Sample records for quality steel products

  1. 76 FR 34101 - Hot-Rolled Flat-Rolled Carbon-Quality Steel Products From Brazil, Japan, and Russia

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-06-10

    ...] Hot-Rolled Flat-Rolled Carbon-Quality Steel Products From Brazil, Japan, and Russia Determinations On...-quality steel products from Russia would be likely to lead to continuation or recurrence of material...) entitled Hot-Rolled Flat-Rolled Carbon-Quality Steel Products from Brazil, Japan, and Russia: Investigation...

  2. 76 FR 22868 - Certain Hot-Rolled Flat-Rolled Carbon-Quality Steel Products From Brazil: Final Results of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-04-25

    ...-Rolled Carbon-Quality Steel Products From Brazil: Final Results of Countervailing Duty Administrative... administrative review of the countervailing duty order on certain hot-rolled flat-rolled carbon- quality steel...-Quality Steel Products From Brazil: Preliminary Results of Countervailing Duty Administrative Review, 75...

  3. 75 FR 19369 - Certain Hot-Rolled Flat-Rolled Carbon Quality Steel Products from Brazil: Preliminary Results of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-04-14

    ...-Rolled Carbon Quality Steel Products from Brazil: Preliminary Results of Antidumping Duty Administrative... duty order on certain hot-rolled flat-rolled carbon quality steel products (hot-rolled steel) from... 1, 2008, through February 28, 2009. We preliminarily determine that the sale of hot-rolled steel...

  4. 75 FR 64246 - Certain Hot-Rolled Flat-Rolled Carbon-Quality Steel Products From Brazil: Correction to Notice of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-10-19

    ...-Rolled Carbon-Quality Steel Products From Brazil: Correction to Notice of Antidumping Duty Order AGENCY... certain hot-rolled flat-rolled carbon-quality steel products from Brazil. See Antidumping Duty Order: Certain Hot-Rolled Flat-Rolled Carbon-Quality Steel Products From Brazil, 67 FR 11093 (March 12, 2002...

  5. 75 FR 75455 - Certain Hot-Rolled Flat-Rolled Carbon-Quality Steel Products From Brazil: Final Results of Full...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-12-03

    ...-Rolled Carbon-Quality Steel Products From Brazil: Final Results of Full Sunset Review of Countervailing... of the countervailing duty (CVD) order on certain hot-rolled flat-rolled carbon-quality steel products (hot-rolled steel) from Brazil, pursuant to section 751(c) of the Tariff Act of 1930, as amended...

  6. 77 FR 2032 - Certain Cut-to-Length Carbon-Quality Steel Plate Products From the Republic of Korea: Preliminary...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-01-13

    ...-Quality Steel Plate Products From the Republic of Korea: Preliminary Results of Antidumping Duty... steel plate products (steel plate) from the Republic of Korea (Korea). This review covers one producer... Federal Register an antidumping duty order on steel plate from Korea. See Notice of Amendment of Final...

  7. 75 FR 29976 - Certain Cut-to-Length Carbon-Quality Steel Plate Products From Italy: Extension of the Final...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-05-28

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-475-826] Certain Cut-to-Length Carbon... preliminary results of the administrative review of the antidumping duty order on certain cut-to-length carbon-quality steel plate products from Italy. See Certain Cut-to-Length Carbon-Quality Steel Plate Products...

  8. 78 FR 29113 - Certain Cut-to-Length Carbon-Quality Steel Plate Products From the Republic of Korea: Final...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-05-17

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-836] Certain Cut-to-Length Carbon... administrative review of the antidumping duty order on certain cut-to-length carbon-quality steel plate products... duty order on certain cut-to-length carbon-quality steel plate products from the Republic of Korea...

  9. 75 FR 62566 - Hot-Rolled Flat-Rolled Carbon-Quality Steel Products From Brazil, Japan, and Russia

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-10-12

    ...)] Hot-Rolled Flat-Rolled Carbon-Quality Steel Products From Brazil, Japan, and Russia AGENCY: United... antidumping duty investigation on hot-rolled steel from Russia. SUMMARY: The Commission hereby gives notice of... suspended investigation on hot-rolled steel from Russia would be likely to lead to continuation or...

  10. 75 FR 16504 - Hot-Rolled Flat-Rolled Carbon-Quality Steel Products From Brazil, Japan, and Russia

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-04-01

    ...)] Hot-Rolled Flat-Rolled Carbon-Quality Steel Products From Brazil, Japan, and Russia AGENCY: United... investigation on hot-rolled steel from Russia. SUMMARY: The Commission hereby gives notice that it has...-rolled steel from Russia would be likely to lead to continuation or recurrence of material injury...

  11. 75 FR 42782 - Hot-Rolled Flat-Rolled Carbon-Quality Steel Products From Brazil, Japan, and Russia

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-07-22

    ...)] Hot-Rolled Flat-Rolled Carbon-Quality Steel Products From Brazil, Japan, and Russia AGENCY: United... Brazil and Japan, and the suspended investigation on hot-rolled steel from Russia. SUMMARY: The... Japan, and the suspended investigation on hot-rolled steel from Russia would be likely to lead to...

  12. Production of High Quality Die Steels from Large ESR Slab Ingots

    NASA Astrophysics Data System (ADS)

    Geng, Xin; Jiang, Zhou-hua; Li, Hua-bing; Liu, Fu-bin; Li, Xing

    With the rapid development of manufacture industry in China, die steels are in great need of large slab ingot of high quality and large tonnage, such as P20, WSM718R and so on. Solidification structure and size of large slab ingots produced with conventional methods are not satisfied. However, large slab ingots manufactured by ESR process have a good solidification structure and enough section size. In the present research, the new slab ESR process was used to produce the die steels large slab ingots with the maximum size of 980×2000×3200mm. The compact and sound ingot can be manufactured by the slab ESR process. The ultra-heavy plates with the maximum thickness of 410 mm can be obtained after rolling the 49 tons ingots. Due to reducing the cogging and forging process, the ESR for large slab ingots process can increase greatly the yield and production efficiency, and evidently cut off product costs.

  13. 75 FR 4779 - Certain Cut-to-Length Carbon-Quality Steel Plate Products From Italy: Preliminary Results of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-01-29

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-475-826] Certain Cut-to-Length Carbon... administrative review of the antidumping duty order on certain cut-to-length carbon- quality steel plate products... Department published in the Federal Register an antidumping duty order on certain cut-to-length carbon...

  14. 75 FR 47777 - Certain Cut-to-Length Carbon-Quality Steel Plate Products From Italy: Final Results of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-08-09

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-475-826] Certain Cut-to-Length Carbon... administrative review of the antidumping duty order on certain cut-to-length carbon-quality steel plate products... the preliminary results of the administrative review of the antidumping duty order on certain cut-to...

  15. 75 FR 32160 - Certain Hot-Rolled Flat-Rolled Carbon-Quality Steel Products from Brazil: Extension of Time Limit...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-06-07

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-351-829] Certain Hot-Rolled Flat... Commerce (the Department) published the countervailing duty order on certain hot-rolled flat- rolled carbon-quality steel products from Brazil. See Agreement Suspending the Countervailing Duty Investigation on Hot...

  16. 75 FR 77828 - Certain Hot-Rolled Flat-Rolled Carbon-Quality Steel Products From Brazil: Extension of Time Limit...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-12-14

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-351-829] Certain Hot-Rolled Flat-Rolled Carbon-Quality Steel Products From Brazil: Extension of Time Limit for Final Results of Countervailing Duty Administrative Review AGENCY: Import Administration, International Trade Administration, Department of Commerce DATES: Effective Date:...

  17. Utilization of steel slag for Portland cement clinker production.

    PubMed

    Tsakiridis, P E; Papadimitriou, G D; Tsivilis, S; Koroneos, C

    2008-04-01

    The aim of the present research work is to investigate the possibility of adding steel slag, a by-product of the conversion of iron to steel process, in the raw meal for the production of Portland cement clinker. Two samples of raw meals were prepared, one with ordinary raw materials, as a reference sample ((PC)(Ref)), and another with 10.5% steel slag ((PC)(S/S)). Both raw meals were sintered at 1450 degrees C. The results of chemical and mineralogical analyses as well as the microscopic examination showed that the use of the steel slag did not affect the mineralogical characteristics of the so produced Portland cement clinker. Furthermore, both clinkers were tested by determining the grindability, setting times, compressive strengths and soundness. The hydration products were examined by XRD analysis at 2, 7, 28 and 90 days. The results of the physico-mechanical tests showed that the addition of the steel slag did not negatively affect the quality of the produced cement.

  18. 78 FR 4385 - Certain Cut-to-Length Carbon-Quality Steel Plate Products From the Republic of Korea: Preliminary...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-01-22

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-836] Certain Cut-to-Length Carbon... the antidumping duty order on certain cut-to- length carbon-quality steel plate products (CTL plate... Decision Memorandum for the Administrative Review of the Antidumping Duty Order on Certain Cut-to- Length...

  19. Products of steel slags an opportunity to save natural resources.

    PubMed

    Motz, H; Geiseler, J

    2001-01-01

    already accepted as a CEN standard and are used for a continuous quality control. Usually the suitability of steel slags is stated by fulfilling the requirements of national and/or international standards and regulations. Based on these standards and regulations in Germany in 1998 about 97% of the produced steel slags have been used as aggregates for road construction (e.g. as surface layer, road base and sub base for high trafficked roads), ways, earthworks, and armourstones for hydraulic structures. Consistent to the successful long-term experience not only products of steel slags but also products of blast furnace slags have been eliminated from the European Waste Catalogue and the European Shipment of Waste Regulation of the European Community, as well as from the lists of OECD for transfrontier movements by the decision of the OECD-Council from 21 September, 1995.

  20. Statistical Methods for Quality Control of Steel Coils Manufacturing Process using Generalized Linear Models

    NASA Astrophysics Data System (ADS)

    García-Díaz, J. Carlos

    2009-11-01

    Fault detection and diagnosis is an important problem in process engineering. Process equipments are subject to malfunctions during operation. Galvanized steel is a value added product, furnishing effective performance by combining the corrosion resistance of zinc with the strength and formability of steel. Fault detection and diagnosis is an important problem in continuous hot dip galvanizing and the increasingly stringent quality requirements in automotive industry has also demanded ongoing efforts in process control to make the process more robust. When faults occur, they change the relationship among these observed variables. This work compares different statistical regression models proposed in the literature for estimating the quality of galvanized steel coils on the basis of short time histories. Data for 26 batches were available. Five variables were selected for monitoring the process: the steel strip velocity, four bath temperatures and bath level. The entire data consisting of 48 galvanized steel coils was divided into sets. The first training data set was 25 conforming coils and the second data set was 23 nonconforming coils. Logistic regression is a modeling tool in which the dependent variable is categorical. In most applications, the dependent variable is binary. The results show that the logistic generalized linear models do provide good estimates of quality coils and can be useful for quality control in manufacturing process.

  1. Semen quality and sex hormones among mild steel and stainless steel welders: a cross sectional study.

    PubMed Central

    Bonde, J P

    1990-01-01

    Welding may be detrimental to the male reproductive system. To test this hypothesis, semen quality was examined in 35 stainless steel welders, 46 mild steel welders, and 54 non-welding metal workers and electricians. These figures represent a participation rate of 37.1% in welders and 36.7% in non-welding subjects. The mean exposure to welding fume particulates was 1.3 mg/m3 (SD 0.8) in stainless steel welders using tungsten inert gas, 3.2 mg/m3 (SD 1.0) in low exposed mild steel welders using manual metal arc or metal active gas (n = 31), and 4.7 mg/m3 (SD 2.1) in high exposed mild steel welders (n = 15). The semen quality of each participant was defined in terms of the mean values of the particular semen parameters in three semen samples delivered at monthly intervals in a period with occupational exposure in a steady state. The sperm concentration was not reduced in either mild steel or stainless steel welders. The sperm count per ejaculate, the proportion of normal sperm forms, the degree of sperm motility, and the linear penetration rate of the sperm were significantly decreased and the sperm concentration of follicle stimulating hormone (FSH) was non-significantly increased in mild steel welders. A dose response relation between exposure to welding fumes and these semen parameters (sperm count excepted) was found. Semen quality decreased and FSH concentrations increased with increasing exposure. Significant deteriorations in some semen parameters were also observed in stainless steel welders. An analysis of information from questionnaires obtained from the whole population including subjects who declined to participate indicated an underestimation of effects due to selection bias. Potential confounding was treated by restriction and statistical analysis. The results support the hypothesis that mild steel welding and to a lesser extent stainless steel welding with tungsten inert gas is associated with reduced semen quality at exposure in the range of the

  2. Semen quality and sex hormones among mild steel and stainless steel welders: a cross sectional study.

    PubMed

    Bonde, J P

    1990-08-01

    Welding may be detrimental to the male reproductive system. To test this hypothesis, semen quality was examined in 35 stainless steel welders, 46 mild steel welders, and 54 non-welding metal workers and electricians. These figures represent a participation rate of 37.1% in welders and 36.7% in non-welding subjects. The mean exposure to welding fume particulates was 1.3 mg/m3 (SD 0.8) in stainless steel welders using tungsten inert gas, 3.2 mg/m3 (SD 1.0) in low exposed mild steel welders using manual metal arc or metal active gas (n = 31), and 4.7 mg/m3 (SD 2.1) in high exposed mild steel welders (n = 15). The semen quality of each participant was defined in terms of the mean values of the particular semen parameters in three semen samples delivered at monthly intervals in a period with occupational exposure in a steady state. The sperm concentration was not reduced in either mild steel or stainless steel welders. The sperm count per ejaculate, the proportion of normal sperm forms, the degree of sperm motility, and the linear penetration rate of the sperm were significantly decreased and the sperm concentration of follicle stimulating hormone (FSH) was non-significantly increased in mild steel welders. A dose response relation between exposure to welding fumes and these semen parameters (sperm count excepted) was found. Semen quality decreased and FSH concentrations increased with increasing exposure. Significant deteriorations in some semen parameters were also observed in stainless steel welders. An analysis of information from questionnaires obtained from the whole population including subjects who declined to participate indicated an underestimation of effects due to selection bias. Potential confounding was treated by restriction and statistical analysis. The results support the hypothesis that mild steel welding and to a lesser extent stainless steel welding with tungsten inert gas is associated with reduced semen quality at exposure in the range of the

  3. Challenges in Special Steel Making

    NASA Astrophysics Data System (ADS)

    Balachandran, G.

    2018-02-01

    Special bar quality [SBQ] is a long steel product where an assured quality is delivered by the steel mill to its customer. The bars have enhanced tolerance to higher stress application and it is demanded for specialised component making. The SBQ bars are sought for component making processing units such as closed die hot forging, hot extrusion, cold forging, machining, heat treatment, welding operations. The final component quality of the secondary processing units depends on the quality maintained at the steel maker end along with quality maintained at the fabricator end. Thus, quality control is ensured at every unit process stages. The various market segments catered to by SBQ steel segment is ever growing and is reviewed. Steel mills need adequate infrastructure and technological capability to make these higher quality steels. Some of the critical stages of processing SBQ and the critical quality maintenance parameters at the steel mill in the manufacture has been brought out.

  4. A Goal Programming Optimization Model for The Allocation of Liquid Steel Production

    NASA Astrophysics Data System (ADS)

    Hapsari, S. N.; Rosyidi, C. N.

    2018-03-01

    This research was conducted in one of the largest steel companies in Indonesia which has several production units and produces a wide range of steel products. One of the important products in the company is billet steel. The company has four Electric Arc Furnace (EAF) which produces liquid steel which must be procesed further to be billet steel. The billet steel plant needs to make their production process more efficient to increase the productvity. The management has four goals to be achieved and hence the optimal allocation of the liquid steel production is needed to achieve those goals. In this paper, a goal programming optimization model is developed to determine optimal allocation of liquid steel production in each EAF, to satisfy demand in 3 periods and the company goals, namely maximizing the volume of production, minimizing the cost of raw materials, minimizing maintenance costs, maximizing sales revenues, and maximizing production capacity. From the results of optimization, only maximizing production capacity goal can not achieve the target. However, the model developed in this papare can optimally allocate liquid steel so the allocation of production does not exceed the maximum capacity of the machine work hours and maximum production capacity.

  5. 19 CFR 12.145 - Entry or admission of certain steel products.

    Code of Federal Regulations, 2013 CFR

    2013-04-01

    ... 19 Customs Duties 1 2013-04-01 2013-04-01 false Entry or admission of certain steel products. 12...; DEPARTMENT OF THE TREASURY SPECIAL CLASSES OF MERCHANDISE Steel Products § 12.145 Entry or admission of certain steel products. In any case in which a steel import license number is required to be obtained...

  6. 19 CFR 12.145 - Entry or admission of certain steel products.

    Code of Federal Regulations, 2014 CFR

    2014-04-01

    ... 19 Customs Duties 1 2014-04-01 2014-04-01 false Entry or admission of certain steel products. 12...; DEPARTMENT OF THE TREASURY SPECIAL CLASSES OF MERCHANDISE Steel Products § 12.145 Entry or admission of certain steel products. In any case in which a steel import license number is required to be obtained...

  7. 19 CFR 12.145 - Entry or admission of certain steel products.

    Code of Federal Regulations, 2012 CFR

    2012-04-01

    ... 19 Customs Duties 1 2012-04-01 2012-04-01 false Entry or admission of certain steel products. 12...; DEPARTMENT OF THE TREASURY SPECIAL CLASSES OF MERCHANDISE Steel Products § 12.145 Entry or admission of certain steel products. In any case in which a steel import license number is required to be obtained...

  8. 19 CFR 12.145 - Entry or admission of certain steel products.

    Code of Federal Regulations, 2011 CFR

    2011-04-01

    ... 19 Customs Duties 1 2011-04-01 2011-04-01 false Entry or admission of certain steel products. 12...; DEPARTMENT OF THE TREASURY SPECIAL CLASSES OF MERCHANDISE Steel Products § 12.145 Entry or admission of certain steel products. In any case in which a steel import license number is required to be obtained...

  9. 19 CFR 12.145 - Entry or admission of certain steel products.

    Code of Federal Regulations, 2010 CFR

    2010-04-01

    ... 19 Customs Duties 1 2010-04-01 2010-04-01 false Entry or admission of certain steel products. 12...; DEPARTMENT OF THE TREASURY SPECIAL CLASSES OF MERCHANDISE Steel Products § 12.145 Entry or admission of certain steel products. In any case in which a steel import license number is required to be obtained...

  10. Regional distribution and losses of end-of-life steel throughout multiple product life cycles-Insights from the global multiregional MaTrace model.

    PubMed

    Pauliuk, Stefan; Kondo, Yasushi; Nakamura, Shinichiro; Nakajima, Kenichi

    2017-01-01

    Substantial amounts of post-consumer scrap are exported to other regions or lost during recovery and remelting, and both export and losses pose a constraint to desires for having regionally closed material cycles. To quantify the challenges and trade-offs associated with closed-loop metal recycling, we looked at the material cycles from the perspective of a single material unit and trace a unit of material through several product life cycles. Focusing on steel, we used current process parameters, loss rates, and trade patterns of the steel cycle to study how steel that was originally contained in high quality applications such as machinery or vehicles with stringent purity requirements gets subsequently distributed across different regions and product groups such as building and construction with less stringent purity requirements. We applied MaTrace Global, a supply-driven multiregional model of steel flows coupled to a dynamic stock model of steel use. We found that, depending on region and product group, up to 95% of the steel consumed today will leave the use phase of that region until 2100, and that up to 50% can get lost in obsolete stocks, landfills, or slag piles until 2100. The high losses resulting from business-as-usual scrap recovery and recycling can be reduced, both by diverting postconsumer scrap into long-lived applications such as buildings and by improving the recovery rates in the waste management and remelting industries. Because the lifetimes of high-quality (cold-rolled) steel applications are shorter and remelting occurs more often than for buildings and infrastructure, we found and quantified a tradeoff between low losses and high-quality applications in the steel cycle. Furthermore, we found that with current trade patterns, reduced overall losses will lead to higher fractions of secondary steel being exported to other regions. Current loss rates, product lifetimes, and trade patterns impede the closure of the steel cycle.

