Dawlee, S; Jayabalan, Muthu
2011-10-01
Biofunctionally active and inherently radiopaque polymers are the emerging need for biomedical applications. Novel segmented polyurethane elastomer with inherent radiopacity was prepared using aliphatic chain extender 2,3-diiodo-2-butene-1,4-diol, polyol polytetramethylene glycol and 4,4'-methylenebis(phenyl isocyanate) (MDI) for blood compatible applications. Aliphatic polyurethane was also prepared using hexamethylene diisocyanate for comparison. X-ray analysis of the polyurethanes revealed good radiopacity even at a relatively low concentration of 3% iodine in aromatic polyurethane and 10% in aliphatic polyurethane. The polyurethanes also possessed excellent thermal stability. MDI-based polyurethane showed considerably higher tensile strength than the analogous HDI-based polyurethane. MDI-based aromatic polyurethane exhibited a dynamic surface morphology in aqueous medium, resulting in the segregation of hydrophilic domains which was more conducive to anti-thrombogenic properties. The polyurethane was cytocompatible with L929 fibroblast cells, non-hemolytic, and possessed good blood compatibility.
Highly fluorinated polyurethanes
NASA Technical Reports Server (NTRS)
Stump, E. C., Jr.; Rochow, S. E. (Inventor)
1972-01-01
New polyurethanes containing a high degree of fluorine atoms are reported. The presence of the fluorine atoms in the polyurethane resins provides material having good thermal stability and chemical resistance. These polyurethanes are derived from a new hydroxy-terminated perfluoro polyether. The hydroxy terminated material is reacted with a diisocyanate to produce the polyurethanes. The polyurethanes can be used to form seals, coatings, potting material, hoses and the like.
NASA Astrophysics Data System (ADS)
Beliaev, A.; Svistkov, A.; Iziumov, R.; Osorgina, I.; Kondyurin, A.; Bilek, M.; McKenzie, D.
2016-04-01
Production of biocompatible implants made of polyurethane treated with plasma is very perspective. During plasma treatment the surface of polyurethane acquires unique physic-chemical properties. However such treatment may change the mechanical properties of polyurethane which may adversely affect the deformation behaviour of the real implant. Therefore careful study of the mechanical properties of the plasma-modified polyurethane is needed. In this paper, experimental observations of the elastic characteristics of plasma treated polyurethane and modelling of the deformation behaviour of polyurethane bio-implants are reported.
Brzeska, Joanna; Morawska, Magda; Heimowska, Aleksandra; Sikorska, Wanda; Wałach, Wojciech; Hercog, Anna; Kowalczuk, Marek; Rutkowska, Maria
2018-01-01
The surface morphology and thermal properties of polyurethanes can be correlated to their chemical composition. The hydrophilicity, surface morphology, and thermal properties of polyurethanes (differed in soft segments and in linear/cross-linked structure) were investigated. The influence of poly([ R , S ]-3-hydroxybutyrate) presence in soft segments and blending of polyurethane with polylactide on surface topography were also estimated. The linear polyurethanes (partially crystalline) had the granular surface, whereas the surface of cross-linked polyurethanes (almost amorphous) was smooth. Round aggregates of polylactide un-uniformly distributed in matrix of polyurethane were clearly visible. It was concluded that some modification of soft segment (by mixing of poly([ R , S ]-3-hydroxybutyrate) with different polydiols and polytriol) and blending of polyurethanes with small amount of polylactide influence on crystallinity and surface topography of obtained polyurethanes.
[Modern polyurethanes in cardiovascular surgery].
Gostev, A A; Laktionov, P P; Karpenko, A A
Currently, there is great clinical demand for synthetic tissue-engineered cardiovascular prostheses with good long-term patency. Polyurethanes belong to the class of polymers with excellent bio- and hemocompatibility. They are known to possess good mechanical properties, but are prone to processes of degradation in conditions of functioning in living organisms. Attempts at solving this problem have resulted in the development of various new subclasses of polyurethanes such as thermoplastic polyether polyurethanes, polyurethanes with a silicone segment, polycarbonate polyurethanes and nanocomposite polyurethanes. This was accompanied and followed by offering a series of new technologies of production of implantable medical devices such as vascular grafts, heart valves and others. In the presented review, we discuss biological and mechanical properties of modern subclasses of polyurethanes, as well as modern methods of manufacturing implantable medical devices made of polyurethanes, especially small-diameter vascular prostheses.
Stable Polyurethane Coatings for Electronic Circuits
NASA Technical Reports Server (NTRS)
Morris, D. E.
1983-01-01
Alkane-based polyurethanes resist deterioration while maintaining good dielectric properties. Weight loss after prolonged immersion in hot water far less for alkane-based polyurethanes than for more common ether based polyurethanes, at any given oxygen content. Major uses of polyurethanes are as connector potting materials and conformal coatings for printed circuit boards.
Cregut, Mickael; Bedas, M; Durand, M-J; Thouand, G
2013-12-01
Polyurethanes are polymeric plastics that were first used as substitutes for traditional polymers suspected to release volatile organic hazardous substances. The limitless conformations and formulations of polyurethanes enabled their use in a wide variety of applications. Because approximately 10 Mt of polyurethanes is produced each year, environmental concern over their considerable contribution to landfill waste accumulation appeared in the 1990s. To date, no recycling processes allow for the efficient reuse of polyurethane waste due to their high resistance to (a)biotic disturbances. To find alternatives to systematic accumulation or incineration of polyurethanes, a bibliographic analysis was performed on major scientific advances in the polyurethane (bio)degradation field to identify opportunities for the development of new technologies to recondition this material. Until polymers exhibiting oxo- or hydro-biodegradative traits are generated, conventional polyurethanes that are known to be only slightly biodegradable are of great concern. The research focused on polyurethane biodegradation highlights recent attempts to reprocess conventional industrial polyurethanes via microbial or enzymatic degradation. This review describes several wonderful opportunities for the establishment of new processes for polyurethane recycling. Meeting these new challenges could lead to the development of sustainable management processes involving polymer recycling or reuse as environmentally safe options for industries. The ability to upgrade polyurethane wastes to chemical compounds with a higher added value would be especially attractive. © 2013.
Novel route of synthesis for cellulose fiber-based hybrid polyurethane
NASA Astrophysics Data System (ADS)
Ikhwan, F. H.; Ilmiati, S.; Kurnia Adi, H.; Arumsari, R.; Chalid, M.
2017-07-01
Polyurethanes, obtained by the reaction of a diisocyanate compound with bifunctional or multifunctional reagent such as diols or polyols, have been studied intensively and well developed. The wide range modifier such as chemical structures and molecular weight to build polyurethanes led to designs of materials that may easily meet the functional product demand and to the extraordinary spreading of these materials in market. Properties of the obtained polymer are related to the chemical structure of polyurethane backbone. A number polyurethanes prepared from biomass-based monomers have been reported. Cellulose fiber, as a biomass material is containing abundant hydroxyl, promising material as chain extender for building hybrid polyurethanes. In previous researches, cellulose fiber was used as filler in synthesis of polyurethane composites. This paper reported a novel route of hybrid polyurethane synthesis, which a cellulose fiber was used as chain extender. The experiment performed by reacting 4,4’-Methylenebis (cyclohexyl isocyanate) (HMDI) and polyethylene glycol with variation of molecular weight to obtained pre-polyurethane, continued by adding micro fiber cellulose (MFC) with variation of type and composition in the mixture. The experiment was evaluated by NMR, FTIR, SEM and STA measurement. NMR and FTIR confirmed the reaction of the hybrid polyurethane. STA showed hybrid polyurethane has good thermal stability. SEM showed good distribution and dispersion of sorghum-based MFC.
Code of Federal Regulations, 2012 CFR
2012-07-01
... polyurethane foam production-HAP ABA emissions from the production line. 63.1297 Section 63.1297 Protection of... Pollutants for Flexible Polyurethane Foam Production § 63.1297 Standards for slabstock flexible polyurethane... § 63.1293(a)(1) shall control HAP ABA emissions from the slabstock polyurethane foam production line in...
Code of Federal Regulations, 2010 CFR
2010-07-01
... polyurethane foam production-HAP ABA emissions from the production line. 63.1297 Section 63.1297 Protection of... Pollutants for Flexible Polyurethane Foam Production § 63.1297 Standards for slabstock flexible polyurethane... § 63.1293(a)(1) shall control HAP ABA emissions from the slabstock polyurethane foam production line in...
Code of Federal Regulations, 2011 CFR
2011-07-01
... polyurethane foam production-HAP ABA emissions from the production line. 63.1297 Section 63.1297 Protection of... Pollutants for Flexible Polyurethane Foam Production § 63.1297 Standards for slabstock flexible polyurethane... § 63.1293(a)(1) shall control HAP ABA emissions from the slabstock polyurethane foam production line in...
Chan-Chan, L H; Vargas-Coronado, R F; Cervantes-Uc, J M; Cauich-Rodríguez, J V; Rath, R; Phelps, E A; García, A J; San Román Del Barrio, J; Parra, J; Merhi, Y; Tabrizian, M
2013-08-01
Biodegradable segmented polyurethanes were prepared with poly(caprolactone) diol as a soft segment, 4,4'-methylene bis(cyclohexyl isocyanate) (HMDI) and either butanediol or dithioerythritol as chain extenders. Platelet adhesion was similar in all segmented polyurethanes studied and not different from Tecoflex® although an early stage of activation was observed on biodegradable segmented polyurethane prepared with dithioerythritol. Relative viability was higher than 80% on human umbilical vein endothelial cells in contact with biodegradable segmented polyurethane extracts after 1, 2 and 7 days. Furthermore, both biodegradable segmented polyurethane materials supported human umbilical vein endothelial cell adhesion, spreading, and viability similar to Tecoflex® medical-grade polyurethane. These biodegradable segmented polyurethanes represent promising materials for cardiovascular applications.
Efficient continuous dryer for flexible polyurethane foam and cleaning apparatus
Jody, Bassam; Daniels, Edward; Libera, Joseph A.
1999-01-01
A method of cleaning polyurethane foams where the material is transported through a wash station while alternately soaking the polyurethane foam in an organic solvent and squeezing solvent from the polyurethane foam a number of times. Then the polyurethane foam is sent through a rinse or solvent transfer station for reducing the concentration of solvent in the foam. The rinsed polyurethane foam is sent to a drying station wherein the foam is repeatedly squeezed while being exposed to hot air to remove wet air from the foam.
Efficient continuous dryer for flexible polyurethane foam and cleaning apparatus
Jody, B.; Daniels, E.; Libera, J.A.
1999-03-16
A method of cleaning polyurethane foams where the material is transported through a wash station while alternately soaking the polyurethane foam in an organic solvent and squeezing solvent from the polyurethane foam a number of times. Then the polyurethane foam is sent through a rinse or solvent transfer station for reducing the concentration of solvent in the foam. The rinsed polyurethane foam is sent to a drying station wherein the foam is repeatedly squeezed while being exposed to hot air to remove wet air from the foam. 4 figs.
Skeletal myotube formation enhanced by electrospun polyurethane carbon nanotube scaffolds
Sirivisoot, Sirinrath; Harrison, Benjamin S
2011-01-01
Background This study examined the effects of electrically conductive materials made from electrospun single- or multiwalled carbon nanotubes with polyurethane to promote myoblast differentiation into myotubes in the presence and absence of electrical stimulation. Methods and results After electrical stimulation, the number of multinucleated myotubes on the electrospun polyurethane carbon nanotube scaffolds was significantly larger than that on nonconductive electrospun polyurethane scaffolds (5% and 10% w/v polyurethane). In the absence of electrical stimulation, myoblasts also differentiated on the electrospun polyurethane carbon nanotube scaffolds, as evidenced by expression of Myf-5 and myosin heavy chains. The myotube number and length were significantly greater on the electrospun carbon nanotubes with 10% w/v polyurethane than on those with 5% w/v polyurethane. The results suggest that, in the absence of electrical stimulation, skeletal myotube formation is dependent on the morphology of the electrospun scaffolds, while with electrical stimulation it is dependent on the electrical conductivity of the scaffolds. Conclusion This study indicates that electrospun polyurethane carbon nanotubes can be used to modulate skeletal myotube formation with or without application of electrical stimulation. PMID:22072883
40 CFR 721.8082 - Polyester polyurethane acrylate.
Code of Federal Regulations, 2011 CFR
2011-07-01
... 40 Protection of Environment 31 2011-07-01 2011-07-01 false Polyester polyurethane acrylate. 721... Substances § 721.8082 Polyester polyurethane acrylate. (a) Chemical substance and significant new uses subject to reporting. (1) The chemical substance identified generically as polyester polyurethane acrylate...
40 CFR 721.8082 - Polyester polyurethane acrylate.
Code of Federal Regulations, 2010 CFR
2010-07-01
... 40 Protection of Environment 30 2010-07-01 2010-07-01 false Polyester polyurethane acrylate. 721... Substances § 721.8082 Polyester polyurethane acrylate. (a) Chemical substance and significant new uses subject to reporting. (1) The chemical substance identified generically as polyester polyurethane acrylate...
Sustained Release Drug Delivery Applications of Polyurethanes.
Lowinger, Michael B; Barrett, Stephanie E; Zhang, Feng; Williams, Robert O
2018-05-09
Since their introduction over 50 years ago, polyurethanes have been applied to nearly every industry. This review describes applications of polyurethanes to the development of modified release drug delivery. Although drug delivery research leveraging polyurethanes has been ongoing for decades, there has been renewed and substantial interest in the field in recent years. The chemistry of polyurethanes and the mechanisms of drug release from sustained release dosage forms are briefly reviewed. Studies to assess the impact of intrinsic drug properties on release from polyurethane-based formulations are considered. The impact of hydrophilic water swelling polyurethanes on drug diffusivity and release rate is discussed. The role of pore formers in modulating drug release rate is examined. Finally, the value of assessing mechanical properties of the dosage form and approaches taken in the literature are described.
Development of polyurethanes for bone repair.
Marzec, M; Kucińska-Lipka, J; Kalaszczyńska, I; Janik, H
2017-11-01
The purpose of this paper is to review recent developments on polyurethanes aimed at the design, synthesis, modifications, and biological properties in the field of bone tissue engineering. Different polyurethane systems are presented and discussed in terms of biodegradation, biocompatibility and bioactivity. A comprehensive discussion is provided of the influence of hard to soft segments ratio, catalysts, stiffness and hydrophilicity of polyurethanes. Interaction with various cells, behavior in vivo and current strategies in enhancing bioactivity of polyurethanes are described. The discussion on the incorporation of biomolecules and growth factors, surface modifications, and obtaining polyurethane-ceramics composites strategies is held. The main emphasis is placed on the progress of polyurethane applications in bone regeneration, including bone void fillers, shape memory scaffolds, and drug carrier. Copyright © 2017 Elsevier B.V. All rights reserved.
40 CFR 721.9959 - Polyurethane polymer (generic).
Code of Federal Regulations, 2010 CFR
2010-07-01
... 40 Protection of Environment 30 2010-07-01 2010-07-01 false Polyurethane polymer (generic). 721... Substances § 721.9959 Polyurethane polymer (generic). (a) Chemical substance and significant new uses subject to reporting. (1) The chemical substance identified generically as a polyurethane polymer (PMN P-01...
40 CFR 721.9959 - Polyurethane polymer (generic).
Code of Federal Regulations, 2011 CFR
2011-07-01
... 40 Protection of Environment 31 2011-07-01 2011-07-01 false Polyurethane polymer (generic). 721... Substances § 721.9959 Polyurethane polymer (generic). (a) Chemical substance and significant new uses subject to reporting. (1) The chemical substance identified generically as a polyurethane polymer (PMN P-01...
40 CFR 721.9959 - Polyurethane polymer (generic).
Code of Federal Regulations, 2013 CFR
2013-07-01
... 40 Protection of Environment 32 2013-07-01 2013-07-01 false Polyurethane polymer (generic). 721... Substances § 721.9959 Polyurethane polymer (generic). (a) Chemical substance and significant new uses subject to reporting. (1) The chemical substance identified generically as a polyurethane polymer (PMN P-01...
40 CFR 721.9959 - Polyurethane polymer (generic).
Code of Federal Regulations, 2014 CFR
2014-07-01
... 40 Protection of Environment 31 2014-07-01 2014-07-01 false Polyurethane polymer (generic). 721... Substances § 721.9959 Polyurethane polymer (generic). (a) Chemical substance and significant new uses subject to reporting. (1) The chemical substance identified generically as a polyurethane polymer (PMN P-01...
40 CFR 721.9959 - Polyurethane polymer (generic).
Code of Federal Regulations, 2012 CFR
2012-07-01
... 40 Protection of Environment 32 2012-07-01 2012-07-01 false Polyurethane polymer (generic). 721... Substances § 721.9959 Polyurethane polymer (generic). (a) Chemical substance and significant new uses subject to reporting. (1) The chemical substance identified generically as a polyurethane polymer (PMN P-01...
40 CFR 721.8095 - Silylated polyurethane.
Code of Federal Regulations, 2010 CFR
2010-07-01
... 40 Protection of Environment 30 2010-07-01 2010-07-01 false Silylated polyurethane. 721.8095... Substances § 721.8095 Silylated polyurethane. (a) Chemical substance and significant new uses subject to reporting. (1) The chemical substance identified generically as a silylated polyurethane (PMN P-95-1356) is...
40 CFR 63.1293 - Standards for slabstock flexible polyurethane foam production.
Code of Federal Regulations, 2014 CFR
2014-07-01
... polyurethane foam production. 63.1293 Section 63.1293 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY... CATEGORIES (CONTINUED) National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1293 Standards for slabstock flexible polyurethane foam production. Each owner or...
40 CFR 63.1293 - Standards for slabstock flexible polyurethane foam production.
Code of Federal Regulations, 2013 CFR
2013-07-01
... polyurethane foam production. 63.1293 Section 63.1293 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY... CATEGORIES (CONTINUED) National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1293 Standards for slabstock flexible polyurethane foam production. Each owner or...
40 CFR 63.8782 - Am I subject to this subpart?
Code of Federal Regulations, 2011 CFR
2011-07-01
...) National Emission Standards for Hazardous Air Pollutants: Flexible Polyurethane Foam Fabrication Operations... you own or operate a flexible polyurethane foam fabrication plant site that operates a flame... flexible polyurethane foam fabrication plant site is a plant site where pieces of flexible polyurethane...
40 CFR 63.8782 - Am I subject to this subpart?
Code of Federal Regulations, 2014 CFR
2014-07-01
...) National Emission Standards for Hazardous Air Pollutants: Flexible Polyurethane Foam Fabrication Operations... you own or operate a flexible polyurethane foam fabrication plant site that operates a flame... flexible polyurethane foam fabrication plant site is a plant site where pieces of flexible polyurethane...
40 CFR 63.8782 - Am I subject to this subpart?
Code of Federal Regulations, 2013 CFR
2013-07-01
...) National Emission Standards for Hazardous Air Pollutants: Flexible Polyurethane Foam Fabrication Operations... you own or operate a flexible polyurethane foam fabrication plant site that operates a flame... flexible polyurethane foam fabrication plant site is a plant site where pieces of flexible polyurethane...
Code of Federal Regulations, 2014 CFR
2014-07-01
... polyurethane foam production-diisocyanate emissions. 63.1294 Section 63.1294 Protection of Environment... Pollutants for Flexible Polyurethane Foam Production § 63.1294 Standards for slabstock flexible polyurethane foam production—diisocyanate emissions. Each new and existing slabstock affected source shall comply...
40 CFR 63.8782 - Am I subject to this subpart?
Code of Federal Regulations, 2010 CFR
2010-07-01
...) National Emission Standards for Hazardous Air Pollutants: Flexible Polyurethane Foam Fabrication Operations... you own or operate a flexible polyurethane foam fabrication plant site that operates a flame... flexible polyurethane foam fabrication plant site is a plant site where pieces of flexible polyurethane...
Code of Federal Regulations, 2013 CFR
2013-07-01
... polyurethane foam production-diisocyanate emissions. 63.1294 Section 63.1294 Protection of Environment... Pollutants for Flexible Polyurethane Foam Production § 63.1294 Standards for slabstock flexible polyurethane foam production—diisocyanate emissions. Each new and existing slabstock affected source shall comply...
40 CFR 63.8782 - Am I subject to this subpart?
Code of Federal Regulations, 2012 CFR
2012-07-01
...) National Emission Standards for Hazardous Air Pollutants: Flexible Polyurethane Foam Fabrication Operations... you own or operate a flexible polyurethane foam fabrication plant site that operates a flame... flexible polyurethane foam fabrication plant site is a plant site where pieces of flexible polyurethane...
Hong, Suk-Min; Kim, Jong-Wan; Knowles, Jonathan C; Gong, Myoung-Seon
2017-02-01
In this study, polycarbonate diol/isosorbide-based antibacterial polyurethane nanofiber fabrics containing Ag nanoparticles were prepared by electrospinning process. Bio-based highly elastic polyurethane was prepared from hexamethylene diisocyanate and isosorbide/polycarbonate diol (8/2) by a simple one-shot bulk polymerization. Ag nanoparticles were formed using simple thermal reduction of silver 2-ethylhexylcarbamate at 120℃. The structural and morphological properties of polyurethane/Ag nanofibers were characterized by X-ray diffraction and scanning electron microscopy. The polyurethane nanofiber fabrics were flexible, with breaking strains from 355% to 950% under 7.28 to 23.1 MPa tensile stress. The antibacterial effects of the treated polyurethane/Ag fabrics against Staphylococcus aureus and methicillin resistant Staphylococcus aureus were examined and found to be excellent. Cell proliferation using the immortalized human keratinocyte HaCaT cell line was performed in order to determine cell viability in the presence of polyurethane and polyurethane/Ag fabrics, showing cytocompatiblility and a lack of toxicity.
Polyurethane membranes for surgical gown applications
NASA Astrophysics Data System (ADS)
Ukpabi, Pauline Ozoemena
The Occupational Safety and Health Administration (OSHA) recently issued a directive requiring all employers to supply personnel protective equipment to employees who are at risk of exposure to blood or other potentially infectious body fluids. For the healthcare worker, a wide variety of surgical gowns is available commercially but there are concerns over their barrier effectiveness and/or wearer comfort. To successfully create a barrier fabric which combines resistance to fluid penetration with comfort, a complete understanding of the relationship between membrane structure and functional properties is required. In this study, we investigated the surface properties of hydrophilicity and hydrophobicity in polyurethane membranes intended for use in surgical gowns. The polyurethane membranes were grafted with side chains of varying lengths, polyethylene glycol (PEG) being used for the hydrophilic modifications and perfluoroalkyl compounds (a monofunctional acid and a difunctional amino alcohol) for the hydrophobic modifications. The hydrophilic treatment was intended to improve the comfort properties of monolithic membranes without adversely affecting their barrier properties. The hydrophobic treatment, on the other hand, was intended to improve the fluid repellency and hence barrier properties of microporous membranes without adversely affecting their comfort properties. Reflection infrared spectroscopy showed that fluorine was successfully grafted onto the polyurethane backbone during the hydrophobic modification, but was not sensitive enough to detect PEG grafting in leached polyethylene glycol-treated polyurethanes. X-ray photoelectron spectroscopy showed that the perfluoroalkylated polyurethanes contained up to 40% fluorine on their surfaces and the PEG-treated polyurethanes showed an increase in their C-O content over the unmodified polyurethane. Scanning electron microscopy not only showed that perfluoroalkylation yielded polyurethane membranes with very rough surfaces compared to the unmodified membrane, it also showed varying degrees of surface roughness on the perfluoroalkylated polyurethanes depending on whether the monofunctional acid or the difunctional amino alcohol was used as modifier. The PEG-treated samples exhibited smooth surfaces under the SEM. Perfluoroalkylation yielded samples with slightly higher contact angles than the untreated polyurethane while the PEG treatment resulted in polyurethanes with lower contact angles than the untreated polyurethane. The perfluoroalkylated materials were more thermally stable than the unmodified polyurethanes.
40 CFR 721.8090 - Polyurethane polymer.
Code of Federal Regulations, 2010 CFR
2010-07-01
... 40 Protection of Environment 30 2010-07-01 2010-07-01 false Polyurethane polymer. 721.8090 Section... Substances § 721.8090 Polyurethane polymer. (a) Chemical substance and significant new uses subject to reporting. (1) The chemical substance identified generically as a polyurethane polymer (P-94-47) is subject...
40 CFR 721.8090 - Polyurethane polymer.
Code of Federal Regulations, 2011 CFR
2011-07-01
... 40 Protection of Environment 31 2011-07-01 2011-07-01 false Polyurethane polymer. 721.8090 Section... Substances § 721.8090 Polyurethane polymer. (a) Chemical substance and significant new uses subject to reporting. (1) The chemical substance identified generically as a polyurethane polymer (P-94-47) is subject...
40 CFR 721.8090 - Polyurethane polymer.
Code of Federal Regulations, 2012 CFR
2012-07-01
... 40 Protection of Environment 32 2012-07-01 2012-07-01 false Polyurethane polymer. 721.8090 Section... Substances § 721.8090 Polyurethane polymer. (a) Chemical substance and significant new uses subject to reporting. (1) The chemical substance identified generically as a polyurethane polymer (P-94-47) is subject...
40 CFR 721.8090 - Polyurethane polymer.
Code of Federal Regulations, 2013 CFR
2013-07-01
... 40 Protection of Environment 32 2013-07-01 2013-07-01 false Polyurethane polymer. 721.8090 Section... Substances § 721.8090 Polyurethane polymer. (a) Chemical substance and significant new uses subject to reporting. (1) The chemical substance identified generically as a polyurethane polymer (P-94-47) is subject...
40 CFR 721.8090 - Polyurethane polymer.
Code of Federal Regulations, 2014 CFR
2014-07-01
... 40 Protection of Environment 31 2014-07-01 2014-07-01 false Polyurethane polymer. 721.8090 Section... Substances § 721.8090 Polyurethane polymer. (a) Chemical substance and significant new uses subject to reporting. (1) The chemical substance identified generically as a polyurethane polymer (P-94-47) is subject...
Code of Federal Regulations, 2010 CFR
2010-07-01
... 40 Protection of Environment 11 2010-07-01 2010-07-01 true Standards for slabstock flexible polyurethane foam production-diisocyanate emissions. 63.1294 Section 63.1294 Protection of Environment... Flexible Polyurethane Foam Production § 63.1294 Standards for slabstock flexible polyurethane foam...
40 CFR 63.1300 - Standards for molded flexible polyurethane foam production.
Code of Federal Regulations, 2010 CFR
2010-07-01
... polyurethane foam production. 63.1300 Section 63.1300 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY... CATEGORIES National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1300 Standards for molded flexible polyurethane foam production. Each owner or operator of a new...
Code of Federal Regulations, 2012 CFR
2012-07-01
... 40 Protection of Environment 12 2012-07-01 2011-07-01 true Standards for slabstock flexible polyurethane foam production-diisocyanate emissions. 63.1294 Section 63.1294 Protection of Environment... Flexible Polyurethane Foam Production § 63.1294 Standards for slabstock flexible polyurethane foam...
40 CFR 63.1300 - Standards for molded flexible polyurethane foam production.
Code of Federal Regulations, 2011 CFR
2011-07-01
... polyurethane foam production. 63.1300 Section 63.1300 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY... CATEGORIES National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1300 Standards for molded flexible polyurethane foam production. Each owner or operator of a new...
40 CFR 63.1293 - Standards for slabstock flexible polyurethane foam production.
Code of Federal Regulations, 2010 CFR
2010-07-01
... polyurethane foam production. 63.1293 Section 63.1293 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY... CATEGORIES National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1293 Standards for slabstock flexible polyurethane foam production. Each owner or operator of a...
Code of Federal Regulations, 2011 CFR
2011-07-01
... 40 Protection of Environment 11 2011-07-01 2011-07-01 false Standards for slabstock flexible polyurethane foam production-diisocyanate emissions. 63.1294 Section 63.1294 Protection of Environment... Flexible Polyurethane Foam Production § 63.1294 Standards for slabstock flexible polyurethane foam...
40 CFR 63.1293 - Standards for slabstock flexible polyurethane foam production.
Code of Federal Regulations, 2012 CFR
2012-07-01
... polyurethane foam production. 63.1293 Section 63.1293 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY... CATEGORIES National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1293 Standards for slabstock flexible polyurethane foam production. Each owner or operator of a...
40 CFR 63.1300 - Standards for molded flexible polyurethane foam production.
Code of Federal Regulations, 2012 CFR
2012-07-01
... polyurethane foam production. 63.1300 Section 63.1300 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY... CATEGORIES National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1300 Standards for molded flexible polyurethane foam production. Each owner or operator of a new...
40 CFR 63.1293 - Standards for slabstock flexible polyurethane foam production.
Code of Federal Regulations, 2011 CFR
2011-07-01
... polyurethane foam production. 63.1293 Section 63.1293 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY... CATEGORIES National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1293 Standards for slabstock flexible polyurethane foam production. Each owner or operator of a...
Polyurethane-Coated Breast Implants Revisited: A 30-Year Follow-Up
Castel, Nikki; Soon-Sutton, Taylor; Deptula, Peter; Flaherty, Anna
2015-01-01
Background Polyurethane coating of breast implants has been shown to reduce capsular contracture in short-term follow-up studies. This 30-year study is the longest examination of the use of polyurethane-coated implants and their correlation with capsular contracture. Methods This study evaluates the senior surgeon's (F.D.P.) experience with the use of polyurethane-coated implants in aesthetic breast augmentation in 382 patients over 30 years. Follow-up evaluations were conducted for six months after surgery. After the six-month follow-up period, 76 patients returned for reoperation. The gross findings, histology, and associated capsular contracture were noted at the time of explantation. Results No patient during the six-month follow-up period demonstrated capsular contracture. For those who underwent reoperation for capsular contracture, Baker II/III contractures were noted nine to 10 years after surgery and Baker IV contractures were noted 12 to 21 years after surgery. None of the explanted implants had macroscopic evidence of polyurethane, which was only found during the first five years after surgery. The microscopic presence of polyurethane was noted in all capsules up to 30 years after the original operation. Conclusions An inverse correlation was found between the amount of polyurethane coating on the implant and the occurrence of capsular contracture. Increasingly severe capsular contracture was associated with a decreased amount of polyurethane coating on the surface of the implants. No contracture occurred in patients whose implants showed incomplete biodegradation of polyurethane, as indicated by the visible presence of polyurethane coating. We recommend research to find a non-toxic, non-biodegradable synthetic material as an alternative to polyurethane. PMID:25798390
Code of Federal Regulations, 2011 CFR
2011-07-01
... polyurethane foam production-HAP ABA equipment leaks. 63.1296 Section 63.1296 Protection of Environment... Flexible Polyurethane Foam Production § 63.1296 Standards for slabstock flexible polyurethane foam... emissions from leaks from transfer pumps, valves, connectors, pressure-relief valves, and open-ended lines...
Code of Federal Regulations, 2012 CFR
2012-07-01
... polyurethane foam production-HAP ABA equipment leaks. 63.1296 Section 63.1296 Protection of Environment... Flexible Polyurethane Foam Production § 63.1296 Standards for slabstock flexible polyurethane foam... emissions from leaks from transfer pumps, valves, connectors, pressure-relief valves, and open-ended lines...
Code of Federal Regulations, 2010 CFR
2010-07-01
... polyurethane foam production-HAP ABA equipment leaks. 63.1296 Section 63.1296 Protection of Environment... Flexible Polyurethane Foam Production § 63.1296 Standards for slabstock flexible polyurethane foam... emissions from leaks from transfer pumps, valves, connectors, pressure-relief valves, and open-ended lines...
40 CFR 721.8079 - Isophorone diisocyanate neopentyl glycol adipate polyurethane prepolymer.
Code of Federal Regulations, 2010 CFR
2010-07-01
... glycol adipate polyurethane prepolymer. 721.8079 Section 721.8079 Protection of Environment ENVIRONMENTAL... adipate polyurethane prepolymer. (a) Chemical substance and significant new uses subject to reporting. (1... polyurethane prepolymer (PMN P-94-1743) is subject to reporting under this section for the significant new uses...
Code of Federal Regulations, 2010 CFR
2010-07-01
... 40 Protection of Environment 11 2010-07-01 2010-07-01 true Standards for slabstock flexible polyurethane foam production-HAP ABA storage vessels. 63.1295 Section 63.1295 Protection of Environment... Flexible Polyurethane Foam Production § 63.1295 Standards for slabstock flexible polyurethane foam...
40 CFR 63.1300 - Standards for molded flexible polyurethane foam production.
Code of Federal Regulations, 2013 CFR
2013-07-01
... polyurethane foam production. 63.1300 Section 63.1300 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY... Foam Production § 63.1300 Standards for molded flexible polyurethane foam production. Each owner or... polyurethane foam process, with the following exception. Diisocyanates may be used to flush the mixhead and...
Code of Federal Regulations, 2011 CFR
2011-07-01
... 40 Protection of Environment 11 2011-07-01 2011-07-01 false Standards for slabstock flexible polyurethane foam production-HAP ABA storage vessels. 63.1295 Section 63.1295 Protection of Environment... Flexible Polyurethane Foam Production § 63.1295 Standards for slabstock flexible polyurethane foam...
Code of Federal Regulations, 2012 CFR
2012-07-01
... 40 Protection of Environment 12 2012-07-01 2011-07-01 true Standards for slabstock flexible polyurethane foam production-HAP ABA storage vessels. 63.1295 Section 63.1295 Protection of Environment... Flexible Polyurethane Foam Production § 63.1295 Standards for slabstock flexible polyurethane foam...
40 CFR 63.1300 - Standards for molded flexible polyurethane foam production.
Code of Federal Regulations, 2014 CFR
2014-07-01
... polyurethane foam production. 63.1300 Section 63.1300 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY... Foam Production § 63.1300 Standards for molded flexible polyurethane foam production. Each owner or... polyurethane foam process, with the following exception. Diisocyanates may be used to flush the mixhead and...
Aoki, Daisuke; Ajiro, Hiroharu
2018-06-13
In order to prepare thermoresponsive polyurethane gels, a novel polyurethane bearing oligo(ethylene glycol) (OEG) as the side chain is successfully synthesized with hexamethylene diisocyanate and OEG tartrate ester. The aqueous solution of the polyurethane shows sharp and clear lower critical solution temperature behavior at 34 °C. Furthermore, a hydrogel based on the same polyurethane is also successfully prepared using glycerol as the crosslinker. This polyurethane hydrogel including 10 mol% of glycerol presents a large swelling ratio change between 4 °C and 37 °C from 250% to 40%. © 2018 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.
Malanchuk, V O; Astapenko, O O; Halatenko, N A; Rozhnova, R A
2013-09-01
Dates about the research of biodegradation of epoxy-polyurethane composite material used in reconstructive and reparative surgery of maxillofacial area are reflected in the article. Was founded: 1) notable biodegradation of species from epoxy-polyurethane composition in the term of observation up to 6 months was not founded. That testifies their preservation of physical and mechanical properties. 2) founded, that in species from epoxy-polyurethane composition, which contain levamisole, processes of biodegradation are faster then in species from pure epoxy-polyurethane composition and in species from epoxy-polyurethane composition with hydroxyapatite; 3) material from epoxy-polyurethane composition, which contains levamisole and hydroxyapatite, stays in biological environment in small quantity of petty fragments during the incubation in term of 2 years. So, it biodegrades practically totally. Authors suggest on the basis of achieved information, that the use of epoxy-polyurethane constructions that biodegrade, is pertinently in reconstructive maxillofacial surgery.
Code of Federal Regulations, 2013 CFR
2013-07-01
... polyurethane foam production-HAP ABA equipment leaks. 63.1296 Section 63.1296 Protection of Environment... Pollutants for Flexible Polyurethane Foam Production § 63.1296 Standards for slabstock flexible polyurethane foam production—HAP ABA equipment leaks. Each owner or operator of a new or existing slabstock affected...
Code of Federal Regulations, 2014 CFR
2014-07-01
... polyurethane foam production-HAP ABA equipment leaks. 63.1296 Section 63.1296 Protection of Environment... Pollutants for Flexible Polyurethane Foam Production § 63.1296 Standards for slabstock flexible polyurethane foam production—HAP ABA equipment leaks. Each owner or operator of a new or existing slabstock affected...
Code of Federal Regulations, 2014 CFR
2014-07-01
... polyurethane foam production-HAP emissions from equipment cleaning. 63.1298 Section 63.1298 Protection of... Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1298 Standards for slabstock flexible polyurethane foam production—HAP emissions from equipment cleaning. Each owner or operator of a...
Code of Federal Regulations, 2010 CFR
2010-07-01
... polyurethane foam production-HAP emissions from equipment cleaning. 63.1298 Section 63.1298 Protection of... Pollutants for Flexible Polyurethane Foam Production § 63.1298 Standards for slabstock flexible polyurethane foam production—HAP emissions from equipment cleaning. Each owner or operator of a new or existing...
Code of Federal Regulations, 2013 CFR
2013-07-01
... polyurethane foam production-HAP emissions from equipment cleaning. 63.1298 Section 63.1298 Protection of... Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1298 Standards for slabstock flexible polyurethane foam production—HAP emissions from equipment cleaning. Each owner or operator of a...
Code of Federal Regulations, 2014 CFR
2014-07-01
... polyurethane foam production-HAP ABA storage vessels. 63.1295 Section 63.1295 Protection of Environment... Pollutants for Flexible Polyurethane Foam Production § 63.1295 Standards for slabstock flexible polyurethane foam production—HAP ABA storage vessels. Each owner or operator of a new or existing slabstock affected...
Code of Federal Regulations, 2013 CFR
2013-07-01
... polyurethane foam production-HAP ABA emissions from the production line. 63.1297 Section 63.1297 Protection of... Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1297 Standards for slabstock flexible polyurethane foam production—HAP ABA emissions from the production line. (a) Each owner or...
Code of Federal Regulations, 2010 CFR
2010-07-01
... polyurethane foam production-source-wide emission limitation. 63.1299 Section 63.1299 Protection of Environment... Flexible Polyurethane Foam Production § 63.1299 Standards for slabstock flexible polyurethane foam... procedures in paragraphs (c)(1) through (4) of this section, unless a recovery device is used. Slabstock foam...
Code of Federal Regulations, 2012 CFR
2012-07-01
... polyurethane foam production-source-wide emission limitation. 63.1299 Section 63.1299 Protection of Environment... Flexible Polyurethane Foam Production § 63.1299 Standards for slabstock flexible polyurethane foam... procedures in paragraphs (c)(1) through (4) of this section, unless a recovery device is used. Slabstock foam...
Code of Federal Regulations, 2013 CFR
2013-07-01
... polyurethane foam production-HAP ABA storage vessels. 63.1295 Section 63.1295 Protection of Environment... Pollutants for Flexible Polyurethane Foam Production § 63.1295 Standards for slabstock flexible polyurethane foam production—HAP ABA storage vessels. Each owner or operator of a new or existing slabstock affected...
Code of Federal Regulations, 2011 CFR
2011-07-01
... polyurethane foam production-HAP emissions from equipment cleaning. 63.1298 Section 63.1298 Protection of... Pollutants for Flexible Polyurethane Foam Production § 63.1298 Standards for slabstock flexible polyurethane foam production—HAP emissions from equipment cleaning. Each owner or operator of a new or existing...
Code of Federal Regulations, 2014 CFR
2014-07-01
... polyurethane foam production-source-wide emission limitation. 63.1299 Section 63.1299 Protection of Environment... Pollutants for Flexible Polyurethane Foam Production § 63.1299 Standards for slabstock flexible polyurethane foam production—source-wide emission limitation. Each owner or operator of a new or existing slabstock...
Code of Federal Regulations, 2011 CFR
2011-07-01
... polyurethane foam production-source-wide emission limitation. 63.1299 Section 63.1299 Protection of Environment... Flexible Polyurethane Foam Production § 63.1299 Standards for slabstock flexible polyurethane foam... procedures in paragraphs (c)(1) through (4) of this section, unless a recovery device is used. Slabstock foam...
Code of Federal Regulations, 2014 CFR
2014-07-01
... polyurethane foam production-HAP ABA emissions from the production line. 63.1297 Section 63.1297 Protection of... Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1297 Standards for slabstock flexible polyurethane foam production—HAP ABA emissions from the production line. (a) Each owner or...
Code of Federal Regulations, 2013 CFR
2013-07-01
... polyurethane foam production-source-wide emission limitation. 63.1299 Section 63.1299 Protection of Environment... Pollutants for Flexible Polyurethane Foam Production § 63.1299 Standards for slabstock flexible polyurethane foam production—source-wide emission limitation. Each owner or operator of a new or existing slabstock...
Code of Federal Regulations, 2012 CFR
2012-07-01
... polyurethane foam production-HAP emissions from equipment cleaning. 63.1298 Section 63.1298 Protection of... Pollutants for Flexible Polyurethane Foam Production § 63.1298 Standards for slabstock flexible polyurethane foam production—HAP emissions from equipment cleaning. Each owner or operator of a new or existing...
Cui, Zhengshan; He, Wanxia; Liu, Jun; Wei, Wei; Jiang, Liang; Huang, Jun; Lv, Xiaomeng
2016-10-01
Through sol-gel and dip-coating processes, commercial polyurethane sponge modified by polysiloxane was fabricated under low temperature (60 °C) and atmosphere. The contact angle of the obtained polysiloxane/polyurethane sponge is 145 ± 5°. Hence, the polysiloxane/polyurethane sponge could float on water and selectively absorb organics from the surface of the water, indicating simultaneous properties of hydrophobicity and oleophilicity. The absorbent maximum value is 50-150 times of its own weight. The polysiloxane/polyurethane sponge exhibited excellent recyclability, which could be reused by squeezing the sponge due to its high mechanical stability and flexibility. Thermogravimetry-differential thermal analysis test indicated that the polysiloxane/polyurethane sponge exhibited good thermal stability and the stable contact angle of samples tested under increasing temperature indicated its good weather resistance. Due to the commercial property of polyurethane sponge and easy-handling of polysiloxane, the polysiloxane/polyurethane sponge can be easily scaled up to recover a large-area oil spill in water and further work based on the designed equipment has been under consideration.
100% Solids Polyurethane Sequestration Coating
2014-04-11
Distribution Unlimited 100% Solids Polyurethane Sequestration Coating The views, opinions and/or findings contained in this report are those of the...Papers published in non peer-reviewed journals: 100% Solids Polyurethane Sequestration Coating Report Title Report developed under Topic #CBD13-101...Final Technical Report Contract #: W911NF-13-P-0010 Proposal #: 63958CHSB1 Project: 100% Solids Polyurethane Sequestration Coating
Jia, Lin; Prabhakaran, Molamma P; Qin, Xiaohong; Ramakrishna, Seeram
2014-09-01
Fabricating scaffolds that can simulate the architecture and functionality of native extracellular matrix is a huge challenge in vascular tissue engineering. Various kinds of materials are engineered via nano-technological approaches to meet the current challenges in vascular tissue regeneration. During this study, nanofibers from pure polyurethane and hybrid polyurethane/collagen in two different morphologies (random and aligned) and in three different ratios of polyurethane:collagen (75:25; 50:50; 25:75) are fabricated by electrospinning. The fiber diameters of the nanofibrous scaffolds are in the range of 174-453 nm and 145-419 for random and aligned fibers, respectively, where they closely mimic the nanoscale dimensions of native extracellular matrix. The aligned polyurethane/collagen nanofibers expressed anisotropic wettability with mechanical properties which is suitable for regeneration of the artery. After 12 days of human aortic smooth muscle cells culture on different scaffolds, the proliferation of smooth muscle cells on hybrid polyurethane/collagen (3:1) nanofibers was 173% and 212% higher than on pure polyurethane scaffolds for random and aligned scaffolds, respectively. The results of cell morphology and protein staining showed that the aligned polyurethane/collagen (3:1) scaffold promote smooth muscle cells alignment through contact guidance, while the random polyurethane/collagen (3:1) also guided cell orientation most probably due to the inherent biochemical composition. Our studies demonstrate the potential of aligned and random polyurethane/collagen (3:1) as promising substrates for vascular tissue regeneration. © The Author(s) 2014 Reprints and permissions: sagepub.co.uk/journalsPermissions.nav.
Arévalo, Fabian; Uscategui, Yomaira L; Diaz, Luis; Cobo, Martha; Valero, Manuel F
2016-11-01
In the present study, polyurethane materials were obtained from castor oil, polycaprolactone and isophorone diisocyanate by incorporating different concentrations of chitosan (0.5, 1.0 and 2.0% w/w) as an additive to improve the mechanical properties and the biological activity of polyurethanes. The polyurethanes were characterized by Fourier transform infrared spectroscopy, thermogravimetric analysis, scanning electron microscopy, stress/strain fracture tests and swelling analysis, and the hydrophilic character of the surface was determined by contact angle trials. The objectives of the study were to evaluate the effect of the incorporation of chitosan on the changes of the physico-chemical and mechanical properties and the in vitro biological activity of the polyurethanes. It was found that the incorporation of chitosan enhances the ultimate tensile strength of the polyurethanes and does not affect the strain at fracture in polyurethanes with 5% w/w of polycaprolactone and concentrations of chitosan ranging from 0 to 2% w/w. In addition, PCL5-Q-PU formulations and their degradation products did not affect cell viability of L929 mouse fibroblast and 3T3, respectively. Polyurethane formulations showed antibacterial activities against Staphylococcus aureus and Escherichia coli bacteria. The results of this study have highlighted the potential biomedical application of this polyurethanes related to soft and cardiovascular tissues. © The Author(s) 2016.
Durability of one-part polyurethane bonds to wood improved by HMR coupling agent
Charles B. Vick; E. Arnold Okkonen
2000-01-01
In a previous study on the strength and durability of a new class of wood adhesives called one-part polyurethanes, four commercial one-part polyurethanes, along with a resorcinol-formaldehyde adhesive representing a standard of performance, were compared in bonds to yellow birch and Douglas-fir in a series of industry-accepted tests (7). The polyurethanes all performed...
Marine biofouling resistance of polyurethane with biodegradation and hydrolyzation.
Xu, Wentao; Ma, Chunfeng; Ma, Jielin; Gan, Tiansheng; Zhang, Guangzhao
2014-03-26
We have prepared polyurethane with poly(ε-caprolactone) (PCL) as the segments of the main chain and poly(triisopropylsilyl acrylate) (PTIPSA) as the side chains by a combination of radical polymerization and a condensation reaction. Quartz crystal microbalance with dissipation studies show that polyurethane can degrade in the presence of enzyme and the degradation rate decreases with the PTIPSA content. Our studies also demonstrate that polyurethane is able to hydrolyze in artificial seawater and the hydrolysis rate increases as the PTIPSA content increases. Moreover, hydrolysis leads to a hydrophilic surface that is favorable to reduction of the frictional drag under dynamic conditions. Marine field tests reveal that polyurethane has good antifouling ability because polyurethane with a biodegradable PCL main chain and hydrolyzable PTIPSA side chains can form a self-renewal surface. Polyurethane was also used to carry and release a relatively environmentally friendly antifoulant, and the combined system exhibits a much higher antifouling performance even in a static marine environment.
Dawlee, S; Jayabalan, M
2015-05-01
Radiopaque polyurethanes are used for medical applications as it allows post-operative assessment of the biomaterial devices using X-ray. Inherently, radiopaque polyurethanes based on polytetramethylene glycol (PTMG), polypropylene glycol, 4,4'-methylenebis(phenyl isocyanate), and a new iodinated chain extender 4,4'-isopropylidenebis[2-(2,6-diiodophenoxy)ethanol] with flexible spacers were synthesized and characterized. The iodinated polyurethanes were clear, optically transparent, and had high molecular weights. The polyurethanes also possessed excellent radiopacity and high thermal stability. The biocompatibility of the most promising iodinated polyurethane was evaluated both in vitro (cytotoxicity evaluation by direct contact and MTT assay, using L929 mouse fibroblast cells) and in vivo (toxicology studies in rabbits and subcutaneous implantation in rats). The material was nontoxic and well tolerated by the animals. Thus, these radiopaque and transparent polyurethanes are expected to have potential for various biomedical applications. © The Author(s) 2014 Reprints and permissions: sagepub.co.uk/journalsPermissions.nav.
Chen, Yuan; Wang, Li; Ma, Fang; Yang, Ji-xian; Qiu, Shan
2014-01-01
The process of simultaneous nitrification and denitrification (SND) of immobilized microorganisms in polyurethane form is discussed. The effect of different positions within the polyurethane carrier on microbial community response for the SND process is investigated by a combination of denaturing gradient gel electrophoresis profiles of the 16S rRNA gene V3 region and scanning electron microscopy. Results show that polyurethane, which consists of a unique porous structure, is an ideal platform for biofilm stratification of aerobe, anaerobe and facultative microorganisms in regard to the SND process. The community structure diversity response to different positions was distinct. The distributions of various functional microbes, detected from the surface aerobic stratification to the interior anaerobic stratification of polyurethane, were mainly nitrifying and denitrifying bacteria. Meanwhile aerobic denitrifying bacteria such as Paracoccus sp., Agrobacterium rubi and Ochrobactrum sp. were also adhered to the interior and surface of polyurethane. The SND process occurring on polyurethane foam was carried out by two independent processes: nitrogen removal and aerobic denitrification.
Hydrophilic polyurethane matrix promotes chondrogenesis of mesenchymal stem cells☆
Nalluri, Sandeep M.; Krishnan, G. Rajesh; Cheah, Calvin; Arzumand, Ayesha; Yuan, Yuan; Richardson, Caley A.; Yang, Shuying; Sarkar, Debanjan
2016-01-01
Segmental polyurethanes exhibit biphasic morphology and can control cell fate by providing distinct matrix guided signals to increase the chondrogenic potential of mesenchymal stem cells (MSCs). Polyethylene glycol (PEG) based hydrophilic polyurethanes can deliver differential signals to MSCs through their matrix phases where hard segments are cell-interactive domains and PEG based soft segments are minimally interactive with cells. These coordinated communications can modulate cell–matrix interactions to control cell shape and size for chondrogenesis. Biphasic character and hydrophilicity of polyurethanes with gel like architecture provide a synthetic matrix conducive for chondrogenesis of MSCs, as evidenced by deposition of cartilage-associated extracellular matrix. Compared to monophasic hydrogels, presence of cell interactive domains in hydrophilic polyurethanes gels can balance cell–cell and cell–matrix interactions. These results demonstrate the correlation between lineage commitment and the changes in cell shape, cell–matrix interaction, and cell–cell adhesion during chondrogenic differentiation which is regulated by polyurethane phase morphology, and thus, represent hydrophilic polyurethanes as promising synthetic matrices for cartilage regeneration. PMID:26046282
The In Vivo Pericapsular Tissue Response to Modern Polyurethane Breast Implants.
Frame, James; Kamel, Dia; Olivan, Marcelo; Cintra, Henrique
2015-10-01
Polyurethane breast implants were first introduced by Ashley (Plast Reconstr Surg 45:421-424, 1970), with the intention of trying to reduce the high incidence of capsular contracture associated with smooth shelled, high gel bleed, silicone breast implants. The sterilization of the polyurethane foam in the early days was questionable. More recently, ethylene oxide (ETO)-sterilized polyurethane has been used in the manufacturing process and this has been shown to reduce the incidence of biofilm. The improved method of attachment of polyurethane onto the underlying high cohesive gel, barrier shell layered, silicone breast implants also encourages bio-integration. Polyurethane covered, cohesive gel, silicone implants have also been shown to reduce the incidence of other problems commonly associated with smooth or textured silicone implants, especially with reference to displacement, capsular contracture, seroma, reoperation, biofilm and implant rupture. Since the introduction of the conical polyurethane implant (Silimed, Brazil) into the United Kingdom in 2009 (Eurosurgical, UK), we have had the opportunity to review histology taken from the capsules of polyurethane implants in three women ranging from a few months to over 3 years after implantation. All implants had been inserted into virgin subfascial, extra-pectoral planes. The results add to the important previously described histological findings of Bassetto et al. (Aesthet Plast Surg 34:481-485, 2010). Five distinct layers are identified and reasons for the development of each layer are discussed. Breast capsule around polyurethane implants, in situ for fifteen and 20 years, has recently been obtained and analysed in Brazil, and the histology has been incorporated into this study. After 20 years, the polyurethane is almost undetectable and capsular contracture may appear. These findings contribute to our understanding of polyurethane implant safety, and give reasoning for a significant reduction in clinical capsular contracture rate, up to 10 years after implantation, compared to contemporary silicone implants. A more permanent matrix equivalent to polyurethane may be the solution for reducing long-term capsular contracture. This journal requires that authors assign a level of evidence to each article. For a full description of these Evidence-Based Medicine ratings, please refer to the Table of Contents or the online Instructions to Authors www.springer.com/00266 .
