied since the 1990s. The simultaneous spin and charge doping via hetero-valent (Ga(3+),Mn(2+)) substitution, however, resulted in severely limited solubility without availability of bulk specimens. Here we report the synthesis of a new diluted magnetic semiconductor (Ba(1-x)K(x))(Zn(1-y)Mn(y))(2)As(2), which is isostructural to the 122 iron-based superconductors with the tetragonal ThCr(2)Si(2) (122) structure. Holes are doped via (Ba(2+), K(1+)) replacements, while spins via isovalent (Zn(2+),Mn(2+)) substitutions. Bulk samples with x=0.1-0.3 and y=0.05-0.15 exhibit ferromagnetic order with T(C) up to 180 K, which is comparable to the highest T(C) for (Ga,Mn)As and significantly enhanced from T(C) up to 50 K of the '111'-based Li(Zn,Mn)As. Moreover, ferromagnetic (Ba,K)(Zn,Mn)(2)As(2) shares the same 122 crystal structure with semiconducting BaZn(2)As(2), antiferromagnetic BaMn(2)As(2) and superconducting (Ba,K)Fe(2)As(2), which makes them promising for the development of multilayer functional devices.

  13. Molecular controls on Cu and Zn isotopic fractionation in Fe-Mn crusts

    NASA Astrophysics Data System (ADS)

    Little, S. H.; Sherman, D. M.; Vance, D.; Hein, J. R.

    2014-06-01

    The isotopic systems of the transition metals are increasingly being developed as oceanic tracers, due to their tendency to be fractionated by biological and/or redox-related processes. However, for many of these promising isotope systems the molecular level controls on their isotopic fractionations are only just beginning to be explored. Here we investigate the relative roles of abiotic and biotic fractionation processes in controlling modern seawater Cu and Zn isotopic compositions. Scavenging to Fe-Mn oxides represents the principal output for Cu and Zn to sediments deposited under normal marine (oxic) conditions. Using Fe-Mn crusts as an analogue for these dispersed phases, we investigate the phase association and crystal chemistry of Cu and Zn in such sediments. We present the results of an EXAFS study that demonstrate unequivocally that Cu and Zn are predominantly associated with the birnessite (δ-MnO2) phase in Fe-Mn crusts, as previously predicted from sequential leaching experiments (e.g., Koschinsky and Hein, 2003). The crystal chemistry of Cu and Zn in the crusts implies a reduction in coordination number in the sorbed phase relative to the free metal ion in seawater. Thus, theory would predict equilibrium fractionations that enrich the heavy isotope in the sorbed phase (e.g., Schauble, 2004). In natural samples, Fe-Mn crusts and nodules are indeed isotopically heavy in Zn isotopes (at ∼1‰) compared to deep seawater (at ∼0.5‰), consistent with the predicted direction of equilibrium isotopic fractionation based on our observations of the coordination environment of sorbed Zn. Further, ∼50% of inorganic Zn‧ is chloro-complexed (the other ∼50% is present as the free Zn2+ ion), and complexation by Cl- is also predicted to favour equilibrium partitioning of light Zn isotopes into the dissolved phase. The heavy Zn isotopic composition of Fe-Mn crusts and nodules relative to seawater can therefore be explained by an inorganic fractionation during uptake. However, Cu in Fe-Mn crusts is isotopically light (at ∼0.3 to 0.5‰) compared to the dissolved phase in seawater (at ∼0.9‰). We suggest that this is because dissolved Cu in the oceans is overwhelmingly complexed to strong organic ligands, which are better competitors for the heavy isotope.

  14. Electronic structure, optical and magnetic studies of PLD-grown (Mn, P)-doped ZnO nanocolumns at room temperature

    NASA Astrophysics Data System (ADS)

    Phan, The-Long; Ho, T. A.; Dang, N. T.; Nguyen, Manh Cuong; Dao, Van-Duong

    2017-07-01

    We prepared well-aligned Zn1-x Mn x O:yP nanocolumns (x  =  0-0.02, and y  =  0 and 1 mol%) on SiO2/Si(0 0 1) substrates by using pulsed laser deposition (PLD) and then investigated their electronic structure and optical and magnetic properties at room temperature. The analyses of x-ray photoelectron and x-ray absorption fine structure spectra revealed Mn2+ and/or P ions existing in nanocolumns, where Mn2+ ions are situated in the Zn2+ site of the ZnO-wurtzite structure. Although the incorporation of Mn2+ and/or P ions did not form secondary phases, as confirmed by x-ray and electron diffraction patterns, more lattice defects were created, and consequently changed the band-gap energy as well as the electron-phonon interactions in the nanocolumns. Magnetization versus magnetic-field measurements revealed that all the samples exhibited FM order. In particular, the (Mn, P) co-doping with x  =  0.02 and y  =  1 remarkably enhanced the magnetic moment up to 2.92 µ B/Mn. Based on the results obtained from analyzing the electronic structures, UV-Vis absorption and resonant Raman scattering spectra, and theoretical calculations, we believe that the enhancement of the FM order in (Mn, P)-doped ZnO nanocolumns is due to exchange interactions taking place between vacancy-mediated Mn2+ ions.

  15. [Determination of 22 inorganic elements in different parts of Lantana camara by ICP-OES].

    PubMed

    Zhou, Wei-ming; Wang, Ru-yi; Chen, Liu-sheng; Huang, Chuan-bin

    2014-10-01

    To determine the contents of 22 inorganic elements in different parts of Lantana camara by inductively coupled plasma optical emission spectroscopy (ICP-OES). HNO3-H2O2 digested system was used to completely decompose the organic compounds effectually by microwave digestion. The 22 inorganic elements such as K, Ca, Mg, Fe, Al, Na, Zn, Mn and Cr were determined by ICP-OES under set up working conditions. The contents of K, Ca and Mg were the most in different parts of Lantana camara; The contents of K, Ca, Mg, Mn, Sr and Cu in the leaf were more those that in the root and branch; The contents of Fe, Na, Cr and Ni in the root were more than those in the leaf and branch; The contents of Mn, Zn, Sr and Cu in the branch were more than those in the root and the leaf; The contents of Pb and Cd were higher than the national standard and Cr had high content in different parts of Lantana camara. The determination method is quick, easy and accurate with high sensitivity, which can determine the contents of 22 inorganic elements accurately in different parts of Lantana camara.

  16. Mineralogic sources of metals in leachates from the weathering of sedex, massive sulfide, and vein deposit mining wastes

    USGS Publications Warehouse

    Diehl, S.F.; Hageman, P.L.; Seal, R.R.; Piatak, N.M.; Lowers, H.

    2011-01-01

    Weathered mine waste consists of oxidized primary minerals and chemically unstable secondary phases that can be sources of readily soluble metals and acid rock drainage. Elevated concentrations of metals such as Cd, Cu, Fe, Mn, Ni, Pb, and Zn are observed in deionized water-based leachate solutions derived from complex sedex and Cu-Pb-Zn mine wastes. Leachate (USGS FLT) from the Elizabeth mine, a massive sulfide deposit, has a pH of 3.4 and high concentrations of Al (16700 ug/L), Cu (440 ug/L), and Zn (8620 ug/L). Leachate from the sedex Faro mine has a pH of 3.5 and high concentrations of Al (2040 ug/L), Cu (1930 ug/L), Pb (2080 ug/L), and Zn (52900 ug/L). In contrast, higher-pH leachates produced from tailings of polymetallic vein deposits have order of magnitude lower metal concentrations. These data indicate that highly soluble secondary mineral phases exist at the surface of waste material where the samples were collected. Sulfide minerals from all sites exhibit differential degrees of weathering, from dissolution etched grain rims, to rinds of secondary minerals, to skeletal remnants. These microscale mineral-dissolution textures enhance weathering and metal teachability of waste material. Besides the formation of secondary minerals, sulfide grains from dried tailings samples may be coated by amorphous Fe-Al-Si minerals that also adsorb metals such as Cu, Ni, and Zn.

  17. Origin and chemical composition of the amorphous material from the intergrain pores of self-assembled cubic ZnS:Mn nanocrystals

    NASA Astrophysics Data System (ADS)

    Stefan, Mariana; Vlaicu, Ioana Dorina; Nistor, Leona Cristina; Ghica, Daniela; Nistor, Sergiu Vasile

    2017-12-01

    We have shown in previous investigations that the low temperature collective magnetism observed in mesoporous cubic ZnS:Mn nanocrystalline powders prepared by colloidal synthesis, with nominal doping concentrations above 0.2 at.%, is due to the formation of Mn2+ clusters with distributed antiferromagnetic coupling localized in an amorphous phase found between the cubic ZnS:Mn nanocrystals. Here we investigate the composition, origin and thermal annealing behavior of this amorphous phase in such a mesoporous ZnS:Mn sample doped with 5 at.% Mn nominal concentration. Correlated analytical transmission electron microscopy, multifrequency electron paramagnetic resonance and Fourier transform infrared spectroscopy data show that the amorphous nanomaterial consists of unreacted precursor hydrated zinc and manganese acetates trapped inside the pores and on the surface of the cubic ZnS nanocrystals. The decomposition of the acetates under isochronal annealing up to 270 °C, where the mesoporous structure is still preserved, lead to changes in the nature and strength of the magnetic interactions between the aggregated Mn2+ ions. These results strongly suggest the possibility to modulate the magnetic properties of such transition metal ions doped II-VI mesoporous structures by varying the synthesis conditions and/or by post-synthesis thermochemical treatments.

  18. Vascular plants as ecological indicators of metals in alpine vegetation (Karkonosze, SW Poland).

    PubMed

    Wojtuń, Bronisław; Samecka-Cymerman, Aleksandra; Żołnierz, Ludwik; Rajsz, Adam; Kempers, Alexander J

    2017-08-01

    Calluna vulgaris, Carex rigida, Deschampsia flexuosa, Nardus stricta and Vaccinium myrtillus are abundant in the vegetation of mountainous areas in Northern and Central Europe. Knowledge of their ability to accumulate increased amounts of metals could be useful in the evaluation of environmental pollution in the alpine tundra of high mountains. Additionally, this investigation may contribute to understanding the rate and direction of recent vegetation change in Karkonosze and similar types of environments. Our investigation revealed that Carex rigida, C. vulgaris and V. myrtillus contain excessive Mn concentrations in shoots with the highest BF for this element compared to the BFs of other elements. C. rigida, with Cu, Mn and Zn concentrations exceeding the toxicity thresholds for plants, seems to be the best metal phytoaccumulator for Nardus stricta grasslands Carici (rigidae)-Nardetum (CrN) and alpine heathlands Carici (rigidae)-Festucetum airoidis (CrFa) associations in the Karkonosze. Based on relevant BFs >1, it can be stated that the following plant available metals were transferred to shoots: Cu, Mn and Ni by C. vulgaris; Cd, Cu, Mn, Ni and Zn by C. rigida; Cd, Cu, Mn, Ni and Zn by D. flexuosa; Cu, Mn, Ni and Zn by N. stricta and Cu, Mn and Zn by V. myrtillus.

  19. A simplified soil extraction sequence to monitor the main and trace element speciation in soil after compost and mineral fertilizer additions upon the composition of wheat grains

    NASA Astrophysics Data System (ADS)

    Sager, Manfred; Erhart, Eva

    2016-04-01

    High quality biological waste treatment aims at producing compost in order to maintain a clean environment and to sustain soil organic carbon levels. Fertilization with compost as a source of organic carbon, nutrients, and accessory elements, as well as fertilization with mineral N- and PK fertilizer have been tested in a field experiment on a calcaric Fluvisol in the Danube wetlands, at 4 levels each. Yields of wheat were recorded, and grains and soils were sampled from each treatment, and analyzed for main and trace element composition. The corresponding soils were characterized by mobile phases, obtained by leaching with 0,16M acetic acid to cover exchangeables plus carbonates, and subsequently by 0,1M oxalate buffer pH 3 to dissolve the pedogenic oxides. Total amounts were obtained from digests with perchloric- nitric-hydrofluoric acid. For quasi-total amounts, aqua regia was replaced by pressure decomposition with KClO3 in dilute nitric acid. The proposed extraction sequence permits to analyze and interpret soil for main elements, trace elements, nutrients and anions simultaneously. Factor analyses of soil extracts obtained from dilute acetic acid revealed Ba-Be-Cd-Cu-Li-S (traces), Ca-Mg-Mn (main carbonates), Al-Fe-B, Y, and P-K (nutrients) as chemically feasible principal components. Subsequent soil extracts from oxalate contained Al-B-Co-K-Na-Pb-Si-V-S (maybe acid silicate weathering), Cr-Li-Ni-Sr-Ti (maybe basic silicate weathering), Be-Cu-Fe-P, Co-Mg-Mn-Zn (Mn-oxides) and Ba-Sc as principal components. Factor analyses of total element data distinguished the principal components Ce-La-Li-Sc-Y-P (rare earths), Al-Ca-Fe-K-Mg-Na-P (main elements), Cd-Co-Cr-Cu-Ni-Zn (trace elements), As-Pb (contaminants), Ba-Mn-Sr, and Ti, which looks chemically feasible also. Factor analyses of those soil fractions which presumably form the main fractions of exchangeables, carbonates, pedogenic oxides and silicates, showed no cross connections, except for P. Oxalate-soluble Fe together with P and S was independent from oxalate-soluble Al-Mn-Si. In the crops, all element levels were within a non-contaminated and non-deficient range, therefore correlations with concentrations as well as loads in the wheat grains where largely not pronounced. Maximum correlations between plant and soil data were obtained with Li and Be. The load data (concentration times yield, given in g/ha) were much more intercorrelated than the concentrations. Regarding the same element, correlation coefficients between loads and respective concentrations were larger than 0,800 for Al, Ba, Cd, Co, Cr, Li, Mo, Na, Ni, Se, and Sr, which means the transfer remained independent from the load. In case of Ca, Mg, P, S, Zn, however, correlation coefficients between loads and concentrations were < 0,500, thus the transfer was not constant because of obvious metabolic influences. The proposed method of soil characterization was applied at a field trial here for the first time, and offers new possibilities of intercorrelations between plant uptake and geochemical soil fractions.

  20. Compensation effect of bacterium containing biofertilizer on the growth of Cucumis sativus L. under Al-stress conditions.

    PubMed

    Tóth, Brigitta; Lévai, L; Kovács, B; Varga, Mária Borbélyné; Veres, Szilvia

    2013-03-01

    Biofertilizers are used to improve soil fertility and plant production in sustainable agriculture. However, their applicability depends on several environmental parameters. The aim of our study was to evaluate the effect of free-living bacteria containing fertilizer on the growth of cucumber (Cucumis sativus L. cvs. Delicates) under aluminium (Al) stress. Different responses to Al stress of cucumber growth parameters were examined in terms of root elongation and physiological traits, such as Spad index (relative chlorophyll value), biomass accumulation of root and shoot, Al uptake and selected element contents (Fe, Mn, Zn, Mg) of leaves and root. The applied bacteria containing biofertilizer contains Azotobacter chroococcum and Bacillus megaterium. The dry weights of cucumber shoots and roots decreased in line with the increasing Al concentration. Due to different Al treatments (10-3 M, 10-4 M) higher Al concentration was observed in the leaves, while the amounts of other elements (Fe, Mn, Zn, Mg) decreased. This high Al content of the leaves decreased below the control value when biofertilizer was applied. In the case of the roots the additional biofertilizer treatments compensated the effect of Al. The relative chlorophyll content was reduced during Al-stress in older plants and the biofertilizer moderated this effect. The root/shoot ratio was decreased in all the Al-treatments in comparison to the control. The living bacteria containing fertilizer also had a modifying effect. The root/shoot ratio increased at the 10-4 M Al2(SO4)2 + biofertilizer and 10-4 M Al(NO3)3 + biofertilizer treatments compared to the control and Al-treatments. According to our results the biofertilizer is an alternative nutrient supply for replacing chemical fertilizers because it enhances dry matter production. Biofertilizer usage is also offered under Al polluted environmental conditions. Although, the nutrient solution is a clean system where we can examine the main processes without other effects of natural soils. The soil can modify the results, e.g. the soil-born microorganisms affect nutrient availability, and also can modify the harmful effects of different heavy metals. The understanding of basic processes will help us to know more about the soil behaviour.

  1. Luminescence Characteristics of ZnGa2O4 Thick Film Doped with Mn2+ and Cr3+ at Various Sintering Temperatures

    NASA Astrophysics Data System (ADS)

    Cha, Jae Hyeok; Kim, Kyung Hwan; Park, Yong Seo; Kwon, Sang Jik; Choi, Hyung Wook

    2007-10-01

    ZnGa2O4 phosphor separately doped with Mn2+ and Cr3+ was synthesized by solid-state reaction, and thick films were deposited by screen printing. The X-ray diffraction (XRD) patterns of ZnGa2O4 phosphor thick films show a (311) main peak and a spinal phase. Uniform distribution and filled morphology of the doped ZnGa2O4 phosphor thick films were formed at the sintering temperature of 1100 °C. The CL spectrum of Mn2+-doped ZnGa2O4 shows the main peak of 512 nm green emission with the 4T1→6A1 transition of Mn2+ ions and the CL spectrum of Cr3+-doped ZnGa2O4 shows the main peak of 716 nm red emission with the 2E→4A2 transition of Cr3+ ions.

  2. Boric acid flux synthesis, structure and magnetic property of MB₁₂O₁₄(OH)₁₀ (M=Mn, Fe, Zn)

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Yang, Dingfeng; Cong, Rihong; Gao, Wenliang, E-mail: gaowl@cqu.edu.cn

    2013-05-01

    Three new borates MB₁₂O₁₄(OH)₁₀ (M=Mn, Fe, Zn) have been synthesized by boric acid flux methods, which are isotypic to NiB₁₂O₁₄(OH)₁₀. Single-crystal XRD was performed to determine the crystal structures in detail. They all crystallize in the monoclinic space group P2₁/c. The size of MO{sub 6} (M=Mg, Mn, Fe, Co, Ni, Zn) octahedron shows a good agreement with the Shannon effective ionic radii of M²⁺. Magnetic measurements indicate MnB₁₂O₁₄(OH)₁₀ is antiferromagnetic without a long-range ordering down to 2 K. The values of its magnetic superexchange constants were evaluated by DFT calculations, which explain the observed magnetic behavior. The UV–vis diffuse reflectancemore » spectrum of ZnB₁₂O₁₄(OH)₁₀ suggests a band gap ~4.6 eV. DFT calculations indicate it has a direct band gap 4.9 eV. The optical band gap is contributed by charge transfers from the occupied O 2p to the unoccupied Zn 4s states. - Graphical abstract: Experimental and theoretical studies indicate MnB₁₂O₁₄(OH)₁₀ is antiferromagnetic without a long-range ordering. DFT calculations show ZnB₁₂O₁₄(OH)₁₀ has a direct band gap of 4.9 eV. Highlights: • MB₁₂O₁₄(OH)₁₀ (M=Mn, Fe, Zn) are synthesized by two-step boric acid flux method. • Single-crystal XRD was performed to determine the crystal structures in detail. • Size of MO₆ (M=Mg, Mn, Fe, Co, Ni, Zn) agrees with the effective ionic radii. • MnB₁₂O₁₄(OH)₁₀ is antiferromagnetic without a long-range ordering down to 2 K. • DFT calculations indicate ZnB₁₂O₁₄(OH)₁₀ has a direct band gap 4.9 eV.« less

  3. Metallic ions catalysis for improving bioleaching yield of Zn and Mn from spent Zn-Mn batteries at high pulp density of 10.

    PubMed

    Niu, Zhirui; Huang, Qifei; Wang, Jia; Yang, Yiran; Xin, Baoping; Chen, Shi

    2015-11-15

    Bioleaching of spent batteries was often conducted at pulp density of 1.0% or lower. In this work, metallic ions catalytic bioleaching was used for release Zn and Mn from spent ZMBs at 10% of pulp density. The results showed only Cu(2+) improved mobilization of Zn and Mn from the spent batteries among tested four metallic ions. When Cu(2+) content increased from 0 to 0.8 g/L, the maximum release efficiency elevated from 47.7% to 62.5% for Zn and from 30.9% to 62.4% for Mn, respectively. The Cu(2+) catalysis boosted bioleaching of resistant hetaerolite through forming a possible intermediate CuMn2O4 which was subject to be attacked by Fe(3+) based on a cycle of Fe(3+)/Fe(2+). However, poor growth of cells, formation of KFe3(SO4)2(OH)6 and its possible blockage between cells and energy matters destroyed the cycle of Fe(3+)/Fe(2+), stopping bioleaching of hetaerolite. The chemical reaction controlled model fitted best for describing Cu(2+) catalytic bioleaching of spent ZMBs. Copyright © 2015 Elsevier B.V. All rights reserved.

  4. Investigation of the Genotoxicity of Aluminum Oxide, β-Tricalcium Phosphate, and Zinc Oxide Nanoparticles In Vitro.

    PubMed

    Akbaba, Giray Buğra; Türkez, Hasan

    The aim of this study was to investigate the genotoxicity of aluminum oxide (Al 2 O 3 ), β-tricalcium phosphate (β-TCP) (Ca 3 (PO 4 ) 2 ), and zinc oxide (ZnO) nanoparticles (NPs) that were 4.175, 9.058, and 19.8 nm sized, respectively, on human peripheral blood lymphocytes using micronucleus (MN) and chromosome aberration (CA) techniques. Aluminum oxide and β-TCP NPs did not show genotoxic effects on human peripheral blood cultures in vitro, even at the highest concentrations; therefore, these materials may be suitable for use as biocompatible materials. It was observed that, even at a very low dose (≥12.5 ppm), ZnO NPs had led to genotoxicity. In addition, at high concentrations (500 ppm and above), ZnO NPs caused mortality of lymphocytes. For these reasons, it was concluded that ZnO NPs are not appropriate for using as a biocompatible biomaterial.

  5. Heavy metals in water, sediments, plants and fish of Kali Nadi U. P. (India)

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Ajmal, M.; Uddin, R.; Khan, A.U.

    1988-01-01

    The distribution of heavy metals viz., Cd, Co, Cr, Cu, Fe, Mn, Ni, Pb and Zn in the water, sediments, plants and fish samples collected from the Kali Nadi (India) have been determined. The studies have shown that there was considerable variation in the concentration of heavy metals from one sampling station to the other which may be due to the variation in the quality of industrial and sewage wastes being added to the river at different places. The orders of the concentration of heavy metals in water, sediments, plants (Eicchornia crassipes) and fish (Heteropnuestes fossilis) were Fe > Znmore » > Cu > Mn > Cr > Ni > Pb > Co > Cd; Fe > Zn > Mn > Ni > Cr > Co > Cu > Pb > Cd; Fe > Mn > Zn > Cu > Ni > Co > Pb > Cr > Cd and Fe > Zn > Mn > Ni > Pb >Co > Cr > Cu > Cd, respectively.« less

  6. Spatial distribution, ecological and health risk assessment of heavy metals in marine surface sediments and coastal seawaters of fringing coral reefs of the Persian Gulf, Iran.

    PubMed

    Ranjbar Jafarabadi, Ali; Riyahi Bakhtiyari, Alireza; Shadmehri Toosi, Amirhossein; Jadot, Catherine

    2017-10-01

    Concentrations of 13 heavy metals (Al, Fe, Mn, Zn, Cu, Cr, Co, Ni, V, As, Cd, Hg, Pb) in 360 reef surface sediments (0-5 cm) and coastal seawater samples from ten coral Islands in the Persian Gulf were analyzed to determine their spatial distribution and potential ecological risks. Different sediment quality indices were applied to assess the surface sediment quality. The mean concentrations of metals in studied sediments followed the order: Al > Fe > Ni > V > Mn > Zn > Cu > Cr > Co > As > Cd > Pb > As. Average Cd and Hg exceeded coastal background levels at most sampling sites. With the exception of As, concentrations of heavy metals decreased progressively from the west to the east of the Persian Gulf. Based on the Enrichment Factor (EF) and Potential Ecological Risk Index (RI), concentrations of V, Ni, Hg and Cd indicated moderate contamination and is of some concern. The mean values of heavy metals Toxic Units (TUs) were calculated in the following order: Hg (0.75)> Cr (0.41)> Cd (0.27)> As (0.23)> Cu (0.12)> Zn (0.05)> Pb (0.009). Furthermore, the mean contributing ratios of six heavy metals to Toxic Risk Index (TRI) values were 79% for Hg, 11.48% for Cd, 6.16% for Cr, 3.27% for Cu, 0.07% for Zn and 0.01% for Pb. Calculated values of potential ecological risk factor, revealed that the risk of the heavy metals followed the order Cd > Pb > Ni > Cr > V > Cu > Zn. The results reflected that the level of heavy metals, especially Hg and Cd, are on rise due to emerging oil exploration, industrial development, and oil refineries along the entire Gulf. Fe, Mn, Cu, Zn, V and Ni concentrations in seawater were significantly higher (p < 0.05) than the other detected dissolved heavy metals in the sampling sites. A health risk assessment using the hazard quotient index (HQ) recommended by the USEPA suggests that there is no adverse health effect through dermal exposure, and there is no carcinogenic and non-carcinogenic harm to human health. Copyright © 2017 Elsevier Ltd. All rights reserved.

  7. The effect of an oil drilling operation on the trace metal concentrations in offshore bottom sediments of the Campos Basin oil field, SE Brazil.

    PubMed

    Rezende, C E; Lacerda, L D; Ovalle, A R C; Souza, C M M; Gobo, A A R; Santos, D O

    2002-07-01

    The concentrations of Al, Fe, Mn, Zn, Cu, Pb, Ni, Cr, Ba, V, Sn and As in offshore bottom sediments from the Bacia de Campos oil field, SE Brazil, were measured at the beginning and at 7 months after completion of the drilling operation. Concentrations of Al, Fe, Ba, Cr, Ni and Zn were significantly higher closer to the drilling site compared to stations far from the site. Average concentrations of Al, Cu, and in particular of Ni, were significantly higher at the end of the drilling operation than at the beginning. Comparison between drilling area sediments with control sediments of the continental platform, however, showed no significant difference in trace metal concentrations. Under the operation conditions of this drilling event, the results show that while changes in some trace metal concentrations do occur during drilling operations, they are not significantly large to be distinguished from natural variability of the local background concentrations.

  8. Superparamagnetic and ferrimagnetic behavior of nanocrystalline ZnO(MnO)

    NASA Astrophysics Data System (ADS)

    Kuryliszyn-Kudelska, I.; Dobrowolski, W.; Arciszewska, M.; Romčević, N.; Romčević, M.; Hadžić, B.; Sibera, D.; Narkiewicz, U.

    2018-04-01

    We have studied the magnetic properties of nanocrystals of ZnO:MnO prepared by traditional wet chemistry method. The detailed structural and morphological characterization was performed. The results of systematic measurements of AC magnetic susceptibility as a function of temperature and frequency as well as DC magnetization are reported. We observed two different types of magnetic behavior depending on the concentration doping. For samples with low nominal content (up to 30 wt% of MnO), superparamagnetic behavior was observed. We attribute the observed superparamagnetism to the presence of nanosized ZnMnO3 phase. For nanocrystals doped above nominal 60 wt% of MnO ferrimagnetism was detected with TC at around 42 K. This magnetic behavior we assign to the presence of nanosized Mn3O4 phase.

  9. High-temperature hematite and spinel phases in iron-rich slags produced in shales above burned coal seams

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Modreski, P.J.; Herring, J.R.

    1985-01-01

    Ultrametamorphic effects (1300+ /sup 0/C) in shales above burned coal seams in the Powder River Basin, Wyoming, include the formation of droplets and stalactites of congealed iron-rich melt (40.3 wt.% SiO/sub 2/, 35.5% Fe as Fe/sub 2/O/sub 3/, 13.5% Al/sub 2/O/sub 3/, 2.2% MgO, 5.0% CaO, 0.3% MnO, 1.0% K/sub 2/O, 0.5% TiO/sub 2/, 1.3% P/sub 2/O/sub 5/, <0.2% Na/sub 2/O, 0.55% LOI, total 100.2%). This melt, quartz-normative and comparable to an iron-rich basalt, formed along fractures which served as chimneys for escape of burning gases; pyrite or other iron-rich concretions in the shale may have been the source ofmore » the iron in the melts. Oxide phases, dominantly intergrown hematite+magnetite, in the droplets reflect a high-T, low-P, high-f(O/sub 2/) environment. Hematite ranges from nearly pure Fe/sub 2/O/sub 3/ near the droplet rims (Hm-1) to Al- and Ti-rich in the interiors (Hm-2 to -5). Magnetite contains Mg and Al (Mt-1); in the droplet interiors it is richer in Mg and Al (Mt-2 = host+lamellae) and contains lamellae of exsolved hercynite spinel (Sp-1). Near droplet rims, hematite occurs with magnesioferrite spinel (Mf-1) enriched in Mn and Zn (up to 7 wt.% ZnO), a product of reaction with gases during cooling. Averaged microprobe analyses are provided.« less

  10. Short-term low-severity spring grassland fire impacts on soil extractable elements and soil ratios in Lithuania.

    PubMed

    Pereira, Paulo; Cerda, Artemi; Martin, Deborah; Úbeda, Xavier; Depellegrin, Daniel; Novara, Agata; Martínez-Murillo, Juan F; Brevik, Eric C; Menshov, Oleksandr; Comino, Jesus Rodrigo; Miesel, Jessica

    2017-02-01

    Spring grassland fires are common in boreal areas as a consequence of slash and burn agriculture used to remove dry grass to increase soil nutrient properties and crop production. However, few works have investigated fire impacts on these grassland ecosystems, especially in the immediate period after the fire. The objective of this work was to study the short-term impacts of a spring grassland fire in Lithuania. Four days after the fire we established a 400m 2 sampling grid within the burned area and in an adjacent unburned area with the same topographical, hydrological and pedological characteristics. We collected topsoil samples immediately after the fire (0months), 2, 5, 7 and 9months after the fire. We analysed soil pH, electrical conductivity (EC), major nutrients including calcium (Ca), magnesium (Mg), sodium (Na), and potassium (K), and the minor elements aluminium (Al), manganese (Mn), iron (Fe) and zinc (Zn). We also calculated the soil Na and K adsorption ratio (SPAR), Ca:Mg and Ca:Al. The results showed that this low-severity grassland fire significantly decreased soil pH, Al, and Mn but increased EC, Ca, Mg, and K,. There was no effect on Na, Fe, and Zn. There was a decrease of EC, Ca, Mg, and Na from 0months after the fire until 7months after the fire, with an increase during the last sampling period. Fire did not significantly affect SPAR. Ca:Mg decreased significantly immediately after the fire, but not to critical levels. Ca:Al increased after the fire, reducing the potential effects of Al on plants. Overall, fire impacts were mainly limited to the immediate period after the fire. Copyright © 2016 Elsevier B.V. All rights reserved.

  11. Surface Selective Oxidation of Sn-Added CMnSi TRIP Steel

    NASA Astrophysics Data System (ADS)

    Cho, Lawrence; Seo, Eun Jung; Jung, Geun Su; Suh, Dong Woo; De Cooman, Bruno C.

    2016-04-01

    The influence of the addition of Sn on the selective oxidation and the reactive wetting of CMnSi transformation-induced plasticity (TRIP) steels was studied by means of galvanizing simulator tests. A reference TRIP steel and TRIP steels containing Sn in the range of 0.05 to 1 wt pct were intercritically annealed at 1093 K (820 °C) in an N2+ 5 pct H2 gas atmosphere with a dew point of -60 °C. The thin-film oxides formed on the surface of the Sn-added CMnSi TRIP steel were investigated using transmission electron microscopy and 3-dimensional atom probe tomography. The addition of Sn (≥0.05 wt pct) changed the morphology of the xMnO·SiO2 surface oxides from a continuous film morphology to a lens-shaped island morphology. It also suppressed the formation of the Mn-rich oxides of MnO and 2MnO·SiO2. The changes in the morphology and chemistry of the surface oxides were clearly related to the surface segregation of Sn, which appeared to result in a decrease of the oxygen permeability at the surface. The formation of lens-shaped oxides improved the wettability of the CMnSi TRIP steel surface by the molten Zn. The improved wetting effect was attributed to an increased area fraction of the surface where the oxide layer was thinner. This enabled a direct, unhindered reaction between Fe and the Al in the liquid Zn and the formation of the inhibition layer in the initial stages of the hot dipping. The addition of a small amount of Sn was also found to decrease significantly the density of Zn-coating defects on CMnSi TRIP steel.

  12. Microstructure and electroluminescent performance of chemical vapor deposited zinc sulfide doped with manganese films for integration in thin film electroluminescent devices

    NASA Astrophysics Data System (ADS)

    Topol, Anna Wanda

    Zinc sulfide (ZnS) doped with manganese (Mn), ZnS:Mn, is widely recognized as the brightest and most effective electroluminescent (EL) phosphor used in current thin film electroluminescent (TFEL) devices. ZnS acts as a host lattice for the luminescent activator, Mn, leading to a highly efficient yellow-orange EL emission, and resulting in a wide array of applications in monochrome, multi-color and full color displays. Although this wide band dap (3.7 eV) material can be prepared by several deposition techniques, the chemical vapor deposition (CVD) is the most promising for TFEL applications in terms of viable deposition rates, high thickness and composition uniformity, and excellent yield over large area panels. This study describes the development and optimization of a CVD ZnS:Mn process using diethylzinc [(C2H5)2Zn, DEZ], di-pi-cyclopentadienylmanganese [(C5H5)2Mn, CPMn], and hydrogen sulfide [H2S] as the chemical sources for, respectively, Zn, Mn, and S. The effects of key deposition parameters on resulting Film microstructure and performance are discussed, primarily in the context of identifying an optimized process window for best electroluminescence behavior. In particular, substrate temperature was observed to play a key role in the formation of high quality crystalline ZnS:Mn films leading to improved brightness and EL efficiency. Further investigations of the influence of temperature treatment on the structural characteristics and EL performance of the CVD ZnS:Mn film were carried out. In this study, the influence of post-deposition annealing both in-situ and ex-situ annealing processes, on chemical, structural, and electroluminescent characteristics of the phosphor layer are described. The material properties of the employed dielectric are among the key factors determining the performance, stability and reliability of the TFEL display and therefore, the choice of dielectric material for use in ACTFEL displays is crucial. In addition, the luminous efficiency depends on the density of the interface states and their depth at the insulator-phosphor interfaces. Hence, critical integration issues are discussed in terms of the incorporation of ZnS:Mn films in dielectricsemiconductor-dielectric (DSD) structures with silicon nitride (SiNx) and aluminum titanium oxide (ATO) as top and bottom insulators.

  13. Distribution of potentially toxic elements (PTEs) in tailings, soils, and plants around Gol-E-Gohar iron mine, a case study in Iran

    PubMed Central

    Soltani, Naghmeh; Keshavarzi, Behnam; Moore, Farid; Sorooshian, Armin; Ahmadi, Mohamad Reza

    2017-01-01

    This study investigated the concentration of potentially toxic elements (PTEs) including Al, As, Cd, Co, Cr, Cu, Fe, Hg, Mn, Mo, Ni, Pb, Sb, V, and Zn in 102 soils (in the Near and Far areas of the mine), 7 tailings, and 60 plant samples (shoots and roots of Artemisia sieberi and Zygophylum species) collected at the Gol-E-Gohar iron ore mine in Iran. The elemental concentrations in tailings and soil samples (in Near and Far areas) varied between 7.4 and 35.8 mg kg−1 for As (with a mean of 25.39 mg kg−1 for tailings), 7.9 and 261.5 mg kg−1 (mean 189.83 mg kg−1 for tailings) for Co, 17.7 and 885.03 mg kg−1 (mean 472.77 mg kg−1 for tailings) for Cu, 12,500 and 400,000 mg kg−1 (mean 120,642.86 mg kg−1 for tailings) for Fe, and 28.1 and 278.1 mg kg−1 (mean 150.29 mg kg−1 for tailings) for Ni. A number of physicochemical parameters and pollution index for soils were determined around the mine. Sequential extractions of tailings and soil samples indicated that Fe, Cr, and Co were the least mobile and that Mn, Zn, Cu, and As were potentially available for plants uptake. Similar to soil, the concentration of Al, As, Co, Cr, Cu, Fe, Mn, Mo, Ni, and Zn in plant samples decreased with the distance from the mining/processing areas. Data on plants showed that metal concentrations in shoots usually exceeded those in roots and varied significantly between the two investigated species (Artemisia sieberi > Zygophylum). All the reported results suggest that the soil and plants near the iron ore mine are contaminated with PTEs and that they can be potentially dispersed in the environment via aerosol transport and deposition. PMID:28620857

  14. L-serine capped ZnS:Mn nanocrystals for plant cell biological studies and as a growth enhancing agent for micropropagation of Bacopa monnieri Linn. (Brahmi:Scrophulariaceae)

    NASA Astrophysics Data System (ADS)

    Augustine, M. Sajimol; Mathew, Lizzy; Alex, Roselin; Deepa, G. D.; Jayalekshmi, S.

    2014-01-01

    In the present work, the prospects of ZnS:Mn nanocrystals capped with L- serine, a bio-compatible amino acid, synthesized by wet chemical route, as efficient fluorescent probes for plant cell biological studies have been investigated. The present synthesis route using bio-compatible material is a low cost and easy to control method. The colloidal stability of the capped nano crystals is very good as they remain stable without settling down for long time. It is observed that L- serine significantly modifies the structural and optical characteristics of the ZnS:Mn nanocrystals and hence is suitable as a bio-compatible capping agent. The structural properties of L- serine capped nanocrystals were investigated by XRD technique. The size of the L- serine capped ZnS:Mn nanocrystals is found to be around 2 nm . The optical characterization of the nanocrystals was carried out on the basis of photoluminescence (PL) spectroscopic studies. The intense photoluminescence emission observed around 597nm for L-serine capped ZnS:Mn offers high prospects of applications in bio-imaging fields. The unique optical properties of nanoparticles make them appealing as in vivo and in vitro fluorophores in a variety of biological investigations. In the present study, L-serine capped ZnS:Mn nanocrystals were used as a staining dye in fluorescent microscope for observing cell division, cell structure etc. These nanocrystals were also incorporated into the culture media along with the normal auxin- cytokinin hormone combinations in Murashige and Skoog (MS) medium for micropropagation of Bacopa monnieri Linn. (Brahmi:Scrophulariaceae), an Ayurvedic medicine. The results suggest that L-serine capped ZnS:Mn nanocrystals can act as efficient enhancers towards quick callusing and shoot proliferation.

  15. Analysis of the Metals in Soil-Water Interface in a Manganese Mine

    PubMed Central

    Ren, Bozhi; Wang, Qian; Chen, Yangbo; Ding, Wenjie; Zheng, Xie

    2015-01-01

    In order to reveal the influence of the metals of soil-water interface in a manganese mine (Xiangtan, China), on local water environment, there are six kinds of metals (Mn, Ni, Cu, Zn, Cd, and Pb) characterized by measuring their concentration, correlation, source, and special distribution using principal component analysis, single factor, and Nemero comprehensive pollution index. The results showed that the corresponding average concentration was 0.3358, 0.045, 0.0105, 0.0148, 0.0067, and 0.0389 mg/L. The logarithmic concentration of Mn, Zn, and Pb was normal distribution. The correlation coefficients (between Mn and Pb, Mn and Zn, Mn and Ni, Cu and Zn, Cu and Pb, and Zn and Cd) were found to range from 0.5 to 0.6, and those between Cu and Ni and Cu and Cd were below 0.3. It was found that Zn and Mn pollution were caused primarily by ore mining, mineral waste transportation, tailing slag, and smelting plants, while Cu and Ni mainly originate from the mining industry activities and the traffic transportation in the mining area. In addition, the Cd was considered to be produced primarily from the agricultural or anthropogenic activities. The pollution indexes indicated that metal pollution degree was different in soil-water interface streams as listed in increasing order of pollution level as Zn > Ni > Cu > Pb > Mn > Cd. For all of the pollution of the soil-water interface streams, there was moderate metal pollution but along the eastern mine area the pollution seemed to get more serious. There was only a small amount of soil-water interface streams not contaminated by the metals. PMID:26167333

  16. Mineral Composition of Wild and Cultivated Blueberries.

    PubMed

    Dróżdż, Paulina; Šėžienė, Vaida; Pyrzynska, Krystyna

    2018-01-01

    The concentrations of 13 elements (Al, Ca, Cd, Cr, Cu, Fe, K, Mg, Mn, Na, Ni, Pb, and Zn) were determined in several samples of native (wild) naturally growing and cultivated blueberry fruits. The total metal contents after mineralization were analyzed by inductively coupled plasma optical emission spectrometry. Reliability of the procedure was checked by the analysis of the certified reference materials Mixed Polish Herbs (INGT-MPH-2) and Leaves of Poplar (NCS DC 73350). In the fruits collected in the forest (wild blueberries), higher contents of Ca, Na, and Mg as well as Mn and Zn were observed. Similar levels of Cu, Cr, Fe, and Ni were detected in both wild-growing and cultivated plants. The significantly higher content of Fe and Cd in cultivated blueberries was connected with the content of these metals in soil samples collected from the same places. The metal extraction efficiency by hot water varied widely for the different blueberries (wild or cultivated) as well as their form (fresh or dried).