  11. 77 FR 64468 - Circular Welded Carbon-Quality Steel Pipe From India: Final Affirmative Countervailing Duty...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-10-22

    ...-Quality Steel Pipe From India: Final Affirmative Countervailing Duty Determination AGENCY: Import... exporters of circular welded carbon-quality steel pipe (``circular welded pipe'') from India. For... determination.\\1\\ \\1\\ See Circular Welded Carbon-Quality Steel Pipe From India: Preliminary Affirmative...

  12. Production of Green Steel from Red Mud: A Novel Concept

    NASA Astrophysics Data System (ADS)

    Bhoi, Bhagyadhar; Behera, Pravas Ranjan; Mishra, Chitta Ranjan

    Red mud of Indian origin contains around 55% plus of Fe2O3 and is considered as a hazardous waste for the alumina industry. For production of one tone of alumina employing the Bayer's Process, around two tones of red mud is generated from three tones of Bauxite. Conventional process of steel making is not devoid of environmental pollution. In the present investigation, efforts have been made to produce steel from red mud by adopting reduction roasting, magnetic separation and hydrogen plasma smelting route. Magnetic fraction, containing enriched iron oxide and minimal content of alumina, is produced following the first two stages which is then subjected to hydrogen plasma smelting process for production of steel. This novel concept follows a green path way for production of steel free from pollution and is termed as green steel. Further, the only by-product that is produced in the process, is water, which is eco-friendly and recyclable.

  13. 75 FR 1031 - Certain Hot-Rolled Carbon Steel Flat Products from India: Notice of Preliminary Results of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-01-08

    ... measuring at least 10 times the thickness. Universal mill plate (i.e., flat-rolled products rolled on four... determinations. If the Department chooses as facts available a calculated dumping margin from the investigation... questionnaire. See Certain Cut-to-Length Carbon-Quality Steel Plate Products from the Republic of Korea: Final...

  14. 77 FR 36256 - Circular Welded Carbon-Quality Steel Pipe From India: Postponement of Final Determination of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-06-18

    ...-Quality Steel Pipe From India: Postponement of Final Determination of Antidumping Duty Investigation...- quality steel pipe from India.\\1\\ On June 1, 2012, the Department published its preliminary determination... is currently due on August 6, 2012. \\1\\ See Circular Welded Carbon-Quality Steel Pipe from India, the...

  15. 78 FR 5170 - Circular Welded Carbon Quality Steel Pipe From the People's Republic of China: Rescission of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-01-24

    ... Steel Tube Manufacturing Co., Ltd., Huludao City Steel Pipe Industrial, Jiangsu Changbao Steel Tube Co... Quality Steel Pipe From the People's Republic of China: Rescission of Antidumping Duty Administrative... of the antidumping duty order on circular welded carbon quality steel pipe from the People's Republic...

  16. Assessment of air quality in and around a steel industry with direct reduction iron route.

    PubMed

    Jena, Pradip K; Behera, Dillip K; Mishra, C S K; Mohanty, Saswat K

    2011-10-01

    The coal based Direct Reduced Iron (DRI) route for secondary steel production is now a preferred choice in India. Steel making is invariably associated with emission of air pollutants into the environment. Air quality monitoring was carried out in Winter, Summer and Rainy seasons of 2008 in eight monitoring stations in the work zone and five stations in the residential zone of an Integrated Steel Industry located in Orissa state, India. Four air quality parameters i.e. SPM, RSPM, SO2 and NO2 were monitored. Mean SPM and RSPM values were found to be significantly high (p < 0.01) at stations nearer to source in both work zone and residential zone .The highest average SPM and RSPM values in the work zone recorded were 4869 microg/m3 and 1420 microg/m3 and in the residential zone 294 microg/m3 and 198 microg/m3 respectively. No significant difference in the SO2 and NO2 levels was observed between the work and residential zones. In general, the values of air pollutants were highest in Winter followed by Summer and Rainy season. SPM and RSPM values exceeded the National Air Quality Standards (NAAQS) in both the residential and work zones.

  17. 78 FR 31577 - Diffusion-Annealed, Nickel-Plated Flat-Rolled Steel Products From Japan

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-05-24

    ..., Nickel-Plated Flat-Rolled Steel Products From Japan Determination On the basis of the record \\1... imports from Japan of diffusion-annealed, nickel-plated flat-rolled steel products, provided for primarily... flat-rolled steel products from Japan. Accordingly, effective March 27, 2013, the Commission instituted...

  18. 77 FR 21527 - Certain Cut-to-Length Carbon-Quality Steel Plate Products From the Republic of Korea: Final...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-04-10

    ... in coils) and without patterns in relief), of iron or non-alloy quality steel; and (2) flat-rolled... rectangular or non-rectangular cross section where such non-rectangular cross-section is achieved subsequent... characteristics that are painted, varnished, or coated with plastic or other non-metallic substances are included...

  19. 78 FR 9676 - Circular Welded Carbon Quality Steel Pipe From the People's Republic of China: Rescission of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-02-11

    ... Tube Manufacturing Co., Ltd.; Huludao City Steel Pipe Industrial; Jiangsu Changbao Steel Tube Co., Ltd... Quality Steel Pipe From the People's Republic of China: Rescission of Countervailing Duty Administrative... countervailing duty order on circular welded carbon quality steel pipe from the People's Republic of China (``PRC...

  20. 77 FR 65712 - Circular Welded Carbon-Quality Steel Pipe From Vietnam; Termination of Investigation

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-10-30

    ... INTERNATIONAL TRADE COMMISSION [Investigation No. 701-TA-485 (Final)] Circular Welded Carbon-Quality Steel Pipe From Vietnam; Termination of Investigation AGENCY: United States International Trade... carbon-quality steel pipe from Vietnam (investigation No. 701-TA-485 (Final)) is terminated. DATES...

  1. Survey and comparison of sleep quality among fixed and changing shift staff in a steel factory in Tehran, Iran.

    PubMed

    Mohammadian, Farugh; Abbasinia, Marzieh; Rahmani, Abdolrasoul; Monazzam, Mohammad Reza; Asghari, Mehdi; Ahmadnezhad, Iman; Asadi, Ali

    2013-01-01

    Given the hazardous nature of the work in steel factories and that the staff has to deal with hazardous equipment and machines, improper sleep quality and drowsiness among the works tackles performance and boosts rate of job accidents. This study is aimed to survey the quality of sleep and sleepiness status and the pertinent factors among the workers in a rolling mill and a steel production company in Tehran, Iran. In a Cross-Sectional study 2011, 180 workers were selected randomly from a rolling mill and a steel production company in Tehran. A questionnaire was designed to collect demographic data and variables of work condition. Pitersborg's sleep quality questionnaire was used to survey quality and problems of Participants' sleep. Epworth Sleepiness questionnaire was used to deals with sleepiness during work, studying, watching TV, or during time spent in public. Average score of sleep quality for the fixed shift staff and changing shift staff were 7.5±2.82 and 8.49±2.95 respectively. Surveys of sleep quality for the two groups of the participants based on T-test showed a significant difference between the two groups so that the changing shift staff group suffered poorer sleep quality (p=0.03). Comparison of average drowsiness scores between the two groups of participants based on Mann-Whitney test showed no significant difference (p>0.005). Chi square test showed a significant difference between severity of drowsiness and type of working shift (p =0.028 and 0.009). Staff in revolving shifts suffers poor sleep quality comparing with staff with fixed working shift. Moreover, type of working shift greatly affects severity of drowsiness as staff at different work shift experienced different level of sleepiness. It is essential to survey sleep disorder of the staff in the industry and pay more emphasis on sleep disorder epidemic in other fields of industry.

  2. 78 FR 23905 - Diffusion-Annealed, Nickel-Plated Flat-Rolled Steel Products From Japan: Initiation of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-04-23

    ...-Plated Flat-Rolled Steel Products From Japan: Initiation of Antidumping Duty Investigation AGENCY: Import... products from Japan (``certain nickel-plated, flat-rolled steel''), filed in proper form by Thomas Steel... Antidumping Duty Petition on Diffusion-Annealed, Nickel- Plated Steel Flat-Rolled Products from Japan, dated...

  3. 30. LOOKING SOUTHEAST AT THE CLEAN STEEL PRODUCTION BUILDING WITH ...

    Library of Congress Historic Buildings Survey, Historic Engineering Record, Historic Landscapes Survey

    30. LOOKING SOUTHEAST AT THE CLEAN STEEL PRODUCTION BUILDING WITH THE BOP SHOP IN BACKGROUND. - U.S. Steel Duquesne Works, Basic Oxygen Steelmaking Plant, Along Monongahela River, Duquesne, Allegheny County, PA

  4. 49 CFR 661.6 - Certification requirements for procurement of steel or manufactured products.

    Code of Federal Regulations, 2010 CFR

    2010-10-01

    ... § 661.6 Certification requirements for procurement of steel or manufactured products. If steel, iron, or... 49 Transportation 7 2010-10-01 2010-10-01 false Certification requirements for procurement of steel or manufactured products. 661.6 Section 661.6 Transportation Other Regulations Relating to...

  5. 76 FR 76944 - Circular Welded Carbon Quality Steel Pipe From the People's Republic of China: Rescission of the...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-12-09

    ... Zhongyuan Steel Pipe Manufacturer (``Hebei Zhongyuan''), Hefei Zijin Steel Tube Manufacturing Co., Ltd... Quality Steel Pipe From the People's Republic of China: Rescission of the 2010-2011 Antidumping Duty... antidumping duty order on circular welded carbon quality steel pipe (``CWP'') from the People's Republic of...

  6. 78 FR 15376 - Determinations: Corrosion-Resistant Carbon Steel Flat Products From Germany and Korea

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-03-11

    ...)] Determinations: Corrosion-Resistant Carbon Steel Flat Products From Germany and Korea On the basis of the record... revocation of the countervailing duty order on corrosion-resistant carbon steel flat products from Korea and the antidumping duty orders on corrosion-resistant carbon steel flat products from Germany and Korea...

  7. 77 FR 263 - Certain Cut-To-Length Carbon-Quality Steel Plate From Italy and Japan: Revocation of Antidumping...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-01-04

    ...] Certain Cut-To-Length Carbon-Quality Steel Plate From Italy and Japan: Revocation of Antidumping and...'') that revocation of the antidumping duty (``AD'') orders on certain cut-to-length carbon-quality steel... rates likely to prevail were the orders revoked. See Certain Cut-to-Length Carbon- Quality Steel Plate...

  8. 76 FR 12702 - Certain Cut-to-Length Carbon-Quality Steel Plate From India, Indonesia, Italy, and the Republic...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-03-08

    ...-837] Certain Cut-to-Length Carbon-Quality Steel Plate From India, Indonesia, Italy, and the Republic...-to-length carbon-quality steel plate from India, Indonesia, Italy, and the Republic of Korea (``Korea...-length carbon-quality steel plate from India, Indonesia, Italy, and Korea pursuant to section 751(c) of...

  9. 78 FR 50378 - Diffusion-Annealed, Nickel-Plated Flat-Rolled Steel Products From Japan: Postponement of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-08-19

    ...-Plated Flat-Rolled Steel Products From Japan: Postponement of Preliminary Determination of Antidumping... investigation of diffusion-annealed, nickel-plated flat-rolled steel products from Japan. See Diffusion- Annealed, Nickel-Plated Flat-Rolled Steel Products From Japan: Initiation of Antidumping Duty Investigation...

  10. Lowest cost due to highest productivity and highest quality

    NASA Astrophysics Data System (ADS)

    Wenk, Daniel

    2003-03-01

    Since global purchasing in the automotive industry has been taken up all around the world there is one main key factor that makes a TB-supplier today successful: Producing highest quality at lowest cost. The fact that Tailored Blanks, which today may reach up to 1/3 of a car body weight, are purchased on the free market but from different steel suppliers, especially in Europe and NAFTA, the philosophy on OEM side has been changing gradually towards tough evaluation criteria. "No risk at the stamping side" calls for top quality Tailored- or Tubular Blank products. Outsourcing Tailored Blanks has been starting in Japan but up to now without any quality request from the OEM side like ISO 13919-1B (welding quality standard in Europe and USA). Increased competition will automatically push the quality level and the ongoing approach to combine high strength steel with Tailored- and Tubular Blanks will ask for even more reliable system concepts which enables to weld narrow seams at highest speed. Beside producing quality, which is the key to reduce one of the most important cost driver "material scrap," in-line quality systems with true and reliable evaluation is going to be a "must" on all weld systems. Traceability of all process related data submitted to interfaces according to customer request in combination with ghost-shift-operation of TB systems are tomorrow's state-of-the-art solutions of Tailored Blank-facilities.

  11. Online aptitude automatic surface quality inspection system for hot rolled strips steel

    NASA Astrophysics Data System (ADS)

    Lin, Jin; Xie, Zhi-jiang; Wang, Xue; Sun, Nan-Nan

    2005-12-01

    Defects on the surface of hot rolled steel strips are main factors to evaluate quality of steel strips, an improved image recognition algorithm are used to extract the feature of Defects on the surface of steel strips. Base on the Machine vision and Artificial Neural Networks, establish a defect recognition method to select defect on the surface of steel strips. Base on these research. A surface inspection system and advanced algorithms for image processing to hot rolled strips is developed. Preparing two different fashion to lighting, adopting line blast vidicon of CCD on the surface steel strips on-line. Opening up capacity-diagnose-system with level the surface of steel strips on line, toward the above and undersurface of steel strips with ferric oxide, injure, stamp etc of defects on the surface to analyze and estimate. Miscarriage of justice and alternate of justice rate not preponderate over 5%.Geting hold of applications on some big enterprises of steel at home. Experiment proved that this measure is feasible and effective.

  12. 76 FR 7546 - Certain Hot-Rolled Carbon Steel Flat Products From Brazil: Rescission of Countervailing Duty...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-02-10

    ... Steel Flat Products From Brazil: Rescission of Countervailing Duty Administrative Review AGENCY: Import... hot- rolled carbon steel flat products (hot-rolled steel) from Brazil for the period January 1, 2009... countervailing duty order on hot-rolled steel from Brazil. See Agreement Suspending the Countervailing Duty...

  13. 77 FR 24221 - Corrosion-Resistant Carbon Steel Flat Products From Germany and Korea; Notice of Commission...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-04-23

    ...)] Corrosion-Resistant Carbon Steel Flat Products From Germany and Korea; Notice of Commission Determinations... countervailing duty order on corrosion-resistant carbon steel flat products from Korea and the antidumping duty orders on corrosion- resistant carbon steel flat products from Germany and Korea would be likely to lead...

  14. Effect of Cut Quality on Hybrid Laser Arc Welding of Thick Section Steels

    NASA Astrophysics Data System (ADS)

    Farrokhi, F.; Nielsen, S. E.; Schmidt, R. H.; Pedersen, S. S.; Kristiansen, M.

    From an industrial point of view, in a laser cutting-welding production chain, it is of great importance to know the influence of the attainable laser cut quality on the subsequent hybrid laser arc welding process. Many studies have been carried out in the literature to obtain lower surface roughness values on the laser cut edge. However, in practice, the cost and reliability of the cutting process is crucial and it does not always comply with obtaining the highest surface quality. In this study, a number of experiments on 25 mm steel plates were carried out to evaluate the influence of cut surface quality on the final quality of the subsequent hybrid laser welded joints. The different cut surfaces were obtained by different industrial cutting methods including laser cutting, abrasive water cutting, plasma cutting, and milling. It was found that the mentioned cutting methods could be used as preparation processes for the subsequent hybrid laser arc welding. However, cut quality could determine the choice of process parameters of the following hybrid laser arc welding.

  15. Cause-specific mortality in Finnish ferrochromium and stainless steel production workers.

    PubMed

    Huvinen, M; Pukkala, E

    2016-04-01

    Although stainless steel has been produced for more than a hundred years, exposure-related mortality data for production workers are limited. To describe cause-specific mortality in Finnish ferrochromium and stainless steel workers. We studied Finnish stainless steel production chain workers employed between 1967 and 2004, from chromite mining to cold rolling of stainless steel, divided into sub-cohorts by production units with specific exposure patterns. We obtained causes of death for the years 1971-2012 from Statistics Finland. We calculated standardized mortality ratios (SMRs) as ratios of observed and expected numbers of deaths based on population mortality rates of the same region. Among 8088 workers studied, overall mortality was significantly decreased (SMR 0.77; 95% confidence interval [CI] 0.70-0.84), largely due to low mortality from diseases of the circulatory system (SMR 0.71; 95% CI 0.61-0.81). In chromite mine, stainless steel melting shop and metallurgical laboratory workers, the SMR for circulatory disease was below 0.4 (SMR 0.33; 95% CI 0.07-0.95, SMR 0.22; 95% CI 0.05-0.65 and SMR 0.16; 95% CI 0.00-0.90, respectively). Mortality from accidents (SMR 0.84; 95% CI 0.67-1.04) and suicides (SMR 0.72; 95% CI 0.56-0.91) was also lower than in the reference population. Working in the Finnish ferrochromium and stainless steel industry appears not to be associated with increased mortality. © The Author 2015. Published by Oxford University Press on behalf of the Society of Occupational Medicine.

  16. Technical Requirements for the Development of Marine Steel in China

    NASA Astrophysics Data System (ADS)

    Su, Hang; Pan, Tao; Chai, Feng; Yang, Caifu

    China now experiences a fast development in shipbuilding and marine steel, the self-developed steel could meet the needs among 95% domestic clients. But in the items of some special high-end products, there are still certain gaps with advanced foreign countries, and these are mainly high-quality and strong-capacity products, large-size products, low-temperature products, and anti-corrosion, anti-fatigue and high-level failure arrest products. In the present paper, some domestic research and development (R& D) results in industry have been introduced, also, it points out that to eliminate these gaps, should rely on both the tech-progress in iron and steel industry, shipbuilding, and marine steel industry, and the establishment and improvement of the R& D system in researching, manufacturing, testing, producing and application.

  17. Ultrasonic Spectroscopy of Stainless Steel Sandwich Panels

    NASA Technical Reports Server (NTRS)

    Cosgriff, Laura M.; Lerch, Bradley A.; Hebsur, Mohan G.; Baaklini, George Y.; Ghosn, Louis J.

    2003-01-01

    Enhanced, lightweight material systems, such as 17-4PH stainless steel sandwich panels are being developed for use as fan blades and fan containment material systems for next generation engines. In order to improve the production for these systems, nondestructive evaluation (NDE) techniques, such as ultrasonic spectroscopy, are being utilized to evaluate the brazing quality between the 17-4PH stainless steel face plates and the 17-4PH stainless steel foam core. Based on NDE data, shear tests are performed on sections representing various levels of brazing quality from an initial batch of these sandwich structures. Metallographic characterization of brazing is done to corroborate NDE findings and the observed shear failure mechanisms.