Wagenführ-Júnior, Jorge; Ribas Filho, Jurandir Marcondes; Nascimento, Marcelo Mazza do; Ribas, Fernanda Marcondes; Wanka, Marcus Vinícius; Godoi, Andressa de Lima
2012-12-01
To evaluate whether polyurethane foam leads more intense foreign-body reaction than silicone foam. To compare the vascularization of the capsules surrounding the foam implants. To investigate if the capsule of polyurethane foam implanted has greater amount of collagen than that of silicone foam. Sixty-four young male Wistar rats were allocated into two groups: polyurethane foam and silicone foam. Subcutaneous discs were implanted into the dorsum of the animals in both groups. The capsules were assessed 28 days, two months, three months and six months postoperatively. Microscopic analysis with H&E stain was performed to evaluate the acute and chronic inflammatory process, foreign-body reaction and neovascularization. The analysis with picrosirius red was performed using the ImageProPlus software, to measure the number of vessels and collagen types I and III. There were no statistical differences between the two groups regarding the acute and chronic inflammatory processes. All rats from the polyurethane group, in all times, exhibited moderate or intense foreign-body reaction, with statistic significant difference (p=0.046) when compared with the silicone group, in which the reaction was either mild or nonexistent at two months. Vascular proliferation was significantly different between the groups at 28 days (p=0.0002), with the polyurethane group displaying greater neovascularization with H&E stain. Similar results were obtained with picrosirius red, which revealed in the polyurethane group a much greater number of vessels than in the silicone group (p=0.001). The collagen area was larger in the polyurethane group, significantly at 28 days (p=0.001) and at two months (p=0.030). Polyurethane foam elicited more intense foreign-body reaction when compared with silicone foam. The number of vessels was higher in the capsules of the polyurethane foam implants 28 days after the operation. The capsule of the polyurethane foam implants showed a greater amount of collagen than that of the silicone foam implants.
Comparison of polyurethane with cyanoacrylate in hemostasis of vascular injury in guinea pigs.
Kubrusly, Luiz Fernando; Formighieri, Marina Simões; Lago, José Vitor Martins; Graça, Yorgos Luiz Santos de Salles; Sobral, Ana Cristina Lira; Lago, Marianna Martins
2015-01-01
To evaluate the behavior of castor oil-derived polyurethane as a hemostatic agent and tissue response after abdominal aortic injury and to compare it with 2-octyl-cyanoacrylate. Twenty-four Guinea Pigs were randomly divided into three groups of eight animals (I, II, and III). The infrarenal abdominal aorta was dissected, clamped proximally and distally to the vascular puncture site. In group I (control), hemostasis was achieved with digital pressure; in group II (polyurethane) castor oil-derived polyurethane was applied, and in group III (cyanoacrylate), 2-octyl-cyanoacrylate was used. Group II was subdivided into IIA and IIB according to the time of preparation of the hemostatic agent. Mean blood loss in groups IIA, IIB and III was 0.002 grams (g), 0.008 g, and 0.170 g, with standard deviation of 0.005 g, 0.005 g, and 0.424 g, respectively (P=0.069). The drying time for cyanoacrylate averaged 81.5 seconds (s) (standard deviation: 51.5 seconds) and 126.1 s (standard deviation: 23.0 s) for polyurethane B (P=0.046). However, there was a trend (P=0.069) for cyanoacrylate to dry more slowly than polyurethane A (mean: 40.5 s; SD: 8.6 s). Furthermore, polyurethane A had a shorter drying time than polyurethane B (P=0.003), mean IIA of 40.5 s (standard deviation: 8.6 s). In group III, 100% of the animals had mild/severe fibrosis, while in group II only 12.5% showed this degree of fibrosis (P=0.001). Polyurethane derived from castor oil showed similar hemostatic behavior to octyl-2-cyanoacrylate. There was less perivascular tissue response with polyurethane when compared with cyanoacrylate.
Comparison of polyurethane with cyanoacrylate in hemostasis of vascular injury in guinea pigs
Kubrusly, Luiz Fernando; Formighieri, Marina Simões; Lago, José Vitor Martins; Graça, Yorgos Luiz Santos de Salles; Sobral, Ana Cristina Lira; Lago, Marianna Martins
2015-01-01
Objective To evaluate the behavior of castor oil-derived polyurethane as a hemostatic agent and tissue response after abdominal aortic injury and to compare it with 2-octyl-cyanoacrylate. Methods Twenty-four Guinea Pigs were randomly divided into three groups of eight animals (I, II, and III). The infrarenal abdominal aorta was dissected, clamped proximally and distally to the vascular puncture site. In group I (control), hemostasis was achieved with digital pressure; in group II (polyurethane) castor oil-derived polyurethane was applied, and in group III (cyanoacrylate), 2-octyl-cyanoacrylate was used. Group II was subdivided into IIA and IIB according to the time of preparation of the hemostatic agent. Results Mean blood loss in groups IIA, IIB and III was 0.002 grams (g), 0.008 g, and 0.170 g, with standard deviation of 0.005 g, 0.005 g, and 0.424 g, respectively (P=0.069). The drying time for cyanoacrylate averaged 81.5 seconds (s) (standard deviation: 51.5 seconds) and 126.1 s (standard deviation: 23.0 s) for polyurethane B (P=0.046). However, there was a trend (P=0.069) for cyanoacrylate to dry more slowly than polyurethane A (mean: 40.5 s; SD: 8.6 s). Furthermore, polyurethane A had a shorter drying time than polyurethane B (P=0.003), mean IIA of 40.5 s (standard deviation: 8.6 s). In group III, 100% of the animals had mild/severe fibrosis, while in group II only 12.5% showed this degree of fibrosis (P=0.001). Conclusion Polyurethane derived from castor oil showed similar hemostatic behavior to octyl-2-cyanoacrylate. There was less perivascular tissue response with polyurethane when compared with cyanoacrylate. PMID:25859876
Impact of Medium and Substrate on Growth of Pseudomonas Fluorescens Biofilms on Polyurethane Paint
2011-02-01
biofilm formation on polyurethane (PU) coatings, and to define how those parameters contribute to polyurethane biodegradation. We used a batch flow system...determine which factors best support the growth and persistence of Pseudomonas fluorescens biofilms . Factors that enhance biofilm formation and...AFRL-RX-WP-TP-2011-4131 IMPACT OF MEDIUM AND SUBSTRATE ON GROWTH OF PSEUDOMONAS FLUORESCENS BIOFILMS ON POLYURETHANE PAINT Wendy L. Goodson
Bio-Based Polyurethane Containing Isosorbide for Use in Composites and Coatings
2015-04-01
ARL-TR-7259 ● APR 2015 US Army Research Laboratory Bio-Based Polyurethane Containing Isosorbide for Use in Composites and...copyright notation hereon. ARL-TR-7259 ● APR 2015 US Army Research Laboratory Bio-Based Polyurethane Containing Isosorbide for Use...4. TITLE AND SUBTITLE Bio-Based Polyurethane Containing Isosorbide for Use in Composites and Coatings 5a. CONTRACT NUMBER 5b. GRANT NUMBER 5c
The bactericidal activity of glutaraldehyde-impregnated polyurethane.
Sehmi, Sandeep K; Allan, Elaine; MacRobert, Alexander J; Parkin, Ivan
2016-10-01
Although glutaraldehyde is known to be bactericidal in solution, its potential use to create novel antibacterial polymers suitable for use in healthcare environments has not been evaluated. Here, novel materials were prepared in which glutaraldehyde was either incorporated into polyurethane using a simple "swell-encapsulation-shrink" method (hereafter referred to as "glutaraldehyde-impregnated polyurethane"), or simply applied to the polymer surface (hereafter referred to as "glutaraldehyde-coated polyurethane"). The antibacterial activity of glutaraldehyde-impregnated and glutaraldehyde-coated polyurethane samples was tested against Escherichia coli and Staphylococcus aureus. Glutaraldehyde-impregnated polyurethane resulted in a 99.9% reduction in the numbers of E. coli within 2 h and a similar reduction of S. aureus within 1 h, whereas only a minimal reduction in bacterial numbers was observed when the biocide was bound to the polymer surface. After 15 days, however, the bactericidal activity of the impregnated material was substantially reduced presumably due to polymerization of glutaraldehyde. Thus, although glutaraldehyde retains antibacterial activity when impregnated into polyurethane, activity is not maintained for extended periods of time. Future work should examine the potential of chemical modification of glutaraldehyde and/or polyurethane to improve the useful lifespan of this novel antibacterial polymer. © 2016 The Authors. MicrobiologyOpen published by John Wiley & Sons Ltd.
NASA Astrophysics Data System (ADS)
Triwulandari, Evi; Ramadhan, Mohammad Kemilau; Ghozali, Muhammad
2017-01-01
Polyurethane modified epoxy based on glycerol monooleate (PME-GMO) was synthesized. GMO as polyol for synthesis of PME-GMO was synthesized via Fisher Esterification between oleic acid from palm oil and glycerol by using sulfuric acid as catalyst with time variation i.e. 3, 4, 5 and 6 hours at 160°C. Characterizations of GMO were carried out by analysis of acid number, hydroxyl value and FTIR. The data show that the conversion of oleic acid to ester compound is directly proportional with the increasing of reaction time but the enhancement is not significant after 3 hours. Furthermore, GMO product was used as polyol for modification of epoxy with polyurethane. Modification of epoxy with polyurethane was performed by reacted epoxy, tolonate and GMO simultaneously in one step. In this research, the reaction condition was varied i.e. time reaction (0.5; 1; 1.5; 2; 2.5 hours), composition of polyurethane used (10%, 20% toward epoxy) and rasio of tolonate and GMO (NCO/OH ratio) as component of polyurethane (1.5 and 2.5). Characterization of polyurethane modified epoxy based on glycerol (PME-GMO) was conducted by viscosity and FTIR analysis. The viscosity of PME-GMO increased with increasing of reaction time, polyurethane composition and NCO/OH ratio.
Coneski, Peter N.
2013-01-01
Nitric oxide (NO)-releasing polyurethanes capable of releasing up to 0.20 μmol NO cm−2 were synthesized by incorporating active S-nitrosothiol functionalities into hard and soft segment domains using thiol group protection and post-polymerization modifications, respectively. The nitrosothiol position within the hard and soft segment domains of the polyurethanes impacted both the total NO release and NO release kinetics. The NO storage and release properties were correlated to both chain extender modification and ensuing phase miscibility of the polyurethanes. Thorough material characterization is provided to examine the effects of hard and soft segment modifications on the resultant polyurethane properties. PMID:23418409
Hydrophilic polyurethane matrix promotes chondrogenesis of mesenchymal stem cells.
Nalluri, Sandeep M; Krishnan, G Rajesh; Cheah, Calvin; Arzumand, Ayesha; Yuan, Yuan; Richardson, Caley A; Yang, Shuying; Sarkar, Debanjan
2015-09-01
Segmental polyurethanes exhibit biphasic morphology and can control cell fate by providing distinct matrix guided signals to increase the chondrogenic potential of mesenchymal stem cells (MSCs). Polyethylene glycol (PEG) based hydrophilic polyurethanes can deliver differential signals to MSCs through their matrix phases where hard segments are cell-interactive domains and PEG based soft segments are minimally interactive with cells. These coordinated communications can modulate cell-matrix interactions to control cell shape and size for chondrogenesis. Biphasic character and hydrophilicity of polyurethanes with gel like architecture provide a synthetic matrix conducive for chondrogenesis of MSCs, as evidenced by deposition of cartilage-associated extracellular matrix. Compared to monophasic hydrogels, presence of cell interactive domains in hydrophilic polyurethanes gels can balance cell-cell and cell-matrix interactions. These results demonstrate the correlation between lineage commitment and the changes in cell shape, cell-matrix interaction, and cell-cell adhesion during chondrogenic differentiation which is regulated by polyurethane phase morphology, and thus, represent hydrophilic polyurethanes as promising synthetic matrices for cartilage regeneration. Copyright © 2015 Elsevier B.V. All rights reserved.
Ganji, Yasaman; Kasra, Mehran; Salahshour Kordestani, Soheila; Bagheri Hariri, Mohiedin
2014-09-01
Gold nanotubes/nanowires (GNT/NW) were synthesized by using the template-assisted electrodeposition technique and mixed with castor oil-polyethylene glycol based polyurethane (PU) to fabricate porous composite scaffolds for biomedical application. 100 and 50 ppm of GNT/NW were used to synthesize composites. The composite scaffolds were characterized by Fourier transform infrared spectroscopy, dynamic mechanical thermal analysis, differential scanning calorimetry, and scanning electron microscopy. Cell attachment on polyurethane-GNT/NW composites was investigated using fat-derived mesenchymal stem cells. Addition of 50 or 100 ppm GNT/NW had significant effects on thermal, mechanical, and cell attachment of polyurethane. Higher crosslink density and better cell attachment and proliferation were observed in polyurethane containing 50 ppm GNT/NW. The results revealed that GNT/NW formed hydrogen bonding with the polyurethane matrix and improved the thermomechanical properties of nanocomposites. Compared with pure PU, better cellular attachment on polyurethane-GNT/NW composites was observed resulting from the improved surface properties of composites. Copyright © 2014 Elsevier B.V. All rights reserved.
Polyurethane Masks Large Areas in Electroplating
NASA Technical Reports Server (NTRS)
Beasley, J. L.
1985-01-01
Polyurethane foam provides effective mask in electroplating of copper or nickel. Thin layer of Turco maskant painted on area to be masked: Layer ensures polyurethane foam removed easily after served its purpose. Component A, isocyanate, and component B, polyol, mixed together and brushed or sprayed on mask area. Mixture reacts, yielding polyurethane foam. Foam prevents deposition of nickel or copper on covered area. New method saves time, increases productivity and uses less material than older procedures.
NASA Astrophysics Data System (ADS)
Yang, Pengfei; Wang, Yongqing; Lu, Ling; Yu, Xi; Liu, Lian
2018-03-01
Dodecyl diaryl diazomethane was firstly synthesized from 4,4-dihydroxybenzophenone and 1-bromododecane by a series of reaction steps. Then water-borne polyurethane films with different amount of DMPA were prepared, as well as a type of solvent-borne polyurethane film for comparison. Finally, all these polyurethane films were modified by dodecyl diaryl diazomethane. The dodecyl diaryl carbene was generated from dodecyl diaryl diazomethane by strong solar light, which was very convenient to insert into the Xsbnd H bonds (X = C, N) on the surface of polyurethane films. The contact angle test was used to characterize these films and depict the surface property. DSC analysis and tensile test were used to investigate the physical properties of polyurethane films before and after modification. It was suggested that the hydrophobic modification protocol with carbene insertion was very useful and convenient to prepare water-proof coatings outdoors under direct solar-light exposure.
[In Situ Polymerization and Characterization of Hydroxyapatite/polyurethane Implanted Material].
Gu, Muqing; Xiao, Fengjuan; Liang, Ye; Yue, Lin; Li, Song; Li, Lanlan; Feng, Feifei
2015-08-01
In order to improve the interfacial bonding strength of hydroxyapatite/polyurethane implanted material and dispersion of hydroxyapatite in the polyurethane matrix, we in the present study synthesized nano-hydroxyapatite/polyurethane composites by in situ polymerization. We then characterized and analyzed the fracture morphology, thermal stability, glass transition temperature and mechanical properties. We seeded MG63 cells on composites to evaluate the cytocompatibility of the composites. In situ polymerization could improve the interfacial bonding strength, ameliorate dispersion of hydroxyapatite in the properties of the composites. After adding 20 wt% hydroxyapatite into the polyurethane, the thermal stability was improved and the glass transition temperatures were increased. The tensile strength and maximum elongation were 6.83 MPa and 861.17%, respectively. Compared with those of pure polyurethane the tensile strength and maximum elongation increased by 236.45% and 143.30%, respectively. The composites were helpful for cell adhesion and proliferation in cultivation.
IDENTIFICATION OF CFC AND HCFC SUBSTITUTES FOR BLOWING POLYURETHANE FOAM INSULATION PRODUCTS
The report gives results of a cooperative effort to identiry chlorofluorocarbons and hydrochlorofluorocarbon substitutes for blowing polyurethane foam insulation products. The substantial ongoing effort is identifying third-generation blowing agets for polyurethane foams to repla...
40 CFR 63.1307 - Recordkeeping requirements.
Code of Federal Regulations, 2014 CFR
2014-07-01
...) National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63... section. Each flexible polyurethane foam slabstock source complying with the emission point specific... this section. Each flexible polyurethane foam slabstock source complying with the source-wide...
40 CFR 63.1307 - Recordkeeping requirements.
Code of Federal Regulations, 2013 CFR
2013-07-01
...) National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63... section. Each flexible polyurethane foam slabstock source complying with the emission point specific... this section. Each flexible polyurethane foam slabstock source complying with the source-wide...
Thermal behaviour and corrosion resistance of nano-ZnO/polyurethane film
NASA Astrophysics Data System (ADS)
Virgawati, E.; Soegijono, B.
2018-03-01
Hybrid materials Nano-ZnO/polyurethane film was prepared with different zinc oxide (ZnO) content in polyurethane as a matrix. The film was deposited on low carbon steel plate using high volume low pressure (HVLP) method. To observe thermal behaviour of the film, the sample was investigated using thermogravimetric analysis (TGA) and differential scanning calorimetry (DSC). Fourier transform infrared spectroscopy (FTIR) was used to see whether any chemical reaction of ZnO in polyurethane occured. TGA and FTIR results showed that the decomposition temperature shifted to a higher point and the chemical reaction of zinc oxide in polyurethane occurred. The surface morphology changed and the corrosion resistance increased with an increase of ZnO content
Functionalised polyurethane for efficient laser micromachining
NASA Astrophysics Data System (ADS)
Brodie, G. W. J.; Kang, H.; MacMillan, F. J.; Jin, J.; Simpson, M. C.
2017-02-01
Pulsed laser ablation is a valuable tool that offers a much cleaner and more flexible etching process than conventional lithographic techniques. Although much research has been undertaken on commercially available polymers, many challenges still remain, including contamination by debris on the surface, a rough etched appearance and high ablation thresholds. Functionalizing polymers with a photosensitive group is a novel way and effective way to improve the efficiency of laser micromachining. In this study, several polyurethane films grafted with different concentrations of the chromophore anthracene have been synthesized which are specifically designed for 248 nm KrF excimer laser ablation. A series of lines etched with a changing number of pulses and fluences by the nanosecond laser were applied to each polyurethane film. The resultant ablation behaviours were studied through optical interference tomography and Scanning Electron Microscopy. The anthracene grafted polyurethanes showed a vast improvement in both edge quality and the presence of debris compared with the unmodified polyurethane. Under the same laser fluence and number of pulses the spots etched in the anthracene contained polyurethane show sharp depth profiles and smooth surfaces, whereas the spots etched in polyurethane without anthracene group grafted present rough cavities with debris according to the SEM images. The addition of a small amount of anthracene (1.47%) shows a reduction in ablation threshold from unmodified polyurethane showing that the desired effect can be achieved with very little modification to the polymer.
Hydroxyapatite-silver nanoparticles coatings on porous polyurethane scaffold.
Ciobanu, Gabriela; Ilisei, Simona; Luca, Constantin
2014-02-01
The present paper is focused on a study regarding the possibility of obtaining hydroxyapatite-silver nanoparticle coatings on porous polyurethane scaffold. The method applied is based on a combined strategy involving hydroxyapatite biomimetic deposition on polyurethane surface using a Supersaturated Calcification Solution (SCS), combined with silver ions reduction and in-situ crystallization processes on hydroxyapatite-polyurethane surface by sample immersing in AgNO3 solution. The morphology, composition and phase structure of the prepared samples were characterized by scanning electron microscopy coupled with energy dispersive X-ray spectroscopy (SEM-EDX), X-ray diffraction (XRD), UV-Vis spectroscopy and X-ray photoelectron spectroscopy (XPS) measurements. The data obtained show that a layer of hydroxyapatite was deposited on porous polyurethane support and the silver nanoparticles (average size 34.71 nm) were dispersed among and even on the hydroxyapatite crystals. Hydroxyapatite/polyurethane surface acts as a reducer and a stabilizing agent for silver ions. The surface plasmon resonance peak in UV-Vis absorption spectra showed an absorption maximum at 415 nm, indicating formation of silver nanoparticles. The hydroxyapatite-silver polyurethane scaffolds were tested against Staphylococcus aureus and Escherichia coli and the obtained data were indicative of good antibacterial properties of the materials. © 2013.
Brzeska, Joanna; Morawska, Magda; Sikorska, Wanda; Tercjak, Agnieszka; Kowalczuk, Marek; Rutkowska, Maria
2017-01-01
In many areas of application of conventional non-degradable cross-linked polyurethanes (PUR), there is a need for their degradation under the influence of specific environmental factors. It is practiced by incorporation of sensitive to degradation compounds (usually of natural origin) into the polyurethane structure, or by mixing them with polyurethanes. Cross-linked polyurethanes (with 10 and 30%wt amount of synthetic poly([ R,S ]-3-hydroxybutyrate) (R,S-PHB) in soft segments) and their physical blends with poly([d,l]-lactide) (PDLLA) were investigated and then degraded under hydrolytic (phosphate buffer solution) and oxidative (CoCl 2 /H 2 O 2 ) conditions. The rate of degradation was monitored by changes of samples mass, morphology of surface and their thermal properties. Despite the small weight losses of samples, the changes of thermal properties of polymers and topography of their surface indicated that they were susceptible to gradual degradation under oxidative and hydrolytic conditions. Blends of PDLLA and polyurethane with 30 wt% of R,S -PHB in soft segments and PUR/PDLLA blends absorbed more water and degraded faster than polyurethane with low amount of R,S -PHB.
Mohammed, Issam Ahmed; Al-Mulla, Emad Abbas Jaffar; Kadar, Nurul Khizien Abdul; Ibrahim, Mazlan
2013-01-01
Palm and soya oils were converted to monoglycerides via transesterification of triglycerides with glycerol by one step process to produce renewable polyols. Thermoplastic polyurethanes (TPPUs) were prepared from the reaction of the monoglycerides which act as polyol with 4,4'-methylenediphenyldiisocyanate (MDI) whereas, thermosetting polyurethanes (TSPUs) were prepared from the reaction of glycerol, MDI and monoglycerides in one pot. Characterization of the polyurethanes was carried out by FT-IR, (1)H NMR, and iodine value and sol-gel fraction. The TSPUs showed good thermal properties compared to TPPUs as well as TSPUs exhibits good properties in pencil hardness and adhesion, however poorer in flexural and impact strength compared to TPPUs. The higher percentage of cross linked fraction, the higher degree of cross linking occurred, which is due to the higher number of double bond presents in the TSPUs. These were reflected in iodine value test as the highest iodine value of the soya-based thermosetting polyurethanes confirmed the highest degree of cross linking. Polyurethanes based on soya oil showed better properties compared to palm oil. This study is a breakthrough development of polyurethane resins using palm and soya oils as one of the raw materials.
A novel approach for synthesis of zwitterionic polyurethane coating with protein resistance.
Wang, Chunhua; Ma, Chunfeng; Mu, Changdao; Lin, Wei
2014-11-04
We have developed a novel approach to introduce zwitterions into polyurethane for the preparation of antibiofouling coating. First, the thiol-ene click reaction between 2-(dimethylamino)ethyl methacrylate (DMAEMA) and 3-mercapto-1,2-propanediol (TPG) is used to synthesize dihydroxy-terminated DMAEMA (DMA(OH)2) under UV catalysis. The product has been proved by gel permeation chromatography (GPC), Fourier transform infrared spectrum (FT-IR), proton nuclear magnetic resonance ((1)H NMR), and high resolution mass spectrometry (HRMS). DMA(OH)2 is then incorporated into polyurethane as side groups by polyaddition with diisocyanate and further reacts with 1,3-propane sultone to obtain the zwitterionic polyurethanes. The presence of sulfobetaine zwitterions side groups has been demonstrated by FT-IR and X-ray photoelectron spectroscopy (XPS). Thermal analysis indicates that the thermal stability is decreased with the increasing content of zwitterionions. The antibiofouling property of polyurethanes has been investigated by the measurement of adsorption of fibrinogen, bovine serum albumin (BSA), and lysozyme on the polyurethanes surface using quartz crystal microbalance with dissipation (QCM-D). The results show that the polyurethane coatings exhibit effective nonspecific protein resistance at higher content of zwitterionic side groups.
Kim, Hyo-Jin; Kang, Min-Sil; Knowles, Jonathan C
2014-01-01
Bio-based high elastic polyurethanes were prepared from hexamethylene diisocyanate and various ratios of isosorbide to poly(tetramethylene glycol) as a diol by a simple one-shot bulk polymerization without a catalyst. Successful synthesis of the polyurethanes was confirmed by Fourier transform-infrared spectroscopy and 1H nuclear magnetic resonance. Thermal properties were determined by differential scanning calorimetry and thermogravimetric analysis. The glass transition temperature was −47.8℃. The test results showed that the poly(tetramethylene glycol)/isosorbide-based elastomer exhibited not only excellent stress–strain properties but also superior resilience to the existing polyether-based polyurethane elastomers. The static and dynamic properties of the polyether/isosorbide-based thermoplastic elastomer were more suitable for dynamic applications. Moreover, such rigid diols impart biocompatible and bioactive properties to thermoplastic polyurethane elastomers. Degradation tests performed at 37℃ in phosphate buffer solution showed a mass loss of 4–9% after 8 weeks, except for the polyurethane with the lowest isosorbide content, which showed an initial rapid weight loss. These polyurethanes offer significant promise due to soft, flexible and biocompatible properties for soft tissue augmentation and regeneration. PMID:24812276
Code of Federal Regulations, 2013 CFR
2013-07-01
... water. Flexible polyurethane foams are open-celled, permit the passage of air through the foam, and... Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1292 Definitions. All... for the purposes of this subpart. Cured foam means flexible polyurethane foam with fully developed...
Code of Federal Regulations, 2011 CFR
2011-07-01
... water. Flexible polyurethane foams are open-celled, permit the passage of air through the foam, and... Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1292 Definitions. All terms used in... purposes of this subpart. Cured foam means flexible polyurethane foam with fully developed physical...
Code of Federal Regulations, 2014 CFR
2014-07-01
... water. Flexible polyurethane foams are open-celled, permit the passage of air through the foam, and... Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1292 Definitions. All... for the purposes of this subpart. Cured foam means flexible polyurethane foam with fully developed...
Code of Federal Regulations, 2012 CFR
2012-07-01
... water. Flexible polyurethane foams are open-celled, permit the passage of air through the foam, and... Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1292 Definitions. All terms used in... purposes of this subpart. Cured foam means flexible polyurethane foam with fully developed physical...
Biobased composites from cross-linked soybean oil and thermoplastic polyurethane
USDA-ARS?s Scientific Manuscript database
Soybean oil is an important sustainable material. Crosslinked acrylated epoxidized soybean oil (AESO) is brittle and the incorporation of thermoplastic polyurethane improves its toughness. The hydrophilic functional groups from both oil and polyurethane contribute to the adhesion of the blend compon...
USDA-ARS?s Scientific Manuscript database
Soybean oil is an important sustainable material. Crosslinked acrylated epoxidized soybean oil (AESO) is brittle without flexibility and the incorporation of thermoplastic polyurethane improves its toughness for industrial applications. The hydrophilic functional groups from both oil and polyurethan...
40 CFR 63.11415 - What are my compliance dates?
Code of Federal Regulations, 2011 CFR
2011-07-01
...) National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production and... you own or operate an existing slabstock flexible polyurethane foam production affected source, you... or operate an existing molded flexible polyurethane foam affected source, an existing rebond foam...
40 CFR 63.11415 - What are my compliance dates?
Code of Federal Regulations, 2012 CFR
2012-07-01
...) National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production and... you own or operate an existing slabstock flexible polyurethane foam production affected source, you... or operate an existing molded flexible polyurethane foam affected source, an existing rebond foam...
40 CFR 63.11415 - What are my compliance dates?
Code of Federal Regulations, 2010 CFR
2010-07-01
...) National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production and... you own or operate an existing slabstock flexible polyurethane foam production affected source, you... or operate an existing molded flexible polyurethane foam affected source, an existing rebond foam...
Fiber glass prevents cracking of polyurethane foam insulation on cryogenic vessels
NASA Technical Reports Server (NTRS)
Forge, D. A.
1968-01-01
Fiber glass material, placed between polyurethane foam insulation and the outer surfaces of cryogenic vessels, retains its resilience at cryogenic temperatures and provides an expansion layer between the metal surfaces and the polyurethane foam, preventing cracking of the latter.
40 CFR 63.11415 - What are my compliance dates?
Code of Federal Regulations, 2013 CFR
2013-07-01
...) National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production and... you own or operate an existing slabstock flexible polyurethane foam production affected source, you... or operate an existing molded flexible polyurethane foam affected source, an existing rebond foam...
40 CFR 63.11415 - What are my compliance dates?
Code of Federal Regulations, 2014 CFR
2014-07-01
...) National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production and... you own or operate an existing slabstock flexible polyurethane foam production affected source, you... or operate an existing molded flexible polyurethane foam affected source, an existing rebond foam...
Molecular simulation of fibronectin adsorption onto polyurethane surfaces
USDA-ARS?s Scientific Manuscript database
Polyethylene glycol-based polyurethanes have been widely used in biomedical applications, however are prone to swelling. A natural polyol, castor oil can be incorporated into these polyurethanes to control the degree of the swelling, which alters mechanical properties and protein adsorption characte...
NASA Astrophysics Data System (ADS)
Azmi, M. A.; Abdullah, H. Z.; Idris, M. I.
2013-12-01
This research focuses on the fabrication and characterization of sandwich composite panels using glass fiber composite skin and polyurethane foam reinforced coconut coir fiber core. The main objectives are to characterize the physical and mechanical properties and to elucidate the effect of coconut coir fibers in polyurethane foam cores and sandwich composite panels. Coconut coir fibers were used as reinforcement in polyurethane foams in which later were applied as the core in sandwich composites ranged from 5 wt% to 20 wt%. The physical and mechanical properties found to be significant at 5 wt% coconut coir fiber in polyurethane foam cores as well as in sandwich composites. It was found that composites properties serve better in sandwich composites construction.
Synthesis of a Novel Biodegradable Polyurethane with Phosphatidylcholines
Cao, Jun; Chen, Niancao; Chen, Yuanwei; Luo, Xianglin
2010-01-01
A novel polyurethane was successfully synthesized by chain-extension of biodegradable poly (l-lactide) functionalized phosphatidylcholine (PC) with hexamethylene diisocyanate (HDI) as chain extender (PUR-PC). The molecular weights, glass transition temperature (Tg) increased significantly after the chain-extension. The hydrophilicity of PUR-PC was better than the one without PC, according to a water absorption test. Moreover, the number of adhesive platelets and anamorphic platelets on PUR-PC film were both less than those on PUR film. These preliminary results suggest that this novel polyurethane might be a better scaffold than traditional biodegradable polyurethanes for tissue engineering due to its better blood compatibility. Besides, this study also provides a new method to prepare PC-modified biodegradable polyurethanes. PMID:20480047
40 CFR 721.10298 - MDI terminated polyester polyurethane polymer (generic).
Code of Federal Regulations, 2014 CFR
2014-07-01
... polymer (generic). 721.10298 Section 721.10298 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY... Specific Chemical Substances § 721.10298 MDI terminated polyester polyurethane polymer (generic). (a... generically as MDI terminated polyester polyurethane polymer (P-11-662) is subject to reporting under this...
40 CFR 721.10298 - MDI terminated polyester polyurethane polymer (generic).
Code of Federal Regulations, 2013 CFR
2013-07-01
... polymer (generic). 721.10298 Section 721.10298 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY... Specific Chemical Substances § 721.10298 MDI terminated polyester polyurethane polymer (generic). (a... generically as MDI terminated polyester polyurethane polymer (P-11-662) is subject to reporting under this...
40 CFR 721.10298 - MDI terminated polyester polyurethane polymer (generic).
Code of Federal Regulations, 2012 CFR
2012-07-01
... polymer (generic). 721.10298 Section 721.10298 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY... Specific Chemical Substances § 721.10298 MDI terminated polyester polyurethane polymer (generic). (a... generically as MDI terminated polyester polyurethane polymer (P-11-662) is subject to reporting under this...
Polyurethane Filler for Electroplating
NASA Technical Reports Server (NTRS)
Beasley, J. L.
1984-01-01
Polyurethane foam proves suitable as filler for slots in parts electroplated with copper or nickel. Polyurethane causes less contamination of plating bath and of cleaning and filtering tanks than wax fillers used previously. Direct cost of maintenance and indirect cost of reduced operating time during tank cleaning also reduced.
Cryogenic line insulation made from prefabricated polyurethane shells
NASA Technical Reports Server (NTRS)
Lerma, G.
1975-01-01
Prefabricated polyurethane foam insulation is inexpensive and easily installed on cryogenic lines. Insulation sections are semicircular half shells. Pair of half shells is placed to surround cryogenic line. Cylindrically-shaped knit sock is pulled over insulation then covered with polyurethane resin to seal system.
Microwave-assisted synthesis of cyclodextrin polyurethanes
USDA-ARS?s Scientific Manuscript database
Cyclodextrin (CD) has often been incorporated into polyurethanes in order to facilitate its use in encapsulation or removal of organic species for various applications. In this work a microwave-assisted method has been developed to produce polyurethanes consisting of alpha-, ß-, and gamma-CD and thr...
2016-01-01
Nitric oxide (NO) releasing polymers are promising in improving the biocompatibility of medical devices. Polyurethanes are commonly used to prepare/fabricate many devices (e.g., catheters); however, the transport properties of NO within different polyurethanes are less studied, creating a gap in the rational design of new NO releasing devices involving polyurethane materials. Herein, we study the diffusion and partitioning of NO in different biomedical polyurethanes via the time-lag method. The diffusion of NO is positively correlated with the PDMS content within the polyurethanes, which can be rationalized by effective media theory considering various microphase morphologies. Using catheters as a model device, the effect of these transport properties on the NO release profiles and the distribution around an asymmetric dual lumen catheter are simulated using finite element analysis and validated experimentally. This method can be readily applied in studying other NO release medical devices with different configurations. PMID:27660819
Sub-Surface and Bulk Creep Behaviour of Polyurethane/Clay Nanocomposites.
Jin, J; Yusoh, K; Zhang, H X; Song, M
2016-03-01
A series of exfoliated and intercalated polyurethane organoclay nanocomposites were prepared by in situ polymerization of polyol/organoclay mixture, chain extender and diisocyanate. The creep behaviour of subsurface and bulk of the polyurethane coatings was investigated by nanoindentation technique and uniaxial conventional creep testing method, respectively. The results showed that the creep resistance of the nanocomposites was significantly improved by incorporation of organoclay. The enhancement of creep resistance was dependent on clay content as well as organoclay structure (exfoliation or intercalation) in the polymer matrix. With 1 wt% organoclay, the creep resistance increased by about 50% for the intercalated organoclay and 6% for the exfoliated organoclay systems, respectively, compared to the pristine polyurethane. Viscoelastic model was employed to investigate the effect of organoclay loadings on the creep performance of the polyurethane. Results showed the model was in good agreement with the experimental data. Incorporation of clay leads to an increase in elastic deformation especially in exfoliated polyurethane nanocomposites and induces a higher initial displacement at the early stage of creep.
Facile preparation of mussel-inspired polyurethane hydrogel and its rapid curing behavior.
Sun, Peiyu; Wang, Jing; Yao, Xiong; Peng, Ying; Tu, Xiaoxiong; Du, Pengfei; Zheng, Zhen; Wang, Xinling
2014-08-13
A facile method was found to incorporate a mussel-inspired adhesive moiety into synthetic polymers, and mussel mimetic polyurethanes were developed as adhesive hydrogels. In these polymers, a urethane backbone was substituted for the polyamide chain of mussel adhesive proteins, and dopamine was appended to mimic the adhesive moiety of adhesive proteins. A series of mussel mimetic polyurethanes were created through a step-growth polymerization based on hexamethylene diisocyanate as a hard segment, PEG having different molecular weights as a soft segment, and lysine-dopamine as a chain extender. Upon a treatment with Fe(3+), the aqueous mussel mimetic polyurethane solutions can be triggered by pH adjustment to form adhesive hydrogels instantaneously; these materials can be used as injectable adhesive hydrogels. Upon a treatment with NaIO4, the mussel mimetic polyurethane solutions can be cured in a controllable period of time. The successful combination of the unique mussel-inspired adhesive moiety with a tunable polyurethane structure can result in a new kind of mussel-inspired adhesive polymers.
The Effect of Plant Source on the Structural Properties of Lignin-based Polyurethane Blends
NASA Astrophysics Data System (ADS)
Lang, Jason; Dadmun, Mark
The development of polyurethane materials based on incorporating lignin from a variety of plant sources (softwood, hardwood, and non-wood) were synthesized. Further experiments study the physical properties of the resulting lignin-based polyurethane as a function of the lignin structure, which varies with plant source. Here, we report the effect that internal crosslinking of the lignin structure has on the modulus, hardness, glass transition temperature, and thermal decomposition of the synthesized lignin-based polyurethane composites. The lignins used in this work were a softwood kraft lignin, hardwood lignosulfonate, and a wheat straw soda lignin. The lignin, acting as a polyol and the hardblock segment, reacts with TDI-endcapped PPG (2,300 MN) as the rubbery softblock component to produce lignin-based polyurethanes with varying lignin content (10, 20, 30, 40, 50, and 60 wt%). Results show that the wheat straw lignin provides the superior mechanical properties and thermal resistance. These properties are correlated to the two-phase morphology of the resultant polyurethane.
Xing, Juan; Ma, Yufei; Lin, Manping; Wang, Yuanliang; Pan, Haobo; Ruan, Changshun; Luo, Yanfeng
2016-10-01
Programming such as stretching, compression and bending is indispensible to endow polyurethanes with shape memory effects. Despite extensive investigations on the contributions of programming processes to the shape memory effects of polyurethane, less attention has been paid to the nanostructures of shape memory polyurethanes surface during the programming process. Here we found that stretching could induce the reassembly of hard domains and thereby change the nanostructures on the film surfaces with dependence on the stretching ratios (0%, 50%, 100%, and 200%). In as-cast polyurethane films, hard segments sequentially assembled into nano-scale hard domains, round or fibrillar islands, and fibrillar apophyses. Upon stretching, the islands packed along the stretching axis to form reoriented fibrillar apophyses along the stretching direction. Stretching only changed the chemical patterns on polyurethane films without significantly altering surface roughness, with the primary composition of fibrillar apophyses being hydrophilic hard domains. Further analysis of osteoblasts morphology revealed that the focal adhesion formation and osteoblasts orientation were in accordance with the chemical patterns of the underlying stretched films, which corroborates the vital roles of stretching-induced nanostructures in regulating osteoblasts morphology. These novel findings suggest that programming might hold great potential for patterning polyurethane surfaces so as to direct cellular behavior. In addition, this work lays groundwork for guiding the programming of shape memory polyurethanes to produce appropriate nanostructures for predetermined medical applications. Copyright © 2016 Elsevier B.V. All rights reserved.
Wang, Anning; Gao, Hui; Sun, Yanfang; Sun, Yu-long; Yang, Ying-Wei; Wu, Guolin; Wang, Yinong; Fan, Yunge; Ma, Jianbiao
2013-01-30
A series of temperature- and pH-responsive polyurethanes based on hexamethylene diisocyanate (HDI) and 4,4'-diphenylmethane diisocyanate (MDI) were synthesized by a coupling reaction with bis-1,4-(hydroxyethyl) piperazine (HEP), N-methyldiethanolamine (MDEA) and N-butyldiethanolamine (BDEA), respectively. The chemical structure, molecular weight, thermal property and crystallization properties were characterized by Fourier transform infrared (FT-IR) spectroscopy, nuclear magnetic resonance (NMR) spectroscopy, gel permeation chromatography (GPC), differential scanning calorimetry (DSC) and X-ray diffraction (XRD) spectroscopy. The resulting polyurethanes were then used to prepare nanoparticles either by direct dispersion method or dialysis method. Their pH and temperature responsibilities were evaluated by optical transmittance and size measurement in aqueous media. Interestingly, HDI-based and MDI-based polyurethanes exhibited different pH and temperature responsive properties. Nanoparticles based on HDI-HEP and HDI-MDEA were temperature-responsive, while MDI-based biomaterials were not. All of them showed pH-sensitive behavior. The possible responsive mechanism was investigated by (1)H NMR spectroscopy. The cytotoxicity of the polyurethanes was evaluated using methylthiazoletetrazolium (MTT) assay in vitro. It was shown that the HDI-based polyurethanes were non-toxic, and could be applied to doxorubicin (DOX) encapsulation. The experimental results indicated that DOX could be efficiently encapsulated into polyurethane nanoparticles and uptaken by Huh-7 cells. The loaded DOX molecules could be released from the drug-loaded polyurethane nanoparticles upon pH and temperature changes, responsively. Copyright © 2012 Elsevier B.V. All rights reserved.
Iyer, Kartik; Dearman, Bronwyn L; Wagstaff, Marcus J D; Greenwood, John E
2016-01-01
Auricular reconstruction poses a challenge for reconstructive and burns surgeons. Techniques involving cartilage tissue engineering have shown potential in recent years. A biodegradable polyurethane matrix developed for dermal reconstruction offers an alternative to autologous, allogeneic, or xenogeneic biologicals for cartilage reconstruction. This study assesses such a polyurethane matrix for this indication in vivo and in vitro. To evaluate intrinsic cartilage repair, three pigs underwent auricular surgery to create excisional cartilage ± perichondrial defects, measuring 2 × 3 cm in each ear, into which acellular polyurethane matrices were implanted. Biopsies were taken at day 28 for histological assessment. Porcine chondrocytes ± perichondrocytes were cultured and seeded in vitro onto 1 × 1 cm polyurethane scaffolds. The total culture period was 42 days; confocal, histological, and immunohistochemical analyses of scaffold cultures were performed on days 14, 28, and 42. In vivo, the polyurethane matrices integrated with granulation tissue filling all biopsy samples. Minimal neocartilage invasion was observed marginally on some samples. Tissue composition was identical between ears whether perichondrium was left intact, or not. In vitro, the polyurethane matrix was biocompatible with chondrocytes ± perichondrocytes and supported production of extracellular matrix and Type II collagen. No difference was observed between chondrocyte culture alone and chondrocyte/perichondrocyte scaffold coculture. The polyurethane matrix successfully integrated into the auricular defect and was a suitable scaffold in vitro for cartilage tissue engineering, demonstrating its potential application in auricular reconstruction.
MORPHOLOGICAL CHANGES IN POLYURETHANE COATINGS ON EXPOSURE TO WATER. (R828081E01)
When a polyurethane self-priming coating on a sol-gel treated aluminum panel was immersed in dilute Harrison's solution, subsequent change of the polyurethane coating surface was inspected with atomic force microscopy (AFM) and scanning electron microscopy (SEM). After immersi...
40 CFR 63.11417 - What are the compliance requirements for new and existing sources?
Code of Federal Regulations, 2010 CFR
2010-07-01
... Flexible Polyurethane Foam Production and Fabrication Area Sources Standards and Compliance Requirements... a slabstock flexible polyurethane foam production affected source, you must comply with the... affected source, or a loop slitter at a flexible polyurethane foam fabrication affected source you must...
40 CFR 63.1290 - Applicability.
Code of Federal Regulations, 2014 CFR
2014-07-01
... Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1290 Applicability. (a) The provisions of this subpart apply to each new and existing flexible polyurethane foam or rebond...) Produces flexible polyurethane or rebond foam; (2) Emits a HAP, except as provided in paragraph (c)(2) of...
40 CFR 63.11417 - What are the compliance requirements for new and existing sources?
Code of Federal Regulations, 2012 CFR
2012-07-01
... Flexible Polyurethane Foam Production and Fabrication Area Sources Standards and Compliance Requirements... a slabstock flexible polyurethane foam production affected source, you must comply with the... affected source, or a loop slitter at a flexible polyurethane foam fabrication affected source you must...
40 CFR 63.11417 - What are the compliance requirements for new and existing sources?
Code of Federal Regulations, 2011 CFR
2011-07-01
... Flexible Polyurethane Foam Production and Fabrication Area Sources Standards and Compliance Requirements... a slabstock flexible polyurethane foam production affected source, you must comply with the... affected source, or a loop slitter at a flexible polyurethane foam fabrication affected source you must...
40 CFR 63.11417 - What are the compliance requirements for new and existing sources?
Code of Federal Regulations, 2014 CFR
2014-07-01
... Flexible Polyurethane Foam Production and Fabrication Area Sources Standards and Compliance Requirements... a slabstock flexible polyurethane foam production affected source, you must comply with the... affected source, or a loop slitter at a flexible polyurethane foam fabrication affected source you must...
Formulation, Preparation, and Characterization of Polyurethane Foams
ERIC Educational Resources Information Center
Pinto, Moises L.
2010-01-01
Preparation of laboratory-scale polyurethane foams is described with formulations that are easy to implement in experiments for undergraduate students. Particular attention is given to formulation aspects that are based on the main chemical reactions occurring in polyurethane production. This allows students to develop alternative formulations to…
40 CFR 63.11417 - What are the compliance requirements for new and existing sources?
Code of Federal Regulations, 2013 CFR
2013-07-01
... Flexible Polyurethane Foam Production and Fabrication Area Sources Standards and Compliance Requirements... a slabstock flexible polyurethane foam production affected source, you must comply with the... affected source, or a loop slitter at a flexible polyurethane foam fabrication affected source you must...
40 CFR 63.1290 - Applicability.
Code of Federal Regulations, 2013 CFR
2013-07-01
... Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1290 Applicability. (a) The provisions of this subpart apply to each new and existing flexible polyurethane foam or rebond...) Produces flexible polyurethane or rebond foam; (2) Emits a HAP, except as provided in paragraph (c)(2) of...
Electrically conductive rigid polyurethane foam
Neet, T.E.; Spieker, D.A.
1983-12-08
A rigid, moldable polyurethane foam comprises about 2 to 10 weight percent, based on the total foam weight, of a carbon black which is CONDUCTEX CC-40-220 or CONDUCTEX SC, whereby the rigid polyurethane foam is electrically conductive and has essentially the same mechanical properties as the same foam without carbon black added.
Tests Of Polyurethane And Dichromate Coats On Aluminum
NASA Technical Reports Server (NTRS)
Danford, M. D.
1992-01-01
Report describes experiments to determine relative effectiveness of new polyurethane and more-conventional dichromate coat in helping to retard corrosion of anodized 6061-T6 aluminum. Concludes by suggesting greater protection against corrosion achieved by combining polyurethane-sealing method with hard-anodizing method and by increasing thickness of coat.
Electrically conductive rigid polyurethane foam
Neet, Thomas E.; Spieker, David A.
1985-03-19
A rigid, polyurethane foam comprises about 2-10 weight percent, based on the total foam weight, of a carbon black which is CONDUCTEX CC-40-220 or CONDUCTEX SC, whereby the rigid polyurethane foam is electrically conductive and has essentially the same mechanical properties as the same foam without carbon black added.
40 CFR 63.8784 - What parts of my plant does this subpart cover?
Code of Federal Regulations, 2013 CFR
2013-07-01
... CATEGORIES (CONTINUED) National Emission Standards for Hazardous Air Pollutants: Flexible Polyurethane Foam... flexible polyurethane foam fabrication. (b) The affected sources are defined in this section in paragraphs... to bond foam to foam at a flexible polyurethane foam fabrication plant site. (2) The flame lamination...
40 CFR 63.11419 - What definitions apply to this subpart?
Code of Federal Regulations, 2014 CFR
2014-07-01
... (CONTINUED) National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam...; § 63.8830 of subpart MMMMM; § 63.2 of subpart A; and in this section as follows: Flexible polyurethane foam fabrication facility means a facility where pieces of flexible polyurethane foam are cut, bonded...
40 CFR 63.11414 - Am I subject to this subpart?
Code of Federal Regulations, 2011 CFR
2011-07-01
...) National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production and... that produces flexible polyurethane foam or rebond foam as defined in § 63.1292 of subpart III. (2) You own or operate a flexible polyurethane foam fabrication facility, as defined in § 63.11419. (b) The...
40 CFR 63.8784 - What parts of my plant does this subpart cover?
Code of Federal Regulations, 2012 CFR
2012-07-01
... CATEGORIES (CONTINUED) National Emission Standards for Hazardous Air Pollutants: Flexible Polyurethane Foam... flexible polyurethane foam fabrication. (b) The affected sources are defined in this section in paragraphs... to bond foam to foam at a flexible polyurethane foam fabrication plant site. (2) The flame lamination...
40 CFR 63.8784 - What parts of my plant does this subpart cover?
Code of Federal Regulations, 2010 CFR
2010-07-01
... CATEGORIES (CONTINUED) National Emission Standards for Hazardous Air Pollutants: Flexible Polyurethane Foam... flexible polyurethane foam fabrication. (b) The affected sources are defined in this section in paragraphs... to bond foam to foam at a flexible polyurethane foam fabrication plant site. (2) The flame lamination...
40 CFR 63.11414 - Am I subject to this subpart?
Code of Federal Regulations, 2012 CFR
2012-07-01
...) National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production and... that produces flexible polyurethane foam or rebond foam as defined in § 63.1292 of subpart III. (2) You own or operate a flexible polyurethane foam fabrication facility, as defined in § 63.11419. (b) The...
40 CFR 63.11419 - What definitions apply to this subpart?
Code of Federal Regulations, 2010 CFR
2010-07-01
... (CONTINUED) National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam...; § 63.8830 of subpart MMMMM; § 63.2 of subpart A; and in this section as follows: Flexible polyurethane foam fabrication facility means a facility where pieces of flexible polyurethane foam are cut, bonded...
Storage-stable foamable polyurethane is activated by heat
NASA Technical Reports Server (NTRS)
1966-01-01
Polyurethane foamable mixture remains inert in storage unit activated to produce a rapid foaming reaction. The storage-stable foamable composition is spread as a paste on the surface of an expandable structure and, when heated, yields a rigid open-cell polyurethane foam that is self-bondable to the substrate.
40 CFR 63.11414 - Am I subject to this subpart?
Code of Federal Regulations, 2013 CFR
2013-07-01
...) National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production and... that produces flexible polyurethane foam or rebond foam as defined in § 63.1292 of subpart III. (2) You own or operate a flexible polyurethane foam fabrication facility, as defined in § 63.11419. (b) The...
40 CFR 63.1290 - Applicability.
Code of Federal Regulations, 2011 CFR
2011-07-01
... Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1290 Applicability. (a) The provisions of this subpart apply to each new and existing flexible polyurethane foam or rebond foam process... polyurethane or rebond foam; (2) Emits a HAP, except as provided in paragraph (c)(2) of this section; and (3...
40 CFR 63.11419 - What definitions apply to this subpart?
Code of Federal Regulations, 2013 CFR
2013-07-01
... (CONTINUED) National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam...; § 63.8830 of subpart MMMMM; § 63.2 of subpart A; and in this section as follows: Flexible polyurethane foam fabrication facility means a facility where pieces of flexible polyurethane foam are cut, bonded...
40 CFR 63.8784 - What parts of my plant does this subpart cover?
Code of Federal Regulations, 2011 CFR
2011-07-01
... CATEGORIES (CONTINUED) National Emission Standards for Hazardous Air Pollutants: Flexible Polyurethane Foam... flexible polyurethane foam fabrication. (b) The affected sources are defined in this section in paragraphs... to bond foam to foam at a flexible polyurethane foam fabrication plant site. (2) The flame lamination...
40 CFR 63.11414 - Am I subject to this subpart?
Code of Federal Regulations, 2010 CFR
2010-07-01
...) National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production and... that produces flexible polyurethane foam or rebond foam as defined in § 63.1292 of subpart III. (2) You own or operate a flexible polyurethane foam fabrication facility, as defined in § 63.11419. (b) The...
40 CFR 63.11419 - What definitions apply to this subpart?
Code of Federal Regulations, 2011 CFR
2011-07-01
... (CONTINUED) National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam...; § 63.8830 of subpart MMMMM; § 63.2 of subpart A; and in this section as follows: Flexible polyurethane foam fabrication facility means a facility where pieces of flexible polyurethane foam are cut, bonded...
40 CFR 63.1290 - Applicability.
Code of Federal Regulations, 2012 CFR
2012-07-01
... Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1290 Applicability. (a) The provisions of this subpart apply to each new and existing flexible polyurethane foam or rebond foam process... polyurethane or rebond foam; (2) Emits a HAP, except as provided in paragraph (c)(2) of this section; and (3...
40 CFR 63.8784 - What parts of my plant does this subpart cover?
Code of Federal Regulations, 2014 CFR
2014-07-01
... CATEGORIES (CONTINUED) National Emission Standards for Hazardous Air Pollutants: Flexible Polyurethane Foam... flexible polyurethane foam fabrication. (b) The affected sources are defined in this section in paragraphs... to bond foam to foam at a flexible polyurethane foam fabrication plant site. (2) The flame lamination...