  17. [Determination of Mineral Elements in Choerospondias Axillaris and Its Extractives by ICP-AES].

    PubMed

    Zhai, Yu-xin; Chen, Jun; Li, Ti; Liu, Ji-yan; Wang, Xie-yi; Cheng, Chao; Liu, Cheng-mei

    2015-04-01

    Nine elements in Choerospondias axillaris flesh, peels, aqueous extractives and gastric digesta were determined by the inductively coupled plasma atomic emission spectrometry (ICP-AES) in the present study. The results showed that the contents of Fe, Ca, Zn, Mn, Al, Mg, Cu, K and P in the flesh were 27.37, 269.88, 1.51, 2.45, 1.95, 195.30, 2.45, 2,970.11, and 133.94 µg · g(-1), respectively. They are lower than that in the peels, about 40.31%, 11.70%, 21.68%, 4.27%, 10.58%, 15.76%, 68.72%, 42.04%, and 22.59%, respectively. For microwave assistant extraction, the release rate of Mn was highest (81.68%), while Fe was lowest (4.42%) in the flesh. The release rate of Zn was the highest (79.00%), while that of A1 was the lowest (4.94%) in the peels. Except Fe, Cu and Zn, the release rates of the other elements in flesh were higher than those in the peels. After gastric digestion, the release rates of nine elements were 3.25%-87.51% in the flesh and 7.11%-50.69% in the peels. The release rates of minerals in the flesh were found to be higher than those in the peels except Fe and Cu. Microwave assistant extraction can more efficiently release Fe, Ca, Mn, Mg and K from the flesh than the gastric digestion do. While gastric digestion had a significant effect on the peels, the release rates of elements, except Zn, were higher than those in microwave assistant extraction. Therefore, the difference of distribution and release of mineral elements between peels and flesh of Choerospondias axillaris was understood, which will provide a positive guide for further study of bioavailability of minerals for human body.

  18. Structure, magnetic, and electrical properties of Zn1-xMnxO material

    NASA Astrophysics Data System (ADS)

    Sebayang, P.; Hulu, S. F.; Nasruddin, Aryanto, D.; Kurniawan, C.; Subhan, A.; Sudiro, T.; Ginting, M.

    2017-07-01

    ZnO and MnO2 powder were synthesized using solid state reaction method to produce Zn1-xMnxO materials. Effect of dopant concentrations at the material of Zn1-xMnxO (x = 0.015, 0.02, 0.025) to the change of crystal structure, electrical and magnetic properties was studied. The X-ray diffraction (XRD) result of the samples that were doped with Mn showed a hexagonal wurtzite polycrystalline structure. The addition of Mn dopant resulting the decrease of lattice parameters and peaks intensity. The significant increase of the peak intensity occurred at x = 0.02, which also indicated an increase in the crystal quality of ZnO. The change of the ZnO structure affected the electrical and magnetic properties of the samples.

  19. Surface Properties and Photocatalytic Activities of the Colloidal ZnS:Mn Nanocrystals Prepared at Various pH Conditions

    PubMed Central

    Heo, Jungho; Hwang, Cheong-Soo

    2015-01-01

    Water-dispersible ZnS:Mn nanocrystals (NC) were synthesized by capping the surface with mercaptoacetic acid (MAA) molecules at three different pH conditions. The obtained ZnS:Mn-MAA NC products were physically and optically characterized by corresponding spectroscopic methods. The UV-Visible absorption spectra and PL emission spectra showed broad peaks at 310 and 590 nm, respectively. The average particle sizes measured from the HR-TEM images were 5 nm, which were also supported by the Debye-Scherrer calculations using the X-ray diffraction (XRD) data. Moreover, the surface charges and the degrees of aggregation of the ZnS:Mn-MAA NCs were determined by electrophoretic and hydrodynamic light scattering methods, indicating formation of agglomerates in water with various sizes (50–440 nm) and different surface charge values accordingly the preparation conditions of the NCs (−7.59 to −24.98 mV). Finally, the relative photocatalytic activities of the ZnS:Mn-MAA NCs were evaluated by measuring the degradation rate of methylene blue (MB) molecule in a pseudo first-order reaction condition under the UV-visible light irradiation. As a result, the ZnS:Mn-MAA NC prepared at the pH 7 showed the best photo-degradation efficiency of the MB molecule with the first-order rate constant (kobs) of 2.0 × 10−3·min−1. PMID:28347105

  20. Chemical fractionation of heavy metals in urban soils of Guangzhou, China.

    PubMed

    Lu, Ying; Zhu, Feng; Chen, Jie; Gan, Haihua; Guo, Yanbiao

    2007-11-01

    Knowledge of the total concentration of heavy metals is not enough to fully assess the environmental impact of urban soils. For this reason, the determination of metal speciation is important to evaluate their environment and the mobilization capacity. Sequential extraction technique proposed by the former European Community Bureau of Reference (BCR) was used to speciate Cd, Cu, Fe, Mn, Ni, Pb, and Zn in urban soils from Guangzhou into four operationally defined fractions: HOAc extractable, reducible, oxidizable, and residual. The Cu, Fe, Ni, and Zn were predominantly located in the residual fraction, Pb in the reducible fraction, and Cd and Mn within the HOAc extractable fraction. The order of Cd in each fraction was generally HOAc extractable > reducible > residual > oxidizable; Cu and Fe were residual > reducible > oxidizable > HOAc extractable; Mn was HOAc extractable > residual > reducible > oxidizable; Ni and Zn were residual > reducible > HOAc extractable > oxidizable; and Pb was reducible > residual > oxidizable > HOAc extractable. Cadmium was identified as being the most mobile of the elements, followed by Mn, Zn, Ni, Cu, Pb and Fe. Iron-Mn oxides can play an important role in binding Cd, Cu, Ni, Pb, and Zn and in decreasing their proportion associated with the residual fraction in the soils. With total concentrations of Cd, Cu, Ni, Pb, Zn, and Mn increase, these metals more easily release and may produce more negative effects on the urban environment.

  1. ZnO@MnO2 Core-Shell Nanofiber Cathodes for High Performance Asymmetric Supercapacitors.

    PubMed

    Radhamani, A V; Shareef, K M; Rao, M S Ramachandra

    2016-11-09

    Asymmetric supercapacitors (ASCs) with aqueous electrolyte medium have recently become the focus of increasing research. For high performance ASCs, selection of cathode materials play a crucial role, and core-shell nanostructures are found to be a good choice. We successfully synthesized, ZnO@MnO 2 core-shell nanofibers (NFs) by modification of high-aspect-ratio-electrospun ZnO NFs hydrothermally with MnO 2 nanoflakes. High conductivity of the ZnO NFs and the exceptionally high pseudocapacitive nature of MnO 2 nanoflakes coating delivered a specific capacitance of 907 Fg -1 at 0.6 Ag -1 for the core-shell NFs. A simple and cost-effective ASC construction was demonstrated with ZnO@MnO 2 NFs as a battery-type cathode material and a commercial-quality activated carbon as a capacitor-type anode material. The fabricated device functioned very well in a voltage window of 0-2.0 V, and a red-LED was illuminated using a single-celled fabricated ASC device. It was found to deliver a maximum energy density of 17 Whkg -1 and a power density of 6.5 kWkg -1 with capacitance retention of 94% and Coulombic efficiency of 100%. The novel architecture of the ZnO@MnO 2 core-shell nanofibrous material implies the importance of using simple design of fiber-based electrode material by mere changes of core and shell counterparts.

  2. Autosomal-Recessive Intellectual Disability with Cerebellar Atrophy Syndrome Caused by Mutation of the Manganese and Zinc Transporter Gene SLC39A8.

    PubMed

    Boycott, Kym M; Beaulieu, Chandree L; Kernohan, Kristin D; Gebril, Ola H; Mhanni, Aziz; Chudley, Albert E; Redl, David; Qin, Wen; Hampson, Sarah; Küry, Sébastien; Tetreault, Martine; Puffenberger, Erik G; Scott, James N; Bezieau, Stéphane; Reis, André; Uebe, Steffen; Schumacher, Johannes; Hegele, Robert A; McLeod, D Ross; Gálvez-Peralta, Marina; Majewski, Jacek; Ramaekers, Vincent T; Nebert, Daniel W; Innes, A Micheil; Parboosingh, Jillian S; Abou Jamra, Rami

    2015-12-03

    Manganese (Mn) and zinc (Zn) are essential divalent cations used by cells as protein cofactors; various human studies and animal models have demonstrated the importance of Mn and Zn for development. Here we describe an autosomal-recessive disorder in six individuals from the Hutterite community and in an unrelated Egyptian sibpair; the disorder is characterized by intellectual disability, developmental delay, hypotonia, strabismus, cerebellar atrophy, and variable short stature. Exome sequencing in one affected Hutterite individual and the Egyptian family identified the same homozygous variant, c.112G>C (p.Gly38Arg), affecting a conserved residue of SLC39A8. The affected Hutterite and Egyptian individuals did not share an extended common haplotype, suggesting that the mutation arose independently. SLC39A8 is a member of the solute carrier gene family known to import Mn, Zn, and other divalent cations across the plasma membrane. Evaluation of these two metal ions in the affected individuals revealed variably low levels of Mn and Zn in blood and elevated levels in urine, indicating renal wasting. Our findings identify a human Mn and Zn transporter deficiency syndrome linked to SLC39A8, providing insight into the roles of Mn and Zn homeostasis in human health and development. Copyright © 2015 The American Society of Human Genetics. Published by Elsevier Inc. All rights reserved.

  3. Magnetic Photocatalyst BiVO₄/Mn-Zn ferrite/Reduced Graphene Oxide: Synthesis Strategy and Its Highly Photocatalytic Activity.

    PubMed

    Xie, Taiping; Li, Hui; Liu, Chenglun; Yang, Jun; Xiao, Tiancun; Xu, Longjun

    2018-05-29

    Magnetic photocatalyst BiVO₄/Mn-Zn ferrite (Mn 1- x Zn x Fe₂O₄)/reduced graphene oxide (RGO) was synthesized by a simple calcination and reduction method. The magnetic photocatalyst held high visible light-absorption ability with low band gap energy and wide absorption wavelength range. Electrochemical impedance spectroscopies illustrated good electrical conductivity which indicated low charge-transfer resistance due to incorporation of Mn 1- x Zn x Fe₂O₄ and RGO. The test of photocatalytic activity showed that the degradation ratio of rhodamine B (RhB) reached 96.0% under visible light irradiation after only 1.5 h reaction. The photocatalytic mechanism for the prepared photocatalyst was explained in detail. Here, the incorporation of RGO enhanced the specific surface area compared with BiVO4/Mn 1- x Zn x Fe₂O₄.The larger specific surface area provided more active surface sites, more free space to improve the mobility of photo-induced electrons, and further facilitated the effective migration of charge carriers, leading to the remarkable improvement of photocatalytic performance. Meanwhile, RGO was the effective acceptor as well as transporter of photo-generated electron hole pairs. •O₂ - was the most active species in the photocatalytic reaction. BiVO₄/Mn 1- x Zn x Fe₂O₄/RGO had quite a wide application in organic contaminants removal or environmental pollution control.

  4. Bioavailability and health risk assessment of potentially toxic elements in Thriasio Plain, near Athens, Greece.

    PubMed

    Antoniadis, Vasileios; Golia, Evangelia E; Shaheen, Sabry M; Rinklebe, Jörg

    2017-04-01

    Elevated concentrations of potentially toxic elements (PTEs) are usually found in areas of intense industrial activity. Thriasio Plain is a plain near Athens, Greece, where most of the heavy industry of the country has been situated for decades, but it also is a residential and horticultural area. We aimed at measuring the levels of PTEs in soils and indigenous plant species and assessing the health risk associated with direct soil ingestion. Samples of soils at roadsides and growing plants were collected from 31 sites of that area. Concentrations of Al, As, Cd, Co, Cr, Cu, Fe, Mn, Mo, Ni, Pb, V and Zn were measured in both soils (as pseudo-total) and aerial plant tissues. We found that As, Cd, Cr, Cu, Ni, Pb and Zn were higher than maximum regulatory limits. Element concentrations in plants were rather lower than expected, probably because indigenous plants have developed excluder behaviour over time. Copper and Zn soil-to-plant coefficients were highest among the other elements; for Cu this was unexpected, and probably associated with recent Cu-releasing industrial activity. Risk assessment analysis indicated that As was the element contributing more than 50 % of the health risk related to direct soil ingestion, followed by Cr, Pb, and, surprisingly, Mn. We concluded that in a multi-element contamination situation, elevated risk of PTEs (such as As, Cr and Pb) may reduce the tolerance limits of exposure to less-toxic elements (here, Mn).

  5. Evidence For Different Reaction Pathways For Liquid And Granular Micronutrients In A Calcareous Soil

    EPA Science Inventory

    The benefits of Mn and Zn fluid fertilizers over conventional granular products in calcareous sandy loam soils have been agronomically demonstrated. We hypothesized that the differences in the effectiveness between granular and fluid Mn and Zn fertilizers is due to different Mn ...

  6. Marine Chemistry in the People’s Republic of China.

    DTIC Science & Technology

    1984-08-01

    Eh, Fe, Al, Mn, Cu, Pb, Zn, Cd, Hg, Cr, and also the sedimentation rate by Pb- 210 method. (2) The effects of flow rate, eddy diffusion, axial length of...sediments, distribution, determination, radium-226, uranium-238, radon-222, polonium - 210 , bismuth- 210 , lead-206, particulates, adsorption, polonium ...sediments, distribution, radium-226, uranium-238, radon-222, polonium - 210 , bismuth- 210 , lead-206, particulates, adsorption, polonium , dating, Zhujiang

  7. Comparison of structural and magnetic properties of Zn{sub x}Mg{sub 1.5-x}Mn{sub 0.5}FeO{sub 4} and MgAl{sub x}Cr{sub x}Fe{sub 2-2x}O{sub 4} spinel oxides

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Thummer, K. P., E-mail: kpthummer@yahoo.co.in; Tanna, A. R., E-mail: ashish.tanna@rku.ac.in; Joshi, H. H.

    2016-05-23

    The spinel oxides Zn{sub x}Mg{sub 1.5-x}Mn{sub 0.5}FeO{sub 4} (x = 0.0 to 0.6) and MgAl{sub x}Cr{sub x}Fe{sub 2-2x}O{sub 4} (x = 0.0 to 0.6) abbreviated as ZMMFO and MACFO respectively, were synthesized by standard ceramic processing. The compositional purity of all the specimens was checked by EDAX technique. The X-ray diffractometry was employed to determine the lattice constants and distribution of cations in the interstitial voids. The initial decrease of cell edge parameter (a) for ZMMFO up to x = 0.2 and thereafter expected rise in the ‘a’ and the initial slower rate of reduction in the lattice constant formore » MACFO are explained as basic of cation occupancy. The magnetic ordering in both systems is explained by invoking statistical canting models. The compositional variation of magneton number (n{sub B}) for ZMMFO could be very well explained by Localized canting of spin (LCS) model while Random canting of spin (RCS) model was used for MACFO system.« less

  8. Method and apparatus for preparation of spherical metal carbonates and lithium metal oxides for lithium rechargeable batteries

    DOEpatents

    Kang, Sun-Ho [Naperville, IL; Amine, Khalil [Downers Grove, IL

    2008-10-14

    A number of materials with the composition Li.sub.1+xNi.sub..alpha.Mn.sub..beta.Co.sub..gamma.M'.sub..delta.O.sub.2-- zF.sub.z (M'=Mg,Zn,Al,Ga,B,Zr,Ti) for use with rechargeable batteries, wherein x is between about 0 and 0.3, .alpha. is between about 0.2 and 0.6, .beta. is between about 0.2 and 0.6, .gamma. is between about 0 and 0.3, .delta. is between about 0 and 0.15, and z is between about 0 and 0.2. Adding the above metal and fluorine dopants affects capacity, impedance, and stability of the layered oxide structure during electrochemical cycling. Another aspect of the invention includes materials with the composition Li.sub.1+xNi.sub..alpha.Co.sub..beta.Mn.sub..gamma.M'.sub..delta.O.sub.yF- .sub.z (M'=Mg,Zn,Al,Ga,B,Zr,Ti), where the x is between 0 and 0.2, the .alpha. between 0 and 1, the .beta. between 0 and 1, the .gamma. between 0 and 2, the .delta. between about 0 and about 0.2, the y is between 2 and 4, and the z is between 0 and 0.5.

  9. Direct analysis of deodorants for determination of metals by inductively coupled plasma optical emission spectrometry.

    PubMed

    da Costa, Wiviane Kássia Oliveira Correia; da Silva, Caroline Santos; Figueiredo, José Fernando Dagnone; Nóbrega, Joaquim Araujo; Paim, Ana Paula Silveira

    2018-06-05

    A fast and simple dilute-and-shoot procedure for determination of Al, As, Ba, Cd, Cu, Fe, Mg, Mn, Ni, Pb, Sc, Ti, V, Zn and Zr in deodorants by inductively coupled plasma optical emission spectrometry (ICP OES) was developed. Sample preparation was carried out by diluting 1 mL of deodorant sample in 1% (v v -1 ) HNO 3 . The accuracy of the analytical procedure was evaluated using addition and recovery experiments, and recoveries ranged from 80 to 119%. The limits of detection varied from 0.001 to 0.76 mg kg -1 . Nine deodorants samples of different brands were analyzed. The maximum concentrations found (mg kg -1 ) were: Fe (1.0), Mn (0.1), Ti (1.02), V (0.33), Zn (255.2) and Zr (0.5); for Al and Mg, determined concentrations varied from 0.01 to 7.0% and from 0.005 to 1.44 mg kg -1 , respectively, showing wide variation depending on the sample type. The developed procedure was adequate for determining these analytes in routine analysis presenting high sample throughput and demonstrated the feasibility of direct analysis measurements after simple dilution step. Copyright © 2018 Elsevier B.V. All rights reserved.

  10. Multivariate statistical analysis of heavy metal concentration in soils of Yelagiri Hills, Tamilnadu, India--spectroscopical approach.

    PubMed

    Chandrasekaran, A; Ravisankar, R; Harikrishnan, N; Satapathy, K K; Prasad, M V R; Kanagasabapathy, K V

    2015-02-25

    Anthropogenic activities increase the accumulation of heavy metals in the soil environment. Soil pollution significantly reduces environmental quality and affects the human health. In the present study soil samples were collected at different locations of Yelagiri Hills, Tamilnadu, India for heavy metal analysis. The samples were analyzed for twelve selected heavy metals (Mg, Al, K, Ca, Ti, Fe, V, Cr, Mn, Co, Ni and Zn) using energy dispersive X-ray fluorescence (EDXRF) spectroscopy. Heavy metals concentration in soil were investigated using enrichment factor (EF), geo-accumulation index (Igeo), contamination factor (CF) and pollution load index (PLI) to determine metal accumulation, distribution and its pollution status. Heavy metal toxicity risk was assessed using soil quality guidelines (SQGs) given by target and intervention values of Dutch soil standards. The concentration of Ni, Co, Zn, Cr, Mn, Fe, Ti, K, Al, Mg were mainly controlled by natural sources. Multivariate statistical methods such as correlation matrix, principal component analysis and cluster analysis were applied for the identification of heavy metal sources (anthropogenic/natural origin). Geo-statistical methods such as kirging identified hot spots of metal contamination in road areas influenced mainly by presence of natural rocks. Copyright © 2014 Elsevier B.V. All rights reserved.

  11. Toxic and essential mineral elements content of black tea leaves and their tea infusions consumed in Iran.

    PubMed

    Salahinejad, Maryam; Aflaki, Fereydoon

    2010-04-01

    The metal contents of eleven black tea samples, four cultivated in Iran and seven imported, and their tea infusions were determined. Twelve elements consisting toxic metals (Al, As, Pb, Cr, Cd, and Ni) and essential mineral elements (Fe, Zn, Cu, Mn, Ca, and Mg) were analyzed using inductively coupled plasma atomic emission spectroscopy (ICP-AES). Al, Ca, Mg, and Mn ranged in black tea leaves at mg g(-1) levels, while Cr, Fe, Ni, Cu, Zn were at microg g(-1) levels. Analysis of variance showed no statistically significant differences among most elements determined in cultivated and imported black teas in Iran except for Ni and Cu. The extraction efficiency of each element into tea infusions was evaluated. The solubility of measured metals in infusion extracts varied widely and ranged from 0 to 59.3%. Among the studied elements, Cr, Pb, and Cd showed the lowest rates of solubility and Ni had the highest rates of solubility. The amount of toxic metals and essential mineral elements that one may take up through consumption of black tea infusion was estimated. The amount of realizing each element into tea infusions and acceptable daily intake, for safety consumption of black tea, was compared.

  12. Plant growth, nutrients and potentially toxic elements in leaves of yerba mate clones in response to phosphorus in acid soils.

    PubMed

    Barbosa, Julierme Z; Motta, Antonio C V; Consalter, Rangel; Poggere, Giovana C; Santin, Delmar; Wendling, Ivar

    2018-01-01

    Native to subtropical region of South America, yerba mate is responsive to P under some conditions, but the degree of influence of genetic and soil on the growth and composition of the leaf is unknown. The aim of study was to evaluate plant growth, nutrients and potentially toxic elements in leaves of yerba mate clones in response to P application in acid soils. In greenhouse condition, two yerba mate clone seedlings were grown (210 days) in pots, each clone in a completely randomized design in factorial scheme (with and without P; four acid soils). The elemental composition of leaves and the growth of plants were determined. Phosphorus promoted plant growth, but this was not accompanied by increased P in leaf tissue in all conditions tested. The P effect on the elemental composition varied: decrease/null (N, K, Mg, Mn, Cu, Ni, B, Mo, Al, Cd); increase/null (C/N, C, Ca, Fe, V); increase/decrease/null (Zn, Ba, Pb) and; null (Cr). The soils affect the elemental composition of the leaves, especially Mn, with accumulation greater than 1000 mg kg-1. The Ba, Pb, Al and Zn in the leaves varied among clones. Yerba mate response to P was affected by edaphic and plant factors.

  13. Ultrasensitive, Real-time and Discriminative Detection of Improvised Explosives by Chemiresistive Thin-film Sensory Array of Mn2+ Tailored Hierarchical ZnS

    NASA Astrophysics Data System (ADS)

    Zhou, Chaoyu; Wu, Zhaofeng; Guo, Yanan; Li, Yushu; Cao, Hongyu; Zheng, Xuefang; Dou, Xincun

    2016-05-01

    A simple method combing Mn2+ doping with a hierarchical structure was developed for the improvement of thin-film sensors and efficient detection of the explosives relevant to improvised explosive devices (IEDs). ZnS hierarchical nanospheres (HNs) were prepared via a solution-based route and their sensing performances were manipulated by Mn2+ doping. The responses of the sensors based on ZnS HNs towards 8 explosives generally increase firstly and then decrease with the increase of the doped Mn2+ concentration, reaching the climate at 5% Mn2+. Furthermore, the sensory array based on ZnS HNs with different doping levels achieved the sensitive and discriminative detection of 6 analytes relevant to IEDs and 2 military explosives in less than 5 s at room temperature. Importantly, the superior sensing performances make ZnS HNs material interesting in the field of chemiresistive sensors, and this simple method could be a very promising strategy to put the sensors based on thin-films of one-dimensional (1D) nanostructures into practical IEDs detection.

  14. Effect of combustion temperature on the emission of trace elements under O2/CO2 atmosphere during coal combustion

    NASA Astrophysics Data System (ADS)

    Qu, Chengrui; Zhang, Mo; Mann, Michael. D.

    2018-03-01

    The effect of combustion temperature on the emission of trace elementswas studied under O2/CO2 atmosphere during coal combustion in a laboratory scale fluidized bed combustor. The elemental composition of fine fly ash particles collected with a low pressure impactor(LPI)was quantified by X-Ray F1uorescence Spectrometer (XRF). The elemental composition of coal and bottom ash was quantified byinductively coupled plasma-atomic emission spectroscopy (ICP-AES). The results indicate that the contents of Mn, Zn, Cd and Cr in the fly ash increase with the rise of combustion temperature. It is found that the enrichment of Zn and Cd is greater in the submicrometer particles than the supermicrometer particles, but Mn and Cr do not enrich in the submicrometer particles. Mn, Zn, Cd and Cr display one peak around 0.1 μm. The relative enrichment factor (Rij) of four elements is in the order of Zn, Cd, Mn and Cr. Zn and Cd are mostly retained in fly ashwhileMn and Cr are retained in both the fly ash and bottom ash.

  15. Ultrasensitive, Real-time and Discriminative Detection of Improvised Explosives by Chemiresistive Thin-film Sensory Array of Mn2+ Tailored Hierarchical ZnS

    PubMed Central

    Zhou, Chaoyu; Wu, Zhaofeng; Guo, Yanan; Li, Yushu; Cao, Hongyu; Zheng, Xuefang; Dou, Xincun

    2016-01-01

    A simple method combing Mn2+ doping with a hierarchical structure was developed for the improvement of thin-film sensors and efficient detection of the explosives relevant to improvised explosive devices (IEDs). ZnS hierarchical nanospheres (HNs) were prepared via a solution-based route and their sensing performances were manipulated by Mn2+ doping. The responses of the sensors based on ZnS HNs towards 8 explosives generally increase firstly and then decrease with the increase of the doped Mn2+ concentration, reaching the climate at 5% Mn2+. Furthermore, the sensory array based on ZnS HNs with different doping levels achieved the sensitive and discriminative detection of 6 analytes relevant to IEDs and 2 military explosives in less than 5 s at room temperature. Importantly, the superior sensing performances make ZnS HNs material interesting in the field of chemiresistive sensors, and this simple method could be a very promising strategy to put the sensors based on thin-films of one-dimensional (1D) nanostructures into practical IEDs detection. PMID:27161193

  16. Geochemical interactions between constituents in acidic groundwater and alluvium in an aquifer near Globe, Arizona

    USGS Publications Warehouse

    Stollenwerk, Kenneth G.

    1994-01-01

    Acidic water from a copper-mining area has contaminated an alluvial aquifer and stream near Globe, Arizona. The most contaminated groundwater has a pH of 3.3, and contains about 100 mmol/1 SO4, 50 mmol/1 Fe, 11 mmol/1 Al and 3 mmol/1 Cu. Reactions between alluvium and acidic groundwater were first evaluated in laboratory column experiments. A geochemical model was developed and used in the equilibrium speciation program, MINTEQA2, to simulate breakthrough curves for different constituents from the column. The geochemical model was then used to simulate the measured changes in concentration of aqueous constituents along a flow path in the aquifer.The pH was predominantly controlled by reaction with carbonate minerals. Where carbonates had been dissolved, adsorption of H+ by iron oxides was used to simulate pH. Acidic groundwater contained little or no dissolved oxygen, and most aqueous Fe was present as Fe(II). In the anoxic core of the plume, Fe(II) was oxidized by MnO2 to Fe(III), which then precipitated as Fe(OH)3. Attenuation of aqueous Cu, Co, Mn, Ni and Zn was a function of pH and could be quantitatively modeled with the diffuse-layer, surface complexation model in MINTEQA2. Aluminum precipitated as amorphous Al(OH)3 at pH < 4.7 and as AlOHSO4 at pH < 4.7. Aqueous Ca and SO4were close to equilibrium with gypsum.After the alluvium in the column had reached equilibrium with acidic groundwater, uncontaminated groundwater was eluted through the column to evaluate the effect of reactants on groundwater remediation. The concentration of Fe, Mn, Cu, Co, Ni and Zn rapidly decreased to the detection limits within a few pore volumes. All of the gypsum that had precipitated initially redissolved, resulting in elevated Ca and SO4concentrations for about 5 pore volumes. Aluminum and pH exhibited the most potential for continued adverse effects on groundwater quality. As H+ desorbed from Fe(OH)3, pH remained below 4.5 for more than 20 pore volumes, resulting in dissolution of AlOHSO4 and elevated aqueous Al.

  17. High-O2, low-CO2 atmosphere on early Mars inferred from manganese oxide deposits

    NASA Astrophysics Data System (ADS)

    Sekine, Y.; Imanura, S.; Noda, N.; Takahashi, Y.; Uesugi, S.; Kurisu, M.; Hartmann, J.

    2017-12-01

    The atmospheric composition and its redox state are central to understanding of geochemical cycles, aqueous environment, and habitability on early Mars. Findings of manganese (Mn) oxide deposits together with some trace metals (e.g., Zn and Ni) by the Curiosity and Opportunity rovers suggest a more oxidizing surface environments on early Mars, possibly with higher amount of O2, than in the present day [Lanza et al., 2016; Arvidson et al., 2016; Hurowitz et al., 2017]. However, the abundance and formation mechanism of O2 have been poorly constrained. In the present study, we report results of laboratory experiments to constrain the redox state of the aqueous environment and atmospheric composition responsible for formation of the Mn oxides on early Mars. Our results of scavenging pattern of trace metals show that the Mn oxides found by the rovers are MnO2, which requires highly oxidizing water (Eh > 0.4 V at pH 7-8) and high atmospheric O2 (> a few mbar) for deposition. We suggest that a low-CO2 condition are also required to prevent formation of Mn carbonate in the aqueous environments. We suggest a low CO2/O2 atmosphere, e.g., CO2/O2 < 1, on early Mars at the time of deposition. This in turn implies that O2 would not have been derived mainly from CO2 photolysis and may require more effective paths (e.g., H2O photolysis and effective atmospheric escape) for producing O2 in the very early stage of Mars' history.

  18. Correlations between elements in the fur of wild animals.

    PubMed

    Długaszek, Maria; Kopczyński, Krzysztof

    2014-07-01

    There is little data on the elemental composition of wild animals fur. In the paper, an attempt has been made to evaluate the concentration of elements in the fur of roe deer, wild boar and hare. The contents of following elements: calcium (Ca), magnesium (Mg), zinc (Zn), copper (Cu), iron (Fe), manganese (Mn), lead (Pb), cadmium (Cd), aluminium (Al), chromium (Cr), nickel (Ni) were determined by atomic absorption spectrometry method. Their content was in the range 0.01 (Cd) to 1,519 (Ca) μg/g. Correlations between the content of Mn, Al, Ca, Pb, Cr, Ni in the fur of animals, liver and muscle tissues were found. Thus it can be assumed that the fur of wild animals can provide an information on the bioavailability of elements and environmental exposure and can be considered as an useful biomarker in animals and environmental studies, although research on this subject should be continued.

  19. A Two-Phase Intergrowth in Genthelvite from Mont Saint-Hilaire, Quebec

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Antao, Sytle M.; Hassan, Ishmael; West Indies)

    Synchrotron high-resolution powder X-ray-diffraction (HRPXRD) data and Rietveld structure refinement were used to examine a two-phase intergrowth of genthelvite, ideally Zn{sub 8}[Be{sub 6}Si{sub 6}O{sub 24}]S{sub 2}, from the alkaline intrusive complex at Mont Saint-Hilaire, Quebec, where genthelvite occurs in nepheline syenite pegmatites. The structural parameters obtained for the two phases are slightly different from each other. The unit-cell parameters are 8.119190(7) {angstrom} (51% phase 1) and 8.128914(9) {angstrom} (49% phase 2). The refinement gives the chemical formulae and interstitial M cation in terms of Zn and Mn (the Fe content is practically zero) for the Mn-poor genthelvite phase 1 asmore » (Zn{sub 7.8}Mn{sub 0.2}){Sigma}{sub 8}[Be{sub 6}Si{sub 6}O{sub 24}]S{sub 2}, and the Mn-rich genthelvite phase 2 as (Zn{sub 7.0}Mn{sub 1.0}){Sigma}{sub 8}[Be{sub 6}Si{sub 6}O{sub 24}]S{sub 2}. These formulae are comparable to the Mn-poor and Mn-rich phases obtained by electron-microprobe analysis. The intergrowth indicates that diffusion is absent among the interstitial M cations of similar size (Zn{sup 2+}, Fe{sup 2+} and Mn{sup 2+}). Such intergrowths may form under distinct f(O{sub 2}) conditions and probably low temperature of crystallization that inhibits diffusion of M cations.« less

  20. Effects of co-dopants on the microstructure and electroluminescence of ZnS:Mn thin film phosphors

    NASA Astrophysics Data System (ADS)

    Zhai, Qing

    The objective of this study is to investigate the effects of the co-dopants of KCl and Ga2S3 and post-deposition annealing on the microstructure and electroluminescence (EL) properties of ZnS:Mn thin film phosphors. ZnS:Mn thin films are deposited by radio frequency (RF) magnetron sputtering from ZnS and Mn targets onto pre-deposited indium tin oxide (ITO) and aluminum titanium oxide (ATO) layers on Corning 7059 glass. Argon at 20mTorr is the sputtering ambient. The substrates are held at 180°C during deposition. Co-dopants are thermally evaporated after the ZnS:Mn films, and diffused into the ZnS:Mn films by ex situ annealing between 600°C and 800°C for 5 minutes in a nitrogen ambient. Brightness versus the applied voltage, luminous efficiency, and photoluminescence (PL) are used to characterize the EL devices. The figures of merit are the threshold voltage Vth, at which luminescence is first detected, B40 and eta40, the brightness and efficiency at 40V above the threshold voltage, respectively. In the as-deposited ZnS:Mn phosphor, the microstructure is heavily defected with two different grain morphologies: a roughly 100nm layer of equiaxed fine grains at the insulator/phosphor interface and columnar grains with an average diameter of 89nm in the rest of the film. The EL properties of as-deposited films are poor, with a Vth of 125V, B40 of 48.7nits, and a eta40 of 0.2275lm/W. Annealing at 700°C for 5 minutes raises B40 to 99.6nits and eta40 to 0.4463lm/W, with little change in Vth. In KCl doped ZnS:Mn samples, after 5 minutes of annealing at 700°C, SIMS indicates a uniform distribution of K and a complete diffusion of Cl throughout the phosphor. KCl co-doping enhances grain growth by improving dislocation motion, and the columnar grain size increases from 132nm to 187nm. EL properties are improved, with a B40 of 252nits and eta 40 of 0.9879lm/W. A slight increase in Vth is observed. In ZnS:Mn samples with Ga2S3, the grain growth is less than that in undoped ZnS:Mn. Energy dispersive spectrometry (EDS) data show Ga segregation to grain boundaries and triple points. Decreases of 40V in Vth and 10nits in B40 are observed from ZnS:Mn,Ga 2S3 samples annealed at 800°C. It is postulated that Ga2S3 creates a range of shallow donor states at the interface close to the conduction band, which causes lower threshold voltages and "leaky" turn-on properties. The low EL brightness is attributed to the low threshold voltage. The lack of reduction of the defects in the microstructure of ZnS:Mn,Ga2S3 during anneal is another reason for the poor EL properties. When samples are doped with Ga2S3 first followed by KCl, much better EL properties are observed than from samples doped with KCl first followed by Ga2S3 (B40 of 120nits versus 64.2nits). (Abstract shortened by UMI.)

  1. Phytoextraction with Salix viminalis in a moderately to strongly contaminated area.

    PubMed

    Tőzsér, Dávid; Harangi, Sándor; Baranyai, Edina; Lakatos, Gyula; Fülöp, Zoltán; Tóthmérész, Béla; Simon, Edina

    2018-02-01

    We tested the suitability of Salix viminalis for phytoextraction with the analysis of selected elements in soil, root, and leaf, and by visual tree condition assessment in an area with varying levels of contamination. Bioconcentration factor (BCF) and translocation factor (TF) were used to assess the phytoextraction potential of willows. The middle part of the study area was strongly contaminated, while the northern and southern parts were moderately contaminated. We found increasing element concentrations toward deeper layers. Mean concentrations of elements in roots were similar among the three parts, while in leaves the highest concentrations were found in the strongly contaminated part of the study area. Tree condition scores were the lowest in the strongly contaminated part of the study area, which was caused by Al, Ca, K, Mg, Ni, Sr, and Zn concentration. These elements induced leaf disease and leaf feeders. The highest BCF values were found for Cu, Fe, Mn, and Zn in root, and for Cd and Zn in leaves, indicating that S. viminalis had high accumulation potential of these elements. Furthermore, TF values were high for Cd, Mn, Sr, and Zn. Our results also demonstrated that soil element composition has major influence on the condition of S. viminalis individuals. Furthermore, visual condition assessment was found to be a useful tool to assess the phytoextraction potential of trees.

  2. The geochemical cycling of trace elements in a biogenic meromictic lake

    NASA Astrophysics Data System (ADS)

    Balistrieri, Laurie S.; Murray, James W.; Paul, Barbara

    1994-10-01

    The geochemical processes affecting the behavior and speciation of As, Co, Cr, Cu, Fe, Mn, Mo, Ni, Pb, V, and Zn in Hall Lake, Washington, USA, are assessed by examining dissolved and acid soluble particulate profiles of the elements and utilizing results from thermodynamic calculations. The water column of this meromictic lake is highly stratified and contains distinctive oxic, suboxic, and anoxic layers. Changes in the redox state of the water column with depth affect the distribution of all the elements studied. Most noticeable are increases in dissolved Co, Cr, Fe, Mn, Ni, Pb, and Zn concentrations across the oxic-suboxic boundary, increases in dissolved As, Co, Cr, Fe, Mn, and V concentrations with depth in the anoxic layer, significant decreases in dissolved Cu, Ni, Pb, and Zn concentrations in the anoxic region below the sulfide maximum, and large increases in acid soluble particulate concentrations of As, Cr, Cu, Fe, Mo, Ni, Pb, V, and Zn in the anoxic zone below the sulfide maximum. Thermodynamic calculations for the anoxic region indicate that all redox sensitive elements exist in their reduced forms, the primary dissolved forms of Cu, Ni, Pb, and Zn are metal sulfide solution complexes, and solid sulfide phases of Cu, Fe, Mo, and Pb are supersaturated. Calculations using a vertical diffusion and reaction model indicate that the oxidation rate constant for Mn(II) in Hall Lake is estimated to be 0.006 d -1 and is at the lower end of the range of microbial oxidation rates observed in other natural systems. The main geochemical processes influencing the distribution and speciation of trace elements in Hall Lake appear to be transformations of dissolved elements between their oxidation states (As, Cr, Cu, Fe, Mn, V), cocycling of trace elements with Mn and Fe (As, Co, Cr, Cu, Mo, Ni, Pb, V, Zn), formation of soluble metal sulfide complexes (Co, Cu, Ni, Pb, Zn), sorption (As, Co, Cr, Ni, V), and precipitation (Cu, Fe, Mn, Mo, Pb, Zn).

  3. The geochemical cycling of trace elements in a biogenic meromictic lake

    USGS Publications Warehouse

    Balistrieri, L.S.; Murray, J.W.; Paul, B.

    1994-01-01

    The geochemical processes affecting the behavior and speciation of As, Co, Cr, Cu, Fe, Mn, Mo, Ni, Pb, V, and Zn in Hall Lake, Washington, USA, are assessed by examining dissolved and acid soluble particulate profiles of the elements and utilizing results from thermodynamic calculations. The water column of this meromictic lake is highly stratified and contains distinctive oxic, suboxic, and anoxic layers. Changes in the redox state of the water column with depth affect the distribution of all the elements studied. Most noticeable are increases in dissolved Co, Cr, Fe, Mn, Ni, Pb, and Zn concentrations across the oxic-suboxic boundary, increases in dissolved As, Co, Cr, Fe, Mn, and V concentrations with depth in the anoxic layer, significant decreases in dissolved Cu, Ni, Pb, and Zn concentrations in the anoxic region below the sulfide maximum, and large increases in acid soluble particulate concentrations of As, Cr, Cu, Fe, Mo, Ni, Pb, V, and Zn in the anoxic zone below the sulfide maximum. Thermodynamic calculations for the anoxic region indicate that all redox sensitive elements exist in their reduced forms, the primary dissolved forms of Cu, Ni, Pb, and Zn are metal sulfide solution complexes, and solid sulfide phases of Cu, Fe, Mo, and Pb are supersaturated. Calculations using a vertical diffusion and reaction model indicate that the oxidation rate constant for Mn(II) in Hall Lake is estimated to be 0.006 d-1 and is at the lower end of the range of microbial oxidation rates observed in other natural systems. The main geochemical processes influencing the distribution and speciation of trace elements in Hall Lake appear to be transformations of dissolved elements between their oxidation states (As, Cr, Cu, Fe, Mn, V), cocycling of trace elements with Mn and Fe (As, Co, Cr, Cu, Mo, Ni, Pb, V, Zn), formation of soluble metal sulfide complexes (Co, Cu, Ni, Pb, Zn), sorption (As, Co, Cr, Ni, V), and precipitation (Cu, Fe, Mn, Mo, Pb, Zn). ?? 1994.