  18. A Comparison of Iron and Steel Production Energy Use and Energy Intensity in China and the U.S.

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Hasanbeigi, Ali; Price, Lynn; Aden, Nathaniel

    Production of iron and steel is an energy-intensive manufacturing process. In 2006, the iron and steel industry accounted for 13.6% and 1.4% of primary energy consumption in China and the U.S., respectively (U.S. DOE/EIA, 2010a; Zhang et al., 2010). The energy efficiency of steel production has a direct impact on overall energy consumption and related carbon dioxide (CO2) emissions. The goal of this study is to develop a methodology for making an accurate comparison of the energy intensity (energy use per unit of steel produced) of steel production. The methodology is applied to the steel industry in China and themore » U.S. The methodology addresses issues related to boundary definitions, conversion factors, and indicators in order to develop a common framework for comparing steel industry energy use. This study uses a bottom-up, physical-based method to compare the energy intensity of China and U.S. crude steel production in 2006. This year was chosen in order to maximize the availability of comparable steel-sector data. However, data published in China and the U.S. are not always consistent in terms of analytical scope, conversion factors, and information on adoption of energy-saving technologies. This study is primarily based on published annual data from the China Iron & Steel Association and National Bureau of Statistics in China and the Energy Information Agency in the U.S. This report found that the energy intensity of steel production is lower in the United States than China primarily due to structural differences in the steel industry in these two countries. In order to understand the differences in energy intensity of steel production in both countries, this report identified key determinants of sector energy use in both countries. Five determinants analyzed in this report include: share of electric arc furnaces in total steel production, sector penetration of energy-efficiency technologies, scale of production equipment, fuel shares in the iron and

  19. [Stainless steels for medical instruments].

    PubMed

    Feofilov, R N

    1981-01-01

    Both in the USSR and abroad similar types of martensitic and austenitic stainless steel are used for the manufacture of medical instruments. Martensitic steel, the cheapest and most economically alloyed, has the best combination of properties necessary for medical instruments. The analysis of the Soviet and foreign experience in using different grades of steel for the production of medical instruments demonstrates the expediency and possibility of improving the quality of martensitic steel and rolled stock, as well as that of medical instruments manufactured from these materials, by improving, the operations of the metallurgical and technological processes and by specifying more precisely the requirements for medical instruments. The possibility and expediency of using, in some technically justified cases, lower grades of alloyed steel instead of grade 12X18H9T for clamps and other instruments made of stainless steel, as well as highly corrosive grades of steel for microinstruments, have been established.

  20. 78 FR 72863 - Circular Welded Carbon-Quality Steel Pipe From the People's Republic of China: Continuation of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-12-04

    ...-Quality Steel Pipe From the People's Republic of China: Continuation of Antidumping Duty Order AGENCY... circular welded carbon-quality steel pipe (``circular welded pipe'') from the People's Republic of China...\\ See Initiation of Five-Year (``Sunset'') Review, 78 FR 33063 (June 3, 2013). \\2\\ See Circular Welded...

  1. 76 FR 68208 - Circular Welded Carbon-Quality Steel Pipe From India, Oman, United Arab Emirates, and Vietnam...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-11-03

    ... (Preliminary)] Circular Welded Carbon-Quality Steel Pipe From India, Oman, United Arab Emirates, and Vietnam... carbon-quality steel pipe from India, Oman, United Arab Emirates, and Vietnam, provided for in... Governments of India, Oman, United Arab Emirates, and Vietnam. Unless the Department of Commerce extends the...

  2. 78 FR 75371 - Diffusion-Annealed, Nickel-Plated Flat-Rolled Steel Products From Japan; Scheduling of the Final...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-12-11

    ...-Plated Flat-Rolled Steel Products From Japan; Scheduling of the Final Phase of an Antidumping... imports from Japan of diffusion-annealed, nickel- plated flat-rolled steel products, provided for... diffusion-annealed, nickel- plated flat-rolled steel products from Japan are being sold in the United States...

  3. 78 FR 24435 - Hot-Rolled Steel Products From China, India, Indonesia, Taiwan, Thailand, and Ukraine

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-04-25

    ... 906-908 (Second Review)] Hot-Rolled Steel Products From China, India, Indonesia, Taiwan, Thailand, and... products from India, Indonesia, and Thailand and antidumping duty orders on hot-rolled steel products from China, India, Indonesia, Taiwan, Thailand, and Ukraine. AGENCY: United States International Trade...

  4. Quantify the energy and environmental benefits of implementing energy-efficiency measures in China’s iron and steel production

    DOE PAGES

    Ma, Ding; Chen, Wenying; Xu, Tengfang

    2015-08-21

    As one of the most energy-, emission- and pollution-intensive industries, iron and steel production is responsible for significant emissions of greenhouse gas (GHG) and air pollutants. Although many energy-efficiency measures have been proposed by the Chinese government to mitigate GHG emissions and to improve air quality, lacking full understanding of the costs and benefits has created barriers against implementing these measures widely. This paper sets out to advance the understanding by addressing the knowledge gap in costs, benefits, and cost-effectiveness of energy-efficiency measures in iron and steel production. Specifically, we build a new evaluation framework to quantify energy benefits andmore » environmental benefits (i.e., CO 2 emission reduction, air-pollutants emission reduction and water savings) associated with 36 energy-efficiency measures. Results show that inclusion of benefits from CO 2 and air-pollutants emission reduction affects the cost-effectiveness of energy-efficiency measures significantly, while impacts from water-savings benefits are moderate but notable when compared to the effects by considering energy benefits alone. The new information resulted from this study should be used to augment future programs and efforts in reducing energy use and environmental impacts associated with steel production.« less

  5. Quantify the energy and environmental benefits of implementing energy-efficiency measures in China’s iron and steel production

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Ma, Ding; Chen, Wenying; Xu, Tengfang

    As one of the most energy-, emission- and pollution-intensive industries, iron and steel production is responsible for significant emissions of greenhouse gas (GHG) and air pollutants. Although many energy-efficiency measures have been proposed by the Chinese government to mitigate GHG emissions and to improve air quality, lacking full understanding of the costs and benefits has created barriers against implementing these measures widely. This paper sets out to advance the understanding by addressing the knowledge gap in costs, benefits, and cost-effectiveness of energy-efficiency measures in iron and steel production. Specifically, we build a new evaluation framework to quantify energy benefits andmore » environmental benefits (i.e., CO 2 emission reduction, air-pollutants emission reduction and water savings) associated with 36 energy-efficiency measures. Results show that inclusion of benefits from CO 2 and air-pollutants emission reduction affects the cost-effectiveness of energy-efficiency measures significantly, while impacts from water-savings benefits are moderate but notable when compared to the effects by considering energy benefits alone. The new information resulted from this study should be used to augment future programs and efforts in reducing energy use and environmental impacts associated with steel production.« less

  6. 78 FR 15703 - Certain Hot-Rolled Carbon Steel Flat Products From India, Indonesia, the People's Republic of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-03-12

    ...-835, A-549-817, A-823-811] Certain Hot-Rolled Carbon Steel Flat Products From India, Indonesia, the... steel flat products from India, Indonesia, the People's Republic of China (PRC), Taiwan, Thailand, and... steel flat products from India, Indonesia, the PRC, Taiwan, Thailand, and Ukraine, pursuant to section...

  7. 76 FR 15299 - Certain Hot-Rolled Carbon Steel Flat Products From India: Preliminary Rescission of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-03-21

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-533-821] Certain Hot-Rolled Carbon... on certain hot-rolled carbon steel flat products from India. See Antidumping or Countervailing Duty... products covered under this order are certain hot-rolled flat- rolled carbon steel flat products of a...

  8. 76 FR 80963 - Cut-To-Length Carbon-Quality Steel Plate From India, Indonesia, Italy, Japan, and Korea

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-12-27

    ... Review)] Cut-To-Length Carbon-Quality Steel Plate From India, Indonesia, Italy, Japan, and Korea... cut-to-length carbon-quality steel plate from India, Indonesia, and Korea would be likely to lead to... Plate from India, Indonesia, Italy, Japan, and Korea: Investigation Nos. 701-TA-388-391 and 731-TA-817...

  9. 78 FR 69371 - Diffusion-Annealed, Nickel-Plated Flat-Rolled Steel Products From Japan: Preliminary...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-11-19

    ... Memorandum 1. Background 2. Scope of the Investigation 3. Respondent Selection 4. Discussion of Methodology a...: Scope of the Investigation The diffusion-annealed, nickel-plated flat-rolled steel products included in this investigation are flat-rolled, cold-reduced steel products, regardless of chemistry; whether or...

  10. Spatial distribution of crystalline corrosion products formed during corrosion of stainless steel in concrete

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Serdar, Marijana; Meral, Cagla; Kunz, Martin

    2015-05-15

    The mineralogy and spatial distribution of nano-crystalline corrosion products that form in the steel/concrete interface were characterized using synchrotron X-ray micro-diffraction (μ-XRD). Two types of low-nickel high-chromium reinforcing steels embedded into mortar and exposed to NaCl solution were investigated. Corrosion in the samples was confirmed by electrochemical impedance spectroscopy (EIS). μ-XRD revealed that goethite (α-FeOOH) and akaganeite (β-FeOOH) are the main iron oxide–hydroxides formed during the chloride-induced corrosion of stainless steel in concrete. Goethite is formed closer to the surface of the steel due to the presence of chromium in the steel, while akaganeite is formed further away from themore » surface due to the presence of chloride ions. Detailed microstructural analysis is shown and discussed on one sample of each type of steel. - Highlights: • Synchrotron micro-diffraction used to map the distribution of crystalline phases. • Goethite and akaganeite are the main corrosion products during chloride induced corrosion in mortar. • Layers of goethite and akaganeite are negatively correlated. • EDS showed Cr present in corrosion products identified by SEM.« less

  11. Microbial Methane Production Associated with Carbon Steel Corrosion in a Nigerian Oil Field

    PubMed Central

    Mand, Jaspreet; Park, Hyung S.; Okoro, Chuma; Lomans, Bart P.; Smith, Seun; Chiejina, Leo; Voordouw, Gerrit

    2016-01-01

    Microbially influenced corrosion (MIC) in oil field pipeline systems can be attributed to many different types of hydrogenotrophic microorganisms including sulfate reducers, methanogens and acetogens. Samples from a low temperature oil reservoir in Nigeria were analyzed using DNA pyrotag sequencing. The microbial community compositions of these samples revealed an abundance of anaerobic methanogenic archaea. Activity of methanogens was demonstrated by incubating samples anaerobically in a basal salts medium, in the presence of carbon steel and carbon dioxide. Methane formation was measured in all enrichments and correlated with metal weight loss. Methanogens were prominently represented in pipeline solids samples, scraped from the inside of a pipeline, comprising over 85% of all pyrosequencing reads. Methane production was only witnessed when carbon steel beads were added to these pipeline solids samples, indicating that no methane was formed as a result of degradation of the oil organics present in these samples. These results were compared to those obtained for samples taken from a low temperature oil field in Canada, which had been incubated with oil, either in the presence or in the absence of carbon steel. Again, methanogens present in these samples catalyzed methane production only when carbon steel was present. Moreover, acetate production was also found in these enrichments only in the presence of carbon steel. From these studies it appears that carbon steel, not oil organics, was the predominant electron donor for acetate production and methane formation in these low temperature oil fields, indicating that the methanogens and acetogens found may contribute significantly to MIC. PMID:26793176

  12. 77 FR 69790 - Certain Hot-Rolled Carbon Steel Flat Products From the People's Republic of China: Final Results...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-11-21

    ... fully stabilized; high strength low alloy; and the substrate for motor lamination steel may also enter... Steel Flat Products From the People's Republic of China: Final Results and Final No Shipments... antidumping duty order on certain hot- rolled carbon steel flat products (``hot-rolled steel'') from the...

  13. 75 FR 22555 - Certain Cut-to-Length Carbon-Quality Steel Plate from the Republic of Korea: Rescission of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-04-29

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-836] Certain Cut-to-Length Carbon-Quality Steel Plate from the Republic of Korea: Rescission of Antidumping Duty Administrative Review... certain cut-to-length carbon-quality steel plate (CTL plate) from the Republic of Korea. The period of...

  14. 48 CFR 252.216-7007 - Economic price adjustment-basic steel, aluminum, brass, bronze, or copper mill products...

    Code of Federal Regulations, 2012 CFR

    2012-10-01

    ...-basic steel, aluminum, brass, bronze, or copper mill products-representation. 252.216-7007 Section 252....216-7007 Economic price adjustment—basic steel, aluminum, brass, bronze, or copper mill products... Steel, Aluminum, Brass, Bronze, or Copper Mill Products—Representation (MAR 2012) (a) Definitions. The...

  15. 48 CFR 252.216-7007 - Economic price adjustment-basic steel, aluminum, brass, bronze, or copper mill products...

    Code of Federal Regulations, 2013 CFR

    2013-10-01

    ...-basic steel, aluminum, brass, bronze, or copper mill products-representation. 252.216-7007 Section 252....216-7007 Economic price adjustment—basic steel, aluminum, brass, bronze, or copper mill products... Steel, Aluminum, Brass, Bronze, or Copper Mill Products—Representation (MAR 2012) (a) Definitions. The...

  16. 48 CFR 252.216-7007 - Economic price adjustment-basic steel, aluminum, brass, bronze, or copper mill products...

    Code of Federal Regulations, 2014 CFR

    2014-10-01

    ...-basic steel, aluminum, brass, bronze, or copper mill products-representation. 252.216-7007 Section 252....216-7007 Economic price adjustment—basic steel, aluminum, brass, bronze, or copper mill products... Steel, Aluminum, Brass, Bronze, or Copper Mill Products—Representation (MAR 2012) (a) Definitions. The...

  17. Quality assurance testing of a high performance steel bridge in Virginia.

    DOT National Transportation Integrated Search

    2005-01-01

    One of the original objectives of this study was to recommend appropriate procedures for welding bridge members of high performance steel HPS70W to assure quality welds. The final objective was to determine whether hydrogen-induced microcracking migh...

  18. 77 FR 73674 - Circular Welded Carbon-Quality Steel Pipe From India, Oman, The United Arab Emirates, and Vietnam

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-12-11

    ...)] Circular Welded Carbon-Quality Steel Pipe From India, Oman, The United Arab Emirates, and Vietnam... welded carbon-quality steel pipe from India, Oman, the United Arab Emirates, and Vietnam, provided for in... from India, Oman, the United Arab Emirates, and Vietnam were subsidized and/or dumped within the...

  19. 76 FR 78313 - Circular Welded Carbon-Quality Steel Pipe From India, Oman, the United Arab Emirates, and Vietnam

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-12-16

    ... (Preliminary)] Circular Welded Carbon-Quality Steel Pipe From India, Oman, the United Arab Emirates, and... India, Oman, the United Arab Emirates, and Vietnam of circular welded carbon- quality steel pipe... the Governments of India, Oman, the United Arab Emirates, and Vietnam.\\2\\ \\1\\ The record is defined in...

  20. 77 FR 37711 - Circular Welded Carbon-Quality Steel Pipe From India, Oman, the United Arab Emirates, and Vietnam...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-06-22

    ...)] Circular Welded Carbon-Quality Steel Pipe From India, Oman, the United Arab Emirates, and Vietnam...-fair-value imports from India, Oman, the United Arab Emirates, and Vietnam of circular welded carbon... respect to circular welded carbon-quality steel pipe from Oman and the United Arab Emirates being sold in...

  1. 77 FR 15718 - Circular Welded Carbon-Quality Steel Pipe From India, the Sultanate of Oman, the United Arab...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-03-16

    ...-811] Circular Welded Carbon-Quality Steel Pipe From India, the Sultanate of Oman, the United Arab... Oman (Oman), the United Arab Emirates (UAE), and the Socialist Republic of Vietnam (Vietnam). See Circular Welded Carbon-Quality Steel Pipe From India, the Sultanate of Oman, the United Arab Emirates, and...

  2. 77 FR 25404 - Certain Hot-Rolled Carbon Steel Flat Products From India: Rescission of Antidumping Duty...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-04-30

    ... Steel Flat Products From India: Rescission of Antidumping Duty Administrative Review AGENCY: Import... certain hot- rolled carbon steel flat products from India for the period December 1, 2010, through... Products from India: Customs and Border Protection Data for Selection of Respondents for Individual Review...

  3. 48 CFR 252.216-7000 - Economic price adjustment-basic steel, aluminum, brass, bronze, or copper mill products.

    Code of Federal Regulations, 2011 CFR

    2011-10-01

    ...-basic steel, aluminum, brass, bronze, or copper mill products. 252.216-7000 Section 252.216-7000 Federal... adjustment—basic steel, aluminum, brass, bronze, or copper mill products. As prescribed in 216.203-4-70(a), use the following clause: Economic Price Adjustment—Basic Steel, Aluminum, Brass, Bronze, or Copper...

  4. 48 CFR 252.216-7000 - Economic price adjustment-basic steel, aluminum, brass, bronze, or copper mill products.

    Code of Federal Regulations, 2014 CFR

    2014-10-01

    ...-basic steel, aluminum, brass, bronze, or copper mill products. 252.216-7000 Section 252.216-7000 Federal... adjustment—basic steel, aluminum, brass, bronze, or copper mill products. As prescribed in 216.203-4-70(a)(1), use the following clause: Economic Price Adjustment—Basic Steel, Aluminum, Brass, Bronze, or Copper...

  5. 48 CFR 252.216-7000 - Economic price adjustment-basic steel, aluminum, brass, bronze, or copper mill products.

    Code of Federal Regulations, 2013 CFR

    2013-10-01

    ...-basic steel, aluminum, brass, bronze, or copper mill products. 252.216-7000 Section 252.216-7000 Federal... adjustment—basic steel, aluminum, brass, bronze, or copper mill products. As prescribed in 216.203-4-70(a)(1), use the following clause: Economic Price Adjustment—Basic Steel, Aluminum, Brass, Bronze, or Copper...

  6. 48 CFR 252.216-7000 - Economic price adjustment-basic steel, aluminum, brass, bronze, or copper mill products.

    Code of Federal Regulations, 2012 CFR

    2012-10-01

    ...-basic steel, aluminum, brass, bronze, or copper mill products. 252.216-7000 Section 252.216-7000 Federal... adjustment—basic steel, aluminum, brass, bronze, or copper mill products. As prescribed in 216.203-4-70(a)(1), use the following clause: Economic Price Adjustment—Basic Steel, Aluminum, Brass, Bronze, or Copper...

  7. 78 FR 70069 - Circular Welded Carbon-Quality Steel Pipe From China

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-11-22

    ... INTERNATIONAL TRADE COMMISSION [Investigation Nos. 701-TA-447 and 731-TA-1116 (Review)] Circular Welded Carbon-Quality Steel Pipe From China Determination On the basis of the record \\1\\ developed in the subject five-year reviews, the United States International Trade Commission (Commission) determines...

  8. Influence of shot peening on surface quality of austenitic and duplex stainless steel

    NASA Astrophysics Data System (ADS)

    Vinoth Jebaraj, A.; Sampath Kumar, T.; Ajay Kumar, L.; Deepak, C. R.

    2017-11-01

    In the present investigation, an attempt has been made to enhance the surface quality of austenitic stainless steel 316L and duplex stainless steel 2205 through shot peening process. The study mainly focuses the surface morphology, microstructural changes, surface roughness and microhardness of the peened layers. Metallography analysis was carried out and compared with the unpeened surface characteristics. As result of peening process, surface recrystallization was achieved on the layers of the peened samples. It was found that shot peening plays significant role in enhancing the surface properties of 316L and 2205. Particularly it has greater influence on the work hardening of austenitic stainless steel than the duplex stainless steel due to its more ductility nature under the investigated shot peening parameters. The findings of the present study will be useful with regard to the enhancement of surface texture achieved through peening.

  9. 76 FR 26694 - Certain Hot-Rolled Carbon Steel Flat Products From India: Final Rescission of Countervailing Duty...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-05-09

    ... Steel Flat Products From India: Final Rescission of Countervailing Duty Administrative Review AGENCY... hot-rolled carbon steel flat products from India. See Antidumping or Countervailing Duty Order... Flat Products from India: Preliminary Rescission of Countervailing Duty Administrative Review, 76 FR...

  10. 76 FR 64896 - Certain Cut-to-Length Carbon-Quality Steel Plate From the Republic of Korea: Extension of Time...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-10-19

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-836] Certain Cut-to-Length Carbon-Quality Steel Plate From the Republic of Korea: Extension of Time Limit for Preliminary Results of... on certain cut-to-length carbon-quality steel plate from the Republic of Korea. The period of review...