40 CFR 63.1290 - Applicability.
Code of Federal Regulations, 2010 CFR
2010-07-01
... Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1290 Applicability. (a) The provisions of this subpart apply to each new and existing flexible polyurethane foam or rebond foam process... polyurethane or rebond foam; (2) Emits a HAP, except as provided in paragraph (c)(2) of this section; and (3...
40 CFR 63.11419 - What definitions apply to this subpart?
Code of Federal Regulations, 2012 CFR
2012-07-01
... (CONTINUED) National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam...; § 63.8830 of subpart MMMMM; § 63.2 of subpart A; and in this section as follows: Flexible polyurethane foam fabrication facility means a facility where pieces of flexible polyurethane foam are cut, bonded...
40 CFR 63.11414 - Am I subject to this subpart?
Code of Federal Regulations, 2014 CFR
2014-07-01
...) National Emission Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production and... that produces flexible polyurethane foam or rebond foam as defined in § 63.1292 of subpart III. (2) You own or operate a flexible polyurethane foam fabrication facility, as defined in § 63.11419. (b) The...
Polyurethane-covered mammary implants: a 12-year experience.
Gasperoni, C; Salgarello, M; Gargani, G
1992-10-01
Polyurethane-covered mammary implants are the implants of choice in aesthetic and reconstructive mammary surgery. These implants give very good results in regard to breast contour and consistency, and have a very low complication rate. We present our 12-year experience using polyurethane-covered prostheses. We place the implant mostly in the subglandular or subcutaneous site, and their capsular contracture rate is extremely low (3.3%). Based on our experience, we also review the other complications and side effects occurring with polyurethane prostheses and discuss them in detail.
Corrosion and degradation of a polyurethane/Co-Ni-Cr-Mo pacemaker lead
DOE Office of Scientific and Technical Information (OSTI.GOV)
Sung, P.; Fraker, A.C.
1987-12-01
An investigation to study changes in the metal surfaces and the polyurethane insulation of heart pacemaker leads under controlled in vitro conditions was conducted. A polyurethane (Pellethane 2363-80A)/Co-Ni-Cr-Mo (MP35N) wire lead was exposed in Hanks' physiological saline solution for 14 months and then analyzed using scanning electron microscopy, x-ray energy dispersive analysis, and small angle x-ray scattering. Results showed that some leakage of solution into the lead had occurred and changes were present on both the metal and the polyurethane surfaces.
Physical Training Methods For Mine Rescuers In 2015
NASA Astrophysics Data System (ADS)
Marin, Laurentiu; Pavel, Topala; Marin, Catalina Daniela; Sandu, Teodor
2015-07-01
Research and development activities presented were aimed at obtaining a nanocomposite polyurethane matrix with special anti-wear, anti-slip and fire-resistant properties. Research and development works were materialized by obtaining polyurethane nanocomposite matrix, by its physico-chemical modification in order to give the desired technological properties and by characterization of the obtained material. Polyurethane nanocomposite matrix was obtained by reacting a PETOL 3 type polyetherpolyol (having a molecular weight of 5000 UAM) with a diisocyanate under well-established reaction conditions. Target specific technological properties were obtained by physical and chemical modification of polyurethane nanocomposite matrix. The final result was getting a pellicle material based on modified nanocomposite polyurethane, with anti-wear, anti-slip and fire-resistant properties, compatible with most substrates encountered in civil and industrial construction: wood, concrete, metal.
NASA Astrophysics Data System (ADS)
Hu, Yougen; Zhao, Tao; Wu, Xiaolin; Lai, Maobai; Jiang, Chengming; Sun, Rong
2011-11-01
Thermal energy storage plays an important role in heat management because of the demand for developed energy conservation, and has applications in diverse areas, from buildings to textiles and clothings. In this study, we aimed to improve thermal characteristics of polyurethane rigid foams that have been widely used for thermal insulation in electrical water heaters. Through this work, paraffin waxes with melting point of 55~65°C act as phase change materials. Then the phase change materials were incorporated into the polyurethane foams at certain ratio. The polyurethane/phase change composite materials used as insulation layers in electrical water heaters performed the enthalpy value of 5~15 J/g. Energy efficiency of the electrical water heaters was tested according to the National Standard of China GB 21519-2008. Results show that 24 h energy consumption of the electrical water heaters manufactured by traditional polyurethane rigid foams and polyurethane/phase change material composites was 1.0612 kWh and 0.9833 kWh, respectively. The results further show that the energy-saving rate is 7.36%. These proved that polyurethane/phase change composite materials can be designed as thermal insulators equipped with electrical water heaters and have a significant effect on energy conservation.
NASA Astrophysics Data System (ADS)
Hu, Yougen; Zhao, Tao; Wu, Xiaolin; Lai, Maobai; Jiang, Chengming; Sun, Rong
2012-04-01
Thermal energy storage plays an important role in heat management because of the demand for developed energy conservation, and has applications in diverse areas, from buildings to textiles and clothings. In this study, we aimed to improve thermal characteristics of polyurethane rigid foams that have been widely used for thermal insulation in electrical water heaters. Through this work, paraffin waxes with melting point of 55~65°C act as phase change materials. Then the phase change materials were incorporated into the polyurethane foams at certain ratio. The polyurethane/phase change composite materials used as insulation layers in electrical water heaters performed the enthalpy value of 5~15 J/g. Energy efficiency of the electrical water heaters was tested according to the National Standard of China GB 21519-2008. Results show that 24 h energy consumption of the electrical water heaters manufactured by traditional polyurethane rigid foams and polyurethane/phase change material composites was 1.0612 kWh and 0.9833 kWh, respectively. The results further show that the energy-saving rate is 7.36%. These proved that polyurethane/phase change composite materials can be designed as thermal insulators equipped with electrical water heaters and have a significant effect on energy conservation.
Presence of Biofilms on Polyurethane-Coated Breast Implants: Preliminary Results.
Rieger, Ulrich M; Djedovic, Gabriel; Pattiss, Alexander; Raschke, Gregor F; Frei, Reno; Pierer, Gerhard; Trampuz, Andrej
2016-01-01
Polyurethane-coated breast implants seem to be associated with lower medium- and long-term capsular contracture rates in comparison to textured or smooth implant surfaces. Although the etiology of capsular contracture is uncertain, bacterial biofilms have been suggested to trigger chronic peri-implant inflammation, eventually leading to capsular contracture. It is unknown whether polyurethane-coated implants are less prone to biofilm colonization than other implant surfaces. We extracted data from patient records included in a prospective cohort between 2008 and 2011. All patients who underwent removal of polyurethane-coated implants were included in this current study and screened for presence of biofilms by sonication. In addition, implant- and patient-related data were analyzed. Of the ten included polyurethane-coated breast implants, six had been inserted for reconstructive purposes and four for aesthetic reasons. The median implant indwelling time was 28.3 mo. Overall, sonication cultures were positive in 50% of implants. Propionibacterium acnes and coagulase-negative staphylococci were the predominant pathogens isolated from biofilm cultures. Like other implant surfaces, polyurethane-coated implants are prone to biofilm colonization. Further investigations are needed to determine why capsular contracture rates seem to be lower in polyurethane implants than in other implant surfaces. Notably, in this study, 40% of the implants were explanted from breasts with severe capsular contracture.
Kim, Hyo-Jin; Kang, Min-Sil; Knowles, Jonathan C; Gong, Myoung-Seon
2014-09-01
Bio-based high elastic polyurethanes were prepared from hexamethylene diisocyanate and various ratios of isosorbide to poly(tetramethylene glycol) as a diol by a simple one-shot bulk polymerization without a catalyst. Successful synthesis of the polyurethanes was confirmed by Fourier transform-infrared spectroscopy and (1)H nuclear magnetic resonance. Thermal properties were determined by differential scanning calorimetry and thermogravimetric analysis. The glass transition temperature was -47.8℃. The test results showed that the poly(tetramethylene glycol)/isosorbide-based elastomer exhibited not only excellent stress-strain properties but also superior resilience to the existing polyether-based polyurethane elastomers. The static and dynamic properties of the polyether/isosorbide-based thermoplastic elastomer were more suitable for dynamic applications. Moreover, such rigid diols impart biocompatible and bioactive properties to thermoplastic polyurethane elastomers. Degradation tests performed at 37℃ in phosphate buffer solution showed a mass loss of 4-9% after 8 weeks, except for the polyurethane with the lowest isosorbide content, which showed an initial rapid weight loss. These polyurethanes offer significant promise due to soft, flexible and biocompatible properties for soft tissue augmentation and regeneration. © The Author(s) 2014 Reprints and permissions: sagepub.co.uk/journalsPermissions.nav.
DOE Office of Scientific and Technical Information (OSTI.GOV)
Yang, Yong; Zhou, Yuming, E-mail: ymzhou@seu.edu.cn; Ge, Jianhua
Highlights: ► Silane coupling agent of KH550 was used to connect the ITO and polyurethanes. ► Infrared emissivity values of the hybrids were compared and analyzed. ► Interfacial synergistic action and orderly secondary structure were the key factors. -- Abstract: Optically active polyurethane@indium tin oxide and racemic polyurethane@indium tin oxide nanocomposites (LPU@ITO and RPU@ITO) were prepared by grafting the organics onto the surfaces of modified ITO nanoparticles. LPU@ITO and RPU@ITO composites based on the chiral and racemic tyrosine were characterized by FT-IR, UV–vis spectroscopy, X-ray diffraction (XRD), SEM, TEM, and thermogravimetric analysis (TGA), and the infrared emissivity values (8–14 μm)more » were investigated in addition. The results indicated that the polyurethanes had been successfully grafted onto the surfaces of ITO without destroying the crystalline structure. Both composites possessed the lower infrared emissivity values than the bare ITO nanoparticles, which indicated that the interfacial interaction had great effect on the infrared emissivity. Furthermore, LPU@ITO based on the optically active polyurethane had the virtue of regular secondary structure and more interfacial synergistic actions between organics and inorganics, thus it exhibited lower infrared emissivity value than RPU@ITO based on the racemic polyurethane.« less
Thomas, V; Kumari, T V; Jayabalan, M
2001-01-01
The effect of physical cross-linking in candidate cycloaliphatic and hydrophobic poly(urethane urea) (4,4'-methylenebis(cyclohexylisocyanate), H(12)MDI/hydroxy-terminated polybutadiene, HTPBD/hexamethylenediamine, HDA) and poly(ether urethane urea)s (H(12)MDI/HTPBD-PTMG/HDA) on the in vitro calcification and blood-material interaction was studied. All the candidate poly(urethane urea)s and poly(ether urethane urea)s elicit acceptable hemolytic activity, cytocompatibility, calcification, and blood compatibility in vitro. The studies on blood-material interaction reveal that the present poly(urethane urea)s are superior to polystyrene microtiter plates which were used for the studies on blood-material interaction. The present investigation reveals the influence of physical cross-link density on biological interaction differently with poly(urethane urea) and poly(ether urethane urea)s. The higher the physical cross-link density in the poly(urethane urea)s, the higher the calcification and consumption of WBC in whole blood. On the other hand, the higher the physical cross-link density in the poly(ether urethane urea)s, the lesser the calcification and consumption of WBC in whole blood. However a reverse of the above trend has been observed with the platelet consumption in the poly(urethane urea)s and poly(ether urethane urea)s.
Silva, Eduardo Nascimento; Ribas-Filho, Jurandir Marcondes; Czeczko, Nicolau Gregori; Pachnicki, Jan Pawel Andrade; Netto, Mário Rodrigues Montemor; Lipinski, Leandro Cavalcante; Noronha, Lucia de; Colman, Joelmir; Zeni, João Otavio; Carvalho, Caroline Aragão de
2016-12-01
To assess the capsules formed by silicone implants coated with polyurethane foam and with a textured surface. Sixty-four Wistar albinus rats were divided into two groups of 32 each using polyurethane foam and textured surface. The capsules around the implants were analyzed for 30, 50, 70 and 90 days. Were analyzed the following parameters: foreign body reaction, granulation tissue, presence of myofibroblasts, neoangiogenesis, presence of synovial metaplasia, capsular thickness, total area and collagen percentage of type I and III, in capsules formed around silicone implants in both groups. The foreign body reaction was only present in the four polyurethane subgroups. The formation of granulation tissue and the presence of myofibroblasts were higher in the four polyurethane subgroups. Regarding to neoangiogenesis and synovial metaplasia, there was no statistical difference between the groups. Polyurethane group presented (all subgroups) a greater capsule thickness, a smaller total area and collagen percentage of type I and a higher percentage area of type III, with statistical difference. The use of polyurethane-coated implants should be stimulated by the long-term results in a more stable capsule and a lower incidence of capsular contracture, despite developing a more intense and delayed inflammatory reaction in relation to implants with textured surface.
Polyurethane foam-covered breast implants: a justified choice?
Scarpa, C; Borso, G F; Vindigni, V; Bassetto, F
2015-01-01
Even if the safety of the polyurethane prosthesis has been the subject of many studies and professional and public controversies. Nowadays, polyurethane covered implants are very popular in plastic surgery for the treatment of capsular contracture. We have identified 41 papers (1 is a communication of the FDA) by using search browsers such as Pubmed, Medline, and eMedicine. Eleven manuscripts have been used for an introduction, and the remaining thirty have been subdivided into three tables whose results have been summarized in three main chapters: (1) capsular formation and contracture, (2) complications, (3) biodegradation and cancer risk. (1) The polyurethanic capsule is a well defined foreign body reaction characterized by synovial metaplasia, a thin layer of disarranged collagen fibers and a high vascularization. These features make possible a "young" capsule and a low occurrence of capsular contracture even over a long period (10 years); (2) the polyurethane implants may be difficult to remove but there is no evidence that they cause an increase in the other complications; (3) there is no evidence of polyurethane related cancer in long-term studies (after 5 years). Polyurethane foam covered breast implants remain a valid choice for the treatment of capsular contracture even if it would be very useful to verify the ease of removal of the prosthesis and to continue investigations on biodegradation products.
Multifunctional cationic polyurethanes designed for non-viral cancer gene therapy.
Cheng, Jian; Tang, Xin; Zhao, Jie; Shi, Ting; Zhao, Peng; Lin, Chao
2016-01-01
Nano-polyplexes from bioreducible cationic polymers have a massive promise for cancer gene therapy. However, the feasibility of cationic polyurethanes for non-viral gene therapy is so far not well studied. In this work, a linear cationic polyurethane containing disulfide bonds, urethane linkages and protonable tertiary amino groups was successfully generated by stepwise polycondensation reaction between 2,2'-dithiodiethanol bis(p-nitrophenyl carbonate) and 1,4-bis(3-aminopropyl)piperazine (BAP). We confirmed that the cationic polyurethane (denoted as PUBAP) displayed superior gene delivery properties to its cationic polyamide analogue, thus causing higher in vitro transfection efficiency in MCF-7 and SKOV-3 cells. Besides, further folate-PEGylation and hydrophobic deoxycholic acid (DCA) conjugation to amino-containing PUBAP can be conducted to afford multifunctional polyurethane gene delivery system. After optimization, folate-decorated nano-polyplexes from the PUBAP conjugated with 8 folate-PEG chains and 12 DCA residues exhibited superb colloidal stability under physiological conditions, and performed rapid uptake via folate receptor-mediated endocytosis, efficient intracellular gene release and nucleus translocation into SKOV-3 cells in vitro and in vivo. Importantly, PUBAP based polyplexes possess low cytotoxicity as a result of PUBAP biodegradability. Therefore, marked growth inhibition of SKOV-3 tumor xenografted in Balb/c nude mice was achieved with negligible side effects on the mouse health after intravenous administration of PUBAP based polyplexes with a therapeutic plasmid encoding for TNF-related apoptosis-inducing ligand. This work provides a new insight into biomedical application of bio-responsive polyurethanes for cancer therapy. In this study, we have confirmed that disulfide-based cationic polyurethane presents a new non-viral vector for gene transfer and cancer gene therapy. The significance of this work includes: (1) design and synthesis of a group of novel disulfide-based cationic polyurethane by non-isocyanate chemistry; (2) comparative study of transfection activity between cationic polyurethanes and cationic polyamides; (3) feasibility of bioreducible cationic polyurethanes for in vivo cancer gene therapy. Copyright © 2015 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Sprick, Miriam; Fürst, Anton; Baschnagel, Fabio; Michel, Silvain; Piskoty, Gabor; Hartnack, Sonja; Jackson, Michelle A
2017-09-12
To evaluate the damage inflicted by an unshod hoof and by the various horseshoe materials (steel, aluminium and polyurethane) on the long bones of horses after a simulated kick. Sixty-four equine radii and tibiae were evaluated using a drop impact test setup. An impactor with a steel, aluminium, polyurethane, or hoof horn head was dropped onto prepared bones. An impactor velocity of 8 m/s was initially used with all four materials and then testing was repeated with a velocity of 12 m/s with the polyurethane and hoof horn heads. The impact process was analysed using a high-speed camera, and physical parameters, including peak contact force and impact duration, were calculated. At 8 m/s, the probability of a fracture was 75% for steel and 81% for aluminium, whereas polyurethane and hoof horn did not damage the bones. At 12 m/s, the probability of a fracture was 25% for polyurethane and 12.5% for hoof horn. The peak contact force and impact duration differed significantly between 'hard materials' (aluminium and steel) and 'soft materials' (polyurethane and hoof horn). The observed bone injuries were similar to those seen in analogous experimental studies carried out previously and comparable to clinical fracture cases suggesting that the simulated kick was realistic. The probability of fracture was significantly higher for steel and aluminium than for polyurethane and hoof horn, which suggests that the horseshoe material has a significant influence on the risk of injury for humans or horses kicked by a horse.
Lo Torto, Federico; Relucenti, Michela; Familiari, Giuseppe; Vaia, Nicola; Casella, Donato; Matassa, Roberto; Miglietta, Selenia; Marinozzi, Franco; Bini, Fabiano; Fratoddi, Ilaria; Sciubba, Fabio; Cassese, Raffaele; Tombolini, Vincenzo; Ribuffo, Diego
2018-05-17
The pathogenic mechanism underlying capsular contracture is still unknown. It is certainly a multifactorial process, resulting from human body reaction, biofilm activation, bacteremic seeding, or silicone exposure. The scope of the present article is to investigate the effect of hypofractionated radiotherapy protocol (2.66 Gy × 16 sessions) both on silicone and polyurethane breast implants. Silicone implants and polyurethane underwent irradiation according to a hypofractionated radiotherapy protocol for the treatment of breast cancer. After irradiation implant shells underwent mechanical, chemical, and microstructural evaluation by means of tensile testing, infrared spectra in attenuated total reflectance mode, nuclear magnetic resonance, and field emission scanning electron microscopy. At superficial analysis, irradiated silicone samples show several visible secondary and tertiary blebs. Polyurethane implants showed an open cell structure, which closely resembles a sponge. Morphological observation of struts from treated polyurethane sample shows a more compact structure, with significantly shorter and thicker struts compared with untreated sample. The infrared spectra in attenuated total reflectance mode spectra of irradiated and control samples were compared either for silicon and polyurethane samples. In the case of silicone-based membranes, treated and control specimens showed similar bands, with little differences in the treated one. Nuclear magnetic resonance spectra on the fraction soluble in CDCl3 support these observations. Tensile tests on silicone samples showed a softer behavior of the treated ones. Tensile tests on Polyurethane samples showed no significant differences. Polyurethane implants seem to be more resistant to radiotherapy damage, whereas silicone prosthesis showed more structural, mechanical, and chemical modifications.
Jung, Jae-A; Yoo, Ki-Hyun; Han, Seung-Kyu; Dhong, Eun-Sang; Kim, Woo-Kyung
2016-12-01
To demonstrate the efficacy of a highly hydrophilic polyurethane foam dressing in the treatment of diabetic ulcers. Diabetic foot ulcers often pose a difficult treatment problem. Polyurethane foam dressings have been used worldwide to accelerate wound healing, but only a few clinical studies demonstrate the effect of foam dressing on the healing of diabetic ulcers. Medical records of 1342 patients with diabetic ulcers who were admitted and treated at the authors' institution were reviewed. A total of 208 patients met the study's inclusion criteria. Of these 208 patients, 137 were treated with a highly hydrophilic polyurethane foam dressing, and 71 were treated with saline gauze (control group). Except for the application of polyurethane foam dressing, the treatment method was identical for patients in both groups. The wound healing outcomes of the 2 groups were compared. Complete wound healing occurred in 87 patients (63.5%) in the polyurethane foam dressing group and in 28 patients (39.4%) in the control group within 12 weeks (P < .05, X test). The mean percentage of wound area reduction in both groups was statistically significant (P < .05, Mann-Whitney U test). The mean time required for complete closure in patients who achieved complete healing within 12 weeks was 6.2 (SD, 3.4) weeks and 7.3 (SD, 2.6) weeks in the polyurethane foam dressing and control groups, respectively (P < .05, Mann-Whitney U test). These results indicate that the highly hydrophilic polyurethane foam dressing may provide an effective treatment strategy for diabetic foot ulcers.
Adhesive compositions and methods
DOE Office of Scientific and Technical Information (OSTI.GOV)
Allen, Scott D.; Sendijarevic, Vahid; O'Connor, James
The present invention encompasses polyurethane adhesive compositions comprising aliphatic polycarbonate chains. In one aspect, the present invention encompasses polyurethane adhesives derived from aliphatic polycarbonate polyols and polyisocyanates wherein the polyol chains contain a primary repeating unit having a structure:. In another aspect, the invention provides articles comprising the inventive polyurethane compositions as well as methods of making such compositions.
40 CFR 63.11416 - What are the standards for new and existing sources?
Code of Federal Regulations, 2010 CFR
2010-07-01
... polyurethane foam production affected source, you must meet the requirements in paragraph (b) of this section... in paragraph (d) of this section. If you own or operate a flexible polyurethane foam fabrication... a new or existing slabstock polyurethane foam production affected source, you must comply with the...
40 CFR 63.11416 - What are the standards for new and existing sources?
Code of Federal Regulations, 2013 CFR
2013-07-01
... polyurethane foam production affected source, you must meet the requirements in paragraph (b) of this section... in paragraph (d) of this section. If you own or operate a flexible polyurethane foam fabrication... a new or existing slabstock polyurethane foam production affected source, you must comply with the...
40 CFR 63.11416 - What are the standards for new and existing sources?
Code of Federal Regulations, 2014 CFR
2014-07-01
... polyurethane foam production affected source, you must meet the requirements in paragraph (b) of this section... in paragraph (d) of this section. If you own or operate a flexible polyurethane foam fabrication... a new or existing slabstock polyurethane foam production affected source, you must comply with the...
40 CFR 63.11416 - What are the standards for new and existing sources?
Code of Federal Regulations, 2011 CFR
2011-07-01
... polyurethane foam production affected source, you must meet the requirements in paragraph (b) of this section... in paragraph (d) of this section. If you own or operate a flexible polyurethane foam fabrication... a new or existing slabstock polyurethane foam production affected source, you must comply with the...
40 CFR 63.11416 - What are the standards for new and existing sources?
Code of Federal Regulations, 2012 CFR
2012-07-01
... polyurethane foam production affected source, you must meet the requirements in paragraph (b) of this section... in paragraph (d) of this section. If you own or operate a flexible polyurethane foam fabrication... a new or existing slabstock polyurethane foam production affected source, you must comply with the...
Zhou, Xing; Fang, Changqing; Lei, Wanqing; Du, Jie; Huang, Tingyi; Li, Yan; Cheng, Youliang
2016-01-01
Water plays important roles in organic reactions such as polyurethane synthesis, and the aqueous solution environment affects polymer morphology and other properties. This paper focuses on the morphology and surface properties of waterborne polyurethane resulting from the organic reaction in water involving different forms (solid and liquid), temperatures and aqueous solutions. We provide evidence from TEM observations that the appearance of polyurethane nanoparticles in aqueous solutions presents diverse forms, including imperfect spheres, perfect spheres, perfect and homogenous spheres and tubes. Based on the results on FTIR, GPC, AFM and XRD experiments, we suggest that the shape of the nanoparticles may be decided by the crimp degree (i.e., the degree of polyurethane chains intertangling in the water environment) and order degree, which are determined by the molecular weight (Mn) and hydrogen bonds. Meanwhile, solid water and high-temperature water can both reduce hard segments that gather on the polyurethane film surface to reduce hydrophilic groups and produce a soft surface. Our findings show that water may play key roles in aqueous polymer formation and bring order to molecular chains. PMID:27687001
Daemi, Hamed; Barikani, Mehdi; Barmar, Mohammad
2014-05-01
A number of different ionic aqueous polyurethane dispersions (PUDs) were synthesized based on NCO-terminated prepolymers. Two different anionic and cationic polyurethane samples were synthesized using dimethylol propionic acid and N-methyldiethanolamine emulsifiers, respectively. Then, proper amounts of PUDs and sodium alginate were mixed to obtain a number of aqueous polyurethane dispersions-sodium alginate (PUD/SA) elastomers. The chemical structure, thermal, morphological, thermo-mechanical and mechanical properties, and hydrophilicity content of the prepared samples were studied by FTIR, EDX, DSC, TGA, SEM, DMTA, tensile testing and contact angle techniques. The cationic polyurethanes and their blends with sodium alginate showed excellent miscibility and highly stretchable properties, while the samples containing anionic polyurethanes and alginate illustrated a poor compatibility and no significant miscibility. The morphology of alginate particles shifted from nanoparticles to microparticles by changing the nature of PUDs from cationic to anionic types. The final cationic elastomers not only showed better mechanical properties but also were formulated easier than anionic samples. Copyright © 2014 Elsevier B.V. All rights reserved.
2014-01-01
The work focuses on research related to determination of application possibility of new, ecofriendly boroorganic polyols in rigid polyurethane foams production. Polyols were obtained from hydroxypropyl urea derivatives esterified with boric acid and propylene carbonate. The influence of esterification type on properties of polyols and next on polyurethane foams properties was determined. Nitrogen and boron impacts on the foams' properties were discussed, for instance, on their physical, mechanical, and electric properties. Boron presence causes improvement of dimensional stability and thermal stability of polyurethane foams. They can be applied even at temperature 150°C. Unfortunately, introducing boron in polyurethanes foams affects deterioration of their water absorption, which increases as compared to the foams that do not contain boron. However, presence of both boron and nitrogen determines the decrease of the foams combustibility. Main impact on the decrease combustibility of the obtained foams has nitrogen presence, but in case of proper boron and nitrogen ratio their synergic activity on the combustibility decrease can be easily seen. PMID:24587721
Thermal Stability of Aqueous Polyurethanes Depending on the Applied Catalysts
Cakic, Suzana; Nikolic, Goran; Lacnjevac, Caslav; Gligoric, Miladin; Stamenkovic, Jakov; Rajkovic, Milos B.; Barac, Miroljub
2006-01-01
The thermal stability of aqueous polyurethanes has been measured applying the thermogravimetric analysis. The aqueous polyurethanes (aqPUR) with catalysts of different selectivity have been studied by use of the dynamic method. To obtain degradations of 0.025, 0.05, and 0.10, employing the dynamic method, the heating rates of 0.5, 1, 2, 5, and 10 °C min-1 have been used in the range of 30-500 °C. Using the more selective catalysts in the aqueous polyurethanes, the total resulting time of the decompositon has been on the increase at all degrees of the degradation and at the particular starting temperature. This paper shows that the dynamic method based on the thermogravimetric analysis can be used to assess the thermal stability of the aqueous polyurethanes using the catalysts of different selectivity.
Organically Modified Nanoclay-Reinforced Rigid Polyurethane Films
NASA Astrophysics Data System (ADS)
Park, Yong Tae; Qian, Yuqiang; Lindsay, Chris; Stein, Andreas; Macosko, Christopher
2012-02-01
The nanodispersion of vermiculite in polyurethanes was investigated to produce organoclay-reinforced rigid gas barrier films. Reducing gas transport can improve the insulation performance of closed cell polyurethane foam. In a previous study, the dispersion of vermiculite in polyurethanes without organic modification was not sufficient due to the non-uniform dispersion morphology. When vermiculite was modified by cation exchange with long-chain quaternary ammonium cations, the dispersion in methylene diphenyl diisocyanate (MDI) was significantly improved. Dispersion was improved by combining high intensity dispersive mixing with efficient distributive mixing. Polymerization conditions were also optimized in order to provide a high state of nanodispersion in the polyurethane nanocomposite. The dispersions were characterized using rheological, microscopic and scattering/diffraction techniques. The final nanocomposites showed enhancement of mechanical properties and reduction in permeability to carbon dioxide at low clay concentration (around 2 wt percent).
Method of making thermally removable polyurethanes
Loy, Douglas A.; Wheeler, David R.; McElhanon, James R.; Saunders, Randall S.; Durbin-Voss, Marvie Lou
2002-01-01
A method of making a thermally-removable polyurethane material by heating a mixture of a maleimide compound and a furan compound, and introducing alcohol and isocyanate functional groups, where the alcohol group and the isocyanate group reacts to form the urethane linkages and the furan compound and the maleimide compound react to form the thermally weak Diels-Alder adducts that are incorporated into the backbone of the urethane linkages during the formation of the polyurethane material at temperatures from above room temperature to less than approximately 90.degree. C. The polyurethane material can be easily removed within approximately an hour by heating to temperatures greater than approximately 90.degree. C. in a polar solvent. The polyurethane material can be used in protecting electronic components that may require subsequent removal of the solid material for component repair, modification or quality control.
Ramalingam, N; Prasanna, B Gowtham
2006-09-01
The impact of insoluble phosphorus such as aluminum and rock phosphate on alkaline phosphatase activity of polyurethane foam immobilized cyanobacteria was assessed. Polyurethane foam immobilized Nodularia recorded the highest alkaline phosphatase activity of 9.04 (m. mol p-nitrophenol released h(-1) mg(-1) protein) in vitro. A higher concentration of aluminum phosphate was recorded a 25% reduction in alkaline phosphatase activity, ammonia content, and available phosphorus in culture filtrate of polyurethane foam immobilized cyanobacteria. In general, immobilized cyanobacteria exhibited a higher alkaline phosphatase activity in rock phosphate than aluminum phosphate.
Neumann, Christopher N D; Bulach, Winfried D; Rehahn, Matthias; Klein, Roland
2011-09-01
This paper reports on the synthesis of a new highly reactive diisocyanate monomer based on hydroxymethylfurfural. It further describes its catalyst-free conversion to linear-chain thermoplastic polyurethanes as well as to cross-linked polyurethane foams. In addition, a novel strategy for the synthesis of polyurethane foams without the necessity of using water is developed. Nitrogen is utilized herein as blowing agent which is formed during Curtius rearrangement of a new furan based carboxylic azide into its corresponding diisocyanate. Copyright © 2011 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.
Stachelek, S J; Song, C; Alferiev, I; Defelice, S; Cui, X; Connolly, J M; Bianco, R W; Levy, R J
2004-01-01
The present study investigated a novel approach for gene therapy of heart valve disease and vascular disorders. We formulated and characterized implantable polyurethane films that could also function as gene delivery systems through the surface attachment of replication defective adenoviruses using an anti-adenovirus antibody tethering mechanism. Our hypothesis was that we could achieve site-specific gene delivery to cells interacting with these polyurethane implants, and thereby demonstrate the potential for intravascular devices that could also function as gene delivery platforms for therapeutic vectors. Previous research by our group has demonstrated that polyurethane elastomers can be derivatized post-polymerization through a series of chemical reactions activating the hard segment amide groups with alkyl bromine residues, which can enable a wide variety of subsequent chemical modifications. Furthermore, prior research by our group investigating gene delivery intravascular stents has shown that collagen-coated balloon expandable stents can be configured with anti-adenovirus antibodies via thiol-based chemistry, and can then tether adenoviral vectors at doses that lead to high levels of localized arterial neointima expression, but with virtually no distal spread of vector. Thus, we sought to create two-device configurations for our investigations building on this previous research. (1) Polyurethane films coated with Type I collagen were thiol activated to permit covalent attachment of anti-adenovirus antibodies to enable gene delivery via vector tethering. (2) We also formulated polyurethane films with direct covalent attachment of anti-adenovirus antibodies to polyurethane hard segments derivatized with alkyl-thiol groups, thereby also enabling tethering of replication-defective adenoviruses. Both formulations demonstrated highly localized and efficient transduction in cell culture studies with rat arterial smooth muscle cells. In vivo experiments with collagen-coated polyurethane films investigated an abdominal aorta implant model in pigs using a button configuration that simulated the blood contacting environment of a vascular graft. One week explants of the collagen-coated polyurethane films demonstrated 14.3+/-2.5% of neointimal cells on the surface of the implant transduced with green fluorescent protein - adenovirus (AdGFP) vector loadings of 1 x 10(8) PFU. PCR studies demonstrated no detectable vector DNA in blood or distal organs. Similarly, polyurethane films with direct attachment of antivector antibodies to the surface were used in sheep pulmonary valve leaflet replacement studies, simulating the blood contacting environment of a prosthetic heart valve cusp. Polyurethane films with antibody tethered AdGFP vector (10(8) PFU) demonstrated 25.1+/-5.7% of attached cells transduced in these 1 week studies, with no detectable vector DNA in blood or distal organs. In vivo GFP expression was confirmed with immunohistochemistry. It is concluded that site-specific intravascular delivery of adenoviral vectors for gene therapy can be achieved with polyurethane implants utilizing the antivector antibody tethering mechanism.
Added value of lignin as lignin-based hybrid polyurethane for a compatibilizing agent
NASA Astrophysics Data System (ADS)
Ilmiati, S.; Haris Mustafa, J.; Yaumal, A.; Hanum, F.; Chalid, M.
2017-07-01
As biomass-based material, lignin contains abundant hydroxyl groups promising to be used as chain extender in building hybrid polyurethanes. Consisting of polyehtylene glycol (PEG) content as hydrophobic part and lignin as hydrophilic part, the hybrid PU is expected to be as a novel compatibilizing agent in new materials production such as polyblends and composites. The hybrid PU was synthesized via two reaction stages, viz. pre-polyurethanization through reacting 4,4'-Methylenebis (Cyclohexyl Isocyanate) (HMDI) and PEG as polyol, and chain extention through adding lignin in the pre-polyurethanization system. The composition effect of lignin in hybrid PU syntehsis, to chemical structure corelated to hydrophobic to hydrophilic ratio, thermal and morphological properties, was evaluated by measuring NMR, FTIR, DSC, TGA and FE-SEM. The experiments showed that addition of lignin was able to extend the pre-polyurethane into hybrid polyurethane and to increase the lignin/polyol ratio in the hybrid polyurethanes, which were indicated by NMR and FTIR Analysis. And change of the ratio lead to increase the glass transition from 60.9 until 62.1°C and degradation temperature from 413.9 until 416.0°C. Observation of the morphology implied that addition of lignin gave more agglomerations. A Further investigation for this characterization study should be focused on a feasibility for this modified lignin as a novel compatibilizing agent.
Zhang, Taolin; Zhou, Xiaodong; Yang, Lizhong
2016-03-05
This work investigated experimentally and theoretically the fire hazards of thermal-insulation materials used in diesel locomotives under different radiation heat fluxes. Based on the experimental results, the critical heat flux for ignition was determined to be 6.15 kW/m² and 16.39 kW/m² for pure polyurethane and aluminum-polyurethane respectively. A theoretical model was established for both to predict the fire behaviors under different circumstances. The fire behavior of the materials was evaluated based on the flashover and the total heat release rate (HRR). The fire hazards levels were classified based on different experimental results. It was found that the fire resistance performance of aluminum-polyurethane is much better than that of pure-polyurethane under various external heat fluxes. The concentration of toxic pyrolysis volatiles generated from aluminum-polyurethane materials is much higher than that of pure polyurethane materials, especially when the heat flux is below 50 kW/m². The hazard index HI during peak width time was proposed based on the comprehensive impact of time and concentrations. The predicted HI in this model coincides with the existed N-gas and FED models which are generally used to evaluate the fire gas hazard in previous researches. The integrated model named HNF was proposed as well to estimate the fire hazards of materials by interpolation and weighted average calculation.
Mei, Tingzhen; Zhu, Yonghe; Ma, Tongcui; He, Tao; Li, Linjing; Wei, Chiju; Xu, Kaitian
2014-09-01
A series of alternating block polyurethanes (abbreviated as PULA-alt-PEG) and random block polyurethanes (abbreviated as PULA-ran-PEG) based on poly(L-lactic acid) (PLA) and poly(ethylene glycol) (PEG) were synthesized. The differences of PULA-alt/ran-PEG chemical structure, molecular weight, distribution, thermal properties, mechanical properties and static contact angle were systematically investigated. The PULA-alt/ran-PEG polyurethanes exhibited low T(g) (-47.3 ∼ -34.4°C), wide mechanical properties (stress σ(t): 4.6-32.6 MPa, modulus E: 11.4-323.9 MPa and strain ε: 468-1530%) and low water contact angle (35.4-51.4°). Scanning electron microscope (SEM) observation showed that PULA-alt-PEG film displays rougher and more patterned surface morphology than PULA-ran-PEG does, due to more regular structures of PULA-alt-PEG. Hydrolytic degradation shows that degradation rate of random block polyurethane series PULA-ran-PEG is higher than the alternating counterpart PULA-alt-PEG. PLA segment degradation is faster than urethane linkage and PEG segment almost does not degrade in the buffer solution. Platelet adhesion study showed that all the polyurethanes possess excellent hemocompatibility. The cell culture assay revealed that PULA-alt/ran-PEG polyurethanes were cell inert and unfavorable for the attachment of rat glial cell due to the hydrophilic characters of the materials. © 2013 Wiley Periodicals, Inc.
Santos, Thaisa B; Vieira, Angela A; Paula, Luciana O; Santos, Everton D; Radi, Polyana A; Khouri, Sônia; Maciel, Homero S; Pessoa, Rodrigo S; Vieira, Lucia
2017-04-01
Camphor was incorporated in diamond-like carbon (DLC) films to prevent the Candida albicans yeasts fouling on polyurethane substrates, which is a material commonly used for catheter manufacturing. The camphor:DLC and DLC film for this investigation was produced by plasma enhanced chemical vapor deposition (PECVD), using an apparatus based on the flash evaporation of organic liquid (hexane) containing diluted camphor for camphor:DLC and hexane/methane, mixture for DLC films. The film was deposited at a low temperature of less than 25°C. We obtained very adherent camphor:DLC and DLC films that accompanied the substrate flexibility without delamination. The adherence of camphor:DLC and DLC films on polyurethane segments were evaluated by scratching test and bending polyurethane segments at 180°. The polyurethane samples, with and without camphor:DLC and DLC films were characterized by Raman spectroscopy, scanning electron microscopy, atomic force microscopy, and optical profilometry. Candida albicans biofilm formation on polyurethane, with and without camphor:DLC and DLC, was assessed. The camphor:DLC and DLC films reduced the biofilm growth by 99.0% and 91.0% of Candida albicans, respectively, compared to bare polyurethane. These results open the doors to studies of functionalized DLC coatings with biofilm inhibition properties used in the production of catheters or other biomedical applications. Copyright © 2017 Elsevier Ltd. All rights reserved.
Degradability in vitro of polyurethanes based on synthetic atactic poly[(R,S)-3-hydroxybutyrate].
Brzeska, J; Janeczek, H; Janik, H; Kowalczuk, M; Rutkowska, M
2015-01-01
The aim of the present study was to determine the degradability of aliphatic polyurethanes, based on a different amount of synthetic, atactic poly[(R,S)-3-hydroxybutyrate] (a-PHB), in hydrolytic (phosphate buffer) and oxidative (H2O2/CoCl2) solutions. The soft segments were built with atactic poly[(R,S)-3-hydroxybutyrate] and polycaprolactone or polyoxytetramethylenediols, whereas hard segments were the reaction product of 4,4'-methylenedicyclohexyl diisocyanate and 1,4-butanediol.The selected properties - density and morphology of polymer surfaces - which could influence the sensitivity of polymers to degradation processes - were analyzed.The analysis of molecular mass (GPC), thermal properties (DSC) and the sample weight changes were undertaken to estimate the degree of degradability of polymer samples after incubation in environments studied.Investigated polyurethanes were amorphous with the very low amount of crystalline phases of hard segments.The polyurethane synthesized with a poly[(R,S)-3-hydroxybutyrate] and polyoxytetramethylenediol at a molar ratio of NCO:OH=3.7:1 (prepolymer step) appeared as the most sensitive for both degradative solutions. Its weight and molecular mass losses were the highest in comparison to other investigated polyurethanes.It could be expected that playing with the amount of poly[(R,S)-3-hydroxybutyrate] in polyurethane synthesis the rate of polyurethane degradation after immersion in living body would be modeled.
Zhang, Taolin; Zhou, Xiaodong; Yang, Lizhong
2016-01-01
This work investigated experimentally and theoretically the fire hazards of thermal-insulation materials used in diesel locomotives under different radiation heat fluxes. Based on the experimental results, the critical heat flux for ignition was determined to be 6.15 kW/m2 and 16.39 kW/m2 for pure polyurethane and aluminum-polyurethane respectively. A theoretical model was established for both to predict the fire behaviors under different circumstances. The fire behavior of the materials was evaluated based on the flashover and the total heat release rate (HRR). The fire hazards levels were classified based on different experimental results. It was found that the fire resistance performance of aluminum-polyurethane is much better than that of pure-polyurethane under various external heat fluxes. The concentration of toxic pyrolysis volatiles generated from aluminum-polyurethane materials is much higher than that of pure polyurethane materials, especially when the heat flux is below 50 kW/m2. The hazard index HI during peak width time was proposed based on the comprehensive impact of time and concentrations. The predicted HI in this model coincides with the existed N-gas and FED models which are generally used to evaluate the fire gas hazard in previous researches. The integrated model named HNF was proposed as well to estimate the fire hazards of materials by interpolation and weighted average calculation. PMID:28773295
Matiasek, J; Domig, K J; Djedovic, G; Babeluk, R; Assadian, O
2017-05-02
The aim of this study was to investigate the bacterial bioburden in experimental in vitro wounds during the application of conventional negative pressure wound therapy (NPWT), with and without antimicrobial dressings (polyhexanide, silver), against NPWT instillation of octenidine. Experimental wounds produced in an in vitro porcine wound model were homogenously contaminated with bacterial suspension and treated with NPWT and different options. Group A: non-antimicrobial polyurethane foam dressing; group B: antimicrobial polyurethane foam dressing containing silver; group C: antimicrobial gauze dressing containing polyhexanide; group D: non-antimicrobial polyurethane foam dressing intermittently irrigated with octenidine; group E: negative control (non-antimicrobial polyurethane foam dressing without NPWT). Standard biopsies were harvested after 24 and 28 hours. This study demonstrated that the use of NPWT with intermitted instillation of octenidine (group D) or application of silver-based polyurethane foam dressings (group B) is significantly superior against Staphylococcus aureus colonisation in experimental wounds compared with non-antimicrobial polyurethane foam dressing (group A) after 48 hours. Surprisingly, the polyhexanide-based dressing (group C) used in this model showed no statistical significant effect compared with the control group (group E) after 24 or 48 hours of treatment. Both intermitted instillation of octenidine and silver-based dressings in standard NPWT were significantly superior compared with non-antimicrobial polyurethane foam dressings or PHMB coated gauze dressing after 48 hours.
Defense Industrial Base Capabilities Study: Protection
2004-12-01
Polyurethane Foam (RPF). 2) The Department should establish an Industrial Base Investment Fund to provide better on-ramps for production-ready...Sweep; − Rigid Polyurethane Foam (RPF). RECOMMENDATION 2 The Department should establish an Industrial Base Investment Fund (IBIF) to provide...Reactive RF Jamming 15. Expendable Programmable Acoustic Decoy 16. Rigid Polyurethane Foam 17. Towed Fabric Balloon Pressure Sweep 18. Chemical
Philippart, François; Gaudry, Stéphane; Quinquis, Laurent; Lau, Nicolas; Ouanes, Islem; Touati, Samia; Nguyen, Jean Claude; Branger, Catherine; Faibis, Frédéric; Mastouri, Maha; Forceville, Xavier; Abroug, Fekri; Ricard, Jean Damien; Grabar, Sophie; Misset, Benoît
2015-03-15
The occurrence of ventilator-associated pneumonia (VAP) is linked to the aspiration of contaminated pharyngeal secretions around the endotracheal tube. Tubes with cuffs made of polyurethane rather than polyvinyl chloride or with a conical rather than a cylindrical shape increase tracheal sealing. To test whether using polyurethane and/or conical cuffs reduces tracheal colonization and VAP in patients with acute respiratory failure. We conducted a multicenter, prospective, open-label, randomized study in four parallel groups in four intensive care units between 2010 and 2012. A cohort of 621 patients with expected ventilation longer than 2 days was included at intubation with a cuff composed of cylindrical polyvinyl chloride (n = 148), cylindrical polyurethane (n = 143), conical polyvinyl chloride (n = 150), or conical polyurethane (n = 162). We used Kaplan-Meier estimates and log-rank tests to compare times to events. After excluding 17 patients who secondarily refused participation or had met an exclusion criterion, 604 were included in the intention-to-treat analysis. Cumulative tracheal colonization greater than 10(3) cfu/ml at Day 2 was as follows (median [interquartile range]): cylindrical polyvinyl chloride, 0.66 (0.58-0.74); cylindrical polyurethane, 0.61 (0.53-0.70); conical polyvinyl chloride, 0.67 (0.60-0.76); and conical polyurethane, 0.62 (0.55-0.70) (P = 0.55). VAP developed in 77 patients (14.4%), and postextubational stridor developed in 28 patients (6.4%) (P = 0.20 and 0.28 between groups, respectively). Among patients requiring mechanical ventilation, polyurethane and/or conically shaped cuffs were not superior to conventional cuffs in preventing tracheal colonization and VAP. Clinical trial registered with clinicaltrials.gov (NCT01114022).
Ferreira, A E R; Castro, B F M; Vieira, L C; Cassali, G D; Souza, C M; Fulgêncio, G O; Ayres, E; Oréfice, R L; Jorge, R; Silva-Cunha, A; Fialho, S L
2017-03-01
To evaluate the antiangiogenic activity of bevacizumab-loaded polyurethane using two animal models of neovascularization. The percentage of blood vessels was evaluated in a chicken chorioallantoic membrane model (n=42) and in the rabbit cornea (n=24) with neovascularization induced by alkali injury. In each model, the animals were randomly divided into the groups treated with the bevacizumab-loaded polyurethane device, phosphate-buffered-saline (negative control) and bevacizumab commercial solution (positive control). Clinical examination, as well as histopathological and immunohistochemical evaluation, were performed in the rabbit eyes. Microvascular density in hot spot areas was determined in semi-thin sections of corneal tissue by hematoxylin-eosin staining and factor VIII immunohistochemistry. Immunohistochemical analysis was also performed to evaluate VEGF expression. In the evaluated models, the use of bevacizumab (Avastin ® ) and the bevacizumab-loaded polyurethane device led to similar results with regard to inhibition of neovascularization. In the chorioallantoic membrane model, the bevacizumab-loaded polyurethane device reduced angiogenesis by 50.27% when compared to the negative control group. In the rabbit model of corneal neovascularization, the mean density of vessels/field was reduced by 46.87% on analysis of factor VIII immunohistochemistry photos in the bevacizumab-loaded polyurethane device group as compared to the negative control (PBS) sections. In both models, no significant difference could be identified between the bevacizumab-loaded polyurethane device and the positive control group, leading to similar results with regard to inhibition of neovascularization. The present study shows that the bevacizumab-loaded polyurethane device may release bevacizumab and inhibit neovascularization similarly to commercial bevacizumab solution in the short-term. Copyright © 2017 Elsevier Masson SAS. All rights reserved.
Duxbury, Paula J; Harvey, James R
2016-04-01
Silicone gel implants are used worldwide for breast augmentation and breast reconstruction. Textured silicone implants are the most commonly placed implant, but polyurethane-coated implants are increasingly being used in an attempt to ameliorate the long-term complications associated with implant insertion. This systematic review was conducted according to the Preferred Reporting Items for Systematic Reviews and Meta-analyses guidelines. Electronic searches of MEDLINE, EMBASE, the Cochrane Library and www.ClinicalTrials.gov were undertaken in March 2014 using keywords. Following data extraction, 18 studies were included in the review, including four core studies of textured silicone implants and five studies reporting outcomes for polyurethane-coated silicone implants. There are no clear data reporting revision rates in patients treated with polyurethane implants. In the primary reconstructive setting, capsular contracture rates with silicone implants are 10-15% at 6 years, whilst studies of polyurethane implants report rates of 1.8-3.4%. In the primary augmentation setting, core studies show a capsular contracture rate of 2-15% at 6 years compared with 0.4-1% in polyurethane-coated implants; however, the polyurethane studies are limited by their design and poor follow-up. The use of polyurethane implants should be considered a safe alternative to textured silicone implants. It is likely that an implant surface does influence short- and long-term outcomes; however, the extent of any benefit cannot be determined from the available evidence base. Future implant studies should target the short- and long-term benefits of implant surfacing by procedure with defined outcome measures; a head-to-head comparison would help clarify outcomes. Copyright © 2016 British Association of Plastic, Reconstructive and Aesthetic Surgeons. Published by Elsevier Ltd. All rights reserved.
Zhuang, Yan; Zhang, Qian; Feng, Jinqi; Wang, Na; Xu, Weilin; Yang, Hongjun
2017-04-01
Naturally derived fibers such as silk fibroin can potentially enhance the biocompatibility of currently used biomaterials. This study investigated the physical properties of native silk fibroin powder and its effect on the biocompatibility of biomedical polyurethane. Native silk fibroin powder with an average diameter of 3 µm was prepared on a purpose-built machine. A simple method of phase inversion was used to produce biomedical polyurethane/native silk fibroin powder hybrid membranes at different blend ratios by immersing a biomedical polyurethane/native silk fibroin powder solution in deionized water at room temperature. The physical properties of the membranes including morphology, hydrophilicity, roughness, porosity, and compressive modulus were characterized, and in vitro biocompatibility was evaluated by seeding the human umbilical vein endothelial cells on the top surface. Native silk fibroin powder had a concentration-dependent effect on the number and morphology of human umbilical vein endothelial cells growing on the membranes; cell number increased as native silk fibroin powder content in the biomedical polyurethane/native silk fibroin powder hybrid membrane was increased from 0% to 50%, and cell morphology changed from spindle-shaped to cobblestone-like as the native silk fibroin powder content was increased from 0% to 70%. The latter change was related to the physical characteristics of the membrane, including hydrophilicity, roughness, and mechanical properties. The in vivo biocompatibility of the native silk fibroin powder-modified biomedical polyurethane membrane was evaluated in a rat model; the histological analysis revealed no systemic toxicity. These results indicate that the biomedical polyurethane/native silk fibroin powder hybrid membrane has superior in vitro and in vivo biocompatibility relative to 100% biomedical polyurethane membranes and thus has potential applications in the fabrication of small-diameter vascular grafts and in tissue engineering.
Chang, Ching-Hsien; Liu, Hsia-Wei; Huang, Ching-Cheng
2014-01-01
A series of designed drug-release systems were prepared and established for clear moisture healing. These systems were designed to have an interpenetrating polymer network (IPN) structure, which contained a breathable polyurethane film, hydrocolloidlayer, and polyacrylate adhesive layer. Breathable polyurethane film (2000 g/m(2)/24 hr) with high moisture permeability was employed as a base for new drug-release systems or wound dressings. All drug-release systems having a polyurethane film-backed hydrocolloid acrylated adhesive layer showed an increase of water uptakes with increasing time. After 114 hours, high water uptakes of drug-release systems with 20% hydrocolloid components were observed in the values of 160, 1100, and 1870% for different additional hydrocolloid components of carboxymethylcellulose, sodium alginate, and carbomer U10, respectively. New drug-release systems of polyurethane film-backed hydrocolloid/adhesive layers could be designed and established for wound care managements.
Fast-responding bio-based shape memory thermoplastic polyurethanes
DOE Office of Scientific and Technical Information (OSTI.GOV)
Petrovic, Zoran S.; Milic, Jelena; Zhang, Fan
Fast response shape-memory polyurethanes were prepared from bio-based polyols, diphenyl methane diisocyanate and butane diol. The bio-based polyester polyols were synthesized from 9-hydroxynonanoic acid, a product obtained by ozonolysis of fatty acids extracted from soy oil and castor oil. The morphology of polyurethanes was investigated by synchrotron ultra-small angle X-ray scattering, which revealed the inter-domain spacing between the hard and soft phases, the degree of phase separation, and the level of intermixing between the hard and soft phases. We also conducted thorough investigations of the thermal, mechanical, and dielectric properties of the polyurethanes, and found that high crystallization rate ofmore » the soft segment gives these polyurethanes unique properties suitable for shapememory applications, such as adjustable transition temperatures, high degree of elastic elongations, and good mechanical strength. In conclusion, these materials are also potentially biodegradable and biocompatible, therefore suitable for biomedical and environmental applications.« less
Fast-responding bio-based shape memory thermoplastic polyurethanes
Petrovic, Zoran S.; Milic, Jelena; Zhang, Fan; ...