  4. Effect of composting on the Cd, Zn and Mn content and fractionation in feedstock mixtures with wood chips from a short-rotation coppice and bark.

    PubMed

    Vandecasteele, B; Willekens, K; Zwertvaegher, A; Degrande, L; Tack, F M G; Du Laing, G

    2013-11-01

    Micronutrient content and availability in composts may be affected by the addition of wood chips or tree bark as a bulking agent in the compost feedstock. In the first part of this study, micronutrient levels were assessed in bark and wood of poplar and willow clones in a short-rotation coppice. Large differences between species were observed in bark concentrations for Cd, Zn and Mn. In the second part of the study, we aimed to determine the effect of feedstock composition and composting on Cd, Zn and Mn concentrations and availability. By means of three composting experiments we examined the effect of (a) bark of different tree species, (b) the amount of bark, and (c) the use of bark versus wood chips. In general, compost characteristics such as pH, organic matter and nutrient content varied due to differences in feedstock mixture and composting process. During the composting process, the availability of Cd, Zn and Mn decreased, although the use of willow and poplar bark or wood chips resulted in elevated total Cd, Zn or Mn concentrations in the compost. Cd concentrations in some composts even exceeded legal criteria. Cd and Zn were mainly bound in the reducible fraction extracted with 0.5M NH2OH⋅HCl. A higher acid-extractable fraction for Mn than for Cd and Zn was found. Higher Cd concentrations in the compost due to the use of bark or wood chips did not result in higher risk of Cd leaching. The results of the pH-stat experiment with gradual acidification of composts illustrated that only a strong pH decline in the compost results in higher availability of Cd, Zn and Mn. Copyright © 2013 Elsevier Ltd. All rights reserved.

  5. Disappearance of Ising nature in Ca3ZnMnO6 studied by high-field ESR.

    PubMed

    Ruan, M Y; Ouyang, Z W; Guo, Y M; Cheng, J J; Sun, Y C; Xia, Z C; Rao, G H; Okubo, S; Ohta, H

    2014-06-11

    High-field electron spin resonance measurements of an antiferromagnet Ca3ZnMnO6 isostructure, with the Ising-chain multiferroic Ca3CoMnO6, have been carried out. Two distinct resonance modes were observed below TN = 25 K, which is well explained by conventional antiferromagnetic resonance theory with easy-plane anisotropy. The zero-field spin gap is derived to be about 166 GHz, originating from the easy-plane anisotropy and exchange interaction. Our result suggests that the Dzyaloshinsky-Moriya interaction, which may induce spin canting, is absent. Disappearance of Ising anisotropy in Ca3ZnMnO6 suggests that the Co(4+) ion, as well as the Co-Mn superexchange, plays an important role for the Ising nature in Ca3CoMnO6.

  6. Surface chemistry, friction, and wear of Ni-Zn and Mn-Zn ferrites in contact with metals

    NASA Technical Reports Server (NTRS)

    Miyoshi, K.; Buckley, D. H.

    1983-01-01

    X-ray photoelectron and Auger electron spectroscopy analysis were used in sliding friction experiments. These experiments were conducted with hot-pressed polycrystalline Ni-Zn and Mn-Zn ferrites, and single-crystal Mn-Zn ferrite in contact with various transition metals at room temperature in both vacuum and argon. The results indicate that Ni2O3 and Fe3O4 were present on the Ni-Zn ferrite surface in addition to the nominal bulk constituents, while MnO2 and Fe3O4 were present on the Mn-Zn ferrite surface in addition to the nominal bulk constituents. The coefficients of friction for the ferrites in contact with metals were related to the relative chemical activity of these metals. The more active the metal, the higher is the coefficient of friction. The coefficients of friction for the ferrites were correlated with the free energy of formation of the lowest metal oxide. The interfacial bond can be regarded as a chemical bond between the metal atoms and the oxygen anions in the ferrite surfaces. The adsorption of oxygen on clean metal and ferrite does strengthen the metal-ferrite contact and increase the friction. The ferrites exhibit local cracking and fracture with sliding under adhesive conditions. All the metals transferred to the surfaces of the ferrites in sliding. Previously announced in STAR as N83-19901

  7. Surface chemistry, friction and wear of Ni-Zn and Mn-Zn ferrites in contact with metals

    NASA Technical Reports Server (NTRS)

    Miyoshi, K.; Buckley, D. H.

    1982-01-01

    X-ray photoelectron and Auger electron spectroscopy analysis were used in sliding friction experiments. These experiments were conducted with hot-pressed polycrystalline Ni-Zn and Mn-Zn ferrites, and single-crystal Mn-Zn ferrite in contact with various transition metals at room temperature in both vacuum and argon. The results indicate that Ni2O3 and Fe3O4 were present on the Ni-Zn ferrite surface in addition to the nominal bulk constituents, while MnO2 and Fe3O4 were present on the Mn-Zn ferrite surface in addition to the nominal bulk constituents. The coefficients of friction for the ferrites in contact with metals were related to the relative chemical activity of these metals. The more active the metal, the higher is the coefficient of friction. The coefficients of friction for the ferrites were correlated with the free energy of formation of the lowest metal oxide. The interfacial bond can be regarded as a chemical bond between the metal atoms and the oxygen anions in the ferrite surfaces. The adsorption of oxygen on clean metal and ferrite does strengthen the metal-ferrite contact and increase the friction. The ferrites exhibit local cracking and fracture with sliding under adhesive conditions. All the metals transferred to he surfaces of the ferrites in sliding.

  8. Molecular-beam epitaxy of (Zn,Mn)Se on Si(100)

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Slobodskyy, T.; Ruester, C.; Fiederling, R.

    2004-12-20

    We have investigated the growth by molecular-beam epitaxy of the II-VI diluted magnetic semiconductor (Zn,Mn)Se on As-passivated Si(100) substrates. The growth start has been optimized by using low-temperature epitaxy. Surface properties were assessed by Nomarski and scanning electron microscopy. Optical properties of (Zn,Mn)Se have been studied by photoluminescence and a giant Zeeman splitting of up to 30 meV has been observed. Our observations indicate a high crystalline quality of the epitaxial films.

  9. Mineralogical and geochemical features of the coarse saprolite developed on orthogneiss in the SW of Yaoundé, South Cameroon

    NASA Astrophysics Data System (ADS)

    Ndjigui, P.-D.; Badinane, M. F. B.; Nyeck, B.; Nandjip, H. P. K.; Bilong, P.

    2013-03-01

    A petrological investigation was performed in the coarse saprolite on orthogneiss in Yaoundé (South Cameroon) using combined whole rock geochemical (XRF, ICP-MS) and mineralogical (XRD, SEM) techniques. The orthogneiss has high contents in SiO2 (61.56 wt.%), Ba (916 ppm) and REE (209 ppm), moderate content in Al2O3 (14.34 wt.%) and negative Eu anomaly (Eu/Eu* = 0.68). The weathering leads to the formation of three main constituents in the coarse saprolite: (i) the loose materials (∼85 vol.%) are basically clayey silty with relic structure. They are composed of kaolinite, quartz and goethite. The loose materials have high contents in SiO2 (56-64.83 wt.%) and Al2O3 (21.48-23.96 wt.%), and moderate contents in V (163-236 ppm), Ba (95-340 ppm) and Zr (160-313 ppm). The REE content is low (∼49-169 ppm) relative to the parent rock with LREE-enrichment (LREE/HREE ∼ 7-17). Positive Ce anomaly (Ce/Ce* ∼ 3.35) is observed in the white veins and slight positive Eu anomalies (Eu/Eu* ∼ 1.2-1.4) are noted in all loose samples. The (La/Yb)N ratios (∼0.8-1.5) indicate high REE-fractionation. The mass balance calculation reveals the depletion of several elements except Al, Ti, Sc, Y, Th, Sb and Hf; (ii) the iron duricrust (∼10 vol.%) is located at the bottom and the top of the horizon. The mineral assemblage is dominated by hematite and goethite. The upper iron duricrust has high contents in Fe2O3 (45.60 wt.%) and Cr (1641 ppm), moderate contents in V (459 ppm) and Zn (143 ppm), and low REE content (47 ppm) with low LREE/HREE ratio (4.28). The upper iron duricrust is more enriched in Fe2O3 (53.26 wt.%) than the lower one. Vanadium, Cr and Zr have high contents relative to other trace elements. The REE content is low (39 ppm) as well as the LREE/HREE ratio (2.94). The iron duricrust has negative Ce anomalies (Ce/Ce* ∼ 0.66-0.69) and very low (La/Yb)N ratios (0.1-0.3). Several elements reported in the iron duricrust are highly leached except Fe, Cr, Zn, Sc, V, Pb, Zr, Cu and Th; and (iii) the Mn-rich materials (<5 vol.%) are made up of birnessite, cryptomelane, and low quantities of quartz, kaolinite and goethite. The SEM investigation reveals that Ba and Pb are linked in Mn-bearing phases and Ce-oxides appear as fine-grained intergrowth between Mn-bearing phases. The Mn-bearing phases are enriched in MnO (33.86 wt.%), BaO (4.30 wt.%), Co (1716 ppm), Pb (1315 ppm) and Ce (5202 ppm). Positive Ce and Eu anomalies are observed (Ce/Ce* ∼ 15.60 and Eu/Eu* ∼ 2). The mass balance calculations indicate the strong accumulation of Mn, Ni, Co, Zn, Sc, Cu, Ba, Pb, Y, Ga, Zr and REE. The Mn-bearing phases might be derived from the accumulation of silicate residues and Mn within the parent rock. The transition from the parent rock to the coarse saprolite is marked by high leaching of several elements.

  10. Methods and Strategies for the Ab Initio Design of Novel Manganese Oxide- Based Water Splitting Photocatalyst Materials

    NASA Astrophysics Data System (ADS)

    Kanan, Dalal K.

    Photoelectrochemical cells (PECs) use sunlight to drive endoergic reactions such as carbon dioxide reduction to fuels or water-splitting for renewable hydrogen production. However, materials that combine both the efficiency and low cost needed to make solar-powered catalysis a practical reality have yet to be discovered. This thesis presents methods and new design strategies for developing novel, efficient, robust, and inexpensive photocatalysts based on transition metal oxides (TMOs). Quantum mechanics methodologies are developed and tested for their ability to predict the properties of known materials and then used to predict how altering the composition by alloying and doping with abundant elements affects optical, electronic, transport, and catalytic properties. The first material considered for photocatalysis is MnO, the bio-inspired solid state analogue of the photosystem II active site. GW theory with input from hybrid DFT and ab initio DFT+U capably predicts the photoemission/inverse photoemission (PE/IPE) band gap and dielectric properties. An ab initio value of U-J = 3.5 eV for Mn2+ was determined using unrestricted Hartree-Fock theory on cluster-size-converged electrostatically embedded clusters. The lowest-lying excitations in MnO, studied using ECW theory, are found to be single Mn d → d ligand field excitations (~2.5 eV, ~108 s lifetime), followed by double d → d excitations (~5.2 eV, ~106 s lifetime), Mn 3d-4s excitations (~6.3 eV, ~10-3 s lifetime), and higher-lying O 2p → Mn 3d ligand-to-metal charge-transfer (LMCT) excitations (~10.1 eV, ~10-4 s lifetime). The longer-lived transitions should exhibit better electron-hole pair separation and enhance photoconductivity depending on ease of carrier transport. While MnO possesses suitable band edge energies, its band gap is too large for efficient sunlight absorption. We predict alloying MnO with ZnO in varying amounts reduces the PE/IPE band gap (to 2.6 eV for the 1:1 alloy) while preserving potential redox reactivity. Optical excitation studies show alloying lowers the LMCT transition to ~8.3 eV leaving all other absorption properties relatively unchanged. We find near degeneracies among spin-allowed and spin-forbidden LMCT states that could facilitate intersystem crossing (ISC) resulting in longer lifetimes. We suggest seeking other materials that exhibit similar LMCT excitations but that are visible-light activated as a design strategy for further enhancing photon conversion efficiencies. Additionally, several dopants (Al, Ga, In, Sc, Y, Ti, Sb, Gd, F (n-type dopants) and Li (a p-type dopant)) were assessed for their ability to enhance conductivity in MnO:ZnO. We find Ga, Sc, Ti, F, and Sb dopants create deep traps whereas In forms shallower traps that merit further investigation. In contrast, Y, Al, Gd, and Li dopants should increase the carrier concentration while maintaining favorable electron and hole transport pathways. The adsorption and oxidation of water on MnO:ZnO(001) surface was studied with ab initio DFT+U calculations. The computed phase diagram for the water/MnO:ZnO(001) interface reveals the surface is quite hydrophilic with the half-dissociated 1 ML (2 ML) structure being most stable under water-poor (water-rich) conditions. For the gas phase water oxidation reaction, we compute a thermodynamic overpotential of 0.82 V without yet modeling reaction kinetics or solvation. The overpotential mainly results from the *OOH intermediate being too weakly bound to the surface because of a loss of resonance stabilization in the adsorbate. We suggest judicious doping as a way to stabilize *OOH and potentially reduce the overpotential to just 0.05 V (for 0.5 ML reaction coverage). (Abstract shortened by UMI.)

  11. Liquefied petroleum gas sensor based on manganese (III) oxide and zinc manganese (III) oxide nanoparticles

    NASA Astrophysics Data System (ADS)

    Sharma, Shiva; Chauhan, Pratima; Husain, Shahid

    2018-01-01

    In this paper, {{{Mn}}}2{{{O}}}3 and {{{ZnMn}}}2{{{O}}}4 nanoparticles (NPs) are successfully synthesized using chemical co-precipitation method at room temperature and further annealed at 450 °C. The structure, crystallite size, morphology, specific surface area (SSA) and band gap energy have been determined by x-ray diffraction, transmission electron microscopy, Brunauer-Emmett-Teller surface area analysis, scanning electron microscopy (SEM-EDS) and UV-visible spectrophotometer. The sensor films of the {{{Mn}}}2{{{O}}}3 NPs and {{{ZnMn}}}2{{{O}}}4 NPs have been fabricated onto glass substrate using spin coater system separately. These sensor films are investigated for different concentrations (200-1200 ppm) of liquefied petroleum gas (LPG) at different operating temperatures ranging from 100 °C to 400 °C. A comparative study of gas sensing properties shows that spinel {{{ZnMn}}}2{{{O}}}4 sensor film exhibit excellent response (≈ 80 % ) towards 1000 ppm LPG at 300 °C in comparison to {{{Mn}}}2{{{O}}}3 sensor films. The enhancement in the gas sensing characteristics of {{{ZnMn}}}2{{{O}}}4 sensor film is attributed to the reduced crystallite size, greater SSA, and modification in structure as well as morphology.

  12. Synthesis and characterization of single-phase Mn-doped ZnO

    NASA Astrophysics Data System (ADS)

    Chattopadhyay, S.; Dutta, S.; Banerjee, A.; Jana, D.; Bandyopadhyay, S.; Chattopadhyay, S.; Sarkar, A.

    2009-05-01

    Different samples of Zn 1-xMn xO series have been prepared using conventional solid-state sintering method. We identified up to what extent doping will enable us to synthesize single-phase polycrystalline Mn-doped ZnO sample, which is one of the prerequisites for dilute magnetic semiconductor, and we have analyzed its some other physical aspects. In synthesizing the samples, proportion of Mn varies from 1 to 5 at%. However, the milling time varied (6, 12, 24, 48 and 96 h) only for 2 at% Mn-doped samples while for other samples (1, 3, 4 and 5 at% Mn doped) the milling time has been fixed to 96 h. Room-temperature X-ray diffraction (XRD) data reveal that all of the prepared samples up to 3 at% of Mn doping exhibit wurtzite-type structure, and no segregation of Mn and/or its oxides has been found. The 4 at% Mn-doped samples show a weak peak of ZnMn 2O 4 apart from the other usual peaks of ZnO and the intensity of this impurity peak has been further increased for 5 at% of Mn doping. So beyond 3 at% doping, single-phase behavior is destroyed. Band gap for all the 2 at% Mn-doped samples has been estimated to be between 3.21 and 3.19 eV and the reason for this low band gap values has been explained through the grain boundary trapping model. The room-temperature resistivity measurement shows an increase of resistivity up to 48 h of milling and with further milling it saturates. The defect state of these samples has been investigated using the positron annihilation lifetime (PAL) spectroscopy technique. Here all the relevant lifetime parameters of positron i.e. free annihilation ( τ1) at defect site ( τ2) and average ( τav) increases with milling time.

  13. Assessing heavy metal toxicity in sediments of Chennai Coast of Tamil Nadu using Energy Dispersive X-Ray Fluorescence Spectroscopy (EDXRF) with statistical approach.

    PubMed

    Tholkappian, M; Ravisankar, R; Chandrasekaran, A; Jebakumar, J Prince Prakash; Kanagasabapathy, K V; Prasad, M V R; Satapathy, K K

    2018-01-01

    The concentration of some heavy metals: Al, Ca, K, Fe, Ti, Mg, Mn, V, Cr, Zn, Ni and Co in sediments from Pulicat Lake to Vadanemmeli along Chennai Coast, Tamil Nadu has been determined using EDXRF technique. The mean concentrations of Mg, Al, K, Ca, Ti, Fe, V, Cr, Mn, Co, Ni, and Zn were found to be 1918, 25436, 9832, 9859, 2109, 8209, 41.58, 34.14, 160.80, 2.85. 18.79 and 29.12 mg kg -1 respectively. These mean concentrations do not exceed the world crustal average. The level of pollution attributed to heavy metals was evaluated using several pollution indicators in order to determine anthropogenically derived contaminations. Enrichment Factor (EF), Geoaccumulation Index (I geo ), Contamination Factor (CF) and Pollution Load Index (PLI) were used in evaluating the contamination status of sediments. Enrichment Factors (EF) reveal the anthropogenic sources of V, Cr, Ni and Zn Geoaccumulation Index (I geo ) results reveal that the study area is not contaminated by the heavy metals. Similar results were also obtained by using pollution load index (PLI). The results of pollution indices indicates that most of the locations were not polluted by heavy metals. Multivariate statistical analysis performed using principal components and clustering techniques were used to identify the source of the heavy metals. The result of statistical procedures indicate that heavy metals in sediments are mainly of natural origin. This study provides a relatively novel technique for identifying and mapping the distribution of metal pollutants and their sources in sediment.

  14. Cu, Zn and Mn uptake and redistribution in Cabernet Sauvignon grapes and wine: effect of soil metal content and plant vigor

    NASA Astrophysics Data System (ADS)

    Concepción Ramos, Maria; Romero, María Paz

    2015-04-01

    This study investigated the influence of leaf thinning on micronutrient (Cu, Zn and Mn) uptake and distribution in grape tissues, in a 16 year-old Cabernet Sauvignon vineyard. The analysis was carried out in two plots with differences in vigor (P1- high and P2-low) grown in calcareous soils. Vigour was analysed by the NDVI values. In each plot, two treatments (with and without leaf thinning after bloom) were applied. Total and the CaCl2-DTPA extractable fraction of these micronutrients were evaluated. Nutrient concentration in petiole were evaluated from veraison to harvest as well as the concentration of those elements in seeds and skins at ripening and in wines elaborated with grapes grown in each plot and treatment in 2013. Their relationships were evaluated. The soil extractable fraction did not give a good correlation with petiole concentrations. However, Mn in petiole was strongly correlated with soil total Mn. Cu and Zn had higher concentration at veraison than at harvest, while for Mn it was the opposite. Cu concentration in petiole and seeds was greater in the most vigorous plots, but there were not clear differences between treatments. Cu in seeds and skins correlated significantly but there was not correlation with Cu in petiole. Zn concentration in skins was quite similar in both plots, but with higher values in vines without leaf thinning. Zn concentrations in skins were correlated with Zn in petiole but no significant correlation was found with Zn in seeds. Higher concentrations were found in the no thinning treatment in skins. For Mn, petiole concentrations were greater in the high vigorous plot and in the leaf thinning treatment. However, petiole Zn concentrations were greater in the less vigorous plot and without clear effect of leaf thinning. Mn concentration in skins was greater in the less vigorous vines in both treatments and it was inversely correlated with Mn in seeds, but there were no significant correlation between them and Mn in petiole. In wine, significant differences between both plots were found for Cu and Zn, with greater values in the most vigorous vines and with some differences in the wines elaborated with grapes from the leaf thinning treatment and without it. Cu levels in wine ranged between 0.78 and 0.96 mg/l in plot 1 and between 0.28 and 0.44 mg/L in plot 2, respectively for the areas with and without leaf thinning. For Zn, levels ranged between 0.76 and 0.74 in plot 1and between 0.24 and 0.22 mg/L in plot 2. However, no differences were found between plots for Mn. Mn levels in wine ranged between 1 and 1.9 mg/L in plot 1 and between 1.12 and 1.2 mg/L in plot 2. This behavior was similar to that found in the skins and seed analysis.

  15. Manganese Transport and Toxicity in Polarized WIF-B Hepatocytes.

    PubMed

    Thompson, Khristy J; Hein, Jennifer; Baez, Andrew; Sosa, Jose Carlo; Wessling-Resnick, Marianne

    2018-05-24

    Mn toxicity arises from nutritional problems, community and occupational exposures, and genetic risks. Mn blood levels are controlled by hepatobiliary clearance. The goals of this study were to determine the cellular distribution of Mn transporters in polarized hepatocytes, to establish an in vitro assay for hepatocyte Mn efflux, and to examine possible roles the Mn transporters would play in metal import and export. For these experiments, hepatocytoma WIF-B cells were grown for 12-14 days to achieve maximal polarity. Immunoblots showed that Mn transporters ZIP8, ZnT10, ferroportin (Fpn), and ZIP14 were present. Indirect immunofluorescence microscopy localized Fpn and ZIP14 to WIF-B cell basolateral domains while ZnT10 and ZIP8 associated with intracellular vesicular compartments. ZIP8-positive structures were distributed uniformly throughout the cytoplasm, but ZnT10-positive vesicles were adjacent to apical bile compartments. WIF-B cells were sensitive to Mn toxicity, showing decreased viability after 16 h exposure to > 250 M MnCl2. However, the hepatocytes were resistant to 4 h exposures of up to 500 M MnCl2 despite 50-fold increased Mn content. Washout experiments showed time-dependent efflux with 80% Mn released after a 4 h chase period. Hepcidin reduced levels of Fpn in WIF-B cells, clearing Fpn from the cell surface, but Mn efflux was unaffected. The secretory inhibitor brefeldin A did block release of Mn from WIF-B cells, suggesting vesicle fusion may be involved in export. These results point to a possible role of ZnT10 to import Mn into vesicles that subsequently fuse with the apical membrane and empty their contents into bile.

  16. Study of defects and vacancies in structural properties of Mn, co-doped oxides: ZnO

    NASA Astrophysics Data System (ADS)

    Kumar, Harish; Kaushik, A.; Alvi, P. A.; Dalela, B.; Dalela, S.

    2018-05-01

    The paper deals with the Structural properties on Mn, Co doped oxides ZnO samples using XRD, Positron Annihilation Lifetime (PAL) Spectra and Raman Spectra. The Mn, Co doped ZnO samples crystallize in a wurtzite structure without any impurity phases in XRD Spectra. The defect state of these samples has been investigated by using positron annihilation lifetime (PAL) spectroscopy technique in which all the relevant lifetime parameters are measured for all the spectra. The results are explained in the direction of doping concentration in these samples in terms of defects structure on Zn lattice site VZn and oxygen defects Vo.

  17. Study concerning the recovery of zinc and manganese from spent batteries by hydrometallurgical processes.

    PubMed

    Buzatu, Traian; Popescu, Gabriela; Birloaga, Ionela; Săceanu, Simona

    2013-03-01

    Used batteries contain numerous metals in high concentrations and if not disposed of with proper care, they can negatively affect our environment. These metals represent 83% of all spent batteries and therefore it is important to recover metals such as Zn and Mn, and reuse them for the production of new batteries. The recovery of Zn and Mn from used batteries, in particular from Zn-C and alkaline ones has been researched using hydrometallurgical methods. After comminution and classification of elemental components, the electrode paste resulting from these processes was treated by chemical leaching. Prior to the leaching process the electrode paste has been subjected to two washing steps, in order to remove the potassium, which is an inconvenient element in this type of processes. To simultaneously extract Zn and Mn from this paste, the leaching method in alkaline medium (NaOH solution) and acid medium (sulphuric acid solution) was used. Also, to determine the efficiency of extraction of Zn and Mn from used batteries, the following variables were studied: reagents concentration, S/L ratio, temperature, time. The best results for extraction yield of Zn and Mn were obtained under acid leaching conditions (2M H2SO4, 1h, 80°C). Copyright © 2012 Elsevier Ltd. All rights reserved.

  18. Content and Bioaccumulation of Nine Mineral Elements in Ten Mushroom Species of the Genus Boletus

    PubMed Central

    Wang, Xue-Mei; Zhang, Ji; Li, Tao; Wang, Yuan-Zhong; Liu, Hong-Gao

    2015-01-01

    Concentrations and bioconcentration potential of nine elements (Ca, Cu, Fe, K, Mg, Mn, Na, P, and Zn) in ten species of wild edible Boletus and the corresponding underlying soils were analyzed. The analyses were performed using inductively coupled plasma atomic emission spectrophotometer. Boletus showed relative abundant contents of P, K, Fe, Mg, Ca, and Na and less of Zn, Cu, and Mn. Caps compared to stalks were enriched in P, K, Cu, Mg, and Zn, while stalks were enriched in Mn. The elements such as P and K were accumulated (BCF > 1), while Ca, Fe, Mg, Mn, and Na were excluded (BCF < 1) in the fruiting bodies. The correlation analysis indicated high correlations between Cu, Mn, Ca, and Fe in the mushrooms as compared to the corresponding soils. Significant correlations were also obtained between Cu-P (r = 0.775), Fe-P (r = 0.728), and Zn-P (r = 0.76) for caps and Cu-Mg (r = 0.721), Fe-Mg (r = 0.719), Zn-Mg (r = 0.824), and Zn-P (r = 0.818) for stalks. The results of this study imply that ability of fungi to accumulate elements from substrate could be influenced by mushroom species and underlying soil substrates. PMID:26146585

  19. Content and Bioaccumulation of Nine Mineral Elements in Ten Mushroom Species of the Genus Boletus.

    PubMed

    Wang, Xue-Mei; Zhang, Ji; Li, Tao; Wang, Yuan-Zhong; Liu, Hong-Gao

    2015-01-01

    Concentrations and bioconcentration potential of nine elements (Ca, Cu, Fe, K, Mg, Mn, Na, P, and Zn) in ten species of wild edible Boletus and the corresponding underlying soils were analyzed. The analyses were performed using inductively coupled plasma atomic emission spectrophotometer. Boletus showed relative abundant contents of P, K, Fe, Mg, Ca, and Na and less of Zn, Cu, and Mn. Caps compared to stalks were enriched in P, K, Cu, Mg, and Zn, while stalks were enriched in Mn. The elements such as P and K were accumulated (BCF > 1), while Ca, Fe, Mg, Mn, and Na were excluded (BCF < 1) in the fruiting bodies. The correlation analysis indicated high correlations between Cu, Mn, Ca, and Fe in the mushrooms as compared to the corresponding soils. Significant correlations were also obtained between Cu-P (r = 0.775), Fe-P (r = 0.728), and Zn-P (r = 0.76) for caps and Cu-Mg (r = 0.721), Fe-Mg (r = 0.719), Zn-Mg (r = 0.824), and Zn-P (r = 0.818) for stalks. The results of this study imply that ability of fungi to accumulate elements from substrate could be influenced by mushroom species and underlying soil substrates.

  20. Deformation induced dynamic recrystallization and precipitation strengthening in an Mg−Zn−Mn alloy processed by high strain rate rolling

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Jiang, Jimiao; Song, Min

    2016-11-15

    The microstructure of a high strain-rate rolled Mg−Zn−Mn alloy was investigated by transmission electron microscopy to understand the relationship between the microstructure and mechanical properties. The results indicate that: (1) a bimodal microstructure consisting of the fine dynamic recrystallized grains and the largely deformed grains was formed; (2) a large number of dynamic precipitates including plate-like MgZn{sub 2} phase, spherical MgZn{sub 2} phase and spherical Mn particles distribute uniformly in the grains; (3) the major facets of many plate-like MgZn{sub 2} precipitates deviated several to tens of degrees (3°–30°) from the matrix basal plane. It has been shown that themore » high strength of the alloy is attributed to the formation of the bimodal microstructure, dynamic precipitation, and the interaction between the dislocations and the dynamic precipitates. - Highlights: •A bimodal microstructure was formed in a high strain-rate rolled Mg−Zn−Mn alloy. •Plate-like MgZn{sub 2}, spherical MgZn{sub 2} and spherical Mn phases were observed. •The major facet of the plate-like MgZn{sub 2} deviated from the matrix basal plane.« less

  1. Enhanced persistent red luminescence in Mn2+-doped (Mg,Zn)GeO3 by electron trap and conduction band engineering

    NASA Astrophysics Data System (ADS)

    Katayama, Yumiko; Kayumi, Tomohiro; Ueda, Jumpei; Tanabe, Setsuhisa

    2018-05-01

    The effect of Zn substitution on the persistent luminescence properties of MgGeO3:Mn2+-Ln3+ (Ln = Eu and Yb) red phosphors was investigated. The intensity of the persistent luminescence of the Eu3+ co-doped phosphors increased with increasing Zn content, whereas that of the Yb3+ co-doped samples decreased. For both series of lanthanide co-doped samples, the thermoluminescence (TL) glow peak shifted to the lower temperature side with increasing Zn content. These persistent luminescence properties were well explained in terms of lowering of the bottom of the conduction band relative to the ground state of the divalent lanthanide ions. Especially, in Eu3+ co-doped system, TL peak shifted from 520 K to 318 K by 50% Zn substitution. The persistent radiance of the (Mg0.5 Zn0.5)GeO3: Mn2+-Eu3+ sample at 1 h after ceasing UV light was 46 times stronger than that of MgGeO3:Mn2+-Eu3+, and 11 times stronger than that of ZnGa2O4: Cr3+ standard deep red persistent phosphor.

  2. Trace elements and radon in groundwater across the United States, 1992-2003

    USGS Publications Warehouse

    Ayotte, Joseph D.; Gronberg, Jo Ann M.; Apodaca, Lori E.

    2011-01-01

    Trace-element concentrations in groundwater were evaluated for samples collected between 1992 and 2003 from aquifers across the United States as part of the U.S. Geological Survey National Water-Quality Assessment Program. This study describes the first comprehensive analysis of those data by assessing occurrence (concentrations above analytical reporting levels) and by comparing concentrations to human-health benchmarks (HHBs). Data from 5,183 monitoring and drinking-water wells representing more than 40 principal and other aquifers in humid and dry regions and in various land-use settings were used in the analysis. Trace elements measured include aluminum (Al), antimony (Sb), arsenic (As), barium (Ba), beryllium (Be), boron (B), cadmium (Cd), chromium (Cr), cobalt (Co), copper (Cu), iron (Fe), lead (Pb), lithium (Li), manganese (Mn), molybdenum (Mo), nickel (Ni), selenium (Se), silver (Ag), strontium (Sr), thallium (Tl), uranium (U), vanadium (V), and zinc (Zn). Radon (Rn) gas also was measured and is included in the data analysis. Climate influenced the occurrence and distribution of trace elements in groundwater whereby more trace elements occurred and were found at greater concentrations in wells in drier regions of the United States than in humid regions. In particular, the concentrations of As, Ba, B, Cr, Cu, Mo, Ni, Se, Sr, U, V, and Zn were greater in the drier regions, where processes such as chemical evolution, ion complexation, evaporative concentration, and redox (oxidation-reduction) controls act to varying degrees to mobilize these elements. Al, Co, Fe, Pb, and Mn concentrations in groundwater were greater in humid regions of the United States than in dry regions, partly in response to lower groundwater pH and (or) more frequent anoxic conditions. In groundwater from humid regions, concentrations of Cu, Pb, Rn, and Zn were significantly greater in drinking-water wells than in monitoring wells. Samples from drinking-water wells in dry regions had greater concentrations of As, Ba, Pb, Li, Sr, V, and Zn, than samples from monitoring wells. In humid regions, however, concentrations of most trace elements were greater in monitoring wells than in drinking-water wells; the exceptions were Cu, Pb, Zn, and Rn. Cu, Pb, and Zn are common trace elements in pumps and pipes used in the construction of drinking-water wells, and contamination from these sources may have contributed to their concentrations. Al, Sb, Ba, B, Cr, Co, Fe, Mn, Mo, Ni, Se, Sr, and U concentrations were all greater in monitoring wells than in drinking-water wells in humid regions. Groundwater from wells in agricultural settings had greater concentrations of As, Mo, and U than groundwater from wells in urban settings, possibly owing to greater pH in the agricultural wells. Significantly greater concentrations of B, Cr, Se, Ag, Sr, and V also were found in agricultural wells in dry regions. Groundwater from dry-region urban wells had greater concentrations of Co, Fe, Pb, Li, Mn, and specific conductance than groundwater from agricultural wells. The geologic composition of aquifers and aquifer geochemistry are among the major factors affecting trace-element occurrence. Trace-element concentrations in groundwater were characterized in aquifers from eight major groups based on geologic material, including (1) unconsolidated sand and gravel; (2) glacial unconsolidated sand and gravel; (3) semiconsolidated sand; (4) sandstone; (5) sandstone and carbonate rock; (6) carbonate rock; (7) basaltic and other volcanic rock; and (8) crystalline rock. The majority of groundwater samples and the largest percentages of exceedences of HHBs were in the glacial and nonglacial unconsolidated sand and gravel aquifers; in these aquifers, As, Mn, and U are the most common trace elements exceeding HHBs. Overall, 19 percent of wells (962 of 5,097) exceeded an HHB for at least one trace element. The trace elements with HHBs included in this summary were Sb, As, Ba, Be, B, Cd, Cr,

  3. Effects of transition-metal ions on the morphology and electrochemical properties of δ-MnO2 for supercapacitors

    NASA Astrophysics Data System (ADS)

    Wang, Jia-Wei; Chen, Ya; Chen, Bai-Zhen

    2014-11-01

    δ-MnO2 materials doped with transition-metal cations (Zn, Co, and Ag) were successfully synthesized using a hydrothermal technique. The structures and morphologies of the obtained oxides were analyzed using X-ray diffraction, scanning electron microscopy and Brunauer-Emmett-Teller measurements. Additionally, the electrochemical properties were evaluated through cyclic voltammetry, electrochemical impedance spectroscopy and galvanostatic cycling measurements. The results indicate that the pure and doped samples crystallize in the δ form with a layered structure and that the Mn/Zn, Mn/Co and Mn/Ag molar ratios are all approximately 1:0.09. Both the Zn-doped and pure MnO2 materials exhibit a petal-like morphology; however, the former has a higher specific surface area of up to 98.97m2 g-1. Furthermore, the Zn-doped MnO2 exhibits a near-rectangular cyclic voltammetry (CV) curve with broad quasi-reversible redox peaks and a specific capacitance of 182.9 F g-1 at a CV scan rate of 2 mV s-1. The Co-doped material exhibits a distinct spiny-fiber morphology, and the electrochemical performance of this material is significantly worse than that of pure MnO2. The average attenuation rate of the Ag-doped material is only 0.028% after 1000 cycles, which is lower than that of pure MnO2.

  4. Various soil amendments and environmental wastes affect the (im)mobilization and phytoavailability of potentially toxic elements in a sewage effluent irrigated sandy soil.

    PubMed

    Shaheen, Sabry M; Shams, Mohamed S; Khalifa, Mohamed R; El-Dali, Mohamed A; Rinklebe, Jörg

    2017-08-01

    Contamination of long-term sewage effluent irrigated soils by potentially toxic elements (PTEs) is a serious concern due to its high environmental and health risk. Our scientific hypothesis is that soil amendments can cause contradictory effects on the element mobilization and phytoavailability depending on the type of element and amendment. Therefore, we aimed to assess the impact of the application (1%) of several low cost amendments and environmental wastes on the (im)mobilization, availability, and uptake of Al, Cd, Cr, Cu, Fe, Mn, Ni, and Zn by sorghum (Sorghum bicolor) in a long term sewage effluent irrigated sandy soils collected from Egypt. The used materials include activated charcoal (AC), potassium humate (KH), phosphate rock (PR), phosphogypsum (PG), triple superphosphate (TSP), phosphoric acid (PA), sulfur (S), sugar beet factory lime (SBFL), cement bypass kiln dust (CBD), egg shell (ES), bone mill (BM), brick factory residual (BFR), ceramic powder (CP), and drinking water treatment residual (WTR). The mobilization and availability of the elements in the soil were extracted using NH 4 NO 3 and ammonium bicarbonate- diethylene triamine penta acetic acid (AB-DTPA), respectively. The above-ground biomass samples were analyzed for the elements studied. The results confirmed our hypothesis and concluded that although some amendments like S, PA, and TSP can be used for reducing the plant uptake of Al, Cr, and Fe, they might be used with KH for enhancing the phytoextraction of Cd, Cu, Mn, and Ni. Moreover, several wastes such as BFR and WTR might be used for enhancing the phytoextraction of Al, Cd, Cr, Cu, Fe, and Ni and reducing the uptake of Mn from the studied soil. Although SBFL decreased the plant uptake of Al, Fe, Mn, and Zn, it's increased the plant uptake of Cd, Cu, and Ni. Therefore, the amendments which reduce the plant uptake of an element might be suitable candidates for its immobilization, while the amendments which increase the plant uptake of an element might be used for enhancing its phytoextraction when using bioenergy crops like sorghum in similar contaminated sandy soils. The studied materials offered the potential for effective and low cost media for the treatment of PTEs contaminated sewage effluent irrigated sandy soils. These results should be verified in a field study. Copyright © 2017 Elsevier Inc. All rights reserved.

  5. The effect of trace mineral source and concentration on ruminal digestion and mineral solubility.

    PubMed

    Genther, O N; Hansen, S L

    2015-01-01

    The objective of this experiment was to compare the effect of sources of sulfate trace mineral (STM) and hydroxy trace mineral (HTM) at different inclusions on digestibility of dry matter (DM) and neutral detergent fiber and solubility of Cu, Mn, and Zn in the rumen and abomasum of cattle. Five ruminally cannulated steers were used in a 5×5 Latin square design and individually fed a corn silage-based diet on an ad libitum basis. The 5 dietary treatments were as follows: control: no supplemental Cu, Mn, or Zn, analyzed to contain 7.4mg of Cu, 30.8mg of Mn, and 32.1mg of Zn per kilogram of diet DM (CON); low sulfate: 5mg of Cu/kg of DM supplemented from CuSO4, 15mg of Mn/kg of DM from MnSO4, and 30mg of Zn/kg of DM from ZnSO4; low HTM: 5mg of Cu/kg of DM supplemented from basic copper chloride (IntelliBond C; Micronutrients Inc., Indianapolis, IN), 15mg of Mn/kg of DM from manganese hydroxychloride (IntelliBond M; Micronutrients Inc.), and 30mg of Zn/kg of DM from zinc hydroxychloride (IntelliBond Z; Micronutrients Inc.); high sulfate: 25mg of Cu/kg of DM supplemented from CuSO4, 60mg of Mn/kg of DM from MnSO4, and 120mg of Zn/kg of DM from ZnSO4; and high HTM: 25mg of Cu/kg of DM supplemented from basic copper chloride, 60mg of Mn/kg of DM from manganese hydroxychloride, and 120mg of Zn/kg of DM from zinc hydroxychloride. Periods lasted for 12d, with 10d of diet adaptation. Dacron bags containing the CON total mixed ration were inserted on d 11 at 0h and were removed at 6, 12, 24, and 36h after insertion. Dry matter and neutral detergent fiber disappearances and rumen and simulated abomasal trace mineral solubilities were evaluated. Dietary treatment did not affect DM intake. Dry matter disappearance was lesser in supplemental TM treatments and greater in CON than the STM treatments, although the CON and HTM treatments did not differ. Neutral detergent fiber disappearance was not affected by treatment. Ruminally soluble Cu and Mn concentrations were least in CON and were lesser in HTM-containing treatments compared with STM treatments. However, in the abomasum, solubilities of Cu and Mn were similar across trace mineral sources. Ruminal and simulated abomasal soluble Zn was greater in the HTM treatments than in CON and STM, driven by the greater solubility of the high HTM treatment. Under the conditions of this study, supplementing trace minerals as STM decreased DM digestibility, whereas HTM did not affect DM digestibility. Additionally, Cu and Mn from HTM sources were relatively insoluble in the rumen but had similar solubility as STM at the pH found in the abomasum, suggesting that these minerals should be available for absorption in the intestine. Copyright © 2015 American Dairy Science Association. Published by Elsevier Inc. All rights reserved.