  11. 78 FR 14361 - U.S. Steel Tubular Products, Inc., Mckeesport Tubular Operations Division, Subsidiary of United...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-03-05

    ... Products, Inc., Mckeesport Tubular Operations Division, Subsidiary of United States Steel Corporation, Mckeesport, PA; Notice of Initiation of Investigation To Terminate Certification of Eligibility Pursuant to... Tubular Products, McKeesport Tubular Operations Division, Subsidiary of United States Steel Corporation...

  12. High Fragmentation Steel Production Process

    DTIC Science & Technology

    1981-08-01

    Hsv j , —U -I* : -’ 1 . ’ ; - * - 1 "^Sv i ! :.:.; 1 HEBUCTIOK AHU.,, .../y?.;-’" • jttoireAnoi..|..r!.5^«. ::^;;;i:^l^~!’in...on rmrerae aide 11 neceaaary and Identity by block number) HF- 1 Steel Metallurgical Evaluation MMT-Process improvement 20. ABSTRACT ("ContfBu...ao reraram attba tt n*c*aaMey and. IderUlty by block numbat) Two heats of B0F HF- 1 steel were purchased, one from Republic Steel and one from

  13. Solidification structures grown under induced flow and continuous casting of steel

    NASA Technical Reports Server (NTRS)

    Tsavaras, A. A.

    1984-01-01

    The use of induced flow as a means to control solidification structures in strand cast steel is investigated. The quality problems in strand cast steel stemming from columnar growth can be partially controlled, by Electro Magnetic Stirring (EMS). Induced flow changes the normal morphology of dendrites. Solids grown under intense stirring conditions show both negative and positive segregation which is considered unacceptable by some steel producers. The inclusion size and population is strongly affected by induced flow (EMS). Laboratory and industrial data show substantial reduction in inclusion size and content, but the overall effect of flow on inclusions is affected by the particular type of flow patterns utilized in each case. Productivity and quality are raised substantially in steel strand casting by utilizing EMS.

  14. A Steel Ball Surface Quality Inspection Method Based on a Circumferential Eddy Current Array Sensor.

    PubMed

    Zhang, Huayu; Xie, Fengqin; Cao, Maoyong; Zhong, Mingming

    2017-07-01

    To efficiently inspect surface defects on steel ball bearings, a new method based on a circumferential eddy current array (CECA) sensor was proposed here. The best probe configuration, in terms of the coil quality factor (Q-factor), magnetic field intensity, and induced eddy current density on the surface of a sample steel ball, was determined using 3-, 4-, 5-, and 6-coil probes, for analysis and comparison. The optimal lift-off from the measured steel ball, the number of probe coils, and the frequency of excitation current suitable for steel ball inspection were obtained. Using the resulting CECA sensor to inspect 46,126 steel balls showed a miss rate of ~0.02%. The sensor was inspected for surface defects as small as 0.05 mm in width and 0.1 mm in depth.

  15. 78 FR 37584 - U.S. Steel Tubular Products, Inc., Mckeesport Tubular Operations Division, Subsidiary of United...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-06-21

    ... make the following certification: All workers of U.S. Steel Tubular Products, McKeesport Tubular... Products, Inc., Mckeesport Tubular Operations Division, Subsidiary of United States Steel Corporation, Mckeesport, Pennsylvania; Notice of Amended Certification Pursuant to Section 221 of the Trade Act of 1974...

  16. Continuous steel production and apparatus

    DOEpatents

    Peaslee, Kent D [Rolla, MO; Peter, Jorg J [McMinnville, OR; Robertson, David G. C. [Rolla, MO; Thomas, Brian G [Champaign, IL; Zhang, Lifeng [Trondheim, NO

    2009-11-17

    A process for continuous refining of steel via multiple distinct reaction vessels for melting, oxidation, reduction, and refining for delivery of steel continuously to, for example, a tundish of a continuous caster system, and associated apparatus.

  17. Study of Variable Frequency Induction Heating in Steel Making Process

    NASA Astrophysics Data System (ADS)

    Fukutani, Kazuhiko; Umetsu, Kenji; Itou, Takeo; Isobe, Takanori; Kitahara, Tadayuki; Shimada, Ryuichi

    Induction heating technologies have been the standard technologies employed in steel making processes because they are clean, they have a high energy density, they are highly the controllable, etc. However, there is a problem in using them; in general, frequencies of the electric circuits have to be kept fixed to improve their power factors, and this constraint makes the processes inflexible. In order to overcome this problem, we have developed a new heating technique-variable frequency power supply with magnetic energy recovery switching. This technique helps us in improving the quality of steel products as well as the productivity. We have also performed numerical calculations and experiments to evaluate its effect on temperature distributions on heated steel plates. The obtained results indicate that the application of the technique in steel making processes would be advantageous.

  18. 76 FR 72721 - Galvanized Steel Wire From China and Mexico; Scheduling of the Final Phase of Countervailing Duty...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-11-25

    ...)] Galvanized Steel Wire From China and Mexico; Scheduling of the Final Phase of Countervailing Duty and... galvanized steel wire, provided for in subheading 7217.20 of the Harmonized Tariff Schedule of the United... merchandise as galvanized steel wire which is a cold- drawn carbon quality steel product in coils, of solid...

  19. The steel scrap age.

    PubMed

    Pauliuk, Stefan; Milford, Rachel L; Müller, Daniel B; Allwood, Julian M

    2013-04-02

    Steel production accounts for 25% of industrial carbon emissions. Long-term forecasts of steel demand and scrap supply are needed to develop strategies for how the steel industry could respond to industrialization and urbanization in the developing world while simultaneously reducing its environmental impact, and in particular, its carbon footprint. We developed a dynamic stock model to estimate future final demand for steel and the available scrap for 10 world regions. Based on evidence from developed countries, we assumed that per capita in-use stocks will saturate eventually. We determined the response of the entire steel cycle to stock saturation, in particular the future split between primary and secondary steel production. During the 21st century, steel demand may peak in the developed world, China, the Middle East, Latin America, and India. As China completes its industrialization, global primary steel production may peak between 2020 and 2030 and decline thereafter. We developed a capacity model to show how extensive trade of finished steel could prolong the lifetime of the Chinese steelmaking assets. Secondary steel production will more than double by 2050, and it may surpass primary production between 2050 and 2060: the late 21st century can become the steel scrap age.

  20. 48 CFR 252.216-7000 - Economic price adjustment-basic steel, aluminum, brass, bronze, or copper mill products.

    Code of Federal Regulations, 2010 CFR

    2010-10-01

    ...-basic steel, aluminum, brass, bronze, or copper mill products. 252.216-7000 Section 252.216-7000 Federal... adjustment—basic steel, aluminum, brass, bronze, or copper mill products. As prescribed in 216.203-4-70(a... Mill Products (JUL 1997) (a) Definitions. As used in this clause— Established price means a price which...

  1. AIS/DOE Technology Roadmap Program: Strip Casting: Anticipating New Routes To Steel Sheet

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Prof. Alan W. Camb; Prof. Anthony Rollett

    2001-08-31

    To determine the potential for strip casting in the steel industry and to develop the fundamental knowledge necessary to allow the role of strip casting in the modern steel industry to be understood. Based upon a study of carbon steel strip castings that were either produced for the program at British Steel or were received from a pre-commercial production machine, the following conclusions were made. Strip casting of carbon steels is technically feasible for sheet material from slightly less than 1 mm thick to 3 mm thick, and, assuming that it is economically viable, it will be first applied inmore » carbon steel markets that do not require stringent surface quality or extensive forming. The potential of strip casting as a casting process to be developed for steel castings is very high as the cast strip has some very novel characteristics. Direct cast carbon strip has better surface quality, shape and profile than any other casting process currently available. The more rapidly solidified structure of direct cast strip tends to be strong with low ductility; however, with adequate thermal treatment, it is possible to develop a variety of properties from the same grade. The process is more amenable at this time to production tonnages per year of the order of 500,000 tons and as such will first find niche type applications. This technology is an additional technology for steel production and will be in addition to, rather than a replacement for, current casting machines.« less

  2. Experiments and FE-simulations of stretch flanging of DP-steels with different shear cut edge quality

    NASA Astrophysics Data System (ADS)

    Sigvant, M.; Falk, J.; Pilthammar, J.

    2017-09-01

    Dual-Phase (DP) steels are today used in the automotive industry due to its large strength to weight ratio. However, the high strength of DP-steel does have a negative impact on the general formability in sheet metal forming. Unfavourable process conditions in the press shop will, on top of this, reduce the formability of DP-steels even more. This paper addresses the problem of edge fracture in stretch flanges in sheet metal parts made of DP-steel. The experimental part involves tests of ten different DP590 and DP780 steel grades with three different shear cut qualities. The influence on the fracture strain of the sample orientation of the shear cut are also studied by facing the burr away or towards the punch and testing samples with the cut edge parallel with the rolling direction and the transverse direction. The strains are measured with an ARAMIS system in each test, together with punch displacement and punch force. All tests are then simulated with AutoFormplus R7 and the results from these simulations are compared with the experimental results in order to find the appropriate failure strain for each combination of supplier, coating, thickness and shear cut quality.

  3. Automated surface inspection for steel products using computer vision approach.

    PubMed

    Xi, Jiaqi; Shentu, Lifeng; Hu, Jikang; Li, Mian

    2017-01-10

    Surface inspection is a critical step in ensuring the product quality in the steel-making industry. In order to relieve inspectors of laborious work and improve the consistency of inspection, much effort has been dedicated to the automated inspection using computer vision approaches over the past decades. However, due to non-uniform illumination conditions and similarity between the surface textures and defects, the present methods are usually applicable to very specific cases. In this paper a new framework for surface inspection has been proposed to overcome these limitations. By investigating the image formation process, a quantitative model characterizing the impact of illumination on the image quality is developed, based on which the non-uniform brightness in the image can be effectively removed. Then a simple classifier is designed to identify the defects among the surface textures. The significance of this approach lies in its robustness to illumination changes and wide applicability to different inspection scenarios. The proposed approach has been successfully applied to the real-time surface inspection of round billets in real manufacturing. Implemented on a conventional industrial PC, the algorithm can proceed at 12.5 frames per second with the successful detection rate being over 90% for turned and skinned billets.

  4. 77 FR 16810 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-03-22

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-580-818] Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time Limit for Preliminary Results of... Register the countervailing duty order on corrosion-resistant carbon steel flat products (CORE) from Korea...

  5. 77 FR 25141 - Corrosion-Resistant Carbon Steel Flat Products From Germany and South Korea: Extension of Time...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-04-27

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-428-815, A-580-816] Corrosion...) orders on corrosion-resistant carbon steel flat products (CORE) from Germany and South Korea (Korea..., regarding ``Sunset Reviews of the Antidumping Duty Orders on Corrosion-Resistant Carbon Steel Flat Products...

  6. 75 FR 18153 - Corrosion-Resistant Carbon Steel Flat Products from the Republic of Korea: Extension of Time...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-04-09

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-580-818] Corrosion-Resistant Carbon Steel Flat Products from the Republic of Korea: Extension of Time Limit for Preliminary Results of... countervailing duty order on corrosion-resistant carbon steel flat products (CORE) from Korea. See Countervailing...

  7. 76 FR 20954 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-04-14

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-580-818] Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time Limit for Preliminary Results of... Register the countervailing duty order on corrosion-resistant carbon steel flat products (CORE) from Korea...

  8. 76 FR 65497 - Certain Hot-Rolled Carbon Steel Flat Products From India: Amended Final Results of Countervailing...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-10-21

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-533-821] Certain Hot-Rolled Carbon...-rolled carbon steel flat products (HRCS) from India covering the January 1, 2006, through December 31... Certain Hot-Rolled Carbon Steel Flat Products from India: Final Results of Countervailing Duty...

  9. Mercury mass flow in iron and steel production process and its implications for mercury emission control.

    PubMed

    Wang, Fengyang; Wang, Shuxiao; Zhang, Lei; Yang, Hai; Gao, Wei; Wu, Qingru; Hao, Jiming

    2016-05-01

    The iron and steel production process is one of the predominant anthropogenic sources of atmospheric mercury emissions worldwide. In this study, field tests were conducted to study mercury emission characteristics and mass flows at two iron and steel plants in China. It was found that low-sulfur flue gas from sintering machines could contribute up to 41% of the total atmospheric mercury emissions, and desulfurization devices could remarkably help reduce the emissions. Coal gas burning accounted for 17%-49% of the total mercury emissions, and therefore the mercury control of coal gas burning, specifically for the power plant burning coal gas to generate electricity, was significantly important. The emissions from limestone and dolomite production and electric furnaces can contribute 29.3% and 4.2% of the total mercury emissions from iron and steel production. More attention should be paid to mercury emissions from these two processes. Blast furnace dust accounted for 27%-36% of the total mercury output for the whole iron and steel production process. The recycling of blast furnace dust could greatly increase the atmospheric mercury emissions and should not be conducted. The mercury emission factors for the coke oven, sintering machine and blast furnace were 0.039-0.047gHg/ton steel, and for the electric furnace it was 0.021gHg/ton steel. The predominant emission species was oxidized mercury, accounting for 59%-73% of total mercury emissions to air. Copyright © 2016. Published by Elsevier B.V.

  10. 77 FR 25405 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-04-30

    ... antidumping duty order on corrosion-resistant carbon steel flat products from the Republic of Korea, covering... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time Limit for the Preliminary Results of...

  11. 75 FR 25841 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-05-10

    ... antidumping duty order on corrosion-resistant carbon steel flat products from the Republic of Korea, covering... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time Limits for the Preliminary Results of...

  12. 78 FR 19210 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Final Results of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-03-29

    .... Scope of the Order Products covered by this order are certain corrosion-resistant carbon steel flat... DEPARTMENT OF COMMERCE International Trade Administration [C-580-818] Corrosion-Resistant Carbon... countervailing duty (CVD) order on corrosion-resistant carbon steel flat products from the Republic of Korea for...

  13. 76 FR 21332 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-04-15

    ... antidumping duty order on corrosion-resistant carbon steel flat products from the Republic of Korea, covering... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Extension of Time Limits for the Preliminary Results of...

  14. 78 FR 42039 - Certain Hot-Rolled Carbon Steel Flat Products From the People's Republic of China: Preliminary...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-07-15

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-570-865] Certain Hot-Rolled Carbon... review of the antidumping duty order on certain hot- rolled carbon steel flat products (``hot-rolled...\\ See Notice of Antidumping Duty Order: Certain Hot-Rolled Carbon Steel Flat Products from the People's...

  15. Ways to Improve the Quality of Die Steel 5KhNM

    NASA Astrophysics Data System (ADS)

    Efimov, S. V.; Malykhina, O. Yu; Pavlova, A. G.; Milyuts, V. G.; Tsukanov, V. V.; Vikharev, V. V.

    2017-12-01

    There was performed an analysis of influence of the deoxidation technology, hydrogen content and high concentration of titanium in steel 5KhNM (Rus. “5XHM”) on quality of die blanks, evaluated based on the results of the ultrasonic test. The fractographic examinations of fractures and the X-ray microprobe analysis of chemical composition of non-metallic inclusions were conducted, the evaluation of macro- and micro-structure of a die blank with high titanium content was performed. It is demonstrated that defects of dies from steel 5KhNM (Rus. “5XHM”) are cracks from merged flakes and micro-flakes; in most cases large concentrations of sulphides appeared to be hydrogen collectors for formation of flakes and micro-flakes.

  16. Effect of Ladle Usage on Cleanliness of Bearing Steel

    NASA Astrophysics Data System (ADS)

    Chi, Yunguang; Deng, Zhiyin; Zhu, Miaoyong

    2018-02-01

    To investigate the effects of ladle usage on the inclusions and total oxygen contents of bearing steel, MgO refractory rods with different glazes were used to simulate different ladle usages. The results show that the effects of different ladle usages on the cleanliness of the steel differ from each other. The total oxygen content of steel increases with the decreasing glaze basicity. Ladle glaze having a lower basicity has a more negative impact on the cleanliness of steel in the subsequent production. Inclusions can be generated by the flush-off of ladle glaze, and the initial glaze is important in the evolution of inclusions in the subsequent heats. To avoid the negative effect of ladle usage and to improve the steel cleanliness as much as possible, specialized ladles were suggested for producing high-quality steel grades.

  17. 78 FR 11901 - Hot-Rolled Steel Products From China, India, Indonesia, Taiwan, Thailand, and Ukraine; Notice of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-02-20

    ... 906-908 (Second Review)] Hot-Rolled Steel Products From China, India, Indonesia, Taiwan, Thailand, and..., Indonesia, and Thailand and the revocation of the antidumping duty orders on hot-rolled steel products from China, India, Indonesia, Taiwan, Thailand, and Ukraine would be likely to lead to continuation or...

  18. 77 FR 14341 - Certain Hot-Rolled Carbon Steel Flat Products From Taiwan: Notice of Rescission of Antidumping...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-03-09

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-583-835] Certain Hot-Rolled Carbon... order on certain hot-rolled carbon steel flat products from Taiwan. The period of review is November 1... antidumping duty order on certain hot- rolled carbon steel flat products from Taiwan covering the period...

  19. 77 FR 31877 - Corrosion-Resistant Carbon Steel Flat Products From Germany and Korea; Scheduling of Full Five...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-05-30

    ... INTERNATIONAL TRADE COMMISSION [Investigation Nos. 701-TA-350 and 731-TA-616 and 618 (Third Review)] Corrosion-Resistant Carbon Steel Flat Products From Germany and Korea; Scheduling of Full Five-Year Reviews... corrosion-resistant carbon steel flat products from Korea and the antidumping duty orders on corrosion...

  20. 76 FR 42679 - Certain Hot-Rolled Carbon Steel Flat Products From India: Final Results of Antidumping Duty...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-07-19

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-533-820] Certain Hot-Rolled Carbon... review of the antidumping duty order on certain hot- rolled carbon steel flat products from India... Preliminary Results \\2\\ of this review. \\2\\ See Certain Hot-Rolled Carbon Steel Flat Products From India...

  1. 77 FR 27438 - Certain Corrosion-Resistant Carbon Steel Flat Products From Korea: Final Results of Expedited...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-05-10

    ...- rolled steel products either plated or coated with tin, lead, chromium, chromium oxides, both tin and lead (``terne plate''), or both chromium and chromium oxides (``tin-free steel''), whether or not...

  2. Steel Slag and Shredded Tires as Media for Blind Inlets to Improve Water Quality

    NASA Astrophysics Data System (ADS)

    Gonzalez, J. M.; Smith, D. R.; Livingston, S.

    2015-12-01

    Off-site transport of contaminants through surface runoff affects water quality. Blind inlets are proven conservation practices for reducing surface runoff, and consequently reducing nutrient loadings from small agricultural closed depressions to water bodies. Gravel is the most widely used blind inlet media to reduce flow, but not to sorb contaminants from the water. Readily available byproducts, such as steel slag and shredded tires, could be used as alternative media in blind inlets to sorb nutrients and pesticides from surface runoff. Sorption isotherms were performed to investigate the sorption capabilities of steel slag and shredded tires for phosphate and atrazine in electrolyte background solutions containing either 10 mM CaCl2 or KCl. Results of this research demonstrated that phosphate and atrazine were irreversibly sorbed by the steel slag and shredded tires. The steel slag increased the pH solution increased about 4 pH units after the sorption step; while the pH of the solution with shredded tires remained the same. Desorption of the phosphate and atrazine was low from the steel slag and shredded tires, respectively. Thus, the above results suggest that the steel slag and shredded tires can potentially be used as media to sorb phosphate and atrazine, respectively.