2017-05-31
Fast response shape-memory polyurethanes were prepared from bio-based polyols, diphenyl methane diisocyanate and butane diol. The bio-based polyester polyols were synthesized from 9-hydroxynonanoic acid, a product obtained by ozonolysis of fatty acids extracted from soy oil and castor oil. The morphology of polyurethanes was investigated by synchrotron ultra-small angle X-ray scattering, which revealed the inter-domain spacing between the hard and soft phases, the degree of phase separation, and the level of intermixing between the hard and soft phases. We also conducted thorough investigations of the thermal, mechanical, and dielectric properties of the polyurethanes, and found that high crystallization rate ofmore » the soft segment gives these polyurethanes unique properties suitable for shapememory applications, such as adjustable transition temperatures, high degree of elastic elongations, and good mechanical strength. In conclusion, these materials are also potentially biodegradable and biocompatible, therefore suitable for biomedical and environmental applications.« less
Fast-Responding Bio-Based Shape Memory Thermoplastic Polyurethanes.
Petrović, Zoran S; Milić, Jelena; Zhang, Fan; Ilavsky, Jan
2017-07-14
Novel fast response shape-memory polyurethanes were prepared from bio-based polyols, diphenyl methane diisocyanate and butane diol for the first time. The bio-based polyester polyols were synthesized from 9-hydroxynonanoic acid, a product obtained by ozonolysis of fatty acids extracted from soy oil and castor oil. The morphology of polyurethanes was investigated by synchrotron ultra-small angle X-ray scattering, which revealed the inter-domain spacing between the hard and soft phases, the degree of phase separation, and the level of intermixing between the hard and soft phases. We also conducted thorough investigations of the thermal, mechanical, and dielectric properties of the polyurethanes, and found that high crystallization rate of the soft segment gives these polyurethanes unique properties suitable for shape-memory applications, such as adjustable transition temperatures, high degree of elastic elongations, and good mechanical strength. These materials are also potentially biodegradable and biocompatible, therefore suitable for biomedical and environmental applications.
In vitro analysis of polyurethane foam as a topical hemostatic agent.
Broekema, Ferdinand I; van Oeveren, Wim; Zuidema, Johan; Visscher, Susan H; Bos, Rudolf R M
2011-04-01
Topical hemostatic agents can be used to treat problematic bleedings in patients who undergo surgery. Widely used are the collagen- and gelatin-based hemostats. This study aimed to develop a fully synthetic, biodegradable hemostatic agent to avoid exposure to animal antigens. In this in vitro study the suitability of different newly developed polyurethane-based foams as a hemostatic agent has been evaluated and compared to commonly used agents. An experimental in vitro test model was used in which human blood flowed through the test material. Different modified polyurethane foams were compared to collagen and gelatin. The best coagulation was achieved with collagen. The results of the polyurethane foam improved significantly by increasing the amount of polyethylene glycol. Therefore, the increase of the PEG concentration seems a promising approach. Additional in vivo studies will have to be implemented to assess the application of polyurethane foam as a topical hemostatic agent.
Investigation of Shock Wave Attenuation in Porous Materials
2009-12-01
Foam ...... 38 Table 4. Summary of Material Characteristics of Polyurethane Foams ............ 40 Table 5. Summary of Experiment Results...polyurethane foam , he performed a simple symmetric impact simulation to investigate the material properties and wave propagation characteristics of the...describes the characteristics of the two foam materials studied in this research, namely the aluminum metal foam and rigid polyurethane foam , which
Flame retardant spandex type polyurethanes
NASA Technical Reports Server (NTRS)
Howarth, J. T.; Sheth, S.; Sidman, K. R.; Massucco, A. A. (Inventor)
1978-01-01
Flame retardant elastomeric compositions were developed, comprised of: (1) spandex type polyurethane having incorporated into the polymer chain, halogen containing polyols; (2) conventional spandex type polyurethanes in physical admixture flame retardant additives; and (3) fluoroelastomeric resins in physical admixture with flame retardant additives. Methods of preparing fibers of the flame retardant elastomeric materials are presented and articles of manufacture comprised of the elastomeric materials are mentioned.
Zhifeng Zheng; Hui Pan; Yuanbo Huang; Chung Y. Hse
2011-01-01
Rigid polyurethane foams were prepared from the liquefied wood polyols, which was obtained by the liquefaction of southern pine wood in the presence of polyhydric alcohols with sulfuric acid catalyst by using microwave-assistant as an energy source. The properties of liquefied biomass-based polyols and the rigid polyurethane foams were investigated. The results...
Damage Caused to Polyurethane Foams by Aging, Simulated Sunlight Exposure, Heat and Fire
1984-07-01
vented configuration ............ .................. 11 4 Sample of the tan-colored solid formed upon pyrolysis of blue foam ..... .............. .. 21...54 26 Infrared absorption spectrum of the solid, tan-colored pyrolysis product formed from blue polyurethane foam ..... .............. .. 55 27...Infrared absorption spectrum of the liquid, brown-colored pyrolysis product formed from blue polyurethane foam ..... .............. .. 56 28 Fuel vent
Thermal behaviour properties and corrosion resistance of organoclay/polyurethane film
NASA Astrophysics Data System (ADS)
Kurniawan, O.; Soegijono, B.
2018-03-01
Organoclay/polyurethane film composite was prepared by adding organoclay with different content (1, 3, and 5 wt.%) in polyurethane as a matrix. TGA and DSC showed decomposition temperature shifted to a lower point as organoclay content change. FT-IR spectra showed chemical bonding of organoclay and polyurethane as a matrix, which means that the bonding between filler and matrix occured and the composite was stronger but less bonding occur in composite with 5 wt.% organoclay. The corrosion resistance overall increased with the increasing organoclay content. Composite with 5 wt.% organoclay had more thermal stability and corrosion resistance may probably due to exfoliation of organoclay.
Preparation and Characterization of Soybean Oil-Based Polyurethanes for Digital Doming Applications
Pantone, Vincenzo; Laurenza, Amelita Grazia; Annese, Cosimo; Fracassi, Francesco; Fini, Paola; Nacci, Angelo; Russo, Antonella; Fusco, Caterina
2017-01-01
Polyurethane-resin doming is currently one of the fastest growing markets in the field of industrial graphics and product identification. Semi-rigid bio-based polyurethanes were prepared deriving from soybean oil as a valuable alternative to fossil materials for digital doming and applied to digital mosaic technology. Bio-resins produced can favorably compete with the analogous fossil polymers, giving high-quality surface coatings (ascertained by SEM analyses). In addition, polyurethane synthesis was accomplished by using a mercury- and tin-free catalyst (the commercially available zinc derivative K22) bringing significant benefits in terms of cost efficiency and eco-sustainability. PMID:28773208
NASA Astrophysics Data System (ADS)
Setyowati, Erni; Hardiman, Gagoek; Purwanto
2018-02-01
This research aims to determine the acoustical properties of concrete material made of polyurethane and oyster shell waste as both fine aggregate and coarse aggregate comparing to other concrete mortar. Architecture needs aesthetics materials, so the innovation in architectural material should be driven through the efforts of research on materials for building designs. The DOE methods was used by mixing cement, oyster shell, sands, and polyurethane by composition of 160 ml:40 ml:100 ml: 120 ml respectively. Refer to the results of previous research, then cement consumption is reduced up to 20% to keep the concept of green material. This study compared three different compositions of mortars, namely portland cement concrete with gravel (PCG), polyurethane concrete of oyster shell (PCO) and concrete with plastics aggregate (PCP). The methods of acoustical tests were conducted refer to the ASTM E413-04 standard. The research results showed that polyurethane concrete with oyster shell waste aggregate has absorption coefficient 0.52 and STL 63 dB and has a more beautiful appearance when it was pressed into moulding. It can be concluded that polyurethane concrete with oyster shell aggregate (PCO) is well implemented in architectural acoustics-components.
IFATS Collection: Adipose-Derived Stromal Cells Improve the Foreign Body Response
Prichard, Heather L.; Reichert, William; Klitzman, Bruce
2015-01-01
Many implanted devices fail due to the formation of an avascular capsule surrounding the device. Additionally, fat has long been known to promote healing and vascularization. The goals of this study were to identify potential mechanisms of the provascular actions of adipose-derived stromal cells (ASCs) and to improve implant biocompatibility. First, adult ASCs and fibroblasts from rats were attached to polyurethane and polystyrene in vitro and their cytokine secretion profile was analyzed. Secretion of vascular endothelial growth factor (VEGF) from ASCs was 10 –70 times higher than fibroblasts after 3 and 6 days. Next, polyurethane, bare and with cellular coatings, was implanted subcutaneously in rats. The fibrous capsule surrounding bare polyurethane implants was 17%–32% thicker and the amount of collagen was 27% greater than the capsule surrounding ASC-coated implants. Finally, the microvessel density adjacent to ASC-coated polyurethane was approximately 50%–80% higher than bare polyurethane. In summary, ASCs attached to polyurethane have a dramatically increased VEGF production compared with fibroblasts in vitro, and these cells also produce an increased microvessel density in the surrounding tissue when implanted subcutaneously in rats. PMID:18436858
Miller, Melissa A; Arndt, Jennifer L; Konkle, Mark A; Chenoweth, Carol E; Iwashyna, Theodore J; Flaherty, Kevin R; Hyzy, Robert C
2011-06-01
The aim of this study was to determine whether the use of a polyurethane-cuffed endotracheal tube would result in a decrease in ventilator-associated pneumonia rate. We replaced conventional endotracheal tube with a polyurethane-cuff endotracheal tube (Microcuff, Kimberly-Clark Corporation, Rosewell, Ga) in all adult mechanically ventilated patients throughout our large academic hospital from July 2007 to June 2008. We retrospectively compared the rates of ventilator-associated pneumonia before, during, and after the intervention year by interrupted time-series analysis. Ventilator-associated pneumonia rates decreased from 5.3 per 1000 ventilator days before the use of the polyurethane-cuffed endotracheal tube to 2.8 per 1000 ventilator days during the intervention year (P = .0138). During the first 3 months after return to conventional tubes, the rate of ventilator-associated pneumonia was 3.5/1000 ventilator days. Use of the polyurethane-cuffed endotracheal tube was associated with an incidence risk ratio of ventilator-associated pneumonia of 0.572 (95% confidence interval, 0.340-0.963). In statistical regression analysis controlling for other possible alterations in the hospital environment, as measured by rate of tracheostomy-ventilator-associated pneumonia, the incidence risk ratio of ventilator-associated pneumonia in patients intubated with polyurethane-cuffed endotracheal tube was 0.565 (P = .032; 95% confidence interval, 0.335-0.953). Use of a polyurethane-cuffed endotracheal tube was associated with a significant decrease in the rate of ventilator-associated pneumonia in our study. Copyright © 2011 Elsevier Inc. All rights reserved.
González-García, Dulce M; Téllez Jurado, L; Jiménez-Gallegos, R; Rodríguez-Lorenzo, Luis M
2017-06-01
Titanium compounds have demonstrated great interfacial properties with biological tissues whereas a wide variety of polyurethanes have also been successfully probed in medical applications. However, studies about hybrids based on polyurethanes/TiO 2 for medical applications are scarce. The aim of this work is to design novel biodegradable hybrid materials based on polyurethanes/TiO 2 (80% organic-20% inorganic) and to perform a preliminary study of the potential applications in bone regeneration. The hybrids have been prepared by a sol-gel reaction using titanium isopropoxide as precursor of the inorganic component and polyurethane as the organic one. A series of polyurethanes has been prepared using different polyesters glycol succinate as soft segment, and 1,6-diisocyanatohexane (HDI) and butanediol (BD) as linear hard segment. The spectroscopy techniques used allow to confirm the formation of the required polyurethanes by the identification of bands related to carboxylic groups (COOH), and the amine groups (NH), and also the TiOH bonds and the bonds related to the interconnected network between the inorganic and the organic components from hybrids. The results from SEM/EDS show a homogeneous distribution of the inorganic component into the organic matrix. The nontoxic character of the hybrid (H400) was probed using MG-63 cell line with over 90% of cell viability. Finally, the formation of a hydroxyapatite layer in the material surface after 21days of soaking in SBF shows the bioactive character. Copyright © 2017 Elsevier B.V. All rights reserved.
Li, Linjing; Liu, Xiangyu; Niu, Yuqing; Ye, Jianfu; Huang, Shuiwen; Liu, Chao; Xu, Kaitian
2017-07-01
Alternating block polyurethanes (abbreviated as PULA-alt-PEG) and random block polyurethanes (abbreviated as PULA-ran-PEG) based on biodegradable poly(lactic acid) (PLA) and poly(ethylene glycol) (PEG) were prepared. Results showed that alternating block polyurethane gives higher crystal degree, higher mechanical properties, more patterned and rougher surface than the random counterpart, due to the regular and controlled structure. Water absorptions of the polyurethanes were in the range of 620 to 780%. Cytocompatibility of the amphiphilic block polyurethanes (PU) (water static angle 41.4°-61.8°) was assessed by CCK-8 assay using human embryonic kidney (HEK293) cells. Wound healing evaluation of the PU foam scaffolds was carried out by full-thickness SD rat model experiment, with medical gauze as control. It was found that the skin of rat in PU groups was fully covered with new epithelium without any significant adverse reactions and PU dressings give much rapid and better healing than medical gauze. Histological examination revealed that PU dressings suppress the infiltration of inflammatory cells and accelerate fibroblast proliferation. It was also demonstrated that PULA-alt-PEG exhibits obvious better healing effect than PULA-ran-PEG does. This study has demonstrated that without further modification, plain alternating block polyurethane scaffold would help wound recovery efficiently. © 2016 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 105B: 1200-1209, 2017. © 2016 Wiley Periodicals, Inc.
Patients’ satisfaction with anatomic polyurethane implants
2017-01-01
This paper presents patients satisfaction using anatomical polyurethane breast implants. We performed surgery on 525 patients, 370 of which were primary and 155 were secondary to various causes such as capsular contracture, ruptured implants, volume changes, and incorrect positioning of the implant. The advantages of silicone polyurethane covers shown high level of patient satisfaction, low incidence of capsular contracture, and absence of implant rotation, and late seroma. PMID:28497022
Federal Register 2010, 2011, 2012, 2013, 2014
2010-04-12
... assemblies in the ECS with burned Boeing Material Specification (BMS) 8-39 polyurethane foam insulation. This... duct assemblies in the ECS wrapped with BMS 8-39 polyurethane foam insulation, a material of which the... electrical arc from igniting the BMS 8-39 polyurethane foam insulation on the duct assemblies of the ECS...
Studies on polyurethane adhesives and surface modification of hydrophobic substrates
NASA Astrophysics Data System (ADS)
Krishnamoorthy, Jayaraman
This thesis work deals with (a) Curing of reactive, hot-melt polyurethane adhesives and (b) Adsorption studies using different interactions. Research on polyurethanes involves characterization of polyurethane prepolymers and a novel mechanism to cure isocyanate-terminated polyurethane prepolymer by a "trigger" mechanism. Curing of isocyanate-terminated polyurethane prepolymers has been shown to be influenced by morphology and environmental conditions such as temperature and relative humidity. Although the initial composition, final morphology and curing kinetics are known, information regarding the intermediate prepolymer mixture is yet to be established. Polyurethane prepolymers prepared by the reaction of diisocyanates with the primary hydroxyls of polyester diol (PHMA) and secondary hydroxyls of polyether diol (PPG) were characterized. The morphology and crystallization kinetics of a polyurethane prepolymer was compared with a blend of PPG prepolymer (the product obtained by the reaction of PPG with diisocyanate) and a PHMA prepolymer (the product obtained by the reaction of PHMA with diisocyanate) to study the effect of copolymer formed in the polyurethane prepolymer on the above-mentioned properties. Although the morphology of the polyurethane prepolymer is determined in the first few minutes of application, the chemical curing of isocyanate-terminated prepolymer occurs over hours to days. In the literature, different techniques are described to follow the curing kinetics. But there is no established technique to control the curing of polyurethane prepolymer. To make the curing process independent of environmental factors, a novel approach using a trigger mechanism was designed and implemented by using ammonium salts as curing agents. Ammonium salts that are stable at room temperature but decompose on heating to yield active hydrogen-containing compounds, NH3 and H2O, were used as 'Trojan horses' to cure the prepolymer chemically. Research on adsorption studies involved making functionalized, thickness-controlled, wettability-controlled multilayers on hydrophobic substrates and the adsorption of carboxylic acid-terminated poly(styrene-b-isoprene) on alumina/silica substrates. Poly(vinyl alcohol) has been shown to adsorb onto hydrophobic surfaces irreversibly due to hydrophobic interactions. This thin semicrystalline coating is chemically modified using acid chlorides, butyl isocyanate and butanal to form thicker and hydrophobic coatings. The products of the modification reactions allow adsorption of a subsequent layer of poly(vinyl alcohol) that could subsequently be hydrophobized. This 2-step (adsorption/chemical modification) allows layer-by-layer deposition to prepare coatings with thickness, chemical structure and wettability control on any hydrophobic surface. Research on adsorption characteristics of carboxylic acid-terminated poly(styrene-b-isoprene) involved syntheses of block copolymers with the functional group present at specific ends. Comparative adsorption studies for carboxylic acid-terminated and hydrogen-terminated block copolymers was carried out on alumina and silica substrates.
Influences of the Ratio of Polyol and MDI on the Acoustic Parameters of Polyurethane
NASA Astrophysics Data System (ADS)
Wang, Yonghua; Liu, Zheming; Wu, Haiquan; Zhang, Chengchun; Yu, Huadong; Ren, Luquan; Ichchou, Mohamed
2018-05-01
In this paper, the influence of different ratio of polyol and MDI on the absorption coefficient and acoustic parameters of polyurethane was studied. Ratio of 100:40 and 100:45 show the best sound absorption performance, and the change trend of transmission loss and sound absorption coefficient are opposite. The flow resistance increased with the increasing of the ratio of polyol and MDI, the greater the flow resistance, the worse the high frequency sound absorption property of the polyurethane. When the ratio of polyol and MDI keep 100:45, the minimum porosity of sample, the polyurethane porosity increase with the ratio of polyol and MDI increase.
Condom makers jockey for position in barrier warfare.
1995-01-01
U.S. condom manufacturers are receiving competition from high quality Japanese products. However, the sale of a plastic polyurethane condom by U.S. manufacturer, London International, could potentially outsell Japanese ultra-thin condoms. The polyurethane products can be made at a uniform thinness, resulting in a more sensitive condom. Industry analysts are not sure about the impact of a plastic condom. Some feel that even if they prove to be safer than latex condoms, polyurethane condoms will have a difficult time competing against established brands. Others feel that if consumer response is positive, the potential profits provide a strong incentive for companies to invest in the efficacy studies and marketing of a polyurethane product.
Molecular dynamics studies of polyurethane nanocomposite hydrogels
NASA Astrophysics Data System (ADS)
Strankowska, J.; Piszczyk, Ł.; Strankowski, M.; Danowska, M.; Szutkowski, K.; Jurga, S.; Kwela, J.
2013-10-01
Polyurethane PEO-based hydrogels have a broad range of biomedical applicability. They are attractive for drug-controlled delivery systems, surgical implants and wound healing dressings. In this study, a PEO based polyurethane hydrogels containing Cloisite® 30B, an organically modified clay mineral, was synthesized. Structure of nanocomposite hydrogels was determined using XRD technique. Its molecular dynamics was studied by means of NMR spectroscopy, DMA and DSC analysis. The mechanical properties and thermal stability of the systems were improved by incorporation of clay and controlled by varying the clay content in polymeric matrix. Molecular dynamics of polymer chains depends on interaction of Cloisite® 30B nanoparticles with soft segments of polyurethanes. The characteristic nanosize effect is observed.
[Cost-effectiveness of a TLC-NOSF polyurethane foam dressing].
Arroyo Ana, Abejón; Alvarez Vázquez, Juan Carlos; Blasco García, Carmen; Bermejo Martínez, Mariano; López Casanova, Pablo; Cuesta Cuesta, Juan José; De Haro Fernández, Francisco; Mateo Marín, Emilia; Segovia Gómez, Teresa; Villar Rojas, Antonio Erasto
2012-11-01
Chronic wounds represent a drain on the Spanish health system, nowdays is necessary an optimization of the resources used and that is for this that is necessary justify the use of the products over others through cost-effective studies for to show the economic benefit to professionals and the life quality of patient. This article compares the use of a new technology for format polyurethane foam, TLC-NOSF, with the most commonly used products for treating wounds. This comparison is made using a cost-effectiveness model (Markov Model). The results demonstrate that treatment with polyurethane foam dressing with TLC-NOSF are cost-effective versus treatments with polyurethane foams most commonly used in Spain.
Degradation of pentachlorophenol by polyurethane-immobilized Flavobacterium cells.
O'Reilly, K T; Crawford, R L
1989-01-01
Polyurethane-immobilized Flavobacterium cells (ATCC 39723) degraded pentachlorophenol (PCP) at initial concentrations as high as 300 mg liter-1. The reversible binding of PCP to the polyurethane was shown to be important in the protection of the cells from inhibition of PCP degradation. The degradation activity of the bacteria was monitored for 150 days in semicontinuous batch reactors. The degradation rate dropped by about 0.6% per day. PCP was degraded in a continuous-culture bioreactor at a rate of 3.5 to 4 mg g of foam-1 day-1 for 25 days. Electron micrographs of the polyurethane suggested that the cells were entrapped within 50- to 500-microns-diameter pockets in the foam. PMID:2508552
Time-dependent crashworthiness of polyurethane foam
NASA Astrophysics Data System (ADS)
Basit, Munshi Mahbubul; Cheon, Seong Sik
2018-05-01
Time-dependent stress-strain relationship as well as crashworthiness of polyurethane foam was investigated under constant impact energy with different velocities, considering inertia and strain-rate effects simultaneously during the impact testing. Even though the impact energies were same, the percentage in increase in densification strain due to higher impact velocities was found, which yielded the wider plateau region, i.e. growth in crashworthiness. This phenomenon is analyzed by the microstructure of polyurethane foam obtained from scanning electron microscopy. The equations, coupled with the Sherwood-Frost model and the impulse-momentum theory, were employed to build the constitutive equation of the polyurethane foam and calculate energy absorption capacity of the foam. The nominal stress-strain curves obtained from the constitutive equation were compared with results from impact tests and were found to be in good agreement. This study is dedicated to guiding designer use polyurethane foam in crashworthiness structures such as an automotive bumper system by providing crashworthiness data, determining the crush mode, and addressing a mathematical model of the crashworthiness.
Asefnejad, Azadeh; Khorasani, Mohammad Taghi; Behnamghader, Aliasghar; Farsadzadeh, Babak; Bonakdar, Shahin
2011-01-01
Background Biodegradable polyurethanes have found widespread use in soft tissue engineering due to their suitable mechanical properties and biocompatibility. Methods In this study, polyurethane samples were synthesized from polycaprolactone, hexamethylene diisocyanate, and a copolymer of 1,4-butanediol as a chain extender. Polyurethane scaffolds were fabricated by a combination of liquid–liquid phase separation and salt leaching techniques. The effect of the NCO:OH ratio on porosity content and pore morphology was investigated. Results Scanning electron micrographs demonstrated that the scaffolds had a regular distribution of interconnected pores, with pore diameters of 50–300 μm, and porosities of 64%–83%. It was observed that, by increasing the NCO:OH ratio, the average pore size, compressive strength, and compressive modulus increased. L929 fibroblast and chondrocytes were cultured on the scaffolds, and all samples exhibited suitable cell attachment and growth, with a high level of biocompatibility. Conclusion These biodegradable polyurethane scaffolds demonstrate potential for soft tissue engineering applications. PMID:22072874
Low-Temperature Flex Durability of Fabrics for Polar Sleds
2014-10-06
friction owing to solar gain, so SPoT is systematically replacing older tan bladders with black ones constructed from similar polyurethane -coated...specimens of the existing bladder material (single-layer polyurethane - coated fabric) within a few cycles. Remarkably, the specimens could with- stand...fabrics: • Antarctic traverses should continue to use fuel bladders constructed from ATL-853C (black) polyurethane -coated fabric as supplied by Aero Tec
NASA Astrophysics Data System (ADS)
Yakushin, V. A.; Stirna, U. K.; Zhmud', N. P.
1999-09-01
The dependence of physical and mechanical properties of monolithic and foamed rigid polyurethanes on the content of flame retardants was investigated at 293 and 98 K. The character of the influence of the content of trichloroethyl phosphate on the ultimate tensile elongation and the coefficient of linear thermal expansion for monolithic and foamed polyurethanes at a temperature of 98 K was established.
Chennell, Philip; Feschet-Chassot, Emmanuelle; Sautou, Valérie; Mailhot-Jensen, Bénédicte
2018-05-01
Thermoplastic polyurethanes are widely used in medical devices. In order to limit some of their shortfalls, like microbial attachment, surfaces modifications can be required. In this work, a two-step replication method was used to create ordered macroporous and mesoporous thermoplastic polyurethane surfaces using anodic aluminum oxide as master template. The intermediate mould materials that were tested were polystyrene and a polyacrylate resin with inorganic filler. All obtained surfaces were characterized by scanning electron microscopy. The initial anodic aluminum oxide surfaces possessed macro or mesopores, function of anodization conditions. The intermediate mould structure correctly replicated the pattern, but the polystyrene surface structures (pillars) were less resistant than the polyacrylate resin ones. The thermoplastic polyurethane pattern possessed macropores or mesopores of about 130 nm or 46 nm diameter and of about 300 nm or 99 nm interpore distances, respectively, in accordance with the initial pattern. Thermoplastic polyurethanes pore depth was however less than initial anodic aluminum oxide pore depth, linked to an incomplete replication during intermediate mould preparation (60 to 90% depth replication). The correct replication of the original pattern confirms that this novel fabrication method is a promising route for surface patterning of thermoplastic polyurethanes that could be used for medical applications.
Influence of polyurethane resin dies on the fit and adaptation of full veneer crowns.
Lillywhite, Graeme R R; Vohra, Fahim
2015-01-01
Polyurethane resin is a possible alternative to type IV dental stone for fabrication of indirect restorations however its dimensional accuracy is questionable. The aim was to investigate the dimensional accuracy of silica filled polyurethane resin die material by evaluating the marginal fit and adaptation of indirect gold castings. Experimental, in vitro study. Totally 40 copper plated replicas of a nickel chrome master die analogous to a veneer gold crown preparation were made and impressions recorded using polyvinylsiloxane material. Twenty impressions were poured in type IV dental stone (control group (Vel-mix, Kerr, UK) and the remaining (n = 20) in silica filled polyurethane die material (test group) (Alpha Die MF, CA, USA). Gold castings were fabricated for each die using standardized techniques. The castings were seated on their respective copper plated dies, embedded in resin and sectioned. The specimens were analyzed by measuring marginal opening and the area beneath the casting at a ×63 magnification and using image analysis software. Data were analyzed using a Student's t-test. No significant difference was observed between the experimental groups (P > 0.05). The mean marginal opening for type IV, dental stone and polyurethane resin, was 57 ± 22.6 μm and 63.47 ± 27.1 μm, respectively. Stone displayed a smaller area beneath the casting (31581 ± 16297 μm 2 ) as compared to polyurethane resin (35003 ± 23039 μm 2 ). The fit and adaptation of indirect gold castings made on polyurethane and type IV dental stone dies were comparable.
NASA Astrophysics Data System (ADS)
Doutres, Olivier; Atalla, Noureddine; Dong, Kevin
2013-02-01
This paper proposes simple semi-phenomenological models to predict the sound absorption efficiency of highly porous polyurethane foams from microstructure characterization. In a previous paper [J. Appl. Phys. 110, 064901 (2011)], the authors presented a 3-parameter semi-phenomenological model linking the microstructure properties of fully and partially reticulated isotropic polyurethane foams (i.e., strut length l, strut thickness t, and reticulation rate Rw) to the macroscopic non-acoustic parameters involved in the classical Johnson-Champoux-Allard model (i.e., porosity ϕ, airflow resistivity σ, tortuosity α∝, viscous Λ, and thermal Λ' characteristic lengths). The model was based on existing scaling laws, validated for fully reticulated polyurethane foams, and improved using both geometrical and empirical approaches to account for the presence of membrane closing the pores. This 3-parameter model is applied to six polyurethane foams in this paper and is found highly sensitive to the microstructure characterization; particularly to strut's dimensions. A simplified micro-/macro model is then presented. It is based on the cell size Cs and reticulation rate Rw only, assuming that the geometric ratio between strut length l and strut thickness t is known. This simplified model, called the 2-parameter model, considerably simplifies the microstructure characterization procedure. A comparison of the two proposed semi-phenomenological models is presented using six polyurethane foams being either fully or partially reticulated, isotropic or anisotropic. It is shown that the 2-parameter model is less sensitive to measurement uncertainties compared to the original model and allows a better estimation of polyurethane foams sound absorption behavior.
Barber, F Alan
2013-09-01
To compare the load-to-failure pullout strength of bone-patellar tendon-bone (BPTB) allografts in human cadaver tibias and rigid polyurethane foam blocks. Twenty BPTB allografts were trimmed creating 25 mm × 10 mm × 10 mm tibial plugs. Ten-millimeter tunnels were drilled in 10 human cadaver tibias and 10 rigid polyurethane foam blocks. The BPTB anterior cruciate ligament allografts were inserted into these tunnels and secured with metal interference screws, with placement of 10 of each type in each material. After preloading (10 N), cyclic loading (500 cycles, 10 to 150 N at 200 mm/min) and load-to-failure testing (200 mm/min) were performed. The endpoints were ultimate failure load, cyclic loading elongation, and failure mode. No difference in ultimate failure load existed between grafts inserted into rigid polyurethane foam blocks (705 N) and those in cadaver tibias (669 N) (P = .69). The mean rigid polyurethane foam block elongation (0.211 mm) was less than that in tibial bone (0.470 mm) (P = .038), with a smaller standard deviation (0.07 mm for foam) than tibial bone (0.34 mm). All BPTB grafts successfully completed 500 cycles. The rigid polyurethane foam block showed less variation in test results than human cadaver tibias. Rigid polyurethane foam blocks provide an acceptable substitute for human cadaver bone tibia for biomechanical testing of BPTB allografts and offer near-equivalent results. Copyright © 2013 Arthroscopy Association of North America. Published by Elsevier Inc. All rights reserved.
Highly fluorinated polyurethanes
NASA Technical Reports Server (NTRS)
Stump, E. C., Jr.; Rochow, S. E. (Inventor)
1973-01-01
The reaction perfluorinated hydroxyl terminated polyether with diisocyanate to form polyurethane is discussed. Data are given on the resin's oxidation stability, chemical resistance, and low temperature flexibility.
Reversibly pH-responsive polyurethane membranes for on-demand intravaginal drug delivery.
Kim, Seungil; Chen, Yufei; Ho, Emmanuel A; Liu, Song
2017-01-01
To provide better protection for women against sexually transmitted infections, on-demand intravaginal drug delivery was attempted by synthesizing reversibly pH-sensitive polyether-polyurethane copolymers using poly(ethylene glycol) (PEG) and 1,4-bis(2-hydroxyethyl)piperazine (HEP). Chemical structure and thermo-characteristics of the synthesized polyurethanes were confirmed by attenuated total reflectance-Fourier transform infrared spectroscopy (ATR-FTIR), 1 H-nuclear magnetic resonance ( 1 H-NMR), and melting point testing. Membranes were cast by solvent evaporation method using the prepared pH-sensitive polyurethanes. The impact of varying pH on membrane swelling and surface morphology was evaluated via swelling ratio change and scanning electron microscopy (SEM). The prepared pH-responsive membranes showed two times higher swelling ratio at pH 4 than pH 7 and pH-triggered switchable surface morphology change. The anionic anti-inflammatory drug diclofenac sodium (NaDF) was used as a model compound for release studies. The prepared pH-responsive polyurethane membranes allowed continuous NaDF release for 24h and around 20% release of total NaDF within 3h at pH 7 but little-to-no drug release at pH 4.5. NaDF permeation across the prepared membranes demonstrated a reversible pH-responsiveness. The pH-responsive polyurethane membranes did not show any noticeable negative impact on vaginal epithelial cell viability or induction of pro-inflammatory cytokine production compared to controls. Overall, the non-cytotoxic HEP-based pH-responsive polyurethane demonstrated its potential to be used in membrane-based implants such as intravaginal rings to achieve on-demand "on-and-off" intravaginal drug delivery. A reversible and sharp switch between "off" and "on" drug release is achieved for the first time through new pH-sensitive polyurethane membranes, which can serve as window membranes in reservoir-type intravaginal rings for on-demand drug delivery to prevent sexually transmitted infections (STIs). Close to zero drug release occurs at the normal vaginal pH (4.5) for minimal side effects. Drug release is only triggered by elevation of pH to 7 during heterosexual intercourse. The reversibly sharp and fast "on-and-off" switch arises from the creative incorporation of a pH-sensitive monomer in the soft segment of polyurethane. This polyurethane biomaterial holds great potential to better protect women who are generally at higher risk and are more vulnerable to STIs. Copyright © 2016 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
NASA Technical Reports Server (NTRS)
Bodemeijer, R.
1985-01-01
Brown wax previously used to mask hardware replaced with polyurethane foam in electroplating and electroforming operations. Foam easier to apply and remove than wax and does not contaminate electrolytes.
Improving the Performance of Heat Insulation Polyurethane Foams by Silica Nanoparticles
NASA Astrophysics Data System (ADS)
Nikje, M. M. Alavi; Garmarudi, A. Bagheri; Haghshenas, M.; Mazaheri, Z.
Heat insulation polyurethane foam materials were doped by silica nano particles, to investigate the probable improving effects. In order to achieve the best dispersion condition and compatibility of silica nanoparticles in the polymer matrix a modification step was performed by 3-aminopropyltriethoxysilane (APTS) as coupling agent. Then, thermal and mechanical properties of polyurethane rigid foam were investigated. Thermal and mechanical properties were studied by tensile machine, thermogravimetric analysis and dynamic mechanical analysis.
Primary Stability of Zirconium vs Titanium Implants: An In Vitro Comparison
2015-06-05
Zirconia implant and 4x11.5 Titanium implant placed in artificial bone ( polyurethane foam ) at .08 rotations /sec…………………………………28 viii...measurements as they relate to primary Implant Stability. Artificial Bone made of solid ridged polyurethane foam was used as an alternative test...30 pound per cubic foot solid rigid polyurethane blocks used to substitute human cancellous bone
NASA Astrophysics Data System (ADS)
Orfali, Wasim A.
This article demonstrates the acoustic properties of added small amount of carbon-nanotube and siliconoxide nano powder (S-type, P-Type) to the host material polyurethane composition. By adding CNT and/or nano-silica in the form of powder at different concentrations up to 2% within the PU composition to improve the sound absorption were investigated in the frequency range up to 1600 Hz. Sound transmission loss measurement of the samples were determined using large impedance tube. The tests showed that addition of 0.2 wt.% Silicon Oxide Nano-powder and 0.35 wt.% carbon nanotube to polyurethane composition improved sound transmissions loss (Sound Absorption) up to 80 dB than that of pure polyurethane foam sample.
Treviňo, Lucia; Contreras-Esquivel, Juan C.; Rodríguez-Herrera, Raul; Aguilar, Cristóbal Noé
2007-01-01
The influence of the physical structure of polyurethane matrix as a support in a solid state culture in tannase production and gallic acid accumulation by Aspergillus niger Aa-20 was evaluated. Three different polyurethane matrices were used as the support: continuous, semi-discontinuous and discontinuous. The highest tannase production at 2479.59 U/L during the first 12 h of culture was obtained using the discontinuous matrix. The gallic acid was accumulated at 7.64 g/L at the discontinuous matrix. The results show that the discontinuous matrix of polyurethane is better for tannase production and gallic acid accumulation in a solid state culture bioprocess than the continuous and semi-discontinuous matrices. PMID:17910122
Creating biomimetic polymeric surfaces by photochemical attachment and patterning of dextran
Ferrer, M. Carme Coll; Yang, Shu; Eckmann, David M.; Composto, Russell J.
2010-01-01
In this work, we report the preparation of photoactive dextran and demonstrate its utility by photochemically attaching it onto various polymeric substrates. The attachment of homogeneous and patterned dextran films was performed on polyurethane and polystyrene, with detailed analysis of surface morphology, swelling behavior, and the protein resistance of these substrates. The described photoactive dextran and attachment procedure is applicable to a wide variety of substrates while accommodating surfaces with complex surface and geometries. Dextran with azide content between 22 to 0.3 wt% was produced by esterification with p-azidobenzoic acid. Dextran (1.2 wt% azide) was photografted onto plasma oxidized polyurethane and polystyrene and displayed thicknesses of 5 ± 3 nm and 7 ± 3 nm, respectively. The patterned dextran on oxidized polyurethane was patchy with a nominal height difference between dextranized and non-dextranized regions. The azidated dextran on oxidized polystyrene exhibited a distinct step in height. In the presence of PBS buffer, the dextranized regions became smoother and more uniform without affecting the height difference at the oxidized polyurethane boundary. However, the dextranized regions on oxidized polyurethane were observed to swell by a factor of 3 relative to the dried thickness. These dissimilarities were attributed to hydrogen bonding between the dextran and oxidized polyurethane and were confirmed by the photoimmobiliization in the presence of LiCl. The resulting surface was the smoothest of all the azidated dextran samples (RRMS = 1 ± 0.3 nm) and swelled up to 2 times its dried thickness in PBS buffer. The antifouling properties of dextran functionalized surfaces were verified by the selective adsorption of FITC-labeled human albumin only on the non-dextranized regions of the patterned polyurethane and polystyrene substrates. PMID:20712352
Sharifi-Aghdam, Maryam; Faridi-Majidi, Reza; Derakhshan, Mohammad Ali; Chegeni, Arash; Azami, Mahmoud
2017-07-01
The main objective of this study was to prepare a hybrid three-dimensional scaffold that mimics natural tendon tissues. It has been found that a knitted silk shows good mechanical strength; however, cell growth on the bare silk is not desirable. Hence, electrospun collagen/polyurethane combination was used to cover knitted silk. A series of collagen and polyurethane solutions (4%-7% w/v) in aqueous acetic acid were prepared and electrospun. According to obtained scanning electron microscopy images from pure collagen and polyurethane nanofibers, concentration was set constant at 5% (w/v) for blend solutions of collagen/polyurethane. Afterward, blend solutions with the weight ratios of 75/25, 50/50 and 25/75 were electrospun. Scanning electron microscopy images demonstrated the smooth and uniform morphology for the optimized nanofibers. The least fibers diameter among three weight ratios was found for collagen/polyurethane (25/75) which was 100.86 ± 40 nm and therefore was selected to be electrospun on the knitted silk. Attenuated total reflectance-Fourier transform infrared spectra confirmed the chemical composition of obtained electrospun nanofibers on the knitted silk. Tensile test of the specimens including blend nanofiber, knitted silk and commercial tendon substitute examined and indicated that collagen/polyurethane-coated knitted silk has appropriate mechanical properties as a scaffold for tendon tissue engineering. Then, Alamar Blue assay of the L929 fibroblast cell line seeded on the prepared scaffolds demonstrated appropriate viability of the cells with a significant proliferation on the scaffold containing more collagen content. The results illustrate that the designed structure would be promising for being used as a temporary substitute for tendon repair.
Synergism between polyurethane and polydopamine in the synthesis of Ni-Fe alloy monoliths.
Naresh Kumar, Thangavel; Sivabalan, Santhana; Chandrasekaran, Naveen; Phani, Kanala Lakshminarasimha
2015-02-04
Herein, we report the first synthesis of a light-weight macroporous 3-D alloy monolith of Ni-Fe/C using synergism between polydopamine (pDA) and polyurethane (pU); in situ formed polyurethane (pU) enables efficient mixing of pDA (carbon source) and Ni-FeOx resulting in Ni-Fe alloy monoliths at a temperature as low as ∼600 °C. The monolithic Ni-Fe/C exhibits enhanced oxygen evolution activity.
Isocyanate-Free Elastomers as Replacements for Isocyanate-Cured Polyurethanes (Briefing Charts)
2015-08-20
Polyurethanes (Briefing Charts) 5a. CONTRACT NUMBER In-House 5b. GRANT NUMBER 5c. PROGRAM ELEMENT NUMBER 6. AUTHOR(S) Josiah T. Reams, Andrew J...Standard Form 298 (Rev. 8-98) Prescribed by ANSI Std. 239.18 1 Isocyanate-Free Elastomers as Replacements for Isocyanate-cured Polyurethanes ...paints, foams , sealants, and adhesives that also represent a significant source of occupational health risk for DoD and DOE. DISTRIBUTION A: Approved
Synthesis of Polyurethanes Membranes from Rubber Seed Oil and Methylene Diphenyl Diisocyanates (MDI)
NASA Astrophysics Data System (ADS)
Marlina; Nurman, S.; Saleha, S.; Fitriani; Thanthawi, I.
2017-03-01
Rubber seed oil and methylene diphenyl diisocyanates (MDI) based polyurethane membrane has been prepared in this study. The main objective of this research is manufacture of polyurethane membranes from avocado seed oil, as a filter of this membrane use as a filter of metals from water such as mercury (Hg). In this study, the polyurethane membrane had been synthesized by varying compositions of rubber seed oil and MDI, with ratios of 10:0.2; 10:0.4; 10:0.6; 10:0.8; 10:1.0; 10:1.2; 10:1.4; 10:1.6; 10:1.8 and 10:2.0 (v/w) at 80°C and 170°C as polymerization and curing temperatures, respectively. Optimum polyurethane membrane was obtained at rubber seed oil: MDI 10: 0.8 v/w, it was dry, non-sticky, smooth and blackish brown. The membrane flux was 5,8307 L / m2.h.bar and rejection factor was 35,3015 %. The results of characterization indicated the formation of urethane bonds (NH at 3480 cm-1, C=O at 1620 cm-1, CN at 1374 cm-1, -OC-NH- at 1096 cm-1 and no -NCO at 2270 cm-1), the value of Tg was 55°C. The polyurethane membrane which treated at the optimum treatment conditions were used to the filter of metals from water such as mercury (Hg).
Response of Polyurethane to Shock Waves: An Experimental Investigation
NASA Astrophysics Data System (ADS)
Jayaram, V.; Rao, Keshava Subba; Thanganayaki, N.; Kumara, H. K. T.; Reddy, K. P. J.
Formation of polyurethane (PU) in vacuum environment and controlling density of polyurethane foams are the present day challenges. Polyurethane exists in numerous forms ranging from flexible to rigid and lightweight foams to tough, stiff elastomers [1]. PU can be used to produce lightweight foams for insulation or hard rubber used as wheels to transport heavy loads and it can be used in high pressure applications. The largest volumes of commercial PU elastomers are made from toluene diisocyanate (TDI) or diphenylmethane-4, 4'-diisocyanate (MDI) [2]. Linear polyurethanes can be processed into final products by any of the standard thermoplastic processes (injection molding, extrusion, thermoforming) as well as by low pressure cast processes in presence of catalysts. Tin, tetrabutyl titanate and zirconium chelates are few effective catalysts used to produce polyurethane for particular application [3]. Thermoset elastomers are formed due to irreversible cross-links, when polymers are chemically cured. Highly porous biodegradable PU was synthesized by thermally induced phase separation technique used in tissue engineering and also in bio-degradable based fluids [4]. Properties of PU like hardness, stress/strain modulus, tear strength etc, was determine using ASTM (American Society for Testing and Materials) standard methods. PU possesses extremely high mechanical properties, excellent abrasion, tear and extrusion resistance. It has outstanding low-temperature limit (-600C) and high temperature limit up to (1500C).
Alternating block polyurethanes based on PCL and PEG as potential nerve regeneration materials.
Li, Guangyao; Li, Dandan; Niu, Yuqing; He, Tao; Chen, Kevin C; Xu, Kaitian
2014-03-01
Polyurethanes with regular and controlled block arrangement, i.e., alternating block polyurethanes (abbreviated as PUCL-alt-PEG) based on poly(ε-caprolactone) (PCL-diol) and poly(ethylene glycol) (PEG) was prepared via selectively coupling reaction between PCL-diol and diisocyanate end-capped PEG. Chemical structure, molecular weight, distribution, and thermal properties were systematically characterized by FTIR, (1)H NMR, GPC, DSC, and TGA. Hydrophilicity was studied by static contact angle of H2O and CH2I2. Film surface was observed by scanning electron microscope (SEM) and atomic force microscopy, and mechanical properties were assessed by universal test machine. Results show that alternating block polyurethanes give higher crystal degree, higher mechanical properties, and more hydrophilic and rougher (deep ravine) surface than their random counterpart, due to regular and controlled structure. Platelet adhesion illustrated that PUCL-alt-PEG has better hemocompatibility and the hemacompatibility was affected significantly by PEG content. Excellent hemocompatibility was obtained with high PEG content. CCK-8 assay and SEM observation revealed much better cell compatibility of fibroblast L929 and rat glial cells on the alternating block polyurethanes than that on random counterpart. Alternating block polyurethane PUC20-a-E4 with optimized composition, mechanical, surface properties, hemacompatibility, and highest cell growth and proliferation was achieved for potential use in nerve regeneration. Copyright © 2013 Wiley Periodicals, Inc.
Polyurethane Ionophore-Based Thin Layer Membranes for Voltammetric Ion Activity Sensing.
Cuartero, Maria; Crespo, Gaston A; Bakker, Eric
2016-06-07
We report on a plasticized polyurethane ionophore-based thin film material (of hundreds of nanometer thickness) for simultaneous voltammetric multianalyte ion activity detection triggered by the oxidation/reduction of an underlying poly(3-octylthiophene) film. This material provides excellent mechanical, physical, and chemical robustness compared to other polymers. Polyurethane films did not exhibit leaching of lipophilic additives after rinsing with a direct water jet and exhibited resistance to detachment from the underlying electrode surface, resulting in a voltammetric current response with less than <1.5% RSD variation (n = 50). In contrast, plasticized poly(vinyl chloride), polystyrene, and poly(acrylate) ionophore-based membranes of the same thickness and composition exhibited a significant deterioration of the signal after identical treatment. While previously reported works emphasized fundamental advancement of multi-ion detection with multi-ionophore-based thin films, polyurethane thin membranes allow one to achieve real world measurements without sacrificing analytical performance. Indeed, polyurethane membranes are demonstrated to be useful for the simultaneous determination of potassium and lithium in undiluted human serum and blood with attractive precision.
Luo, Xiaogang; Xiao, Yuqin; Wu, Qiangxian; Zeng, Jian
2018-04-25
Development of biodegradable polyurethane materials is the most promising in the wider context of the "greening" of industrial chemistry. To tackle this challenge, a novel biodegradable polyurethane foam from all bioresource-based polyols (lignin and soy oil-derived polyols) and polymeric methyldiphenyl diisocyanate (pMDI) have been synthesized via a one-pot and self-rising process. All these foam samples have the internal cellular morphology and microstructure. FTIR result exhibits characteristic peaks of polyurethane, and indicates covalent bonds between soy-based polyurethane and lignin, and the lignin powders can react with pMDI via active -H and -CNO. In addition, hydrogen bonding also plays an important role in forming the 3D structures. These interactions and chemical bonds made the prepared foam samples form the 3D macromolecular structure with improved mechanical, thermal, and biodegradable properties. The reaction process is time-saving and cost-effective as it requires no blowing agent and minimum processing steps, while exploring the potential of using the higher content of nature bioresource constituents. Copyright © 2018 Elsevier B.V. All rights reserved.
NASA Astrophysics Data System (ADS)
Bao, Junjie; Shi, Gaojian; Tao, Can; Wang, Chao; Zhu, Chen; Cheng, Liang; Qian, Gang; Chen, Chunhua
2018-06-01
Four kinds of polycarbonate-based polyurethane with 8-14 wt% hard segments content are synthesized via reactions of polycarbonatediol, hexamethylene diisocyanate and diethylene glycol. The mechanical strength of the polyurethanes increase with the increase of hard segments content. Solid polymer electrolytes composed of the polycarbonate-based polyurethanes and LiTFSI exhibits fascinating characteristics for all-solid-state lithium batteries with a high ionic conductivity of 1.12 × 10-4 S cm-1 at 80 °C, an electrochemical stability window up to 4.5 V (vs. Li+/Li), excellent mechanical strength and superior interfacial stability against lithium metal. The all-solid-state batteries using LiFePO4 cathode can deliver high discharge capacities (161, 158, 134 and 93 mAh g-1 at varied rates of 0.2, 0.5, 1 and 2 C) at 80 °C and excellent cycling performance (with 91% capacity retention after 600 cycles at 1 C). All the results indicate that such a polyurethane-based solid polymer electrolyte can be a promising candidate for all-solid-state lithium batteries.
NASA Astrophysics Data System (ADS)
Geng, Jialu; Wang, Caiping; Zhu, Honglang; Wang, Xiaojie
2018-03-01
Elastomeric matrix embedded with magnetic micro-sized particles has magnetically controllable properties, which has been investigated extensively in the last decades. In this study we develop a new magnetically controllable elastomeric material for acoustic applications at lower frequencies. The soft polyurethane foam is used as matrix material due to its extraordinary elastic and acoustic absorption properties. One-step method is used to synthesize polyurethane foam, in which all components including polyether polyols 330N, MDI, deionized water, silicone oil, carbonyl iron particle (CIP) and catalyst are put into one container for curing. Changing any component can induce the change of polyurethane foam's properties, such as physical and acoustic properties. The effect of the content of MDI on acoustic absorption is studied. The CIPs are aligned under extra magnetic field during the foaming process. And the property of polyurethane foam with aligned CIPs is also investigated. Scanning electron microscope (SEM) is used to observe the structure of pore and particle-chain. The two-microphone impedance tube and the transfer function method are used to test acoustic absorption property of the magnetic foams.
Shahrousvand, Mohsen; Mir Mohamad Sadeghi, Gity; Salimi, Ali
2016-12-01
The cells as a tissue component need to viscoelastic, biocompatible, biodegradable, and wettable extracellular matrix for their biological activity. In this study, in order to prepare biomedical polyurethane elastomers with good mechanical behavior and biodegradability, a series of novel polyester-polyether- based polyurethanes (PUs) were synthesized using a two-step bulk reaction by melting pre-polymer method, taking 1,4-Butanediol (BDO) as chain extender, hexamethylene diisocyanate as the hard segment, and poly (tetramethylene ether) glycol (PTMEG) and poly (ε-caprolactone diol) (PCL-Diol) as the soft segment without a catalyst. The soft to the hard segment ratio was kept constant in all samples. Polyurethane characteristics such as thermal and mechanical properties, wettability and water adsorption, biodegradability, and cellular behavior were changed by changing the ratio of polyether diol to polyester diol composition in the soft segment. Our present work provides a new procedure for the preparation of engineered polyurethanes in surface properties and biodegradability, which could be a good candidate for bone, cartilage, and skin tissue engineering.
Diamine curing agents for polyurethanes
NASA Technical Reports Server (NTRS)
Bell, V. L.; St. Clair, T. L.
1975-01-01
Three aromatic diamines have properties that make them promising candidates as curing agents for converting isocyanates to polyurethanes with higher adhesive strengths, higher softening temperatures, better toughness, and improved abrasion resistance.
40 CFR 63.8780 - What is the purpose of this subpart?
Code of Federal Regulations, 2013 CFR
2013-07-01
... (CONTINUED) National Emission Standards for Hazardous Air Pollutants: Flexible Polyurethane Foam Fabrication... national emission standards for hazardous air pollutants (NESHAP) emitted from flexible polyurethane foam...
40 CFR 63.8780 - What is the purpose of this subpart?
Code of Federal Regulations, 2011 CFR
2011-07-01
... (CONTINUED) National Emission Standards for Hazardous Air Pollutants: Flexible Polyurethane Foam Fabrication... national emission standards for hazardous air pollutants (NESHAP) emitted from flexible polyurethane foam...
40 CFR 63.8780 - What is the purpose of this subpart?
Code of Federal Regulations, 2010 CFR
2010-07-01
... (CONTINUED) National Emission Standards for Hazardous Air Pollutants: Flexible Polyurethane Foam Fabrication... national emission standards for hazardous air pollutants (NESHAP) emitted from flexible polyurethane foam...
40 CFR 63.8780 - What is the purpose of this subpart?
Code of Federal Regulations, 2012 CFR
2012-07-01
...) National Emission Standards for Hazardous Air Pollutants: Flexible Polyurethane Foam Fabrication Operations... national emission standards for hazardous air pollutants (NESHAP) emitted from flexible polyurethane foam...