  6. Study of a QCM dimethyl methylphosphonate sensor based on a ZnO-modified nanowire-structured manganese dioxide film.

    PubMed

    Pei, Zhifu; Ma, Xingfa; Ding, Pengfei; Zhang, Wuming; Luo, Zhiyuan; Li, Guang

    2010-01-01

    Sensitive, selective and fast detection of chemical warfare agents is necessary for anti-terrorism purposes. In our search for functional materials sensitive to dimethyl methylphosphonate (DMMP), a simulant of sarin and other toxic organophosphorus compounds, we found that zinc oxide (ZnO) modification potentially enhances the absorption of DMMP on a manganese dioxide (MnO(2)) surface. The adsorption behavior of DMMP was evaluated through the detection of tiny organophosphonate compounds with quartz crystal microbalance (QCM) sensors coated with ZnO-modified MnO(2) nanofibers and pure MnO(2) nanofibers. Experimental results indicated that the QCM sensor coated with ZnO-modified nanostructured MnO(2) film exhibited much higher sensitivity and better selectivity in comparison with the one coated with pure MnO(2) nanofiber film. Therefore, the DMMP sensor developed with this composite nanostructured material should possess excellent selectivity and reasonable sensitivity towards the tiny gaseous DMMP species.

  7. Electrochemical evaluation of manganese reducers - Recovery of Mn from Zn-Mn and Zn-C battery waste

    NASA Astrophysics Data System (ADS)

    Sobianowska-Turek, Agnieszka; Szczepaniak, Włodzimierz; Zabłocka-Malicka, Monika

    2014-12-01

    Extraction of manganese from ores or battery waste involves the use of reductive reagents for transformation of MnO2 to Mn2+ ions. There are many reducers, both organic and inorganic, described in the literature. A series of 18 reducers has been discussed in the paper and they were classified according to standard redox potential (pE = -log ae- where pE is used to express formal electron activity and ae- is formal electron activity). The experiments of manganese extraction from paramagnetic fraction of Zn-C and Zn-Mn battery waste in the laboratory scale have been described for 3 reducers of different origin. The best result was achieved with oxalic acid (75%, with the lowest redox potential) and urea (with typical redox potential) appeared inactive. Extraction supported by hydrogen peroxide resulted in moderate yield (50%). It shows that formal thermodynamic scale is only preliminary information useful for selection of possible reducers for manganese extraction resources.

  8. Study of a QCM Dimethyl Methylphosphonate Sensor Based on a ZnO-Modified Nanowire-Structured Manganese Dioxide Film

    PubMed Central

    Pei, Zhifu; Ma, Xingfa; Ding, Pengfei; Zhang, Wuming; Luo, Zhiyuan; Li, Guang

    2010-01-01

    Sensitive, selective and fast detection of chemical warfare agents is necessary for anti-terrorism purposes. In our search for functional materials sensitive to dimethyl methylphosphonate (DMMP), a simulant of sarin and other toxic organophosphorus compounds, we found that zinc oxide (ZnO) modification potentially enhances the absorption of DMMP on a manganese dioxide (MnO2) surface. The adsorption behavior of DMMP was evaluated through the detection of tiny organophosphonate compounds with quartz crystal microbalance (QCM) sensors coated with ZnO-modified MnO2 nanofibers and pure MnO2 nanofibers. Experimental results indicated that the QCM sensor coated with ZnO-modified nanostructured MnO2 film exhibited much higher sensitivity and better selectivity in comparison with the one coated with pure MnO2 nanofiber film. Therefore, the DMMP sensor developed with this composite nanostructured material should possess excellent selectivity and reasonable sensitivity towards the tiny gaseous DMMP species. PMID:22163653

  9. Time and temperature dependent breakdown characteristics of ZnS:Mn films obtained by rf-magnetron sputtering

    NASA Astrophysics Data System (ADS)

    Zhigal'Skii, A. A.; Mukhachev, V. A.; Troyan, P. E.

    1994-04-01

    Breakdown delay times (tdel) for films of managanese-doped zinc sulfide (ZnS:Mn) were measured in the range 10-6-10-1 s. The maximum value was tdel=10-3-10-2 s. The electrical strength (Ebr) was found to increase as the voltage pulse duration was reduced, the more so the thinner the ZnS:Mn film. The temperature dependence of Ebr exhibited a weak reduction in Ebr as the temperature was raised to roughly 80°C and a sharp reduction in Ebr for T>130°C. A maximum in Ebr was observed at T≈130°C which is presumably explained by a structural modification of the ZnS:Mn film. The experimental results obtained are explained in terms of a combined electronic and thermal breakdown mechanism.

  10. Application of L-Aspartic Acid-Capped ZnS:Mn Colloidal Nanocrystals as a Photosensor for the Detection of Copper (II) Ions in Aqueous Solution

    PubMed Central

    Heo, Jungho; Hwang, Cheong-Soo

    2016-01-01

    Water-dispersible ZnS:Mn nanocrystals (NCs) were synthesized by capping the surface with polar L-aspartic acid (Asp) molecules. The obtained ZnS:Mn-Asp NC product was optically and physically characterized using the corresponding spectroscopic methods. The ultra violet-visible (UV-VIS) absorption spectrum and photoluminescence (PL) emission spectrum of the NCs showed broad peaks at 320 and 590 nm, respectively. The average particle size measured from the obtained high resolution-transmission electron microscopy (HR-TEM) image was 5.25 nm, which was also in accordance with the Debye-Scherrer calculations using the X-ray diffraction (XRD) data. Moreover, the surface charge and degree of aggregation of the ZnS:Mn-Asp NCs were determined by electrophoretic and hydrodynamic light scattering methods, respectively. These results indicated the formation of agglomerates in water with an average size of 19.8 nm, and a negative surface charge (−4.58 mV) in water at ambient temperature. The negatively-charged NCs were applied as a photosensor for the detection of specific cations in aqueous solution. Accordingly, the ZnS:Mn-Asp NCs showed an exclusive luminescence quenching upon addition of copper (II) cations. The kinetic mechanism study on the luminescence quenching of the NCs by the addition of the Cu2+ ions proposed an energy transfer through the ionic binding between the two oppositely-charged ZnS:Mn-Asp NCs and Cu2+ ions. PMID:28335210

  11. Nonplasmonic Hot-Electron Photocurrents from Mn-Doped Quantum Dots in Photoelectrochemical Cells.

    PubMed

    Dong, Yitong; Rossi, Daniel; Parobek, David; Son, Dong Hee

    2016-03-03

    We report the measurement of the hot-electron current in a photoelectrochemical cell constructed from a glass/ITO/Al2 O3 (ITO=indium tin oxide) electrode coated with Mn-doped quantum dots, where hot electrons with a large excess kinetic energy were produced through upconversion of the excitons into hot electron hole pairs under photoexcitation at 3 eV. In our recent study (J. Am. Chem. Soc. 2015, 137, 5549), we demonstrated the generation of hot electrons in Mn-doped II-VI semiconductor quantum dots and their usefulness in photocatalytic H2 production reaction, taking advantage of the more efficient charge transfer of hot electrons compared with band-edge electrons. Here, we show that hot electrons produced in Mn-doped CdS/ZnS quantum dots possess sufficient kinetic energy to overcome the energy barrier from a 5.4-7.5 nm thick Al2 O3 layer producing a hot-electron current in photoelectrochemical cell. This work demonstrates the possibility of harvesting hot electrons not only at the interface of the doped quantum dot surface, but also far away from it, thus taking advantage of the capability of hot electrons for long-range electron transfer across a thick energy barrier. © 2016 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.

  12. Enhanced magnetic properties in Mn0.6Zn0.4-xNixFe2O4 (x=0-0.4) nanoparticles

    NASA Astrophysics Data System (ADS)

    Mallesh, S.; Mandal, P.; Srinivas, V.

    2018-04-01

    Ni substituted MnZn ferrite fine particles were synthesized through sol-gel method. The structure, stability and magnetic properties have been investigated. Thermal stability of as-prepared (AP) particles is improved compared to that of Mn0.6Zn0.4Fe2O4 (MZF) ferrite particles. The as-prepared and samples annealed at 1200 °C exhibit pure spinel ferrite phase, while samples at intermediate temperatures (600 - 1000 °C) exhibit secondary phase of α-Fe2O3 along with ferrite phase. The Mn0.6Zn0.1Ni0.3Fe2O4 (Ni-MZF) sample shows significantly lower volume fraction of secondary phase compared to that of MZF. The observed magnetization of Ni-MZF is twice of that MZF samples. Present results suggest that a small amount (x=0.3) of Ni in place of nonmagnetic Zn in MZF significantly decreases the secondary phase fraction and improves the magnetic properties.

  13. Effect of heavy-metal on synthesis of siderophores by Pseudomonas aeruginosa ZGKD3

    NASA Astrophysics Data System (ADS)

    Shi, Peili; Xing, Zhukang; Zhang, Yuxiu; Chai, Tuanyao

    2017-01-01

    Most siderophore-producing bacteria could improve the plant growth. Here, the effect of heavy-metal on the growth, total siderophore and pyoverdine production of the Cd tolerance Pseudomonas aeruginosa ZGKD3 were investigated. The results showed that ZGKD3 exhibited tolerance to heavy metals, and the metal tolerance decreased in the order Mn2+>Pb2+>Ni2+>Cu2+>Zn2+>Cd2+. The total siderophore and pyoverdine production of ZGKD3 induced by metals of Cd2+, Cu2+, Zn2+, Ni2+, Pb2+ and Mn2+ were different, the total siderophore and pyoverdine production reduced in the order Cd2+>Pb2+>Mn2+>Ni2+>Zn2+ >Cu2+ and Zn2+>Cd2+>Mn2+>Pb2+>Ni2+>Cu2+, respectively. These results suggested that ZGKD3 could grow in heavy-metal contaminated soil and had the potential of improving phytoremediation efficiency in Cd and Zn contaminated soils.

  14. Novel room temperature ferromagnetic semiconductors

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Gupta, Amita

    2004-06-01

    Today's information world, bits of data are processed by semiconductor chips, and stored in the magnetic disk drives. But tomorrow's information technology may see magnetism (spin) and semiconductivity (charge) combined in one 'spintronic' device that exploits both charge and 'spin' to carry data (the best of two worlds). Spintronic devices such as spin valve transistors, spin light emitting diodes, non-volatile memory, logic devices, optical isolators and ultra-fast optical switches are some of the areas of interest for introducing the ferromagnetic properties at room temperature in a semiconductor to make it multifunctional. The potential advantages of such spintronic devices will bemore » higher speed, greater efficiency, and better stability at a reduced power consumption. This Thesis contains two main topics: In-depth understanding of magnetism in Mn doped ZnO, and our search and identification of at least six new above room temperature ferromagnetic semiconductors. Both complex doped ZnO based new materials, as well as a number of nonoxides like phosphides, and sulfides suitably doped with Mn or Cu are shown to give rise to ferromagnetism above room temperature. Some of the highlights of this work are discovery of room temperature ferromagnetism in: (1) ZnO:Mn (paper in Nature Materials, Oct issue, 2003); (2) ZnO doped with Cu (containing no magnetic elements in it); (3) GaP doped with Cu (again containing no magnetic elements in it); (4) Enhancement of Magnetization by Cu co-doping in ZnO:Mn; (5) CdS doped with Mn, and a few others not reported in this thesis. We discuss in detail the first observation of ferromagnetism above room temperature in the form of powder, bulk pellets, in 2-3 mu-m thick transparent pulsed laser deposited films of the Mn (<4 at. percent) doped ZnO. High-resolution transmission electron microscopy (HRTEM) and electron energy loss spectroscopy (EELS) spectra recorded from 2 to 200nm areas showed homogeneous distribution of Mn substituting for Zn a 2 + state in the ZnO lattice. Ferromagnetic Resonance (FMR) technique is used to confirm the existence of ferromagnetic ordering at temperatures as high as 425K. The ab initio calculations were found to be consistent with the observation of ferromagnetism arising from fully polarized Mn 2 + state. The key to observed room temperature ferromagnetism in this system is the low temperature processing, which prevents formation of clusters, secondary phases and the host ZnO from becoming n-type. The electronic structure of the same Mn doped ZnO thin films studied using XAS, XES and RIXS, revealed a strong hybridization between Mn 3d and O 2p states, which is an important characteristic of a Dilute magnetic Semiconductor (DMS). It is shown that the various processing conditions like sintering temperature, dopant concentration and the properties of precursors used for making of DMS have a great influence on the final properties. Use of various experimental techniques to verify the physical properties, and to understand the mechanism involved to give rise to ferromagnetism is presented. Methods to improve the magnetic moment in Mn doped ZnO are also described. New promising DMS materials (such as Cu doped ZnO are explored). The demonstrated new capability to fabricate powder, pellets, and thin films of room temperature ferromagnetic semiconductors thus makes possible the realization of a wide range of complex elements for a variety of new multifunctional phenomena related to Spintronic devices as well as magneto-optic components.« less

  15. Physical properties of antiferromagnetic Mn doped ZnO samples: Role of impurity phase

    NASA Astrophysics Data System (ADS)

    Neogi, S. K.; Karmakar, R.; Misra, A. K.; Banerjee, A.; Das, D.; Bandyopadhyay, S.

    2013-11-01

    Structural, morphological, optical, and magnetic properties of nanocrystalline Zn1-xMnxO samples (x=0.01, 0.02, 0.04, 0.06, 0.08 and 0.10) prepared by the sol-gel route are studied by X-ray diffraction (XRD), Scanning electron microscopy (SEM), UV-visible absorption spectroscopy, Superconducting quantum interference device (SQUID) magnetometry and positron annihilation lifetime spectroscopy (PALS). XRD confirms formation of wurzite structure in all the Mn-substituted samples. A systematic increase in lattice constants and decrease in grain size have been observed with increase in manganese doping concentration up to 6 at% in the ZnO structure. An impurity phase (ZnMnO3) has been detected when percentage of Mn concentration is 6 at% or higher. The optical band gap of the Mn-substituted ZnO samples decrease with increase in doping concentration of manganese whereas the width of the localized states increases. The antiferromagnetic exchange interaction is strong in the samples for 2 and 4 at% of Mn doping but it reduces when the doping level increases from 6 at% and further. Positron life time components τ1 and τ2 are found to decrease when concentration of the dopant exceeds 6 at%. The changes in magnetic properties as well as positron annihilation parameters at higher manganese concentration have been assigned as due to the formation of impurity phase. Single phase structure has been observed up to 6 at% of Mn doping. Impurity phase has been developed above 6 at% of Mn doping. Antiferromagnetic and paramagnetic interactions are present in the samples. Defect parameters show sharp fall as Mn concentration above 6 at%. The magnetic and defect properties are modified by the formation of impurity phase.

  16. Synergistic effect of N-decorated and Mn2+ doped ZnO nanofibers with enhanced photocatalytic activity

    PubMed Central

    Wang, Yuting; Cheng, Jing; Yu, Suye; Alcocer, Enric Juan; Shahid, Muhammad; Wang, Ziyuan; Pan, Wei

    2016-01-01

    Here we report a high efficiency photocatalyst, i.e., Mn2+-doped and N-decorated ZnO nanofibers (NFs) enriched with vacancy defects, fabricated via electrospinning and a subsequent controlled annealing process. This nanocatalyst exhibits excellent visible-light photocatalytic activity and an apparent quantum efficiency up to 12.77%, which is 50 times higher than that of pure ZnO. It also demonstrates good stability and durability in repeated photocatalytic degradation experiments. A comprehensive structural analysis shows that high density of oxygen vacancies and nitrogen are introduced into the nanofibers surface. Hence, the significant enhanced visible photocatalytic properties for Mn-ZnO NFs are due to the synergetic effects of both Mn2+ doping and N decorated. Further investigations exhibit that the Mn2+-doping facilitates the formation of N-decorated and surface defects when annealing in N2 atmosphere. N doping induce the huge band gap decrease and thus significantly enhance the absorption of ZnO nanofibers in the range of visible-light. Overall, this paper provides a new approach to fabricate visible-light nanocatalysts using both doping and annealing under anoxic ambient. PMID:27600260

  17. Heavy metal pollution of coal mine-affected agricultural soils in the northern part of Bangladesh.

    PubMed

    Bhuiyan, Mohammad A H; Parvez, Lutfar; Islam, M A; Dampare, Samuel B; Suzuki, Shigeyuki

    2010-01-15

    Total concentrations of heavy metals in the soils of mine drainage and surrounding agricultural fields in the northern part of Bangladesh were determined to evaluate the level of contamination. The average concentrations of Ti, Mn, Zn, Pb, As, Fe, Rb, Sr, Nb and Zr exceeded the world normal averages and, in some cases, Mn, Zn, As and Pb exceeded the toxic limit of the respective metals. Soil pollution assessment was carried out using enrichment factor (EF), geoaccumulation index (I(geo)) and pollution load index (PLI). The soils show significant enrichment with Ti, Mn, Zn, Pb, As, Fe, Sr and Nb, indicating inputs from mining activities. The I(geo) values have revealed that Mn (1.24+/-0.38), Zn (1.49+/-0.58) and Pb (1.63+/-0.38) are significantly accumulated in the study area. The PLIs derived from contamination factors indicate that the distal part of the coal mine-affected area is the most polluted (PLI of 4.02). Multivariate statistical analyses, principal component and cluster analyses, suggest that Mn, Zn, Pb and Ti are derived from anthropogenic sources, particularly coal mining activities, and the extreme proximal and distal parts are heavily contaminated with maximum heavy metals.

  18. Metal concentrations of wild edible mushrooms from Turkey.

    PubMed

    Sarikurkcu, Cengiz; Tepe, Bektas; Solak, Mehmet Halil; Cetinkaya, Serap

    2012-01-01

    In the present study, the contents of Zn, Fe, Cu, Mn, Co, Ni, Pb, Cd, Cr, Al, Ca, Mg, and K in Agaricus campestris, Agrocybe cylindracea, Collybia dryophila, Helvella leucopus, Russula delica, Tricholoma auratum, Amanita ovoidea, Melanoleuca excissa, Rhizopogon roseolus, Russula chloroides, Volvoriella gloiocephala, Lyophyllum decastes, Morcella angusticeps, Morchella esculenta and Morcella eximia collected from Isparta, Mugla, and Osmaniye provinces (Turkey) were determined by inductively coupled plasma optical emission spectrometry (ICP-OES) after microwave digestion. The intake of heavy metals (Pb, Cd) and other metals (Fe, Cu, Zn) by consumption of 30 g dry weight of mushrooms daily poses no risk at all except in A. cylindracea and H. leucopus (for Cd) for the consumer.

  19. The influence of manganese treatment on the distribution of metal elements in rats and the protection by sodium para-amino salicylic acid.

    PubMed

    Yuan, Zong-Xiang; Chen, Hai-Bin; Li, Shao-Jun; Huang, Xiao-Wei; Mo, Yu-Huan; Luo, Yi-Ni; He, Sheng-Nan; Deng, Xiang-Fa; Lu, Guo-Dong; Jiang, Yue-Ming

    2016-07-01

    Manganese (Mn) overexposure induced neurological damages, which could be potentially protected by sodium para-aminosalicylic acid (PAS-Na). In this study, we systematically detected the changes of divalent metal elements in most of the organs and analyzed the distribution of the metals in Mn-exposed rats and the protection by PAS-Na. Sprague Dawley (SD) rats received intraperitoneal injections of 15mg/kg MnCl2·4H2O (5d/week for 3 weeks), followed by subcutaneous (back) injections of PAS-Na (100 and 200mg/kg, everyday for 5 weeks). The concentrations of Mn and other metal elements [Iron (Fe), Copper (Cu), Zinc (Zn), Magnesium (Mg), Calcium (Ca)] in major organs (liver, spleen, kidney, thighbone and iliac bone, cerebral cortex, hippocampus and testes) and blood by Inductively Coupled Plasma-Atomic Emission Spectrometry (ICP-AES). The results showed that Mn overexposure significantly increased Mn in most organs, Fe and Zn in liver, Fe and Mg in blood; however decreased Fe, Cu, Zn, Mg and Ca in cortex, Cu and Zn in kidney, Cu and Mg in iliac bone, and Zn in blood. In contrast, PAS-Na treatment restored most changes particularly in cortex. In conclusion, excessive Mn exposure disturbed the balance of other metal elements but PAS-Na post-treatments could restore these alterations. Copyright © 2016 Elsevier GmbH. All rights reserved.

  20. X-ray photoelectron spectroscopy and friction studies of nickel-zinc and manganese-zinc ferrites in contact with metals

    NASA Technical Reports Server (NTRS)

    Miyoshi, K.; Buckley, D. H.

    1983-01-01

    X-ray photoelectron spectroscopy analysis and sliding friction experiments were conducted with hot-pressed, polycrystalline Ni-Zn and Mn-Zn ferrites in sliding contact with various transition metals at room temperature in a vacuum of 30 nPa. The results indicate that the coefficients of friction for Ni-Zn and Mn-Zn ferrites in contact with metals are related to the relative chemical activity in these metals: the more active the metal, the higher is the coefficient of friction. The coefficients of friction for the ferrites correlate with the free energy of formation of the lowest metal oxide. The interfacial bond can be regarded as a chemical bond between the metal atoms and the oxygen anions in the ferrite surfaces. The adsorption of oxygen on clean metal and ferrite surfaces increases the coefficients of friction for the Ni-Zn and Mn-Zn ferrite-metal interfaces.

  1. Effect of chromium doping on the structural and vibrational properties of Mn-Zn ferrites

    NASA Astrophysics Data System (ADS)

    Saleem, M.; Varshney, Dinesh

    2018-05-01

    The synthesis of Mn0.5Zn0.5-xCrxFe2O4 (x = 0.0, 0.1, 0.2 and 0.5) via sol-gel Auto-combustion technique is reported. The x-ray diffraction spectra analysis revealed the cubic spinel structure for all the prepared spinel ferrite samples with the space group Fd3m. The structural studies identify the decrease of lattice parameter however the crystallite size decreases on increasing the Cr concentration. The Raman spectrum reveals five active phonon modes at room temperature and shifting of modes toward the higher frequency side on moving from Mn-ZnFe2O4 to Mn-CrFe2O4.

  2. White light emission from Mn2 + doped ZnS nanocrystals through the surface chelating of 8-hydroxyquinoline-5-sulfonic acid

    NASA Astrophysics Data System (ADS)

    Lü, Xiaodan; Yang, Jing; Fu, Yuqin; Liu, Qianqian; Qi, Bin; Lü, Changli; Su, Zhongmin

    2010-03-01

    White light emitting semiconductor nanocrystals (NCs) have been successfully synthesized from 8-hydroxyquinoline-5-sulfonic acid (HQS) decorated manganese doped ZnS NCs through fine tuning the surface-coordination emission and dopant emission of the NC host. The HQS functionalized manganese doped ZnS NCs (QS-ZnS:Mn), with a cubic crystal structure, have the same diameter of about 4.0 nm as ZnS:Mn NCs without HQS. The intensity of the surface-coordination emission peak increased with increasing HQS content or augmenting excited wavelength. The emission of white light was achieved by carefully controlling the dosage of HQS in NCs and appropriately tuning the excited wavelength. The color coordinates (0.35, 0.34) for the efficient white light emitting NCs were very close to the ideal Commission Internationale de l'Eclairage (CIE) chromaticity coordinates for pure white light (0.33, 0.33). The photoluminescence (PL) decay study revealed that the white light emitting NCs exhibited maximum lifetime values at different emission peaks for different NC samples. The study results also indicated that the HQS molecules were attached to the surface of ZnS:Mn NCs in a single coordination fashion due to the steric hindrance effect of the special spherical surface of NCs, which made the QS-ZnS:Mn NCs possess stable and high fluorescent properties in different organic solvents as compared with the conventional small molecule complexes.

  3. Evaluation of the SO(2) and NH(3) gas adsorption properties of CuO/ZnO/Mn(3)O(4) and CuO/ZnO/NiO ternary impregnated activated carbon using combinatorial materials science methods.

    PubMed

    Romero, Jennifer V; Smith, Jock W H; Sullivan, Braden M; Macdonald, Landan; Croll, Lisa M; Dahn, J R

    2013-02-11

    Impregnated activated carbons (IAC) are widely used materials for the removal of toxic gases in personal respiratory protection applications. The combinatorial method has been employed to prepare IACs containing different types of metal oxides in various proportions and evaluate their adsorption performance for low molecular weight gases, such as SO(2) and NH(3), under dry conditions. Among the metal oxides used for the study, Mn(3)O(4) was found to have the highest capacity for retaining SO(2) gas under dry conditions. NiO and ZnO were found to have similar NH(3) adsorption capacities which are higher than the NH(3) capacities observed for the other metal oxide impregnants used in the study. Although Cu- or Zn-based impregnants and their combinations have been extensively studied and used as gas adsorbents, neither Mn(3)O(4) nor NiO have been incorporated in the formulations used. In this study, ternary libraries of IACs with various combinations of CuO/ZnO/Mn(3)O(4) and CuO/ZnO/NiO were studied and evaluated for their adsorption of SO(2) and NH(3) gases. Combinations of CuO, ZnO, and Mn(3)O(4) were found to have the potential to be multigas adsorbents compared to formulations that contain NiO.

  4. Comparison of dry, wet and microwave digestion methods for the multi element determination in some dried fruit samples by ICP-OES.

    PubMed

    Altundag, Huseyin; Tuzen, Mustafa

    2011-11-01

    The aim of this study was used to investigate the level of trace metals (Ba, Pb, Cd, Mn, Cr, Co, Ni, Cu, Mn, Zn, Sr and Fe) in some dried fruits (Prunus domestica L., Ficus carica L., Morus alba L., Vitis vinifera L., Prunus armeniaca L., and Malus domestica) samples from Turkey. Trace elements were determined by ICP-OES after dry, wet and microwave digestion methods in dried fruit samples. Validation of the proposed method was carried out by using a NIST-SRM 1515-Apple Leaves certified reference material. Element concentrations in dried fruit samples were 0.33-1.77 (Ba), 0.12-0.54 (Cd), 0.25-1.03 (Co), 0.45-2.30 (Cr), 0.43-2.74 (Cu), 0.56-4.87 (Mn), 0.61-2.54 (Ni), 0.40-2.14 (Pb), 2.16-6.54 (Zn), 0.83-12.02 (Al), 11.82-40.80 (Fe) and 0.16-6.34 (Sr) μg/g. The analytical parameters show that the microwave oven digestion procedure provided best results as compared to the wet and dry digestion procedures. The results were compared with the literature values. Copyright © 2011 Elsevier Ltd. All rights reserved.

  5. Ultrahigh-resolution crystal structures of Z-DNA in complex with Mn(2+) and Zn(2+) ions.

    PubMed

    Drozdzal, Pawel; Gilski, Miroslaw; Kierzek, Ryszard; Lomozik, Lechoslaw; Jaskolski, Mariusz

    2013-06-01

    X-ray crystal structures of the spermine(4+) form of the Z-DNA duplex with the self-complementary d(CG)3 sequence in complexes with Mn(2+) and Zn(2+) cations have been determined at the ultrahigh resolutions of 0.75 and 0.85 Å, respectively. Stereochemical restraints were only used for the sperminium cation (in both structures) and for nucleotides with dual conformation in the Zn(2+) complex. The Mn(2+) and Zn(2+) cations at the major site, designated M(2+)(1), bind at the N7 position of G6 by direct coordination. The coordination geometry of this site was octahedral, with complete hydration shells. An additional Zn(2+)(2) cation was bis-coordinated in a tetrahedral fashion by the N7 atoms of G10 and G12 from a symmetry-related molecule. The coordination distances of Zn(2+)(1) and Zn(2+)(2) to the O6 atom of the guanine residues were 3.613 (6) and 3.258 (5) Å, respectively. Moreover, a chloride ion was also identified in the coordination sphere of Zn(2+)(2). Alternate conformations were observed in the Z-DNA-Zn(2+) structure not only at internucleotide linkages but also at the terminal C3'-OH group of G12. The conformation of the sperminium chain in the Z-DNA-Mn(2+) complex is similar to the spermine(4+) conformation in analogous Z-DNA-Mg(2+) structures. In the Z-DNA-Zn(2+) complex the sperminium cation is disordered and partially invisible in electron-density maps. In the Z-DNA-Zn(2+) complex the sperminium cation only interacts with the phosphate groups of the Z-DNA molecules, while in the Z-DNA-Mn(2+) structure it forms hydrogen bonds to both the phosphate groups and DNA bases.

  6. Different magnetic origins of (Mn, Fe)-codoped ZnO powders and thin films

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Fan, Jiuping; Jiang, Fengxian; Quan, Zhiyong

    2012-11-15

    Graphical abstract: The effects of the sample forms, fabricated methods, and process conditions on the structural and magnetic properties of (Mn, Fe)-codoped ZnO powders and films were systematically studied. The origins of ferromagnetism in the vacuum-annealed powder and PLD-deposited film are different. The former originates from the impurities of magnetic clusters, whereas the latter comes from the almost homogenous phase. Highlights: ► The magnetic natures of Zn{sub 0.98}Mn{sub 0.01}Fe{sub 0.01}O powders and thin films come from different origins. ► The ferromagnetism of the powder is mainly from the contribution of magnetic clusters. ► Whereas the ferromagnetic behavior of the filmmore » comes from the almost homogenous phase. -- Abstract: The structural and magnetic properties of (Mn, Fe)-codoped ZnO powders as well as thin films were investigated. The X-ray diffraction and magnetic measurements indicated that the higher sintering temperature facilitates more Mn and Fe incorporation into ZnO. Magnetic measurements indicated that the powder sintered in air at 800 °C showed paramagnetic, but it exhibited obvious room temperature ferromagnetism after vacuum annealing at 600 °C. The results revealed that magnetic clusters were the major contributors to the observed ferromagnetism in vacuum-annealed Zn{sub 0.98}Mn{sub 0.01}Fe{sub 0.01}O powder. Interestingly, the room temperature ferromagnetism was also observed in the Zn{sub 0.98}Mn{sub 0.01}Fe{sub 0.01}O film deposited via pulsed laser deposition from the air-sintered paramagnetic target, but the secondary phases in the film were not detected from X-ray diffraction, transmission electron microscopy, and zero-field cooling and field cooling. Apparently, the magnetic natures of powders and films come from different origins.« less

  7. L-serine capped ZnS:Mn nanocrystals for plant cell biological studies and as a growth enhancing agent for micropropagation of Bacopa monnieri Linn. (Brahmi:Scrophulariaceae)

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Augustine, M. Sajimol, E-mail: sajimollazar@gmail.com; Mathew, Lizzy; Alex, Roselin

    2014-01-28

    In the present work, the prospects of ZnS:Mn nanocrystals capped with L- serine, a bio-compatible amino acid, synthesized by wet chemical route, as efficient fluorescent probes for plant cell biological studies have been investigated. The present synthesis route using bio-compatible material is a low cost and easy to control method. The colloidal stability of the capped nano crystals is very good as they remain stable without settling down for long time. It is observed that L- serine significantly modifies the structural and optical characteristics of the ZnS:Mn nanocrystals and hence is suitable as a bio-compatible capping agent. The structural propertiesmore » of L- serine capped nanocrystals were investigated by XRD technique. The size of the L- serine capped ZnS:Mn nanocrystals is found to be around 2 nm . The optical characterization of the nanocrystals was carried out on the basis of photoluminescence (PL) spectroscopic studies. The intense photoluminescence emission observed around 597nm for L-serine capped ZnS:Mn offers high prospects of applications in bio-imaging fields. The unique optical properties of nanoparticles make them appealing as in vivo and in vitro fluorophores in a variety of biological investigations. In the present study, L-serine capped ZnS:Mn nanocrystals were used as a staining dye in fluorescent microscope for observing cell division, cell structure etc. These nanocrystals were also incorporated into the culture media along with the normal auxin- cytokinin hormone combinations in Murashige and Skoog (MS) medium for micropropagation of Bacopa monnieri Linn. (Brahmi:Scrophulariaceae), an Ayurvedic medicine. The results suggest that L-serine capped ZnS:Mn nanocrystals can act as efficient enhancers towards quick callusing and shoot proliferation.« less

  8. Aerosol characteristics and sources for the Amazon basin during the wet season

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Artaxo, P.; Maenhaut, W.; Storms, H.

    1990-09-20

    Fine (< 2.0 {mu}m) and coarse (2.0 - 15 {mu}m) aerosol fractions were collected using stacked filter units, at three sites under the forest canopy and at three levels of a tower inside the jungle. Particle-induced x-ray emission (PIXE) was used to measure concentrations Na, Mg, Al, Si, P, S, Cl, K, Ca, Ti, V, Cr, Mn, Fe, Ni, Cu, Zn, Br, Rb, Sr, Zr, and Pb. Morphological and trace element measurements of individual particles were carried out by automated electron probe x-ray microanalysis. Gravimetric analysis was performed to obtain the fine and coarse aerosol mass concentration. The concentrations ofmore » soil dust related elements (Al, Si, Ti, Fe, Mn) were 5 times larger in the wet season compared to the 1985 ABLE 2A dry season experiment. Biogenic aerosol related elements in the fine fraction showed lower concentrations in the wet season. Fine aerosol mass concentration averaged only 2.1 {plus minus} 0.7 {mu}g m{sup {minus}3}, while the average coarse mass concentration was 6.1 {plus minus} 1.8 {mu}g m{sup {minus}3}. Sulfur concentrations averaged 76 {plus minus} 14 ng m{sup {minus}3} in the fine fraction and 37 {plus minus} 9 ng m{sup {minus}3} in the coarse fraction. Only two factors explained about 90% of the data variability for the fine and coarse aerosol fractions. These were soil dust (represented mainly by Al, Si, Ti, Mn, and Fe) and biogenic aerosol (represented by K, P, Cl, S, Zn, and the aerosol mass concentration). Biogenic particles account for 55-95% of the airborne concentrations and consisted of leaf fragments, pollen grains, fungi, algae, and other types of particles. It is possible that biogenic particles can play an important role in the global aerosol budget and in the global biogeochemical cycles of various elements.« less

  9. Ultra-tiny ZnMn2O4 nanoparticles encapsulated in sandwich-like carbon nanosheets for high-performance supercapacitors.

    PubMed

    Guan, Yongxin; Feng, Yangyang; Mu, Yanping; Fang, Ling; Zhang, Huijuan; Wang, Yu

    2016-11-25

    Known as an excellent energy storage material, ZnMn 2 O 4 has a wide range of applications in supercapacitors. In this report, a special sandwich-like structure of ZnMn 2 O 4 /C has been first designed and synthesized via a simple hydrothermal method and subsequent calcinations. The designed special sandwich-like structure can benefit ion exchange and remit the probable volume changes during a mass of electrochemical reactions. Furthermore, the porous carbon nanosheets, derived from low-cost glucose, can effectively increase ion flux. Therefore, the novel sandwich-like ZnMn 2 O 4 nanoparticles encapsulated in carbon nanosheets can undoubtedly demonstrate an exceptional electrochemical performance for SCs. In this work, the composite material with porous sandwich-like structure exhibits excellent cyclic stability for 5000 cycles (∼5% loss) and high specific capacitance of 1786 F g -1 .

  10. Ultra-tiny ZnMn2O4 nanoparticles encapsulated in sandwich-like carbon nanosheets for high-performance supercapacitors

    NASA Astrophysics Data System (ADS)

    Guan, Yongxin; Feng, Yangyang; Mu, Yanping; Fang, Ling; Zhang, Huijuan; Wang, Yu

    2016-11-01

    Known as an excellent energy storage material, ZnMn2O4 has a wide range of applications in supercapacitors. In this report, a special sandwich-like structure of ZnMn2O4/C has been first designed and synthesized via a simple hydrothermal method and subsequent calcinations. The designed special sandwich-like structure can benefit ion exchange and remit the probable volume changes during a mass of electrochemical reactions. Furthermore, the porous carbon nanosheets, derived from low-cost glucose, can effectively increase ion flux. Therefore, the novel sandwich-like ZnMn2O4 nanoparticles encapsulated in carbon nanosheets can undoubtedly demonstrate an exceptional electrochemical performance for SCs. In this work, the composite material with porous sandwich-like structure exhibits excellent cyclic stability for 5000 cycles (˜5% loss) and high specific capacitance of 1786 F g-1.

  11. Non-adiabatic molecular dynamics investigation of photoionization state formation and lifetime in Mn²⁺-doped ZnO quantum dots.

    PubMed

    Fischer, Sean A; Lingerfelt, David B; May, Joseph W; Li, Xiaosong

    2014-09-07

    The unique electronic structure of Mn(2+)-doped ZnO quantum dots gives rise to photoionization states that can be used to manipulate the magnetic state of the material and to generate zero-reabsorption luminescence. Fast formation and long non-radiative decay of this photoionization state is a necessary requirement for these important applications. In this work, surface hopping based non-adiabatic molecular dynamics are used to demonstrate the fast formation of a metal-to-ligand charge transfer state in a Mn(2+)-doped ZnO quantum dot. The formation occurs on an ultrafast timescale and is aided by the large density of states and significant mixing of the dopant Mn(2+) 3dt2 levels with the valence-band levels of the ZnO lattice. The non-radiative lifetime of the photoionization states is also investigated.

  12. Crystal structure of the Entamoeba histolytica RNA lariat debranching enzyme EhDbr1 reveals a catalytic Zn 2+/Mn 2+ heterobinucleation

    DOE PAGES

    Ransey, Elizabeth; Paredes, Eduardo; Dey, Sourav K.; ...

    2017-05-17

    Here, the RNA lariat debranching enzyme, Dbr1, is a metallophosphoesterase that cleaves 2'-5' phosphodiester bonds within intronic lariats. Previous reports have indicated that Dbr1 enzymatic activity is supported by diverse metal ions including Ni 2+, Mn 2+, Mg 2+, Fe 2+, and Zn 2+. While in initial structures of the Entamoeba histolytica Dbr1 only one of the two catalytic metal-binding sites were observed to be occupied (with a Mn 2+ ion), recent structures determined a Zn 2+/Fe 2+ heterobinucleation. We solved a high-resolution X-ray crystal structure (1.8 Å) of the E. histolytica Dbr1 and determined a Zn 2+/Mn 2+ occupancy.more » ICP-AES corroborate this finding, and in vitro debranching assays with fluorescently labeled branched substrates confirm activity.« less

  13. Enhanced biocompatibility of ZnS:Mn quantum dots encapsulated with Aloe vera extract for therapeutic applications

    NASA Astrophysics Data System (ADS)

    Anilkumar, M.; Bindu, K. R.; Sneha Saj, A.; Anila, E. I.

    2016-08-01

    Toxicity of nanoparticles remains to be a major issue in their application to the biomedical field. Aloe vera (AV) is one of the most widely exploited medicinal plants that have a multitude of amazing properties in the field of medicine. Methanol extract of Aloe vera can be used as a novel stabilising agent for quantum dots to reduce toxicity. We report the synthesis, structural characterization, antibacterial activity and cytotoxicity studies of ZnS:Mn quantum dots synthesized by the colloidal precipitation method, using methanol extract of Aloe vera (AVME) as the capping agent. The ZnS:Mn quantum dots capped with AVME exhibit superior performances in biocompatibility and antibacterial activity compared with ZnS:Mn quantum dots without encapsulation. Project supported by the Science and Engineering Research Board (SERB), Department of Science and Technology (DST), Government of India.

  14. Crystal structure of the Entamoeba histolytica RNA lariat debranching enzyme EhDbr1 reveals a catalytic Zn 2+/Mn 2+ heterobinucleation

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Ransey, Elizabeth; Paredes, Eduardo; Dey, Sourav K.