  3. 78 FR 16252 - Certain Hot-Rolled Carbon Steel Flat Products From India, Indonesia, and Thailand: Final Results...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-03-14

    ...] Certain Hot-Rolled Carbon Steel Flat Products From India, Indonesia, and Thailand: Final Results of... second sunset reviews of the countervailing duty (``CVD'') orders on certain hot-rolled carbon steel flat...). Scope of the Orders The merchandise subject to these orders is hot-rolled steel of a rectangular shape...

  4. 76 FR 72173 - Circular Welded Carbon-Quality Steel Pipe From India, the Sultanate of Oman, the United Arab...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-11-22

    ...-552-810] Circular Welded Carbon-Quality Steel Pipe From India, the Sultanate of Oman, the United Arab... Steel Pipe from India, Oman, the United Arab Emirates, and Vietnam, dated October 26, 2011 (hereinafter... pipe from India, the Sultanate of Oman (``Oman''), the United Arab Emirates (``the UAE''), and the...

  5. 76 FR 62039 - Certain Hot-Rolled Carbon Steel Flat Products From India: Final Results of 2009-2010 Antidumping...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-10-06

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-533-820] Certain Hot-Rolled Carbon... administrative review of the antidumping duty order on certain hot-rolled carbon steel flat products from India (``hot-rolled steel'') manufactured by Ispat Industries Limited (``Ispat''), JSW Steel Limited (``JSW...

  6. 76 FR 31938 - Certain Hot-Rolled Carbon Steel Flat Products From India: Notice of Preliminary Results of 2009...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-06-02

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-533-820] Certain Hot-Rolled Carbon... conducting an administrative review of the antidumping duty order on certain hot-rolled carbon steel flat products from India (``hot-rolled steel'') manufactured by Ispat Industries Limited (``Ispat''), JSW Steel...

  7. 77 FR 41374 - Certain Hot-Rolled Carbon Steel Flat Products From India: Notice of Court Decision Not in Harmony...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-07-13

    ... 14, 2011) (opinion on final results) (U.S. Steel Corp. I); Certain Hot- Rolled Carbon Steel Flat... DEPARTMENT OF COMMERCE International Trade Administration [A-533-820] Certain Hot-Rolled Carbon...-rolled carbon steel flat products from India. See U.S. Steel Corp. v. United States, No. 08-00216, 2012...

  8. Cast CF8C-Plus Stainless Steel for Turbocharger Applications

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Maziasz, P.J.; Shyam, A.; Evans, N.D.

    2010-06-30

    The purpose of this Cooperative Research and Development Agreement (CRADA) project is to provide the critical test data needed to qualify CF8C-Plus cast stainless steel for commercial production and use for turbocharger housings with upgraded performance and durability relative to standard commercial cast irons or stainless steels. The turbocharger technologies include, but are not limited to, heavy-duty highway diesel engines, and passenger vehicle diesel and gasoline engines. This CRADA provides additional critical high-temperature mechanical properties testing and data analysis needed to quality the new CF8C-Plus steels for turbocharger housing applications.

  9. Microalloyed HSLA (High Strength Low Alloy) Steels: Proceedings of Microalloying 󈨜 Held in Conjunction with the 1988 World Materials Congress, Chicago, Illinois, USA, 24-30 September 1988

    DTIC Science & Technology

    1988-01-01

    steels. The high quality linepipe steels are During the last few years, a large scale conducted. During the last few years, API X52 of efforts has been...with satisfied results. mass production of API X52 steels in production line will be demonstrated. The mass production of line pipe steels in the plate...mill of China Steel Corporation has also been conducted. More than eighty Procedures thousand tons of API X52 has been manufactured during the last 2

  10. 78 FR 40428 - Certain Hot-Rolled Carbon Steel Flat Products from India: Rescission of Antidumping Duty...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-07-05

    ...The Department of Commerce (the Department) is rescinding the administrative review of the antidumping duty order on certain hot- rolled carbon steel flat products (hot rolled steel) from India for the period December 1, 2011, through November 30, 2012.

  11. Effect of Auxiliary Preheating of the Filler Wire on Quality of Gas Metal Arc Stainless Steel Claddings

    NASA Astrophysics Data System (ADS)

    Shahi, Amandeep S.; Pandey, Sunil

    2008-02-01

    Weld cladding is a process for producing surfaces with good corrosion resistant properties by means of depositing/laying of stainless steels on low-carbon steel components with an objective of achieving maximum economy and enhanced life. The aim of the work presented here was to investigate the effect of auxiliary preheating of the solid filler wire in mechanized gas metal arc welding (GMAW) process (by using a specially designed torch to preheat the filler wire independently, before its emergence from the torch) on the quality of the as-welded single layer stainless steel overlays. External preheating of the filler wire resulted in greater contribution of arc energy by resistive heating due to which significant drop in the main welding current values and hence low dilution levels were observed. Metallurgical aspects of the as welded overlays such as chemistry, ferrite content, and modes of solidification were studied to evaluate their suitability for service and it was found that claddings obtained through the preheating arrangement, besides higher ferrite content, possessed higher content of chromium, nickel, and molybdenum and lower content of carbon as compared to conventional GMAW claddings, thereby giving overlays with superior mechanical and corrosion resistance properties. The findings of this study not only establish the technical superiority of the new process, but also, owing to its productivity-enhanced features, justify its use for low-cost surfacing applications.

  12. Characterization of particle exposure in ferrochromium and stainless steel production.

    PubMed

    Järvelä, Merja; Huvinen, Markku; Viitanen, Anna-Kaisa; Kanerva, Tomi; Vanhala, Esa; Uitti, Jukka; Koivisto, Antti J; Junttila, Sakari; Luukkonen, Ritva; Tuomi, Timo

    2016-07-01

    This study describes workers' exposure to fine and ultrafine particles in the production chain of ferrochromium and stainless steel during sintering, ferrochromium smelting, stainless steel melting, and hot and cold rolling operations. Workers' personal exposure to inhalable dust was assessed using IOM sampler with a cellulose acetate filter (AAWP, diameter 25 mm; Millipore, Bedford, MA). Filter sampling methods were used to measure particle mass concentrations in fixed locations. Particle number concentrations and size distributions were examined using an SMPS+C sequential mobile particle sizer and counter (series 5.400, Grimm Aerosol Technik, Ainring, Germany), and a hand-held condensation particle counter (CPC, model 3007, TSI Incorporated, MN). The structure and elemental composition of particles were analyzed using TEM-EDXA (TEM: JEM-1220, JEOL, Tokyo, Japan; EDXA: Noran System Six, Thermo Fisher Scientific Inc., Madison,WI). Workers' personal exposure to inhalable dust averaged 1.87, 1.40, 2.34, 0.30, and 0.17 mg m(-3) in sintering plant, ferrochromium smelter, stainless steel melting shop, hot rolling mill, and the cold rolling mill, respectively. Particle number concentrations measured using SMPS+C varied from 58 × 10(3) to 662 × 10(3) cm(-3) in the production areas, whereas concentrations measured using SMPS+C and CPC3007 in control rooms ranged from 24 × 10(3) to 243 × 10(3) cm(-3) and 5.1 × 10(3) to 97 × 10(3) cm(-3), respectively. The elemental composition and the structure of particles in different production phases varied. In the cold-rolling mill non-process particles were abundant. In other sites, chromium and iron originating from ore and recycled steel scrap were the most common elements in the particles studied. Particle mass concentrations were at the same level as that reported earlier. However, particle number measurements showed a high amount of ultrafine particles, especially in sintering, alloy smelting and melting, and tapping

  13. Carbon emissions due to deforestation for the production of charcoal used in Brazil’s steel industry

    NASA Astrophysics Data System (ADS)

    Sonter, Laura J.; Barrett, Damian J.; Moran, Chris J.; Soares-Filho, Britaldo S.

    2015-04-01

    Steel produced using coal generates 7% of global anthropogenic CO2 emissions annually. Opportunities exist to substitute this coal with carbon-neutral charcoal sourced from plantation forests to mitigate project-scale emissions and obtain certified emission reduction credits under the Kyoto Protocol’s Clean Development Mechanism. This mitigation strategy has been implemented in Brazil and is one mechanism among many used globally to reduce anthropogenic CO2 emissions; however, its potential adverse impacts have been overlooked to date. Here, we report that total CO2 emitted from Brazilian steel production doubled (91 to 182 MtCO2) and specific emissions increased (3.3 to 5.2 MtCO2 per Mt steel) between 2000 and 2007, even though the proportion of coal used declined. Infrastructure upgrades and a national plantation shortage increased industry reliance on charcoal sourced from native forests, which emits up to nine times more CO2 per tonne of steel than coal. Preventing use of native forest charcoal could have avoided 79% of the CO2 emitted from steel production between 2000 and 2007; however, doing so by increasing plantation charcoal supply is limited by socio-economic costs and risks further indirect deforestation pressures and emissions. Effective climate change mitigation in Brazil’s steel industry must therefore minimize all direct and indirect carbon emissions generated from steel manufacture.

  14. Quality assurance in the production of pipe fittings by automatic laser-based material identification

    NASA Astrophysics Data System (ADS)

    Moench, Ingo; Peter, Laszlo; Priem, Roland; Sturm, Volker; Noll, Reinhard

    1999-09-01

    In plants of the chemical, nuclear and off-shore industry, application specific high-alloyed steels are used for pipe fittings. Mixing of different steel grades can lead to corrosion with severe consequential damages. Growing quality requirements and environmental responsibilities demand a 100% material control in the production of the pipe fittings. Therefore, LIFT, an automatic inspection machine, was developed to insure against any mix of material grades. LIFT is able to identify more than 30 different steel grades. The inspection method is based on Laser-Induced Breakdown Spectrometry (LIBS). An expert system, which can be easily trained and recalibrated, was developed for the data evaluation. The result of the material inspection is transferred to an external handling system via a PLC interface. The duration of the inspection process is 2 seconds. The graphical user interface was developed with respect to the requirements of an unskilled operator. The software is based on a realtime operating system and provides a safe and reliable operation. An interface for the remote maintenance by modem enables a fast operational support. Logged data are retrieved and evaluated. This is the basis for an adaptive improvement of the configuration of LIFT with respect to changing requirements in the production line. Within the first six months of routine operation, about 50000 pipe fittings were inspected.

  15. Utilizing steel slag in environmental application - An overview

    NASA Astrophysics Data System (ADS)

    Lim, J. W.; Chew, L. H.; Choong, T. S. Y.; Tezara, C.; Yazdi, M. H.

    2016-06-01

    Steel slags are generated as waste material or byproduct every day from steel making industries.The potential environmental issues which are related with the slag dump or reprocessing for metal recovery are generally being focused in the research. However the chemistry and mineralogy of slag depends on metallurgical process which is able to determine whether the steel slag can be the reusable products or not. Nowadays, steel slag are well characterized by using several methods, such as X-ray Diffraction, ICP-OES, leaching test and many more. About the industrial application, it is mainly reused as aggregate for road construction, as armour stones for hydraulic engineering constructions and as fertilizers for agricultural purposes. To ensure the quality of steel slag for the end usage, several test methods are developed for evaluating the technical properties of steel slag, especially volume stability and environmental behaviour. In order to determine its environmental behaviour, leaching tests have been developed. The focus of this paper however is on those applications that directly affect environmental issues including remediation, and mitigation of activities that negatively impact the environment.

  16. Steel Industry Wastes.

    ERIC Educational Resources Information Center

    Schmidtke, N. W.; Averill, D. W.

    1978-01-01

    Presents a literature review of wastes from steel industry, covering publications of 1976-77. This review covers: (1) coke production; (2) iron and steel production; (3) rolling operations; and (4) surface treatment. A list of 133 references is also presented. (NM)

  17. Fabrication of stainless steel clad tubing. [gas pressure bonding

    NASA Technical Reports Server (NTRS)

    Kovach, C. W.

    1978-01-01

    The feasibility of producing stainless steel clad carbon steel tubing by a gas pressure bonding process was evaluated. Such a tube product could provide substantial chromium savings over monolithic stainless tubing in the event of a serious chromium shortage. The process consists of the initial assembly of three component tubesets from conventionally produced tubing, the formation of a strong metallurgical bond between the three components by gas pressure bonding, and conventional cold draw and anneal processing to final size. The quality of the tubes produced was excellent from the standpoint of bond strength, mechanical, and forming properties. The only significant quality problem encountered was carburization of the stainless clad by the carbon steel core which can be overcome by further refinement through at least three different approaches. The estimated cost of clad tubing produced by this process is greater than that for monolithic stainless tubing, but not so high as to make the process impractical as a chromium conservation method.

  18. 75 FR 59689 - Certain Hot-Rolled Carbon Steel Flat Products From India: Notice of Court Decision Not in Harmony...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-09-28

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-533-821] Certain Hot-Rolled Carbon... certain hot-rolled carbon steel flat products (HRCS) from India covering the period of review (POR) of January 1, 2006, through December 31, 2006. See Certain Hot-Rolled Carbon Steel Flat Products from India...

  19. 77 FR 264 - Certain Cut-To-Length Carbon-Quality Steel Plate From India, Indonesia, and the Republic of Korea...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-01-04

    ...-806, A-580-836, C-580-837] Certain Cut-To-Length Carbon-Quality Steel Plate From India, Indonesia, and... steel plate (``CTL Plate'') from India, Indonesia, and the Republic of Korea (``Korea'') would likely...'') orders on CTL Plate from India, Indonesia, and Korea would likely lead to the continuation or recurrence...

  20. Influence of Mn contents in 0Cr18Ni10Ti thin wall stainless steel tube on TIG girth weld quality

    NASA Astrophysics Data System (ADS)

    Liu, Bo

    2017-03-01

    Three kinds of cold worked 0Cr18Ni10Ti thin wall stainless steel tubes with the manganese contents of 1.27%, 1.35% and 1.44% and the cold worked 0Cr18Ni10Ti stainless steel end plug with manganese content of 1.35% were used for TIG girth welding in the present investigation. The effect of different manganese contents in stainless steel tube on weld quality was studied. The results showed that under the same welding conditions, the metallographic performance of the girth weld for the thin wall stainless steel tube with the manganese element content 1.44% welded with end plug was the best. Under the appropriate welding conditions, the quality of the girth weld increased with the increase of the manganese content till 1.44%. It was found that in the case of the Mn content of 1.44%, and under the proper welding condition the welding defects, such as welding cracks were effectively avoided, and the qualified weld penetration can be obtained.. It is concluded that the appropriate increase of the manganese content can significantly improve the TIG girth weld quality of the cold worked 0Cr18Ni10Ti stainless steel tube.

  1. Improvement of the Mechanical Properties of 1022 Carbon Steel Coil by Using the Taguchi Method to Optimize Spheroidized Annealing Conditions.

    PubMed

    Yang, Chih-Cheng; Liu, Chang-Lun

    2016-08-12

    Cold forging is often applied in the fastener industry. Wires in coil form are used as semi-finished products for the production of billets. This process usually requires preliminarily drawing wire coil in order to reduce the diameter of products. The wire usually has to be annealed to improve its cold formability. The quality of spheroidizing annealed wire affects the forming quality of screws. In the fastener industry, most companies use a subcritical process for spheroidized annealing. Various parameters affect the spheroidized annealing quality of steel wire, such as the spheroidized annealing temperature, prolonged heating time, furnace cooling time and flow rate of nitrogen (protective atmosphere). The effects of the spheroidized annealing parameters affect the quality characteristics of steel wire, such as the tensile strength and hardness. A series of experimental tests on AISI 1022 low carbon steel wire are carried out and the Taguchi method is used to obtain optimum spheroidized annealing conditions to improve the mechanical properties of steel wires for cold forming. The results show that the spheroidized annealing temperature and prolonged heating time have the greatest effect on the mechanical properties of steel wires. A comparison between the results obtained using the optimum spheroidizing conditions and the measures using the original settings shows the new spheroidizing parameter settings effectively improve the performance measures over their value at the original settings. The results presented in this paper could be used as a reference for wire manufacturers.

  2. Application of lap laser welding technology on stainless steel railway vehicles

    NASA Astrophysics Data System (ADS)

    Wang, Hongxiao; Wang, Chunsheng; He, Guangzhong; Li, Wei; Liu, Liguo

    2016-10-01

    Stainless steel railway vehicles with so many advantages, such as lightweight, antirust, low cost of maintenance and simple manufacturing process, so the production of high level stainless steel railway vehicles has become the development strategy of European, American and other developed nations. The current stainless steel railway vehicles body and structure are usually assembled by resistance spot welding process. The weak points of this process are the poor surface quality and bad airtight due to the pressure of electrodes. In this study, the partial penetration lap laser welding process was investigated to resolve the problems, by controlling the laser to stop at the second plate in the appropriate penetration. The lap laser welding joint of stainless steel railway vehicle car body with partial penetration has higher strength and surface quality than those of resistance spot welding joint. The biggest problem of lap laser welding technology is to find the balance of the strength and surface quality with different penetrations. The mechanism of overlap laser welding of stainless steel, mechanical tests, microstructure analysis, the optimization of welding parameters, analysis of fatigue performance, the design of laser welding stainless steel railway vehicles structure and the development of non-destructive testing technology were systematically studied before lap laser welding process to be applied in manufacture of railway vehicles. The results of the experiments and study show that high-quality surface state and higher fatigue strength can be achieved by the partial penetration overlap laser welding of the side panel structure, and the structure strength of the car body can be higher than the requirements of En12663, the standard of structural requirements of railway vehicles bodies. Our company has produced the stainless steel subway and high way railway vehicles by using overlap laser welding technology. The application of lap laser welding will be a big

  3. The influence of the corrosion product layer generated on the high strength low-alloy steels welded by underwater wet welding with stainless steel electrodes in seawater

    NASA Astrophysics Data System (ADS)

    Bai, Qiang; Zou, Yan; Kong, Xiangfeng; Gao, Yang; Dong, Sheng; Zhang, Wei

    2017-02-01

    The high strength low-alloy steels are welded by underwater wet welding with stainless steel electrodes. The micro-structural and electrochemical corrosion study of base metal (BM), weld zone (WZ) and heat affected zone (HAZ) are carried out to understand the influence of the corrosion product layer generated on the high strength low-alloy steels welded by underwater wet welding with stainless steel electrodes, methods used including, potentiodynamic polarization, electrochemical impedance spectroscopy (EIS) and scanning electron microscope (SEM). The results indicate that the WZ acts as a cathode and there is no corrosion product on it throughout the immersion period in seawater. The HAZ and BM acts as anodes. The corrosion rates of the HAZ and BM change with the immersion time increasing. In the initial immersion period, the HAZ has the highest corrosion rate because it has a coarse tempered martensite structure and the BM exhibites a microstructure with very fine grains of ferrite and pearlite. After a period of immersion, the BM has the highest corrosion rate. The reason is that the corrosion product layer on the HAZ is dense and has a better protective property while that on the BM is loose and can not inhibit the diffusion of oxygen.

  4. Promising Sparingly Alloyed Boron-Bearing Steels for the Production of High-Strength Fasteners

    NASA Astrophysics Data System (ADS)

    Bobylev, M. V.; Koroleva, E. G.; Shtannikov, P. A.

    2005-05-01

    The main advantages of boron-bearing steels used for production of rolled sections at cold upset shops of Russian automotive plants are considered. A thermodynamic model for the majority of boron-bearing steels for high-strength fasteners is used to plot nomograms characterizing the effect of titanium, aluminum, nitrogen, and boron on the amount of nitrides and oxides segregated in crystallization and on the content of effective boron. The effect of effective boron on the characteristics of hardenability is estimated. The studies conducted are used for determining the range of permissible contents of titanium and aluminum ensuring through hardenability of rolled bars from steels 12G1R, 20G2R, and 30G1R up to 25 mm in diameter.