40 CFR 63.8780 - What is the purpose of this subpart?
Code of Federal Regulations, 2014 CFR
2014-07-01
... (CONTINUED) National Emission Standards for Hazardous Air Pollutants: Flexible Polyurethane Foam Fabrication... national emission standards for hazardous air pollutants (NESHAP) emitted from flexible polyurethane foam...
NASA Astrophysics Data System (ADS)
Manap, Siti Munirah; Ahmad, Azizan; Anuar, Farah Hannan
2016-11-01
A polyurethane films consisting of PLLA, PPG and PLLA-PPG were prepared using solution casting method. Three types of polyurethane were prepared: PPLA:PMDI, PPG:PMDI and PLLA-PPG:PMDI in the presence of polymeric diphenylmethane diisocyanate (PMDI) as the coupling agent and catalyst, Sn(Oct)2. The aim of this research was to improve the physicals properties of PLLA and PPG homopolymers through copolymerization between the two polymers. The homopolymers and polyurethane films were characterized using ATR-FTIR spectroscopy. Chemical reaction between PLLA, PPG and PMDI before and after the reaction were confirmed by observing the shifting of wavenumber for the carbonyl and ether group. Other than that, the additional band for N-H after the reaction indicated that the reaction was successful.
Synthesis and Characterization of High-Dielectric-Constant Nanographite-Polyurethane Composite
NASA Astrophysics Data System (ADS)
Mishra, Praveen; Bhat, Badekai Ramachandra; Bhattacharya, B.; Mehra, R. M.
2018-05-01
In the face of ever-growing demand for capacitors and energy storage devices, development of high-dielectric-constant materials is of paramount importance. Among various dielectric materials available, polymer dielectrics are preferred for their good processability. We report herein synthesis and characterization of nanographite-polyurethane composite with high dielectric constant. Nanographite showed good dispersibility in the polyurethane matrix. The thermosetting nature of polyurethane gives the composite the ability to withstand higher temperature without melting. The resultant composite was studied for its dielectric constant (ɛ) as a function of frequency. The composite exhibited logarithmic variation of ɛ from 3000 at 100 Hz to 225 at 60 kHz. The material also exhibited stable dissipation factor (tan δ) across the applied frequencies, suggesting its ability to resist current leakage.
Investigation of wear resistance of polyurethanes in abrasive soil mass
NASA Astrophysics Data System (ADS)
Napiórkowski, Jerzy; Ligier, Krzysztof
2018-04-01
This paper presents a comparative study of polyurethane wear in different abrasive soil masses. Two types of polyurethanes of various chemical compositions and untreated 38GSA steel were tested, the latter being used as a reference standard. The study was conducted in natural soil mass at a "rotating bowl" stand. Relative wear resistance was determined from measurements of mass wear for the materials under study. The condition of the surface of the materials under wear test was analysed.
Coating processes for increasing the moisture resistance of polyurethane baffle material
NASA Technical Reports Server (NTRS)
Bilow, N.; Sawko, P.
1974-01-01
An investigation was conducted with the objective to improve the hydrolytic stability of reticulated polyurethane baffle material. This material is used in fuel tanks of aircraft and ground vehicles. The most commonly used foam of this type is hydrolytically unstable. Potential moisture barrier coatings which were evaluated include Parylene, epoxy-polysulfide, polyether based polyurethanes, polysulfides, polyolefin rubbers, and several other materials. Parylene coatings of at least 0.2 mil were found to provide the greatest improvement in hydrolytic stability.
Numerical Simulation of Ballistic Impact of Layered Aluminum Nitride Ceramic
2015-09-01
tile(s) Aluminum nitride (AlN) 163 a Polymer layers Polyurethane foam 18 b Backing metal Aluminum 6061-T6 (Al) 23 c Projectile Tungsten heavy alloy...larger (a factor of 3.8) than the most dense polyurethane foam of the available constitutive models. Default options for element failure were imposed in...AlN), a polycrystalline ceramic. The total thickness of the tile(s) is 38.1 mm in all cases. A thin polyurethane laminate separates neighboring tiles
Flame Retardants Used in Flexible Polyurethane Foam
The partnership project on flame retardants in furniture seeks to update the health and environmental profiles of flame-retardant chemicals that meet fire safety standards for upholstered consumer products with polyurethane foam
Fire retardant foams developed to suppress fuel fires
NASA Technical Reports Server (NTRS)
Fish, R.; Gilwee, W. J.; Parker, J. A.; Riccitiello, S. R.
1968-01-01
Heat insulating polyurethane foam retards and suppresses fuel fires. Uniformly dispersed in the foam is a halogenated polymer capable of splitting off hydrogen halide upon heating and charring of the polyurethane.
DOE Office of Scientific and Technical Information (OSTI.GOV)
Javni, Ivan; Bilić, Olivera; Bilić, Nikola
2015-06-30
Isosorbide, a cyclic, rigid and renewable diol was used as a chain extender in two series of thermoplastic polyurethanes. Isosorbide was used in combination with butane diol or alone to examine the effects on polyurethane morphology. Two series of materials were prepared -one with dispersed hard domains in the matrix of polytetramethylene ether glycol soft segments of molecular weight 1400 (at 70% soft segment concentration-SSC) and the other with co-continuous soft and hard phases at 50% SSC. Morphology of materials was studied by optical and atomic force microscopy, as well as with ultra small angle x-ray scattering (USAXS). The radiusmore » of spherical hard domains, correlation lengths, mean separation distances and boundary layer thickness were measured as a function of isosorbide content.« less
Electrical conductivity of rigid polyurethane foam at high temperature
NASA Astrophysics Data System (ADS)
Johnson, R. T., Jr.
1982-08-01
The electrical conductivity of rigid polyurethane foam, used for electronic encapsulation, was measured during thermal decomposition to 3400 C. At higher temperatures the conductance continues to increase. With pressure loaded electrical leads, sample softening results in eventual contact between electrodes which produces electrical shorting. Air and nitrogen environments show no significant dependence of the conductivity on the atmosphere over the temperature range. The insulating characteristics of polyurethane foam below approx. 2700 C are similar to those for silicone based materials used for electronic case housings and are better than those for phenolics. At higher temperatures (greater than or equal to 2700 C) the phenolics appear to be better insulators to approx. 5000 C and the silicones to approx. 6000 C. It is concluded that the Sylgard 184/GMB encapsulant is a significantly better insulator at high temperature than the rigid polyurethane foam.
Detection of halogenated flame retardants in polyurethane foam by particle induced X-ray emission
NASA Astrophysics Data System (ADS)
Maley, Adam M.; Falk, Kyle A.; Hoover, Luke; Earlywine, Elly B.; Seymour, Michael D.; DeYoung, Paul A.; Blum, Arlene; Stapleton, Heather M.; Peaslee, Graham F.
2015-09-01
A novel application of particle-induced X-ray emission (PIXE) has been developed to detect the presence of chlorinated and brominated flame retardant chemicals in polyurethane foams. Traditional Gas Chromatography-Mass Spectrometry (GC-MS) methods for the detection and identification of halogenated flame retardants in foams require extensive sample preparation and data acquisition time. The elemental analysis of the halogens in polyurethane foam performed by PIXE offers the opportunity to identify the presence of halogenated flame retardants in a fraction of the time and sample preparation cost. Through comparative GC-MS and PIXE analysis of 215 foam samples, excellent agreement between the two methods was obtained. These results suggest that PIXE could be an ideal rapid screening method for the presence of chlorinated and brominated flame retardants in polyurethane foams.
Microwave-assisted synthesis of cyclodextrin polyurethanes.
Biswas, Atanu; Appell, Michael; Liu, Zengshe; Cheng, H N
2015-11-20
Cyclodextrin (CD) has often been incorporated into polyurethanes in order to facilitate its use in encapsulation or removal of organic species for various applications. In this work a microwave-assisted method has been developed to produce polyurethanes consisting of α-, β-, and γ-CD and three common diisocyanates. As compared to conventional heating, this new synthetic method saves energy, significantly reduces reaction time, and gets similar or improved yield. The reaction products have been fully characterized with (13)C, (1)H, and two-dimensional NMR spectroscopy. With suitable stoichiometry of starting CD and diisocyanate, the resulting CD polyurethane is organic-soluble and water-insoluble and is shown to remove Nile red dye and phenol from water. Possible applications include the removal of undesirable materials from process streams, toxic compounds from the environment, and encapsulation of color or fragrance molecules. Published by Elsevier Ltd.
Yang, Li; Tong, Rui; Wang, Zhanhua; Xia, Hesheng
2018-03-25
A new kind of fast near-infrared (NIR) light-responsive shape-memory polymer composites was prepared by introducing polydopamine particles (PDAPs) into commercial shape-memory polyurethane (SMPU). The toughness and strength of the polydopamine-particle-filled polyurethane composites (SMPU-PDAPs) were significantly enhanced with the addition of PDAPs due to the strong interface interaction between PDAPs and polyurethane segments. Owing to the outstanding photothermal effect of PDAPs, the composites exhibit a rapid light-responsive shape-memory process in 60 s with a PDAPs content of 0.01 wt%. Due to the excellent dispersion and convenient preparation method, PDAPs have great potential to be used as high-efficiency and environmentally friendly fillers to obtain novel photoactive functional polymer composites. © 2018 Wiley-VCH Verlag GmbH & Co. KGaA, Weinheim.
Lim, Dong-In; Park, Hyung-Seok; Park, Jeong-Hui; Knowles, Jonathan C
2013-01-01
Biodegradable–biocompatible polyurethanes were prepared with fixed hexamethylene diisocyanate and varying ratios of isomannide and poly(ϵ-caprolactone) diol using a simple one-step polymerization without a catalyst. The polyurethane structures were confirmed by 1H-nuclear magnetic resonance, Fourier transform infrared spectroscopy, and gel permeation chromatography. The glass transition temperatures were determined by thermal analysis to be between 25°C and 30°C. Degradation tests performed at 37°C in phosphate buffer produced mass losses of 5%–10% after 8 weeks. After 5 days of culture, using osteoblastic cells, the relative cell number on all the polyurethane films was only slightly lower than that of an optimized tissue culture plastic. These polymers offer significant promise with a simplistic synthesis and controlled degradation. PMID:25076809
Efficacy of a polyurethane dressing versus a soft silicone sheet on hypertrophic scars.
Wigger-Albert, W; Kuhlmann, M; Wilhelm, D; Mrowietz, U; Eichhorn, K; Ortega, J; Bredehorst, A; Wilhelm, K-P
2009-05-01
To compare the efficacy and safety of a polyurethane dressing with a silicone sheet in the treatment of hypertrophic scars. Sixty patients participated in this intra-individual 12-week clinical trial. Each scar was divided into two areas, to which the polyurethane dressing and the silicone sheet were randomly allocated. The primary outcome measure was the percentage change in the overall scar index (SI) between baseline and week 12. Secondary outcome measures included changes in skin redness, objectively measured by chromametry, and patients views on the aesthetic outcome of treatment. Both therapies achieved favourable results for all of the above outcome measures. Results were comparable for the primary outcome measure: 29.4% versus 33.7% for the silicone sheet and polyurethane product respectively. The decrease in the overall SI was significantly more pronounced for the polyurethane product after week 4 (5.6% versus 15.8% for the silicone sheet; p<0.0001) and week 8 (20.2% versus 27.1%; p=0.012). Both regimens were associated with a significant reduction in the clinical signs of hypertrophic scars over 12 weeks of treatment. The polyurethane dressing demonstrated a significantly more pronounced reduction in severity of these clinical signs after four and eight weeks of treatment and was better tolerated than the silicone sheet. l This study was funded by Beiersdorf AG. proDERM is an independent research company, and none of the authors have an interest in the sponsors commercial activities.
Ford, Audrey C; Gramling, Hannah; Li, Samuel C; Sov, Jessica V; Srinivasan, Amrita; Pruitt, Lisa A
2018-03-01
Polycarbonate polyurethane has cartilage-like, hygroscopic, and elastomeric properties that make it an attractive material for orthopedic joint replacement application. However, little data exists on the cyclic loading and fracture behavior of polycarbonate polyurethane. This study investigates the mechanisms of fatigue crack growth in polycarbonate polyurethane with respect to time dependent effects and conditioning. We studied two commercially available polycarbonate polyurethanes, Bionate® 75D and 80A. Tension testing was performed on specimens at variable time points after being removed from hydration and variable strain rates. Fatigue crack propagation characterized three aspects of loading. Study 1 investigated the impact of continuous loading (24h/day) versus intermittent loading (8-10h/day) allowing for relaxation overnight. Study 2 evaluated the effect of frequency and study 3 examined the impact of hydration on the fatigue crack propagation in polycarbonate polyurethane. Samples loaded intermittently failed instantaneously and prematurely upon reloading while samples loaded continuously sustained longer stable cracks. Crack growth for samples tested at 2 and 5Hz was largely planar with little crack deflection. However, samples tested at 10Hz showed high degrees of crack tip deflection and multiple crack fronts. Crack growth in hydrated samples proceeded with much greater ductile crack mouth opening displacement than dry samples. An understanding of the failure mechanisms of this polymer is important to assess the long-term structural integrity of this material for use in load-bearing orthopedic implant applications. Copyright © 2018 Elsevier Ltd. All rights reserved.
Effects of electrocautery on transvenous lead insulation materials.
Lim, Kiam-Khiang; Reddy, Shantanu; Desai, Shrojal; Smelley, Matthew; Kim, Susan S; Beshai, John F; Lin, Albert C; Burke, Martin C; Knight, Bradley P
2009-04-01
Insulation defects are a leading cause of transvenous lead failure. The purpose of this study was to determine the effects of electrocautery on transvenous lead insulation materials. A preparation was done to simulate dissection of a transvenous lead from tissues. Radiofrequency energy was delivered using a standard cautery blade at outputs of 10, 20, and 30 W, for 3 and 6 seconds, using parallel and perpendicular blade orientations on leads with outermost insulations of silicone rubber, polyurethane, and silicone-polyurethane copolymer. Damage to each lead segment was classified after visual and microscopic analysis. Significant insulation damage occurred to almost all polyurethane leads. Full insulation breaches were observed with 30 W regardless of application duration with a parallel direction and with all power outputs with a perpendicular direction. Thermal insulation damage to copolymer insulation was similar to that of the polyurethane leads. In contrast, there was no thermal damage to silicone leads, regardless of the power output and duration of power delivery. However, mechanical insulation damage was observed to all silicone leads when at least 20 W was applied in a direction perpendicular to the lead. Polyurethane (PU55D) and copolymer materials have low thermal stability and are highly susceptible to thermal damage during cautery. Implanting physicians should be aware of the lead insulation materials being used during implant procedures and their properties. The use of direct contact cautery on transvenous leads should be minimized to avoid damage to the lead, especially on leads with polyurethane or copolymer outer insulations.
Mohammadi, Abbas; Barikani, Mehdi; Lakouraj, Moslem Mansour
2016-09-01
In this study, a series of magnetic polyurethane/Fe3O4 elastomer nanocomposites were prepared by covalently embedding novel thiacalix[4]arenes (TC4As) functionalized Fe3O4 nanoparticles (TC4As-Fe3O4) which contain macrocycles with reactive hydroxyl groups. Surface functionalization of Fe3O4 nanoparticles with TC4As macrocycles as unique reactive surface modifier not only gives specific characteristics to Fe3O4 nanoparticles but also improves the interphase interaction between nanoparticles and the polyurethane matrices through covalent attachment of polymer chains to nanoparticle surfaces. The novel synthesized TC4As-Fe3O4 nanoparticles were characterized by FTIR, XRD, TGA, VSM and SEM analysis. Furthermore, the effect of functionalization of Fe3O4 nanoparticles on the various properties of resulting nanocomposites was studied by XRD, TGA, DMTA, SEM, and a universal tensile tester. It was found that the functionalization of nanoparticles with TC4As affords better mechanical and thermal properties to polyurethane nanocomposites in comparison with unmodified nanoparticles. The SEM analysis showed finer dispersion of TC4As-Fe3O4 nanoparticles than unmodified Fe3O4 nanoparticles within the polyurethane matrices, which arising from formation of covalent bonding between TC4As functionalized Fe3O4 nanoparticles and polyurethane matrices. Moreover, the investigation of in vitro biocompatibility of novel nanocomposites showed that these samples are excellent candidate for biomedical use. Copyright © 2016 Elsevier B.V. All rights reserved.
Engineering a degradable polyurethane intravaginal ring for sustained delivery of dapivirine.
Kaur, Manpreet; Gupta, Kavita M; Poursaid, Azadeh E; Karra, Prasoona; Mahalingam, Alamelu; Aliyar, Hyder A; Kiser, Patrick F
2011-06-01
We describe the engineering of a degradable intravaginal ring (IVR) for the delivery of the potent HIV-1 reverse transcriptase inhibitor dapivirine. The degradable polymer used in fabricating the device incorporated poly(caprolactone) ester blocks in a poly(tetramethylene ether) glycol ABA type polyurethane backbone. The polymer was designed to maintain its structure for 1 month during usage and then degrade in the environment post-disposal. In vitro release of dapivirine showed zero-order kinetics for up to 1 month and significant levels of drug release into engineered vaginal tissue. The mechanical properties of the degradable IVR were comparable to those of a widely used contraceptive intravaginal ring upon exposure to simulated vaginal conditions. Incubation under simulated vaginal conditions for a month caused minimal degradation with minimal effect on the mechanical properties of the ring and polymer. The cytotoxicity evaluation of the drug-loaded IVRs against Vk2/E6E7 human vaginal epithelial cells, Lactobacillus jensenii, and engineered vaginal tissue constructs showed the degradable polyurethane to be non-toxic. In vitro evaluation of inflammatory potential monitored through the levels of inflammatory cytokines IL-8, IL-1α, IL-6, IL-1β, and MIP-3α when engineered EpiVaginal™ tissue was incubated with the polyurethanes suggested that the degradable polyurethane was comparable to commercial medical grade polyurethane. These results are encouraging for further development of this degradable IVR for topical vaginal delivery of microbicides.
de la Peña-Salcedo, Jose Abel; Soto-Miranda, Miguel Angel; Lopez-Salguero, Jose Fernando
2012-04-01
Implants with a polyurethane foam cover have been used by plastic surgeons since Ashley described them in 1970. Overwhelming evidence confirms the benefits of these implants, especially the extremely low incidence of capsular contracture (grades 3 and 4, Baker classification). On the other hand, except for a transient and self-limited rash, there is no evidence that polyurethane implants present more complications than texturized or smooth gel implants. Due to concerns of polyurethane-induced cancer, these implants were withdrawn in United States after approximately 110,000 American women had received them. This fact, together with the probability that these implants will be reintroduced in the United States, suggests that continued monitoring of their long-term safety and effectiveness is mandatory. A retrospective study analyzed the outcomes of 996 implants inserted during a period of 15 years. The incidence of early and late complications was analyzed as well as the aesthetic outcome. The complications evaluated included hematoma (0.6%), infection (0.4%), seroma (0.8%), rash (4.3%), wound dehiscence (0%), capsular contracture (0.4%), implant malposition (0.8%), need for revisional surgery (1.2%), implant rupture (0.7%), rippling (1.8%), and polyurethane-related cancer (0%). Regarding the aesthetic outcome, 95% of the patients expressed satisfaction with their final result. The polyurethane foam-covered implants have been proven safe for use in breast surgery. They provide the lowest rate of capsular contracture (0.4% in the current study) and excellent aesthetic results.
Álvarez-Barragán, Joyce; Domínguez-Malfavón, Lilianha; Vargas-Suárez, Martín; González-Hernández, Ricardo; Aguilar-Osorio, Guillermo
2016-01-01
ABSTRACT Polyurethane (PU) is widely used in many aspects of modern life because of its versatility and resistance. However, PU waste disposal generates large problems, since it is slowly degraded, there are limited recycling processes, and its destruction may generate toxic compounds. In this work, we isolated fungal strains able to grow in mineral medium with a polyester PU (PS-PU; Impranil DLN) or a polyether PU (PE-PU; Poly Lack) varnish as the only carbon source. Of the eight best Impranil-degrading strains, the six best degraders belonged to the Cladosporium cladosporioides complex, including the species C. pseudocladosporioides, C. tenuissimum, C. asperulatum, and C. montecillanum, and the two others were identified as Aspergillus fumigatus and Penicillium chrysogenum. The best Impranil degrader, C. pseudocladosporioides strain T1.PL.1, degraded up to 87% after 14 days of incubation. Fourier transform infrared (FTIR) spectroscopy analysis of Impranil degradation by this strain showed a loss of carbonyl groups (1,729 cm−1) and N—H bonds (1,540 and 1,261 cm−1), and gas chromatography-mass spectrometry (GC-MS) analysis showed a decrease in ester compounds and increase in alcohols and hexane diisocyanate, indicating the hydrolysis of ester and urethane bonds. Extracellular esterase and low urease, but not protease activities were detected at 7 and 14 days of culture in Impranil. The best eight Impranil-degrading fungi were also able to degrade solid foams of the highly recalcitrant PE-PU type to different extents, with the highest levels generating up to 65% of dry-weight losses not previously reported. Scanning electron microscopy (SEM) analysis of fungus-treated foams showed melted and thinner cell wall structures than the non-fungus-treated ones, demonstrating fungal biodegradative action on PE-PU. IMPORTANCE Polyurethane waste disposal has become a serious problem. In this work, fungal strains able to efficiently degrade different types of polyurethanes are reported, and their biodegradative activity was studied by different experimental approaches. Varnish biodegradation analyses showed that fungi were able to break down the polymer in some of their precursors, offering the possibility that they may be recovered and used for new polyurethane synthesis. Also, the levels of degradation of solid polyether polyurethane foams reported in this work have never been observed previously. Isolation of efficient polyurethane-degrading microorganisms and delving into the mechanisms they used to degrade the polymer provide the basis for the development of biotechnological processes for polyurethane biodegradation and recycling. PMID:27316963
Álvarez-Barragán, Joyce; Domínguez-Malfavón, Lilianha; Vargas-Suárez, Martín; González-Hernández, Ricardo; Aguilar-Osorio, Guillermo; Loza-Tavera, Herminia
2016-09-01
Polyurethane (PU) is widely used in many aspects of modern life because of its versatility and resistance. However, PU waste disposal generates large problems, since it is slowly degraded, there are limited recycling processes, and its destruction may generate toxic compounds. In this work, we isolated fungal strains able to grow in mineral medium with a polyester PU (PS-PU; Impranil DLN) or a polyether PU (PE-PU; Poly Lack) varnish as the only carbon source. Of the eight best Impranil-degrading strains, the six best degraders belonged to the Cladosporium cladosporioides complex, including the species C. pseudocladosporioides, C. tenuissimum, C. asperulatum, and C. montecillanum, and the two others were identified as Aspergillus fumigatus and Penicillium chrysogenum The best Impranil degrader, C. pseudocladosporioides strain T1.PL.1, degraded up to 87% after 14 days of incubation. Fourier transform infrared (FTIR) spectroscopy analysis of Impranil degradation by this strain showed a loss of carbonyl groups (1,729 cm(-1)) and N-H bonds (1,540 and 1,261 cm(-1)), and gas chromatography-mass spectrometry (GC-MS) analysis showed a decrease in ester compounds and increase in alcohols and hexane diisocyanate, indicating the hydrolysis of ester and urethane bonds. Extracellular esterase and low urease, but not protease activities were detected at 7 and 14 days of culture in Impranil. The best eight Impranil-degrading fungi were also able to degrade solid foams of the highly recalcitrant PE-PU type to different extents, with the highest levels generating up to 65% of dry-weight losses not previously reported. Scanning electron microscopy (SEM) analysis of fungus-treated foams showed melted and thinner cell wall structures than the non-fungus-treated ones, demonstrating fungal biodegradative action on PE-PU. Polyurethane waste disposal has become a serious problem. In this work, fungal strains able to efficiently degrade different types of polyurethanes are reported, and their biodegradative activity was studied by different experimental approaches. Varnish biodegradation analyses showed that fungi were able to break down the polymer in some of their precursors, offering the possibility that they may be recovered and used for new polyurethane synthesis. Also, the levels of degradation of solid polyether polyurethane foams reported in this work have never been observed previously. Isolation of efficient polyurethane-degrading microorganisms and delving into the mechanisms they used to degrade the polymer provide the basis for the development of biotechnological processes for polyurethane biodegradation and recycling. Copyright © 2016, American Society for Microbiology. All Rights Reserved.
Structural Evaluation of Radially Expandable Cardiovascular Stents Encased in a Polyurethane Film
NASA Technical Reports Server (NTRS)
Trigwell, Steve; De, Samiran; Sharma, Rajesh; Mazumder, Malay K.; Mehta, Jawahar L.
2004-01-01
A method of encasing cardiovascular stents with an expandable polyurethane coating has been developed to provide a smooth homogeneous inner wall allowing for a confluent growth of endothelial cells. In this design, the metal wire stent structure is completely covered by the polyurethane film minimizing biocorrosion of the metal (stainless steel or nitinol), and providing a homogeneous surface for surface treatment and incorporation of various eluting drugs to prevent platelet aggregation while supporting endothelialization. The polyurethane surface was treated with a helium plasma for sterilization and promotes growth of cells. The paper details the performance of the coated film to expand with the metal stent up to 225 % during deployment. We present stress/strain behavior of polyurethane films, and subsequent plasma treatment of the surface and the adhesion of the coating to the stent structure upon expansion. A film of less than 25 tm was found to be sufficient for corrosion resistance and flexibility without producing any excess stress on the stent structure. Straining the film to 225 % and plasma modification did not affect the mechanical and surface properties while allowing for improved biocompatibility as determined by the critical surface tension, surface chemistry, and roughness.
Water as foaming agent for open cell polyurethane structures.
Haugen, H; Ried, V; Brunner, M; Will, J; Wintermantel, E
2004-04-01
The problem of moisture in polymer processing is known to any polymer engineer, as air bubbles may be formed. Hence granulates are generally dried prior to manufacturing. This study tried to develop a novel processing methods for scaffolds with controlled moisture content in thermoplastic polyurethane. The common foaming agents for polyurethane are organic solvents, whose residues remaining in the scaffold may be harmful to adherent cells, protein growth factors or nearby tissues. Water was used as a foaming agent and NaCl was used as porogens to achieve an open-cell structure. The polyether-polyurethane samples were processed in a heated press, and achieved a porosity of 64%. The pore size ranged between 50 and 500 microm. Human fibroblasts adhered and proliferate in the scaffold. A non-toxic production process was developed to manufacture a porous structure with a thermoplastic polyether-polyurethane. The process enables a mass-production of samples with adjustable pore size and porosity. In contrast to an existing method (solvent casting), the processing of the samples was not limited by its thickness. The process parameters, which attribute mostly to the pore building, were filling volume, temperature, NaCl-concentration and water-uptake rate.
Trinca, Rafael Bergamo; Abraham, Gustavo A; Felisberti, Maria Isabel
2015-11-01
Biocompatible polymeric scaffolds are crucial for successful tissue engineering. Biomedical segmented polyurethanes (SPUs) are an important and versatile class of polymers characterized by a broad spectrum of compositions, molecular architectures, properties and applications. Although SPUs are versatile materials that can be designed by different routes to cover a wide range of properties, they have been infrequently used for the preparation of electrospun nanofibrous scaffolds. This study reports the preparation of new electrospun polyurethane scaffolds. The segmented polyurethanes were synthesized using low molar masses macrodyols (poly(ethylene glycol), poly(l-lactide) and poly(trimethylene carbonate)) and 1,6-hexane diisocyanate and 1,4-butanodiol as isocyanate and chain extensor, respectively. Different electrospinning parameters such as solution properties and processing conditions were evaluated to achieve smooth, uniform bead-free fibers. Electrospun micro/nanofibrous structures with mean fiber diameters ranging from 600nm to 770nm were obtained by varying the processing conditions. They were characterized in terms of thermal and dynamical mechanical properties, swelling degree and morphology. The elastomeric polyurethane scaffolds exhibit interesting properties that could be appropriate as biomimetic matrices for soft tissue engineering applications. Copyright © 2015 Elsevier B.V. All rights reserved.
Chen, Yuan; Wang, Rui; Wang, Yonghui; Zhao, Weifeng; Sun, Shudong; Zhao, Changsheng
2017-05-01
In the present study, novel heparin-mimetic polyurethane hydrogels were prepared by introducing chemical crosslinked sulfated konjac glucomannan (SKGM). Scanning electron microscopy (SEM) results indicated that the introduction of SKGM and the increase of the molecular weight of diol segments could enlarge the pore sizes of the hydrogels. The swelling behavior corresponded with the SEM results, and the hydrogels could absorb more water after the modification. The modification also led to an improvement in the mechanical property. Meanwhile, the SKGM and the modified polyurethane hydrogels showed excellent hemocompatibility. The thromboplastin time of SKGM could reach up to 182.9s. Gentamycin sulfate (GS) was used as a model drug to be loaded into the hydrogels, and the loading amount was increased ca. 50% after the introduction of SKGM, thus resulting in high bactericidal efficiency. The results indicated that the introduction of SKGM and the alternation in the diol's molecular weight bestowed polyurethane hydrogels with promising properties of integrated blood-compatibility, mechanical properties and drug loading-releasing behavior. Therefore, the heparin-mimetic multifunctional polyurethane hydrogels have great potential to be used in biomedical applications. Copyright © 2017 Elsevier B.V. All rights reserved.
Strankowski, Michał; Korzeniewski, Piotr; Strankowska, Justyna; A S, Anu; Thomas, Sabu
2018-01-06
Polyurethane/graphene nanocomposites were synthesized using commercial thermoplastic polyurethane (TPU, Apilon 52DE55), and two types of graphene derivatives: graphene nanoplatelets (GNP) and reduced graphene oxide (RGO). Fourier Transformation Infrared Spectroscopy Fourier Transformation Infrared Spectroscopy (FTIR) spectroscopy, TEM, and SEM microscopy and XRD techniques were used to chemically and structurally characterize GNP and RGO nanofillers. The properties of the new TPU nanocomposite materials were studied using thermal analysis techniques (Dynamical Mechanical Analysis (DMA), Differential Scanning Calorimetry (DSC), Thermogravimetric Analysis (TG)) to describe the influence of graphene nanofillers on polyurethane matrix. Our investigation describes the comparison of two types of graphene derivatives, commercial one (GNP) and synthesized (RGO) on thermoplastic polyurethanes. These nanofillers provides opportunities to achieve compatibility with the TPU matrix. The property enhancements are attributed commonly to high aspect ratio of graphene nanoplatelets and filler-polymer interactions at the interface. The obtained nanocomposites exhibit higher thermal and mechanical properties due to the good dispersion of both nanofillers into TPU matrix. It was found that the addition of 2 wt % of the nanofiller could lead to a significant reinforcement effect on the TPU matrix. Also, with high content of nanofiller (GNP and RGO), the Payne effect was observed.
DOE Office of Scientific and Technical Information (OSTI.GOV)
Neilsen, Michael K.; Lu, Wei-Yang; Scherzinger, William M.
Numerous experiments were performed to characterize the mechanical response of several different rigid polyurethane foams (FR3712, PMDI10, PMDI20, and TufFoam35) to large deformation. In these experiments, the effects of load path, loading rate, and temperature were investigated. Results from these experiments indicated that rigid polyurethane foams exhibit significant volumetric and deviatoric plasticity when they are compressed. Rigid polyurethane foams were also found to be very strain-rate and temperature dependent. These foams are also rather brittle and crack when loaded to small strains in tension or to larger strains in compression. Thus, a new Unified Creep Plasticity Damage (UCPD) model wasmore » developed and implemented into SIERRA with the name Foam Damage to describe the mechanical response of these foams to large deformation at a variety of temperatures and strain rates. This report includes a description of recent experiments and experimental findings. Next, development of a UCPD model for rigid, polyurethane foams is described. Selection of material parameters for a variety of rigid polyurethane foams is then discussed and finite element simulations with the new UCPD model are compared with experimental results to show behavior that can be captured with this model.« less
Demir, D; Yılmaz, M S; Güven, M; Kara, A; Elden, H; Erkorkmaz, Ü
2018-06-13
To analyse the clinical outcomes of biodegradable synthetic polyurethane foam versus ribbon gauze and ear wick in the treatment of severe acute otitis externa. Ninety-two adults with severe acute otitis externa were randomly assigned to groups receiving ear wick (n = 28), ribbon gauze (n = 34) or biodegradable synthetic polyurethane foam (n = 30). Clinical efficacy, in terms of otalgia, oedema, erythema and tenderness of the external auditory canal, was assessed before packing was applied and at follow up on the 3rd and 7th days of presentation. All packing materials were associated with improved otalgia and oedema on the 3rd day; however, there were significant differences between biodegradable synthetic polyurethane foam and the other packing materials, and there was no significant reduction in tenderness in the biodegradable synthetic polyurethane foam group on the 3rd day. In the ribbon gauze and ear wick groups, improvements in all clinical efficacy scores were statistically significant for all pairwise comparisons. The three packing materials were all quite effective in treating severe acute otitis externa, but ear wick and ribbon gauze were superior to biodegradable synthetic polyurethane foam for relieving signs and symptoms, especially on the 3rd day.
Nano-engineered polyurethane resin-modified concrete.
DOT National Transportation Integrated Search
2014-04-01
The goal of the proposed work is to investigate the application of nano-engineered polyurethane (NEPU) emulsions for latex modified : concrete (LMC). NEPU emulsions are non-toxic, environment friendly, durable over a wide temperature range, provide b...
Soy-based UV resistant polyurethane pultruded composites.
DOT National Transportation Integrated Search
2012-02-01
Aliphatic polyurethane (PU) nanocomposites were synthesized using organically modified nanoclays. X-Ray diffraction results : confirmed good exfoliation of nanoclay particles in the PU resin system. With the addition of just 1% of nanoclay in the bas...
Some physical and mechanical properties of recycled polyurethane foam blends
NASA Astrophysics Data System (ADS)
Bledzki, A. K.; Zicans, J.; Merijs Meri, R.; Kardasz, D.
2008-09-01
Blends of secondary rigid polyurethane foams (RPUFs) with soft polyurethane foams (SPUFs) were investigated. The effect of SPUF content and its chemical nature on some physical and mechanical properties of the blends was evaluated. Owing to the stronger intermolecular interaction and higher values of cohesion energy, the blends of RPUFs with polyester SPUFs showed higher mechanical properties than those with polyether SPUFs. The density, hardness, ultimate strength, and the tensile, shear, and flexural moduli increased, while the impact toughness, ultimate elongation, and damping characteristics decreased with increasing RPUF content in the blends.
NASA Technical Reports Server (NTRS)
Chakar, A.
1984-01-01
A study of the properties and manufacturing techniques for long-fiber reinforced elastomeric composites for flexible and damping structural materials is presented. Attention is given to the usage of polyurethane in the matrix to obtain plastic elastomeric matrices and vitreous transition temperatures which vary from -80 C to 10 C, as well as assure good fiber adhesion. Various polyurethane formulations synthesized from diisocyanate prepolymers are examined in terms of mechanical and thermal properties. The principal reinforcing fiber selected is a unidirectional glass cloth.
Pantone, Vincenzo; Annese, Cosimo; Fusco, Caterina; Fini, Paola; Nacci, Angelo; Russo, Antonella; D'Accolti, Lucia
2017-02-21
An innovative and eco-friendly one-pot synthesis of bio-based polyurethanes is proposed via the epoxy-ring opening of epoxidized soybean oil (ESO) with methanol, followed by the reaction of methoxy bio-polyols intermediates with 2,6-tolyl-diisocyanate (TDI). Both synthetic steps, methanolysis and polyurethane linkage formation, are promoted by a unique catalyst, molybdenum(VI) dichloride dioxide (MoCl₂O₂), which makes this procedure an efficient, cost-effective, and environmentally safer method amenable to industrial scale-up.
NASA Astrophysics Data System (ADS)
Kocaefe, Duygu; Saha, Sudeshna
2012-04-01
High temperature heat-treatment of wood is a very valuable technique which improves many properties (biological durability, dimensional stability, thermal insulating characteristics) of natural wood. Also, it changes the natural color of wood to a very attractive dark brown color. Unfortunately, this color is not stable if left unprotected in external environment and turns to gray or white depending on the wood species. To overcome this problem, acrylic polyurethane coatings are applied on heat-treated wood to delay surface degradations (color change, loss of gloss, and chemical modifications) during aging. The acrylic polyurethane coatings which have high resistance against aging are further modified by adding bark extracts and/or lignin stabilizer to enhance their effectiveness in preventing the wood aging behavior. The aging characteristic of this coating is compared with acrylic polyurethane combined with commercially available organic UV stabilizers. In this study, their performance on three heat-treated North American wood species (jack pine, quaking aspen and white birch) are compared under accelerated aging conditions. Both the color change data and visual assessment indicate improvement in protective characteristic of acrylic polyurethane when bark extracts and lignin stabilizer are used in place of commercially available UV stabilizer. The results showed that although acrylic polyurethane with bark extracts and lignin stabilizer was more efficient compared to acrylic polyurethane with organic UV stabilizers in protecting heat-treated jack pine, it failed to protect heat-treated aspen and birch effectively after 672 h of accelerated aging. This degradation was not due to the coating adhesion loss or coating degradation during accelerated aging; rather, it was due to the significant degradation of heat-treated aspen and birch surface beneath this coating. The XPS results revealed formation of carbonyl photoproducts after aging on the coated surfaces and chain scission of Csbnd N of urethane linkages.
Follow up of injected polyurethane slab jacking.
DOT National Transportation Integrated Search
2003-08-01
GLENN JACKSON BRIDGE FOLLOW-UP REPORT The elevation monitoring in the report entitled Injected Polyurethane Slab Jacking (Soltesz 2000) is continued in this current report. The elevations of the concrete slabs are being monitored to see if polyuretha...
Mitigating ballast fouling and enhancing rail freight capacity.
DOT National Transportation Integrated Search
2012-11-01
In this report, an application using polyurethane void filling and particle bonding technology for stabilizing ballast is : evaluated. Application of rigid-polyurethane foam (RPF) as an in situ stabilization method does not require premixing : with a...
NASA Astrophysics Data System (ADS)
You, Gexin; Liu, Xinsen; Chen, Xiri; Yang, Bo; Zhou, Xiuwen
2018-06-01
In this study, a two-element model consisting of a non-linear spring and a viscous dashpot was proposed to simulate tensile curve of polyurethane fibers. The results showed that the two-element model can simulate the tensile curve of the polyurethane fibers better with a simple and applicable feature compared to the existing three-element model and four-element model. The effects of isocyanate index (R) on the hydrogen bond (H-bond) and the micro-phase separation of polyurethane fibers were investigated by Fourier transform infrared spectroscopy and x-ray pyrometer, respectively. The degree of H-bond and micro-phase separation increased first and then decreased as the R value increased, and gain a maximum at the value of 1.76, which is in good agreement with parameters viscosity coefficient η and the initial modulus c in the model.
Alginate based polyurethanes: A review of recent advances and perspective.
Zia, Khalid Mahmood; Zia, Fatima; Zuber, Mohammad; Rehman, Saima; Ahmad, Mirza Nadeem
2015-08-01
The trend of using biopolymers in combination with synthetic polymers was increasing rapidly from last two or three decades. Polysaccharide based biopolymers especially starch, cellulose, chitin, chitosan, alginate, etc. found extensive applications for different industrial uses, as they are biocompatible, biodegradable, bio-renewable resources and chiefly environment friendly. Segment block copolymer character of polyurethanes that endows them a broad range of versatility in terms of tailoring their properties was employed in conjunction with various natural polymers resulted in modified biomaterials. Alginate is biodegradable, biocompatible, bioactive, less toxic and low cost anionic polysaccharide, as a part of structural component of bacteria and brown algae (sea weed) is quite abundant in nature. It is used in combination with polyurethanes to form elastomers, nano-composites, hydrogels, etc. that especially revolutionized the food and biomedical industries. The review summarized the development in alginate based polyurethanes with their potential applications. Copyright © 2015 Elsevier B.V. All rights reserved.
Starch based polyurethanes: A critical review updating recent literature.
Zia, Fatima; Zia, Khalid Mahmood; Zuber, Mohammad; Kamal, Shagufta; Aslam, Nosheen
2015-12-10
Recent advancements in material science and technology made it obvious that use of renewable feed stock is the need of hour. Polymer industry steadily moved to get rid of its dependence on non-renewable resources. Starch, the second largest occurring biomass (renewable) on this planet provides a cheap and eco-friendly way to form huge variety of materials on blending with other biodegradable polymers. Specific structural versatility design for individual application and tailor-made properties have established the polyurethane (PU) as an important and popular class of synthetic biodegradable polymers. Blending of starch with polyurethane is relatively a developing area in PU chemistry but with lot of attraction for researchers. Herein, various starch based polyurethane materials including blends, grafts, copolymers, composites and nano-composites, as well as the prospects and latest developments are discussed. Additionally, an overview of starch based polymeric materials, including their potential applications are presented. Copyright © 2015 Elsevier Ltd. All rights reserved.
NASA Technical Reports Server (NTRS)
McGill, Preston; Wells, Doug; Morgan, Kristin
2006-01-01
Experimental evaluation of the basic fracture properties of Thermal Protection System (TPS) polyurethane foam insulation materials was conducted to validate the methodology used in estimating critical defect sizes in TPS applications on the Space Shuttle External Fuel Tank. The polyurethane foam found on the External Tank (ET) is manufactured by mixing liquid constituents and allowing them to react and expand upwards - a process which creates component cells that are generally elongated in the foam rise direction and gives rise to mechanical anisotropy. Similarly, the application of successive foam layers to the ET produces cohesive foam interfaces (knitlines) which may lead to local variations in mechanical properties. This study reports the fracture toughness of BX-265, NCFI 24-124, and PDL-1034 closed-cell polyurethane foam as a function of ambient and cryogenic temperatures and knitline/cellular orientation at ambient pressure.
NASA Technical Reports Server (NTRS)
Hilado, C. J.; Miller, C. M.
1976-01-01
Rankings of relative toxicity can be markedly affected by changes in test variables. Revision of the USF/NASA toxicity screening test procedure to eliminate the connecting tube and supporting floor and incorporate a 1.0 g sample weight, 200 C starting temperature, and 800 C upper limit temperature for pyrolysis, reversed the rankings of flexible polyurethane and polychloroprene foams, not only in relation to each other, but also in relation to cotton and red oak. Much of the change is attributed to reduction of the distance between the sample and the test animals, and reduction of the sample weight charged. Elimination of the connecting tube increased the relative toxicity of the polyurethane foams. The materials tested were flexible polyurethane foam, without and with fire retardant; rigid polyurethane foam with fire retardant; flexible polychloroprene foam; cotton, Douglas fir, red oak, hemlock, hardboard, particle board, polystyrene, and polymethyl methacrylate.
Padsalgikar, Ajay; Cosgriff-Hernandez, Elizabeth; Gallagher, Genevieve; Touchet, Tyler; Iacob, Ciprian; Mellin, Lisa; Norlin-Weissenrieder, Anna; Runt, James
2015-01-01
Polyurethane biostability has been the subject of intense research since the failure of polyether polyurethane pacemaker leads in the 1980s. Accelerated in vitro testing has been used to isolate degradation mechanisms and predict clinical performance of biomaterials. However, validation that in vitro methods reproduce in vivo degradation is critical to the selection of appropriate tests. High temperature has been proposed as a method to accelerate degradation. However, correlation of such data to in vivo performance is poor for polyurethanes due to the impact of temperature on microstructure. In this study, we characterize the lack of correlation between hydrolytic degradation predicted using a high temperature aging model of a polydimethylsiloxane-based polyurethane and its in vivo performance. Most notably, the predicted molecular weight and tensile property changes from the accelerated aging study did not correlate with clinical explants subjected to human biological stresses in real time through 5 years. Further, DMTA, ATR-FTIR, and SAXS experiments on samples aged for 2 weeks in PBS indicated greater phase separation in samples aged at 85°C compared to those aged at 37°C and unaged controls. These results confirm that microstructural changes occur at high temperatures that do not occur at in vivo temperatures. In addition, water absorption studies demonstrated that water saturation levels increased significantly with temperature. This study highlights that the multiphase morphology of polyurethane precludes the use of temperature accelerated biodegradation for the prediction of clinical performance and provides critical information in designing appropriate in vitro tests for this class of materials. © 2014 Wiley Periodicals, Inc.
Xiao, Meng; Xiao, Jiangwei; Wu, Gang; Ke, Yu; Fang, Liming; Deng, Chunlin; Liao, Hua
2018-06-01
Protein adsorption on biomaterial surfaces is clinically applied to increase therapeutic effects; however, this adsorption is possibly accompanied by conformational changes and results in loss of protein bioactivity or adverse reactions. In this research, a transforming growth factor β1 (TGF-β1) affinitive peptide HSNGLPL was grafted onto biopolymer surface to stabilize TGF-β1 spatial conformation after adhesion. The peptide with azide end group was combined with the propynyl pendant group on polyurethane via copper-catalyzed azide-alkyne cycloaddition (CuAAC) click reaction. The final polymer was characterized by Fourier transform infrared spectroscopy and proton nuclear magnetic resonance spectroscopy, which indicated that the affinitive peptide was introduced to the polymer. Quartz crystal microbalance with dissipation (QCM-D) was performed to monitor TGF-β1 adsorption and desorption on the surfaces coated with polyurethane with and without peptide combination. Results showed that TGF-β1 adhered on polyurethane surface and formed a compact and rigid layer. This layer showed spatial structural change but presented a loose and diffuse layer on the peptide-grafted polyurethane surface, indicating stable spatial conformation after adherence. Similar regulations were observed on the two surfaces where BSA layer was coated in advance. In vivo animal experiments revealed that immune reactions and tissue regenerations occurred earlier on peptide-modified polyurethane than on polyurethane, which did not undergo peptide grafting. This finding confirmed that affinitive interactions may preserve TGF-β1 bioactivity on polymer surface after adsorption. Copyright © 2018 Elsevier B.V. All rights reserved.
The biodurability of covering materials for metallic stents in a bile flow phantom.
Bang, Byoung Wook; Jeong, Seok; Lee, Don Haeng; Lee, Jung Il; Lee, Se Chul; Kang, Sung-Gwon
2012-04-01
Covered biliary metal stents have been introduced for the purpose of overcoming tumor ingrowth and treatment of benign biliary stricture. The aim of this study was to evaluate the biodurability of three commercially available biliary metal stent covering materials [e-PTFE (expanded polytetrafluoroethylene), silicone, and polyurethane] in a bile flow phantom. By operation of a peristaltic pump, human bile was circulated continuously in an experimental perfusion system containing covered metal stents. Each stent was removed, respectively, 1, 2, 4, and 6 months after bile exposure. We performed a gross inspection of the covered stents. The covering membrane was detached from the stent and observed by scanning electron microscopy (SEM). Finally, we measured tensile and tear strength of the membranes. Bile-staining of the membrane showed gradual progression after bile exposure; however, progress was the fastest in e-PTFE. SEM examination showed that the polyurethane surface was smooth, and the silicone surface was relatively smooth. However, e-PTFE had a rough and uneven surface. After bile exposure, there were no significant changes in polyurethane and silicone; however, biofilms and microcracks were observed in e-PTFE. In contrast to a gradual decrease of tensile/tear strength of polyurethane and silicone, those of e-PTFE showed a rapid reduction despite of the strongest baseline tensile and tear strength. e-PTFE tended to form biofilms more frequently than polyurethane and silicone during bile exposure. e-PTFE seemed to be less durable than silicone and polyurethane, however, as clinically applicable material because of strong absolute tensile/tear strengths.
Polyurethane foam for roadway stabilization NH Route 129, Loudon, NH.
DOT National Transportation Integrated Search
2016-12-12
This report summarizes the evaluation of the performance of polyurethane foam as a method of roadway : stabilization for a rural roadway experiencing substantial frost heaving. : NHDOT is responsible for many roads which have evolved from gravel road...
Polyurethane foam for roadway stabilization NH route 129, Loudon, NH.
DOT National Transportation Integrated Search
2016-12-12
This report summarizes the evaluation of the performance of polyurethane foam as a method of roadway : stabilization for a rural roadway experiencing substantial frost heaving. : NHDOT is responsible for many roads which have evolved from gravel road...
NASA Technical Reports Server (NTRS)
Russell, L. W.
1970-01-01
Open-celled polyurethane foam has a density of 8.3 pounds per cubic foot and a compressive strength of 295 to 325 psi. It is useful as a porous spacer in layered insulation and as an insulation material in vacuum tight systems.
Rigid open-cell polyurethane foam for cryogenic insulation
NASA Technical Reports Server (NTRS)
Faddoul, J. R.; Lindquist, C. R.; Niendorf, L. R.; Nies, G. E.; Perkins, P. J., Jr.
1971-01-01
Lightweight polyurethane foam assembled in panels is effective spacer material for construction of self-evacuating multilayer insulation panels for cryogenic liquid tanks. Spacer material separates radiation shields with barrier that minimizes conductive and convective heat transfer between shields.
Polyurethane foam infill for fiber-reinforced polymer (FRP) bridge deck panels.
DOT National Transportation Integrated Search
2014-05-01
The objective of the proposed research is to develop, test, and evaluate fiber-reinforced, polyurethane foams to replace the costly : honeycomb construction currently used to manufacture FRP bridge deck panels. The effort will focus on developing an ...
Biodegradation Of thermoplastic polyurethanes from vegetable oils
USDA-ARS?s Scientific Manuscript database
Thermoplastic urethanes based on polyricinoleic acid soft segments and MDI/BD hard segments with varied soft segment concentration were prepared. Soft segment concentration was varied fro, 40 to 70 wt %. Biodegradation was studied by respirometry. Segmented polyurethanes with soft segments based ...
Nonwoven glass fiber mat reinforces polyurethane adhesive
NASA Technical Reports Server (NTRS)
Roseland, L. M.
1967-01-01
Nonwoven glass fiber mat reinforces the adhesive properties of a polyurethane adhesive that fastens hardware to exterior surfaces of aluminum tanks. The mat is embedded in the uncured adhesive. It ensures good control of the bond line and increases the peel strength.
Fiber-modified polyurethane foam for ballistic protection
NASA Technical Reports Server (NTRS)
Fish, R. H.; Parker, J. A.; Rosser, R. W.
1975-01-01
Closed-cell, semirigid, fiber-loaded, self-extinguishing polyurethane foam material fills voids around fuel cells in aircraft. Material prevents leakage of fuel and spreading of fire in case of ballistic incendiary impact. It also protects fuel cell in case of exterior fire.
Modeling of skeletal members using polyurethane foam
DOE Office of Scientific and Technical Information (OSTI.GOV)
Sena, J.M.F.; Weaver, R.W.
1983-11-01
At the request of the University of New Mexico's Maxwell Museum of Anthropology, members of the Plastic Section in the Process Development Division at SNLA undertook the special project of the Chaco Lady. The project consisted of polyurethane foam casting of a disinterred female skull considered to be approximately 1000 years old. Rubber latex molds, supplied by the UNM Anthropology Department, were used to produce the polymeric skull requested. The authors developed for the project a modified foaming process which will be used in future polyurethane castings of archaeological artifacts and contemporary skeletal members at the University.
Zhang, Xianyu; Kim, Jin Seuk; Kwon, Younghwan
2017-04-01
Here we describe the synthesis of polyurethane (PU)-based energetic nanocomposites loaded with nano-aluminum (n-Al) particles. The energetic nanocomposite was prepared by polyurethane reaction of poly(glycidyl azide-co-tetramethylene glycol) (PGT) prepolymers and IPDI/N-100 isocyanates with simultaneous catalyst-free azide-alkyne Click reaction in the presence of n-Al. Initial study carried out with various n-Al/fluorinated PGT blends and demonstrated the potential of fluorinated PGT prepolymer for an energetic PU matrix. Thermal analysis of n-Al/fluorinated PGT-based PU energetic nanocomposite was performed using DSC and TGA.
Tiernan, Joan E.
1990-01-01
Highly concentrated and toxic petroleum-based and synthetic fuels wastewaters such as oil shale retort water are treated in a unit treatment process by electrolysis in a reactor containing oleophilic, ionized, open-celled polyurethane foams and subjected to mixing and laminar flow conditions at an average detention time of six hours. Both the polyurethane foams and the foam regenerate solution are re-used. The treatment is a cost-effective process for waste-waters which are not treatable, or are not cost-effectively treatable, by conventional process series.
NASA Astrophysics Data System (ADS)
Ksenofontov, M. A.; Bobkova, E. Yu.; Shundalau, M. B.; Ostrovskaya, L. E.; Vasil'eva, V. S.
2017-11-01
The interaction of the functional groups in the polyurethane foam adsorbent Penopurm® with the cations of some 3d-metals upon their extraction from aqueous solutions has been studied by atomic emission spectroscopy, UV/Vis and vibrational IR spectroscopy, and quantum chemical simulation using density functional theory. Penopurm® absorbs 3d-metal cations from aqueous solutions in the pH range 5-7. Some spectral criteria have been found indicating a predominant interaction of Ni2+ ions with various fragments of the polyurethane foam structure.