    Here, the RNA lariat debranching enzyme, Dbr1, is a metallophosphoesterase that cleaves 2'-5' phosphodiester bonds within intronic lariats. Previous reports have indicated that Dbr1 enzymatic activity is supported by diverse metal ions including Ni 2+, Mn 2+, Mg 2+, Fe 2+, and Zn 2+. While in initial structures of the Entamoeba histolytica Dbr1 only one of the two catalytic metal-binding sites were observed to be occupied (with a Mn 2+ ion), recent structures determined a Zn 2+/Fe 2+ heterobinucleation. We solved a high-resolution X-ray crystal structure (1.8 Å) of the E. histolytica Dbr1 and determined a Zn 2+/Mn 2+ occupancy.more » ICP-AES corroborate this finding, and in vitro debranching assays with fluorescently labeled branched substrates confirm activity.« less

  15. Biogeochemical characteristics of Rosa canina grown in hydrothermally contaminated soils of the Gümüşhane Province, Northeast Turkey.

    PubMed

    Vural, Alaaddin

    2015-08-01

    Kırkpavli alteration area (Gümüşhane, Northeast Turkey) is contaminated by heavy metals such as Cd, Pb, As, Cu and Zn. The quantity of accumulation of heavy metal trace elements and macroelements in 32 leaves of Rosa canina of the Kırkpavli alteration area has been studied within the scope of geochemical studies. Element contents of samples were assessed using various parameters including descriptive statistics, factor analysis, correlation coefficients and bioaccumulation factor. Concentrations were detected in the acceptable range for Mo, Cu, Pb, Ni, As, Cd, Sb, P, Ti, Na, Se and Sn. Concentrations of Co, Mn, Ba and Hg were detected close to the acceptable values, whereas Zn, Fe, Sr, V, Ca, Cr, Mg, B, Al, K, W, Sc, Cs and Rb concentrations were detected above the acceptable values. Principal component analysis was used to identify the elements that have a close relationship with each other and/or similar origins. It has been concluded that Zn, Cu, As and Mo content of the plant were related to hydrothermal alteration process and they behaved together, whereas Mn and Fe were especially products of weathering conditions, also behaved together. In terms of macroelements, Ca, Mg and Na had similar behaviour, while P and K had the same correlation.

  16. Enhanced photoluminescence and phosphorescence properties of green phosphor Zn2GeO4:Mn(2+)via composition modification with GeO2 and MgF2.

    PubMed

    Pan, Yuexiao; Li, Li; Lu, Jing; Pang, Ran; Wan, Li; Huang, Shaoming

    2016-06-21

    A green long-lasting phosphorescence (LLP) phosphor Zn2GeO4:Mn(2+) (ZGOM) has been synthesized by a solid-state method at 1100 °C in air. The luminescence intensity has been improved up to 9 and 6 times through mixing GeO2 and MgF2 into the composition, respectively. The phosphorescence duration of the sample has been prolonged to 5 h. The phosphor, composed of a mixture of Zn2GeO4 (ZGO), GeO2, and MgGeO3 phases, emits enhanced green luminescence with a broad excitation band between 250 nm to 400 nm. Under identical measurement conditions, the optimized phosphor ZGOM has a higher emission intensity and shows longer wavelength emission than those of the commercial green LLP phosphor SrAl2O4:Eu,Dy (SAOED) under an excitation at 336 nm. The quantum yield of the sample modified by GeO2 and MgF2 is as high as 95.0%. Understanding of the formation mechanism for enhancement of emission intensity and prolonging of phosphorescence duration of ZGOM is fundamentally important, which might be extended to other identified solid-state inorganic phosphor materials for advanced properties.

  17. Negative slope of resistivity-temperature curve and positive magnetoresistance in antiperovskite ZnCNi3- x Mn x (1.15≤ x≤1.5)

    NASA Astrophysics Data System (ADS)

    Shi, Lei; Chu, Songnan; Zhao, Jiyin; Wang, Yang; Guo, Yuqiao; Wang, Cailin

    2014-03-01

    In antiperovskite intermetallics ZnCNi3- x Mn x , the negative slope coefficient (NSC) d ρ/d T of resistivity-temperature curves is observed when x=1.15,1.25,1.4,1.5. The sample with x=1.25 shows a semiconductor-like behavior in the whole temperature range of 15-290 K. By study of the magnetization, magnetoresistance, and low-temperature X-ray diffraction, it is found that Mn dopant significantly affects the physical properties of ZnCNi3- x Mn x by changing both the carrier density and the magnetism. The origin of the NSC d ρ/d T can be ascribed to the change of hole-like carrier density, which is adjusted by Mn content. The existence of hole-like carriers can be understood rationally by the two-band model. The change of sign of magnetoresistance from positive to negative has been observed in ZnCNi3- x Mn x with the change of Mn content, which could be ascribed to the competition between the contribution from field-induced suppression of the thermally excited ferromagnetic spin fluctuations and the Lorentz contribution. When Mn content is low, the Lorentz contribution dominates the sign of magnetoresistance. On the other hand, when Mn content is high, the contribution from field-induced suppression of the thermally excited ferromagnetic spin fluctuations dominates the sign of magnetoresistance.

  18. Phosphate base laser glasses

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Izumitani, T.; Tsuru, M.

    1980-12-16

    A phosphate base laser glass comprising 55-70% P2O5, 1-15% Al2O3, 0-25% Li2O, 0-25% Na2O, 0-8% K2O, the total proportion of Li2O, Na2O, and K2O being 10-25%, 0-15% BaO, 0-15% ZnO, 0-15% CaO , 0-15%, sro, 0-15% MgO, the total proportion of BaO, ZnO, CaO, SrO, and MgO being 5-15%, 0-5% Y2O3, 0-5% La2O3, 0-5% GeO2, 0-5% CeO2, 0-3% Nb2O5, 0-3% MnO2, 0-2% Ta2O5, 0-1% Sb2O3, and 0.01-5% Nd2O3, all % being mole %. The phosphate base laser glass of this invention has a high induced emission cross section, a low non-linear refractive index coefficient, and excellent acid resistance and divitrificationmore » resistance. By replacing partially or wholely one or more of LiO2, Na2O, K2O, BaO, ZnO, CaO, SrO, MgO or Al2O3 by LiF, NaF, KF , BaF2ZnF2, CaF2, SrF2, MgF2 or AlF3, respectively, the above properties of the laser glass are further improved.« less

  19. Cation-Deficient Spinel ZnMn2O4 Cathode in Zn(CF3SO3)2 Electrolyte for Rechargeable Aqueous Zn-Ion Battery.

    PubMed

    Zhang, Ning; Cheng, Fangyi; Liu, Yongchang; Zhao, Qing; Lei, Kaixiang; Chen, Chengcheng; Liu, Xiaosong; Chen, Jun

    2016-10-05

    Rechargeable aqueous Zn-ion batteries are attractive cheap, safe and green energy storage technologies but are bottlenecked by limitation in high-capacity cathode and compatible electrolyte to achieve satisfactory cyclability. Here we report the application of nonstoichiometric ZnMn 2 O 4 /carbon composite as a new Zn-insertion cathode material in aqueous Zn(CF 3 SO 3 ) 2 electrolyte. In 3 M Zn(CF 3 SO 3 ) 2 solution that enables ∼100% Zn plating/stripping efficiency with long-term stability and suppresses Mn dissolution, the spinel/carbon hybrid exhibits a reversible capacity of 150 mAh g -1 and a capacity retention of 94% over 500 cycles at a high rate of 500 mA g -1 . The remarkable electrode performance results from the facile charge transfer and Zn insertion in the structurally robust spinel featuring small particle size and abundant cation vacancies, as evidenced by combined electrochemical measurements, XRD, Raman, synchrotron X-ray absorption spectroscopy, FTIR, and NMR analysis. The results would enlighten and promote the use of cation-defective spinel compounds and trifluoromethanesulfonic electrolyte to develop high-performance rechargeable zinc batteries.

  20. Oriented Attachment Is a Major Control Mechanism To Form Nail-like Mn-Doped ZnO Nanocrystals.

    PubMed

    Patterson, Samuel; Arora, Priyanka; Price, Paige; Dittmar, Jasper W; Das, Vijay Kumar; Pink, Maren; Stein, Barry; Morgan, David Gene; Losovyj, Yaroslav; Koczkur, Kallum M; Skrabalak, Sara E; Bronstein, Lyudmila M

    2017-12-26

    Here, we present a controlled synthesis of Mn-doped ZnO nanoparticles (NPs) with predominantly nail-like shapes, whose formation occurs via tip-to-base-oriented attachment of initially formed nanopyramids, followed by leveling of sharp edges that lead to smooth single-crystalline "nails". This shape is prevalent in noncoordinating solvents such as octadecene and octadecane. Yet, the double bond in the former promotes oriented attachment. By contrast, Mn-doped ZnO NP synthesis in a weakly coordinating solvent, benzyl ether, results in dendritic structures because of random attachment of initial NPs. Mn-doped ZnO NPs possess a hexagonal wurtzite structure, and in the majority of cases, the NP surface is enriched with Mn, indicating a migration of Mn 2+ ions to the NP surface during the NP formation. When the NP formation is carried out without the addition of octadecyl alcohol, which serves as a surfactant and a reaction initiator, large, concave pyramid dimers are formed whose attachment takes place via basal planes. UV-vis and photoluminescence spectra of these NPs confirm the utility of controlling the NP shape to tune electro-optical properties.

  1. Measurement of trace elements in tree rings using the PIXE method

    NASA Astrophysics Data System (ADS)

    Aoki, Toru; Katayama, Yukio; Kagawa, Akira; Koh, Susumu; Yoshida, Kohji

    1998-03-01

    Standard materials were prepared in order to calculate element concentrations in tree samples using the particle induced X-ray emission (PIXE) method. Five standard solutions (1) Ti, Fe, Cu, As, Rb, Sr; (2) Ca, V, Co, Zn, As, Rb; (3) Ti, Mn, Ni, As, Sr; (4) K, Mn, Co, As, Rb, Sr; and (5) Ca, Mn, Cu, As, Rb, Sr, were added to filter papers. The dried filter papers were used as standard samples. Pellets of Pepperbush leaves (National Institute for Environmental Studies (NIES)) and Peach leaves (National Institute of Standards and Technology (NIST)) were used as references. The peak counts of Ca, Mn, Cu, Zn, Rb, and Sr in samples taken from a kaki ( Diospros kaki Thunb.) were measured and the concentrations (ppm) of the elements were calculated using the yield curve obtained from the standard filter papers. The concentrations of Mn, Zn, Rb, and Ca were compared with the data obtained from a separate INAA analysis. Concentrations of Mn, Zn, and Ca obtained by both methods were almost the same, but the concentrations of Rb differed slightly. The amounts of trace elements in samples taken from a sugi ( Cryptomeria japonica D. Don) were also measured.

  2. Phytoremediation potential of weeds in heavy metal contaminated soils of the Bassa Industrial Zone of Douala, Cameroon.

    PubMed

    Lum, A Fontem; Ngwa, E S A; Chikoye, D; Suh, C E

    2014-01-01

    Phytoremediation is a promising option for reclaiming soils contaminated with toxic metals, using plants with high potentials for extraction, stabilization and hyperaccumulation. This study was conducted in Cameroon, at the Bassa Industrial Zone of Douala in 2011, to assess the total content of 19 heavy metals and 5 other elements in soils and phytoremediation potential of 12 weeds. Partial extraction was carried out in soil, plant root and shoot samples. Phytoremediation potential was evaluated in terms of the Biological Concentration Factor, Translocation Factor and Biological Accumulation Coefficient. The detectable content of the heavy metals in soils was Cu:70-179, Pb:8-130, Zn:200-971, Ni:74-296, Co:31-90, Mn:1983-4139, V:165-383, Cr:42-1054, Ba:26-239, Sc:21-56, Al:6.11-9.84, Th:7-22, Sr:30-190, La:52-115, Zr:111-341, Y:10-49, Nb:90-172 in mg kg(-1), and Ti:2.73-4.09 and Fe:12-16.24 in wt%. The contamination index revealed that the soils were slightly to heavily contaminated while the geoaccumulation index showed that the soils ranged from unpolluted to highly polluted. The concentration of heavy metals was ranked as Zn > Ni > Cu > V > Mn > Sc > Co > Pb and Cr in the roots and Mn > Zn > Ni > Cu > Sc > Co > V > Pb > Cr > Fe in the shoots. Dissotis rotundifolia and Kyllinga erecta had phytoextraction potentials for Pb and Paspalum orbicularefor Fe. Eleusine indica and K. erecta had phytostabilisation potential for soils contaminated with Cu and Pb, respectively.

  3. Airborne mineral components and trace metals in Paris region: spatial and temporal variability.

    PubMed

    Poulakis, E; Theodosi, C; Bressi, M; Sciare, J; Ghersi, V; Mihalopoulos, N

    2015-10-01

    A variety of mineral components (Al, Fe) and trace metals (V, Cr, Mn, Ni, Cu, Zn, Cd, Pb) were simultaneously measured in PM2.5 and PM10 fractions at three different locations (traffic, urban, and suburban) in the Greater Paris Area (GPA) on a daily basis throughout a year. Mineral species and trace metal levels measured in both fractions are in agreement with those reported in the literature and below the thresholds defined by the European guidelines for toxic metals (Cd, Ni, Pb). Size distribution between PM2.5 and PM10 fractions revealed that mineral components prevail in the coarse mode, while trace metals are mainly confined in the fine one. Enrichment factor analysis, statistical analysis, and seasonal variability suggest that elements such as Mn, Cr, Zn, Fe, and Cu are attributed to traffic, V and Ni to oil combustion while Cd and Pb to industrial activities with regional origin. Meteorological parameters such as rain, boundary layer height (BLH), and air mass origin were found to significantly influence element concentrations. Periods with high frequency of northern and eastern air masses (from high populated and industrialized areas) are characterized by high metal concentrations. Finally, inner city and traffic emissions were also evaluated in PM2.5 fraction. Significant contributions (>50 %) were measured in the traffic site for Mn, Fe, Cr, Zn, and Cu, confirming that vehicle emissions contribute significantly to their levels, while in the urban site, the lower contributions (18 to 33 %) for all measured metals highlight the influence of regional sources on their levels.

  4. Major and trace elements in organically or conventionally produced milk.

    PubMed

    Hermansen, John E; Badsberg, Jens H; Kristensen, Troels; Gundersen, Vagn

    2005-08-01

    A total of 480 samples of milk from 10 organically and 10 conventionally producing dairy farms in Denmark and covering 8 sampling periods over 1 year (triplicate samplings) were analysed for 45 trace elements and 6 major elements by high-resolution inductively coupled plasma mass spectrometry and inductively coupled plasma atomic emission spectrometry. Sampling, sample preparation, and analysis of the samples were performed under carefully controlled contamination-free conditions. The dairy cattle breeds were Danish-Holstein or Jersey. Sources of variance were quantified, and differences between production systems and breeds were tested. The major source of variation for most elements was week of sampling. Concentrations of Al, Cu, Fe, Mo, Rb, Se, and Zn were within published ranges. Concentrations of As, Cd, Cr, Mn and Pb were lower, and concentrations of Co and Sr were higher than published ranges. Compared with Holsteins, Jerseys produced milk with higher concentrations of Ba, Ca, Cu, Fe, Mg, Mn, Mo, P, Rh, and Zn and with a lower concentration of Bi. The organically produced milk, compared with conventionally produced milk, contained a significantly higher concentration of Mo (48 v. 37 ng/g) and a lower concentration of Ba (43 v. 62 ng/g), Eu (4 v. 7 ng/g), Mn (16 v. 20 ng/g) and Zn (4400 v. 5150 ng/g respectively). The investigation yielded typical concentrations for the following trace elements in milk, for which no or very few data are available: Ba, Bi, Ce, Cs, Eu, Ga, Gd, In, La, Nb, Nd, Pd, Pr, Rh, Sb, Sm, Tb, Te, Th, Ti, Tl, U, V, Y, and Zr.

  5. Mechanism of Zn Insertion into Nanostructured δ-MnO 2 : A Nonaqueous Rechargeable Zn Metal Battery

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Han, Sang-Don; Kim, Soojeong; Li, Dongguo

    2017-05-19

    Unlike the more established lithium-ion based energy storage chemistries, the complex intercalation chemistry of multivalent cations in a host lattice is not well understood, especially the relationship between the intercalating species solution chemistry and the prevalence and type of side reactions. Among multivalent metals, a promising model system can be based on nonaqueous Zn2+ ion chemistry. Several examples of these systems support the use of a Zn metal anode, and reversible intercalation cathodes have been reported. This study utilizes a combination of analytical tools to probe the chemistry of a nanostructured delta-MnO2 cathode in association with a nonaqueous acetonitrile-Zn(TFSI)(2) electrolytemore » and a Zn metal anode. As many of the issues related to understanding a multivalent battery relate to the electrolyte electrode interface, the high surface area of a nanostructured cathode provides a significant interface between the electrolyte and cathode host that maximizes the spectroscopic signal of any side reactions or minor mechanistic pathways. Numerous factors affecting capacity fade and issues associated with the second phase formation including Mn dissolution in heavily cycled Zn/delta-MnO2 cells are presented including dramatic mechanistic differences in the storage mechanism of this couple when compared to similar aqueous electrolytes are noted.« less

  6. Recent Compositional Trends within the Murray Formation, Gale Crater, Mars, as seen by APXS: Implications for Sedimentary, Diagenetic and Alteration History.

    NASA Astrophysics Data System (ADS)

    Thompson, L. M.; Yen, A.; Spray, J. G.; Johnson, J. R.; Fraeman, A. A.; Berger, J. A.; Gellert, R.; Boyd, N.; Desouza, E.; O'Connell-Cooper, C.; VanBommel, S.

    2017-12-01

    The >230 m thick Murray Formation is the lower-most unit of the Mount Sharp Group, and interpreted as primarily lacustrine. Representative mudstone, siltstone and fine sandstone targets, encountered above -4330 m elevation, trend to lower Si, Al, Ti, Cr and Ca, and higher Fe, Mn, Zn, P and Mg than the Murray below. Less common, distinctive, coarser grained sandstone lenses tend to exhibit slightly different compositions to the more typical Murray but, overall, show similar elemental trends with elevation, albeit exaggerated. This suggests that the variations observed with elevation in Al, Ti, Cr, K, Fe, Mn, Zn and P within both the coarser sandstones and finer grained Murray are the result of diagenetic and/or alteration processes rather than provenance or physical sedimentary processes such as sorting. This is supported by the chemistry of obvious diagenetic, dark grey nodules, and other potential diagenetic/alteration features within this section, which show variations in the same element concentrations (i.e., P, Mn, Fe, Zn, Mg, Ca and S), distinct from diagenetic features lower down in the stratigraphy, indicating mobility of these elements within this section and changing fluid chemistry. Trends in FeO/MnO generally mimic the presence of ferric absorption features observed in visible/near infrared passive spectra from the ChemCam instrument and from CRISM orbital data, which may be consistent with changes in redox conditions as we climb up section towards Vera Rubin Ridge (Hematite Ridge). Layer-parallel CaSO4 is also common, and not observed below -4330 m. This may represent syndepositional evaporite layers, or late bedding/laminae parallel veins emplaced after lithification, in conjunction with cross-cutting veins. The overall differences in composition between the sandstone targets and finer grained Murray are attributed to distinct provenances and/or sorting during transport. We will discuss the implications of the trends and composition of the Murray above -4330 m elevation and how this pertains to the history and evolution of the Murray Formation as a whole, climatic conditions during the formation of the Murray and the nature of Gale crater lake. Also, what do the trends imply about how circulating fluids have evolved within the Murray sediments and pH, redox, salinity conditions of these fluids?

  7. Mn-doped Zinc Sulphide nanocrystals for immunofluorescent labeling of epidermal growth factor receptors on cells and clinical tumor tissues

    NASA Astrophysics Data System (ADS)

    J, Aswathy; V, Seethalekshmy N.; R, Hiran K.; R, Bindhu M.; K, Manzoor; Nair, Shantikumar V.; Menon, Deepthy

    2014-11-01

    The field of molecular detection and targeted imaging has evolved considerably with the introduction of fluorescent semiconductor nanocrystals. Manganese-doped zinc sulphide nanocrystals (ZnS:Mn NCs), which are widely used in electroluminescent displays, have been explored for the first time for direct immunofluorescent (IF) labeling of clinical tumor tissues. ZnS:Mn NCs developed through a facile wet chemistry route were capped using amino acid cysteine, conjugated to streptavidin and thereafter coupled to biotinylated epidermal growth factor receptor (EGFR) antibody utilizing the streptavidin-biotin linkage. The overall conjugation yielded stable EGFR antibody conjugated ZnS:Mn NCs (EGFR ZnS:Mn NCs) with a hydrodynamic diameter of 65 ± 15 nm, and having an intense orange-red fluorescence emission at 598 nm. Specific labeling of EGF receptors on EGFR+ve A431 cells in a co-culture with EGFR-ve NIH3T3 cells was demonstrated using these nanoprobes. The primary antibody conjugated fluorescent NCs could also clearly delineate EGFR over-expressing cells on clinical tumor tissues processed by formalin fixation as well as cryopreservation with a specificity of 86% and accuracy of 88%, in comparison to immunohistochemistry. Tumor tissues labeled with EGFR ZnS:Mn NCs showed good fluorescence emission when imaged after storage even at 15 months. Thus, ZnS nanobioconjugates with dopant-dependent and stable fluorescence emission show promise as an efficient, target-specific fluorophore that would enable long term IF labeling of any antigen of interest on clinical tissues.

  8. Fast imaging of eccrine latent fingerprints with nontoxic Mn-doped ZnS QDs.

    PubMed

    Xu, Chaoying; Zhou, Ronghui; He, Wenwei; Wu, Lan; Wu, Peng; Hou, Xiandeng

    2014-04-01

    Fingerprints are unique characteristics of an individual, and their imaging and recognition is a top-priority task in forensic science. Fast LFP (latent fingerprint) acquirement can greatly help policemen in screening the potential criminal scenes and capturing fingerprint clues. Of the two major latent fingerprints (LFP), eccrine is expected to be more representative than sebaceous in LFP identification. Here we explored the heavy metal-free Mn-doped ZnS quantum dots (QDs) as a new imaging moiety for eccrine LFPs. To study the effects of different ligands on the LFP image quality, we prepared Mn-doped ZnS QDs with various surface-capping ligands using QDs synthesized in high-temperature organic media as starting material. The orange fluorescence emission from Mn-doped ZnS QDs clearly revealed the optical images of eccrine LFPs. Interestingly, N-acetyl-cysteine-capped Mn-doped ZnS QDs could stain the eccrine LFPs in as fast as 5 s. Meanwhile, the levels 2 and 3 substructures of the fingerprints could also be simultaneously and clearly identified. While in the absence of QDs or without rubbing and stamping the finger onto foil, no fluorescent fingerprint images could be visualized. Besides fresh fingerprint, aged (5, 10, and 50 days), incomplete eccrine LFPs could also be successfully stained with N-acetyl-cysteine-capped Mn-doped ZnS QDs, demonstrating the analytical potential of this method in real world applications. The method was also robust for imaging of eccrine LFPs on a series of nonporous surfaces, such as aluminum foil, compact discs, glass, and black plastic bags.

  9. Correlation of Aflatoxin Contamination With Zinc Content of Chicken Feed †

    PubMed Central

    Jones, Frank T.; Hagler, Winston M.; Hamilton, Pat B.

    1984-01-01

    Feed samples from chicken houses in five commercial chicken operations were analyzed for Zn, Mn, Fe, Cu, Cd, and aflatoxin content. Mean aflatoxin content of these samples was 14 ppb (14 ng/g) as opposed to 1.2 ppb in samples taken when the feed was made. Aflatoxin content of the feed samples correlated (r = 0.325) significantly (P < 0.05) with Zn content but not with Mn, Fe, or Cu, all of which correlated significantly with Zn. Zn content of unamended feed (<20 ppm [20 μg/g]) is normally supplemented with a mineral premix containing Zn, Mn, Fe, and Cu to meet the nutrient requirements of chickens (40 ppm of Zn). The mean zinc concentration of the feed samples (117 ppm) was about threefold greater than the nutrient requirement and ranged from 58 to 162 ppm in individual samples. These field survey results parallel earlier reports of augmented production of aflatoxin in monocultures of aflatoxigenic fungi in corn and other ingredients supplemented with Zn. These results suggest that stricter control of Zn levels during manufacture could reduce aflatoxin contamination of feed consumed by chickens. PMID:16346486

  10. Correlation of aflatoxin contamination with zinc content of chicken feed

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Jones, F.T.; Hagler, W.M. Jr.; Hamilton, P.B.

    Feed samples from chicken houses in five commercial chicken operations were analyzed for Zn, Mn, Fe, Cu, Cd, and aflatoxin content. Mean aflatoxin content of these samples was 14 ppb (14 ng/g) as opposed to 1.2 ppb in samples taken when the feed was made. Aflatoxin content of the feed samples correlated significantly with Zn content but not with Mn, Fe, or Cu, all of which correlated significantly with Zn. Zn content of unamended feed (<20 ppm (20 ..mu..g/g) is normally supplemented with a mineral premix containing Zn, Mn, Fe, and Cu to meet the nutrient requirements of chickens (40more » ppm of Zn). The mean zinc concentration of the feed samples (117 ppm) was about threefold greater than the nutrient requirement and ranged from 58 to 162 ppm in individual samples. These field survey results parallel earlier reports of augmented production of aflatoxin in monocultures of aflatoxigenic fungi in corn and other ingredients supplemented with Zn. These results suggest that stricter control of Zn levels during manufacture could reduce aflatoxing contamination of feed consumed by chickens.« less

  11. Effect of low additives of calcium on corrosion resistance of alloys of the Mg - Al - Zn - Mn system

    NASA Astrophysics Data System (ADS)

    Koltygin, A. V.; Bazlova, T. A.

    2012-03-01

    The effect of calcium (0.2 - 0.5 wt.%) on the resistance of a liquid and solid magnesium alloy to oxidation is investigated. It is shown that calcium may be used as a microalloying additive raising the corrosion resistance of magnesium alloys not only at a high temperature but also at the operating temperature of parts produced from them for both cast and heat treated conditions.

  12. Detergentless ultrasound-assisted extraction of trace elements from edible oils using lipase as an extractant.

    PubMed

    Kara, Derya; Fisher, Andrew; Hill, Steve

    2015-11-01

    A new method for the extraction and preconcentration of trace elements (Al, Ba, Cd, Cu, Fe, Mn, Mo, Ni, Ti, V and Zn) from edible oils by producing detergentless micro-emulsions via an ultrasound-assisted extraction using a water phase containing Lipase at pH 3 as an extractant was developed. The trace elements in the water phase post-extraction were determined against matrix matched standards using ICP-MS. In the first step of the work, the parameters that affect extraction, such as pH, the volume of 1% lipase in the water phase and the ultrasonic and centrifugation times were optimized. Under the optimal conditions, the detection limits (µg kg(-1)) were 0.46, 0.03, 0.007, 0.028, 0.67, 0.038, 0.022, 0.14, 0.17, 0.05 and 0.07 for Al, Ba, Cd, Cu, Fe, Mn, Mo, Ni, Ti, V and Zn respectively for edible oils (3 Sb/m). A certified reference material (EnviroMAT HU-1 Used oil) was analysed to check the accuracy of the developed method. Results obtained were in agreement with certified values with a t-test showing that no significant differences at the 95% confidence levels were found. The proposed method was applied to different edible oils such as sunflower oil, rapeseed oil, olive oil and salmon oil. Copyright © 2015 Elsevier B.V. All rights reserved.

  13. Influence of marine, terrestrial and anthropogenic sources on ionic and metallic composition of rainwater at a suburban site (northwest coast of Spain)

    NASA Astrophysics Data System (ADS)

    Moreda-Piñeiro, Jorge; Alonso-Rodríguez, Elia; Moscoso-Pérez, Carmen; Blanco-Heras, Gustavo; Turnes-Carou, Isabel; López-Mahía, Purificación; Muniategui-Lorenzo, Soledad; Prada-Rodríguez, Darío

    2014-05-01

    In the present research, the rainwater chemistry of soluble (SF) and non-soluble (NSF) fractions is studied over a one a half year period (from March 2011 to August 2012) at a suburban site (Oleiros, A Coruña, Spain). The monthly rainfall in this region during the studied period ranged from 10 to 137 mm, while the NSF ranged from 0.9 to 54 mg L-1. More rainfall occurs within October-January. Eighteen samples, which provide information pertaining to the monthly variation in chemistry, were analyzed. Trace metals (Al, As, Ba, Co, Cu, Cr, Fe, Mn, Ni, Pb, Sr, V, Zn) were enclosed in the study of both fractions of the rainwater. Major inorganic ions (Cl-, NO3-, SO42-, Na+, K+, Ca2+, Mg2+ and NH4+) were also enclosed in the study of the SF of the rainwater. After partition coefficients analysis, univariate and principal components analysis (PCA) and air mass back trajectories analysis, three sources were found for the ionic and metal composition of the SF of rainwater; terrestrial (Ca2+, non sea salt SO42-, Al and Fe), marine (Mg2+, Na+, Cl-) and anthropogenic (K+, NH4+, NO3-, Fe, Mn, Pb, Sr, V and Zn). Results also suggest ubiquitous sources for Ba, Co, Cu, Cr and Ni. One source (terrestrial) was found for NSF of rainwater.

  14. Decadal trends in atmospheric deposition in a high elevation station: Effects of climate and pollution on the long-range flux of metals and trace elements over SW Europe

    NASA Astrophysics Data System (ADS)

    Camarero, Lluís; Bacardit, Montserrat; de Diego, Alberto; Arana, Gorka

    2017-10-01

    Atmospheric deposition collected at remote, high elevation stations is representative of long-range transport of elements. Here we present time-series of Al, Fe, Ti, Mn, Zn, Ni, Cu, As, Cd and Pb deposition sampled in the Central Pyrenees at 2240 m a.s.l, representative of the fluxes of these elements over South West Europe. Trace element deposition did not show a simple trend. Rather, there was statistical evidence of several underlying factors governing the variability of the time-series recorded: seasonal cycles, trends, the effects of the amount of precipitation, climate-controlled export of dust, and changes in anthropogenic emissions. Overall, there were three main modes of variation in deposition. The first mode was related to North Atlantic Oscillation (NAO), and affected Al, Fe, Ti, Mn and Pb. We interpret this as changes in the dust export from Northern Africa under the different meteorological conditions that the NAO index indicates. The second mode was an upward trend related to a rise in the frequency of precipitation events (that also lead to an increase in the amount). More frequent events might cause a higher efficiency in the scavenging of aerosols. As, Cu and Ni responded to this. And finally, the third mode of variation was related to changes in anthropogenic emissions of Pb and Zn.

  15. Hair chemical element contents and influence factors of reproductive-age women in the West Ujimqin Banner, Inner Mongolia, China.

    PubMed

    Zhou, Shanshan; Yuan, Haodong; Ma, Xiaoling; Liu, Ying

    2017-01-01

    Women have an increased risk for chemical element deficiencies during reproductive age, particularly due to higher chemical element requirements and poor diets. Twenty-one chemical elements (Al, B, Ba, Ca, Cd, Co, Cr, Cu, Fe, Mg, Mn, Mo, Ni, Pb, Se, Si, Sn, Sr, Ti, V and Zn) in hair samples, which were collected from 71 non-pregnant and 236 pregnant women living in the West Ujimqin Banner, central Inner Mongolia, China, were measured, and the environment, dietary habits and ethnic group influence factors associated with the biomarker were analyzed. The results indicated that the average values of the chemical element contents from hair were greatly different compared to those from other areas, especially the Al, Cd, Pb, Ca and Sr contents. There was no significant difference among the three ethnicities for any element except Mn and Ti in non-pregnant women. Compared to non-pregnant women, in the first trimester group, the levels of nine chemical elements (Ba, Cd, Cu, Pb, Se, Si, Sn and Ti) decreased, while the others increased, and the contents of all of the chemical elements decreased in the second trimester group, while in the third trimester, there was a slight increase. Three chemical elements (Cu, Mn and Zn) displayed a synergistic correlation between each other in the third trimester group, which may protect the placenta from some oxidant damage. The high levels of Cd and Pb in hair likely originate from house renovations and traffic pollution. This study provided basic and useful information on the levels of chemical elements in reproductive-age women, and the results of this study are helpful to control the contents and improve the health of pregnant and non-pregnant women. Copyright © 2016 Elsevier Ltd. All rights reserved.

  16. Effects of glyphosate on the mineral content of glyphosate-resistant soybeans (Glycine max).

    PubMed

    Duke, Stephen O; Reddy, Krishna N; Bu, Kaixuan; Cizdziel, James V

    2012-07-11

    There are conflicting claims as to whether treatment with glyphosate adversely affects mineral nutrition of glyphosate-resistant (GR) crops. Those who have made claims of adverse effects have argued links between reduced Mn and diseases in these crops. This article describes experiments designed to determine the effects of a recommended rate (0.86 kg ha(-1)) of glyphosate applied once or twice on the mineral content of young and mature leaves, as well as in seeds produced by GR soybeans (Glycine max) in both the greenhouse and field using inductively coupled plasma mass spectrometry (ICP-MS). In the greenhouse, there were no effects of either one application (at 3 weeks after planting, WAP) or two applications (at 3 and 6 WAP) of glyphosate on Ca, Mg, Mn, Zn, Fe, Cu, Sr, Ba, Al, Cd, Cr, Co, or Ni content of young or old leaves sampled at 6, 9, and 12 WAP and in harvested seed. Se concentrations were too low for accurate detection in leaves, but there was also no effect of glyphosate applications on Se in the seeds. In the field study, there were no effects of two applications (at 3 and 6 WAP) of glyphosate on Ca, Mg, Mn, Zn, Fe, Cu, Sr, Ba, Al, Cd, Cr, Co, or Ni content of young or old leaves at either 9 or 12 WAP. There was also no effect on Se in the seeds. There was no difference in yield between control and glyphosate-treated GR soybeans in the field. The results indicate that glyphosate does not influence mineral nutrition of GR soybean at recommended rates for weed management in the field. Furthermore, the field studies confirm the results of greenhouse studies.

  17. Exposure of Mn and FeSODs, but not Cu/ZnSOD, to NO leads to nitrosonium and nitroxyl ions generation which cause enzyme modification and inactivation: an in vitro study.

    PubMed

    Niketíc, V; Stojanović, S; Nikolić, A; Spasić, M; Michelson, A M

    1999-11-01

    The effect of NO treatment in vitro on structural and functional alterations of Cu/Zn, Mn, and Fe type of SODs was studied. Significant difference in response to NO of Cu/ZnSOD compared to the Mn and Fe types was demonstrated. Cu/ZnSOD was shown to be stable with respect to NO: even on prolonged exposure, NO produced negligible effect on its structure and activity. In contrast, both Mn and Fe types were found to be NO-sensitive: exposure to NO led to their fast and extensive inactivation, which was accompanied by extensive structural alterations, including (in some of the samples tested) the cleavage of enzyme polypeptide chains, presumably at His residues of the enzyme metal binding sites. The generation of nitrosonium (NO+) and nitroxyl (NO-) ions in NO treated Mn and FeSODs, which produce enzyme modifications and inactivation, was demonstrated. The physiological and biomedical significance of described findings is briefly discussed.

  18. Long-lived and Well-resolved Mn2+ Ion Emissions in CuInS-ZnS Quantum Dots

    PubMed Central

    Cao, Sheng; Li, Chengming; Wang, Lin; Shang, Minghui; Wei, Guodong; Zheng, Jinju; Yang, Weiyou

    2014-01-01

    CuInS2 (CIS) quantum dots (QDs) have tunable photoluminescence (PL) behaviors in the visible and near infrared spectral range with markedly lower toxicity than the cadmium-based counterparts, making them very promising applications in light emitting and solar harvesting. However, there still remain material- and fabrication- related obstacles in realizing the high-performance CIS-based QDs with well-resolved Mn2+ d-d emission, long emission lifetimes as well as high efficiencies. Here, we demonstrate the growth of high-quality Mn2+-doped CuInS-ZnS (CIS-ZnS) QDs based on a multi-step hot-injection strategy. The resultant QDs exhibit a well-resolved Mn2+ d-d emission with a high PL quantum yield (QY) up to 66% and an extremely long excited state lifetime up to ~3.78 ms, which is nearly two times longer than the longest one of “green” QDs ever reported. It is promising that the synthesized Mn2+-doped CIS-ZnS QDs might open new doors for their practical applications in bioimaging and opto/electronic devices. PMID:25515207

  19. Synthesis, self-assembly, and properties of Mn doped ZnO nanoparticles.

    PubMed

    Barick, K C; Bahadur, D

    2007-06-01

    We report here a novel process to prepare Mn doped ZnO nanoparticles by a soft chemical route at low temperature. The synthesis process is based on the hydrolysis of zinc acetate dihydrate and manganese acetate tetrahydrate heated under reflux to 160-175 degrees C using diethylene glycol as a solvent. X-ray diffraction analysis reveals that the Mn doped ZnO crystallizes in a wurtzite structure with crystal size of 15-25 nm. These nano size crystallites of Mn doped ZnO self-organize into polydisperse spheres in size ranging from 100-400 nm. Transmission Electron Microscopy image also shows that each sphere is made up of numerous nanocrystals of average diameter 15-25 nm. By means of X-ray photoelectron spectroscopy and electron spin resonance spectroscopy, we determined the valence state of Mn ions as 2+. These nanoparticles were found to be ferromagnetic at room temperature. Monodisperse porous spheres (approximately 250 nm) were obtained by size selective separation technique and then self-assembled in a closed pack periodic array through sedimentation with slow solvent evaporation, which gives strong opalescence in visible region.

  20. Electrochemically-induced reversible transition from the tunneled to layered polymorphs of manganese dioxide

    NASA Astrophysics Data System (ADS)

    Lee, Boeun; Yoon, Chong Seung; Lee, Hae Ri; Chung, Kyung Yoon; Cho, Byung Won; Oh, Si Hyoung

    2014-08-01

    Zn-ion batteries are emerging energy storage systems eligible for large-scale applications, such as electric vehicles. These batteries consist of totally environmentally-benign electrode materials and potentially manufactured very economically. Although Zn/α-MnO2 systems produce high energy densities of 225 Wh kg-1, larger than those of conventional Mg-ion batteries, they show significant capacity fading during long-term cycling and suffer from poor performance at high current rates. To solve these problems, the concrete reaction mechanism between α-MnO2 and zinc ions that occur on the cathode must be elucidated. Here, we report the intercalation mechanism of zinc ions into α-MnO2 during discharge, which involves a reversible phase transition of MnO2 from tunneled to layered polymorphs by electrochemical reactions. This transition is initiated by the dissolution of manganese from α-MnO2 during discharge process to form layered Zn-birnessite. The original tunneled structure is recovered by the incorporation of manganese ions back into the layers of Zn-birnessite during charge process.

  1. Structural, optical, and magnetic studies of manganese-doped zinc oxide hierarchical microspheres by self-assembly of nanoparticles.

    PubMed

    Hao, Yao-Ming; Lou, Shi-Yun; Zhou, Shao-Min; Yuan, Rui-Jian; Zhu, Gong-Yu; Li, Ning

    2012-02-02

    In this study, a series of manganese [Mn]-doped zinc oxide [ZnO] hierarchical microspheres [HMSs] are prepared by hydrothermal method only using zinc acetate and manganese acetate as precursors and ethylene glycol as solvent. X-ray diffraction indicates that all of the as-obtained samples including the highest Mn (7 mol%) in the crystal lattice of ZnO have a pure phase (hexagonal wurtzite structure). A broad Raman spectrum from as-synthesized doping samples ranges from 500 to 600 cm-1, revealing the successful doping of paramagnetic Mn2+ ions in the host ZnO. Optical absorption analysis of the samples exhibits a blueshift in the absorption band edge with increasing dopant concentration, and corresponding photoluminescence spectra show that Mn doping suppresses both near-band edge UV emission and defect-related blue emission. In particular, magnetic measurements confirm robust room-temperature ferromagnetic behavior with a high Curie temperature exceeding 400 K, signifying that the as-formed Mn-doped ZnO HMSs will have immense potential in spintronic devices and spin-based electronic technologies.

  2. Synthesis and Characterization of ZNO/MN Nanocomposite by using Sol-Gel Method

    NASA Astrophysics Data System (ADS)

    Ningsih, S. K. W.; Bahrizal, B.; Nasra, E.; Nizar, U. K.; Farisya, R.