  5. 75 FR 13490 - Certain Corrosion-Resistant Carbon Steel Flat Products from the Republic of Korea: Notice of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-03-22

    ... DEPARTMENT OF COMMERCE International Trade Administration (A-580-816) Certain Corrosion-Resistant... results of the antidumping duty administrative review for certain corrosion-resistant carbon steel flat products (CORE) from the Republic of Korea (Korea). See Certain Corrosion-Resistant Carbon Steel Flat...

  6. 76 FR 15291 - Certain Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Notice of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-03-21

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Certain Corrosion-Resistant... results of the antidumping duty administrative review for certain corrosion-resistant carbon steel flat products (CORE) from the Republic of Korea (Korea). See Certain Corrosion-Resistant Carbon Steel Flat...

  7. Influence of refining time on nonmetallic inclusions in a low-carbon, silicon-killed steel

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Fernandes, Marcolino; Pires, Jose Carlos; Cheung, Noe

    2003-12-15

    Nonmetallic inclusions are harmful to the mechanical properties of every kind of steel produced worldwide. The greater the size of the inclusion present in the structure of a determined kind of steel, the greater its negative effect on the quality of the steel. Therefore, the objective of this work was to investigate the size, the quantity, the shape and the chemical composition of nonmetallic inclusions formed throughout the refining process of silicon-killed, low-carbon steel, as a function of the treatment time in a ladle furnace, trying to ensure the flotation of inclusions bigger than 25 {mu}m. This investigation was carriedmore » out using a scanning electron microscope (SEM), with an analysis system using energy dispersive spectometry (EDS). Based on this work, it was possible to know more precisely the nature of the inclusions, the necessary time to ensure flotation of large inclusions, the efficiency of the slag to capture the inclusions, and the inclusion level of the steel throughout its refining process to try to obtain a higher quality steel product.« less

  8. Development of refractories and related products for steel melting, finishing, and casting

    NASA Astrophysics Data System (ADS)

    Smirnov, A. N.

    2013-06-01

    The transformation of the consumption of refractories for the production, out-of-furnace treatment, and casting of steel is considered. The main trends in developing the refractory market are shown to be a significant decrease in the specific consumption of refractories per 1 t liquid steel and the predominant application of refractories based on magnesia raw materials and fused corundum for the working layers of melting units, ladles, and tundishes. The main trend in decreasing the specific costs of refractories is the development of refractories based on alternative sources of raw materials, which are cheaper and more available for refractory manufacturers.

  9. Health, safety, and environmental risk assessment of steel production complex in central Iran using TOPSIS.

    PubMed

    Jozi, S A; Majd, N Moradi

    2014-10-01

    This research was carried out with the aim of presenting an environmental management plan for steel production complex (SPC) in central Iran. Following precise identification of the plant activities as well as the study area, possible sources of environmental pollution and adverse impacts on the air quality, water, soil, biological environment, socioeconomic and cultural environment, and health and safety of the employees were determined considering the work processes of the steel complex. Afterwards, noise, wastewater, and air pollution sources were measured. Subsequently, factors polluting the steel complex were identified by TOPSIS and then prioritized using Excel Software. Based on the obtained results, the operation of the furnaces in hot rolling process with the score 1, effluent derived from hot rolling process with the score 0.565, nonprincipal disposal and dumping of waste at the plant enclosure with the score 0.335, walking beam process with the score 1.483 respectively allocated themselves the highest priority in terms of air, water, soil and noise pollution. In terms of habitats, land cover and socioeconomic and cultural environment, closeness to the forest area and the existence of four groups of wildlife with the score 1.106 and proximity of villages and residential areas to the plant with the score 3.771 respectively enjoyed the highest priorities while impressibility and occupational accidents with the score 2.725 and cutting and welding operations with score 2.134 had the highest priority among health and safety criteria. Finally, strategies for the control of pollution sources were identified and Training, Monitoring and environmental management plan of the SPC was prepared.

  10. 76 FR 2344 - Certain Hot-Rolled Carbon Steel Flat Products From India: Notice of Preliminary Results of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-01-13

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-533-820] Certain Hot-Rolled Carbon... administrative review of the antidumping duty order on certain hot-rolled carbon steel flat products from India (``Indian Hot-Rolled'') manufactured by Essar Steel Limited (``Essar''), Ispat Industries Limited (``Ispat...

  11. 77 FR 45576 - Certain Hot-Rolled Carbon Steel Flat Products From the People's Republic of China: Preliminary...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-08-01

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-570-865] Certain Hot-Rolled Carbon...'') is conducting an administrative review of the antidumping duty order on certain hot- rolled carbon steel flat products (``hot-rolled steel'') from the People's Republic of China (``PRC''), covering the...

  12. Research on Wheel Steel Welding Cracks Caused by Quenching Stress

    NASA Astrophysics Data System (ADS)

    Guan-nan, Li

    Wheel steel products of Han Steel occurred welding cracking when using in a wheel factory, by analyzing the crack in the wheel steel weld cracking with microstructure analysis and spectrum analysis, test results showed the grain in heat affect zone serious grow, and the user at the end of the flash-butt quenched from a high temperature to room temperature at welding seam, larger cooling rate to generate sufficiently large quenching stress, increased the risk of cracking along the grain boundary. When the stress reaches a certain level, there will be a greater area of the grain cracks at the location of welding seam, eventually leading to weld cracking. We develop measures for improvement to solving this problem, we suggest that the cooling mode at welding seam should be slow cooling or air cooling after the rim welding process, welding current range is 7800 9500 amps, upsetting time is 0.2 seconds, these measures can improve the welding quality of wheel steel products and reduce the risk of welding cracks.

  13. Development and Application of High Performance Quenched and Tempered Wear Resistant Steels in Material Handling and Construction Machinery

    NASA Astrophysics Data System (ADS)

    Su, Fenwei; Sidiras, Evangelos

    The demand for more sustainable development promotes the need for components and steel structures with a longer useful life and better performance. Upgrade of wear steel plate used in key industry segments such as mining, recycling and road building results in the stable growth of global market with high quality grade Q&T wear plates (Hardness HBW≥400, and Yield strength ≥690 Mpa). SSAB has now expanded its wear steel product range by both thicker and thinner Q&T plate to meet the needs of the market, and can offer wear plates from 0.7 mm to 160 mm. The continuous research and development is being done to offer even thicker plates. This article introduces the performance and advantages of high quality grade Q&T wear resistant steel products (plate, strip, tube and round bars) produced in SSAB, and also describes typical applications in some industrial segments such as material handling and construction machinery.

  14. A Metallurgical Evaluation of the Powder-Bed Laser Additive Manufactured 4140 Steel Material

    NASA Astrophysics Data System (ADS)

    Wang, Wesley; Kelly, Shawn

    2016-03-01

    Using laser powder bed fusion (PBF-L) additive manufacturing (AM) process for steel or iron powder has been attempted for decades. This work used a medium carbon steel (AISI 4140) powder to explore the feasibility of AM. The high carbon equivalent of 4140 steel (CEIIW ≈ 0.83) has a strong tendency toward cold cracking. As such, the process parameters must be carefully controlled to ensure the AM build quality. Through an orthogonally designed experimental matrix, a laser-welding procedure was successfully developed to produce 4140 steel AM builds with no welding defects. In addition, the microstructure and micro-cleanliness of the as-welded PBF-L AM builds were also examined. The results showed an ultra-fine martensite lath structure and an ultra-clean internal quality with minimal oxide inclusion distribution. After optimizing the PBF-L AM process parameters, including the laser power and scan speed, the as-welded AM builds yielded an average tensile strength higher than 1482 MPa and an average 33 J Charpy V-notch impact toughness at -18°C. The surface quality, tensile strength, and Charpy V-notch impact toughness of AM builds were comparable to the wrought 4140 steel. The excellent mechanical properties of 4140 steel builds created by the PBF-L AM AM process make industrial production more feasible, which shows great potential for application in the aerospace, automobile, and machinery industries.

  15. Part II. Hydrothermal steel slag valorization: hydrogen and nano-magnetite production

    NASA Astrophysics Data System (ADS)

    Crouzet, Camille; Brunet, Fabrice; Recham, Nadir; Auzende, Anne-Line; Findling, Nathaniel; Magnin, Valérie; Ferrasse, Jean-Henry; Goffé, Bruno

    2017-10-01

    The effect of acidic conditions (in a pH range of 3 to 6) and temperature on the kinetics of the hydrothermal oxidation of ferrous iron contained in BOF steel slag has been tested in the 150 – 350°C range for acid acetic concentrations from 0 to 4M. Reaction progress was monitored with the amount of produced H2. Higher temperature and lower pH are found to enhance the hydrothermal oxidation kinetics of the slag. These two parameters are believed to increase iron dissolution rate which has already been identified as the rate limiting step of the hydrothermal oxidation of pure FeO. An activation energy of 28 × 4 kJ/mole is found for the hydrothermal oxidation of the steel slag which compares very well with that of pure FeO under similar conditions. In the case of the slag run in water at 300°C for 70.5 hours, magnetite product has been separated magnetically and characterized. Particles were found to fall in three size ranges: 10 – 30 nm, 100 – 300 nm and 1 – 10 µm. The smallest fraction (10 – 30 nm) is comparable to the 10 – 20 nm size range that is achieved when nanomagnetite are synthesized by co-precipitation methods. Obviously, the production of nanomagnetite enhances the economic interest of the hydrothermal processing of steel slags, which has already proven its capacity to produce high-purity H2.

  16. 76 FR 3613 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Final Results of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-01-20

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-580-818] Corrosion-Resistant Carbon... corrosion-resistant carbon steel flat products (CORE) from the Republic of Korea (Korea) for the period of review (POR) January 1, 2008, through December 31, 2008. See Corrosion-Resistant Carbon Steel Flat...

  17. Cancer incidence among Finnish ferrochromium and stainless steel production workers in 1967-2011: a cohort study.

    PubMed

    Huvinen, Markku; Pukkala, Eero

    2013-11-19

    The aim of the study was to assess the risk of cancer among workers employed in the Finnish ferrochromium and stainless steel industry since the beginning of production in 1967. The study cohort was made up of all persons employed by the Finnish stainless steel production chain from chromite mining to cold rolling of stainless steel during the period 1967-2004, and it was divided into subcohorts by production units with specific exposure patterns of the subcohorts assessed in previous studies. Follow-up for cancer through the files of the Finnish Cancer Registry was performed using the personal identity code as key. Standardised incidence ratios (SIRs) were calculated as the ratios of observed numbers of cancer cases and numbers expected on the basis of incidence rates in the population of the same region. The overall cancer incidence was at the expected level. The lung cancer risk was decreased in the whole cohort (SIR 0.79; 95% CI 0.65 to 1.08). The incidence of prostate cancer was significantly increased (1.31; 1.05 to 1.61) and that for kidney cancer was significantly decreased (0.38; 0.14 to 0.82). None of the department-specific SIRs for lung cancer were significantly different from 1.0. No cancers of the nose and nasal sinuses were observed among workers in the ferrochromium smelter or the stainless steel melting shop. It is not likely that the occupational exposures in the Finnish ferrochromium and stainless steel industry would have increased the risk of cancer.

  18. Advances in Energy Conservation of China Steel Industry

    PubMed Central

    Sun, Wenqiang; Cai, Jiuju; Ye, Zhu

    2013-01-01

    The course, technical progresses, and achievements of energy conservation of China steel industry (CSI) during 1980–2010 were summarized. Then, the paper adopted e-p method to analyze the variation law and influencing factors of energy consumptions of large- and medium-scale steel plants within different stages. It is pointed out that energy consumption per ton of crude steel has been almost one half lower in these thirty years, with 60% as direct energy conservation owing to the change of process energy consumption and 40% as indirect energy conservation attributed to the adjustment of production structure. Next, the latest research progress of some key common technologies in CSI was introduced. Also, the downtrend of energy consumption per ton of crude steel and the potential energy conservation for CSI during 2011–2025 were forecasted. Finally, it is indicated that the key topic of the next 15 years' research on the energy conservation of CSI is the synergistic operation of material flow and energy flow. It could be achieved by the comprehensive study on energy flow network optimization, such as production, allocation, utilization, recovery, reuse, and resource, according to the energy quantity, quality, and user demand following the first and second laws of thermodynamics. PMID:23533344

  19. Advances in energy conservation of China steel industry.

    PubMed

    Sun, Wenqiang; Cai, Jiuju; Ye, Zhu

    2013-01-01

    The course, technical progresses, and achievements of energy conservation of China steel industry (CSI) during 1980-2010 were summarized. Then, the paper adopted e-p method to analyze the variation law and influencing factors of energy consumptions of large- and medium-scale steel plants within different stages. It is pointed out that energy consumption per ton of crude steel has been almost one half lower in these thirty years, with 60% as direct energy conservation owing to the change of process energy consumption and 40% as indirect energy conservation attributed to the adjustment of production structure. Next, the latest research progress of some key common technologies in CSI was introduced. Also, the downtrend of energy consumption per ton of crude steel and the potential energy conservation for CSI during 2011-2025 were forecasted. Finally, it is indicated that the key topic of the next 15 years' research on the energy conservation of CSI is the synergistic operation of material flow and energy flow. It could be achieved by the comprehensive study on energy flow network optimization, such as production, allocation, utilization, recovery, reuse, and resource, according to the energy quantity, quality, and user demand following the first and second laws of thermodynamics.

  20. 75 FR 27297 - Certain Hot-Rolled Carbon Steel Flat Products from India: Notice of Final Results of Antidumping...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-05-14

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-533-820] Certain Hot-Rolled Carbon...'') published the preliminary results of the antidumping duty administrative review for certain hot-rolled carbon steel flat products from India (``Indian Hot-Rolled''). See Certain Hot-Rolled Carbon Steel Flat...

  1. Effect of process parameters on formability of laser melting deposited 12CrNi2 alloy steel

    NASA Astrophysics Data System (ADS)

    Peng, Qian; Dong, Shiyun; Kang, Xueliang; Yan, Shixing; Men, Ping

    2018-03-01

    As a new rapid prototyping technology, the laser melting deposition technology not only has the advantages of fast forming, high efficiency, but also free control in the design and production chain. Therefore, it has drawn extensive attention from community.With the continuous improvement of steel performance requirements, high performance low-carbon alloy steel is gradually integrated into high-tech fields such as aerospace, high-speed train and armored equipment.However, it is necessary to further explore and optimize the difficult process of laser melting deposited alloy steel parts to achieve the performance and shape control.This article took the orthogonal experiment on alloy steel powder by laser melting deposition ,and revealed the influence rule of the laser power, scanning speed, powder gas flow on the quality of the sample than the dilution rate, surface morphology and microstructure analysis were carried out.Finally, under the optimum technological parameters, the Excellent surface quality of the alloy steel forming part with high density, no pore and cracks was obtained.

  2. The effect of microstructure on the sheared edge quality and hole expansion ratio of hot-rolled 700 MPa steel

    NASA Astrophysics Data System (ADS)

    Kaijalainen, A.; Kesti, V.; Vierelä, R.; Ylitolva, M.; Porter, D.; Kömi, J.

    2017-09-01

    The effects of microstructure on the cutting and hole expansion properties of three thermomechanically rolled steels have been investigated. The yield strength of the studied 3 mm thick strip steels was approximately 700 MPa. Detailed microstructural studies using laser scanning confocal microscopy (LCSM), FESEM and FESEM-EBSD revealed that the three investigated materials consist of 1) single-phase polygonal ferrite, 2) polygonal ferrite with precipitates and 3) granular bainite. The quality of mechanically sheared edges were evaluated using visual inspection and LSCM, while hole expansion properties were characterised according to the methods described in ISO 16630. Roughness values (Ra and Rz) of the sheet edge with different cutting clearances varied between 12 µm to 21 µm and 133 µm to 225 µm, respectively. Mean hole expansion ratios varied from 28.4% to 40.5%. It was shown that granular bainite produced the finest cutting edge, but the hole expansion ratio remained at the same level as in the steel comprising single-phase ferrite. This indicates that a single-phase ferritic matrix enhances hole expansion properties even with low quality edges. A brief discussion of the microstructural features controlling the cutting quality and hole expansion properties is given.

  3. Accumulation of radioactive corrosion products on steel surfaces of VVER type nuclear reactors. I. 110mAg

    NASA Astrophysics Data System (ADS)

    Hirschberg, Gábor; Baradlai, Pál; Varga, Kálmán; Myburg, Gerrit; Schunk, János; Tilky, Péter; Stoddart, Paul

    Formation, presence and deposition of corrosion product radionuclides (such as 60Co, 51Cr, 54Mn, 59Fe and/or 110mAg) in the primary circuits of water-cooled nuclear reactors (PWRs) throw many obstacles in the way of normal operation. During the course of the work presented in this series, accumulations of such radionuclides have been studied at austenitic stainless steel type 08X18H10T (GOST 5632-61) surfaces (this austenitic stainless steel corresponds to AISI 321). Comparative experiments have been performed on magnetite-covered carbon steel (both materials are frequently used in some Soviet VVER type PWRs). For these laboratory-scale investigations a combination of the in situ radiotracer `thin gap' method and voltammetry is considered to be a powerful tool due to its high sensitivity towards the detection of the submonolayer coverages of corrosion product radionuclides. An independent technique (XPS) is also used to characterize the depth distribution and chemical state of various contaminants in the passive layer formed on austenitic stainless steel. In the first part of the series the accumulation of 110mAg has been investigated. Potential dependent sorption of Ag + ions (cementation) is found to be the predominant process on austenitic steel, while in the case of magnetite-covered carbon steel the silver species are mainly depleted in the form of Ag 2O. The XPS depth profile of Ag gives an evidence about the embedding of metallic silver into the entire passive layer of the austenitic stainless steel studied.

  4. Steel Industry Analysis Brief

    EIA Publications

    2009-01-01

    The steel industry is critical to the U.S. economy. Steel is the material of choice for many elements of construction, transportation, manufacturing, and a variety of consumer products. It is the backbone of bridges, skyscrapers, railroads, automobiles, and appliances. Most grades of steel used today - particularly high-strength steels that are lighter and more versatile - were not available a decade ago.

  5. Network-based production quality control

    NASA Astrophysics Data System (ADS)

    Kwon, Yongjin; Tseng, Bill; Chiou, Richard

    2007-09-01

    This study investigates the feasibility of remote quality control using a host of advanced automation equipment with Internet accessibility. Recent emphasis on product quality and reduction of waste stems from the dynamic, globalized and customer-driven market, which brings opportunities and threats to companies, depending on the response speed and production strategies. The current trends in industry also include a wide spread of distributed manufacturing systems, where design, production, and management facilities are geographically dispersed. This situation mandates not only the accessibility to remotely located production equipment for monitoring and control, but efficient means of responding to changing environment to counter process variations and diverse customer demands. To compete under such an environment, companies are striving to achieve 100%, sensor-based, automated inspection for zero-defect manufacturing. In this study, the Internet-based quality control scheme is referred to as "E-Quality for Manufacturing" or "EQM" for short. By its definition, EQM refers to a holistic approach to design and to embed efficient quality control functions in the context of network integrated manufacturing systems. Such system let designers located far away from the production facility to monitor, control and adjust the quality inspection processes as production design evolves.

  6. 78 FR 64473 - Certain Hot-Rolled Carbon Steel Flat Products From the People's Republic of China: Final No...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-10-29

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-570-865] Certain Hot-Rolled Carbon... review of the antidumping duty order on certain hot- rolled carbon steel flat products (``hot-rolled... of subject merchandise to the United States during the POR. \\1\\ See Certain Hot-Rolled Carbon Steel...

  7. 78 FR 34340 - Welded Carbon Steel Standard Pipe and Tube Products From Turkey: Preliminary Results of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-06-07

    ... Pipe and Tube Products From Turkey: Preliminary Results of Antidumping Duty Administrative Review; 2011... tube products (welded pipe and tube) from Turkey.\\2\\ The period of review is May 1, 2011, to April 30... order. See Antidumping Duty Order; Welded Carbon Steel Standard Pipe and Tube Products from Turkey, 51...