Relative toxicity of pyrolysis products of some polyurethane and polychloroprene foams
NASA Technical Reports Server (NTRS)
Hilado, C. J.; Slattengren, C. L.; Kourtides, D. A.; Parker, J. A.
1977-01-01
Results of toxicity screening tests on some polyurethane and polychloroprene flexible foams are presented. The test method involves the exposure of four Swiss albino male mice in a 4.2-liter hemispherical chamber to the pyrolysis effluents from 1 g of sample exposed to temperatures rising from 200 to 800 C at a rate of 40 C/min. Mortality and times to incapacitation and to death are recorded. Comparisons indicate that flexible polyurethane foams without fire retardant are more toxic than the corresponding foams containing fire retardant, and polychloroprene foams are least toxic.
Development of Styrene-Grafted Polyurethane by Radiation-Based Techniques
Jeong, Jin-Oh; Park, Jong-Seok; Lim, Youn-Mook
2016-01-01
Polyurethane (PU) is the fifth most common polymer in the general consumer market, following Polypropylene (PP), Polyethylene (PE), Polyvinyl chloride (PVC), and Polystyrene (PS), and the most common polymer for thermosetting resins. In particular, polyurethane has excellent hardness and heat resistance, is a widely used material for electronic products and automotive parts, and can be used to create products of various physical properties, including rigid and flexible foams, films, and fibers. However, the use of polar polymer polyurethane as an impact modifier of non-polar polymers is limited due to poor combustion resistance and impact resistance. In this study, we used gamma irradiation at 25 and 50 kGy to introduce the styrene of hydrophobic monomer on the polyurethane as an impact modifier of the non-polar polymer. To verify grafted styrene, we confirmed the phenyl group of styrene at 690 cm−1 by Attenuated Total Reflection Fourier Transform Infrared Spectroscopy (ATR-FTIR) and at 6.4–6.8 ppm by 1H-Nuclear Magnetic Resonance (1H-NMR). Scanning Electron Microscope (SEM), X-ray Photoelectron Spectroscopy (XPS), Thermogravimetric Analysis (TGA) and contact angle analysis were also used to confirm styrene introduction. This study has confirmed the possibility of applying high-functional composite through radiation-based techniques. PMID:28773561
Yu, Ya-Jen; Hearon, Keith; Wilson, Thomas S; Maitland, Duncan J
2011-08-01
The effect of moisture absorption on the glass transition temperature (T(g)) and stress/strain behavior of network polyurethane shape memory polymer (SMP) foams has been investigated. With our ultimate goal of engineering polyurethane SMP foams for use in blood contacting environments, we have investigated the effects of moisture exposure on the physical properties of polyurethane foams. To our best knowledge, this study is the first to investigate the effects of moisture absorption at varying humidity levels (non-immersion and immersion) on the physical properties of polyurethane SMP foams. The SMP foams were exposed to differing humidity levels for varying lengths of time, and they exhibited a maximum water uptake of 8.0% (by mass) after exposure to 100% relative humidity for 96 h. Differential scanning calorimetry results demonstrated that water absorption significantly decreased the T(g) of the foam, with a maximum water uptake shifting the T(g) from 67 °C to 5 °C. Samples that were immersed in water for 96 h and immediately subjected to tensile testing exhibited 100% increases in failure strains and 500% decreases in failure stresses; however, in all cases of time and humidity exposure, the plasticization effect was reversible upon placing moisture-saturated samples in 40% humidity environments for 24 h.
Yu, Ya-Jen; Hearon, Keith; Wilson, Thomas S.; Maitland, Duncan J.
2011-01-01
The effect of moisture absorption on the glass transition temperature (Tg) and stress/strain behavior of network polyurethane shape memory polymer (SMP) foams has been investigated. With our ultimate goal of engineering polyurethane SMP foams for use in blood contacting environments, we have investigated the effects of moisture exposure on the physical properties of polyurethane foams. To our best knowledge, this study is the first to investigate the effects of moisture absorption at varying humidity levels (non-immersion and immersion) on the physical properties of polyurethane SMP foams. The SMP foams were exposed to differing humidity levels for varying lengths of time, and they exhibited a maximum water uptake of 8.0% (by mass) after exposure to 100% relative humidity for 96 h. Differential scanning calorimetry results demonstrated that water absorption significantly decreased the Tg of the foam, with a maximum water uptake shifting the Tg from 67 °C to 5 °C. Samples that were immersed in water for 96 h and immediately subjected to tensile testing exhibited 100% increases in failure strains and 500% decreases in failure stresses; however, in all cases of time and humidity exposure, the plasticization effect was reversible upon placing moisture-saturated samples in 40% humidity environments for 24 h. PMID:21949469
Leite, Fábio Renato Manzolli; Ramalho, Lizeti Toledo de Oliveira
2008-01-01
Innocuous biocompatible materials have been searched to repair or reconstruct bone defects. Their goal is to restore the function of live or dead tissues. This study compared connective tissue and bone reaction when exposed to demineralized bovine bone matrix and a polyurethane resin derived from castor bean (Ricinus communis). Forty-five rats were assigned to 3 groups of 15 animals (control, bovine bone and polyurethane). A cylindrical defect was created on mandible base and filled with bovine bone matrix and the polyurethane. Control group received no treatment. Analyses were performed after 15, 45 and 60 days (5 animals each). Histological analysis revealed connective tissue tolerance to bovine bone with local inflammatory response similar to that of the control group. After 15 days, all groups demonstrated similar outcomes, with mild inflammatory reaction, probably due to the surgical procedure rather than to the material. In the polymer group, after 60 days, scarce multinucleated cells could still be observed. In general, all groups showed good stability and osteogenic connective tissue with blood vessels into the surgical area. The results suggest biocompatibility of both materials, seen by their integration into rat mandible. Moreover, the polyurethane seems to be an alternative in bone reconstruction and it is an inexhaustible source of biomaterial. PMID:19089203
Wang, Ning; Burugapalli, Krishna; Wijesuriya, Shavini; Far, Mahshid Yazdi; Song, Wenhui; Moussy, Francis; Zheng, Yudong; Ma, Yanxuan; Wu, Zhentao; Li, Kang
2014-01-01
The aim of this study was to introduce bioactivity to the electrospun coating for implantable glucose biosensors. Coaxial fibre membranes having polyurethane as the core and gelatin as the shell were produced using a range of polyurethane concentrations (2, 4, 6 & 8% wt/v) while keeping gelatin concentration (10% wt/v) constant in 2,2,2-trifluoroethanol. The gelatin shell was stabilized using glutaraldehyde vapour. The formation of core-shell structure was confirmed using TEM, SEM and FTIR. The coaxial fibre membranes showed uniaxial tensile properties intermediate to that of the pure polyurethane and the gelatin fibre membranes. The gelatin shell increased hydrophilicity and glucose transport flux across the coaxial fibre membranes. The coaxial fibre membranes having small fibre diameter (541 nm) and a thick gelatin shell (52%) did not affect the sensor sensitivity, but decreased sensor’s linearity in the long run. In contrast, thicker coaxial fibre membranes (1133 nm) having a thin gelatin shell (34%) maintained both sensitivity and linearity till 84 days of the study period. To conclude, polyurethane-gelatin co-axial fibre membranes, due to their faster permeability to glucose, tailorable mechanical properties and bioactivity are potential candidates for coatings to favourably modify the host responses to extend the reliable in vivo lifetime of implantable glucose biosensors. PMID:24346001
Padois, Karine; Bertholle, Valérie; Pirot, Fabrice; Hyunh, Truc Thanh Ngoc; Rossi, Alessandra; Colombo, Paolo; Falson, Françoise; Sonvico, Fabio
2012-12-01
The widespread use of indwelling medical devices has enormously increased the interest in materials incorporating antibiotics and antimicrobial agents as a means to prevent dangerous device-related infections. Recently, chlorhexidine-loaded polyurethane has been proposed as a material suitable for the production of devices which are able to resist microbial contamination. The aim of the present study was to characterize the in vitro release of chlorhexidine from new polymeric orthodontic chains realized with polyurethane loaded with two different chlorhexidine salts: chlorhexidine diacetate or chlorhexidine digluconate. The orthodontic chains constituted of three layers: a middle polyurethane layer loaded with chlorhexidine salt inserted between two layers of unloaded polymer. In vitro release of chlorhexidine diacetate and digluconate from orthodontic chains loaded with 10% or 20% (w/w) chlorhexidine salt was sustained for 42 days and followed Fickian diffusion. The drug diffusion through the polyurethane was found to be dependent not only on chlorhexidine loading, but also on the type of chlorhexidine salt. The antibacterial activity of 0.2% (w/w) chlorhexidine diacetate-loaded orthodontic chain was successfully tested towards clinically isolated biofilm forming ica-positive Staphylococcus epidermidis via agar diffusion test. In conclusion, the chlorhexidine salt-loaded chains could provide an innovative approach in the prevention of oral infections related to the use of orthodontic devices.
NASA Astrophysics Data System (ADS)
Yu, Ya-Jen; Hearon, Keith; Wilson, Thomas S.; Maitland, Duncan J.
2011-08-01
The effect of moisture absorption on the glass transition temperature (Tg) and the stress/strain behavior of network polyurethane shape memory polymer (SMP) foams has been investigated. With our ultimate goal of engineering polyurethane SMP foams for use in blood-contacting environments, we have investigated the effects of moisture exposure on the physical properties of polyurethane foams. To the best of our knowledge, this study is the first to investigate the effects of moisture absorption at varying humidity levels (non-immersion and immersion) on the physical properties of polyurethane SMP foams. The SMP foams were exposed to differing humidity levels for varying lengths of time, and they exhibited a maximum water uptake of 8.0% (by mass) after exposure to 100% relative humidity for 96 h. Differential scanning calorimetry results demonstrated that water absorption significantly decreased the Tg of the foam, with a maximum water uptake shifting the Tg from 67 to 5 °C. Samples that were immersed in water for 96 h and immediately subjected to tensile testing exhibited 100% increases in failure strains and 500% decreases in failure stresses; however, in all cases of time and humidity exposure, the plasticization effect was reversible upon placing moisture-saturated samples in 40% humidity environments for 24 h.
Korzeniewski, Piotr; Strankowska, Justyna; A. S., Anu; Thomas, Sabu
2018-01-01
Polyurethane/graphene nanocomposites were synthesized using commercial thermoplastic polyurethane (TPU, Apilon 52DE55), and two types of graphene derivatives: graphene nanoplatelets (GNP) and reduced graphene oxide (RGO). Fourier Transformation Infrared Spectroscopy Fourier Transformation Infrared Spectroscopy (FTIR) spectroscopy, TEM, and SEM microscopy and XRD techniques were used to chemically and structurally characterize GNP and RGO nanofillers. The properties of the new TPU nanocomposite materials were studied using thermal analysis techniques (Dynamical Mechanical Analysis (DMA), Differential Scanning Calorimetry (DSC), Thermogravimetric Analysis (TG)) to describe the influence of graphene nanofillers on polyurethane matrix. Our investigation describes the comparison of two types of graphene derivatives, commercial one (GNP) and synthesized (RGO) on thermoplastic polyurethanes. These nanofillers provides opportunities to achieve compatibility with the TPU matrix. The property enhancements are attributed commonly to high aspect ratio of graphene nanoplatelets and filler–polymer interactions at the interface. The obtained nanocomposites exhibit higher thermal and mechanical properties due to the good dispersion of both nanofillers into TPU matrix. It was found that the addition of 2 wt % of the nanofiller could lead to a significant reinforcement effect on the TPU matrix. Also, with high content of nanofiller (GNP and RGO), the Payne effect was observed. PMID:29316638
NASA Astrophysics Data System (ADS)
Gultom, G.; Wirjosentono, B.; Ginting, M.; Sebayang, K.
2017-07-01
Microwave-absorptive polymeric composite materials are becoming important to protect interference of any communication systems due to increasing use of microwave-inducing devices. In this work, the microwave-absorptive polyurethane nanocomposites were prepared using natural zeolites of Sarulla North Sumatra and commercial ferric oxide as fillers. Weight ratios of the polyurethane to natural zeolite and ferric oxide were varied (90%:6%:4%; 80%:12%:8%; 70%:24%:6%) by weight. The fillers were prepared using ball milling technique and characterized for their particle size distributions using Particle Size Analyzer. The nanocomposites, prepared using in-situ reaction of polyethylene glycol, toluene diisocyanate and fillers. The complex permittivity (ε’and ε”) and complex permeability (μ’ and μ”) as electromagnetic properties were calculated using NRW method after collecting real and imaginary S parameter using Vector Network Analyzer measurement at X band frequency. Results show ratio of the fillers will affect the permeability, permittivity and reflection loss of the materials. The best reflection loss was shown -40.588 dB (>99 % absorption) at ratio for polyurethane : nanozeolite : ferric oxide (80%:12%:8%) by weight observed at 10.92 GHz. According to the measurement and calculation was shown the polyurethane filled with natural nanozeolite and ferric oxide is a good electromagnetic wave attenuation material.
Cell–material interactions on biphasic polyurethane matrix
Dicesare, Patrick; Fox, Wade M.; Hill, Michael J.; Krishnan, G. Rajesh; Yang, Shuying; Sarkar, Debanjan
2013-01-01
Cell–matrix interaction is a key regulator for controlling stem cell fate in regenerative tissue engineering. These interactions are induced and controlled by the nanoscale features of extracellular matrix and are mimicked on synthetic matrices to control cell structure and functions. Recent studies have shown that nanostructured matrices can modulate stem cell behavior and exert specific role in tissue regeneration. In this study, we have demonstrated that nanostructured phase morphology of synthetic matrix can control adhesion, proliferation, organization and migration of human mesenchymal stem cells (MSCs). Nanostructured biodegradable polyurethanes (PU) with segmental composition exhibit biphasic morphology at nanoscale dimensions and can control cellular features of MSCs. Biodegradable PU with polyester soft segment and hard segment composed of aliphatic diisocyanates and dipeptide chain extender were designed to examine the effect polyurethane phase morphology. By altering the polyurethane composition, morphological architecture of PU was modulated and its effect was examined on MSC. Results show that MSCs can sense the nanoscale morphology of biphasic polyurethane matrix to exhibit distinct cellular features and, thus, signifies the relevance of matrix phase morphology. The role of nanostructured phases of a synthetic matrix in controlling cell–matrix interaction provides important insights for regulation of cell behavior on synthetic matrix and, therefore, is an important tool for engineering tissue regeneration. PMID:23255285
WEATHERING DEGRADATION OF A POLYURETHANE COATING. (R828081E01)
The degradation of polyurethane topcoat over a chromate pigmented epoxy primer was examined by atomic force microscopy (AFM), scanning electronic microscopy (SEM), X-ray photo-electron spectroscopy (XPS) and Fourier transform infra-red spectroscopy (FTIR) after the coated pane...
Preparation of highly fluorinated polyurethanes
NASA Technical Reports Server (NTRS)
Rochow, S. E.; Stump, E. C., Jr.
1971-01-01
New polyurethanes, formed from a reaction of a prepolymer diol and a perfluorinated diisocyanate, are nonflammable and possess high corrosion resistance and good low temperature flexibility. Polymer hardness increases rapidly with increasing ratio of diisocaynate to diol, but its glass transition temperature is not adversely affected.
Field Evaluations Test Plan for Validation of Alternatives to Aliphatic Isocyanate Polyurethanes
NASA Technical Reports Server (NTRS)
Lewis, Pattie
2005-01-01
The objective of this project is to qualify candidate alternatives to Aliphatic Isocyanate Polyurethane coatings under the specifications for the standard system. This project will compare coating performance of the proposed alternatives to existing coating systems or standards.
Thoma, Steven G.; Grubelich, Mark C; Celina, Mathias C.; Vaughn, Mark R.; Knudsen, Steven D.
2017-05-23
A self-consuming structure is disclosed that is formed from a self-consuming composition based on an epoxy or polyurethane having fuel and/or oxidizer molecularly dispersed and/or as particulates in the epoxy or polyurethane. The composition may be used to form self-consuming structural components.
The relationship between onsite manufacture of spray polyurethane foam insulation (SPFI) and potential exposures is not well understood. Currently, no comprehensive standard test methods exist for characterizing and quantifying product emissions. Exposures to diisocyanate compoun...
The accumulation of dust mite allergens on mattresses made of different kinds of materials.
Visitsunthorn, Nualanong; Chirdjirapong, Varakorn; Pootong, Visanu; Jirapongsananuruk, Orathai; Pacharn, Punchama; Weeravejsukit, Sirirat; Mahakittikun, Vanna; Vichyanond, Pakit
2010-01-01
Different mattress materials may affect the accumulation of allergens. To compare the amount of group 1 dust mite allergens (Der p1 + Der f1) on mattresses made of different kinds of materials before and after use. Sixty new mattresses made of kapok, synthetic fiber, coconut fiber and sponge-like polyurethane, were placed in the house officers' dormitory at Siriraj hospital, Thailand. The dust samples were collected before (0), 1, 2, 3, 6, 9 and 12 months after the mattresses were used. Group 1 dust mite allergens were analyzed using two-site monoclonal antibody ELISA. Der f1 made up 86.7 % of group 1 allergens found in the matress dust. After the 2nd month, only the mean level in sponge-like polyurethane mattress was under 2 microg/g dust (sensitized level). At the 6th month, the mean levels were 13.1 in coconut, 21.7 in kapok and 17.3 microg/g dust in synthetic fiber, all of which were more than 10 microg/g dust (symptomatic level). At the 9th month, the level in sponge-like polyurethane mattress was increased to 11.2 microg/g. At 12th month the level in coconut fiber, sponge-like polyurethane synthetic fiber and kapok mattresses were 20.2, 22.4, 28.9 and 32.2 microg/g dust respectively. The accumulation rate in kapok and synthetic mattresses was significantly higher than coconut and sponge-like polyurethane mattresses. The mean level of group 1 mite allergens exceeded 10 microg/g dust after the 6th month of use in coconut fiber, kapok and synthetic fiber and at the 9th month in sponge-like polyurethane mattress.
Chemical speciation of polyurethane polymers by soft-x-ray spectromicroscopy
DOE Office of Scientific and Technical Information (OSTI.GOV)
Rightor, E.G.; Hitchcock, A.P.; Urquhart, S.G.
1997-04-01
Polyurethane polymers are a versatile class of materials which have numerous applications in modern life, from automotive body panels, to insulation, to household furnishings. Phase segregation helps to determine the physical properties of several types of polyurethanes. Polymer scientists believe that understanding the connections between formulation chemistry, the chemical nature of the segregated phases, and the physical properties of the resulting polymer, would greatly advance development of improved polyurethane materials. However, the sub-micron size of segregated features precludes their chemical analysis by existing methods, leaving only indirect means of characterizing these features. For the past several years the authors havemore » been developing near edge X-ray absorption spectromicroscopy to study the chemical nature of individual segregated phases. Part of this work has involved studies of molecular analogues and model polymers, in conjunction with quantum calculations, in order to identify the characteristic near edge spectral transitions of important chemical groups. This spectroscopic base is allowing the authors to study phase segregation in polyurethanes by taking advantage of several unique capabilities of scanning transmission x-ray microscopy (STXM) - high spatial resolution ({approximately} 0.1 {mu}m), high spectral resolution ({approximately}0.1 eV at the C 1s edge), and the ability to record images and spectra with relatively low radiation damage. The beamline 7.0 STXM at ALS is being used to study microtomed sections or cast films of polyurethanes. Based on the pioneering work of Ade, Kirz and collaborators at the NSLS X-1A STXM, it is clear that scanning X-ray transmission microscopy using soft X-rays can provide information about the chemical origin of phase segregation in radiation-sensitive materials on a sub-micron scale. This information is difficult or impossible to obtain by other means.« less
Characterization of a resorbable poly(ester urethane) with biodegradable hard segments.
Dempsey, David K; Robinson, Jennifer L; Iyer, Ananth V; Parakka, James P; Bezwada, Rao S; Cosgriff-Hernandez, Elizabeth M
2014-01-01
The rapid growth of regenerative medicine and drug delivery fields has generated a strong need for improved polymeric materials that degrade at a controlled rate into safe, non-cytotoxic by-products. Polyurethane thermoplastic elastomers offer several advantages over other polymeric materials including tunable mechanical properties, excellent fatigue strength, and versatile processing. The variable segmental chemistry in developing resorbable polyurethanes also enables fine control over the degradation profile as well as the mechanical properties. Linear aliphatic isocyanates are most commonly used in biodegradable polyurethane formulations; however, these aliphatic polyurethanes do not match the mechanical properties of their aromatic counterparts. In this study, a novel poly(ester urethane) (PEsU) synthesized with biodegradable aromatic isocyanates based on glycolic acid was characterized for potential use as a new resorbable material in medical devices. Infrared spectral analysis confirmed the aromatic and phase-separated nature of the PEsU. Uniaxial tensile testing displayed stress-strain behavior typical of a semi-crystalline polymer above its Tg, in agreement with calorimetric findings. PEsU outperformed aliphatic PCL-based polyurethanes likely due to the enhanced cohesion of the aromatic hard domains. Accelerated degradation of the PEsU using 0.1 M sodium hydroxide resulted in hydrolysis of the polyester soft segment on the surface, reduced molecular weight, surface cracking, and a 30% mass loss after four weeks. Calorimetric studies indicated a disruption of the soft segment crystallinity after incubation which corresponded with a drop in initial modulus of the PEsU. Finally, cytocompatibility testing with 3T3 mouse fibroblasts exhibited cell viability on PEsU films comparable to a commercial poly(ether urethane urea) after 24 h followed by 85% cell viability at 72 h. Overall, this new resorbable polyurethane shows strong potential for use in wide range of biomedical applications.
DOE Office of Scientific and Technical Information (OSTI.GOV)
Yang Yong; Zhou Yuming, E-mail: ymzhou@seu.edu.cn; Ge Jianhua
Optically active polyurethane/titania/silica (LPU/TiO{sub 2}/SiO{sub 2}) multilayered core-shell composite microspheres were prepared by the combination of titania deposition on the surface of silica spheres and subsequent polymer grafting. LPU/TiO{sub 2}/SiO{sub 2} was characterized by FT-IR, UV-vis spectroscopy, X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS), thermogravimetric analysis (TGA), SEM and TEM, and the infrared emissivity value (8-14 {mu}m) was investigated in addition. The results indicated that titania and polyurethane had been successfully coated onto the surfaces of silica microspheres. LPU/TiO{sub 2}/SiO{sub 2} exhibited clearly multilayered core-shell construction. The infrared emissivity values reduced along with the increase of covering layers thus provedmore » that the interfacial interactions had direct influence on the infrared emissivity. Besides, LPU/TiO{sub 2}/SiO{sub 2} multilayered microspheres based on the optically active polyurethane took advantages of the orderly secondary structure and strengthened interfacial synergistic actions. Consequently, it possessed the lowest infrared emissivity value. - Graphical Abstract: Optically active polyurethane/titania/silica (LPU/TiO{sub 2}/SiO{sub 2}) multilayered core-shell composite microspheres were prepared by the combination of titania deposition on the surface of silica spheres and subsequent polymer grafting. Highlights: > Optically active polyurethane based on tyrosine was used for the modification of nanoparticles. > LPU/TiO{sub 2}/SiO{sub 2} multilayered core-shell microspheres were prepared and characterized. > Interfacial interactions and secondary structure affected the infrared emissivity of composite.« less
Do You Have Work-Related Asthma? A Guide for You and Your Doctor
... Polyurethane foam • Paints, lacquers, ink, varnishes, sealants, finishes • Insulation materials • Polyurethane rubber • Glues and adhesives • Car manufacture and repair • Building construction (plaster, insulation) • Foam blowing and cutting • Painting • Truck bed liner ...
Code of Federal Regulations, 2014 CFR
2014-07-01
... commercial refrigeration—Rigid polyurethane sandwich panels. HCFC-22; HCFC-142b as substitutes for HCFC-141b... commercial refrigeration, and sandwich panels. —Rigid polyurethane slabstock and other foams. —Polystyrene...
Code of Federal Regulations, 2013 CFR
2013-07-01
... commercial refrigeration—Rigid polyurethane sandwich panels. HCFC-22; HCFC-142b as substitutes for HCFC-141b... commercial refrigeration, and sandwich panels. —Rigid polyurethane slabstock and other foams. —Polystyrene...
Code of Federal Regulations, 2012 CFR
2012-07-01
... commercial refrigeration—Rigid polyurethane sandwich panels. HCFC-22; HCFC-142b as substitutes for HCFC-141b... commercial refrigeration, and sandwich panels. —Rigid polyurethane slabstock and other foams. —Polystyrene...
Code of Federal Regulations, 2011 CFR
2011-07-01
... commercial refrigeration—Rigid polyurethane sandwich panels. HCFC-22; HCFC-142b as substitutes for HCFC-141b... commercial refrigeration, and sandwich panels. —Rigid polyurethane slabstock and other foams. —Polystyrene...
Code of Federal Regulations, 2010 CFR
2010-07-01
... commercial refrigeration—Rigid polyurethane sandwich panels. HCFC-22; HCFC-142b as substitutes for HCFC-141b... commercial refrigeration, and sandwich panels. —Rigid polyurethane slabstock and other foams. —Polystyrene...
Improved primer for bonding polyurethane adhesives to metals
NASA Technical Reports Server (NTRS)
Constanza, L. J.
1969-01-01
Primer ensures effective bonding integrity of polyurethane adhesives on metal surfaces at temperatures ranging from minus 423 degrees to plus 120 degrees F. It provides greater metal surface protection and bond strengths over this temperature range than could be attained with other adhesive systems.
Polyurethane adhesive with improved high temperature properties
NASA Technical Reports Server (NTRS)
Stuckey, J. M.
1977-01-01
A polyurethane resin with paste activator, capable of providing useful bond strengths over the temperature range of -184 C to 149 C, is described. The adhesive system has a pot life of over one hour. Tensile shear strength ratings are given for various adhesive formulations.
Joint Test Protocol for Validation of Alternatives to Aliphatic Isocyanate Polyurethanes
NASA Technical Reports Server (NTRS)
Lewis, Pattie
2005-01-01
The primary objective of this effort is to demonstrate and validate alternatives to aliphatic isocyanate polyurethanes. Successful completion of this project will result in one or more isocyanate-free coatings qualified for use at AFSPC and NASA installations participating in this project.
The relationship between onsite manufacture of spray polyurethane foam insulation (SPFI) and potential exposures to diisocyanates, amines, flame retardants (FRs), blowing agents, aldehydes and other organic compounds that may be emitted from SPFI is not well understood. EPA is de...
Thermoplastic composites for veneering posterior teeth-a feasibility study.
Gegauff, Anthony G; Garcia, Jose L; Koelling, Kurt W; Seghi, Robert R
2002-09-01
This pilot study was conducted to explore selected commercially-available thermoplastic composites that potentially had physical properties superior to currently available dental systems for restoring esthetic posterior crowns. Polyurethane, polycarbonate, and poly(ethylene/tetrafluoroethylene) (ETFE) composites and unfilled polyurethane specimens were injection molded to produce shapes adaptive to five standardized mechanical tests. The mechanical testing included abrasive wear rate, yield strength, apparent fracture toughness (strength ratio), flexural strength, and compressive strength. Compared to commercially available dental composites, abrasion wear rates were lower for all materials tested, yield strength was greater for the filled polycarbonates and filled polyurethane resins, fracture toughness testing was invalid (strength ratios were calculated for comparison of the pilot test materials), flexural strength was roughly similar except for the filled ETFE which was significantly greater, and compressive strength was lower. Commercially available thermoplastic resin composites, such as polyurethane, demonstrate the potential for development of an artificial crown material which exceeds the mechanical properties of currently available esthetic systems, if compressive strength can be improved.
Abd El-Fattah, M; Hasan, Abdulraheim M A; Keshawy, Mohamed; El Saeed, Ashraf M; Aboelenien, Ossama M
2018-03-01
Nanocrystalline cellulose (NCC) and micro-powdered cellulose (MPC) were extracted from rice straw by mechanical and alkali treatment methods, then characterized via infrared spectroscopy and dynamic light scattering. A series of polyurethane nanocrystalline cellulose composite (PNCCC) and polyurethane micro-powdered cellulose composite (PMPCC) coatings were prepared with various loading levels of NCC and MPC from 0.5 to 2.0 wt.%, and the coatings were applied onto the pretreated mild steel substrate at room temperature. The results showed that the NCC and MPC influenced positively the studied properties of the polyurethane coating; furthermore the most pronounced anticorrosive properties were obtained at 1 wt.% NCC and MPC, as confirmed by open circuit potential (OCP) study, electrochemical impedance spectroscopy (EIS) study and salt spray test. However, the optimum enhancement of mechanical properties was found at 1.5 wt.% loading level, after which further loading of NCC and MPC led to the reduction in the mechanical properties. Copyright © 2018 Elsevier Ltd. All rights reserved.
Gabriel, Laís P; Santos, Maria Elizabeth M Dos; Jardini, André L; Bastos, Gilmara N T; Dias, Carmen G B T; Webster, Thomas J; Maciel Filho, Rubens
2017-01-01
In this work, thermoset polyurethane composites were prepared by the addition of hydroxyapatite nanoparticles using the reactants polyol polyether and an aliphatic diisocyanate. The polyol employed in this study was extracted from the Euterpe oleracea Mart. seeds from the Amazon Region of Brazil. The influence of hydroxyapatite nanoparticles on the structure and morphology of the composites was studied using scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS), the structure was evaluated by Fourier transform infrared spectroscopy (FT-IR), thermal properties were analyzed by thermogravimetry analysis (TGA), and biological properties were studied by in vitro and in vivo studies. It was found that the addition of HA nanoparticles promoted fibroblast adhesion while in vivo investigations with histology confirmed that the composites promoted connective tissue adherence and did not induce inflammation. In this manner, this study supports the further investigation of bio-based, polyurethane/hydroxyapatite composites as biocompatible scaffolds for numerous tissue engineering applications. Copyright © 2016 Elsevier Inc. All rights reserved.
Preparation and properties of adjacency crosslinked polyurethane-urea elastomers
NASA Astrophysics Data System (ADS)
Wu, Yuan; Cao, Yu-Yang; Wu, Shou-Peng; Li, Zai-Feng
2012-12-01
Adjacency crosslinked polyurethane-urea (PUU) elastomers with different crosslinking density were prepared by using hydroxyl-terminated liquid butadiene-nitrile (HTBN), toluene diisocyanate (TDI) and chain extender 3,5-dimethyl thio-toluene diamine (DMTDA) as raw materials, dicumyl peroxide (DCP) as initiator, and N,N'-m-phenylene dimaleimide (HVA-2) as the crosslinking agent. The influences of the crosslinking density and temperature on the structure and properties of such elastomers were investigated. The crosslinking density of PUU elastomer was tested by the NMR method. It is found that when the content of HVA-2 is 1.5%, the mechanical properties of polyurethane elastomer achieve optimal performance. By testing thermal performance of PUU, compared with linear PUU, the thermal stability of the elastomers has a marked improvement. With the addition of HVA-2, the loss factor tan δ decreases. FT-IR spectral studies of PUU elastomer at various temperatures were performed. From this study, heat-resistance polyurethane could be prepared, and the properties of PUU at high temperature could be improved obviously.
Hafeman, Andrea E.; Li, Bing; Yoshii, Toshitaka; Zienkiewicz, Katarzyna; Davidson, Jeffrey M.; Guelcher, Scott A.
2013-01-01
Purpose The purpose of this work was to investigate the effects of triisocyanate composition on the biological and mechanical properties of biodegradable, injectable polyurethane scaffolds for bone and soft tissue engineering. Methods Scaffolds were synthesized using reactive liquid molding techniques, and were characterized in vivo in a rat subcutaneous model. Porosity, dynamic mechanical properties, degradation rate, and release of growth factors were also measured. Results Polyurethane scaffolds were elastomers with tunable damping properties and degradation rates, and they supported cellular infiltration and generation of new tissue. The scaffolds showed a two-stage release profile of platelet-derived growth factor, characterized by a 75% burst release within the first 24 h and slower release thereafter. Conclusions Biodegradable polyurethanes synthesized from triisocyanates exhibited tunable and superior mechanical properties compared to materials synthesized from lysine diisocyanates. Due to their injectability, biocompatibility, tunable degradation, and potential for release of growth factors, these materials are potentially promising therapies for tissue engineering. PMID:18516665
Blended Polyurethane and Tropoelastin as a Novel Class of Biologically Interactive Elastomer
Wise, Steven G.; Liu, Hongjuan; Yeo, Giselle C.; Michael, Praveesuda L.; Chan, Alex H.P.; Ngo, Alan K.Y.; Bilek, Marcela M.M.; Bao, Shisan
2016-01-01
Polyurethanes are versatile elastomers but suffer from biological limitations such as poor control over cell attachment and the associated disadvantages of increased fibrosis. We address this problem by presenting a novel strategy that retains elasticity while modulating biological performance. We describe a new biomaterial that comprises a blend of synthetic and natural elastomers: the biostable polyurethane Elast-Eon and the recombinant human tropoelastin protein. We demonstrate that the hybrid constructs yield a class of coblended elastomers with unique physical properties. Hybrid constructs displayed higher elasticity and linear stress–strain responses over more than threefold strain. The hybrid materials showed increased overall porosity and swelling in comparison to polyurethane alone, facilitating enhanced cellular interactions. In vitro, human dermal fibroblasts showed enhanced proliferation, while in vivo, following subcutaneous implantation in mice, hybrid scaffolds displayed a reduced fibrotic response and tunable degradation rate. To our knowledge, this is the first example of a blend of synthetic and natural elastomers and is a promising approach for generating tailored bioactive scaffolds for tissue repair. PMID:26857114
Cost-Benefit Analysis for Alternatives to Aliphatic Isocyanate Polyurethanes
NASA Technical Reports Server (NTRS)
Lewis, Pattie
2007-01-01
NASA and Air Force Space Command (AFSPC) have similar missions and therefore similar facilities and structures in similar environments. The standard practice for protecting metallic substrates in atmospheric environments is the application of an applied coating system. The most common topcoats used in coating systems are polyurethanes that contain isocyanates. Isocyanates are classified as potential human carcinogens and are known to cause cancer in animals. The primary objective of this effort was to demonstrate and validate alternatives to aliphatic isocyanate polyurethanes resulting in one or more isocyanate-free coatings qualified for use at AFSPC and NASA installations participating in this project. This Cost-Benefit Analysis (CBA) quantifies the estimated capital and process costs of coating alternatives and cost savings relative to the current coatings. The estimates in this CBA are to be used for assessing the relative merits of the selected alternatives. The actual economic effects at any specific facility will depend on the alternative material or technology implemented, the number of actual applications converted, future workloads, and other factors . The participants initially considered eighteen (18) alternative coatings as described in the Potential Alternatives Report entitled Potential Alternatives Report for Validation of Alternatives to Aliphatic Isocyanate Polyurethanes, prepared by ITB. Of those, 8 alternatives were selected for testing in accordance with the Joint Test Protocol entitled Joint Test Protocol for Validation of Alternatives to Aliphatic Isocyanate Polyurethanes, and the Field Test Plan entitled Field Evaluations Test Plan for Validation of Alternatives 10 Aliphatic Isocyanate Polyurethanes, both of which were prepared by ITB. A joint Test Report entitled Joint Test Report for Validation of Alternatives to Aliphatic Isocyanate Polyurethanes, prepared by ITB, documents the results of the laboratory and field testing, as well as any test modifications made during the execution of the testing. The coatings selected for evaluation in this CBA are shown in the table below. Only one control coating system is considered in this analysis. These coatings were either downselected for Phase II or performed well enough to be included in the Qualified Products List in the NASA technical standard NASA-STD-5008, Protective Coating of Carbon Steel, Stainless Steel, and Aluminum on Launch Structures, Facilities, and Ground Support Equipment.
The use of polyurethane materials in the surgery of the spine: a review.
St John, Kenneth R
2014-12-01
The spine contains intervertebral discs and the interspinous and longitudinal ligaments. These structures are elastomeric or viscoelastic in their mechanical properties and serve to allow and control the movement of the bony elements of the spine. The use of metallic or hard polymeric devices to replace the intervertebral discs and the creation of fusion masses to replace discs and/or vertebral bodies changes the load transfer characteristics of the spine and the range of motion of segments of the spine. The purpose of the study was to survey the literature, regulatory information available on the Web, and industry-reported device development found on the Web to ascertain the usage and outcomes of the use of polyurethane polymers in the design and clinical use of devices for spine surgery. A systematic review of the available information from all sources concerning the subject materials' usage in spinal devices was conducted. A search of the peer-reviewed literature combining spinal surgery with polyurethane or specific types and trade names of medical polyurethanes was performed. Additionally, information available on the Food and Drug Administration Web site and for corporate Web sites was reviewed in an attempt to identify pertinent information. The review captured devices that are in testing or have entered clinical practice that use elastomeric polyurethane polymers as disc replacements, dynamic stabilization of spinal movement, or motion limitation to relieve nerve root compression and pain and as complete a listing as possible of such devices that have been designed or tested but appear to no longer be pursued. This review summarizes the available information about the uses to which polyurethanes have been tested or are being used in spinal surgery. The use of polyurethanes in medicine has expanded as modifications to the stability of the polymers in the physiological environment have been improved. The potential for the use of elastomeric materials to more closely match the mechanical properties of the structures being replaced and to maintain motion between spinal segments appears to hold promise. The published results from the use of the devices that are discussed show early success with these applications of elastomeric materials. Copyright © 2014 Elsevier Inc. All rights reserved.
NASA Astrophysics Data System (ADS)
Elvistia Firdaus, Flora
2016-04-01
The polyurethanes (PUs) foam were made from vegetable oil; a soybean based polyol. The foams were categorized into flexible and semi rigid. This research is manufacturally designed polyurethane foams by a process requiring the reaction of mixture of 2, 4- and 2, 6-Toluene di Isocyanate isomers, soy polyol in the presence of other ingredients. The objective of this work was to functionalized soy-polyol using phosporic acid catalyst and chain extender, study their collaborative reaction in producing ultimate property of PU foam. Correlates the foam morphology images in accordance to mechanical properties of foams.
NASA Astrophysics Data System (ADS)
Yakushin, V. A.; Stirna, U. K.; Zhmud', N. P.
1999-07-01
The dependence of physical and mechanical properties of oligoether-based foam polyurethanes on the molecular mass (Mc) of polymer chains between the nodes of the polymer network and on the content of rigid segments in the polymer is investigated at 293 and 98K. The values of Mc at which the foam plastics have the best mechanical properties at low temperatures are determined. The content of rigid segments in the polymer at which foam polyurethanes have the best combination of the linear thermal expansion coefficient and mechanical properties in tension at a temperature of 98K is found.
Thomas, Vinoy; Jayabalan, Muthu
2009-04-01
Development of new generation high flex life polyurethane urea (HFL18-PU) with appropriate elastic modulus, biocompatibility, blood compatibility, resistant to calcification, and biodurability for the long-term use as cardiac device is still a challenge. This study reports the development of a fully aliphatic, ether-free physically cross-linked and low elastic modulus (6.841 +/- 0.27 MPa) polyurethane urea having in vivo biostability, in vivo biocompatibility and high flex-life (721 +/- 30 million cycles) that can satisfy the requirements for the fabrication of tri-leaflet heart valve. Copyright 2008 Wiley Periodicals, Inc.
DOE Office of Scientific and Technical Information (OSTI.GOV)
Hartman, E. Frederick; Zarick, Thomas Andrew; Sheridan, Timothy J.
We performed measurements and analyses of the prompt radiation-induced conductivity (RIC) in thin samples of polyurethane foam and glass microballoon foam at the Little Mountain Medusa LINAC facility in Ogden, UT. The RIC coefficient was non-linear with dose rate for polyurethane foam; however, typical values at 1E11 rad(si)/s dose rate was measured as 0.8E-11 mho/m/rad/s for 5 lb./cu ft. foam and 0.3E-11 mho/m/rad/s for 10 lb./cu ft. density polyurethane foam. For encapsulated glass microballoons (GMB) the RIC coefficient was approximately 1E-15 mho/m/rad/s and was not a strong function of dose rate.
NASA Astrophysics Data System (ADS)
Kashinskii, V. I.; Lipovskikh, V. M.; Rotmistrov, Ya. G.
2007-07-01
Results from 10 years of experience using polyurethane foam-insulated pipelines at OAO Moscow Heating-Network Co. are presented. It is shown that the failure rate of such pipelines is considerably lower than that of pipelines laid in conduits.
Interfacial contributions in lignocellulosic firber-reinforced polyurethane composites
Timothy G. Rials; Michael P. Wolcott; John M. Nassar
2001-01-01
Whereas lignocellulosic fibers have received considerable attention as a reinforcing agent in thermoplastic composites, their applicability to reactive polymer systems remains of considerable interest. The hydroxyl-rich nature of natural lignocellulosic fibers suggests that they are particularly useful in thermsetting systems such as polyurethanes. To further this...
Rigid polyurethane and kenaf core composite foams
USDA-ARS?s Scientific Manuscript database
Rigid polyurethane foams are valuable in many construction applications. Kenaf is a bast fiber plant where the surface stem skin provides bast fibers whose strength-to-weight ratio competes with glass fiber. The higher volume product of the kenaf core is an under-investigated area in composite appli...
Post-processing flame-retardant for polyurethane
NASA Technical Reports Server (NTRS)
Monaghan, P.; Sidman, K. R.
1980-01-01
Treatment of polyurethane form with elastomer formulation after processing makes foam fire resistant without compromising physical properties. In testing, once ignition source is removed, combustion stops. Treatment also prevents molten particle formation, generates no smoke or toxic gases in fire, and does not deteriorate under prolonged exposure to Sun.
Novel polyurethanes from xylan and TDI: Preparation and characterization
USDA-ARS?s Scientific Manuscript database
In this work a novel polyurethane was developed involving xylan and tolylene-2,4-diisocyanate (TDI). Polymer synthesis was achieved via conventional heat or microwave-assisted reaction in dimethylsulfoxide. Because xylan has multiple OH groups on each polymer chain, the TDI/xylan molar ratio neede...
Sorption of Ochratoxin A from aqueous solutions using beta-cyclodextrin-polyurethane polymer
USDA-ARS?s Scientific Manuscript database
The ability of a cyclodextrin-polyurethane polymer to remove ochratoxin A from aqueous solutions, including wine, was examined by batch rebinding assays and equilibrium sorption isotherms. The results were fit to two parameter models. Freundlich analysis of the sorption isotherm indicates the polyme...
Ferrer Solà, Marta; Espaulella Panicot, Joan; Altimires Roset, Jacint; Ylla-Català Borè, Elisenda; Moreno Susi, María
2013-01-01
The aim of the study is to determine the incidence of heel pressure ulcers (UPPT) and to compare the two systems for UPPT prevention: classic padded bandage and polyurethane heel. Prospective intervention study in a medium-long hospital stay of all people admitted that had no UPPT but had a risk of UPPT according to the Braden Scale or clinical judgment. The patients were randomized to prevention with classic padded bandage or polyurethane heel. The outcome variable was the incidence of UPPT for each study group, which was recorded every 15 days or when there were clinical changes. Of the 940 patients evaluated, 409 with a mean age of 80.5 years and 59.1% women,were included in the study. Of these, 78% had Barthel score ≤30; 28.6% dementia; delirium 37.6%; 27.6% diabetes; and 19.6% other UPP. The overall incidence was 2.9% UPPT; 2.49% in the classic padded bandage and 3.37% in the polyurethane heel group (p=0.82). No statistically significant differences were observed between the group with the classical dressing and the group with the polyurethane heel dressing. The use of multiple measures to prevent UPPT achieved a low incidence of these. Copyright © 2011 SEGG. Published by Elsevier Espana. All rights reserved.
Omrani, Ismail; Babanejad, Niloofar; Shendi, Hasan Kashef; Nabid, Mohammad Reza
2017-01-01
Polyurethanes are important class of biomaterials that are extensively used in medical devices. In spite of their easy synthesis, polyurethanes that are fully degradable in response to the intracellular reducing environment are less explored for controlled drug delivery. Herein, a novel glutathione degradable waterborne polyurethane (WPU) nanocarrier for redox triggered intracellular delivery of a model lipophilic anticancer drug, doxorubicin (DOX) is reported. The WPU was prepared from polyaddition reaction of isophorone diisocyanate (IPDI) and a novel linear polyester polyol involving disulfide linkage, disulfide labeled chain extender, dimethylolpropionic acid (DMPA) using dibutyltin dilaurate (DBTDL) as a catalyst. The resulting polyurethane self-assembles into nanocarrier in water. The dynamic light scattering (DLS) measurements and scanning electron microscope (SEM) revealed fast swelling and disruption of nanocarriers under an intracellular reduction-mimicking environment. The in vitro release studies showed that DOX was released in a controlled and redox-dependent manner. MTT assays showed that DOX-loaded WPU had a high in vitro antitumor activity in both HDF noncancer cells and MCF- 7 cancer cells. In addition, it is found that the blank WPU nanocarriers are nontoxic to HDF and MCF-7 cells even at a high concentration of 2mg/mL. Hence, nanocarriers based on disulfide labeled WPU have appeared as a new class of biocompatible and redox-degradable nanovehicle for efficient intracellular drug delivery. Copyright © 2016 Elsevier B.V. All rights reserved.
Mehnati, Parinaz; Arash, Mehran; Akhlaghi, Parisa
2018-01-01
The article aims at constructing protective composite shields for breasts in chest computed tomography and investigating the effects of applying these new bismuth composites on dose and image quality. Polyurethane and silicon with 5% of bismuth were fabricated as a protective shield. At first, their efficiency in attenuating the X-ray beam was investigated by calculating the total attenuation coefficients at diagnostic energy range. Then, a physical chest phantom was scanned without and with these shields at tube voltage of 120 kVp, and image parameters together with dose values were studied. The results showed that these two shields have great effects on attenuating the X-ray beam, especially for lower energies (<40 kV), and in average, the attenuation coefficients of bismuth-polyurethane composite are higher in this energy range. The maximum relative differences between the average Hounsfield units (HUs) and noises of images without and with shield for both composites in 13 regions of interest were 4.5% and 15.7%, respectively. Moreover, primary investigation confirmed the ability of both shields (especially polyurethane-bismuth composite) in dose reduction. Comparing these two composites regarding the amount of dose reduction, the changes in HU and noise, and attenuation coefficients in diagnostic energy range, it seems that polyurethane composite is more useful for dose reduction, especially for higher tube voltages. PMID:29628636
This guidance describes basic ventilation principles and strategies to help protect workers and building occupants and promote the safe use of spray polyurethane foam (SPF) insulation. Guia para la ventilacion sobre la application del aerosol de espuma.
Preparation of eugenol-based polyurethane
NASA Astrophysics Data System (ADS)
Li, Yupeng; Luo, Fang; Cheng, Chuanjie
2018-03-01
The regenerative eugenol was used as the starting material to prepare diol species by two steps, with a total yield of 28%. Furthermore, the prepared diol reacts with 1,6-hexadiisocyanate(HDI) to afford the corresponding polyurethane (PU). The structure of intermediates and PU are characterized by 1H-NMR or IR.
Interfacial contributions in lignocellulosic fiber-reinforced polyurethane composites
Timothy G. Rials; Michael P. Wolcott; John M. Nassar
2001-01-01
Whereas lignocellulosic fibers have received considerable attention as a rein- forcing agent in thermoplastic composites, their applicability to reactive polymer systems remains of considerable interest. The hydroxyl-rich nature of natural lignocellulosic fibers suggests that they are particularly useful in thermosetting systems such as polyurethanes. To further this...
Federal Register 2010, 2011, 2012, 2013, 2014
2013-11-13
... Polyurethane Foam Production and Fabrication, Lead Acid Battery Manufacturing, and Wood Preserving (Renewal... Polyurethane Foam Production and Fabrication, Lead Acid Battery Manufacturing, and Wood Preserving (40 CFR Part... battery manufacturing facilities, and 393 existing wood preserving facilities. The total annual responses...
A Review of Battle Damage Prediction and Vulnerability Reduction Methods
2010-10-01
monolithic constructions. Bahei-El-Din and Dvorak [38] showed that the use of a polyurethane or polyurea interlayer used in a sandwich plate in...sandwich plates reinforced with polyurethane/ polyurea interlayers under blast loads. Journal of Sandwich Structures and Materials 9 (3) 261–281. 39
40 CFR 63.1307 - Recordkeeping requirements.
Code of Federal Regulations, 2011 CFR
2011-07-01
... Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1307 Recordkeeping... paragraphs (c)(1)(i), (ii), (iii), and (iv) of this section. Each flexible polyurethane foam slabstock source...) through (C) of this section. (A) A log of foam runs each day. For each run, the log shall include a list...
40 CFR 63.1307 - Recordkeeping requirements.
Code of Federal Regulations, 2012 CFR
2012-07-01
... Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1307 Recordkeeping... paragraphs (c)(1)(i), (ii), (iii), and (iv) of this section. Each flexible polyurethane foam slabstock source...) through (C) of this section. (A) A log of foam runs each day. For each run, the log shall include a list...
40 CFR 63.1307 - Recordkeeping requirements.
Code of Federal Regulations, 2010 CFR
2010-07-01
... Standards for Hazardous Air Pollutants for Flexible Polyurethane Foam Production § 63.1307 Recordkeeping... paragraphs (c)(1)(i), (ii), (iii), and (iv) of this section. Each flexible polyurethane foam slabstock source...) through (C) of this section. (A) A log of foam runs each day. For each run, the log shall include a list...
Washing Off Polyurethane Foam Insulation
NASA Technical Reports Server (NTRS)
Burley, Richard K.; Fogel, Irving
1990-01-01
Jet of hot water removes material quickly and safely. Simple, environmentally sound technique found to remove polyurethane foam insulation from metal parts. Developed for (but not limited to) use during rebuilding of fuel system of Space Shuttle main engine, during which insulation must be removed for penetrant inspection of metal parts.
Xiang, Changsheng; Cox, Paris J; Kukovecz, Akos; Genorio, Bostjan; Hashim, Daniel P; Yan, Zheng; Peng, Zhiwei; Hwang, Chih-Chau; Ruan, Gedeng; Samuel, Errol L G; Sudeep, Parambath M; Konya, Zoltan; Vajtai, Robert; Ajayan, Pulickel M; Tour, James M
2013-11-26
A thermoplastic polyurethane (TPU) composite film containing hexadecyl-functionalized low-defect graphene nanoribbons (HD-GNRs) was produced by solution casting. The HD-GNRs were well distributed within the polyurethane matrix, leading to phase separation of the TPU. Nitrogen gas effective diffusivity of TPU was decreased by 3 orders of magnitude with only 0.5 wt % HD-GNRs. The incorporation of HD-GNRs also improved the mechanical properties of the composite films, as predicted by the phase separation and indicated by tensile tests and dynamic mechanical analyses. The improved properties of the composite film could lead to potential applications in food packaging and lightweight mobile gas storage containers.
Properties of rigid polyurethane foams filled with glass microspheres
NASA Astrophysics Data System (ADS)
Yakushin, V.; Bel'kova, L.; Sevastyanova, I.
2012-11-01
The effect of hollow glass microspheres with a density of 125 kg/m3 on the properties of low-density (54-90 kg/m3) rigid polyurethane foams is investigated. The thermal expansion coefficient of the foams and their properties in tension and compression in relation to the content of the microspheres (0.5-5 wt.%) are determined. An increase in the characteristics of the material in compression in the foam rise direction with increasing content of filler is revealed. The limiting content of the microspheres above which the mechanical characteristics of the filled foams begin to decrease is found. The distribution of the microspheres in elements of the cellular structure of the polyurethane foams is examined.
Parameters estimation of sandwich beam model with rigid polyurethane foam core
NASA Astrophysics Data System (ADS)
Barbieri, Nilson; Barbieri, Renato; Winikes, Luiz Carlos
2010-02-01
In this work, the physical parameters of sandwich beams made with the association of hot-rolled steel, Polyurethane rigid foam and High Impact Polystyrene, used for the assembly of household refrigerators and food freezers are estimated using measured and numeric frequency response functions (FRFs). The mathematical models are obtained using the finite element method (FEM) and the Timoshenko beam theory. The physical parameters are estimated using the amplitude correlation coefficient and genetic algorithm (GA). The experimental data are obtained using the impact hammer and four accelerometers displaced along the sample (cantilevered beam). The parameters estimated are Young's modulus and the loss factor of the Polyurethane rigid foam and the High Impact Polystyrene.
NASA Technical Reports Server (NTRS)
Glasgow, D. G.