    2018-04-01

    Zink oxide doped Mn nanocomposites were synthesized by simple sol-gel method at low temperature by using combination of aquadest with methanol as the solvent and ethylene glycol as the additive. Zink acetate dehydrate and manganese chloride tetrahydrate were used as the precursors. Composition dopants were 1,3,5,and 7%. The crystals were formed by drying at 110°C for 1 hour, after which they were heated at ± 500°C for 2 hours. The as-prepared ZnO/Mn nanocomposites were characterized by X-ray diffraction (XRD) and UV Diffuse Reflectance Spectrometer (UVDRS). The XRD patterns of the ZnO nanocrystals showed that they are mostly hexagonal wurtzite with specific peaks at 2θ = 31, 34, 36, 47, 56, 63, 66 dan 69. The sizes of the ZnO doped Mn particles produced with 1%, 3%, 5% and 7% were18-95; 17-87; 18-96 19-98 nm, respectively. UVDRS analysis showed that the band gap of the ZnO were 2,60; 2,90; 2,99 dan 3,01 eV for 1%, 3%, 5% and 7% Mn respectively.

  3. Synthesis, microstructure, and magnetic properties of monosized Mn x Zn y Fe3 − x − y O4 ferrite nanocrystals

    PubMed Central

    2013-01-01

    We report the synthesis and characterization of ferrite nanocrystals which exhibit high crystallinity and narrow size distributions. The three types of samples including Zn ferrite, Mn ferrite, and Mn-Zn ferrite were prepared via a non-aqueous nanoemulsion method. The structural, chemical, and magnetic properties of the nanocrystals are analyzed by transmission electron microscopy, X-ray diffraction, X-ray fluorescence, and physical property measurement system. The characterization indicates that the three types of ferrite nanocrystals were successfully produced, which show well-behaved magnetic properties, ferrimagnetism at 5 K and superparamagnetism at 300 K, respectively. In addition, the magnetization value of the ferrites increases with the increasing concentration of Mn. PMID:24344630

  4. Geochemical behaviour of PM10 aerosol constituents under the influence of succeeding anticyclonic/cyclonic situations: case of Sfax City, southern Tunisia.

    PubMed

    Bahloul, Moez; Chabbi, Iness; Dammak, Rim; Amdouni, Ridha; Medhioub, Khaled; Azri, Chafai

    2015-12-01

    The present study investigates the geochemical behaviour of PM10 aerosol constituents (Cl, Na, Si, Al, Ca, Fe, Mg, Mn, Pb, Zn, S) at Sfax City (Tunisia) under succeeding meteorological conditions, including short-lived anticyclonic, cyclonic and prolonged anticyclonic situations. The results revealed daily total concentrations fluctuating between 4.07 and 88.51 μg/m(3). The highest level recorded was noted to occur under the effect of the short-lived anticyclonic situation characterized by low wind speeds. It was 1.5 times higher than those recorded during cyclonic and long-lived anticyclonic situations characterized by moderate to high wind speeds. During the cyclonic situation, the marked increase of (Na and Cl) concentrations is associated with relatively high sea wind speeds (6 to 9 m/s), which are in turn responsible for a slight increase of crustal elements such as Al, Ca, Si, Fe and Mg, by the entrainment in the air of dust from roads and undeveloped areas. During the two anticyclonic situations, the simultaneous increase (due to communal transport) of crustal (Ca, Si, Al, Fe, Mg) and man-made (Mn, S, Pb, Zn) elements was noted to be associated with the dominance of terrigenious wind flows with speeds varying between 1.5 and 4 m/s. However, the significant contribution rates observed for Cl under the prevalence of such winds as compared to other crustal elements such as Fe suggested the influence of the sebkhas of Southern Tunisia.

  5. Sorption of metals on humic acid

    NASA Astrophysics Data System (ADS)

    Kerndorff, H.; Schnitzer, M.

    1980-11-01

    The sorption on humic acid (HA) of metals from an aqueous solution containing Hg(II). Fe(III), Pb, Cu, Al, Ni, Cr(III), Cd, Zn, Co and Mn, was investigated with special emphasis on effects of pH, metal concentration and HA concentration. The sorption efficiency tended to increase with rise in pH, decrease in metal concentration and increase in HA concentration of the equilibrating solution. At pH 2.4. the order of sorption was: Hg≫ Fe≫ Pb≫ CuAl ≫ Ni ≫ CrZnCdCoMn. At pH 3.7. the order was: Hg and Fe were always most readily removed, while Co and Mn were sorbed least readily. There were indications of competition for active sites (CO 2H and phenolic OH groups) on the HA between the different metals. We were unable to find correlations between the affinities of the eleven metals to sorb on HA and their atomic weights, atomic numbers, valencies, and crystal and hydrated ionic radii. The sorption of the eleven metals on the HA could be described by the equation Y = 100/[1 + exp - (A + BX)], where Y = % metal removed by HA; X = mgHA; and A and B are empirical constants.

  6. Chromium doping effects on structural and dielectric properties of Mn-Zn cobaltites

    NASA Astrophysics Data System (ADS)

    Yadav, A.; Dar, Mashkoor A.; Choudhary, P.; Shah, P.; Varshney, Dinesh

    2016-05-01

    The effect of transition metal Cr2+ ion as a dopant of Zn2+ in Mn0.5Zn0.5Co2O4 is investigated. Co-doped Mn0.5Zn0.5-xCrxCo2O4 (x = 0, 0.3 and 0.5) cobaltites were prepared by solid-state reaction route. X-ray powder diffraction (XRD) analysis reveals that the samples prepared are polycrystalline single-phase cubic spinel in structure having a space group Fd3m. An increase in average particle size observed with Cr2+ doping. However other structural parameters such as X-ray density, micro strain and dislocation density shows almost a similar decreasing trend with increase in Cr2+. High value of permittivity ˜105 is observed for the parent Mn0.5Zn0.5Co2O4 and shows a substantial decrease with increase in the Cr2+ doping. Higher doping of Cr2+ also increases the dielectric loss and hence limits its technological importance. At lower frequencies ac conductivity has been found to increase with increase in Cr2+ content.

  7. Source discrimination of heavy metals in sediment and water of To Lich River in Hanoi City using multivariate statistical approaches.

    PubMed

    Thuong, Nguyen Thi; Yoneda, Minoru; Ikegami, Maiko; Takakura, Masato

    2013-10-01

    The concentrations of Mn, Fe, Ni, Cr, Cu, Pb, Zn, As, and Cd were determined to evaluate the level of contamination of To Lich River in Hanoi City. All metal concentrations in 0-10-cm water samples, except Mn, were lower than the maximum permitted concentration for irrigation water standard. Meanwhile, concentrations of As, Cd, and Zn in 0-30-cm sediments were likely to have adverse effects on agriculture and aquatic life. Sediment pollution assessment was undertaken using enrichment factor and geoaccumulation index (I geo). The I geo results indicated that the sediment was not polluted with Cr, Mn, Fe, and Ni, and the pollution level increased in the order of Cu < Pb < Zn < As < Cd. Meanwhile, significant enrichment was shown for Cd, As, Zn, and Pb. Cluster and principal component analyses suggest that As and Mn in sediment were derived from both lithogenic and anthropogenic sources, while Cu, Pb, Zn, Cr, Cd, and Ni originated from anthropogenic sources such as vehicular fumes for Pb and metallic discharge from industrial sources and fertilizer application for other metals.

  8. Synthesis, properties, and formation mechanism of Mn-doped Zn 2 SiO 4 nanowires and associated heterostructures

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Liu, Haiqing; Moronta, Dominic; Li, Luyao

    In this study, we have put forth a facile hydrothermal approach to synthesize an array of one-dimensional (1D) Mn-doped Zn 2SiO 4 nanostructures. Specifically, we have probed and correlated the effects of controllable reaction parameters such as the pH and Mn dopant concentrations with the resulting crystal structures and morphologies of the products obtained. Based upon our results, we find that careful tuning of the pH versus the Mn dopant level gives rise to opposite trends with respect to the overall size of the resulting one-dimensional nanostructures. Significantly, we have highlighted the role of the Mn dopant ion concentration asmore » a potentially generalizable reaction parameter in solution-based synthesis for controlling morphology and hence, the observed optical behavior. Indeed, such a strategy can be potentially generalized to systems such as but not limited to Mn-doped ZnS, CdS, and CdSe quantum dots (QD), which, to the best of our knowledge, denote promising candidates for a variety of optoelectronic applications. Specifically, we have carefully optimized the synthesis conditions in order to generate a series of chemically well-defined Mn-doped Zn 2SiO 4 not only possessing Mn concentrations ranging from 3% to 8% but also characterized by highly crystalline, monodisperse wire-like motifs measuring ~30 nm in diameter and ~700 nm in length. Optically, the photoluminescence signals associated with the 1D series yielded a volcano-shaped relationship between PL intensities and the Mn dopant level. In additional experiments, we have immobilized CdSe quantum dots (QDs) onto the external surfaces of our as-synthesized Mn-doped Zn 2SiO 4 nanowires, in order to form novel composite heterostructures. The optical properties of the CdSe QD–Mn:Zn 2SiO 4 heterostructures have been subsequently examined. Our results have demonstrated the likely co-existence of both energy transfer and charge transfer phenomena between the two constituent components of our as-prepared composites. Specifically, when both components are photoexcited, both energy transfer and charge transfer were found to plausibly occur, albeit in opposite directions. When the CdSe QDs are excited alone for example, charge transfer probably takes place from the CdSe QDs to the dopant Mn 2+ ions. We believe that our as-processed heterostructures are therefore promising as a tunable light-harvesting motif. Essentially, these materials have broadened the effective light absorption range for optical ‘accessibility’, not only through their incorporation of dopant-tunable Zn 2SiO 4 possessing complementary absorption properties to those of the QDs but also through their integration of CdSe QDs with size-tailorable optical behavior.« less

  9. Synthesis, properties, and formation mechanism of Mn-doped Zn 2 SiO 4 nanowires and associated heterostructures

    DOE PAGES

    Liu, Haiqing; Moronta, Dominic; Li, Luyao; ...

    2018-03-28

    In this study, we have put forth a facile hydrothermal approach to synthesize an array of one-dimensional (1D) Mn-doped Zn 2SiO 4 nanostructures. Specifically, we have probed and correlated the effects of controllable reaction parameters such as the pH and Mn dopant concentrations with the resulting crystal structures and morphologies of the products obtained. Based upon our results, we find that careful tuning of the pH versus the Mn dopant level gives rise to opposite trends with respect to the overall size of the resulting one-dimensional nanostructures. Significantly, we have highlighted the role of the Mn dopant ion concentration asmore » a potentially generalizable reaction parameter in solution-based synthesis for controlling morphology and hence, the observed optical behavior. Indeed, such a strategy can be potentially generalized to systems such as but not limited to Mn-doped ZnS, CdS, and CdSe quantum dots (QD), which, to the best of our knowledge, denote promising candidates for a variety of optoelectronic applications. Specifically, we have carefully optimized the synthesis conditions in order to generate a series of chemically well-defined Mn-doped Zn 2SiO 4 not only possessing Mn concentrations ranging from 3% to 8% but also characterized by highly crystalline, monodisperse wire-like motifs measuring ~30 nm in diameter and ~700 nm in length. Optically, the photoluminescence signals associated with the 1D series yielded a volcano-shaped relationship between PL intensities and the Mn dopant level. In additional experiments, we have immobilized CdSe quantum dots (QDs) onto the external surfaces of our as-synthesized Mn-doped Zn 2SiO 4 nanowires, in order to form novel composite heterostructures. The optical properties of the CdSe QD–Mn:Zn 2SiO 4 heterostructures have been subsequently examined. Our results have demonstrated the likely co-existence of both energy transfer and charge transfer phenomena between the two constituent components of our as-prepared composites. Specifically, when both components are photoexcited, both energy transfer and charge transfer were found to plausibly occur, albeit in opposite directions. When the CdSe QDs are excited alone for example, charge transfer probably takes place from the CdSe QDs to the dopant Mn 2+ ions. We believe that our as-processed heterostructures are therefore promising as a tunable light-harvesting motif. Essentially, these materials have broadened the effective light absorption range for optical ‘accessibility’, not only through their incorporation of dopant-tunable Zn 2SiO 4 possessing complementary absorption properties to those of the QDs but also through their integration of CdSe QDs with size-tailorable optical behavior.« less

  10. Effects of Long-Term Exposure to Zinc Oxide Nanoparticles on Development, Zinc Metabolism and Biodistribution of Minerals (Zn, Fe, Cu, Mn) in Mice

    PubMed Central

    Wang, Chao; Lu, Jianjun; Zhou, Le; Li, Jun; Xu, Jiaman; Li, Weijian; Zhang, Lili; Zhong, Xiang; Wang, Tian

    2016-01-01

    Zinc oxide nanoparticles (nano-ZnOs) are widely used and possess great potentials in agriculture and biomedicine. It is inevitable for human exposure to these nanoparticles. However, no study had been conducted to investigate the long term effects of nano-ZnOs. This study aimed at investigating effects of nano-ZnOs on development, zinc metabolism and biodistribution of minerals (Zn, Fe, Cu, and Mn) in mice from week 3 to 35. After the characteristics of nano-ZnOs were determined, they were added into the basal diet at 0, 50, 500 and 5000 mg/kg. Results indicated that added 50 and 500 mg/kg nano-ZnOs showed minimal toxicity. However, 5000 mg/kg nano-ZnOs significantly decreased body weight (from week 4 to 16) and increased the relative weights of the pancreas, brain and lung. Added 5000 mg/kg nano-ZnOs significantly increased the serum glutamic-pyruvic transaminase activity and zinc content, and significantly enhanced mRNA expression of zinc metabolism-related genes, including metallothionein 1(32.66 folds), metallothionein 2 (31.42 folds), ZIP8 (2.21folds), ZIP14 (2.45 folds), ZnT1 (4.76 folds), ZnT2 (6.19 folds) and ZnT4 (1.82 folds). The biodistribution determination showed that there was a significant accumulation of zinc in the liver, pancreas, kidney, and bones (tibia and fibula) after receiving 5000 mg/kg nano-ZnO diet, while no significant effects on Cu, Fe, and Mn levels, except for liver Fe content and pancreas Mn level. Our results demonstrated that long term exposure to 50 and 500 mg/kg nano-ZnO diets showed minimal toxicity. However, high dose of nano-ZnOs (5000 mg/kg) caused toxicity on development, and altered the zinc metabolism and biodistribution in mice. PMID:27732669

  11. Effects of Long-Term Exposure to Zinc Oxide Nanoparticles on Development, Zinc Metabolism and Biodistribution of Minerals (Zn, Fe, Cu, Mn) in Mice.

    PubMed

    Wang, Chao; Lu, Jianjun; Zhou, Le; Li, Jun; Xu, Jiaman; Li, Weijian; Zhang, Lili; Zhong, Xiang; Wang, Tian

    2016-01-01

    Zinc oxide nanoparticles (nano-ZnOs) are widely used and possess great potentials in agriculture and biomedicine. It is inevitable for human exposure to these nanoparticles. However, no study had been conducted to investigate the long term effects of nano-ZnOs. This study aimed at investigating effects of nano-ZnOs on development, zinc metabolism and biodistribution of minerals (Zn, Fe, Cu, and Mn) in mice from week 3 to 35. After the characteristics of nano-ZnOs were determined, they were added into the basal diet at 0, 50, 500 and 5000 mg/kg. Results indicated that added 50 and 500 mg/kg nano-ZnOs showed minimal toxicity. However, 5000 mg/kg nano-ZnOs significantly decreased body weight (from week 4 to 16) and increased the relative weights of the pancreas, brain and lung. Added 5000 mg/kg nano-ZnOs significantly increased the serum glutamic-pyruvic transaminase activity and zinc content, and significantly enhanced mRNA expression of zinc metabolism-related genes, including metallothionein 1(32.66 folds), metallothionein 2 (31.42 folds), ZIP8 (2.21folds), ZIP14 (2.45 folds), ZnT1 (4.76 folds), ZnT2 (6.19 folds) and ZnT4 (1.82 folds). The biodistribution determination showed that there was a significant accumulation of zinc in the liver, pancreas, kidney, and bones (tibia and fibula) after receiving 5000 mg/kg nano-ZnO diet, while no significant effects on Cu, Fe, and Mn levels, except for liver Fe content and pancreas Mn level. Our results demonstrated that long term exposure to 50 and 500 mg/kg nano-ZnO diets showed minimal toxicity. However, high dose of nano-ZnOs (5000 mg/kg) caused toxicity on development, and altered the zinc metabolism and biodistribution in mice.

  12. Concentrations of Zn, Mn, Cu and Cd in different tissues of perch (Perca fluviatilis) and in perch intestinal parasite (Acanthocephalus lucii) from the stream near Prague (Czech Republic)

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Jankovska, Ivana, E-mail: jankovska@af.czu.cz; Miholova, Daniela; Lukesova, Daniela

    2012-01-15

    We monitored concentrations of Cd, Cu, Mn and Zn in acantocephalan parasites (Acanthocephalus lucii) and its final host (Perca fluviatilis). The concentrations in parasites were found to be significantly higher than those found in the muscle, gonads and liver of fish host. The bioaccumulation factor values were 194, 24.4, 2.2 and 4.7 for Cd, Cu, Mn and Zn, respectively. This suggests a benefit for the host due to the high accumulation of toxic cadmium.

  13. Phosphorescent quantum dots/doxorubicin nanohybrids based on photoinduced electron transfer for detection of DNA.

    PubMed

    Miao, Yanming; Zhang, Zhifeng; Gong, Yan; Yan, Guiqin

    2014-09-15

    MPA-capped Mn-doped ZnS QDs/DXR nanohybrids (MPA: 3-mercaptopropionic acid; QDs: quantum dots; DXR: cetyltrimethyl ammonium bromide) were constructed via photoinduced electron transfer (PIET) and then used as a room-temperature phosphorescence (RTP) probe for detection of DNA. DXR as a quencher will quench the RTP of Mn-doped ZnS QDs via PIET, thereby forming Mn-doped ZnS QDs/DXR nanohybrids and storing RTP. With the addition of DNA, it will be inserted into DXR and thus DXR will be competitively desorbed from the surface of Mn-doped ZnS QDs, thereby releasing the RTP of Mn-doped ZnS QDs. Based on this, a new method for DNA detection was built. The sensor for DNA has a detection limit of 0.039 mg L(-1) and a linear range from 0.1 to 14 mg L(-1). The present QDs-based RTP method does not need deoxidants or other inducers as required by conventional RTP detection methods, and avoids interference from autofluorescence and the scattering light of the matrix that are encountered in spectrofluorometry. Therefore, this method can be used to detect the DNA content in body fluid. Copyright © 2014 Elsevier B.V. All rights reserved.

  14. Alternating current magnetic susceptibility and heat dissipation by Mn{sub 1−x}Zn{sub x}Fe{sub 2}O{sub 4} nanoparticles for hyperthermia treatment

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Kondo, T.; Mori, K.; Hachisu, M.

    2015-05-07

    Mn-Zn ferrite, Mn{sub 1−x}Zn{sub x}Fe{sub 2}O{sub 4} nanoparticles encapsulated in amorphous SiO{sub 2} were prepared using our original wet chemical method. X-ray diffraction patterns confirmed that the diameters of these particles were within 7–30 nm. Magnetization measurements for various sample compositions revealed that the saturation magnetization (M{sub s}) of 7 nm particles was maximum for the x = 0.2 sample. AC magnetic susceptibility measurements were performed for Mn{sub 0.8}Zn{sub 0.2}Fe{sub 2}O{sub 4} (x = 0.2) samples with 13–30 nm particles. The peak of the imaginary part of the magnetic susceptibility χ″ shifted to higher temperatures as the particle size increased. An AC field was found to causemore » the increase in temperature, with the 18 nm particles exhibiting the highest temperature increase, as expected. In addition, in vitro experiments were carried out to study the hyperthermia effects of Mn{sub 1−x}Zn{sub x}Fe{sub 2}O{sub 4} (x = 0.2, 18 nm) particles on human cancer cells.« less

  15. New metal oxides of the family Am[( TO) q]: ALiMn 3O 4 and ALiZn 3O 4 ( A = K, Rb)

    NASA Astrophysics Data System (ADS)

    Hoppe, R.; Seipp, E.; Baier, R.

    1988-01-01

    The new compounds KLiMn 3O 4 ( I), RbLiMn 3O 4 ( II), KLiZn 3O 4 ( III) and RbLiZn 3O 4 ( IV) have been prepared by solid state reaction of A2O ( A = K, Rb), Li 2O, and MO ( M = Mn, Zn). The isomorphous compounds are tetragonal, space group {I4}/{m}, Z = 2 , with lattice constants a = 838.32(4) pm, c = 341.88(3) pm for I; a = 840.66(8) pm, c = 344.85(4) pm for II; a = 819.27(9) pm, c = 334.20(7) pm for III,a = 823.62(9) pm, c = 339.73(7) pm for IV, as determined from Guinier X-ray powder patterns. The orange-colored manganates and colorless zincates are sensitive to moisture. The crystal structures of II and III have been determined by single-crystal X-ray techniques and refined to R = 0.09 ( II) and R = 0.06 ( III). The structure is built up from chains of face-shared cubes, 1∞[A O{8}/{2}] (A = K, Rb) , running parallel to the c axis. These are connected by Li + and M2+ ( M = Mn, Zn), statistically distributed on tetrahedral positions between the chains.

  16. Optical and Structural Properties of Zn2TiO4:Mn2+

    NASA Astrophysics Data System (ADS)

    Sosman, L. P.; López, A.; Camara, A. R.; Pedro, S. S.; Carvalho, I. C. S.; Cella, N.

    2017-12-01

    Polycrystalline Zn2TiO4 samples with Mn2+ doping level of 0%, 0.1%, 1.0%, and 5.0% have been produced by conventional solid-state method and their optical and structural properties investigated. Rietveld refinement of x-ray diffraction patterns revealed the formed phases and the crystallographic parameters. The chemical composition was obtained by x-ray fluorescence measurements. The optical properties were studied by photoluminescence, excitation, reflectance, and photoacoustic spectroscopy. All measurements were performed at room temperature. The photoluminescence spectrum of the pure sample (0% Mn2+) showed a band in the red region associated with Zn2TiO4, while the sample with 0.1% Mn2+ exhibited two bands, in the green and red spectral regions, assigned to Mn2+ ions at tetrahedral and octahedral sites. No emission was observed for the samples with 1.0% or 5.0% Mn2+. The excitation results for the sample with 0.1% Mn2+ ions showed characteristic peaks of Mn2+ transitions. Tanabe-Sugano theory was used to obtain the crystal field Dq, B, and C Racah parameters from the energy peak positions in the excitation spectrum of the sample with 0.1% Mn2+. Photoacoustic measurements revealed a broad band, characteristic of semiconductor materials, hiding the Mn2+ transitions.

  17. Characteristics and impacts of trace elements in atmospheric deposition at a high-elevation site, southern China.

    PubMed

    Nie, Xiaoling; Wang, Yan; Li, Yaxin; Sun, Lei; Li, Tao; Yang, Minmin; Yang, Xueqiao; Wang, Wenxing

    2017-10-01

    To investigate the regional background trace element (TE) level in atmospheric deposition (dry and wet), TEs (Fe, Al, V, Cr, Mn, Ni, Cu, Zn, As, Se, Mo, Cd, Ba, and Pb) in 52 rainwater samples and 73 total suspended particles (TSP) samples collected in Mt. Lushan, Southern China, were analyzed using inductively coupled plasma-mass spectrometry (ICP-MS). The results showed that TEs in wet and dry deposition of the target area were significantly elevated compared within and outside China and the volume weight mean pH of rainwater was 4.43. The relative contributions of wet and dry depositions of TEs vary significantly among elements. The wet deposition fluxes of V, As, Cr, Se, Zn, and Cd exceeded considerably their dry deposition fluxes while dry deposition dominated the removal of pollution elements such as Mo, Cu, Ni, Mn, and Al. The summed dry deposition flux was four times higher than the summed wet deposition flux. Prediction results based on a simple accumulation model found that the content of seven toxic elements (Cr, Ni, Cu, Zn, As, Cd, and Pb) in soils could increase rapidly due to the impact of annual atmospheric deposition, and the increasing amounts of them reached 0.063, 0.012, 0.026, 0.459, 0.076, 0.004, and 0.145 mg kg -1 , respectively. In addition, the annual increasing rates ranged from 0.05% (Cr and Ni) to 2.08% (Cd). It was also predicted that atmospheric deposition induced the accumulation of Cr and Cd in surface soils. Cd was the critical element with the greatest potential ecological risk among all the elements in atmospheric deposition.

  18. Mineralogical, geochemical, and magnetic signatures of surface sediments from the Canadian Beaufort Shelf and Amundsen Gulf (Canadian Arctic)

    NASA Astrophysics Data System (ADS)

    Gamboa, Adriana; Montero-Serrano, Jean-Carlos; St-Onge, Guillaume; Rochon, André; Desiage, Pierre-Arnaud

    2017-02-01

    Mineralogical, geochemical, magnetic, and siliciclastic grain-size signatures of 34 surface sediment samples from the Mackenzie-Beaufort Sea Slope and Amundsen Gulf were studied in order to better constrain the redox status, detrital particle provenance, and sediment dynamics in the western Canadian Arctic. Redox-sensitive elements (Mn, Fe, V, Cr, Zn) indicate that modern sedimentary deposition within the Mackenzie-Beaufort Sea Slope and Amundsen Gulf took place under oxic bottom-water conditions, with more turbulent mixing conditions and thus a well-oxygenated water column prevailing within the Amundsen Gulf. The analytical data obtained, combined with multivariate statistical (notably, principal component and fuzzy c-means clustering analyses) and spatial analyses, allowed the division of the study area into four provinces with distinct sedimentary compositions: (1) the Mackenzie Trough-Canadian Beaufort Shelf with high phyllosilicate-Fe oxide-magnetite and Al-K-Ti-Fe-Cr-V-Zn-P contents; (2) Southwestern Banks Island, characterized by high dolomite-K-feldspar and Ca-Mg-LOI contents; (3) the Central Amundsen Gulf, a transitional zone typified by intermediate phyllosilicate-magnetite-K-feldspar-dolomite and Al-K-Ti-Fe-Mn-V-Zn-Sr-Ca-Mg-LOI contents; and (4) mud volcanoes on the Canadian Beaufort Shelf distinguished by poorly sorted coarse-silt with high quartz-plagioclase-authigenic carbonate and Si-Zr contents, as well as high magnetic susceptibility. Our results also confirm that the present-day sedimentary dynamics on the Canadian Beaufort Shelf is mainly controlled by sediment supply from the Mackenzie River. Overall, these insights provide a basis for future studies using mineralogical, geochemical, and magnetic signatures of Canadian Arctic sediments in order to reconstruct past variations in sediment inputs and transport pathways related to late Quaternary climate and oceanographic changes.

  19. Geochemical properties of topsoil around the coal mine and thermoelectric power plant.

    PubMed

    Stafilov, Trajče; Šajn, Robert; Arapčeska, Mila; Kungulovski, Ivan; Alijagić, Jasminka

    2018-03-19

    The results of the systematic study of the spatial distribution of trace metals in surface soil over the Bitola region, Republic of Macedonia, known for its coal mine and thermo-electrical power plant activities are reported. The investigated region (3200 km 2 ) is covered by a sparse sampling grid of 5 × 5 km, but in the urban zone and around the thermoelectric power plant the sampling grid is denser (1 × 1 km). In total, 229 soil samples from 149 locations were collected including top-soil (0-5 cm) and bottom-soil samples (20-30 cm and 0-30 cm). Inductively coupled plasma - atomic emission spectrometry (ICP-AES) was applied for the determinations of 21 elements (Al, As, B, Ba, Ca, Cd, Co, Cr, Cu, Fe, K, Li, Mg, Mn, Na, Ni, P, Pb, Sr, V and Zn). Based on the results of factor analyses, three geogenic associations of elements have been defined: F1 (Fe, Ni, V, Co, Cr, Mn and Li), F2 (Zn, B, Cu, Cd, Na and K) and F3 (Ca, Sr, Mg, Ba and Al). Even typical trace metals such as As, Cd, Cu, Ni, P, Pb and Zn are not isolated into anthropogenic geochemical associations by multivariate statistical methods still show some trends of local anthropogenic enrichment. The distribution maps for each analyzed element is showing the higher content of these elements in soil samples collected around the thermoelectric power plants than their average content for the soil samples collected from the whole Bitola Region. It was found that this enrichment is a result of the pollution by fly ash from coal burning which deposited near the plant having a high content of these elements.

  20. Trace elements in lake sediments measured by the PIXE technique

    NASA Astrophysics Data System (ADS)

    Gatti, Luciana V.; Mozeto, Antônio A.; Artaxo, Paulo

    1999-04-01

    Lakes are ecosystems where there is a great potential of metal accumulation in sediments due to their depositional characteristics. Total concentration of trace elements was measured on a 50 cm long sediment core from the Infernão Lake, that is an oxbow lake of the Moji-Guaçu River basin, in the state of São Paulo, Brazil. Dating of the core shows up to 180 yrs old sediment layers. The use of the PIXE technique for elemental analysis avoids the traditional acid digestion procedure common in other techniques. The multielemental characteristic of PIXE allows a simultaneous determination of about 20 elements in the sediment samples, such as, Al, Si, P, S, Cl, K, Ca, Ti, V, Cr, Mn, Fe, Ni, Cu, Zn, Rb, Sr, Zr, Ba, and Pb. Average values for the elemental composition were found to be similar to the bulk crustal composition. The lake flooding pattern strongly influences the time series of the elemental profiles. Factor analysis of the elemental variability shows five factors. Two of the factors represent the mineralogical matrix, and others represent the organic component, a factor with lead, and another loaded with chromium. The mineralogical component consists of elements such as, Fe, Al, V, Ti, Mn, Ni, K, Zr, Sr, Cu and Zn. The variability of Si is explained by two distinct factors, because it is influenced by two different sources, aluminum-silicates and quartz, and the effect of inundation are different for each other. The organic matter is strongly associated with calcium, and also bounded with S, Zn, Cu and P. Lead and chromium appears as separated factors, although it is not clear the evidences for their anthropogenic origin. The techniques developed for sample preparation and PIXE analysis was proven as advantageous and provided very good reproducibility and accuracy.

  1. Elemental analysis of different varieties of rice samples using XRF technique

    NASA Astrophysics Data System (ADS)

    Kaur, Jaspreet; Kumar, Anil

    2016-05-01

    Rice is most consumed staple food in the world providing over 21% of the calorie intake of world's population having high yielding capacity. Elements detected in rice are Al, As, Br, Cd, Cl, Co, Cs, Cu, Fe, Hg, K, Mg, Mn, Mo, Rb, Se and Zn by using Instrumental Neutron Activation with k0 standardization (R. Jayasekera etal,2004). Some of these trace elements are C, H, O, N, S, Ca, P, K, Na, Cl, Mn, Ti, Mg, Cu, Fe, Ni, Si and Zn are essential for growth of human physique The deficiency or excess of these elements in food is known to cause a variety of malnutrition or health disorders in the world. Every year, various varieties of rice are launched by Punjab Agriculture University, Ludhiana. The main purpose of which is to increases the yield to attain the maximum profit. But this leads to changing the elemental concentration in them, which may affect the human health according to variation in the nutrition values. The main objective is to study the presence of elemental concentration in various varieties of rice using EDXRF technique.

  2. [Dietary reference intakes of trace elements for Japanese and problems in clinical fields].

    PubMed

    Inoue, Yoshifumi

    2016-07-01

    In the dietary reference intakes, EAR(estimated average requirement), RDA(recommended dietary allowance), AL(adequate intake), DG(tentative dietary goal for preventing life style related diseases) and UL(tolerable upper intake level) of eight types of trace elements (iron: Fe, zinc: Zn, copper: Cu, manganese: Mn, iodine: I, selenium: Se, chromium: Cr, molybdenum: Mo) have been set. However, in the meals of hospitals, only iron of which has been taken into account. The content of these trace elements in the enteral nutrient released after 2000 was determined by considering the content of dietary reference intakes of trace elements for Japanese and considered so not fall into deficiency. However, enteral nutrient must be used considering the content of Zn, Cu and the Zn/Cu ratio, the selenium content, and the route of administration, in order to avoid falling into deficiency.

  3. Evaluating the influence of National Research Council levels of copper, iron, manganese, and zinc using organic (Bioplex) minerals on resulting tissue mineral concentrations, metallothionein, and liver antioxidant enzymes in grower-finisher swine diets.

    PubMed

    Gowanlock, D W; Mahan, D C; Jolliff, J S; Hill, G M

    2015-03-01

    Graded levels of a trace mineral premix containing an organic (Bioplex) source of Cu, Fe, Mn, and Zn was evaluated with additional treatments containing organic Zn or Fe. Grower-finisher pigs were fed from 25 to 115 kg BW. The number of pigs in the experiment, the breeding/genetics of the pigs, the management, and the average age of the pigs were previously reported. The experiment was conducted as a randomized complete block design in 7 replicates. Treatments were 1) basal diet without supplemental Cu, Fe, Mn, and Zn; 2) basal diet + 2.5 mg/kg Cu, 50 mg/kg Fe, 1.5 mg/kg Mn, and 40 mg/kg Zn (50% NRC); 3) basal diet + 5 mg/kg Cu, 100 mg/kg Fe, 3 mg/kg Mn, and 80 mg/kg Zn (100% NRC); 4) basal diet + 25 mg Zn/kg; 5) basal diet + 50 mg Zn/kg; and 6) basal diet + 50 mg Fe/kg. Selenium and I were added to all diets at 0.3 and 0.14 mg/kg, respectively. Diets were composed of corn-soybean meal, dicalcium phosphate, and limestone with phytase added to enhance mineral availability. Three pigs per pen were bled at 55, 80, and 115 kg BW and plasma was analyzed for microminerals. When the average replicate BW was 115 kg, 3 pigs per pen of an equal gender ratio were killed. The liver, kidney, and heart were removed and analyzed for microminerals. Liver, duodenum, and jejunal metallothionein and the antioxidant enzymes in the liver containing these microminerals were determined. The results demonstrated that plasma minerals were unaffected at the 3 BW intervals. Liver and duodenum metallothionein protein were greater ( < 0.05) as dietary micromineral levels increased but jejunum metallothionein did not change as microminerals increased. The activity of Cu/Zn superoxide dismutase (SOD) was not affected as the levels of the micromineral increased, whereas the activity of Mn SOD increased slightly ( < 0.05) to the 50% NRC treatment level. Liver Zn (relative and total) increased ( < 0.05) as dietary micromineral levels increased and also when Zn was added singly to the diet. Liver, kidney, and heart Cu and Mn concentrations were similar at the various micromineral levels. The activities of liver enzymes containing graded levels of Zn were not affected by dietary microminerals at 115 kg BW. These results indicate that the supplemental levels of Cu, Fe, and Mn were not necessary for grower-finisher pigs and that these innate microminerals in a corn-soybean meal diet were adequate, whereas a need for supplemental Zn was demonstrated.

  4. Synthesis and Optical Properties of MnS–ZnS and MnS–CdS Nanoparticles in Montmorillonite.

    PubMed

    Kabilaphat, Jirabhorn; Poosimma, Poonsuk; Khaorapapong, Nithima; Intachai, Sonchai; Ogawa, Makoto

    2017-02-01

    The incorporation of metal sulfide mixture, manganese sulfide and zinc sulfide (MnS–ZnS) or manganese sulfide and cadmium sulfide (MnS–CdS), in two types of montmorillonites (sodium montmorillonite and cetyltrimethylammonium modified montmorillonite) was investigated. The hybrids were characterized by powder X-ray diffraction, thermogravimetric-differential thermal analysis, transmission electron microscopy (TEM), and Raman, UV-visible and photoluminescence spectroscopies. The experimental evidences such as the expansion of the interlayer spaces and the presence of the absorption and photoluminescence due to MnS, ZnS and/or CdS revealed that the mixed metal sulfides formed in the interlayer space of montmorillonites. TEM images of the hybrids showed diskor plate-shaped nanoparticles with a mean diameter of ca. 2 nm. The increase of the luminescence intensities of the hybrids was assumed to be caused by quantum confinement effect in the interlayer space of montmorillonite.

  5. Dynamical control of Mn spin-system cooling by photogenerated carriers in a (Zn,Mn)Se/BeTe heterostructure

    NASA Astrophysics Data System (ADS)

    Debus, J.; Maksimov, A. A.; Dunker, D.; Yakovlev, D. R.; Tartakovskii, I. I.; Waag, A.; Bayer, M.

    2010-08-01

    The magnetization dynamics of the Mn spin system in an undoped (Zn,Mn)Se/BeTe type-II quantum well was studied by a time-resolved pump-probe photoluminescence technique. The Mn spin temperature was evaluated from the giant Zeeman shift of the exciton line in an external magnetic field of 3 T. The relaxation dynamics of the Mn spin temperature to the equilibrium temperature of the phonon bath after the pump-laser-pulse heating can be accelerated by the presence of free electrons. These electrons, generated by a control laser pulse, mediate the spin and energy transfer from the Mn spin system to the lattice and bypass the relatively slow direct spin-lattice relaxation of the Mn ions.

  6. Assessment of groundwater quality and contamination problems ascribed to an abandoned uranium mine (Cunha Baixa region, Central Portugal)

    NASA Astrophysics Data System (ADS)

    Neves, O.; Matias, M. J.

    2008-02-01

    The assessment of groundwater quality and its environmental implications in the region of the abandoned Cunha Baixa uranium mine (Central Portugal) was carried out from 1995 to 2004. Shallow groundwater is the major water supply source for irrigation in the neighbourhood of Cunha Baixa village. Water samples from the mine site as well as from private wells were collected in order to identify the mining impact on water composition, the extent of contamination and the seasonal and temporal groundwater quality variations. Some of the sampled private wells contain waters having low pH (<4.5 5) and high values of EC, TDS, SO4, F, Ca, Mg, Al, Mn, Ni, U, Zn and 226Ra. The wells located through the ESE WSE groundwater flow path (1 km down gradient of the mining site) display the most contaminated water. In the summer season, the levels of SO4, Al, Mn, and U were 50 120 times higher than those registered for uncontaminated waters and exceeded the quality limits for irrigation purposes, presenting soil degradation risks. Nevertheless, this study indicates that groundwater contamination suffered a small decrease from 1999 to 2004. The bioaccumulation of toxic metals such as Al, Mn, and U within the food chain may cause a serious health hazard to the Cunha Baixa village inhabitants.

  7. Room temperature synthesis of Mn2+ doped ZnS d-dots and observation of tunable dual emission: Effects of doping concentration, temperature, and ultraviolet light illumination

    NASA Astrophysics Data System (ADS)

    Kole, A. K.; Tiwary, C. S.; Kumbhakar, P.

    2013-03-01

    Mn2+ doped (0-50.0 molar %) ZnS d-dots have been synthesized in water medium by using an environment friendly low cost chemical technique. Tunable dual emission in UV and yellow-orange regions is achieved by tailoring the Mn2+ doping concentration in the host ZnS nanocrystal. The optimum doping concentration for achieving efficient photoluminescence (PL) emission is determined to be ˜1.10 (at. %) corresponding to 40.0 (molar %) of Mn2+ doping concentration used during synthesis. The mechanism of charge transfer from the host to the dopant leading to the intensity modulated tunable (594-610 nm) yellow-orange PL emission is straightforwardly understood as no capping agent is used. The temperature dependent PL emission measurements are carried out, viz., in 1.10 at. % Mn2+ doped sample and the experimental results are explained by using a theoretical PL emission model. It is found that the ratio of non-radiative to radiative recombination rates is temperature dependent and this phenomenon has not been reported, so far, in Mn2+ doped ZnS system. The colour tuning of the emitted light from the samples are evident from the calculated chromaticity coordinates. UV light irradiation for 150 min in 40.0 (molar %) Mn2+ doped sample shows an enhancement of 33% in PL emission intensity.

  8. Geochemistry of oceanic igneous rocks - Ridges, islands, and arcs - With emphasis on manganese, scandium, and vanadium

    USGS Publications Warehouse

    Doe, B.R.