  8. 75 FR 10207 - Certain Cut-to-Length Carbon-Quality Steel Plate From the Republic of Korea: Final Results of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-03-05

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-836] Certain Cut-to-Length Carbon... cut-to-length carbon-quality steel plate from the Republic of Korea and the intent to rescind the... results of the administrative review of the antidumping duty order on certain cut-to-length carbon-quality...

  9. 75 FR 1495 - Certain Hot-Rolled Carbon Steel Flat Products From India: Preliminary Results of Countervailing...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-01-11

    ...The Department of Commerce (the Department) is conducting an administrative review of the countervailing duty (CVD) order on certain hot-rolled carbon steel flat products from India for the period of review (POR) January 1, 2008, through December 31, 2008. These preliminary results cover one company Tata Steel Limited (Tata). For the information on the net subsidy rate for the reviewed company, see the ``Preliminary Results of Review'' section.

  10. Data Envelopment Analysis for steel production with the use of Total Material Requirement

    NASA Astrophysics Data System (ADS)

    Oyaizu, Akira; Cravioto, Jordi; Yamasue, Eiji; Daigo, Ichiro

    2018-06-01

    High properties of stainless steels can be achieved by adding alloying elements and/or by structure control through complex heat treatments. Evaluations of such processes have so far been made in terms of the carbon dioxide emissions emitted or the energy consumption, but less attention has been given to resource intensity and "hidden flows". Using Data Envelopment Analysis (DEA), this study evaluates the efficiency of the environmental impact, characterised through Total Material Requirement (TMR), a measurement of hidden flows, and three properties (two mechanical and one chemical) of the materials obtained after manufacturing. Out of sample of 72 stainless steels it was found that seven (SUS312L, SUS836L, SUS447J1, SUSXM27, SUS410, SUS420F2, and SUS329J4L) showed the highest comparative efficiency, and that, when classifying the sample into four groups, the production of martensitic steels showed the highest efficiency (88%), followed by ferritic and duplex (82.6% each) and lastly austenitic (43.3%).

  11. Effect of steel structure and defects on reliability of parts of impact mechanisms

    NASA Astrophysics Data System (ADS)

    Popelyukh, AI; Repin, AA; Alekseev, SE

    2018-03-01

    The paper discusses selection of materials suitable for manufacturing critical parts of impact mechanisms. It is shown that in order to extend life of parts exposed to high dynamic loading, it is expedient to use medium- and high-carbon alloy-treated steels featuring low impurity with nonmetallic inclusions and high hardening characteristics. Application of thermally untreated parts is undesirable as steel having ferrite–pearlite structure possesses low fatigue strength. Aimed to ensure high reliability of parts with a hardness of 42–55 HRC, steel should be reinforced by thermal treatement with the formation of multicomponent martensite–bainite structure. High-quality production should include defectoscopy and incoming material control.

  12. 77 FR 64473 - Circular Welded Carbon-Quality Steel Pipe From the Sultanate of Oman: Final Affirmative...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-10-22

    ...-Quality Steel Pipe From the Sultanate of Oman: Final Affirmative Countervailing Duty Determination AGENCY... Sultanate of Oman (``Oman''). DATES: Effective Date: October 22, 2012. FOR FURTHER INFORMATION CONTACT... Sultanate of Oman (``GSO'') on April 5, April 20, and May 10, 2012. We received the GSO's responses...

  13. [Studies on the recovery of pharmaceutical drug substances from surfaces made of defined stainless-steel alloys].

    PubMed

    Kloss, S; Müller, U; Oelschläger, H

    2005-09-01

    Facilities for the manufacturing of pharmaceutical drug substances on the pilot-plant and the industrial scale as well as chemical reactors and vessels used for chemical work-up mainly consist of alloyed stainless steel. The influence of the alloy composition and the surface condition, i.e. of the roughness of the stainless-steel materials, on the adsorption of structurally diverse steroidal substances and, hence, on the quality of the products was studied. In general, stainless-steel alloys with smooth, not so rough surfaces are to be favored as reactor material. However, it was demonstrated in this study that, on account of the weak interaction between active substances and steel materials, mechanically polished materials of a medium roughness up to approx. 0.4 microm can be employed instead of the considerably more cost-intensive electrochemically polished stainless-steel surfaces. The type of surface finishing up to a defined roughness, then, has no influence on the quality of these pharmaceutical products. Substances that, because of their molecular structure, can function as "anions" in the presence of polar solvents, are adsorbed on very smooth surfaces prepared by electrochemical methods, forming an amorphous surface film. For substances with this structural characteristics, the lower-cost mechanically polished reactor materials of a medium roughness up to approx. 0.5 microm should be used exclusively.

  14. Tool life and cutting speed for the maximum productivity at the drilling of the stainless steel X22CrMoV12-1

    NASA Astrophysics Data System (ADS)

    Vlase, A.; Blăjină, O.; Iacob, M.; Darie, V.

    2015-11-01

    Two addressed issues in the research regarding the cutting machinability, establishing of the optimum cutting processing conditions and the optimum cutting regime, do not yet have sufficient data for solving. For this reason, in the paper it is proposed the optimization of the tool life and the cutting speed at the drilling of a certain stainless steel in terms of the maximum productivity. For this purpose, a nonlinear programming mathematical model to maximize the productivity at the drilling of the steel is developed in the paper. The optimum cutting tool life and the associated cutting tool speed are obtained by solving the numerical mathematical model. Using this proposed model allows increasing the accuracy in the prediction of the productivity for the drilling of a certain stainless steel and getting the optimum tool life and the optimum cutting speed for the maximum productivity. The results presented in this paper can be used in the production activity, in order to increase the productivity of the stainless steels machining. Also new research directions for the specialists in this interested field may come off from this paper.

  15. 76 FR 78887 - Circular Welded Carbon Quality Steel Pipe From the People's Republic of China: Rescission of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-12-20

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-570-911] Circular Welded Carbon Quality Steel Pipe From the People's Republic of China: Rescission of Countervailing Duty Administrative Review AGENCY: Import Administration, International Trade Administration, Department of Commerce. DATES: Effective Date: December 20, 2011. FOR...

  16. 75 FR 71672 - Circular Welded Carbon Quality Steel Pipe From the People's Republic of China: Rescission of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-11-24

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-570-911] Circular Welded Carbon Quality Steel Pipe From the People's Republic of China: Rescission of Countervailing Duty Administrative Review AGENCY: Import Administration, International Trade Administration, Department of Commerce. DATES: Effective Date: November 24, 2010. FOR...

  17. 78 FR 40429 - Certain Hot-Rolled Carbon Steel Flat Products From India: Rescission of Countervailing Duty...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-07-05

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-533-821] Certain Hot-Rolled Carbon Steel Flat Products From India: Rescission of Countervailing Duty Administrative Review; 2012 AGENCY...

  18. Symbiosis of Steel, Energy, and CO2 Evolution in Korea

    NASA Astrophysics Data System (ADS)

    Lee, Hyunjoung; Matsuura, Hiroyuki; Sohn, Il

    2016-09-01

    This study looks at the energy intensity of the steel industry and the greenhouse gas intensity involved with the production of steel. Using several sources of steel production data and the corresponding energy sources used provides a time-series analysis of the greenhouse gas (GHG) and energy intensity from 1990 to 2014. The impact of the steel economy with the gross domestic product (GDP) provides indirect importance of the general manufacturing sector within Korea and in particular the steel industry. Beyond 2008, the shift in excess materials production and significant increase in total imports have led to an imbalance in the Korean steel market and continue to inhibit the growth of the domestic steel market. The forecast of the GHG and energy intensity along with the steel production up to 2030 is provided using the auto regressive integrated moving average analysis.

  19. Fluid Force-Induced Detachment Criteria for Nonmetallic Inclusions Adhered to a Refractory/Molten Steel Interface

    NASA Astrophysics Data System (ADS)

    Dieguez Salgado, Uxia; Weiß, Christian; Michelic, Susanne K.; Bernhard, Christian

    2018-05-01

    Since nonmetallic inclusions (NMIs) in steel cannot be completely avoided, a greater understanding of their development and evolution during the steelmaking process is required. In particular, this includes the adhesion of microinclusions to the refractory/steel interface in the flow control system between the tundish and the mold. This phenomenon, commonly referred to as clogging, causes losses in productivity and product quality. Inclusions transported from the bulk melt to the boundary layer may adhere to the refractory/steel interface due to formation of a fluid cavity. A detailed model was derived for the detachment of NMIs adhering to a nozzle wall and is based on the local hydrodynamic conditions combined with the specific interfacial properties in the system consisting of the inclusions, the refractories, and the steel. The model is evaluated for three different application-oriented cases. This study has been focused on providing a better understanding of fluid flow in the near-wall region in order to reduce clogging during steelmaking.

  20. Simple Heat Treatment for Production of Hot-Dip Galvanized Dual Phase Steel Using Si-Al Steels

    NASA Astrophysics Data System (ADS)

    Equihua-Guillén, F.; García-Lara, A. M.; Muñíz-Valdes, C. R.; Ortíz-Cuellar, J. C.; Camporredondo-Saucedo, J. E.

    2014-01-01

    This work presents relevant metallurgical considerations to produce galvanized dual phase steels from low cost aluminum-silicon steels which are produced by continuous strip processing. Two steels with different contents of Si and Al were austenized in the two-phase field ferrite + austenite (α + γ) in a fast manner to obtain dual phase steels, suitable for hot-dip galvanizing process, under typical parameters of continuous annealing processing line. Tensile dual phase properties were obtained from specimens cooled from temperature below Ar3, held during 3 min, intermediate cooling at temperature above Ar1 and quenching in Zn bath at 465 °C. The results have shown typical microstructure and tensile properties of galvanized dual phase steels. Finally, the synergistic effect of aluminum, silicon, and residual chromium on martensite start temperature ( M s), critical cooling rate ( C R), volume fraction of martensite, and tensile properties has been studied.

  1. Management of MSW in Spain and recovery of packaging steel scrap.

    PubMed

    Tayibi, Hanan; Peña, Carmen; López, Félix A; López-Delgado, Aurora

    2007-01-01

    Packaging steel is more advantageously recovered and recycled than other packaging material due to its magnetic properties. The steel used for packaging is of high quality, and post-consumer waste therefore produces high-grade ferrous scrap. Recycling is thus an important issue for reducing raw material consumption, including iron ore, coal and energy. Household refuse management consists of collection/disposal, transport, and processing and treatment - incineration and composting being the most widely used methods in Spain. Total Spanish MSW production exceeds 21 million tons per year, of which 28.1% and 6.2% are treated in compost and incineration plants, respectively. This paper presents a comprehensive study of incineration and compost plants in Spain, including a review of the different processes and technologies employed and the characteristics and quality of the recovered ferrous scrap. Of the total amount of packaging steel scrap recovered from MSW, 38% comes from compost plants and 14% from incineration plants. Ferrous scrap from incineration plants presents a high degree of chemical alteration as a consequence of the thermal process to which the MSW is subjected, particularly the conditions in which the slag is cooled, and accordingly its quality diminishes. Fragmentation and magnetic separation processes produce an enhancement of the scrap quality. Ferrous scrap from compost plants has a high tin content, which negatively affects its recycling. Cleaning and detinning processes are required prior to recycling.

  2. Development of High Heat Input Welding High Strength Steel Plate for Oil Storage Tank in Xinyu Steel Company

    NASA Astrophysics Data System (ADS)

    Zhao, Hemin; Dong, Fujun; Liu, Xiaolin; Xiong, Xiong

    This essay introduces the developed high-heat input welding quenched and tempered pressure vessel steel 12MnNiVR for oil storage tank by Xinyu Steel, which passed the review by the Boiler and Pressure Vessel Standards Technical Committee in 2009. The review comments that compared to the domestic and foreign similar steel standard, the key technical index of enterprise standard were in advanced level. After the heat input of 100kJ/cm electro-gas welding, welded points were still with excellent low temperature toughness at -20°C. The steel plate may be constructed for oil storage tank, which has been permitted by thickness range from 10 to 40mm, and design temperature among -20°C-100°C. It studied microstructure genetic effects mechanical properties of the steel. Many production practices indicated that the mechanical properties of products and the steel by stress relief heat treatment of steel were excellent, with pretreatment of hot metal, converter refining, external refining, protective casting, TMCP and heat treatment process measurements. The stability of performance and matured technology of Xinyu Steel support the products could completely service the demand of steel constructed for 10-15 million cubic meters large oil storage tank.

  3. [Characteristic of Mercury Emissions and Mass Balance of the Typical Iron and Steel Industry].

    PubMed

    Zhang, Ya-hui; Zhang, Cheng; Wang, Ding-yong; Luo, Cheng-zhong; Yang, Xi; Xu, Feng

    2015-12-01

    To preliminarily discuss the mercury emission characteristics and its mass balance in each process of the iron and steel production, a typical iron and steel enterprise was chosen to study the total mercury in all employed materials and estimate the input and output of mercury during the steel production process. The results showed that the mercury concentrations of input materials in each technology ranged 2.93-159.11 µg · kg⁻¹ with the highest level observed in ore used in blast furnace, followed by coal of sintering and blast furnace. The mercury concentrations of output materials ranged 3.09-18.13 µg · kg⁻¹ and the mercury concentration of dust was the highest, followed by converter slag. The mercury input and the output in the coking plant were 1346.74 g · d⁻¹ ± 36.95 g · d⁻¹ and 177.42 g · d⁻¹ ± 13.73 g · d⁻¹, respectively. In coking process, mercury mainly came from the burning of coking coal. The sintering process was the biggest contributor for mercury input during the iron and steel production with the mercury input of 1075. 27 g · d⁻¹ ± 60.89 g · d⁻¹ accounting for 68.06% of the total mercury input during this production process, and the ore powder was considered as the main mercury source. For the solid output material, the output in the sintering process was 14.15 g · d⁻¹ ± 0.38 g · d⁻¹, accounting for 22.61% of the total solid output. The mercury emission amount from this studied iron and steel enterprise was estimated to be 553.83 kg in 2013 with the emission factor of 0.092 g · t⁻¹ steel production. Thus, to control the mercury emissions, iron and steel enterprises should combine with production practice, further reduce energy consumption of coking and sintering, or improve the quality of raw materials and reduce the input of mercury.

  4. 78 FR 79665 - Welded Carbon Steel Standard Pipe and Tube Products From Turkey: Final Results of Antidumping...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-12-31

    ... Pipe and Tube Products From Turkey: Final Results of Antidumping Duty Administrative Review; 2011-2012... pipe and tube products (welded pipe and tube) from Turkey.\\1\\ The period of review (POR) is May 1, 2011... during the POR.\\2\\ \\1\\ See Welded Carbon Steel Standard Pipe and Tube Products from Turkey: Preliminary...

  5. 78 FR 72863 - Circular Welded Carbon Quality Steel Pipe From the People's Republic of China: Continuation of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-12-04

    ... Quality Steel Pipe From the People's Republic of China: Continuation of Countervailing Duty Order AGENCY...) from the People's Republic of China (PRC) would likely lead to continuation or recurrence of net... reasonably foreseeable time.\\3\\ \\1\\ See Initiation of Five-Year (``Sunset'') Review, 78 FR 33063 (June 3...

  6. Quality transitivity and traceability system of herbal medicine products based on quality markers.

    PubMed

    Liu, Changxiao; Guo, De-An; Liu, Liang

    2018-05-15

    Due to a variety of factors to affect the herb quality, the existing quality management model is unable to evaluate the process control. The development of the concept of "quality marker" (Q-marker) lays basis for establishing an independent process quality control system for herbal products. To ensure the highest degree of safety, effectiveness and quality process control of herbal products, it is aimed to establish a quality transitivity and traceability system of quality and process control from raw materials to finished herbal products. Based on the key issues and challenges of quality assessment, the current status of quality and process controls from raw materials to herbal medicinal products listed in Pharmacopoeia were analyzed and the research models including discovery and identification of Q-markers, analysis and quality management of risk evaluation were designed. Authors introduced a few new technologies and methodologies, such as DNA barcoding, chromatographic technologies, fingerprint analysis, chemical markers, bio-responses, risk management and solution for quality process control. The quality and process control models for herbal medicinal products were proposed and the transitivity and traceability system from raw materials to the finished products was constructed to improve the herbal quality from the entire supply and production chain. The transitivity and traceability system has been established based on quality markers, especially on how to control the production process under Good Engineering Practices, as well as to implement the risk management for quality and process control in herbal medicine production. Copyright © 2018 Elsevier GmbH. All rights reserved.

  7. Responses of Microbial Community Composition to Temperature Gradient and Carbon Steel Corrosion in Production Water of Petroleum Reservoir.

    PubMed

    Li, Xiao-Xiao; Yang, Tao; Mbadinga, Serge M; Liu, Jin-Feng; Yang, Shi-Zhong; Gu, Ji-Dong; Mu, Bo-Zhong

    2017-01-01

    Oil reservoir production systems are usually associated with a temperature gradient and oil production facilities frequently suffer from pipeline corrosion failures. Both bacteria and archaea potentially contribute to biocorrosion of the oil production equipment. Here the response of microbial populations from the petroleum reservoir to temperature gradient and corrosion of carbon steel coupons were investigated under laboratory condition. Carbon steel coupons were exposed to production water from a depth of 1809 m of Jiangsu petroleum reservoir (China) and incubated for periods of 160 and 300 days. The incubation temperatures were set at 37, 55, and 65°C to monitoring mesophilic, thermophilic and hyperthermophilic microorganisms associated with anaerobic carbon steel corrosion. The results showed that corrosion rate at 55°C (0.162 ± 0.013 mm year -1 ) and 37°C (0.138 ± 0.008 mm year -1 ) were higher than that at 65°C (0.105 ± 0.007 mm year -1 ), and a dense biofilm was observed on the surface of coupons under all biotic incubations. The microbial community analysis suggests a high frequency of bacterial taxa associated with families Porphyromonadaceae, Enterobacteriaceae, and Spirochaetaceae at all three temperatures. While the majority of known sulfate-reducing bacteria, in particular Desulfotignum , Desulfobulbus and Desulfovibrio spp., were predominantly observed at 37°C; Desulfotomaculum spp., Thermotoga spp. and Thermanaeromonas spp. as well as archaeal members closely related to Thermococcus and Archaeoglobus spp. were substantially enriched at 65°C. Hydrogenotrophic methanogens of the family Methanobacteriaceae were dominant at both 37 and 55°C; acetoclastic Methanosaeta spp. and methyltrophic Methanolobus spp. were enriched at 37°C. These observations show that temperature changes significantly alter the microbial community structure in production fluids and also affected the biocorrosion of carbon steel under anaerobic conditions.