1976-01-01
The effects of novel aromatic diamine structures on the adhesive properties of epoxy and polyurethane adhesives were studied. Aromatic diamines based on benzophenone and diphenyl-methane isomers were evaluated as curing agents for epoxy resins and benzophenone and diphenyl-methane based diamine isomers were evaluated as curing agents for polyurethane adhesives. Polyurethane adhesives were prepared based on m, m prime-diisocyanato-diphenyl-methane and m, m prime-diisocyanato-benzophenone. The m, m prime-diisocayanato-diphenyl-methane based adhesive had properties comparable to state-of-the-art adhesives. The m, m prime-diisocyanato-benzophenone based adhesive was extremely reactive.
NASA Astrophysics Data System (ADS)
Schmit, Amanda L.
This thesis is broken down into two main projects. First, studies of the Kaneda reaction in the synthesis of oocydin A/haterumalide NA and, second, polyurethanes from renewable resources: polyols from soybean oil. In Chapter I, the stereoselectivity of the Kaneda reaction was studied. The driving interest stemmed from the hypothesis that one epimer of an acyclic precursor could give the desired bicyclic core of oocydin A/haterumalide NA. In Chapter II, the work toward new polyols from soybean oil is discussed. Renewable content in polyurethanes on the market is still low because of economics and performance. Our ideas for new polyol systems are presented.
Synthesis and characterization of polyurethane/CdS-SiO 2 nanocomposites via ultrasonic process
NASA Astrophysics Data System (ADS)
Chen, Jing; Zhou, Yu-Ming; Nan, Qiu-Li; Ye, Xiao-Yun; Sun, Yan-Qing; Wang, Zhi-Qiang; Zhang, Shi-Ming
2008-12-01
In this study, the high-intensity ultrasound was applied in the preparation of chiral polyurethane/CdS-SiO 2 nanocomposites. The polyurethane/CdS-SiO 2 nanocomposites were analyzed by powder X-ray diffraction, thermogravimetric analysis (TGA), TEM and SEM. The results indicated that the heat stability of the nanocomposites was improved in the presence of CdS-SiO 2 core-shell nanoparticles. The infrared emissivity (8-14 μm) study revealed that the nanocomposites possessed much lower infrared values compared with those of the neat polymers and nanoparticles, respectively. A possible mechanism of ultrasonic induced composite reaction was proposed based on the experimental results.
Tests of two new polyurethane foam wheelchair tires.
Gordon, J; Kauzlarich, J J; Thacker, J G
1989-01-01
The performance characteristics of four 24-inch wheelchair tires are considered; one pneumatic and three airless. Specifically, two new airless polyurethane foam tires (circular and tapered cross-section) were compared to both a molded polyisoprene tire and a rubber pneumatic tire. Rolling resistance, coefficient of static friction, spring rate, tire roll-off, impact absorption, wear resistance, and resistance to compression set were the characteristics considered for the basis of comparison. Although the pneumatic tire is preferred by many wheelchair users, the two new polyurethane foam tires were found to offer a performance similar to the high-pressure pneumatic tire. In addition, the foam tires are less expensive and lighter in weight than the other tires tested.
77 FR 56639 - Certain New Chemicals; Receipt and Status Information
Federal Register 2010, 2011, 2012, 2013, 2014
2012-09-13
... notice end Manufacturer/ Use Chemical date date importer P-12-0488 08/01/2012 10/29/2012 CBI (G) Additive... 10/29/2012 CBI (G) Additive to (G) Hydroxy polyurethane containing oil, foam. polymer with alkylene.../2012 CBI (G) Additive to (G) Alkanol, polyurethane oxybis-, foam. polymer with aromatic isocyanate...
1980-05-01
34 4,. * ., Table B-I. CPR-739 Rigid Polyurethane Foam Component Characteristics [ Cream Time, 120 sec; Rise Time, 13 sec; Cure Time, 24 hr at 750F...INC. E Colic Soil Tech Dept. Pennsauken. NJ SANDIA LABORATORIES Library Div., Livermore CA SCHUPACK ASSOC SO. NORWALK. CT (SCHUPACK) SHELL OIL CO
The 1990 Clean Air Act Amendments require EPA to develop standards for major emission sources of 189 hazardous air pollutants (HAPs). EPA has identified the flexible polyurethane foam industry as a large emitter of HAPs and has slated the industry for regulation under Title III, ...
Strength and durability of one-part polyurethane adhesive bonds to wood
C. B. Vick; E. A. Okkonen
1998-01-01
One-part polyurethane wood adhesives comprise a new class of general purpose consumer products. Manufacturersa claims of waterproof bonds brought many inquiries to the Forest Products Laboratory (FPL) from users constructing aircraft, boats, lawn furniture, and other laminated materials for outdoor use. Although FPL has technical information on several types of...
Sorption of Triangular Silver Nanoplates on Polyurethane Foam
NASA Astrophysics Data System (ADS)
Furletov, A. A.; Apyari, V. V.; Garshev, A. V.; Volkov, P. A.; Tolmacheva, V. V.; Dmitrienko, S. G.
2018-02-01
The sorption of triangular silver nanoplates on polyurethane foam is investigated as a procedure for creating a nanocomposite sensing material for subsequent use in optical means of chemical analysis. Triangular silver nanoplates are synthesized and characterized, and a simple sorption technique for the formation of a composite material based on these nanoplates is proposed.
An epoxy primer with a high gloss polyurethane topcoat coating system was exposed either only in a QUV chamber or exposed in a QUV chamber and a Prohesion chamber, alternatively, in this study. AFM studies found that micro blisters formed on the coating surface after both expo...
Vegetable Oil-Based Hyperbranched Thermosetting Polyurethane/Clay Nanocomposites
2009-01-01
The highly branched polyurethanes and vegetable oil-based polymer nanocomposites have been showing fruitful advantages across a spectrum of potential field of applications.Mesua ferreaL. seed oil-based hyperbranched polyurethane (HBPU)/clay nanocomposites were prepared at different dose levels by in situ polymerization technique. The performances of epoxy-cured thermosetting nanocomposites are reported for the first time. The partially exfoliated structure of clay layers was confirmed by XRD and TEM. FTIR spectra indicate the presence of H bonding between nanoclay and the polymer matrix. The present investigation outlines the significant improvement of tensile strength, scratch hardness, thermostability, water vapor permeability, and adhesive strength without much influencing impact resistance, bending, and elongation at break of the nanocomposites compared to pristine HBPU thermoset. An increment of two times the tensile strength, 6 °C of melting point, and 111 °C of thermo-stability were achieved by the formation of nanocomposites. An excellent shape recovery of about 96–99% was observed for the nanocomposites. Thus, the formation of partially exfoliated clay/vegetable oil-based hyperbranched polyurethane nanocomposites significantly improved the performance. PMID:20596546
Waterborne Polyurethane Coatings with Covalently Linked Black Dye Sudan Black B
Sun, Wei; Xu, Haiyan; Xu, Fei
2017-01-01
Colored waterborne polyurethanes have been widely used in paintings, leathers, textiles, and coatings. Here, a series of black waterborne polyurethanes (WPUs) with different ratios of black dye, Sudan Black B (SDB), were prepared by step-growth polymerization. WPU emulsions as obtained exhibit low particle sizes and remarkable storage stability at the same time. At different dye loadings, essential structural, statistical and thermal properties are characterized. FTIR (fourier transform infrared) spectra indicate that SDB is covalently linked into waterborne polyurethane chains. All of the WPUs with covalently linked SDB show better color fastness and resistance of thermal migration than those with SDB mixed physically. Besides, WPUs incorporated SDB covalently with different polymeric diols, polytetramethylene ether glycol (PTMG), polypropylene glycol (PPG), poly-1, 4-butylene adipate glycol (PBA) and polycaprolactone glycol (PCL), were prepared to obtain different properties to cater to a variety of practical demands. By a spraying method, the black WPUs can be directly used as metal coatings without complex dyeing process by simply mixing coating additive and other waterborne resins, which exhibit excellent coating performance. PMID:29143785
Vegetable Oil-Based Hyperbranched Thermosetting Polyurethane/Clay Nanocomposites.
Deka, Harekrishna; Karak, Niranjan
2009-04-25
The highly branched polyurethanes and vegetable oil-based polymer nanocomposites have been showing fruitful advantages across a spectrum of potential field of applications. Mesua ferrea L. seed oil-based hyperbranched polyurethane (HBPU)/clay nanocomposites were prepared at different dose levels by in situ polymerization technique. The performances of epoxy-cured thermosetting nanocomposites are reported for the first time. The partially exfoliated structure of clay layers was confirmed by XRD and TEM. FTIR spectra indicate the presence of H bonding between nanoclay and the polymer matrix. The present investigation outlines the significant improvement of tensile strength, scratch hardness, thermostability, water vapor permeability, and adhesive strength without much influencing impact resistance, bending, and elongation at break of the nanocomposites compared to pristine HBPU thermoset. An increment of two times the tensile strength, 6 degrees C of melting point, and 111 degrees C of thermo-stability were achieved by the formation of nanocomposites. An excellent shape recovery of about 96-99% was observed for the nanocomposites. Thus, the formation of partially exfoliated clay/vegetable oil-based hyperbranched polyurethane nanocomposites significantly improved the performance.
DOE Office of Scientific and Technical Information (OSTI.GOV)
Neilsen, Michael K.; Lu, Wei-Yang; Werner, Brian T.
Experiments were performed to characterize the mechanical response of a 15 pcf flexible polyurethane foam to large deformation at different strain rates and temperatures. Results from these experiments indicated that at room temperature, flexible polyurethane foams exhibit significant nonlinear elastic deformation and nearly return to their original undeformed shape when unloaded. However, when these foams are cooled to temperatures below their glass transition temperature of approximately -35 o C, they behave like rigid polyurethane foams and exhibit significant permanent deformation when compressed. Thus, a new model which captures this dramatic change in behavior with temperature was developed and implemented intomore » SIERRA with the name Flex_Foam to describe the mechanical response of both flexible and rigid foams to large deformation at a variety of temperatures and strain rates. This report includes a description of recent experiments. Next, development of the Flex Foam model for flexible polyurethane and other flexible foams is described. Selection of material parameters are discussed and finite element simulations with the new Flex Foam model are compared with experimental results to show behavior that can be captured with this new model.« less
NASA Astrophysics Data System (ADS)
Ching, Yern Chee; Yaacob, Iskandar Idris
2011-06-01
Polyethylene (PE) film was coated with polyurethane/nanosilica composite layer using rod Mayer process. The polyurethane/nanosilica system was prepared by dispersing nanosilica powder into solvent borne polyurethane (PU) binder under vigorous stirring. The silica nanoparticle used has an average diameter of 16 nm, and their weight fraction were varied from 0 % to 14 %. Two different thicknesses of the PU/nanosilica coating layer were fabricated which were about 4 μm and 8 μm. The structure and thermal mechanical features of the nanocomposite coated PE film were characterized by scanning electron microscope (SEM), dynamic mechanical analyzer (DMA), thermogravimetric analyzer (TGA) as well as tensile tests. The results showed that thin layer coating of the PU/nanosilica composite reduced tensile strength of PE substrate slightly. However, the nanocomposite coating of up to 8 μm reduced the elongation % of PE substrate significantly. PU/nanosilica composite coating layer increased the tensile modulus and stiffness of PE substrate. There was no influence of the PU/nanosilica composite coating to the thermal degradation rate of PE film.
Cruz, Karina Ferreira Noronha; Formaggio, Daniela Maria Ducatti; Tada, Dayane Batista; Cristovan, Fernando Henrique; Guerrini, Lilia Müller
2017-02-01
Electroactive nanofibers based on thermoplastic polyurethane (TPU) and poly(alkoxy anilines) produced by electrospinning has been explored for biomaterials applications. The thermoplastic polyurethane is a biocompatible polymer with good mechanical properties. The production of TPU nanofibers requires the application of high voltage during electrospinning in order to prepare uniform mats due to its weak ability to elongate during the process. To overcome this limitation, a conductive polymer can be incorporated to the process, allowing generates mats without defects. In this study, poly(o-ethoxyaniline) POEA doped with dodecylbenzene sulfonic acid (DBSA) was blended with thermoplastic polyurethane (TPU) by solution method. Films were produced by casting and nanofibers were prepared by electrospinning. The effect of the POEA on morphology, distribution of diameter and cell viability of the nanofibers was evaluated. The results demonstrated that the incorporation of POEA in TPU provided to the mats a suitable morphology for cellular growth. © 2016 Wiley Periodicals, Inc. J Biomed Mater Res Part A: 105A: 601-607, 2017. © 2016 Wiley Periodicals, Inc.
A multilayered polyurethane foam technique for skin graft immobilization.
Nakamura, Motoki; Ito, Erika; Kato, Hiroshi; Watanabe, Shoichi; Morita, Akimichi
2012-02-01
Several techniques are applicable for skin graft immobilization. Although the sponge dressing is a popular technique, pressure failure near the center of the graft is a weakness of the technique that can result in engraftment failure. To evaluate the efficacy of a new skin graft immobilization technique using multilayered polyurethane foam in vivo and in vitro. Twenty-six patients underwent a full-thickness skin graft. Multiple layers of a hydrocellular polyurethane foam dressing were used for skin graft immobilization. In addition, we created an in vitro skin graft model that allowed us to estimate immobilization pressure at the center and edges of skin grafts of various sizes. Overall mean graft survival was 88.9%. In the head and neck region (19 patients), mean graft survival was 93.6%. Based on the in vitro outcomes, this technique supplies effective pressure (<30 mmHg) to the center region of the skin graft. This multilayered polyurethane foam dressing is simple, safe, and effective for skin graft immobilization. © 2011 by the American Society for Dermatologic Surgery, Inc. Published by Wiley Periodicals, Inc.
PLATELET ADHESION TO POLYURETHANE UREA UNDER PULSATILE FLOW CONDITIONS
Navitsky, Michael A.; Taylor, Joshua O.; Smith, Alexander B.; Slattery, Margaret J.; Deutsch, Steven; Siedlecki, Christopher A.; Manning, Keefe B.
2014-01-01
Platelet adhesion to a polyurethane urea surface is a precursor to thrombus formation within blood-contacting cardiovascular devices, and platelets have been found to adhere strongly to polyurethane surfaces below a shear rate of approximately 500 s−1. The aim of the current work is to determine platelet adhesion properties to the polyurethane urea surface as a function of time varying shear exposure. A rotating disk system is used to study the influence of steady and pulsatile flow conditions (e.g. cardiac inflow and sawtooth waveforms) for platelet adhesion to the biomaterial surface. All experiments retain the same root mean square angular rotation velocity (29.63 rad/s) and waveform period. The disk is rotated in platelet rich bovine plasma for two hours with adhesion quantified by confocal microscopy measurements of immunofluorescently labeled bovine platelets. Platelet adhesion under pulsating flow is found to exponentially decay with increasing shear rate. Adhesion levels are found to depend upon peak platelet flux and shear rate regardless of rotational waveform. In combination with flow measurements, these results may be useful for predicting regions susceptible to thrombus formation within ventricular assist devices. PMID:24721222
Okunribido, Olanrewaju O
2013-01-01
This article is a report of a study of the effect of the seat cushion on risk of falling from a wheelchair. Two laboratory studies and simulated assistant propelled wheelchair transfers were conducted with four healthy female participants. For the laboratory studies there were three independent variables: trunk posture (upright/flexed forward), seat cushion (flat polyurethane/propad low profile), and feet condition (dangling/supported), and two dependent variables: occupied wheelchair (wheelchair) center of gravity (CG), and stability. For the simulated transfers there was one independent variable: seat cushion (flat polyurethane/propad low profile), and one dependent variable: perception of safety (risk of falling). Results showed that the wheelchair CG was closer to the front wheels, and stability lower for the propad low profile cushion compared to the polyurethane cushion, when the participants sat with their feet dangling. During the simulated transfers, sitting on the propad low profile cushion caused participants to feel more apprehensive (anxious or uneasy) compared to sitting on the polyurethane cushion. The findings can contribute to the assessment of risk and care planning of non-ambulatory wheelchair users.
Agarwal, Manika; Wible, Emily; Ramir, Tyler; Altun, Sibel; Viana, Grace; Evans, Carla; Lukic, Henry; Megremis, Spiro; Atsawasuwan, Phimon
2018-05-01
To evaluate the long-term effects of seven different cleaning methods on light transmittance, surface roughness, and flexural modulus of a polyurethane retainer material. Polyurethane retainer specimens (Vivera®, Align Technology Inc) (70 specimens, n = 10 per method, 50.8 mm × 12.7 mm × 1.0 mm) were exposed to seven cleaning methods twice a week for 6 months. Before treatment and after 6 months, light transmittance, surface roughness, and flexural modulus of the specimens were quantified. Qualitative assessment of randomly selected specimens from each solution was performed at baseline and after 6 months using a scanning electron microscope. Statistical analyses were performed at the .05 significance level. Of the three test variables, light transmittance through the specimens was the only one that changed significantly from baseline to 6 months for all cleaning solutions, with all of them causing a decrease. However, except for 0.6% sodium hypochlorite showing a change in surface roughness values and 2.5% vinegar and toothbrushing showing an increase in flexural modulus, none of the other four cleaning methods resulted in significant changes in surface roughness or flexural modulus values for the polyurethane specimens between baseline and after 6 months. Of the seven cleaning methods, Invisalign® cleaning crystals, Polident®, and Listerine® showed the least amount of change in light transmittance values for the polyurethane specimens over 6 months, and they had no effect on surface roughness and flexural modulus values.
Grzesiak, Jakub; Marycz, Krzysztof; Szarek, Dariusz; Bednarz, Paulina; Laska, Jadwiga
2015-01-01
Research concerning the elaboration and application of biomaterial which may support the nerve tissue regeneration is currently one of the most promising directions. Biocompatible polymer devices are noteworthy group among the numerous types of potentially attractive biomaterials for regenerative medicine application. Polylactides and polyurethanes may be utilized for developing devices for supporting the nerve regeneration, like nerve guide conduits or bridges connecting the endings of broken nerve tracts. Moreover, the combination of these biomaterial devices with regenerative cell populations, like stem or precursor cells should significantly improve the final therapeutic effect. Therefore, the composition and structure of final device should support the proper adhesion and growth of cells destined for clinical application. In current research, the three polymer mats elaborated for connecting the broken nerve tracts, made from polylactide, polyurethane and their blend were evaluated both for physical properties and in vitro, using the olfactory-bulb glial cells and mesenchymal stem cells. The evaluation of Young's modulus, wettability and roughness of obtained materials showed the differences between analyzed samples. The analysis of cell adhesion, proliferation and morphology showed that the polyurethane-polylactide blend was the most neutral for cells in culture, while in the pure polymer samples there were significant alterations observed. Our results indicated that polyurethane-polylactide blend is an optimal composition for culturing and delivery of glial and mesenchymal stem cells. Copyright © 2015. Published by Elsevier B.V.
Encapsulation of β-Sitosterol in Polyurethane by Sol-Gel Electrospinning.
Amina, Musarat; Amna, Touseef; Al-Musayeib, Nawal; Zabin, Sami A; Hassan, M Shamshi; Khil, Myung-Seob
2017-06-01
Pristine β-sitosterol or in combination with other phytosterols is utilized in an array of enriched commercial foods. Considering the presence of β-sitosterol in different functional foods and its potential role in prevention and cure of neurodegenerative diseases, the aims of our investigation were to encapsulate β-sitosterol in nanofibers and to estimate influence of β-sitosterol on proliferation of fibroblasts. Electrospun nanofibers have widely been used as scaffolds to mimic natural extracellular matrix. Herein, our group for the first time establishes an innovative scaffold based on β-sitosterol and polyurethane using electrospinning. β-Sitosterol promotes epithelialization and possesses anti-oxidant and anti-inflammatory activities, whereas polyurethane, besides possessing biomedical uses, also enhances epithelial growth. We optimized the concentration (5%) of β-sitosterol in polyurethane to obtain homogenous solution, which can be spun without difficulty for the synthesis of β-sitosterol amalgamated scaffold. The resulted twisted nanofibers have been characterized via scanning electron microscopy and Fourier transform infrared spectroscopy. The viability of cells on twisted scaffold was examined using NIH 3T3 fibroblasts as model cell line. Incorporation of β-sitosterol in polyurethane changed the structure and size of nanofibers, and the twisted scaffolds were non-cytotoxic. Thus, the twisted nanoribbons, which contain anti-inflammatory β-sitosterol, can be utilized as a promising future material, which will help to ease inflammation and also aid in wound healing. In conclusion, the outcome of the preliminary research evidently points out the potential of twisted scaffold in biomedical applications.
2013-01-01
Background The primary objective of this study was to determine the efficiency of a pneumatic device in controlling cuff pressure (Pcuff) in patients intubated with polyurethane-cuffed tracheal tubes. Secondary objectives were to determine the impact of continuous control of Pcuff, and cuff shape on microaspiration of gastric contents. Methods Prospective randomized controlled study. All patients requiring intubation and mechanical ventilation ≥48 h were eligible. The first 32 patients were intubated with tapered polyurethane-cuffed, and the 32 following patients were intubated with cylindrical polyurethane-cuffed tracheal tubes. Patients randomly received 24 h of continuous control of Pcuff using a pneumatic device (Nosten®), and 24 h of routine care of Pcuff using a manometer. Target Pcuff was 25 cmH2O. Pcuff was continuously recorded, and pepsin was quantitatively measured in all tracheal aspirates during these periods. Results The pneumatic device was efficient in controlling Pcuff (med [IQ] 26 [24, 28] vs 22 [20, 28] cmH2O, during continuous control of Pcuff and routine care, respectively; p = 0.017). In addition, percentage of patients with underinflation (31% vs 68%) or overinflation (53% vs 100%) of tracheal cuff, and percentage of time spent with underinflation (0.9 [0, 17] vs 14% [4, 30]) or overinflation (0 [0, 2] vs 32% [9, 54]) were significantly (p < 0.001) reduced during continuous control of Pcuff compared with routine care. No significant difference was found in microaspiration of gastric content between continuous control of Pcuff compared with routine care, or between patients intubated with tapered compared with cylindrical polyurethane-cuffed tracheal tubes. Conclusion The pneumatic device was efficient in controlling Pcuff in critically ill patients intubated with polyurethane-cuffed tracheal tubes. Trial registration The Australian New Zealand Clinical Trials Registry (NCT01351259) PMID:24369057
Guan, Yayuan; Su, Yuling; Zhao, Lili; Meng, Fancui; Wang, Quanxin; Yao, Yongchao; Luo, Jianbin
2017-06-01
Polyurethane micelles with disulfide linkage located at the interface of hydrophilic shell and hydrophobic core (PU-SS-I) have been shown enhanced drug release profiles. However, the payloads could not be released completely. The occurrence of aggregation of hydrophobic cores upon shedding hydrophilic PEG coronas was considered as the reason for the incomplete release. To verify the above hypothesis and to develop a new polyurethane based micelles with dual stimuli respond properties and controllable location of pH and reduction responsive groups in the PU main chains, a tertiary amine was incorporated into the hydrophobic core PU-SS-I, which resulted polyurethane with both reduction and pH sensitive properties (PU-SS-N). Biodegradable polyurethane with only disulfide linkages located between the hydrophilic PEG segment and the hydrophobic PCL segments (PU-SS-I) and polyurethane with only pH sensitive tertiary amine at the hydrophobic core (PU-N-C) were used as comparisons. Paclitaxel (PTX) was chosen as mode hydrophobic drug to evaluate the loading and redox triggered release profiles of the PU micelles. It was demonstrated that PU-SS-N micelles disassembled instantly at the presence of 10mM GSH and at an acidic environment (pH=5.5), which resulted the nearly complete release (~90%) of the payloads within 48h, while about ~70% PTX was released from PU-SS-I and PU-SS-N micelles at neutral environment (pH=7.4) with the presence of 10mM GSH. The rapid and complete redox and pH stimuli release properties of the PU-SS-N nanocarrier will be a promising anticancer drug delivery system to ensure sufficient drug concentration to kill the cancer cells and to prevent the emergency of MDR. The in vitro cytotoxicity and cell uptake of the PTX-loaded micelles was also assessed in H460 and HepG2 cells. Copyright © 2017 Elsevier B.V. All rights reserved.
Forni, Cristiana; Loro, Loretta; Tremosini, Morena; Mini, Sandra; Pignotti, Elettra; Bigoni, Ombretta; Guzzo, Giuseppe; Bellini, Laura; Trofa, Carmela; Di Cataldo, Anna M; Guzzi, Marilena
2011-03-01
The aim of this study was to test the effectiveness of polyurethane foam in contact with the heel inside a plaster cast to decrease the rate of pressure sores in the population at most risk. The rate of pressure sores caused by the plaster cast is reported to be 14-15% in the paediatric population, 33.3% in patients having undergone chemotherapy for bone tumours and 43% in orthopaedic patients who already have sore skin when the cast is applied (grade 1 lesion) to the heel. Controlled clinical trial. From November 2007-January 2009, all consecutive subjects requiring lower limb casts having undergone chemotherapy and/or presenting heel soreness received polyurethane foam in contact with the skin of the heel before applying the cast. The results were compared with those of patients with the same risk factors but were not administered the foam and were enrolled from May 2005-August 2006. In total, 156 patients were enrolled, 85 in the control group and 71 in the experimental group. In the experimental group, 2 of the 56 patients (3.6%) with sore skin developed a pressure sore compared with 21 of 49 (42.9%) in the control group without polyurethane foam (p < 0.0005). In the experimental group, one of the 24 patients (4.2%) patients undergoing chemotherapy developed a pressure sore compared with 18 of 54 (33.3%) in the control group (p = 0.005). Placing polyurethane foam in contact with the skin of the heel inside a plaster cast prevents the formation of pressure sores. This study provides evidence that using polyurethane foam to prevent sores even inside plaster casts in populations at most risk is a simple and cost-effective strategy and decreases the discomfort, pain and risks in these patients. © 2011 Blackwell Publishing Ltd.
Managing burn wounds with SMARTPORE Technology polyurethane foam: two case reports.
Imran, Farrah-Hani; Karim, Rahamah; Maat, Noor Hidayah
2016-05-12
Successful wound healing depends on various factors, including exudate control, prevention of microbial contaminants, and moisture balance. We report two cases of managing burn wounds with SMARTPORE Technology polyurethane foam dressing. In Case 1, a 2-year-old Asian girl presented with a delayed (11 days) wound on her right leg. She sustained a thermal injury from a hot iron that was left idle on the floor. Clinical inspection revealed an infected wound with overlying eschar that traversed her knee joint. As her parents refused surgical debridement under general anesthesia, hydrotherapy and wound dressing using SMARTPORE Technology Polyurethane foam were used. Despite the delay in presentation of this linear thermal pediatric burn injury that crossed the knee joint, the patient's response to treatment and its outcome were highly encouraging. She was cooperative and tolerated each dressing change without the need of supplemental analgesia. Her wound was healed by 24 days post-admission. In Case 2, a 25-year-old Asian man presented with a mixed thickness thermal flame burn on his left leg. On examination, the injury was a mix of deep and superficial partial thickness burn, comprising approximately 3% of his total body surface area. SMARTPORE Technology polyurethane foam was used on his wound; his response to the treatment was very encouraging as the dressing facilitated physiotherapy and mobility. The patient rated the pain during dressing change as 2 on a scale of 10 and his pain score remained the same in every subsequent change. His wound showed evidence of epithelialization by day 7 post-burn. There were no adverse events reported. Managing burn wounds with SMARTPORE Technology polyurethane foam resulted in reduced pain during dressing changes and the successful healing of partial and mixed thickness wounds. The use of SMARTPORE Technology polyurethane foam dressings showed encouraging results and requires further research as a desirable management option in burn wounds.
Nerve regeneration using tubular scaffolds from biodegradable polyurethane.
Hausner, T; Schmidhammer, R; Zandieh, S; Hopf, R; Schultz, A; Gogolewski, S; Hertz, H; Redl, H
2007-01-01
In severe nerve lesion, nerve defects and in brachial plexus reconstruction, autologous nerve grafting is the golden standard. Although, nerve grafting technique is the best available approach a major disadvantages exists: there is a limited source of autologous nerve grafts. This study presents data on the use of tubular scaffolds with uniaxial pore orientation from experimental biodegradable polyurethanes coated with fibrin sealant to regenerate a 8 mm resected segment of rat sciatic nerve. Tubular scaffolds: prepared by extrusion of the polymer solution in DMF into water coagulation bath. The polymer used for the preparation of tubular scaffolds was a biodegradable polyurethane based on hexamethylene diisocyanate, poly(epsilon-caprolactone) and dianhydro-D-sorbitol. EXPERIMENTAL MODEL: Eighteen Sprague Dawley rats underwent mid-thigh sciatic nerve transection and were randomly assigned to two experimental groups with immediate repair: (1) tubular scaffold, (2) 180 degrees rotated sciatic nerve segment (control). Serial functional measurements (toe spread test, placing tests) were performed weekly from 3rd to 12th week after nerve repair. On week 12, electrophysiological assessment was performed. Sciatic nerve and scaffold/nerve grafts were harvested for histomorphometric analysis. Collagenic connective tissue, Schwann cells and axons were evaluated in the proximal nerve stump, the scaffold/nerve graft and the distal nerve stump. The implants have uniaxially-oriented pore structure with a pore size in the range of 2 micorm (the pore wall) and 75 x 700 microm (elongated pores in the implant lumen). The skin of the tubular implants was nonporous. Animals which underwent repair with tubular scaffolds of biodegradable polyurethanes coated with diluted fibrin sealant had no significant functional differences compared with the nerve graft group. Control group resulted in a trend-wise better electrophysiological recovery but did not show statistically significant differences. There was a higher level of collagenic connective tissue within the scaffold and within the distal nerve stump. Schwann cells migrated into the polyurethane scaffold. There was no statistical difference to the nerve graft group although Schwann cell counts were lower especially within the middle of the polyurethane scaffold. Axon counts showed a trend-wise decrease within the scaffold. These results suggest that biodegradable polyurethane tubular scaffolds coated with diluted fibrin sealant support peripheral nerve regeneration in a standard gap model in the rat up to 3 months. Three months after surgery no sign of degradation could be seen.
Development of a smart, anti-water polyurethane polymer hair coating for style setting.
Liu, Y; Liu, Y J; Hu, J; Ji, F L; Lv, J; Chen, S J; Zhu, Y
2016-06-01
The goal of this work was to develop a novel polyurethane polymer coating for the surface of the hair that could be used for style setting via the shape memory effect (SME). The features of the films are in accordance with conventional hair styling methods used in the laboratory. In this study, a new polyurethane polymer was synthesized; the morphology and mechanical behaviour of the coated hair were systematically investigated using a scanning electron microscope (SEM) and an Instron 5566 (with a temperature oven). The SME of the hair was tested using a 35-g weight and over five washing and drying cycles. The experimental result shows that the polyurethane polymer has effects on the mechanical behaviour of the hair. It indicates that the fixed shape (at 22°C) and recover rate (at 60°C) of different casted thickness films are similar. And the stress of the film becomes larger with increasing film thickness. Furthermore, the shape memory ability could be endowed with the hair styling using this polymer; the hair fibre could recover to the 65% of its original shape after five cycle deformation by 35 g mass under the heat-treated condition; it could recover its original setting styling even after 5th water washing and drying. The SEM results indicated that the microsurface of the hair is coated with the polymer membrane; it contributes to the shape memory ability of the coated hair to keep and recover to the original setting styling. The styling hair can return to the original hair because the polyurethane polymer can be washed out by water with suitable strength and shampoo totally which does not leave any flake. The polyurethane polymer-based hair setting agent has been developed successfully, and it could be coated evenly on the human hair with good hand feeling and SMEs. The SME is highly related to the quantity of polyurethane polymer solution, and the effect could be improved by increasing the solution quantity. The maximum deformation of the coated hair could be recovered 94% at 75°C, once its shape is changed by an external force. The treated hair can withstand warm water rinsing for at least five cycles, and it can keep 65% of its original setting style after water rinsing. The polyurethane polymer could be totally removed by shampooing the hair and hot towel covering for 5-10 min. This research provides an effective way for the development of new intelligent shaping agents. © 2015 Society of Cosmetic Scientists and the Société Française de Cosmétologie.
Federal Register 2010, 2011, 2012, 2013, 2014
2013-05-03
..., ultra-violet light cured polyurethanes, oil or oil-modified or water based polyurethanes, wax, epoxy... obscure the grain, texture or markings of wood include, but are not limited to, paper, aluminum, high... to the CBP. See Notice of Final Determination of Sales at Less Than Fair Value, and Negative...
Influence of carbon nanotubes on mechanical properties and structure of rigid polyurethane foam
NASA Astrophysics Data System (ADS)
Ciecierska, E.; Jurczyk-Kowalska, M.; Bazarnik, P.; Kulesza, M.; Lewandowska, M.; Kowalski, M.; Krauze, S.
2014-08-01
In this work, the influence of carbon nanotubes addition on foam structure and mechanical properties of rigid polyurethane foam/nanotube composites was investigated. Scanning electron microscopy was performed to reveal the foam porous structure and distribution of carbon nanotubes. To determine the mechanical properties, three point bending tests were carried out.
Xingyan Huang; Cornelis F. De Hoop; Jiulong Xie; Chung-Yun Hse; Jinqiu Qi; Tingxing Hu
2017-01-01
Lignin samples fractionated from microwave liquefied switchgrass were applied in the preparation of semirigid polyurethane (PU) foams without purification.The objective of this study was to elucidate the influence of lignin in the PU matrix on themorphological, chemical, mechanical, and thermal properties of thePU foams.The scanning electron microscopy (SEM) images...
Federal Register 2010, 2011, 2012, 2013, 2014
2013-06-19
... Activities; Submission to OMB for Review and Approval; Comment Request; NESHAP for Flexible Polyurethane Foam... Reading Room is open from 8:30 a.m. to 4:30 p.m., Monday through Friday, excluding legal holidays. The... www.regulations.gov . Title: NESHAP for Flexible Polyurethane Foam Production (Renewal) ICR Numbers...
Federal Register 2010, 2011, 2012, 2013, 2014
2012-06-25
... Activities; Submission to OMB for Review and Approval; Comment Request; NESHAP for Flexible Polyurethane Foam... Constitution Avenue NW., Washington, DC. The EPA Docket Center Public Reading Room is open from 8:30 a.m. to 4... Flexible Polyurethane Foam Fabrication (Renewal). ICR Numbers: EPA ICR Number 2027.05, OMB Control Number...
John, Johnson V; Thomas, Reju George; Lee, Hye Ri; Chen, Hongyu; Jeong, Yong Yeon; Kim, Il
2016-08-01
Nanoscale drug carriers fabricated by phospholipid end-capped polyurethane bearing acetal backbones that degrade in acidic conditions are fabricated. These micelles effectively allow drugs to enter the blood circulation, and then disintegrate in acidic endosomes and lysosomes for intelligent delivery of payloads. © 2016 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.
DOT National Transportation Integrated Search
2015-02-01
A case study was conducted by the Louisiana Transportation Research Center (LTRC) to assess the effectiveness of reducing faulting on jointed concrete : pavement (JCP) with polyurethane foam (PF) on LA 1 Bypass, S.P. 034-30-0023. The PF fault correct...
A contractor checklist aimed at helping spray polyurethane foam (SPF) professional contractors protect themselves, workers and others. Guía de las prácticas seguras en el lugar de trabajo para la aplicación del aerosol de espuma aislante de poliuretano.
Code of Federal Regulations, 2014 CFR
2014-07-01
... refrigeration, and sandwich panels —Rigid polyurethane slabstock and other foams —Polystyrene extruded... 29, 2004 Foam Blowing—Unacceptable Substitutes End-use Substitute Decision Comments All foam end-uses: HCFC-141b Unacceptable Alternatives exist with lower or zero = ODP. —Rigid polyurethane and...
Effect of foam age on toxicity of pyrolysis gases from polyurethane flexible foams
NASA Technical Reports Server (NTRS)
Hilado, C. J.; Murphy, R. M.
1978-01-01
The toxicity of the pyrolysis gases from some samples of polyurethane flexible foams appears to have decreased with age, while other samples seem to exhibit no significant change with age in this respect. The changes observed were greater than could be accounted for by variations in the material, or test variations or artifacts.
Code of Federal Regulations, 2013 CFR
2013-07-01
... refrigeration, and sandwich panels —Rigid polyurethane slabstock and other foams —Polystyrene extruded... 29, 2004 Foam Blowing—Unacceptable Substitutes End-use Substitute Decision Comments All foam end-uses: HCFC-141b Unacceptable Alternatives exist with lower or zero = ODP. —Rigid polyurethane and...
Highly stretchable nanoalginate based polyurethane elastomers.
Daemi, Hamed; Barikani, Mehdi; Barmar, Mohammad
2013-06-20
Highly stretchable elastomeric samples based on cationic polyurethane dispersions-sodium alginate nanoparticles (CPUD/SA) were prepared by the solution blending of sodium alginate and aqueous polyurethane dispersions. CPUDs were synthesized by step growth polymerization technique using N-methyldiethanolamine (MDEA) as a source of cationic emulsifier. The chemical structure and thermal-mechanical properties of these systems were characterized using FTIR and DMTA, respectively. The presence of nanoalginate particles including nanobead and nanorod particles were proved by SEM and EDX. It was observed that thermal properties of composites increased with increasing SA content. All prepared samples were known as thermoplastic-elastomers with high percentages of elongation. Excellent compatibility of prepared nanocomposites was proved by the DMTA data. Copyright © 2013 Elsevier Ltd. All rights reserved.
Investigation on Thermal Properties of Kenaf Fibre Reinforced Polyurethane Bio-Composites
NASA Astrophysics Data System (ADS)
Athmalingam, Mathan; Vicki, W. V.
2018-01-01
This research focuses on the effect of Kenaf fibre on thermal properties of Polyurethane (PU) reinforced kenaf bio-composites. The samples were prepared using the polymer casting method with different percentages of kenaf fibre content (5 wt%, 10 wt%, 15 wt%). The thermal properties of Kenaf/PU bio-composite are determined through the Thermogravimetric Analysis and Differential Scanning Calorimeter test. The TGA results revealed that 10 wt% Kenaf/PU bio-composite appeared to be more stable. DSC results show that the glass transition temperature (Tg) value of 10 wt% Kenaf/PU composite is significant to pure polyurethane. It can be said that the thermal stability of 10 wt% Kenaf/PU bio-composite exhibits higher thermal stability compared to other samples.
Investigation into reversion of polyurethane encapsulants
NASA Technical Reports Server (NTRS)
Lynch, C. R.
1973-01-01
The effect of high humidity (95% RH) at 60 C, 70 C, 85 C and 100 C on the solid-to-liquid reversion of polyurethane elastomers (used for potting electrical connectors and conformal coating printed circuit boards) was investigated. Hardness measurements were conducted on eleven elastomers to track reversion for a 101-day period. The primary purpose of the tests was to provide data to predict service life for the polyurethane elastomers. This was not accomplished as the hardness did not deteriorate rapidly enough at the lower test temperatures. The tests did determine that the potting and coating materials most widely used on the S-1C Program are susceptible to reversion but appear adequate for service in the S-1C environment.
Fabrication of a superhydrophobic polyurethane foam and its application for continuous oil removal
NASA Astrophysics Data System (ADS)
Liu, Hai-Dong; Gu, Bin; Yuan, Wei-Feng; He, Qi
2018-02-01
A new polyurethane foam with superhydrophobicity and excellent lipophilicity is presented and demonstrated experimentally in this work. The superhydrophobic foam is synthesized by dip coating the polyurethane foam with a mixture solution of silicone resine and silicon dioxide nanoparticles. Its superhydrophobic and oleophilic capacity is characterized and verified via the SEM images, the water contact angle measurement, the adsorption tests and recyclability tests for water and some typical oils. Combining with the vacuum assisted oil-water separation technology (VAST), continuous recovery of oil spill at the lab scale is realized on the new superhydrophobic foam. Moreover, the break through pressure for water penetrating through the superhydrophobic foam is determined experimentally and referred as the maximum operation pressure in the VAST.
Open-pore polyurethane product
Jefferson, R.T.; Salyer, I.O.
1974-02-17
The method is described of producing an open-pore polyurethane foam having a porosity of at least 50% and a density of 0.1 to 0.5 g per cu cm, and which consists of coherent spherical particles of less than 10 mu diam separated by interconnected interstices. It is useful as a filter and oil absorbent. The product is admirably adapted to scavenging of crude oil from the surface of seawater by preferential wicking. The oil-soaked product may then be compressed to recover the oil or burned for disposal. The crosslinked polyurethane structures are remarkably solvent and heat-resistance as compared with known thermoplastic structures. Because of their relative inertness, they are useful filters for gasoline and other hydrocarbon compounds. (7 claims)
Neng, N R; Pinto, M L; Pires, J; Marcos, P M; Nogueira, J M F
2007-11-09
In this contribution, polyurethane foams are proposed as new polymeric phases for stir bar sorptive extraction (SBSE). Assays performed for polyurethane synthesis demonstrated that four series of formulations (P(1), P(2), P(3) and P(4)) present remarkable stability and excellent mechanical resistance to organic solvents. For polymer clean-up treatment, acetonitrile proved to be the best solvent under sonification, ensuring the reduction of the contamination and interferences. SBSE assays performed on these polyurethane polymers followed by liquid desorption and high-performance liquid chromatography-diode array detection (LD-HPLC-DAD) or large volume injection-capillary gas chromatography-mass spectrometry (LD-LVI-GC-MS), showed that P(2) presents the best recovery yields for atrazine, 2,3,4,5-tetrachlorophenol and fluorene, used as model compounds in water samples at a trace level. SBSE(P(2)) assays performed on this polymer mixed up with several adsorbent materials, i.e. activated carbon, a mesoporous material and a calixarene, did not bring any advantages in relation with the polymeric matrix alone. The comparison between assays performed by SBSE(P(2)) and by the conventional SBSE(PDMS) showed much better performance for the former phase on aqueous samples spiked with atrazine, 2,3,4,5-tetrachlorophenol and fluorene, in which the foremost two analytes present recovery values 3- and 10-fold higher, respectively. The polyurethanes proposed as new polymeric phases for SBSE provided powerful capabilities for the enrichment of organic compounds from aqueous matrices, showing to be indicated mainly in the case of the more polar analytes.
Vedicherla, Srujana; Romanazzo, Sara; Kelly, Daniel J; Buckley, Conor T; Moran, Cathal J
2017-11-28
Purpose/aim of study: Menisectomies account for over 1.5 million surgical interventions in Europe annually, and there is a growing interest in regenerative strategies to improve outcomes in meniscal replacement. The overall objective of this study was to evaluate the role of intraoperatively applied fresh chondrocyte (FC) isolates compared to minced cartilage (MC) fragments, used without cell isolation, to improve bioactivity and tissue integration when combined with a polyurethane replacement. First, to optimize the intraoperative cell isolation protocol, caprine articular cartilage biopsies were digested with 750 U/ml or 3000 U/ml collagenase type II (ratio of 10 ml per g of tissue) for 30 min, 1 h or 12 h with constant agitation and compared to culture-expanded chondrocytes in terms of matrix deposition when cultured on polyurethane scaffolds. Finally, FCs and MC-augmented polyurethane scaffolds were evaluated in a caprine meniscal explant model to assess the potential enhancements on tissue integration strength. Adequate numbers of FCs were harvested using a 30 min chondrocyte isolation protocol and were found to demonstrate improved matrix deposition compared to standard culture-expanded cells in vitro. Upon evaluation in a meniscus explant defect model, both FCs and MC showed improved matrix deposition at the tissue-scaffold interface and enhanced push-out strength, fourfold and 2.5-fold, respectively, compared with the acellular implant. Herein, we have demonstrated a novel approach that could be applied intraoperatively, using FCs or MC for improved tissue integration with a polyurethane meniscal replacement.
Flexible Graphene Composites for Human Space Flight Applications
NASA Technical Reports Server (NTRS)
Sosa, Edward D.
2013-01-01
Graphene oxide allows for better dispersion stability in aqueous and organic solvents. Stabilizers provide dispersion of pristine graphene. Roll coating provide the best coverage of polyurethane sheets. Graphene and GO coated polyurethane used to fabricate flexible laminate composite. Permeation testing indicates that pristine graphene acts as a better gas barrier material. Continuous graphene films are expected to provide even better gas barrier properties.
Self-Calibrating, Variable-Flow Pumping System
NASA Technical Reports Server (NTRS)
Walls, Joe T.
1994-01-01
Pumping system provides accurate, controlled flows of two chemical liquids mixed in spray head and react to form rigid or flexible polyurethane or polyisocyanurate foam. Compatible with currently used polyurethane-based coating materials and gas-bubble-forming agents (called "blowing agents" in industry) and expected to be compatible with materials that used in near future. Handles environmentally acceptable substitutes for chlorofluorocarbon foaming agents.
Polymer compositions and methods
DOE Office of Scientific and Technical Information (OSTI.GOV)
Allen, Scott D.; Willkomm, Wayne R.
The present invention encompasses polyurethane compositions comprising aliphatic polycarbonate chains. In one aspect, the present invention encompasses polyurethane foams, thermoplastics and elastomers derived from aliphatic polycarbonate polyols and polyisocyanates wherein the polyol chains contain a primary repeating unit having a structure: ##STR00001## In another aspect, the invention provides articles comprising the inventive foam and elastomer compositions as well as methods of making such compositions.
Cyanide toxicity from the thermal degradation of rigid polyurethane foam.
Bell, R H; Stemmer, K L; Barkley, W; Hollingsworth, L D
1979-09-01
Thermal degradation products (tdp) from a model, rigid polyurethane foam were collected in such a manner as to eliminate carbon monoxide and other gases with low boiling points. The effects in rats resulting from intratracheal intubation (I.T.) of the tdp are discussed. Cyanide was found to be a major factor associated with severe toxic responses of the experimental rats.
Light-Weight Low-Loss Dielectric Polymer Composites Containing Carbon Nanostructure
2014-10-17
increases in temperature. Subsequent thermal breakdown and carbonization of the polyurethane coating and polyimide substrate significantly reduced the RF...measurements through HD-GNR films. For the highly uniform films produced in separate experiments on a glass substrate with sufficient thermal conductivity ...further carbonized the polyurethane- coated polyimide substrate. This was attributed to the electromagnetic and the resulting thermal energy
Measuring Rind Thickness on Polyurethane Foam
NASA Technical Reports Server (NTRS)
Johnson, C.; Miller, J.; Brown, H.
1985-01-01
Nondestructive test determines rind thickness of polyurethane foam. Surface harness of foam measured by Shore durometer method: hardness on Shore D scale correlates well with rind thickness. Shore D hardness of 20, for example, indicates rind thickness of 0.04 inch (1 millimeter). New hardness test makes it easy to determine rind thickness of sample nondestructively and to adjust fabrication variables accordingly.
Polymer compositions and methods
Allen, Scott D.; Willkomm, Wayne R.
2016-09-27
The present invention encompasses polyurethane compositions comprising aliphatic polycarbonate chains. In one aspect, the present invention encompasses polyurethane foams, thermoplastics and elastomers derived from aliphatic polycarbonate polyols and polyisocyanates wherein the polyol chains contain a primary repeating unit having a structure: ##STR00001## In another aspect, the invention provides articles comprising the inventive foam and elastomer compositions as well as methods of making such compositions.
Self-organization of the reticular structure of polyurethane
NASA Astrophysics Data System (ADS)
Kiselev, M. R.; Roldugin, V. I.
2010-08-01
The morphology of block samples and coatings of reticular polyurethane were studied by transmission electron microscopy. The morphology was correlated with the internal stresses that appeared in the coatings during their formation. A scenario of the self-assembly of complex structures in reticular polymers was suggested. The boundary between the structural elements of the supermolecular level was found to be strained.
Cakic, Suzana; Lacnjevac, Caslav; Stamenkovic, Jakov; Ristic, Nikola; Takic, Ljiljana; Barac, Miroljub; Gligoric, Miladin
2007-01-01
Two kinds of aqueous acrylic polyols (single step and multi step synthesis type) have been investigated for their performance in the two-component aqueous polyurethane application, by using more selective catalysts. The aliphatic polyfunctional isocyanates based on hexamethylen diisocyanates have been employed as suitable hardeners. The complex of zirconium, commercially known as K-KAT®XC-6212, and manganese (III) complexes with mixed ligands based on the derivative of maleic acid have been used as catalysts in this study. Both of the aqueous polyols give good results, in terms of application and hardness, when elevated temperatures and more selective catalysts are applied. A more selective catalyst promotes the reaction between the isocyanate and polyol component. This increases the percentage of urethane bonds and the degree of hardness in the films formed from the two components of aqueous polyurethane lacquers. The polyol based on the single step synthesis route is favourable concerning potlife and hardness. The obtained results show that the performance of the two-component aqueous polyurethane coatings depends on the polymer structure of the polyols as well as on the selectivity of the employed catalyst.
Shape Memory Polyurethane Materials Containing Ferromagnetic Iron Oxide and Graphene Nanoplatelets
Urban, Magdalena
2017-01-01
Intelligent materials, such as memory shape polymers, have attracted considerable attention due to wide range of possible applications. Currently, intensive research is underway, in matters of obtaining memory shape materials that can be actuated via inductive methods, for example with help of magnetic field. In this work, an attempt was made to develop a new polymer composite—polyurethane modified with graphene nanoplates and ferromagnetic iron oxides—with improved mechanical properties and introduced magnetic and memory shape properties. Based on the conducted literature review, gathered data were compared to the results of similar materials. Obtained materials were tested for their thermal, rheological, mechanical and shape memory properties. Structure of both fillers and composites were also analyzed using various spectroscopic methods. The addition of fillers to the polyurethane matrix improved the mechanical and shape memory properties, without having a noticeable impact on thermal properties. As it was expected, the high content of fillers caused a significant change in viscosity of filled prepolymers (during the synthesis stage). Each of the studied composites showed better mechanical properties than the unmodified polyurethanes. The addition of magnetic particles introduced additional properties to the composite, which could significantly expand the functionality of the materials developed in this work. PMID:28906445
Uthamaraj, Susheil; Tefft, Brandon J; Jana, Soumen; Hlinomaz, Ota; Kalra, Manju; Lerman, Amir; Dragomir-Daescu, Dan; Sandhu, Gurpreet S
2016-10-26
Stent-grafts are widely used for the treatment of various conditions such as aortic lesions, aneurysms, emboli due to coronary intervention procedures and perforations in vasculature. Such stent-grafts are manufactured by covering a stent with a polymer membrane. An ideal stent-graft should have a biocompatible stent covered by a porous, thromboresistant, and biocompatible polymer membrane which mimics the extracellular matrix thereby promoting injury site healing. The goal of this protocol is to manufacture a small caliber stent-graft by encapsulating a balloon expandable stent within two layers of electrospun polyurethane nanofibers. Electrospinning of polyurethane has been shown to assist in healing by mimicking native extracellular matrix, thereby promoting endothelialization. Electrospinning polyurethane nanofibers on a slowly rotating mandrel enabled us to precisely control the thickness of the nanofibrous membrane, which is essential to achieve a small caliber balloon expandable stent-graft. Mechanical validation by crimping and expansion of the stent-graft has shown that the nanofibrous polyurethane membrane is sufficiently flexible to crimp and expand while staying patent without showing any signs of tearing or delamination. Furthermore, stent-grafts fabricated using the methods described here are capable of being implanted using a coronary intervention procedure using standard size guide catheters.
Amphiphilic Polyurethane Hydrogels as Smart Carriers for Acidic Hydrophobic Drugs.
Fonseca, Lucas P; Trinca, Rafael B; Isabel Felisberti, Maria
2018-05-14
Amphiphilic hydrogels are widely reported as systems with great potential for controlled drug release. Nevertheless, the majority of studies make use of functionalization or attachment of drugs to the polymer chains. In this study, we propose a strategy of combining amphiphilic polyurethanes with pH-responsive drugs to develop smart drug carriers. While the amphiphilic character of the polymer imparts an efficient load of hydrophobic and hydrophilic drugs, the drug's characteristics determine the selectivity of the medium delivery. Drug loading and release behavior as well as hydrolytic degradation of chemically crosslinked polyurethane hydrogels based on PEG and PCL-triol (PU (polyurethane) hydrogels) synthesized by an easy one-pot route were studied. PU hydrogels have been shown to successfully load the hydrophobic acidic drug sodium diclofenac, reaching a partition coefficient of 8 between the most hydrophobic PU and diclofenac/ethanol solutions. Moreover, an oral administration simulation was conducted by changing the environment from an acidic to a neutral medium. PU hydrogels release less than 5 % of the drug in an acidic medium; however, in a PBS pH 7.4 solution, diclofenac is delivered in a sustained fashion for up to 40 hours, achieving 80% of cumulative release. Copyright © 2018. Published by Elsevier B.V.