    1997-01-01

    A database on a number of elements in oceanic volcanic rocks is presented, including the principal major-element oxides - SiO2, TiO2, Al2O3, Fe2O3(T), MnO, MgO, CaO, Na2O, K2O, and P2O5 (where T refers to total iron) - and the trace elements - Ba, Ce, Cr, Cu, Ni, Sc, Sr, V, Pb (mainly by isotope dilution), Yb, Zn, and Zr. Interpretations are given for transition metals, with emphasis on Mn, Sc, and V, in order to determine the concentration of the elements in primitive melts and assess their trends in magmatic differentiation. Transition metals are not enriched in plagioclase, so all are incompatible with pure plagioclase removal - that is, they become enriched in the melt. Both Cr and Ni are known to be highly compatible with olivine separation - i.e., they are depleted in the melt early in differentiation. Also, Sc is compatible with clinopyroxene (Cpx) removal from the melt and is depleted by separation of Cpx. Copper does not fit well in any of the principal silicates, but Cu, like Ni, is greatly enriched in sulfides that may remain in the source or separate from the magma. Decreasing Ni abundances and increasing Cu contents during differentiation are a sign of olivine separation. In the analysis presented herein, V - in the absence of Cpx separation - is found to behave remarkably like the moderately incompatible element Zn, and these two elements add to the list of element pairs of similar incompatibility whose ratios are insensitive to differentiation and to submarine weathering as well. Both are enhanced in titanomagnetite, so both would he compatible during titanomagnetite separation. When Cpx separates, however, V becomes compatible like Sc, but Zn remains incompatible. Thus, decreasing V (and Sc) contents and increasing Zn contents during differentiation are a sign of Cpx separation. Manganese often behaves much like Zn and therefore is moderately incompatible, but Mn is less compatible than Zn and V in titanomagnetite. Thus, decreasing Zn and V with increasing Mn is an indication of titanomagnetite removal. Dual compatible and incompatible trends with differentiation are found chiefly for Cu, Sc, and Sr. Distinguishing mid-ocean ridge basalts (MORB), oceanic-island volcanic rocks (OIV), and island-arc volcanic rocks (IAV) may be accomplished by plots of Ce/Yb versus Ba/Ce, where OIV plot to higher values of Ce/Yb than do MORB, and IAV data plot to higher values of Ba/Ce than do those of MORB. These ratios do not seem to be significantly affected by submarine weathering.

  9. Reactivity and effectiveness of traditional and novel ligands for multi-micronutrient fertilization in a calcareous soil

    PubMed Central

    López-Rayo, Sandra; Nadal, Paloma; Lucena, Juan J.

    2015-01-01

    This study compares the effectiveness of multi-micronutrient formulations containing iron (Fe), manganese (Mn), and zinc (Zn) with traditional (EDTA, DTPA, HEEDTA, and EDDHAm) or novel chelates (o,p-EDDHA, S,S-EDDS, and IDHA) and natural complexing agents (gluconate and lignosulfonate). The stability and reactivity of the formulations were studied on batch experiments with calcareous soil and by speciation modeling. Formulations containing traditional ligands maintained higher Mn but lower Zn concentration in soil solution than the novel ligands. The gluconate and lignosulfonate maintained low concentrations of both Mn and Zn in soil solution. Selected formulations were applied into calcareous soil and their efficacy was evaluated in a pot experiment with soybean. The formulation containing DTPA led to the highest Zn concentration in plants, as well as the formulation containing S,S-EDDS in the short-term, which correlated with its biodegradability. The application of traditional or novel ligands in formulations did not result in sufficient plant Mn concentrations, which was related to the low Mn stability observed for all formulations under moderate oxidation conditions. The results highlight the need to consider the effect of metals and ligands interactions in multi-nutrient fertilization and the potential of S,S-EDDS to be used for Zn fertilization. Furthermore, it is necessary to explore new sources of Mn fertilization for calcareous soils that have greater stability and efficiency, or instead to use foliar fertilization. PMID:26442065

  10. Reactivity and effectiveness of traditional and novel ligands for multi-micronutrient fertilization in a calcareous soil.

    PubMed

    López-Rayo, Sandra; Nadal, Paloma; Lucena, Juan J

    2015-01-01

    This study compares the effectiveness of multi-micronutrient formulations containing iron (Fe), manganese (Mn), and zinc (Zn) with traditional (EDTA, DTPA, HEEDTA, and EDDHAm) or novel chelates (o,p-EDDHA, S,S-EDDS, and IDHA) and natural complexing agents (gluconate and lignosulfonate). The stability and reactivity of the formulations were studied on batch experiments with calcareous soil and by speciation modeling. Formulations containing traditional ligands maintained higher Mn but lower Zn concentration in soil solution than the novel ligands. The gluconate and lignosulfonate maintained low concentrations of both Mn and Zn in soil solution. Selected formulations were applied into calcareous soil and their efficacy was evaluated in a pot experiment with soybean. The formulation containing DTPA led to the highest Zn concentration in plants, as well as the formulation containing S,S-EDDS in the short-term, which correlated with its biodegradability. The application of traditional or novel ligands in formulations did not result in sufficient plant Mn concentrations, which was related to the low Mn stability observed for all formulations under moderate oxidation conditions. The results highlight the need to consider the effect of metals and ligands interactions in multi-nutrient fertilization and the potential of S,S-EDDS to be used for Zn fertilization. Furthermore, it is necessary to explore new sources of Mn fertilization for calcareous soils that have greater stability and efficiency, or instead to use foliar fertilization.

  11. SHI irradiation effect on pure and Mn doped ZnO thin films

    NASA Astrophysics Data System (ADS)

    Khawal, H. A.; Raskar, N. D.; Dole, B. N.

    2017-05-01

    Investigated the structural, surface, electrical and modifications induced by Swift Heavy Ions (SHI) irradiation on pure and Mn substituted ZnO thin films were observed. Thin films of Zn1-xMnxO (x = 0.00, 0.04) were synthesized using the dip coating technique. All thin films irradiated by Li3+ swift heavy ions with fluence 5 × 1013 ions/cm2. The XRD peak reveals that all the samples exhibit wurtzite structures. Surface morphology of samples was investigated by SEM, it was observed that pristine samples of ZnO thin film shows spherical shape but for 4 % Mn substituted ZnO thin film with 5 × 1013 ions/cm2 fluence, it reveals that big grain spherical morphology like structure respectively. I-V characteristics were recorded in the voltage range -5 to 5 V. All curves were passed through origin and nearly linear exhibit ohmic in nature for the films.

  12. Synthesis, characterization and magnetic properties of MWCNTs decorated with Zn-substituted MnFe2O4 nanoparticles using waste batteries extract

    NASA Astrophysics Data System (ADS)

    Gabal, M. A.; Al-Harthy, E. A.; Al Angari, Y. M.; Abdel Salam, M.; Asiri, A. M.

    2016-06-01

    Mn1-xZnxFe2O4 (x=0.2-0.8) nano-crystals, synthesized from recycling of Zn-C batteries, were successfully self-assembled alongside multi-walled carbon nanotubes (MWCNTs) via an environmentally friend sucrose auto-combustion method. The effect of Zn-content on structural and magnetic properties were investigated and discussed. XRD revealed the formation of single-phase ferrites. DTA-TG experiment showed that the auto-combustion reaction finished at about 350 °C. TEM exhibited that the MWCNTs are well decorated with ferrite particles. Hysteresis loop measurements revealed ferromagnetic behavior, with saturation magnetization decrease by the addition of MWCNTs or increasing Zn-Content. The kinetics of methylene blue dye (MB) removal using MWCNTs/Mn0.8Zn0.2Fe2O nano-composite was investigated and discussed.

  13. Effects of Oral Administration of CrCl3 on the Contents of Ca, Mg, Mn, Fe, Cu, and Zn in the Liver, Kidney, and Heart of Chicken.

    PubMed

    Liu, Yanhan; Zhao, Xiaona; Zhang, Xiao; Zhao, Xuejun; Liu, Yongxia; Liu, Jianzhu

    2016-06-01

    This study aimed to investigate the effects of oral administration of trivalent chromium on the contents of Ca, Mg, Mn, Fe, Cu, and Zn in the heart, liver, and kidney. Different levels of 1/8, 1/4, and 1/2 LD50 (LD50 = 5000 mg/kg body mass) CrCl3 milligrams per kilogram body mass daily were added into the water to establish the chronic poisoning model. Ca, Mg, Mn, Fe, Cu, and Zn were detected with the flame atomic absorption spectrometry in the organs exposed 14, 28, and 42 days to CrCl3, respectively. Results showed that Cr was accumulated in the heart, liver, and kidney significantly (P < 0.05) with extended time and dose. The contents of Ca and Fe increased, whereas those of Mg, Mn, Cu, and Zn decreased in the heart, liver, and kidney of each treated group, which had a dose- and time-dependent relationship, but the contents of Mg and Zn in the heart took on a fluctuated change. These particular observations were different from those in the control group. In conclusion, the oral administration of CrCl3 could change the contents of Ca, Mg, Mn, Fe, Cu, and Zn in the heart, liver, and kidney, which may cause disorders in the absorption and metabolism of the metal elements of chickens.

  14. Esterification of phenyl acetic acid with p-cresol using metal cation exchanged montmorillonite nanoclay catalysts

    PubMed Central

    Bhaskar, M.; Surekha, M.; Suma, N.

    2018-01-01

    The liquid phase esterification of phenyl acetic acid with p-cresol over different metal cation exchanged montmorillonite nanoclays yields p-cresyl phenyl acetate. Different metal cation exchanged montmorillonite nanoclays (Mn+ = Al3+, Zn2+, Mn2+, Fe3+, Cu2+) were prepared and the catalytic activity was studied. The esterification reaction was conducted by varying molar ratio of the reactants, reaction time and catalyst amount on the yield of the ester. Among the different metal cation exchanged catalysts used, Al3+-montmorillonite nanoclay was found to be more active. The characterization of the material used was studied under different techniques, namely X-ray diffraction, scanning electron microscopy and thermogravimetric analysis. The product obtained, p-cresyl phenyl acetate, was identified by thin-layer chromotography and confirmed by Fourier transform infrared, 1H NMR and 13C NMR. The regeneration activity of used catalyst was also investigated up to fourth generation. PMID:29515855

  15. Estimation of Heavy Metal Contamination in Groundwater and Development of a Heavy Metal Pollution Index by Using GIS Technique.

    PubMed

    Tiwari, Ashwani Kumar; Singh, Prasoon Kumar; Singh, Abhay Kumar; De Maio, Marina

    2016-04-01

    Heavy metal (Al, As, Ba, Cr, Cu, Fe, Mn, Ni, Se and Zn) concentration in sixty-six groundwater samples of the West Bokaro coalfield were analyzed using inductively coupled plasma-mass spectroscopy for determination of seasonal fluctuation, source apportionment and heavy metal pollution index (HPI). Metal concentrations were found higher in the pre-monsoon season as compared to the post-monsoon season. Geographic information system (GIS) tool was attributed to study the metals risk in groundwater of the West Bokaro coalfield. The results show that 94 % of water samples were found as low class and 6 % of water samples were in medium class in the post-monsoon season. However, 79 % of water samples were found in low class, 18 % in medium class and 3 % in high class in the pre-monsoon season. The HPI values were below the critical pollution index value of 100. The concentrations of Al, Fe, Mn, and Ni are exceeding the desirable limits in many groundwater samples in both seasons.

  16. Geological-hydrogeochemical characteristics of a “silver spring” water source (the Lozovy ridge)

    NASA Astrophysics Data System (ADS)

    Ivanova, I. S.; Bragin, I. V.; Chelnokov, G. A.; Bushkareva, K. Yu; Shvagrukova, E. V.

    2016-03-01

    Geological and hydrogeological characteristics of the Lozovy ridge (Southern Primorye) are studied, as far as karst phenomena are widely distributed within its boundaries. Water-bearing rocks of the karst water source “Silver Spring” (“Serebryany Klyuch”), which is located near the bottom of the “Bear’s fang” (“Medvezhiy klyk”) cave, are investigated. It is found that karst rocks are presented by calcite (CaCO3), and an accessory mineral is barite (BaSO4). It is determined that among the trace elements forming the composition of carbonate water-bearing rocks the maximum concentrations are typical for Sr, Ba, Fe, Al, Za, Mn, Cu, and Ni. Also, the chemical composition of the waters taken from the “Silver Spring” water source is studied. These waters are fresh, hydrocarbonate, calcium, and weakly alkaline. Among the elements of the spring, such elements as Sr, Ba, Fe, Al, Zn, Mn, Cu, and Ni have the maximum concentration. The other elements have concentrations less than 1 µg/l.

  17. Electrochemical hydrogen storage alloys and batteries fabricated from Mg containing base alloys

    DOEpatents

    Ovshinsky, Stanford R.; Fetcenko, Michael A.

    1996-01-01

    An electrochemical hydrogen storage material comprising: (Base Alloy).sub.a M.sub.b where, Base Alloy is an alloy of Mg and Ni in a ratio of from about 1:2 to about 2:1, preferably 1:1; M represents at least one modifier element chosen from the group consisting of Co, Mn, Al, Fe, Cu, Mo, W, Cr, V, Ti, Zr, Sn, Th, Si, Zn, Li, Cd, Na, Pb, La, Mm, and Ca; b is greater than 0.5, preferably 2.5, atomic percent and less than 30 atomic percent; and a+b=100 atomic percent. Preferably, the at least one modifier is chosen from the group consisting of Co, Mn, Al, Fe, and Cu and the total mass of the at least one modifier element is less than 25 atomic percent of the final composition. Most preferably, the total mass of said at least one modifier element is less than 20 atomic percent of the final composition.

  18. Toxic trace elements in solid airborne particles and ecological risk assessment in the vicinity of local boiler house plants

    NASA Astrophysics Data System (ADS)

    Talovskaya, Anna V.; Osipova, Nina A.; Yazikov, Egor G.; Shakhova, Tatyana S.

    2017-11-01

    The article deals with assessment of anthropogenic pollution in vicinity of local boilers using the data on microelement composition of solid airborne particles deposited in snow. The anthropogenic feature of elevated accumulation levels of solid airborne particles deposited in snow in the vicinity of coal-fired boiler house is revealed in elevated concentrations (3-25 higher than background) of Cd, Sb, Mo, Pb, Sr, Ba, Ni, Mo, Zn and Co. In the vicinity oil-fired boiler house the specific elements as parts of solid airborne particles deposited in snow are V, Ni and Sb, as their content exceeds the background from 3 to 8 times. It is determined that the maximum shares in non-carcinogenic human health risk from chronic inhalation of trace elements to the human body in the vicinity of coal-fired boiler house belong to Al, Mn, Cu, Ba, Co, Pb, whereas in the vicinity of oil-fired boiler house - Al, Mn, Cu, Ni, V.

  19. Inorganic Macro- and Micronutrients in "Superberries" Black Chokeberries (Aronia melanocarpa) and Related Teas.

    PubMed

    Juranović Cindrić, Iva; Zeiner, Michaela; Mihajlov-Konanov, Darija; Stingeder, Gerhard

    2017-05-18

    Black chokeberries ( Aronia melanocarpa ) are considered to be functional food containing high amounts of anthocyanins, phenols, antioxidants, vitamins and minerals. Whereas organic compounds are well studied, there is little research on the mineral composition of the chokeberries. Thus, the presented study is focused on the determination of Al, As, Ba, Ca, Cd, Co, Cr, Cu, Fe, K, Li, Mg, Mn, Mo, Na, Ni, Pb, Se, Sr and Zn in black chokeberry fruits and infusions to study the metals' extractability. The nutrients Ca, K and Mg are present in the fruits (dried matter) at g/kg level, whereas the other elements are present from µg/kg up to mg/kg level. The extraction yields of the metals from the infusion range from 4 (Al, Mn) up to 44% (Na). The toxic elements present do not pose any health risk when berries or infusions are consumed. Concluding, Aronia berries, as well as infusions derived from them, are a good dietary source of essential metals in addition to the organic compounds also contained.

  20. Recovery of manganese and zinc from spent Zn-C cell powder: Experimental design of leaching by sulfuric acid solution containing glucose.

    PubMed

    Biswas, Ranjit K; Karmakar, Aneek K; Kumar, Sree L

    2016-05-01

    The spent Zn-C cell powder, containing ZnMn2O4, ZnO, MnO(OH) and possibly Mn2O3 and Mn3O4, can be leached by a sulfuric acid solution mixed with some glucose. The leaching is found to be dependent on solid to liquid (S/L) ratio, amount of glucose, concentration of sulfuric acid solution, time and pulp agitation speed. For 5g powder (S), 1h leaching time and 300rpm pulp agitation speed, two-level four-factor (2(4)) experimental designs have been carried out to derive models for extraction of both Mn(II) and Zn(II). Amount of glucose (G, g), concentration of H2SO4 solution (C, mol/L), volume of H2SO4 solution as leachant (L, mL) and leaching temperature (T, °C) are considered as factors (variables). The model in both cases consists of mean, factor effects and interaction effects. The four-factor interaction effect is observed in neither of the cases. Some two-factor and three-factor effects are found to have produced positive or negative contributions to dissolution percentage in both cases. The models are examined for comparison with experimental results with good fits and also used for optimization of factors. At optimized condition (G=0.50g, C=2mol/L, L=250mL and T=100°C), an aliquot of 5g powder in 1h and at 300rpm produces a solution containing (7.08±0.10)g/L Mn(II) and (2.20±0.06)g/L Zn(II) corresponding to almost 100% extraction of both metal ions. Copyright © 2015 Elsevier Ltd. All rights reserved.

  1. Combined effect of demagnetizing field and induced magnetic anisotropy on the magnetic properties of manganese-zinc ferrite composites

    NASA Astrophysics Data System (ADS)

    Babayan, V.; Kazantseva, N. E.; Moučka, R.; Sapurina, I.; Spivak, Yu. M.; Moshnikov, V. A.

    2012-01-01

    This work is devoted to the analysis of factors responsible for the high-frequency shift of the complex permeability (μ*) dispersion region in polymer composites of manganese-zinc (MnZn) ferrite, as well as to the increase in their thermomagnetic stability. The magnetic spectra of the ferrite and its composites with polyurethane (MnZn-PU) and polyaniline (MnZn-PANI) are measured in the frequency range from 1 MHz to 3 GHz in a longitudinal magnetization field of up to 700 Ое and in the temperature interval from -20 °С to +150 °С. The approximation of the magnetic spectra by a model, which takes into account the role of domain wall motion and magnetization rotation, allows one to determine the specific contribution of resonance processes associated with domain wall motion and the natural ferromagnetic resonance to the μ*. It is established that, at high frequencies, the μ* of the MnZn ferrite is determined solely by magnetization rotation, which occurs in the region of natural ferromagnetic resonance when the ferrite is in the “single domain” state. In the polymer composites of the MnZn ferrite, the high-frequency permeability is also determined mainly by the magnetization rotation; however, up to high values of magnetizing fields, there is a contribution of domain wall motion, thus the “single domain” state in ferrite is not reached. The frequency and temperature dependence of μ* in polymer composites are governed by demagnetizing field and the induced magnetic anisotropy. The contribution of the induced magnetic anisotropy is crucial for MnZn-PANI. It is attributed to the elastic stresses that arise due to the domain wall pinning by a polyaniline film adsorbed on the surface of the ferrite during in-situ polymerization.

  2. DOE Office of Scientific and Technical Information (OSTI.GOV)

    Handali, Melody; Neupane, Durga P.; Roychowdhury, Hridindu

    Here, ATP-binding cassette (ABC) transporters of the cluster 9 family are ubiquitous among bacteria and essential for acquiring Zn 2+ and Mn 2+ from the environment or, in the case of pathogens, from the host. These rely on a substrate-binding protein (SBP) to coordinate the relevant metal with high affinity and specificity and subsequently release it to a membrane permease for translocation into the cytoplasm. Although a number of cluster 9 SBP structures have been determined, the structural attributes conferring Zn 2+ or Mn 2+ specificity remain ambiguous. Here we describe the gene expression profile, in vitro metal binding properties,more » and crystal structure of a new cluster 9 SBP from Paracoccus denitrificans we have called AztC. Although all of our results strongly indicate Zn 2+ over Mn 2+ specificity, the Zn 2+ ion is coordinated by a conserved Asp residue only observed to date as a metal ligand in Mn 2+-specific SBPs. The unusual sequence properties of this protein are shared among close homologues, including members from the human pathogens Klebsiella pneumonia and Enterobacter aerogenes, and would seem to suggest a subclass of Zn 2+-specific transporters among the cluster 9 family. In any case, the unusual coordination environment of AztC expands the already considerable range of those available to Zn 2+-specific SBPs and highlights the presence of a His-rich loop as the most reliable indicator of Zn 2+ specificity.« less

  3. Mechanism of Zn Insertion into Nanostructured δ-MnO 2 : A Nonaqueous Rechargeable Zn Metal Battery

    DOE PAGES

    Han, Sang-Don; Kim, Soojeong; Li, Dongguo; ...

    2017-05-08

    Unlike the more established lithium-ion based energy storage chemistries, the complex intercalation chemistry of multivalent cations in a host lattice is not well understood, especially the relationship between the intercalating species solution chemistry and the prevalence and type of side reactions. Among multivalent metals, a promising model system can be based on nonaqueous Zn 2+ ion chemistry. There are several examples of these systems support the use of a Zn metal anode, and reversible intercalation cathodes have been reported. Our study utilizes a combination of analytical tools to probe the chemistry of a nanostructured δ-MnO 2 cathode in association withmore » a nonaqueous acetonitrile–Zn(TFSI) 2 electrolyte and a Zn metal anode. As many of the issues related to understanding a multivalent battery relate to the electrolyte–electrode interface, the high surface area of a nanostructured cathode provides a significant interface between the electrolyte and cathode host that maximizes the spectroscopic signal of any side reactions or minor mechanistic pathways. There are numerous factors affecting capacity fade and issues associated with the second phase formation including Mn dissolution in heavily cycled Zn/δ-MnO 2 cells are presented including dramatic mechanistic differences in the storage mechanism of this couple when compared to similar aqueous electrolytes are noted.« less

  4. Synthesis and photoluminescent and nonlinear optical properties of manganese doped ZnS nanoparticles

    NASA Astrophysics Data System (ADS)

    Nazerdeylami, Somayeh; Saievar-Iranizad, Esmaiel; Dehghani, Zahra; Molaei, Mehdi

    2011-01-01

    In this work we synthesized ZnS:Mn 2+ nanoparticles by chemical method using PVP (polyvinylpyrrolidone) as a capping agent in aqueous solution. The structure and optical properties of the resultant product were characterized using UV-vis optical spectroscopy, X-ray diffraction (XRD), photoluminescence (PL) and z-scan techniques. UV-vis spectra for all samples showed an excitonic peak at around 292 nm, indicating that concentration of Mn 2+ ions does not alter the band gap of nanoparticles. XRD patterns showed that the ZnS:Mn 2+ nanoparticles have zinc blende structure with the average crystalline sizes of about 2 nm. The room temperature photoluminescence (PL) spectrum of ZnS:Mn 2+ exhibited an orange-red emission at 594 nm due to the 4T 1- 6A 1 transition in Mn 2+. The PL intensity increased with increase in the Mn 2+ ion concentration. The second-order nonlinear optical properties of nanoparticles were studied using a continuous-wave (CW) He-Ne laser by z-scan technique. The nonlinear refractive indices of nanoparticles were in the order of 10 -8 cm 2/W with negative sign and the nonlinear absorption indices of these nanoparticles were obtained to be about 10 -3 cm/W with positive sign.

  5. Influence of Gas Atmosphere Dew Point on the Galvannealing of CMnSi TRIP Steel

    NASA Astrophysics Data System (ADS)

    Cho, Lawrence; Kim, Myung Soo; Kim, Young Ha; De Cooman, Bruno C.

    2013-11-01

    The Fe-Zn reaction occurring during the galvannealing of a Si-bearing transformation-induced plasticity (TRIP) steel was investigated by field-emission electron probe microanalysis and field-emission transmission electron microscopy. The galvannealing was simulated after hot dipping in a Zn bath containing 0.13 mass pct Al at 733 K (460 °C). The galvannealing temperature was in the range of 813 K to 843 K (540 °C to 570 °C). The kinetics and mechanism of the galvannealing reaction were strongly influenced by the gas atmosphere dew point (DP). After the galvannealing of a panel annealed in a N2+10 pct H2 gas atmosphere with low DPs [213 K and 243 K (-60 °C and -30 °C)], the coating layer consisted of δ (FeZn10) and η (Zn) phase crystals. The Mn-Si compound oxides formed during intercritical annealing were present mostly at the steel/coating interface after the galvannealing. Galvannealing of a panel annealed in higher DP [263 K and 273 K, and 278 K (-10 °C, 0 °C, and +5 °C)] gas atmospheres resulted in a coating layer consisting of δ and Г (Fe3Zn10) phase crystals, and a thin layer of Г 1 (Fe11Zn40) phase crystals at the steel/coating interface. The Mn-Si oxides were distributed homogeneously throughout the galvannealed (GA) coating layer. When the surface oxide layer thickness on panels annealed in a high DP gas atmosphere was reduced, the Fe content at the GA coating surface increased. Annealing in a higher DP gas atmosphere improved the coating quality of the GA panels because a thinner layer of oxides was formed. A high DP atmosphere can therefore significantly contribute to the suppression of Zn-alloy coating defects on CMnSi TRIP steel processed in hot dip galvanizing lines.

  6. Distribution of potentially toxic elements (PTEs) in tailings, soils, and plants around Gol-E-Gohar iron mine, a case study in Iran.

    PubMed

    Soltani, Naghmeh; Keshavarzi, Behnam; Moore, Farid; Sorooshian, Armin; Ahmadi, Mohamad Reza

    2017-08-01

    This study investigated the concentration of potentially toxic elements (PTEs) including Al, As, Cd, Co, Cr, Cu, Fe, Hg, Mn, Mo, Ni, Pb, Sb, V, and Zn in 102 soils (in the Near and Far areas of the mine), 7 tailings, and 60 plant samples (shoots and roots of Artemisia sieberi and Zygophylum species) collected at the Gol-E-Gohar iron ore mine in Iran. The elemental concentrations in tailings and soil samples (in Near and Far areas) varied between 7.4 and 35.8 mg kg -1 for As (with a mean of 25.39 mg kg -1 for tailings), 7.9 and 261.5 mg kg -1 (mean 189.83 mg kg -1 for tailings) for Co, 17.7 and 885.03 mg kg -1 (mean 472.77 mg kg -1 for tailings) for Cu, 12,500 and 400,000 mg kg -1 (mean 120,642.86 mg kg -1 for tailings) for Fe, and 28.1 and 278.1 mg kg -1 (mean 150.29 mg kg -1 for tailings) for Ni. A number of physicochemical parameters and pollution index for soils were determined around the mine. Sequential extractions of tailings and soil samples indicated that Fe, Cr, and Co were the least mobile and that Mn, Zn, Cu, and As were potentially available for plants uptake. Similar to soil, the concentration of Al, As, Co, Cr, Cu, Fe, Mn, Mo, Ni, and Zn in plant samples decreased with the distance from the mining/processing areas. Data on plants showed that metal concentrations in shoots usually exceeded those in roots and varied significantly between the two investigated species (Artemisia sieberi > Zygophylum). All the reported results suggest that the soil and plants near the iron ore mine are contaminated with PTEs and that they can be potentially dispersed in the environment via aerosol transport and deposition.

  7. Blood and urinary levels of metals and metalloids in the general adult population of Northern France: The IMEPOGE study, 2008-2010.

    PubMed

    Nisse, Catherine; Tagne-Fotso, Romuald; Howsam, Mike; Richeval, Camille; Labat, Laurence; Leroyer, Ariane

    2017-04-01

    The assessment of human chemical risks related to occupational or environmental exposure to pollutants requires the use of both accurate exposure indicators and reference values. The objective of this study was to evaluate the blood and urinary levels of various metals and metalloids in a sample of adults aged 20-59 years of the general population of Northern France, a formerly heavily industrialised area that retains some industrial activity. A cross-sectional study was conducted between 2008 and 2010, enrolling 2000 residents of Northern France. The quota method was used to guarantee the representativeness of the participants on a sex, age, social category and smoking status basis, according to the census done by the French National Institute of Statistics and Economic Studies. The levels of 14 metals: aluminium (Al), antimony (Sb), total arsenic (As), beryllium (Be), cadmium (Cd), cobalt (Co), chromium (Cr), mercury (Hg), manganese (Mn), nickel (Ni), lead (Pb), thallium (Tl), vanadium (V) and zinc (Zn) were quantified by ICP-MS in urine and blood samples. A total of 982 men and 1018 women participated, allowing the analysis of 1992 blood and 1910 urine samples. Some metal(loid)s were detected in over 99% of the blood (Cd, Co, Mn, Ni, Pb) and urine (As, Co, Pb, Zn) samples and the remaining metals in 84-99% of the samples, with the exception of blood V (19%), blood Be (57%) and urine Be (58%). Mean blood levels of Pb and Zn were significantly higher in men, and Mn, Co and Cr in women. In urine, mean Pb, Tl and Sb concentrations were significantly higher in men, and Al and Co in women. Current smokers had significantly higher mean levels of blood Cd and Pb and lower blood Co, Mn and Hg. In urine (adjusted on urinary creatinine), the smokers had higher mean levels of Cd, Pb, V and Zn and lower mean levels of As, Co, and Hg. Overall, the mean urinary levels of most metal(loid)s found in the general population of Northern France were higher than those found in the French national survey for the same period except for urinary V. Mean blood lead level was markedly less than that of the French national population. This first biomonitoring survey of a large number of metal(loid)s in the general population of Northern France provides useful information on exposure levels to toxic elements and highlights the specificity of the regional environment. These data could be used, in complement to the national human biomonitoring reference values, for the interpretation of biomonitoring results. Copyright © 2016 Elsevier GmbH. All rights reserved.

  8. Synthesis of Mn-doped ZnS architectures in ternary solution and their optical properties

    NASA Astrophysics Data System (ADS)

    Wang, Xinjuan; Zhang, Qinglin; Zou, Bingsuo; Lei, Aihua; Ren, Pinyun

    2011-10-01

    Mn-doped ZnS sea urchin-like architectures were fabricated by a one-pot solvothermal route in a ternary solution made of ethylenediamine, ethanolamine and distilled water. The as-prepared products were characterized by X-ray diffraction (XRD), field-emission scanning electron microscopy (FE-SEM), transmission electron microscopy (TEM) and photoluminescence spectra (PL). It was demonstrated that the as-prepared sea urchin-like architectures with diameter of 0.5-1.5 μm were composed of nanorods, possessing a wurtzite structures. The preferred growth orientation of nanorods was found to be the [0 0 2] direction. The PL spectra of the Mn-doped ZnS sea urchin-like architectures show a strong orange emission at 587 nm, indicating the successful doping of Mn 2+ ions into ZnS host. Ethanolamine played the role of oriented-assembly agent in the formation of sea urchin-like architectures. A possible growth mechanism was proposed to explain the formation of sea urchin-like architectures.

  9. Factors influencing the Zn and Mn extraction from pyrometallurgical sludge in the steel manufacturing industry.

    PubMed

    Mocellin, J; Mercier, G; Morel, J L; Blais, J F; Simonnot, M O

    2015-08-01

    In this laboratory study, a process has been developed for selectively leaching zinc and manganese from pyrometallurgical sludge produced in the steel manufacturing industry. In the first part, the yield of Zn extraction was studied using four factors and four levels of the Box-Behnken response surface design. The optimum conditions for the step of Zn leaching were determined to be a sulfuric acid concentration of 0.25 mol/L, a pulp density of 10%, an extraction temperature of 20 °C, and three stages of leaching. Under such conditions, 75% of the Zn should be leached. For Mn leaching, the optimum conditions were determined to be a sulfuric acid concentration of 0.25 mol/L, a Na2S2O5/Mn stoichiometry of 1, a leaching time of 120 min and two leaching steps. In this case, 100% of the Mn should be leached. Copyright © 2015 Elsevier Ltd. All rights reserved.

  10. New Fluoride-arsenide Diluted Magnetic Semiconductor (Ba,K)F(Zn,Mn)As with Independent Spin and Charge Doping

    NASA Astrophysics Data System (ADS)

    Chen, Bijuan; Deng, Zheng; Li, Wenmin; Gao, Moran; Liu, Qingqing; Gu, C. Z.; Hu, F. X.; Shen, B. G.; Frandsen, Benjamin; Cheung, Sky; Lian, Liu; Uemura, Yasutomo J.; Ding, Cui; Guo, Shengli; Ning, Fanlong; Munsie, Timothy J. S.; Wilson, Murray Neff; Cai, Yipeng; Luke, Graeme; Guguchia, Zurab; Yonezawa, Shingo; Li, Zhi; Jin, Changqing

    2016-11-01

    We report the discovery of a new fluoride-arsenide bulk diluted magnetic semiconductor (Ba,K)F(Zn,Mn)As with the tetragonal ZrCuSiAs-type structure which is identical to that of the “1111” iron-based superconductors. The joint hole doping via (Ba,K) substitution & spin doping via (Zn,Mn) substitution results in ferromagnetic order with Curie temperature up to 30 K and demonstrates that the ferromagnetic interactions between the localized spins are mediated by the carriers. Muon spin relaxation measurements confirm the intrinsic nature of the long range magnetic order in the entire volume in the ferromagnetic phase. This is the first time that a diluted magnetic semiconductor with decoupled spin and charge doping is achieved in a fluoride compound. Comparing to the isostructure oxide counterpart of LaOZnSb, the fluoride DMS (Ba,K)F(Zn,Mn)As shows much improved semiconductive behavior that would be benefit for further application developments.

  11. Evaluation of occupational exposure to toxic metals released in the process of aluminum welding.

    PubMed

    Matczak, Wanda; Gromiec, Jan

    2002-04-01

    The objective of this study was to evaluate occupational exposure to welding fumes and its elements on aluminum welders in Polish industry. The study included 52 MIG/Al fume samples and 18 TIG/Al samples in 3 plants. Air samples were collected in the breathing zone of welders (total and respirable dust). Dust concentration was determined gravimetrically, and the elements in the collected dust were determined by AAS. Mean time-weighted average (TWA) concentrations of the welding dusts/fumes and their components in the breathing zone obtained for different welding processes were, in mg/m3: MIG/Al fumes mean 6.0 (0.8-17.8), Al 2.1 (0.1-7.7), Mg 0.2 (< 0.1-0.9), Mn 0.014 (0.002-0.049), Cu 0.011 (0.002-0.092), Zn 0.016 (0.002-0.14), Pb 0.009 (0.005-0.025), Cr 0.003 (0.002-0.007), and TIG/Al fumes 0.7 (0.3-1.4), Al 0.17 (0.07-0.50). A correlation has been found between the concentration of the main components and the fume/dust concentrations in MIG/Al and TIG/Al fumes. Mean percentages of the individual components in MIG/Al fumes/dusts were Al: 30 (9-56) percent; Mg: 3 (1-5.6) percent; Mn: 0.2 (0.1-0.3) percent; Cu: 0.2 (< 0.1-1.8) percent; Zn: 0.2 (< 0.1-0.8) percent; Pb: 0.2 (< 0.1-1) percent; Cr: < 0.1 percent. The proportion of the respirable fraction in the fumes and their constituents varied between 10 percent and 100 percent. The results showed that MIG/Al fumes concentration was 1.2 times higher than the American Conference of Governmental Industrial Hygienists (ACGIH) threshold limit value (TLV), and the index of the combined exposure to the determined agents was 2.3 (0.4-8.0), mostly because of high Al2O3 contribution. The background concentrations of the components (ca. 5-10 times lower than those in the breathing zone of the welders) did not exceed the Polish MAC value. The elemental composition of total and respirable fume/dust may differ considerably depending on welding methods, the nature of welding-related operations, and work environment conditions.

  12. Improved passive treatment of high Zn and Mn concentrations using caustic magnesia (MgO): particle size effects.

    PubMed

    Rötting, Tobias S; Ayora, Carlos; Carrera, Jesus

    2008-12-15

    High concentrations of divalent metals such as Zn, Mn, Cu, Pb, Ni, Cd, Co, etc. are not removed satisfactorily in conventional (calcite- or organic matter-based) passive treatment systems. Caustic magnesia ("MgO") has been used successfully as an alternative alkaline material to remove these metals almost completely from water, but columns with coarse-grained MgO lost reactivity or permeability due to the accumulation of precipitates when only a small portion of the reagent had been spent. In the present study, MgO was mixed with wood chips to overcome these problems. Two columns with different MgO grain sizes were used to treat Zn- and Mn-rich water during one year. Performance was compared by measuring depth profiles of chemical parameters and hydraulic conductivity. The column containing 25% (v/v) of MgO with median particle size of about 3 mm displayed low reactivity and poor metal retention. In contrast, the column containing only 12.5% (v/v) of MgO with median particle size of 0.15 mm depleted Zn and Mn below detection limit throughout the study and had a good hydraulic performance. 95% of the applied MgO was consumed in the zone where Zn and Mn accumulated. The fine alkaline grains can dissolve almost completely before the growing layer of precipitates passivates them, whereas clogging is prevented by the large pores of the coarse inert matrix (wood chips). A reactive transport model corroborated the hypotheses that Zn(II) was removed due to its low solubility at pH near 10 achieved by MgO dissolution, whereas Mn(II) was removed due to rapid oxidation to Mn(III) at this pH and subsequent precipitation. The model also confirmed that the small size and large specific surface area of the MgO particles are the key factor to achieve a sufficiently fast dissolution.

  13. Moessbauer studies in Zn(2+)0.3 Mn(2+)0.7 Mn(3+) (2-y) Fe(3+) (2-y) O4

    NASA Technical Reports Server (NTRS)

    Gupta, R. G.; Mendiratta, R. G.; Escue, W. T.

    1975-01-01

    The Mossbauer effect has proven to be effective in the study of nuclear hyperfine interactions. Ferrite systems having the formula (Zn(2+)0.3)(Mn(2+)0.7)(Mn(3+)y)(Fe(3+)2-y)(O4) were prepared and studied. These systems can be interpreted as mangacese-doped zinc and a part of iron ions. A systematic study of these systems is presented to promote an understanding of their microstructure for which various theories were proposed.

  14. Metal accumulation in eggs of the red-eared slider (Trachemys scripta elegans) in the Lower Illinois River.

    PubMed

    Tryfonas, Anna E; Tucker, John K; Brunkow, Paul E; Johnson, Kevin A; Hussein, Hussein S; Lin, Zhi-Qing

    2006-03-01

    The Illinois River is a highly utilized navigable waterway in the US Midwest, and has historically been contaminated with metal toxicants from various industrial and municipal pollution sources. Little information on metal contamination is available in the Lower Illinois River, and in particular, in the habitat of the red-eared slider (Trachemys scripta elegans) at the southern end of the river near Grafton, IL. This study was conducted to determine current levels of metal contamination in water, sediment, soil, and plants in the habitat, as well as to reveal temporal and spatial variations of metal accumulation in eggs of the red-eared slider. Aluminum, Cd, Cr, Cu, Mn, Ni, Pb, V, Sn, and Zn were analyzed by inductively-coupled plasma spectroscopy. High concentrations of metals were observed in lake sediment, compared with the concentrations in water, soil, and plant tissues. Sediment Ni concentrations (mg kg(-1)) varied from 66 to 95 and Sn from 1100 to 1600. Five detectable metals in egg content were Zn (24.2 +/- 13), Al (2.2 +/- 1.2), Sn (1.8 +/- 1.1), Mn (1.1 +/- 0.6), and Cu (0.9 +/- 0.5); nine detectable metals in egg shell were Zn (6.8 +/- 3.9), Sn (3.7 +/- 3.1), Cu (1.9 +/- 1.3), Cr (1.6 +/- 1.5), V (1.6 +/- 1.4), Pb (1.3 +/- 0.7), Ni (1.3 +/- 0.9), Mn (1.0 +/- 0.8), and Cd (0.16 +/- 0.11). Zinc accumulation in egg content was significantly correlated with Zn in egg shell (r = 0.445, P < 0.002, n = 42). While significant spatial variation was observed in egg shell, metal accumulation in eggs (content and shell) collected from the same ground of turtles consecutively for 4 years did not show a significant temporal change.

  15. The size distribution of chemical elements of atmospheric aerosol at a semi-rural coastal site in Venice (Italy). The role of atmospheric circulation.