Preparation and characterization of plasticized palm-based polyurethane solid polymer electrolyte
DOE Office of Scientific and Technical Information (OSTI.GOV)
Daud, Farah Nadia; Ahmad, Azizan; Badri, Khairiah Haji
2013-11-27
Palm-based polyurethane solid polymer electrolyte was prepared via prepolymerization method between palm kernel oil based polyols (PKO-p) and 2,4’-diphenylmethane diisocyanate (2,4’-MDI) in acetone at room temperature with the vary amount of lithium trifuoromethanesulfonate (LiCF{sub 3}SO{sub 3}) salt and polyethylene glycol (PEG). The film was analyzed using attenuated total reflection infrared (ATR-IR) spectroscopy, electrochemical impedance spectroscopy (EIS) and X-ray diffractometry (XRD). EIS result indicated ionic conductivity obtained with 30 wt% LiCF3SO3 increased to 6.55 × 10{sup −6} S cm{sup −1} when 10 wt.% of plasticizer was added into the system. FTIR analysis showed the interaction between lithium ions and amine (-N-H)more » at 3600–3100 cm{sup −1}, carbonyl (-C=O) at 1750–1650 cm{sup −1} and ether (-C-O-C-) at 1150–1000 cm{sup −1} of the polyurethane forming polymer-salt complexes. The XRD result confirmed that LiCF{sub 3}SO{sub 3} salt completely dissociated within the polyurethane film with the absence of crystalline peaks of LiCF{sub 3}SO{sub 3}.« less
Matsumura, Hajime; Imai, Ryutaro; Ahmatjan, Niyaz; Ida, Yukiko; Gondo, Masahide; Shibata, Dai; Wanatabe, Katsueki
2014-02-01
In recent years, adhesive wound dressings have been increasingly applied postoperatively because of their ease of use as they can be kept in place without having to cut and apply surgical tapes and they can cover a wound securely. However, if a wound dressing strongly adheres to the wound, a large amount of stratum corneum is removed from the newly formed epithelium or healthy periwound skin. Various types of adhesives are used on adhesive wound dressings and the extent of skin damage depends on how much an adhesive sticks to the wound or skin surface. We quantitatively determined and compared the amount of stratum corneum removed by eight different wound dressings including polyurethane foam using acrylic adhesive, silicone-based adhesive dressing, composite hydrocolloid and self-adhesive polyurethane foam in healthy volunteers. The results showed that wound dressings with silicone adhesive and self-adhesive polyurethane foam removed less stratum corneum, whereas composite hydrocolloid and polyurethane foam using acrylic adhesive removed more stratum corneum. © 2012 The Authors. International Wound Journal © 2012 Medicalhelplines.com Inc and John Wiley & Sons Ltd.
Li, Yang; Ren, Hongfeng; Ragauskas, Arthur J
2011-08-01
Novel rigid polyurethane nanocomposite foams have been prepared by the polymerization of a sucrose-based polyol, a glycerol-based polyol and polymeric diphenylmethane diisocyanate in the presence of cellulose whiskers. Varying amounts of sulfuric acid hydrolyzed cellulose whiskers (0.25, 0.50, 0.75 and 1.00 wt%) prepared from a commercial fully bleached softwood kraft pulp were incorporated to investigate the effect of its dosage on the mechanical and thermal properties of polyurethane nanocomposites. Fourier transform infrared spectra of the nanocomposite foams suggested that additional hydrogen bonds were developed and crosslinking occurred between the hydroxyl groups of cellulose whiskers and isocyanate groups which increased the phase separation of soft and hard segments in the polyurethane. The closed cells of control foam and nanocomposite foams were homogeneously dispersed and the cell sizes were approximately 350 microm in diameter as observed by scanning electron microscope. A substantial improvement of mechanical properties at low whisker content (< or = 1.00 wt%) was obtained, especially the compressive strength and modulus at 1.00 wt% whiskers content which were increased by 269.7% and 210.0%, respectively. Thermal stability of the nanocomposites was also enhanced as determined by differential scanning calorimetry and thermogravimetric analysis.
Numerical model describing optimization of fibres winding process on open and closed frame
NASA Astrophysics Data System (ADS)
Petrů, M.; Mlýnek, J.; Martinec, T.
2016-08-01
This article discusses a numerical model describing optimization of fibres winding process on open and closed frame. The quality production of said type of composite frame depends primarily on the correct winding of fibers on a polyurethane core. It is especially needed to ensure the correct angles of the fibers winding on the polyurethane core and the homogeneity of individual winding layers. The article describes mathematical model for use an industrial robot in filament winding and how to calculate the trajectory of the robot. When winding fibers on the polyurethane core which is fastened to the robot-end-effector so that during the winding process goes through a fibre-processing head on the basis of the suitably determined robot-end-effector trajectory. We use the described numerical model and matrix calculus to enumerate the trajectory of the robot-end-effector to determine the desired passage of the frame through the fibre-processing head. The calculation of the trajectory was programmed in the Delphi development environment. Relations of the numerical model are important for use a real solving of the passage of a polyurethane core through fibre-processing head.
Shahrousvand, Mohsen; Hoseinian, Monireh Sadat; Ghollasi, Marzieh; Karbalaeimahdi, Ali; Salimi, Ali; Tabar, Fatemeh Ahmadi
2017-05-01
Nowadays, the discovery of cell behaviors and their responses in communication with the stem cell niches and/or microenvironments are one of the major topics in tissue engineering and regenerative medicine. In this study, incorporated organic-inorganic polyurethane (PU) nanocomposites were prepared for better understanding of cell signaling and the effect of magnetite nanoparticles on cell proliferation and cell responses. The properties of PU-IONs were evaluated by fourier transform infrared spectroscopy (FTIR), scanning electron microscopy (SEM), atomic-force microscopy (AFM), differential scanning calorimetry (DSC), X-ray diffraction (XRD) and electrochemical impedance spectroscopy (EIS). The presence of the iron oxide nanoparticles (IONs) affects on the properties of polyurethane nanocomposites such as bulk morphology, mechanical, electrochemical, and biological properties. The electrical conductivity and hydrophilicity of PU-IONs were improved by increasing the magnetite nanoparticles; therefore water absorption, biodegradation and cell viability were changed. The biocompatibility of PU-IONs was investigated by MTT assay, cell attachment and cell staining. According to the results, the magnetite polyurethane nanocomposites could be a potential choice for cell therapy and tissue engineering, especially nerve repair. Copyright © 2016 Elsevier B.V. All rights reserved.
Lavrador, Catarina; Mascarenhas, Ramiro; Coelho, Paulo; Brites, Cláudia; Pereira, Alfredo; Gogolewski, Sylwester
2016-03-01
Bone substitutes have been a critical issue as the natural source can seldom provide enough bone to support full healing. No bone substitute complies with all necessary functions and characteristics that an autograft does. Polyurethane sponges have been used as a surgical alternative to cancellous bone grafts for critical bone defect donor sites. Critical bone defects were created on the tibial tuberosity and iliac crest using an ovine model. In group I (control-untreated), no bone regeneration was observed in any animal. In group II (defects left empty but covered with a microporous polymeric membrane), the new bone bridged the top ends in all animals. In groups III and IV, bone defects were implanted with polyurethane scaffolds modified with biologically active compounds, and bone regeneration was more efficient than in group II. In groups III and IV there were higher values of bone regeneration specific parameters used for evaluation (P < 0.05) although the comparison between these groups was not possible. The results obtained in this study suggest that biodegradable polyurethane substitutes modified with biologically active substances may offer an alternative to bone graft, reducing donor site morbidity associated with autogenous cancellous bone harvesting.
NASA Astrophysics Data System (ADS)
He, Chunli; Wang, Miao; Cai, Xianmei; Huang, Xiaobo; Li, Li; Zhu, Haomiao; Shen, Jian; Yuan, Jiang
2011-11-01
To improve hydrophilicity and blood compatibility properties of polyurethane (PU) film, we chemically induced graft copolymerization of 2-hydroxyethyl methacrylate (HEMA) onto the surface of polyurethane film using benzoyl peroxide as an initiator. The effects of grafting temperature, grafting time, monomer and initiator concentrations on the grafting yields were studied. The maximum grafting yield value was obtained 0.0275 g/cm2 for HEMA. Characterization of the films was carried out by attenuated total reflection Fourier transform infrared spectroscopy (ATR-FTIR), water contact angle measurements. ATR-FTIR data showed that HEMA was successfully grafted onto the PU films surface. Water contact angle measurement demonstrated the grafted films possessed a relatively hydrophilic surface. The blood compatibility of the grafted films was preliminarily evaluated by a platelet-rich plasma adhesion test and hemolysis test. The results of platelet adhesion experiment showed that polyurethane grafted polymerization with monomer of 2-hydroxyethyl methacrylate had good blood compatibility featured by the low platelet adhesion. Hemolysis rate of the PU-g-PHEMA films was dramatically decreased than the ungrafted PU films. This kind of new biomaterials grafted with HEMA monomers might have a potential usage for biomedical applications.
Shape Memory Polyurethane Materials Containing Ferromagnetic Iron Oxide and Graphene Nanoplatelets.
Urban, Magdalena; Strankowski, Michał
2017-09-14
Intelligent materials, such as memory shape polymers, have attracted considerable attention due to wide range of possible applications. Currently, intensive research is underway, in matters of obtaining memory shape materials that can be actuated via inductive methods, for example with help of magnetic field. In this work, an attempt was made to develop a new polymer composite-polyurethane modified with graphene nanoplates and ferromagnetic iron oxides-with improved mechanical properties and introduced magnetic and memory shape properties. Based on the conducted literature review, gathered data were compared to the results of similar materials. Obtained materials were tested for their thermal, rheological, mechanical and shape memory properties. Structure of both fillers and composites were also analyzed using various spectroscopic methods. The addition of fillers to the polyurethane matrix improved the mechanical and shape memory properties, without having a noticeable impact on thermal properties. As it was expected, the high content of fillers caused a significant change in viscosity of filled prepolymers (during the synthesis stage). Each of the studied composites showed better mechanical properties than the unmodified polyurethanes. The addition of magnetic particles introduced additional properties to the composite, which could significantly expand the functionality of the materials developed in this work.
NASA Astrophysics Data System (ADS)
Caon, Thiago; Zanetti-Ramos, Betina Giehl; Lemos-Senna, Elenara; Cloutet, Eric; Cramail, Henri; Borsali, Redouane; Soldi, Valdir; Simões, Cláudia Maria Oliveira
2010-06-01
The in vitro cytotoxicity and DNA damage evaluation of biodegradable polyurethane-based micro- and nanoparticles were carried out on animal fibroblasts. For cytotoxicity measurement and primary DNA damage evaluation, MTT and Comet assays were used, respectively. Different formulations were tested to evaluate the influence of chemical composition and physicochemical characteristics of particles on cell toxicity. No inhibition of cells growth surrounding the polyurethane particles was observed. On the other hand, a decrease of cell viability was verified when the anionic surfactant sodium dodecyl sulfate (SDS) was used as droplets stabilizer of monomeric phase. Polyurethane nanoparticles stabilized with Tween 80 and Pluronic F68 caused minor cytotoxic effects. These results indicated that the surface charge plays an important role on cytotoxicity. Particles synthesized from MDI displayed a higher cytotoxicity than those synthesized from IPDI. Size and physicochemical properties of the particles may explain the higher degree of DNA damage produced by two tested formulations. In this way, a rational choice of particles' constituents based on their cytotoxicity and genotoxicity could be very useful for conceiving biomaterials to be used as drug delivering systems.
Kavanaugh, Taylor E.; Clark, Amy Y.; Chan-Chan, Lerma H.; Ramírez-Saldaña, Maricela; Vargas-Coronado, Rossana F.; Cervantes-Uc, José M.; Hernández-Sánchez, Fernando; García, Andrés J.; Cauich-Rodríguez, Juan V.
2016-01-01
The development of elastomeric, bioresorbable and biocompatible segmented polyurethanes (SPUs) for use in tissue-engineering applications has attracted considerable interest because of the existing need of mechanically tunable scaffolds for regeneration of different tissues, but the incorporation of osteoinductive molecules into SPUs has been limited. In this study, segmented polyurethanes were synthesized from poly (ε-caprolactone)diol, 4,4’-methylene bis(cyclohexyl isocyanate) (HMDI) using biologically active compounds such as ascorbic acid, L-glutamine, β-glycerol phosphate, and dexamethasone as chain extenders. Fourier Transform Infrared Spectroscopy (FTIR) revealed the formation of both urethanes and urea linkages while Differential Scanning Calorimetry, Dynamic Mechanical Analysis, X-ray Diffraction and mechanical testing showed that these polyurethanes were semi-crystalline polymers exhibiting high deformations. Cytocompatibility studies showed that only SPUs containing β-glycerol phosphate supported human mesenchymal stem cell (hMSC) adhesion, growth, and osteogenic differentiation, rendering them potentially suitable for bone tissue regeneration, whereas other SPUs failed to support either cell growth or osteogenic differentiation, or both. This study demonstrates that modification of SPUs with osteogenic compounds can lead to new cytocompatible polymers for regenerative medicine applications. PMID:26704555
Reva, V A; Litinskii, M A; Denisov, A V; Sokhranov, M V; Telitskii, S Yu; Samokhvalov, I M
2015-04-01
Today self-expanding polymers are considered as the most promising as means for intracavitary hemostasis in case of continuing bleeding after trauma. Testing of domestic open-cell polyurethane foam composition "Locus" was carried out on the developed experimental model simulating liver trauma of V degree. After damaging 6 experimental rabbits were injected intraperitoneally with 80 ml of the composition. 5 experimental rabbits were included into to control group (haemostatic agent was not given). Estimated blood loss was 111-124 ml. The two-hour survival rate didn't differ significantly: 3 animals survived in the experimental group; 2 animal survived in the control. Despite the 3-4-fold widening of the foam, due to open cells it absorbed 72.6 +/- 8.3 g of blood. Thus, open-cell polyurethane foam intraperitoneal administration of the composition didn't provide a temporary intra-abdominal hemostasis in liver. In order to enhance the hemostatic effect it requires changing the formulation of the polyurethane composition. For a more accurate assessment of the results it is neccessary to perform additional researches on larger animals.
NASA Astrophysics Data System (ADS)
Shakir, Amira Shakim Abdul; Badri, Khairiah Haji; Hua, Chia Chin
2016-11-01
An environmental-friendly blowing agent has been used to fabricate flexible polyurethane (PU) foam. Polyurethane foam was prepared from palm kernel oil-based monoester polyol (PKO-p) via prepolymerization method. Acetone has been used as solvent in this study. The developed polyurethane foam was characterized using tensile, differential scanning calorimetry analysis (DSC), thermogravimetric analysis (TGA), optical microscope and drop shape analyzer. The mechanical properties of the PU-reference (PU-R) and PU-NaHCO3 foam was analyzed by tensile using ASTM D 3574-01. From the results, the elongation of PU- NaHCO3 shows reduction to 26.3 % compared to PU-R. The DSC showed two glass transition temperatures in all samples that belonged to the PU-R and PU-NaHCO3. TGA revealed that the incorporation of sodium hydrogen carbonate into the PU system did not show significant difference as compared to the control PU. The morphology of both PU was investigated using optical microscope. Contact angle has been measured to determine the hydrophobicity of the PU. The PU- NaHCO3 exhibited an increase in contact angle (93.1°).
Green waste cooking oil-based rigid polyurethane foam
NASA Astrophysics Data System (ADS)
Enderus, N. F.; Tahir, S. M.
2017-11-01
Polyurethane is a versatile polymer traditionally prepared using petroleum-based raw material. Petroleum, however, is a non-renewable material and polyurethane produced was found to be non-biodegradable. In quest for a more environmentally friendly alternative, wastecooking oil, a highly abundant domestic waste with easily derivatized structure, is a viable candidate to replace petroleum. In this study,an investigation to determine physical and chemical properties of rigid polyurethane (PU) foam from waste cooking oil (WCO) was carried out. WCO was first adsorbed by using coconut husk activated carbon adsorbent prior to be used for polyol synthesis. The purified WCO was then used to synthesize polyol via transesterification reaction to yield alcohol groups in the WCO chains structure. Finally, the WCO-based polyol was used to prepare rigid PU foam. The optimum formulation for PU formation was found to be 90 polyol: 60 glycerol: 54 water: 40 diethanolamine: 23 diisocyanate. The rigid PU foam has density of 208.4 kg/m3 with maximum compressive strength and capability to receive load at 0.03 MPa and 0.09 kN, respectively. WCO-based PU can potentially be used to replace petroleum-based PU as house construction materials such as insulation panels.
Tunable Elastomers with an Antithrombotic Component for Cardiovascular Applications.
Stahl, Alexander M; Yang, Yunzhi Peter
2018-05-31
This study reports the development of a novel family of biodegradable polyurethanes for use as tissue engineered cardiovascular scaffolds or blood-contacting medical devices. Covalent incorporation of the antiplatelet agent dipyridamole into biodegradable polycaprolactone-based polyurethanes yields biocompatible materials with improved thromboresistance and tunable mechanical strength and elasticity. Altering the ratio of the dipyridamole to the diisocyanate linking unit and the polycaprolactone macromer enables control over both the drug content and the polymer cross-link density. Covalent cross-linking in the materials achieves significant elasticity and a tunable range of elastic moduli similar to that of native cardiovascular tissues. Interestingly, the cross-link density of the polyurethanes is inversely related to the elastic modulus, an effect attributed to decreasing crystallinity in the more cross-linked polymers. In vitro characterization shows that the antiplatelet agent is homogeneously distributed in the materials and is released slowly throughout the polymer degradation process. The drug-containing polyurethanes support endothelial cell and vascular smooth muscle cell proliferation, while demonstrating reduced levels of platelet adhesion and activation, supporting their candidacy as promising substrates for cardiovascular tissue engineering. © 2018 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.
Probing nanodispersions of clays for reactive foaming.
Harikrishnan, G; Lindsay, Chris I; Arunagirinathan, M A; Macosko, Christopher W
2009-09-01
Nanodispersions of clays in polyurethane components have been prepared. Nanoclays (both natural and organically modified) of various aspect ratios are used. The fillers are dispersed separately in polyurethane components, viz., polyol and polyisocyanate. The nanodispersions are characterized by the combined use of solution rheology, X-ray scattering, cryo-electron microscopy, and IR spectroscopy. Reactive foaming of these nanodispersions is carried out to make polyurethane nanocomposite foams. The status of the dispersion of fillers in components and in foams has been compared to investigate the effect of the foaming process in exfoliation. Interpretation of the results from different characterization techniques describes the state of the dispersion of fillers in components and in foam. The rheological and physicochemical behaviors of nanodispersions are shown to have a significant influence on the properties of nanocomposite foams.
Ma, Shuang; Zhang, Huiyi; Sablong, Rafaël J; Koning, Cor E; van Benthem, Rolf A T M
2018-05-01
t-Butyl-oxycarbonylated diamines ("di-Boc-carbamates") are investigated as dicarbamate monomers for diamine/dicarbamate polymerizations. Polyureas (PUs) and polyurethanes (PURs) with high molecular weights are prepared from stoichiometric polymerizations of diamines or diols with N-N'-di-t-butyl-oxycarbonyl isophorone diamine (DiBoc-IPDC) using KOt-Bu as a catalyst, while gelation is observed when an excess of DiBoc-IPDC is used with respect to the diamines or diols. Stable dispersions are obtained from PUs and PURs with 3,3'-diamino-N-methyldipropylamine (DMDPA) as internal dispersing agent. The corresponding PU-based coatings exhibit superior mechanical properties and solvent resistances compared to the polyurethane urea coatings synthesized from diols, DiBoc-IPDC, and DMDPA. © 2018 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.
Positron lifetime spectroscopy in thin polymer coatings
NASA Technical Reports Server (NTRS)
Singh, Jag J.; Eftekhari, Abe; Sprinkle, Danny R.
1990-01-01
Polymer coatings are finding increasing applications in aerospace industry. The effectiveness of coatings depends strongly on their microstructure and adhesion to the substrates. Currently, there is no technique for adequately monitoring the quality of the coatings. We adapted positron lifetime spectroscopy for the investigation of thin coatings. Results of measurements on 0.001-in-thick polyurethane coatings on aluminum and steel substrates and thicker (0.080-in.) self-standing polyurethane discs were compared. In all cases, we find positron lifetime groups centered around 560 ps, corresponding to the presence of 0.9 A exp 3 free volume cells. However, the number of free volume cells in thin coatings is larger, suggesting that the morphology of thin coatings is different from that of bulk polyurethane. These results and their structural implications are discussed.
Federal Register 2010, 2011, 2012, 2013, 2014
2010-07-01
... the environmental control system (ECS). This AD results from reports of duct assemblies in the ECS... assemblies in the ECS wrapped with BMS 8-39 polyurethane foam insulation, a material of which the fire... igniting the BMS 8-39 polyurethane foam insulation on the duct assemblies of the ECS, which could propagate...
2014-10-02
Journal article published in International Biodeterioration & Biodegradation 95 (2014) 311-319. The U.S. Government is joint author of the work and...SUBJECT TERMS pseudomonas biofilms, polyurethane, biodegradation , FTIR spectroscopy, citrate, impranil 16. SECURITY CLASSIFICATION OF: 17. LIMITATION OF...International Biodeterioration & Biodegradation 95 (2014) 311e319Contents lists avaiInternational Biodeterioration & Biodegradation journal homepage
Characterization of Tape Adhesion to Chemical Agent Resistant Coatings
2015-01-01
use by OEM’s and depots. More specifically, each tape was tested on water dispersible and solvent borne polyurethane topcoats in the two most common...andGenerally, systems formulated to be water dispersible produced films that were slightly hydrophilic (water contact angle < 90°) whereas systems...8). Table 8: Average water contact angle of various CARC systems. advancing contact angle of water (degrees) waterborne polyurethane
Dynamic Multivariate Accelerated Corrosion Test Protocol
2014-10-01
atmospheric, accelerated, AA2024-T3, AA6061-T6, AA7075-T3, 1010 steel, AgCl, rare earth conversion coat, magnesium rich primer, polyurethane , Eyring, Monte...morphology and elemental analysis by scanning electron microscopy-energy dispersive spectroscopy (SEM-EDS) and electrochemical determinations of...in the FT-IR analysis; degradation of the components of the high performance polyurethane coatings exposed in the UV/ozone chamber were more
Jen-Chieh Liu; Darren J. Martin; Robert J. Moon; Jeffrey P. Youngblood
2015-01-01
Freeze-dried cellulose nanocrystals (CNCs) were dispersed in the thermoplastic polyurethane [Pellethane 2363-55D (P55D)] by a solvent casting method to fabricate CNC-reinforced nanocomposites. This study demonstrated that the addition of small amounts (1â5 wt %) of CNCs to P55D increased the thermal degradation temperature while maintaining a similar stiffness,...
Analysis Techniques, Materials, and Methods for Treatment of Thermal Bridges in Building Envelopes
2013-08-01
effects of the R-value for given increment of time ............................................. 89 64 Crystals on a post-conditioned Aspen Aerogel ... aerogel on specific sites compared to conventional polyurethane foam insulation. Figures 55 and 56 show two examples of preliminary parametric... Aerogel , and (4) Honeywell’s polyurethane. Table 14 lists the four tested insulation ma- terials, their experimental thermal properties (derived
Shock Tube Test for Energy Absorbing Materials
2013-09-13
rigid and lightweight foam material with a closed-cell structure, and a very high strength-to-weight ratio (7). It is commonly used as a sandwich...including application in helmet liners (8). Zorbium™ is the viscoelastic polyurethane foam used in military helmet suspension system pads (9). 8...viscoelastic polyurethane foam which shows strain rate dependent behavior when compressed. This is displayed by the significant difference in response
NASA Astrophysics Data System (ADS)
Yakushin, V. A.; Zhmud', N. P.; Stirna, U. K.
2002-05-01
The effect of processing factors on the inhomogeneity and physicomechanical characteristics of spray-on polyurethane foams is studied. The dependences of the basic characteristics of foam plastics on the apparent density and cell-shape factor are determined. A method is offered for evaluating the effect of the technological surface skin on the tensile characteristics of foam plastics under normal and low temperatures.
Inhibition of Microbial Growth by Fatty Amine Catalysts from Polyurethane Foam Test Tube Plugs
Bach, John A.; Wnuk, Richard J.; Martin, Delano G.
1975-01-01
When polyurethane foam test tube plugs are autoclaved, they release volatile fatty amines that inhibit the growth of some microorganisms. The chemical structures of these amines were determined by the use of a gas chromatographmass spectrometer. They are catalysts used to produce the foam. The problem of contaminating growth media with toxic substances released from polymeric materials is discussed. PMID:1096816
Maurer, C A; Renzulli, P; Baer, H U; Mettler, D; Uhlschmid, G; Neuenschwander, P; Suter, U W; Triller, J; Zimmermann, A
2000-02-01
In an attempt to overcome some of the problems encountered with the materials available for liver embolisation, we investigated a novel radiopaque polymer of the polyurethane family (Degra-Bloc). Hepatic artery embolisation of one liver lobe using polyurethane was performed in 19 healthy pigs. Microcirculatory changes were assessed by laser Doppler flowmetry. Radiological and pathological examinations of the livers, hearts and lungs removed provided information about the extent and effect of the embolisation. None of the pigs died due to hepatic failure or toxicity of polyurethane. Microcirculation of embolised liver lobes significantly decreased from 106 (+/-15) perfusion units (PU) to 45 (+/-6) PU immediately after embolisation and further to 28 (+/-7) PU before euthanasia. At this time conventional and angiographic X-ray controls demonstrated the radiopaque casts extending up to the peripheral arteries with signs of degradation over time but without formation of collateral vessels. The main pathological findings consisted of destruction of the portal tract structures and also of large areas of liver necrosis. Polyurethane was encountered in arterioles as small as 10-20 microm, but not in liver sinusoids, hearts or lungs. The novel polymer called DegraBloc is a biocompatible, slowly degradable, radiopaque embolic agent. The occlusion of the arterial tree up to the smallest arteriolar diameter combined with concomitant portal vein occlusion leads to sharp segmental necrosis in pig livers without formation of significant collaterals and without systemic embolism. In the treatment of liver tumours polyurethane might provide a promising alternative to conventional embolic materials, provided that it is used with care in patients with advanced liver cirrhosis.
Design and milling manufacture of polyurethane custom contoured cushions for wheelchair users.
da Silva, Fabio Pinto; Beretta, Elisa Marangon; Prestes, Rafael Cavalli; Kindlein Junior, Wilson
2011-01-01
The design of custom contoured cushions manufactured in flexible polyurethane foams is an option to improve positioning and comfort for people with disabilities that spend most of the day seated in the same position. These surfaces increase the contact area between the seat and the user. This fact contributes to minimise the local pressures that can generate problems like decubitus ulcers. The present research aims at establishing development routes for custom cushion production to wheelchair users. This study also contributes to the investigation of Computer Numerical Control (CNC) machining of flexible polyurethane foams. The proposed route to obtain the customised seat began with acquiring the user's contour in adequate posture through plaster cast. To collect the surface geometry, the cast was three-dimensionally scanned and manipulated in CAD/CAM software. CNC milling parameters such as tools, spindle speeds and feed rates to machine flexible polyurethane foams were tested. These parameters were analysed regarding the surface quality. The best parameters were then tested in a customised seat. The possible dimensional changes generated during foam cutting were analysed through 3D scanning. Also, the customised seat pressure and temperature distribution was tested. The best parameters found for foams with a density of 50kg/cm(3) were high spindle speeds (24000 rpm) and feed rates between 2400-4000mm/min. Those parameters did not generate significant deformities in the machined cushions. The custom contoured cushion satisfactorily increased the contact area between wheelchair and user, as it distributed pressure and heat evenly. Through this study it was possible to define routes for the development and manufacturing of customised seats using direct CNC milling in flexible polyurethane foams. It also showed that custom contoured cushions efficiently distribute pressure and temperature, which is believed to minimise tissue lesions such as pressure ulcers.
Cosgriff-Hernandez, Elizabeth; Tkatchouk, Ekaterina; Touchet, Tyler; Sears, Nick; Kishan, Alysha; Jenney, Christopher; Padsalgikar, Ajay D; Chen, Emily
2016-07-01
Although silicone-based polyurethanes have demonstrated increased oxidative stability, there have been conflicting reports of the long-term hydrolytic stability of Optim™ and PurSil(®) 35 based on recent temperature-accelerated hydrolysis studies. The goal of the current study was to identify in vitro-in vivo correlations to determine the relevance of this accelerated in vitro model for predicting clinical outcomes. Temperature-accelerated hydrolytic aging of three commonly used cardiac lead insulation materials, Optim™, Elasthane™ 55D, Elasthane™ 80A, and a related silicone-polyurethane, PurSil(®) 35, was performed. After 1 year at 85°C, similar losses in Mn and Mz were observed for the poly(ether urethanes), but an increase in Mz loss as compared to Mn loss was observed for the silicone-based polyurethanes. A similar trend of increased Mz loss as compared to Mn loss was observed in explanted Optim™ leads after 2-3 years; however, no statistically significant Mn loss was detected between 2-3 and 7-8 years of implantation. Given this preferential loss of high molecular weight chains, it was hypothesized that the observed differences between the polyurethanes were due to allophanate dissociation rather than backbone chain scission. Following full dissociation of the small percentage of allophanates in vivo, the observed molecular weight stability and proven clinical performance of Optim™ was attributed to the well-documented stability of the urethane bond under physiological conditions. This allophanate dissociation reaction is incompatible with the first order mechanism proposed in previous temperature-accelerated hydrolysis studies and may be the reason for the model's inaccurate prediction of significant and progressive molecular weight loss in vivo. © 2016 Wiley Periodicals, Inc. J Biomed Mater Res Part A: 104A: 1805-1816, 2016. © 2016 Wiley Periodicals, Inc.
Synthesis and characterization of novel fluoroalkyl-terminated hyperbranched polyurethane latex
NASA Astrophysics Data System (ADS)
Xu, Wei; Zhao, Weijia; Hao, Lifen; Wang, Sha; Pei, Mengmeng; Wang, Xuechuan
2018-04-01
Waterborne polyurethane (PU) emulsions are widely used in various fields and the demand for them is ever-increasing over the years. However, the hydrophilic chain extender inevitably bonded into the PU backbone can affect the water tolerance of PU. Thus, it is of great importance to improve PU water resistance effectively. Herein, novel fluoroalkyl-terminated hyperbranched polyurethane (HBPUF) latex was accordingly synthesized by graft reaction of perfluorohexyl ethyl alcohol and hyperbranched polyurethane (HBPU), which was previously obtained from interaction between hydroxyl-terminated hyperbranched polymer and PU prepolymer manufactured via the acetone process, as well as using neutralization, adding water, and high-speed stirring operations. We characterized the resultants and investigated its surface properties by IR, NMR, TEM, XRD, TGA, DSC, FE-SEM, AFM, XPS, and contact angle measurements, etc. IR and NMR tests confirmed that the fluorinated fragments had been grafted onto the tail end of HBPU. TEM, XRD, DSC, and FE-SEM results all accounted for the fact that there were multi-crystals in PU, HBPU and HBPUF. TGA results showed that thermal stabilities of the PU, HBPU, and HBPUF latex films were enhanced in turn. XPS and AFM analyses demonstrated that the fluorine-containing segments from the HBPUF terminals were prone to migrate and enrich on the film-air surface of the HBPUF latex film, which made water contact angle and water absorption of the HBPUF film be as 113.9° and 11.1%, respectively, compared to those of the PU film (77.8° and 136.2%). This research indicates that water resistance of the PU film can be efficiently enhanced by fluorinated polyurethane with novel fluoroalkyl-terminated hyperbranched structure.
Hearon, Keith; Besset, Celine J.; Lonnecker, Alexander T.; Ware, Taylor; Voit, Walter E.; Wilson, Thomas S.; Wooley, Karen L.; Maitland, Duncan J.
2014-01-01
The synthetic design and thermomechanical characterization of shape memory polymers (SMPs) built from a new polyurethane chemistry that enables facile, bulk and tunable cross-linking of low-molecular weight thermoplastics by electron beam irradiation is reported in this study. SMPs exhibit stimuli-induced geometry changes and are being proposed for applications in numerous fields. We have previously reported a polyurethane SMP system that exhibits the complex processing capabilities of thermoplastic polymers and the mechanical robustness and tunability of thermomechanical properties that are often characteristic of thermoset materials. These previously reported polyurethanes suffer practically because the thermoplastic molecular weights needed to achieve target cross-link densities severely limit high-throughput thermoplastic processing and because thermally unstable radiation-sensitizing additives must be used to achieve high enough cross-link densities to enable desired tunable shape memory behavior. In this study, we demonstrate the ability to manipulate cross-link density in low-molecular weight aliphatic thermoplastic polyurethane SMPs (Mw as low as ~1.5 kDa) without radiation-sensitizing additives by incorporating specific structural motifs into the thermoplastic polymer side chains that we hypothesized would significantly enhance susceptibility to e-beam cross-linking. A custom diol monomer was first synthesized and then implemented in the synthesis of neat thermoplastic polyurethane SMPs that were irradiated at doses ranging from 1 to 500 kGy. Dynamic mechanical analysis (DMA) demonstrated rubbery moduli to be tailorable between 0.1 and 55 MPa, and both DMA and sol/gel analysis results provided fundamental insight into our hypothesized mechanism of electron beam cross-linking, which enables controllable bulk cross-linking to be achieved in highly processable, low-molecular weight thermoplastic shape memory polymers without sensitizing additives. PMID:25411511
Experiment evaluation of impact attenuator for a racing car under static load
NASA Astrophysics Data System (ADS)
Imanullah, Fahmi; Ubaidillah, Prasojo, Arfi Singgih; Wirawan, Adhe Aji
2018-02-01
The automotive world is a world where one of the factors that must be considered carefully is the safety aspect. In the formula student car one of the safety factor in the form of impact attenuator. Impact attenuator is used as anchoring when a collision occurs in front of the vehicle. In the rule of formula society of automotive engineer (FSAE) student, impact attenuator is required to absorb the energy must meet or exceed 7350 Joules with a slowdown in speed not exceeding 20 g average and peak of 40 g. The student formula participants are challenged to pass the boundaries so that in designing and making the impact attenuator must pay attention to the strength and use of the minimum material so that it can minimize the expenditure. In this work, an impact attenuator was fabricated and tested using static compression. The primary goal was evaluating the actual capability of the impact attenuator for impact energy absorption. The prototype was made of aluminum alloy in a prismatic shape, and the inside wall was filled with rooftop plastic slices and polyurethane hard foam. The compression test has successfully carried out, and the load versus displacement data could be used in calculating energy absorption capability. The result of the absorbent energy of the selected impact attenuator material. Impact attenuator full polyurethane absorbed energy reach 6380 Joule. For impact attenuator with aluminum polyurethane with a slashed rooftop material as section absorbed energy reach 6600 Joule. Impact attenuator with Aluminum Polyurethane with aluminum orange peel partitions absorbed energy reach 8800 Joule. From standard student formula, energy absorbed in this event must meet or exceed 7350 Joules that meet aluminum polyurethane with aluminum orange peel partitions with the ability to absorb 8800 Joule.
Investigation on the mechanical properties of palm-based flexible polyurethane foam
NASA Astrophysics Data System (ADS)
On, Ahmad Zuhdi Mohd; Badri, Khairiah Haji
2015-09-01
A series of modification polyurethane (PU) system was prepared by introducing palm kernel based polyol (PKO-p) to progressively replaced commercial polyether polyol from petrochemical based material. This paper describes the effect of PKO-p on the physical-mechanical properties of polyurethane foams. Stress-strain analysis in tensile mode was conducted with physicochemical analysis by performing Fourier transform infrared (FTIR). The morphological studies were observed by the optical microscope. The foam showed an increment on the modulus up to 458.3kPa as more incorporation of PKO-p introduced to the system. In contrast, tensile strength of PU foam depicted the highest up to 162 kPa at 60:40. The elongation at break showed decrement as the composition of the renewable polyol increased to a ratio 60/40 of PKO-p to petrochemical based polyol.
NASA Astrophysics Data System (ADS)
Sekkar, Venkataraman; Alex, Ancy Smitha; Kumar, Vijendra; Bandyopadhyay, G. G.
2018-01-01
Polyurethane networks between hydroxyl terminated polybutadiene (HTPB) and butanediol (BD) were prepared using toluene diisocyanate (TDI) as the curative. HTPB and BD were taken at equivalent ratios viz.: 1:0, 1:1, 1:2, 1:4, and 1:8. Crosslink density (CLD) was theoretically calculated using α-model equations developed by Marsh. CLD for the polyurethane networks was experimentally evaluated from equilibrium swell and stress-strain data. Young's modulus and Mooney-Rivlin approaches were adopted to calculate CLD from stress-strain data. Experimentally obtained CLD values were enormously higher than theoretical values especially at higher BD/HTPB equivalent ratios. The difference in the theoretical and experimental values for CLD was explained in terms of local crystallization due to the formation of hard segments and hydrogen bonded interactions.
NASA Astrophysics Data System (ADS)
Bozkurt, Y.; Sahin, A.; Sunulu, A.; Aydogdu, M. O.; Altun, E.; Oktar, F. N.; Ekren, N.; Gunduz, O.
2017-04-01
Polyurethane (PU) is a synthetic polymer that is used for construction of scaffold in tissue engineering applications in order to obtain desirable mechanical, physical and chemical properties like elasticity and durability. Bovine derived hydroxyapatite (BHAp) is a ceramic based natural polymer that is used as the most preferred implant material in orthopedics and dentistry due to their chemically and biologically similarity to the mineral phase found in the human bone structure. PU and bovine derived hydroxyapatite (BHAp) solutions with different concentrations were prepared with dissolving polyurethane and BHAp in Dimethylformamide (DMF) and Tetrahydrofuran (THF) solutions. Blended PU-BHAp solutions in different concentrations were used for electrospinning technique to create nanofiber scaffolds and new biocomposite material together. SEM, FTIR and physical analysis such as viscosity, electrical conductivity, density measurement and tensile strength measurement tests were carried out after production process.
Podsiadlo, Paul; Qin, Ming; Cuddihy, Meghan; Zhu, Jian; Critchley, Kevin; Kheng, Eugene; Kaushik, Amit K; Qi, Ying; Kim, Hyoung-Sug; Noh, Si-Tae; Arruda, Ellen M; Waas, Anthony M; Kotov, Nicholas A
2009-12-15
Multilayered thin films prepared with the layer-by-layer (LBL) assembly technique are typically "brittle" composites, while many applications such as flexible electronics or biomedical devices would greatly benefit from ductile, and tough nanostructured coatings. Here we present the preparation of highly ductile multilayered films via LBL assembly of oppositely charged polyurethanes. Free-standing films were found to be robust, strong, and tough with ultimate strains as high as 680% and toughness of approximately 30 MJ/m(3). These results are at least 2 orders of magnitude greater than most LBL materials presented until today. In addition to enhanced ductility, the films showed first-order biocompatibility with animal and human cells. Multilayered structures incorporating polyurethanes open up a new research avenue into the preparation of multifunctional nanostructured films with great potential in biomedical applications.
Assessment of Multiaxial Mechanical Response of Rigid Polyurethane Foams
NASA Astrophysics Data System (ADS)
Pettarin, Valeria; Fasce, Laura A.; Frontini, Patricia M.
2014-02-01
Multiaxial deformation behavior and failure surface of rigid polyurethane foams were determined using standard experimental facilities. Two commercial foams of different densities were assayed under uniaxial, biaxial, and triaxial stress states. These different stress states were reached in a uniaxial universal testing machine using suitable testing configurations which imply the use of special grips and lateral restricted samples. Actual strains were monitored with a video extensometer. Polyurethane foams exhibited typical isotropic brittle behavior, except under compressive loads where the response turned out to be ductile. A general failure surface in the stress space which accounts for density effects could be successfully generated. All of failure data, determined at the loss of linear elasticity point, collapsed in a single locus defined as the combination of a brittle crushing of closed-cell cellular materials criterion capped by an elastic buckling criterion.
The management of amputations of the leg using a new rigid foam plaster for prosthetic fitting.
Hölter, W; Echterhoff, M; Blömer, A; Verfürden, H
1980-01-01
This paper describes the use of a rigid polyurethane foam to construct a stump socket for immediate or early prosthetic fitting in 15 patients with amputation through the leg. The foam plaster is poured into a prepared cotton sleeve, with a zip incorporated, and rolled out to a layer 4 mm thick. The filled sleeve is put around the stump and the zip closed, moulding the sleeve firmly to the stump. The closed sleeve hardens into a rigid polyurethane shell within 20 min. Aferwards the skeletal prosthetic components are fixed with the same rigid foam. The polyurethane foam socket is quickly and cleanly prepared, only one third of the weight of a plaster of Paris cast and is easily removed by means of the zip, allowing access to the stump.
Kalita, Hemjyoti; Karak, Niranjan
2014-07-01
Here, bio-based shape memory polymers have generated immense interest in recent times. Here, Bio-based hyperbranched polyurethane/triethanolamine functionalized multi-walled carbon nanotube (TEA-f-MWCNT) nanocomposites were prepared by in-situ pre-polymerization technique. The Fourier transform infrared spectroscopy and the transmission electron microscopic studies showed the strong interfacial adhesion and the homogeneous distribution of TEA-f-MWCNT in the polyurethane matrix. The prepared epoxy cured thermosetting nanocomposites exhibited enhanced tensile strength (6.5-34.5 MPa), scratch hardness (3.0-7.5 kg) and thermal stability (241-288 degrees C). The nanocomposites showed excellent shape fixity and shape recovery. The shape recovery time decreases (24-10 s) with the increase of TEA-f-MWCNT content in the nanocomposites. Thus the studied nanocomposites have potential to be used as advanced shape memory materials.
Olsen, Peter C.; Gordon, N. Ross; Simmons, Kevin L.
1993-01-01
The present invention is a material and method of making the material that exhibits improved radiation attenuation simulation of real lungs, i.e., an "authentic lung tissue" or ALT phantom. Specifically, the ALT phantom is a two-part polyurethane medium density foam mixed with calcium carbonate, potassium carbonate if needed for K-40 background, lanthanum nitrate, acetone, and a nitrate or chloride form of a radionuclide. This formulation is found to closely match chemical composition and linear attenuation of real lungs. The ALT phantom material is made according to established procedures but without adding foaming agents or preparing thixotropic concentrate and with a modification for ensuring uniformity of density of the ALT phantom that is necessary for accurate simulation. The modification is that the polyurethane chemicals are mixed at a low temperature prior to pouring the polyurethane mixture into the mold.
Olsen, P.C.; Gordon, N.R.; Simmons, K.L.
1993-11-30
The present invention is a material and method of making the material that exhibits improved radiation attenuation simulation of real lungs, i.e., an ``authentic lung tissue`` or ALT phantom. Specifically, the ALT phantom is a two-part polyurethane medium density foam mixed with calcium carbonate, potassium carbonate if needed for K-40 background, lanthanum nitrate, acetone, and a nitrate or chloride form of a radionuclide. This formulation is found to closely match chemical composition and linear attenuation of real lungs. The ALT phantom material is made according to established procedures but without adding foaming agents or preparing thixotropic concentrate and with a modification for ensuring uniformity of density of the ALT phantom that is necessary for accurate simulation. The modification is that the polyurethane chemicals are mixed at a low temperature prior to pouring the polyurethane mixture into the mold.
The corrosion protection of 6061-T6 aluminum by a polyurethane-sealed anodized coat
NASA Technical Reports Server (NTRS)
Danford, M. D.
1990-01-01
The corrosion protection of 6061-T6 anodized aluminum afforded by a newly patented polyurethane seal was studied using the ac impedance technique. Values of the average corrosion rates over a 27-day exposure period in 3.5 percent NaCl solutions at pH 5.2 and pH 9.5 compared very favorably for Lockheed-prepared polyurethane-sealed and dichromate-sealed coats of the same thickness. Average corrosion rates for both specimens over the first 7 days of exposure compared well with those for a hard anodized, dichromate-sealed coat, but rose well above those for the hard anodized coat over the entire 27-day period. This is attributed both to the greater thickness of the hard anodized coat, and possibly to its inherently better corrosion protective capability.
Polyurethane foams obtained from residues of PET manufacturing and modified with carbon nanotubes
NASA Astrophysics Data System (ADS)
Stiebra, L.; Cabulis, U.; Knite, M.
2016-04-01
In this work we report the preparation of rigid microcellular polyurethane/carbon nanotube nanocomposites with different CNT loadings (0.09-0.46%) and various isocyanate indexes (110-260). Water was used as a blowing agent for samples. Density of all obtained samples - 200 ± 10 kg/m3. Electrical properties, as well as heat conductivity, cellular structure and mechanical properties of these nanocomposites were investigated.
The Shock and Vibration Digest. Volume 18, Number 1
1986-01-01
polyurethanes reduced the loss factor and emphasized the correlation between molecular storage modulus by increasing the length of the structure and...one tempera- static deformations. He gave storage and loss ture/frequency range is difficult with copoly- moduli for a carbon black filled and an...has been described (18). The shear loss author states that the frequency dependence of and storage moduli of a void-filled polyurethane the elastomers
Properties of Multiphase Polyurethane Systems.
1983-07-01
segment - diphenylmethane-diisocyanate/ N - methyldiethanolamine (MDI/ MDEA ). Each polymer was synthesized using a two step reaction technique. The number...OF MULTIPHASE POLYURETHANE SYSTEMS Final Report for Period July 1, 1982-June 30, 1983 Naval Air Systems Command Code 5304 C2 ONavy Contract # N 00019...and COB, UA groups. The existence of 3-dimensional hydrogen bonding (two C-O groups bonded to one N -H group) should shift the COB,UA peak to lower
Development of Encapsulated Dye for Surface Impact Damage Indicator System.
1987-09-01
GROUP SUB-GROUP Composites Ultrasonics Dye Impact Microcapsules 11 04 NDE polyurethane 11 1 0Encapsulation Paint 19. ABSTRACT (Continue on reverse if...encapsulation, microencapsule incorporation into the USAF polyurethane paint, dnd initial correlation study of impact damage to impact coating indication. It is...project were to: 1. Refine the microcapsule formulation to be compatible with MIL-C-83286 paint. 2. Fabricate composite panels from isotropic graphite
Jiulong Xie; Jinqiu Qi; Chung-Yun Hse; Todd F. Shupe
2014-01-01
Bamboo residues were subjected to a microwave-assisted liquefaction process for the production of crude bio-polyols (CBP). The fractionated bio-polyols (FBP) were obtained by the removal of lignin derivatives from the crude bio-polyols (CBP) using a simple method. Polyurethane (PU) foams were successfully prepared from both CBP and FBP. The object of this study was to...
Rigid Polyurethane Foam (RPF) Technology for Countermine (SEA) Program - Phase 1
1997-01-01
Form ApprovedOMB No. 0704-0188 Public reporting burden for the collection of information is estimated to average 1 hour...05 MAY 1997 2. REPORT TYPE 3. DATES COVERED 00-00-1997 to 00-00-1997 4. TITLE AND SUBTITLE Rigid Polyurethane Foam (RPF) Technology for...unclassified b. ABSTRACT unclassified c. THIS PAGE unclassified Standard Form 298 (Rev. 8-98) Prescribed by ANSI Std Z39-18
Structures and Properties of Polyurethanes. Part II,
1979-03-23
effect was observed for polymethyl methacrylate (222, 2721. The polyol, which contain fluorine , decrease adhesion, in spite DOC = 79011112 PAGE S4% of...small differences in the hardness of films on the basis of the fluorine -bearing polyol and generally accepted polyol. Is investigated the etfect ot...polyurethane, to rigid surface. DOC 79011112 P A * S The effect of the solvent, utilized for obtaining the varnish , on adhesion is investigated in
Preparation of linear hydroxy substituted polyphosphazenes. [flame retardant polyurethane foam
NASA Technical Reports Server (NTRS)
Paciorek, K. L.; Ito, T. I.; Kratzer, R. H.
1978-01-01
The synthesis of partially hydroxy-substituted phosphazene prepolymers amenable to processing into cellular, flexible polyurethane foams was investigated. Factors determined include (1) the environment of the hydroxyl group; (2) the ease of the hexachlorocyclotriphosphazene polymerization; (3) the nature of the nonreactive substituents; and (4) the mode of introduction of the hydroxyl entity. The specific approaches taken, the rationale of the selections made, and the results are discussed.
Polyurethane retainers for ball bearings
NASA Technical Reports Server (NTRS)
Christy, R. I.
1973-01-01
Evaluation of a new ball bearing retainer material is reported. A special composite polyurethane foam ball retainer has been developed that has virtually zero wear, is chemically inert to hydrocarbon lubricants, and stores up to 60 times as much lubricant per unit volume as the most commonly used retainer material, cotton phenolic. This new retainer concept shows promise of years of ball bearing operation without reoiling, based on life testing in high vacuum.
Physical and chemical evaluation of furniture waste briquettes.
Moreno, Ana Isabel; Font, Rafael; Conesa, Juan A
2016-03-01
Furniture waste is mainly composed of wood and upholstery foam (mostly polyurethane foam). Both of these have a high calorific value, therefore, energy recovery would be an appropriate process to manage these wastes. Nevertheless, the drawback is that the energy content of these wastes is limited due to their low density mainly that of upholstery foam. Densification of separate foam presents difficulties due to its elastic character. The significance of this work lies in obtaining densified material by co-densification of furniture wood waste and polyurethane foam waste. Densification of furniture wood and the co-densification of furniture wood waste with polyurethane foam have been studied. On the one hand, the parameters that have an effect on the quality of the furniture waste briquettes have been analysed, i.e., moisture content, compaction pressure, presence of lignin, etc. The maximum weight percentage of polyurethane foam that can be added with furniture wood waste to obtain durable briquettes and the optimal moisture were determined. On the other hand, some parameters were analysed in order to evaluate the possible effect on the combustion. The chemical composition of waste wood was compared with untreated wood biomass; the higher nitrogen content and the concentration of some metals were the most important differences, with a significant difference of Ti content. Copyright © 2016 Elsevier Ltd. All rights reserved.
Martin del Campo, Martha; Camacho, Rosa M; Mateos-Díaz, Juan C; Müller-Santos, Marcelo; Córdova, Jesus; Rodríguez, Jorge A
2015-11-01
Halophilic archaea are extremophiles, adapted to high-salt environments, showing a big biotechnological potential as enzyme, lipids and pigments producers. Four inert supports (perlite, vermiculite, polyurethane foam and glass fiber) were employed for solid-state fermentation (SSF) of the halophilic archaeon Natronococcus sp. TC6 to investigate biomass and esterase production. A very low esterase activity and high water activity were observed when perlite, vermiculite and polyurethane were used as supports. When glass fiber was employed, an important moisture loss was observed (8.6%). Moreover, moisture retention was improved by mixing polyurethane and glass fiber, resulting in maximal biomass and esterase production. Three halophilic archaea: Natronococcus sp. TC6, Halobacterium sp. NRC-1 and Haloarcula marismortui were cultured by submerged fermentation (SmF) and by SSF; an improvement of 1.3- to 6.2-fold was observed in the biomass and esterase production when SSF was used. Growth was not homogeneous in the mixture, but was predominant in the glass fiber thus was probably because the glass fiber provides a holder to the cells, while the polyurethane acts as an impregnation medium reservoir. To the best of our knowledge, this work is the first report on haloarchaea cultivation by SSF aiming biomass and esterase/lipase activity production.
Novel Poly(3-hydroxybutyrate-g-vinyl alcohol) Polyurethane Scaffold for Tissue Engineering
NASA Astrophysics Data System (ADS)
Reyes, Adriana Pétriz; Martínez Torres, Ataúlfo; Carreón Castro, Ma. Del Pilar; Rodríguez Talavera, José Rogelio; Muñoz, Susana Vargas; Aguilar, Víctor Manuel Velázquez; Torres, Maykel González
2016-08-01
The design of new synthetic grafted poly(3-hydroxybutyrate) as composite 3D-scaffolds is a convenient alternative for tissue engineering applications. The chemically modified poly(3-hydroxybutyrate) is receiving increasing attention for use as biomimetic copolymers for cell growth. As of yet, these copolymers cannot be used efficiently because of the lack of good mechanical properties. Here, we address this challenge, preparing a composite-scaffold of grafted poly(3-hydroxybutyrate) polyurethane for the first time. However, it is unclear if the composite structure and morphology can also offer a biological application. We obtained the polyurethane by mixing a polyester hydroxylated resin with polyisocyanate and the modified polyhydroxyalkanoates. The results show that the poly(3-hydroxybutyrate) grafted with poly(vinyl alcohol) can be successfully used as a chain extender to form a chemically-crosslinked thermosetting polymer. Furthermore, we show a proposal for the mechanism of the polyurethane synthesis, the analysis of its morphology and the ability of the scaffolds for growing mammalian cells. We demonstrated that astrocytes isolated from mouse cerebellum, and HEK293 can be cultured in the prepared material, and express efficiently fluorescent proteins by adenoviral transduction. We also tested the metabolism of Ca2+ to obtain evidence of the biological activity.