    PubMed

    Masiol, Mauro; Squizzato, Stefania; Ceccato, Daniele; Pavoni, Bruno

    2015-01-01

    The concentrations of selected elemental tracers were determined in the aerosol of a semi-rural coastal site near Venice (Italy). Size-segregated aerosol samples were collected using an 8-stage cascade impactor set at 15m above ground, during the cold season (late autumn and winter), when high levels of many pollutants are known to cause risks for human health. From the experimental data, information was extracted on potential pollutant sources by investigating the relationships between elements in the different size fractions. Moreover, an approach to highlight the importance of local atmospheric circulation and air mass origin in influencing the PM composition and fractional distribution is proposed. Anthropogenic elements are strongly inter-correlated in the submicrometric (<1 μm) (S, K, Mn, Cu, Fe and Zn) and intermediate mode (1-4 μm) (Mn, Cu, Zn, Ni) and their relationships highlight the presence of several sources (combustions, secondary aerosol, road traffic). In the intermediate mode, associations having geochemical significance exist between marine (Na, Cl and Mg) and crustal (Si, Mg, Ca, Al, Ti and K) elements. In the coarse mode (>4 μm) Fe and Zn are well correlated and are probably linked to tire and brake wear emissions. Regarding atmospheric circulation, results show increasing levels of elements related to pollution sources (S, K, Mn, Ni, Cu, Zn) when air masses come from Central and Eastern Europe direction and on the ground wind blows from NWN-N-NE (from mainland Venice). Low wind speed and high percentage of wind calm hours favor element accumulation in the submicrometric and intermediate modes. Furthermore, strong winds favor the formation of sea-spray and the increase of Si in the coarse mode due to the resuspension of sand fine particles. Copyright © 2014 Elsevier Ltd. All rights reserved.

  16. Pollution characteristics, source apportionment, and health risk of heavy metals in street dust of Suzhou, China.

    PubMed

    Lin, Manli; Gui, Herong; Wang, Yao; Peng, Weihua

    2017-01-01

    To analyze the pollution characteristics, source apportionment, and health risk of heavy metals (HMs) in street dust of Suzhou, China, 23 sampling sites were selected and periodically sampled for 12 months. A total of 276 samples were collected, and the concentrations of selected HMs (e.g., Cr, Cu, Fe, Mn, Pb, V, and Zn) were examined with an X-ray fluorescence spectrum analyzer. Results showed that the mean concentrations of Cr, Cu, Fe, Mn, Pb, V, and Zn in the street dust of Suzhou were 112.9, 27.5, 19941.3, 410.3, 45.2, 75.6, and 225.3 mg kg -1 , respectively. Cr, Cu, Pb, and Zn exceeded their background values in local natural soils by 1.3-3.6-fold, whereas Fe, Mn, and V were all within their background values. However, enrichment factor analysis revealed that Cr, Cu, Mn, Pb, V, and Zn, especially Cr, Cu, Pb, and Zn, were enriched in Suzhou street dust. The HMs showed no significant seasonal changes overall, but spatial distribution analysis implied that the high values of Cr, Cu, Mn, Pb, V, and Zn were mainly distributed in areas with frequent human activities. Results of multivariate techniques (e.g., Pearson correlation, hierarchical cluster, and principal components analyses) suggested that Pb and Zn had complicated sources; Cu and V mainly originated from traffic sources; Fe and Mn mainly came from natural sources; and Cr was dominantly related to industrial district. Health risk assessment revealed that a single heavy metal might not cause both non-cancer and carcinogenic risks to local residents. Nevertheless, the sum of the hazard index of all selected HMs for children slightly exceeded the safety value, thereby implying that the HMs from Suzhou street dust can possibly produce significant risk to children. Cr was the priority pollutant in the study area because of its high concentration, high enrichment, and high contribution to non-cancer risk values.

  17. The influence of hydrous Mn–Zn oxides on diel cycling of Zn in an alkaline stream draining abandoned mine lands

    USGS Publications Warehouse

    Shope, Christopher L.; Xie, Ying; Gammons, Christopher H.

    2006-01-01

    Many mining-impacted streams in western Montana with pH near or above neutrality display large (up to 500%) diel cycles in dissolved Zn concentrations. The streams in question typically contain boulders coated with a thin biofilm, as well as black mineral crusts composed of hydrous Mn–Zn oxides. Laboratory mesocosm experiments simulating diel behavior in High Ore Creek (one of the Montana streams with particularly high Zn concentrations) show that the Zn cycles are not caused by 24-h changes in streamflow or hyporheic exchange, but rather to reversible in-stream processes that are driven by the solar cycle and its attendant influence on pH and water temperature (T). Laboratory experiments using natural Mn–Zn precipitates from the creek show that the mobilities of Zn and Mn increase nearly an order of magnitude for each unit decrease in pH, and decrease 2.4-fold for an increase in T from 5 to 20 °C. The response of dissolved metal concentration to small changes in either pH or T was rapid and reversible, and dissolved Zn concentrations were roughly an order of magnitude higher than Mn. These observations are best explained by sorption of Zn2+ and Mn2+ onto the secondary Mn–Zn oxide surfaces. From the T-dependence of residual metal concentrations in solution, approximate adsorption enthalpies of +50 kJ/mol (Zn) and +46 kJ/mol (Mn) were obtained, which are within the range of enthalpy values reported in the literature for sorption of divalent metal cations onto hydrous metal oxides. Using the derived pH- and T-dependencies from the experiments, good agreement is shown between predicted and observed diel Zn cycles for several historical data sets collected from High Ore Creek.

  18. Reducing mineral usage in feedlot diets for Nellore cattle: I. Impacts of calcium, phosphorus, copper, manganese, and zinc contents on microbial efficiency and ruminal, intestinal, and total digestibility of dietary constituents.

    PubMed

    Sathler, D F T; Prados, L F; Zanetti, D; Silva, B C; Filho, S C Valadares; Pacheco, M V C; Amaral, P M; Rennó, L N; Paulino, M F

    2017-04-01

    This study evaluated intake, microbial efficiency, and ruminal, small and large intestinal, and total digestibility of DM, OM, CP, and NDF, as well as availability of Ca, P, Mg, Na, K, Cu, Mn, and Zn in Zebu cattle fed with or without supplemental sources of Ca and P or a micromineral premix. Five rumen- and ileum-cannulated Nellore bulls (BW = 200 ± 10.5 kg; 9 mo) were used in the experiment, distributed in a 5 × 5 Latin square design. The experiment was developed in a 2 × 2 + 1 factorial design to measure the effects of mineral supplementation on intake, digestibility, and site of nutrient absorption. The factors consisted of 2 Ca and P levels (macromineral factor; CaP+ or CaP-) and 2 microminerals levels (micromineral factor; CuMnZn+ or CuMnZn-). In addition, a treatment with alimentary restriction (REST) was evaluated at 1.7% of BW. Nutrient fluxes were measured in the omasum and ileum, in addition to intake and fecal excretion. Microbial efficiency was estimated using purine derivative excretion. Dry matter, OM, NDF, CP intake, and total digestibility were not affected ( ≥ 0.058) by the absence of Ca, P, Cu, Mn, and Zn supplementation. Intake of Ca, P, and Mg were reduced ( < 0.01) by CaP-. The absence of CuMnZn reduced ( < 0.01) Cu, Mn, and Zn intake. Ruminal recycling of P, Na, and K is significant for increasing the influx of these minerals to the digestive tract; however, influences of treatments were not observed. The small and large intestines contributed to mineral absorption in different proportions ( < 0.05), according to minerals and treatments. Because of the similarity ( > 0.05) of OM, NDF, and CP digestion sites and coefficients, we assume that omitting supplemental sources of Ca, P, Cu, Mn, and Zn may be an option in raising cattle on feedlots. If supplementation is viable, knowledge about the specific absorption site of each mineral could positively impact choices about the supplemental source.

  19. Diluted magnetic semiconductors with narrow band gaps

    NASA Astrophysics Data System (ADS)

    Gu, Bo; Maekawa, Sadamichi

    2016-10-01

    We propose a method to realize diluted magnetic semiconductors (DMSs) with p - and n -type carriers by choosing host semiconductors with a narrow band gap. By employing a combination of the density function theory and quantum Monte Carlo simulation, we demonstrate such semiconductors using Mn-doped BaZn2As2 , which has a band gap of 0.2 eV. In addition, we found a nontoxic DMS Mn-doped BaZn2Sb2 , of which the Curie temperature Tc is predicted to be higher than that of Mn-doped BaZn2As2 , the Tc of which was up to 230 K in a recent experiment.

  20. Broiler litter as a micronutrient source for cotton: concentrations in plant parts.

    PubMed

    Tewolde, H; Sistani, K R; Rowe, D E

    2005-01-01

    Analytically, poultry litter contains nearly all essential micronutrients but the extent of phytoavailability of these nutrients and whether cotton (Gossypium hirsutum L.) and other crop plants can receive adequate amounts of these nutrients from litter is not fully known. The objective of this research was to determine whether cotton receives sufficient amounts of Fe, Cu, Mn, and Zn from litter and estimate the efficiency of cotton in extracting these metal nutrients from litter in the absence of any other source of the micronutrients. The greenhouse research used plastic pots filled with approximately 11 kg of a 2:1 (v/v) sand to vermiculite growing mix. Cotton (cv. Stoneville 474) was grown in the pots fertilized with broiler litter at rates of 30, 60, 90, or 120 g pot(-1) in a factorial combination with four supplemental nutrient solution (NS) treatments. The nutrient solutions consisted of full Hoagland's nutrient solution (NS-full); a solution of the macronutrients N, P, K, Ca, and Mg (NS-macro); a solution of the micronutrients Fe, Zn, Mn, Cu, B, and Mo (NS-micro); and water (NS-none). Based on tissue nutrient analysis, a one-time broiler litter application supplied adequate amounts of Fe, Cu, and Mn to bring the concentration of these nutrients in upper leaves within published sufficiency ranges. Zinc, with <17 mg kg(-1) concentration in the upper leaves, was the only micronutrient below the established sufficiency range regardless of the rate of applied litter. Cotton extracted Fe and Mn more efficiently than Cu or Zn, removing as much as 8.8% of Fe and 7.2% of Mn supplied by 30 g litter pot(-1). In contrast, the extraction efficiency was 1.7% for Cu and 1.9% for Zn. Roots accumulated 58% of the total absorbed Fe and 64% of Cu, and leaves accumulated 32% of the Fe and only 13% of the Cu supplied by litter. In contrast, only 16% of the total absorbed Mn and 23% of Zn accumulated in roots while leaves accumulated 64% of the total Mn and 37% of Zn. These results demonstrate that broiler litter is a valuable source of the metal nutrients supplying Fe, Cu, and Mn in full and Zn in part, but a very large fraction of the litter-supplied metal nutrients remained in the growing mix.

  1. Dietary Manganese Modulates PCB126 Toxicity, Metal Status, and MnSOD in the Rat

    PubMed Central

    Wang, Bingxuan; Klaren, William D.; Wels, Brian R.; Simmons, Donald L.; Olivier, Alicia K.; Wang, Kai; Robertson, Larry W.; Ludewig, Gabriele

    2016-01-01

    PCB126 (3,3′,4,4′,5-pentachlorobiphenyl) is a potent aryl hydrocarbon receptor agonist and induces oxidative stress. Because liver manganese (Mn) levels decrease in response to PCB126, a Mn dietary study was designed to investigate the role of Mn in PCB126 toxicity. Male Sprague Dawley rats received diets containing 0, 10, or 150 ppm added Mn for 3 weeks, followed by a single ip injection of corn oil or PCB126 (5 µmol/kg body weight). After 2 weeks, Mn, Cu, Zn, and Fe levels in the heart, liver, and liver mitochondria, and Mn-containing superoxide dismutase (MnSOD) and metallothionein mRNA, MnSOD protein, and MnSOD activity were determined. Mn levels in liver, heart, and liver mitochondria were strongly decreased by the Mn-deficient diet. Small effects on Fe levels and a stepwise increase in MnSOD activity with dietary Mn were also visible. PCB126 caused profound changes in Cu (up), Zn, Fe, and Mn (down) in liver, but not in heart, and differing effects (Cu, Zn, and Fe up, Mn down) in liver mitochondria. Liver MnSOD and metallothionein mRNA levels and MnSOD protein were increased but MnSOD activity was decreased by PCB126. PCB126-induced liver enlargement was dose-dependently reduced with increasing dietary Mn. These changes in metals homeostasis and MnSOD activity in liver but not heart may be a/the mechanism of PCB126 liver-specific toxicity. Specifically, transport of Fenton metals (Cu, Fe) into and Mn out of the mitochondria, a probable mechanism for lower MnSOD activity, may be a/the cause of PCB126-induced oxidative stress. The role of metallothioneins needs further evaluation. Dietary Mn slightly alleviated PCB126-induced toxicities. PMID:26660635

  2. Isolation, Chromosomal Localization, and Differential Expression of Mitochondrial Manganese Superoxide Dismutase and Chloroplastic Copper/Zinc Superoxide Dismutase Genes in Wheat1

    PubMed Central

    Wu, Guohai; Wilen, Ronald W.; Robertson, Albert J.; Gusta, Lawrence V.

    1999-01-01

    Superoxide dismutase (SOD) gene expression was investigated to elucidate its role in drought and freezing tolerance in spring and winter wheat (Triticum aestivum). cDNAs encoding chloroplastic Cu/ZnSODs and mitochondrial MnSODs were isolated from wheat. MnSOD and Cu/ZnSOD genes were mapped to the long arms of the homologous group-2 and -7 chromosomes, respectively. Northern blots indicated that MnSOD genes were drought inducible and decreased after rehydration. In contrast, Cu/ZnSOD mRNA was not drought inducible but increased after rehydration. In both spring and winter wheat seedlings exposed to 2°C, MnSOD transcripts attained maximum levels between 7 and 49 d. Transcripts of Cu/ZnSOD mRNA were detected sooner in winter than in spring wheat; however, they disappeared after 21 d of acclimation. Transcripts of both classes of SOD genes increased during natural acclimation in both spring and winter types. Exposure of fully hardened plants to three nonlethal freeze-thaw cycles resulted in Cu/Zn mRNA accumulation; however, MnSOD mRNA levels declined in spring wheat but remained unchanged in winter wheat. The results of the dehydration and freeze-thaw-cycle experiments suggest that winter wheat has evolved a more effective stress-repair mechanism than spring wheat. PMID:10364402

  3. Conjugation of glucose oxidase onto Mn-doped ZnS quantum dots for phosphorescent sensing of glucose in biological fluids.

    PubMed

    Wu, Peng; He, Yu; Wang, He-Fang; Yan, Xiu-Ping

    2010-02-15

    Integrating various enzymes with nanomaterials provides various nanohybrids with new possibilities in biosensor applications. Furthermore, the enzymatic activity and stability are also improved due to the large surface area of nanomaterials. Here we report the conjugation of glucose oxidase (GOD) onto phosphorescent Mn-doped ZnS quantum dots (QDs) using 1-ethyl-3-(3-dimethylaminopropy)carbodiimide (EDC)/N-hydroxysuccinimide (NHS) as coupling reagents for glucose biosensing based on the effective quenching of the room temperature phosphorescence (RTP) of Mn-doped ZnS QDs by the H(2)O(2) generated from GOD-catalyzed oxidation of glucose. The obtained bioconjugate not only provided improved enzymatic performance with Michaelis-Menten constant of 0.70 mM but also favored biological applications because the phosphorescent detection mode avoided the interference from autofluorescence and scattering light from the biological matrix. In addition, the GOD-conjugated Mn-doped ZnS QDs showed better thermal stability in the temperature range of 20-80 degrees C. The GOD-Mn-doped ZnS QDs based RTP sensor for glucose gave a detection limit of 3 microM and two linear ranges from 10 microM to 0.1 mM and from 0.1 to 1 mM. The developed biosensor was successfully applied to the determination of glucose in real serum samples without the need for any complicated sample pretreatments.

  4. Optical detection of organophosphorus compounds based on Mn-doped ZnSe d-dot enzymatic catalytic sensor.

    PubMed

    Gao, Xue; Tang, Guangchao; Su, Xingguang

    2012-01-01

    In this paper, we report a sensitive and selective method for detection of organophosphorus compounds (OPs) based on Mn:ZnSe d-dots-enzyme-hydrogen peroxide (H(2)O(2)) fluorescence quenching system. Acetylcholine esterase (AChE) can hydrolyze acetylcholine (ACh) to choline. Subsequently, choline oxidase (ChOx) oxidizes choline to generate H(2)O(2). The enzyme-generated H(2)O(2) can quench the fluorescence of Mn:ZnSe d-dots. When paraoxon are introduced in solution, it can interact with the active centers of AChE and decrease the enzyme activity. This leads to the decrease of the H(2)O(2) production and then the fluorescence quenching rate of Mn:ZnSe d-dots. Experimental results showed that the enzyme inhibition percentage of Mn:ZnSe d-dots-ChOx-AChE-ACh system was proportional to the logarithm of paraoxon in the range 4.84×10(-11) to 4.84×10(-6) mol/L with the detection limit (S/N=3) of 1.31×10(-11) mol/L. The proposed biosensor has been employed for quick determination of paraoxon in tap water and milk samples with satisfactory reproducibility and accuracy. This nano-biosensor was proved to be sensitive, rapid, simple and tolerance of most interfering substances. Copyright © 2012 Elsevier B.V. All rights reserved.

  5. Synthesis and stability of hetaerolite, ZnMn2O4, at 25°C

    USGS Publications Warehouse

    Hem, J.D.; Roberson, C.E.; Lind, Carol J.

    1987-01-01

    Hetaerolite appears to be more stable than hausmannite with respect to spontaneous conversion to γMnOOH. The value of the standard free energy of formation of hetaerolite was estimated from the experimental data to be −289.4 ± 0.8 kcal per mole. Solids intermediate in composition between hetaerolite and hausmannite can be prepared by altering the Mn/Zn ratio in the feed solution.

  6. Structural and electrical properties of Zn1.10CuxMn1.90-xO4 (0 ≤ x ≤ 0.15) for application in IR detectors

    NASA Astrophysics Data System (ADS)

    Kim, Kyeong-Min; Lee, Sung-Gap; Lee, Dong-Jin; Kwon, Min-Su

    2017-05-01

    In this study, Zn1.10CuxMn1.90-xO4 (0 ≤ x ≤ 0.15) systems were prepared through the conventional solid state reaction method. All specimens were sintered in air at 1200 °C for 12 h and cooled at a rate of 2 °C/min to 800 °C, subsequently quenching to room temperature. Structural investigations were carried out using X-ray diffraction patterns and energy dispersive spectrometry. For x ≥ 0.10, formation of a tetragonal phase with a Zn-rich Zn-Cu-Mn-O segregated second phase was observed. In the microstructure, the grain size increased from 5.10 μm to 9.68 μm with an increase in Cu content. The resistivity at room temperature, B-value, responsivity and detectivity of the Zn1.10Cu0.05Mn1.85O4 specimen were found to be 300.2 kΩ·cm, 4665, 0.025 V/W, and 2.12 ×104 cmHz1/2/W, respectively. [Figure not available: see fulltext.

  7. Effect of Zn doping on the magneto-caloric effect and critical constants of Mott insulator MnV{sub 2}O{sub 4}

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Shahi, Prashant; Kumar, A.; Shukla, K. K.

    2014-09-15

    X-ray absorption near edge spectra (XANES) and magnetization of Zn doped MnV{sub 2}O{sub 4} have been measured and from the magnetic measurement the critical exponents and magnetocaloric effect have been estimated. The XANES study indicates that Zn doping does not change the valence states in Mn and V. It has been shown that the obtained values of critical exponents β, γ and δ do not belong to universal class and the values are in between the 3D Heisenberg model and the mean field interaction model. The magnetization data follow the scaling equation and collapse into two branches indicating that themore » calculated critical exponents and critical temperature are unambiguous and intrinsic to the system. All the samples show large magneto-caloric effect. The second peak in magneto-caloric curve of Mn{sub 0.95}Zn{sub 0.05}V{sub 2}O{sub 4} is due to the strong coupling between orbital and spin degrees of freedom. But 10% Zn doping reduces the residual spins on the V-V pairs resulting the decrease of coupling between orbital and spin degrees of freedom.« less

  8. Effect of Synthesis Temperature and NaOH Concentration on Microstructural and Magnetic Properties of Mn0.5Zn0.5Fe2O4 Nanoparticles

    NASA Astrophysics Data System (ADS)

    Siregar, N.; Indrayana, I. P. T.; Suharyadi, E.; Kato, T.; Iwata, S.

    2017-05-01

    Mn0.5Zn0.5Fe2O4 nanoparticles have been successfully synthesized through coprecipitation method by varying NaOH concentrations from 0.5 M to 6 M and synthesis temperatures from 30 to 120 °C. The X-ray diffraction (XRD) pattern indicates samples consisting of multiphase structures such as spinel of Mn0.5Zn0.5Fe2O4, α-MnO2, ZnO, λ-MnO2, and γ-Fe2O3. The crystallite size of Mn0.5Zn0.5Fe2O4 is in the range of 14.1 to 26.7 nm. The Transmission electron microscope (TEM) image shows that sample was agglomerate. The hysteresis loops confirm that nanoparticles are soft magnetic materials with low coercivity (H c) in the range of 45.9 to 68.5 Oe. Those values increased relatively with increasing particles size. For NaOH concentration variation, the maximum magnetization of the sample increased from 10.4 emu/g to 11.6 emu/g with increasing ferrite content. Meanwhile, the maximum magnetization increased from 7.9 to 15.7 emu/g for samples with various synthesis temperature. The highest coercivity of 68.5 Oe was attained for a sample of 6 M NaOH under 90 °C. The highest magnetization of 15.7 emu/g was achieved for a sample of 1.5 M NaOH under 120 °C caused by the maximum crystallinity of sample.

  9. Total content and bioavailability of plant essential nutrients and heavy metals in top-soils of an industrialized area of Northwestern Greece

    NASA Astrophysics Data System (ADS)

    Barouchas, Pantelis; Avramidis, Pavlos; Salachas, Georgios; Koulopoulos, Athanasios; Christodoulopoulou, Kyriaki; Liopa-Tsakalidi, Aglaia

    2017-04-01

    Thirty surface soil samples from northwestern Greece in the Ptolemais-Kozani basin, were collected and analyzed for their total content in thirteen elements (Al, Ca, Fe, K, Mg, Mn, Na, P, Cd, Cr, Cu, Ni, Pb, Zn) by ICP-AES and bioavailable content from a plant nutrition scope of view for (Ca, Fe, K, Mg, Mn, Na, P, Zn) by AAS and colorimetric techniques. Particle size distribution, Cation Exchange Capacity (CEC) and the magnetic susceptibility, in a low and a high frequency (at 47kHz and 0.47kHz), of soil samples were measured also in order to correlate the results. Total carbonates were tested by the pressure technique (BD Inventions, FOGII digital soil calcimeter). The concentrations of these elements were compared with international standards and guidelines. The results indicated that Cu, Cd, Zn and Pb are found enriched in the top soils of the study area, mainly as a consequence of natural processes from the surrounding rocks. Moreover, the bioavailability of some of these elements with a plant nutrition interest was tested and results indicate that they do not pose an immediate threat to the environment or crops as it all demonstrated values in an adequate range. Magnetic susceptibility in low and high frequency was correlated with clay content.

  10. [Long-term effects of tillage methods on heavy metal accumulation and availability in purple paddy soil].

    PubMed

    Chang, Tong-Ju; Cui, Xiao-Qiang; Ruan, Zhen; Zhao, Xiu-Lan

    2014-06-01

    A long-term experiment, conducted at Southwest University since 1990, was used to evaluate the effect of tillage methods on the total and available contents of heavy metals (Fe, Mn, Cu, Zn, Pb, Cd) in the profile of purple paddy soil and the contents of those metals in root, stem leaf and brown rice. The experiment included five tillage methods: conventional tillage, paddy-upland rotation, no-tillage and fallow in winter, ridge-no-tillage and compartments-no-tillage. The results showed that the total concentrations of Fe, Cu, Zn, Pb and Cd in the soil profile had no significant differences among five treatments, but it was found that total Mn has a significant decline in 0-20 cm under conventional tillage, paddy-upland rotation and no-tillage and fallow in winter compared with ridge-no-tillage and compartments-no-tillage. The availability of Fe, Cu, Zn, Pb and Cd decreased with the increase of soil depth in all treatments, but the availability of Mn was found to be the highest in the 20-40 cm layers except those in the paddy-upland rotation. In the ploughed layer, the contents of available Fe, Mn was the highest in paddy-upland rotation, while the contents of available Zn and Pb was the highest in conventional tillage, but tillage treatments had not significant influence to the contents of available Cu. Correlation analysis showed that available Fe was significantly negatively related to the pH values and significantly negatively related to the organic matter of soils, available Mn was significantly negatively related to the pH values and organic matter of soils, whereas the available Zn was significantly positively related to total Zn. The contents of Fe, Mn in rice root, the contents of Fe, Mn, Cu and Cd in rice straw and Cu in brown rice were higher under paddy-upland rotation, ridge-no-tillage and compartments-no-tillage than those in conventional tillage and no-tillage and fellow in winter. Paddy-upland rotation can significantly lower the migration coefficient value of Cd in brown rice, and the Pb, Cd concentration in brown rice in the treatment of paddy-upland rotation was lower than the upper limit (< 0.2 mg x kg(-1)) of the National Standard for Food Hygiene for Cd concentration. The content of Fe in root was significantly and negatively related with soil pH and significantly and positively related with soil available Fe, the content of Mn in root was significantly negatively related with soil pH and significantly positively related with soil available Mn, the content of Mn in straw was significantly negatively related with soil pH, significantly positively related with soil total Mn and significantly positively related with soil available Mn, the content of Cu in straw and brown rice was significantly negatively related with soil pH, the content of Zn was significant related with soil pH and significant related with soil CEC. The content of Fe in root, Mn in root and straw and Cd in straw was positively related with soil available Fe, Mn and Cd, respectively, but was negatively related with pH in plough layer soil, Zn in straw was also negatively related with plough layer soil pH. From the results as above, it is concluded that different tillage methods can change the values of soil pH, alter the availability of heavy metal in soils, consequently affect uptake of heavy metal by rice. Of the tillage methods, paddy-upland rotation could increase the availability of Fe and Mn, but decrease the availability of Zn, Pb and Cd in purple paddy soils. Paddy-upland rotation can also increase the contents of Fe, Mn in rice root and straw, but decrease Cd content in brown rice, and could reduce the Pb, Cd contents in brown rice in a certain extent, however, attention should be given to long-term paddy-upland rotation cause of leaching of soil surface Mn.

  11. Electrophoretic properties of BSA-coated quantum dots.

    PubMed

    Bücking, Wendelin; Massadeh, Salam; Merkulov, Alexei; Xu, Shu; Nann, Thomas

    2010-02-01

    Low toxic InP/ZnS quantum dots (QDs), ZnS:Mn(2+)/ZnS nanocrystals and CdSe/ZnS nanoparticles were rendered water-dispersible by different ligand-exchange methods. Eventually, they were coated with bovine serum albumin (BSA) as a model protein. All particles were characterised by isotachophoresis (ITP), laser Doppler velocimetry (LDV) and agarose gel electrophoresis. It was found that the electrophoretic mobility and colloidal stability of ZnS:Mn(2+)/ZnS and CdSe/ZnS nanoparticles, which bore short-chain surface ligands, was primarily governed by charges on the nanoparticles, whereas InP/ZnS nanocrystals were not charged per se. BSA-coated nanoparticles showed lower electrophoretic mobility, which was attributed to their larger size and smaller overall charge. However, these particles were colloidally stable. This stability was probably caused by steric stabilisation of the BSA coating.

  12. Simultaneous recovery of Zn and Mn from used batteries in acidic and alkaline mediums: A comparative study.

    PubMed

    Abid Charef, S; Affoune, A M; Caballero, A; Cruz-Yusta, M; Morales, J

    2017-10-01

    A parallel study of acidic and alkaline leaching for the recovery of Mn and Zn from spent alkaline batteries is outlined. Using H 2 SO 4 as solvent and selecting appropriate conditions of temperature and concentration, all residues were dissolved except carbon. The separation and recovery of the two components were performed by electrodeposition with satisfactory results at pH values above 4 (current efficiency above 70% for Zn and Mn) but rather lower efficiencies as the pH decreased. Most of the Zn was selectively dissolved by alkaline leaching using a 6.5M NaOH solution, and its recovery was examined by means of both electrochemical and chemical processes. The expected formation of pure Zn by electrowinning failed due to the formation of ZnO, the content of which was highly dependent on the electrodeposition time. For short periods, Zn was the main component. For longer periods the electrodeposit consisted of agglomerated microparticles of ZnO with a minor fraction of Zn metal (barely 3% as measured by X-ray diffraction). A chemical reaction of the element with oxygen released at the anode surface might be responsible for its conversion to ZnO. A simple chemical route is described for the first time for the direct conversion of Zn(OH) 4 2- solution to nanostructured ZnO by lowering the pH to values around 12 using 2M HCl solution. Copyright © 2017 Elsevier Ltd. All rights reserved.

  13. Trace metals in estuaries in the Russian Far East and China: case studies from the Amur River and the Changjiang.

    PubMed

    Shulkin, Vladimir; Zhang, Jing

    2014-11-15

    This paper compares the distributions of dissolved and particulate forms of Mn, Fe, Ni, Cu, Zn, Cd, and Pb in the estuaries of the largest rivers in East Asia: the Amur River and the Changjiang (Yangtze River). High suspended solid concentrations, elevated pH, and relatively low dissolved trace metal concentrations are characteristics of the Changjiang. Elevated dissolved Fe and Mn concentrations, neutral pH, and relatively low suspended solid concentrations are characteristics of the Amur River. The transfer of dissolved Fe to suspended forms is typical in the Amur River estuary, though Cd and Mn tend to mobilize to solution, and Cu and Ni are diluted in the estuarine system. Metal concentrations in suspended matter in the Amur River estuary are controlled by the ratio of terrigenous riverine material, enriched in Al and Fe, and marine biogenic particles, enriched in Cu, Mn, Cd, and in some cases Ni. The increase in dissolved forms of Mn, Fe, Ni, Cu, Cd, and Pb compared with river end-member is unique to the Changjiang estuary. Particle-solution interactions are not reflected in bulk suspended-solid metal concentrations in the Changjiang estuary due to the dominance of particulate forms of these metals. Cd is an exception in the Changjiang estuary, where the increase in dissolved Cd is of comparable magnitude to the decrease in particulate Cd. Despite runoff in the Amur River being lower than that in the Changjiang, the fluxes of dissolved Mn, Zn and Fe in the Amur River exceed those in the Changjiang. Dissolved Ni, and Cd fluxes are near equal in both estuaries, but dissolved Cu is lower in the Amur River estuary. The hydrological and physico-chemical river characteristics are dominated at the assessment of river influence on the adjoining coastal sea areas despite differences in estuarine processes. Copyright © 2014 Elsevier B.V. All rights reserved.

  14. Electrodeposition synthesis and electrochemical properties of nanostructured γ-MnO 2 films

    NASA Astrophysics Data System (ADS)

    Chou, Shulei; Cheng, Fangyi; Chen, Jun

    The thin films of carambola-like γ-MnO 2 nanoflakes with about 20 nm in thickness and at least 200 nm in width were prepared on nickel sheets by combination of potentiostatic and cyclic voltammetric electrodeposition techniques. The as-prepared MnO 2 nanomaterials, which were characterized by scanning electron microscopy (SEM), transmission electron microscopy (TEM), X-ray diffraction (XRD), and X-ray photoelectron spectroscopy (XPS), were used as the active material of the positive electrode for primary alkaline Zn/MnO 2 batteries and electrochemical supercapacitors. Electrochemical measurements showed that the MnO 2 nanoflake films displayed high potential plateau (around 1.0 V versus Zn) in primary Zn/MnO 2 batteries at the discharge current density of 500 mA g -1 and high specific capacitance of 240 F g -1 at the current density of 1 mA cm -2. This indicated the potential application of carambola-like γ-MnO 2 nanoflakes in high-power batteries and electrochemical supercapacitors. The growth process for the one- and three-dimensional nanostructured MnO 2 was discussed on the basis of potentiostatic and cyclic voltammetric techniques. The present synthesis method can be extended to the preparation of other nanostructured metal-oxide films.

  15. Intrinsic borohydride fuel cell/battery hybrid power sources

    NASA Astrophysics Data System (ADS)

    Hong, Jian; Fang, Bin; Wang, Chunsheng; Currie, Kenneth

    The electrochemical oxidation behaviors of NaBH 4 on Zn, Zn-MH, and MH (metal-hydride) electrodes were investigated, and an intrinsic direct borohydride fuel cell (DBFC)/battery hybrid power source using MH (or Zn-MH) as the anode and MnO 2 as the cathode was tested. Borohydride cannot be effectively oxidized on Zn electrodes at the Zn oxidation potential because of the poor electrocatalytic ability of Zn for borohydride oxidation and the high overpotential, even though borohydride has the same oxidation potential of Zn in an alkaline solution. The borohydride can be electrochemically oxidized on Ni and MH electrodes through a 4e reaction at a high overpotential. Simply adding borohydride into an alkaline electrolyte of a Zn/air or MH/air battery can greatly increase the capacity, while an intrinsic DBFC/MH(or Zn)-MnO 2 battery can deliver a higher peak power than regular DBFCs.

  16. Metal Complexation in Xylem Fluid 1

    PubMed Central

    White, Michael C.; Chaney, Rufus L.; Decker, A. Morris

    1981-01-01

    The capacity of ligands in xylem fluid to form metal complexes was tested with a series of in vitro experiments using paper electrophoresis and radiographs. The xylem fluid was collected hourly for 8 hours from soybean (Glycine max L. Merr.) and tomato (Lycopersicon esculentum Mill.) plants grown in normal and Zn-phytotoxic nutrient solutions. Metal complexation was assayed by anodic or reduced cathodic movement of radionuclides (63Ni, 65Zn, 109Cd, 54Mn) that were presumed to have formed negatively charged complexes. Electrophoretic migration of Ni, Zn, Cd, and Mn added to xylem exudate and spotted on KCl- or KNO3-wetted paper showed that stable Ni, Zn, and Cd metal complexes were formed by exudate ligands. No anodic Mn complexes were observed in this test system. Solution pH, plant species, exudate collection time, and Zn phytotoxicity all affected the amount of metal complex formed in exudate. As the pH increased, there was increased anodic metal movement. Soybean exudate generally bound more of each metal than did tomato exudate. Metal binding usually decreased with increasing exudate collection time, and less metal was bound by the high-Zn exudate. Ni, Zn, Cd, and Mn in exudate added to exudate-wetted paper demonstrated the effect of ligand concentration on stable metal complex formation. Complexes for each metal were demonstratable with this method. Cathodic metal movement increased with time of exudate collection, and it was greater in the high-Zn exudate than in the normal-Zn exudate. A model study illustrated the effect of ligand concentration on metal complex stability in the electrophoretic field. Higher ligand (citric acid) concentrations increased the stability for all metals tested. Images PMID:16661666

  17. Transcriptional Regulation, Metal Binding Properties and Structure of Pden1597, an Unusual Zinc Transport Protein from Paracoccus denitrificans*

    PubMed Central

    Handali, Melody; Neupane, Durga P.; Roychowdhury, Hridindu; Yukl, Erik T.

    2015-01-01

    ATP-binding cassette (ABC) transporters of the cluster 9 family are ubiquitous among bacteria and essential for acquiring Zn2+ and Mn2+ from the environment or, in the case of pathogens, from the host. These rely on a substrate-binding protein (SBP) to coordinate the relevant metal with high affinity and specificity and subsequently release it to a membrane permease for translocation into the cytoplasm. Although a number of cluster 9 SBP structures have been determined, the structural attributes conferring Zn2+ or Mn2+ specificity remain ambiguous. Here we describe the gene expression profile, in vitro metal binding properties, and crystal structure of a new cluster 9 SBP from Paracoccus denitrificans we have called AztC. Although all of our results strongly indicate Zn2+ over Mn2+ specificity, the Zn2+ ion is coordinated by a conserved Asp residue only observed to date as a metal ligand in Mn2+-specific SBPs. The unusual sequence properties of this protein are shared among close homologues, including members from the human pathogens Klebsiella pneumonia and Enterobacter aerogenes, and would seem to suggest a subclass of Zn2+-specific transporters among the cluster 9 family. In any case, the unusual coordination environment of AztC expands the already considerable range of those available to Zn2+-specific SBPs and highlights the presence of a His-rich loop as the most reliable indicator of Zn2+ specificity. PMID:25787075

  18. Transcriptional regulation, metal binding properties and structure of Pden1597, an unusual zinc transport protein from Paracoccus denitrificans

    DOE PAGES

    Handali, Melody; Neupane, Durga P.; Roychowdhury, Hridindu; ...

    2015-03-18

    Here, ATP-binding cassette (ABC) transporters of the cluster 9 family are ubiquitous among bacteria and essential for acquiring Zn 2+ and Mn 2+ from the environment or, in the case of pathogens, from the host. These rely on a substrate-binding protein (SBP) to coordinate the relevant metal with high affinity and specificity and subsequently release it to a membrane permease for translocation into the cytoplasm. Although a number of cluster 9 SBP structures have been determined, the structural attributes conferring Zn 2+ or Mn 2+ specificity remain ambiguous. Here we describe the gene expression profile, in vitro metal binding properties,more » and crystal structure of a new cluster 9 SBP from Paracoccus denitrificans we have called AztC. Although all of our results strongly indicate Zn 2+ over Mn 2+ specificity, the Zn 2+ ion is coordinated by a conserved Asp residue only observed to date as a metal ligand in Mn 2+-specific SBPs. The unusual sequence properties of this protein are shared among close homologues, including members from the human pathogens Klebsiella pneumonia and Enterobacter aerogenes, and would seem to suggest a subclass of Zn 2+-specific transporters among the cluster 9 family. In any case, the unusual coordination environment of AztC expands the already considerable range of those available to Zn 2+-specific SBPs and highlights the presence of a His-rich loop as the most reliable indicator of Zn 2+ specificity.« less

  19. Dissolved trace elements in a nitrogen-polluted river near to the Liaodong Bay in Northeast China.

    PubMed

    Bu, Hongmei; Song, Xianfang; Guo, Fen

    2017-01-15

    Dissolved trace element concentrations (Ba, Fe, Mn, Si, Sr, and Zn) were investigated in the Haicheng River near to the Liaodong Bay in Northeast China during 2010. Dissolved Ba, Fe, Mn, and Sr showed significant spatial variation, whereas dissolved Fe, Mn, and Zn displayed seasonal variations. Conditions such as water temperature, pH, and dissolved oxygen were found to have an important impact on redox reactions involving dissolved Ba, Fe, and Zn. Dissolved Fe and Mn concentrations were regulated by adsorption or desorption of Fe/Mn oxyhydroxides and the effects of organic carbon complexation on dissolved Ba and Sr were found to be significant. The sources of dissolved trace elements were found to be mainly from domestic sewage, industrial waste, agricultural surface runoff, and natural origin, with estimated seasonal and annual river fluxes established as important inputs of dissolved trace elements from the Haicheng River into the Liaodong Bay or Bohai Sea. Copyright © 2016 Elsevier Ltd. All rights reserved.

  20. Baseline blood levels of manganese, lead, cadmium, copper, and zinc in residents of Beijing suburb

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Zhang, Long-Lian, E-mail: Longlian57@163.com; Lu, Ling; Pan, Ya-Juan

    Baseline blood concentrations of metals are important references for monitoring metal exposure in environmental and occupational settings. The purpose of this study was to determine the blood levels of manganese (Mn), copper (Cu), zinc (Zn), lead (Pb), and cadmium (Cd) among the residents (aged 12–60 years old) living in the suburb southwest of Beijing in China and to compare the outcomes with reported values in various developed countries. Blood samples were collected from 648 subjects from March 2009 to February 2010. Metal concentrations in the whole blood were determined by ICP-MS. The geometric means of blood levels of Mn, Cu,more » Zn, Pb and Cd were 11.4, 802.4, 4665, 42.6, and 0.68 µg/L, respectively. Male subjects had higher blood Pb than the females, while the females had higher blood Mn and Cu than the males. There was no gender difference for blood Cd and Zn. Smokers had higher blood Cu, Zn, and Cd than nonsmokers. There were significant age-related differences in blood levels of all metals studied; subjects in the 17–30 age group had higher blood levels of Mn, Pb, Cu, and Zn, while those in the 46–60 age group had higher Cd than the other age groups. A remarkably lower blood level of Cu and Zn in this population as compared with residents of other developed countries was noticed. Based on the current study, the normal reference ranges for the blood Mn were estimated to be 5.80–25.2 μg/L; for blood Cu, 541–1475 μg/L; for blood Zn, 2349–9492 μg/L; for blood Pb, <100 μg/L; and for blood Cd, <5.30 μg/L in the general population living in Beijing suburbs. - Highlights: • Baseline blood levels of metals in residents of Beijing suburb are investigated. • BMn and BPb in this cohort are higher than those in other developed countries. • Remarkably lower blood levels of Cu and Zn in this Chinese cohort are noticed. • The reference values for blood levels of Mn, Cu, Zn, Pb, and Cd are established.« less

Top