  8. Responses of Microbial Community Composition to Temperature Gradient and Carbon Steel Corrosion in Production Water of Petroleum Reservoir

    PubMed Central

    Li, Xiao-Xiao; Yang, Tao; Mbadinga, Serge M.; Liu, Jin-Feng; Yang, Shi-Zhong; Gu, Ji-Dong; Mu, Bo-Zhong

    2017-01-01

    Oil reservoir production systems are usually associated with a temperature gradient and oil production facilities frequently suffer from pipeline corrosion failures. Both bacteria and archaea potentially contribute to biocorrosion of the oil production equipment. Here the response of microbial populations from the petroleum reservoir to temperature gradient and corrosion of carbon steel coupons were investigated under laboratory condition. Carbon steel coupons were exposed to production water from a depth of 1809 m of Jiangsu petroleum reservoir (China) and incubated for periods of 160 and 300 days. The incubation temperatures were set at 37, 55, and 65°C to monitoring mesophilic, thermophilic and hyperthermophilic microorganisms associated with anaerobic carbon steel corrosion. The results showed that corrosion rate at 55°C (0.162 ± 0.013 mm year-1) and 37°C (0.138 ± 0.008 mm year-1) were higher than that at 65°C (0.105 ± 0.007 mm year-1), and a dense biofilm was observed on the surface of coupons under all biotic incubations. The microbial community analysis suggests a high frequency of bacterial taxa associated with families Porphyromonadaceae, Enterobacteriaceae, and Spirochaetaceae at all three temperatures. While the majority of known sulfate-reducing bacteria, in particular Desulfotignum, Desulfobulbus and Desulfovibrio spp., were predominantly observed at 37°C; Desulfotomaculum spp., Thermotoga spp. and Thermanaeromonas spp. as well as archaeal members closely related to Thermococcus and Archaeoglobus spp. were substantially enriched at 65°C. Hydrogenotrophic methanogens of the family Methanobacteriaceae were dominant at both 37 and 55°C; acetoclastic Methanosaeta spp. and methyltrophic Methanolobus spp. were enriched at 37°C. These observations show that temperature changes significantly alter the microbial community structure in production fluids and also affected the biocorrosion of carbon steel under anaerobic conditions. PMID:29259586

  9. Quantifying Recycling and Losses of Cr and Ni in Steel Throughout Multiple Life Cycles Using MaTrace-Alloy.

    PubMed

    Nakamura, Shinichiro; Kondo, Yasushi; Nakajima, Kenichi; Ohno, Hajime; Pauliuk, Stefan

    2017-09-05

    Alloying metals are indispensable ingredients of high quality alloy steel such as austenitic stainless steel, the cyclical use of which is vital for sustainable resource management. Under the current practice of recycling, however, different metals are likely to be mixed in an uncontrolled manner, resulting in function losses and dissipation of metals with distinctive functions, and in the contamination of recycled steels. The latter could result in dilution loss, if metal scrap needed dilution with virgin iron to reduce the contamination below critical levels. Management of these losses resulting from mixing in repeated recycling of metals requires tracking of metals over multiple life cycles of products with compositional details. A new model (MaTrace-alloy) was developed that tracks the fate of metals embodied in each of products over multiple life cycles of products, involving accumulation, discard, and recycling, with compositional details at the level of both alloys and products. The model was implemented for the flow of Cr and Ni in the Japanese steel cycle involving 27 steel species and 115 final products. It was found that, under a high level of scrap sorting, greater than 70% of the initial functionality of Cr and Ni could be retained over a period of 100 years, whereas under a poor level of sorting, it could plunge to less than 30%, demonstrating the relevance of waste management technology in circular economy policies.

  10. Impact of the interaction of material production and mechanical processing on the magnetic properties of non-oriented electrical steel

    NASA Astrophysics Data System (ADS)

    Leuning, Nora; Steentjes, Simon; Stöcker, Anett; Kawalla, Rudolf; Wei, Xuefei; Dierdorf, Jens; Hirt, Gerhard; Roggenbuck, Stefan; Korte-Kerzel, Sandra; Weiss, Hannes A.; Volk, Wolfram; Hameyer, Kay

    2018-04-01

    Thin laminations of non-grain oriented (NO) electrical steels form the magnetic core of rotating electrical machines. The magnetic properties of these laminations are therefore key elements for the efficiency of electric drives and need to be fully utilized. Ideally, high magnetization and low losses are realized over the entire polarization and frequency spectrum at reasonable production and processing costs. However, such an ideal material does not exist and thus, achievable magnetic properties need to be deduced from the respective application requirements. Parameters of the electrical steel such as lamination thickness, microstructure and texture affect the magnetic properties as well as their polarization and frequency dependence. These structural features represent possibilities to actively alter the magnetic properties, e.g., magnetization curve, magnetic loss or frequency dependence. This paper studies the influence of production and processing on the resulting magnetic properties of a 2.4 wt% Si electrical steel. Aim is to close the gap between production influence on the material properties and its resulting effect on the magnetization curves and losses at different frequencies with a strong focus on occurring interdependencies between production and mechanical processing. The material production is realized on an experimental processing route that comprises the steps of hot rolling, cold rolling, annealing and punching.

  11. CRN5EXP: Expert system for statistical quality control

    NASA Technical Reports Server (NTRS)

    Hentea, Mariana

    1991-01-01

    The purpose of the Expert System CRN5EXP is to assist in checking the quality of the coils at two very important mills: Hot Rolling and Cold Rolling in a steel plant. The system interprets the statistical quality control charts, diagnoses and predicts the quality of the steel. Measurements of process control variables are recorded in a database and sample statistics such as the mean and the range are computed and plotted on a control chart. The chart is analyzed through patterns using the C Language Integrated Production System (CLIPS) and a forward chaining technique to reach a conclusion about the causes of defects and to take management measures for the improvement of the quality control techniques. The Expert System combines the certainty factors associated with the process control variables to predict the quality of the steel. The paper presents the approach to extract data from the database, the reason to combine certainty factors, the architecture and the use of the Expert System. However, the interpretation of control charts patterns requires the human expert's knowledge and lends to Expert Systems rules.

  12. Stainless steel corrosion scale formed in reclaimed water: Characteristics, model for scale growth and metal element release.

    PubMed

    Cui, Yong; Liu, Shuming; Smith, Kate; Hu, Hongying; Tang, Fusheng; Li, Yuhong; Yu, Kanghua

    2016-10-01

    Stainless steels generally have extremely good corrosion resistance, but are still susceptible to pitting corrosion. As a result, corrosion scales can form on the surface of stainless steel after extended exposure to aggressive aqueous environments. Corrosion scales play an important role in affecting water quality. These research results showed that interior regions of stainless steel corrosion scales have a high percentage of chromium phases. We reveal the morphology, micro-structure and physicochemical characteristics of stainless steel corrosion scales. Stainless steel corrosion scale is identified as a podiform chromite deposit according to these characteristics, which is unlike deposit formed during iron corrosion. A conceptual model to explain the formation and growth of stainless steel corrosion scale is proposed based on its composition and structure. The scale growth process involves pitting corrosion on the stainless steel surface and the consecutive generation and homogeneous deposition of corrosion products, which is governed by a series of chemical and electrochemical reactions. This model shows the role of corrosion scales in the mechanism of iron and chromium release from pitting corroded stainless steel materials. The formation of corrosion scale is strongly related to water quality parameters. The presence of HClO results in higher ferric content inside the scales. Cl - and SO 4 2- ions in reclaimed water play an important role in corrosion pitting of stainless steel and promote the formation of scales. Copyright © 2016. Published by Elsevier B.V.

  13. 76 FR 78615 - Circular Welded Carbon-Quality Steel Pipe From India, the Sultanate of Oman, the United Arab...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-12-19

    ...-810] Circular Welded Carbon-Quality Steel Pipe From India, the Sultanate of Oman, the United Arab..., the Sultanate of Oman (``Oman''), The United Arab Emirates (``the UAE''), and the Socialist Republic... Oman, the United Arab Emirates, and the Socialist Republic of Vietnam: Initiation of Countervailing...

  14. 76 FR 56797 - Cut-to-Length Carbon-Quality Steel Plate From India, Indonesia, Italy, Japan, and Korea; Revised...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-09-14

    ... INTERNATIONAL TRADE COMMISSION [Investigation Nos. 701-TA-388-391 and 731-TA-817-821 ;Second Review] Cut-to-Length Carbon-Quality Steel Plate From India, Indonesia, Italy, Japan, and Korea; Revised schedule for the subject reviews. AGENCY: United States International Trade Commission. ACTION: Notice...

  15. Identification of corrosion product on medium carbon steel under the exposure of Banda Aceh’s atmosphere

    NASA Astrophysics Data System (ADS)

    Thalib, Sulaiman; Ikhsan, Muharil; Fonna, Syarizal; Huzni, Syifaul; Ridha, Syahrir

    2018-05-01

    This research was conducted to study the form of corrosion products of medium carbon steel under the exposure of Banda Aceh’s atmosphere. The medium carbon steel samples which the size based on ASTM G 50 were exposed in open areas around the Engineering Faculty, Syiah Kuala University, Darussalam - Banda Aceh, Aceh province, Indonesia. The study was carried out from January through December 2016. The corrosion product formed on the surface of the samples was studied using X-ray Diffraction (XRD) and Scanning Electron Microscope (SEM) method. Measurements of weight loss due to atmospheric corrosion as a basis for calculating corrosion rates was referring to ASTM G1. Corrosion product found based on XRD analysis was lepidocrocite (FeO2, γ-FeOOH) and goethite (FeO2, α-FeOOH). The results agreed with SEM analysis that also indicates to lepidocrocite and goethite. The corrosion rate for twelve months showed that the highest rate occurs in the period of March-April that was 0.024 mpy. During twelve months exposure, the corrosion products consist of lepidocrocite and goethite. Significant changes began to occur in the eighth month, where the product of corrosion was almost entirely goethite.

  16. Operational CryoSat Product Quality Assessment

    NASA Astrophysics Data System (ADS)

    Mannan, Rubinder; Webb, Erica; Hall, Amanda; Bouzinac, Catherine

    2013-12-01

    The performance and quality of the CryoSat data products are routinely assessed by the Instrument Data quality Evaluation and Analysis Service (IDEAS). This information is then conveyed to the scientific and user community in order to allow them to utilise CryoSat data with confidence. This paper presents details of the Quality Control (QC) activities performed for CryoSat products under the IDEAS contract. Details of the different QC procedures and tools deployed by IDEAS to assess the quality of operational data are presented. The latest updates to the Instrument Processing Facility (IPF) for the Fast Delivery Marine (FDM) products and the future update to Baseline-C are discussed.

  17. Discussion on Coking Wastewater Treatment and Control Measures in Iron and Steel Enterprises

    NASA Astrophysics Data System (ADS)

    Zhang, Lei; Hwang, Jiannyang; Leng, Ting; Xue, Gaifeng; Wu, Gaoming

    According to the water quality characteristics of coking wastewater and the environmental protection requirements, the status of coking wastewater treatment technologies at home and abroad was described. Several methods and control measures of coking wastewater treatment were discussed in the effluent from iron and steel enterprises. It is an effective way to makes use of cleaner production technologies to reduce the amount of coking phenol cyanide wastewater produced from the source, and then adopt water supply for different water quality or series classification in-house according to the demand of water characters. It is necessary though looking for the available disposal way to reduce the coking wastewater effluent, which can provide a reference for process selection and research on treatment of coking wastewater in iron and steel enterprise.

  18. Wetting and Interfacial Reactivity of Zn-Coated Steel Products with Cu-Si, Cu-Sn and Al-Si Filler Metals for Laser Brazing Application

    NASA Astrophysics Data System (ADS)

    Koltsov, Alexey; Cretteur, Laurent

    2018-03-01

    The laser brazing process is successfully applied in automotive industry for joining of roofs and hatchbacks of vehicles. The bad wetting of the brazing alloy during the process can lead to the formation of random external porosities which are not allowed on visible parts. This paper describes the wettability and reactivity mechanisms at short contact time of Cu and Al matrix brazing alloys with different reactive elements (Si, Sn) on different steel products such as hot-dip galvanized steels, galvannealed steel and bare steel. Wetting experiments were carried out by the dispensed drop technique. The effects of alloying elements and brazing alloy matrix on interfacial reactivity are discussed. It was found that Cu matrix containing 3 wt.% Si is the most favorable for short time liquid/solid adhesion relatively to the other studied brazing alloy compositions. The brazing ability of different steel products is well correlated with the wettability and interfacial reactivity results.

  19. Microstructural characterization in dissimilar friction stir welding between 304 stainless steel and st37 steel

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Jafarzadegan, M.; State Key Laboratory of Advanced Welding Production Technology, School of Materials Science and Eng., Harbin Institute of Technology, P.O. Box: 150001, Harbin; Feng, A.H.

    2012-12-15

    In the present study, 3 mm-thick plates of 304 stainless steel and st37 steel were welded together by friction stir welding at a welding speed of 50 mm/min and tool rotational speed of 400 and 800 rpm. X-ray diffraction test was carried out to study the phases which might be formed in the welds. Metallographic examinations, and tensile and microhardness tests were used to analyze the microstructure and mechanical properties of the joint. Four different zones were found in the weld area except the base metals. In the stir zone of the 304 stainless steel, a refined grain structure withmore » some features of dynamic recrystallization was evidenced. A thermomechanically-affected zone was characterized on the 304 steel side with features of dynamic recovery. In the other side of the stir zone, the hot deformation of the st37 steel in the austenite region produced small austenite grains and these grains transformed to fine ferrite and pearlite and some products of displacive transformations such as Widmanstatten ferrite and martensite by cooling the material after friction stir welding. The heat-affected zone in the st37 steel side showed partially and fully refined microstructures like fusion welding processes. The recrystallization in the 304 steel and the transformations in the st37 steel enhanced the hardness of the weld area and therefore, improved the tensile properties of the joint. - Highlights: Black-Right-Pointing-Pointer FSW produced sound welds between st37 low carbon steel and 304 stainless steel. Black-Right-Pointing-Pointer The SZ of the st37 steel contained some products of allotropic transformation. Black-Right-Pointing-Pointer The material in the SZ of the 304 steel showed features of dynamic recrystallization. Black-Right-Pointing-Pointer The finer microstructure in the SZ increased the hardness and tensile strength.« less

  20. Scientific and Technological Principles of Development of New Cold-Resistant Arc-Steels (Steels for Arctic Applications)

    NASA Astrophysics Data System (ADS)

    Sych, O. V.; Khlusova, E. I.; Yashin, E. A.

    2017-12-01

    The paper presents the results of quantitative analysis of C, Mn, Ni and Cu content on strength and cold-resistance of rolled plates. Relations between the ferritic-bainitic structure morphology and anisotropy and steel performance characteristics have been established. Influence of thermal and deformation rolling patterns on steel structure has been studied. The steel chemical composition has been improved and precision thermomechanical processing conditions for production of cold-resistant Arc-steel plates have been developed.

  1. Electro-catalytic biodiesel production from canola oil in methanolic and ethanolic solutions with low cost stainless steel and hybrid ion-exchange resin grafted electrodes

    NASA Astrophysics Data System (ADS)

    Allioux, Francois-Marie; Holland, Brendan J.; Kong, Lingxue; Dumée, Ludovic F.

    2017-07-01

    Biodiesel is a growing alternative to petroleum fuels and is produced by the catalysed transesterification of fats in presence of an alcohol base. Transesterification processes using homogeneous catalysts are considered to be amongst the most efficient methods but rely on the feedstock quality and low water content in order to avoid undesirable saponification reactions. In this work, the electro-catalytic conversion of canola oil to biodiesel in a 1% aqueous methanolic and ethanolic reaction mixture was performed without the addition of external catalyst or co-solvent. An inexpensive stainless steel electrode and a hybrid stainless steel electrode coated with an ion-exchange resin catalyst were used as cathode materials while the anode was composed of a plain carbon paper. The cell voltages were varied from 10 to 40 V and the reaction temperature maintained at 20 or 40°C. The canola oil conversion rates were found to be superior at 40°C without saponification reactions for cell voltages below 30 V. The conversion rates were as high as 87% for the hybrid electrode and 81% for the plain stainless steel electrode. This work could inspire new process development for the conversion of high water content feedstock for the production of second-generation biodiesel.

  2. 7 CFR 58.142 - Product quality and stability.

    Code of Federal Regulations, 2010 CFR

    2010-01-01

    ... production of the highest quality of finished product and improve product stability. Milk should not be more... 7 Agriculture 3 2010-01-01 2010-01-01 false Product quality and stability. 58.142 Section 58.142... Procedures § 58.142 Product quality and stability. The receiving, holding and processing of milk and cream...

  3. High productivity injection practices at Rouge Steel

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Barker, D.H.; Hegler, G.L.; Falls, C.E.

    1995-12-01

    Rouge Steel Company, located in Dearborn, Michigan, operates two blast furnaces. The smaller of the pair, ``B`` Furnace, has a hearth diameter of 20 feet and 12 tuyeres. It has averaged 2,290 NTHM (net ton of hot metal) per day of 8.2 NTHM per 100 cubic feet of working volume. ``C`` Furnace has a hearth diameter of 29 feet and 20 tuyeres. Both of these furnaces are single tap hole furnaces. Prior to its reline in 1991, ``C`` Furnace was producing at a rate of 3,300 NTHM/day or about 6.25 NTHM/100 cfwv. In November, 1994 it averaged 5,106 NTHM/day ormore » 9.6 NTHM/100 cfwv. This paper discusses how the current production rates were achieved. Also, the areas that needed to be addressed as production increased will be described. These areas include casthouse arrangement and workload, hot metal ladle capacity, slag pot capacity and charging capability. Coupled with the high blast temperature capability, the furnace was provided with a new natural gas injection system that injected the gas through the blowpipes and a natural gas injection system to enrich the stove gas. Following the furnace reline, natural gas has been used in three ways: tuyere level control; combination injection; and stove gas enrichment. Coke consumption rate has also decreased per NTHM.« less

  4. Transformation process for production of ultrahigh carbon steels and new alloys

    DOEpatents

    Strum, M.J.; Goldberg, A.; Sherby, O.D.; Landingham, R.L.

    1995-08-29

    Ultrahigh carbon steels with superplastic properties are produced by heating a steel containing ferrite and carbide phases to a soaking temperature approximately 50 C above the A{sub 1} transformation temperature, soaking the steel above the A{sub 1} temperature for a sufficient time that the major portion of the carbides dissolve into the austenite matrix, and then cooling the steel in a controlled manner within predetermined limits of cooling rate or transformation temperature, to obtain a steel having substantially spheroidal carbides. New alloy compositions contain aluminum and solute additions which promote the formation of a fine grain size and improve the resistance of the carbides to coarsening at the forming temperature. 9 figs.

  5. Transformation process for production of ultrahigh carbon steels and new alloys

    DOEpatents

    Strum, Michael J.; Goldberg, Alfred; Sherby, Oleg D.; Landingham, Richard L.

    1995-01-01

    Ultrahigh carbon steels with superplastic properties are produced by heating a steel containing ferrite and carbide phases to a soaking temperature approximately 50.degree. C. above the A.sub.1 transformation temperature, soaking the steel above the A.sub.1 temperature for a sufficient time that the major portion of the carbides dissolve into the austenite matrix, and then cooling the steel in a controlled manner within predetermined limits of cooling rate or transformation temperature, to obtain a steel having substantially spheroidal carbides. New alloy compositions contain aluminum and solute additions which promote the formation of a fine grain size and improve the resistance of the carbides to coarsening at the forming temperature.

  6. 76 FR 12322 - Certain Cut-to-Length Carbon-Quality Steel Plate From India, Indonesia, Italy, Japan, and the...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-03-07

    ...-847, A-580-836] Certain Cut-to-Length Carbon-Quality Steel Plate From India, Indonesia, Italy, Japan...) from India, Indonesia, Italy, Japan, and the Republic of Korea, pursuant to section 751(c) of the... initiation of the second sunset reviews of the antidumping duty orders on CTL Plate from India, Indonesia...

  7. 76 FR 55004 - Certain Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Preliminary...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-09-06

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Certain Corrosion-Resistant...) is conducting the seventeenth administrative review of the antidumping order on corrosion-resistant carbon steel flat products (CORE) from the Republic of Korea \\1\\ (Korea). This review covers eight...

  8. Iron nutrition, biomass production, and plant product quality.

    PubMed

    Briat, Jean-François; Dubos, Christian; Gaymard, Frédéric

    2015-01-01

    One of the grand challenges in modern agriculture is increasing biomass production, while improving plant product quality, in a sustainable way. Of the minerals, iron (Fe) plays a major role in this process because it is essential both for plant productivity and for the quality of their products. Fe homeostasis is an important determinant of photosynthetic efficiency in algae and higher plants, and we review here the impact of Fe limitation or excess on the structure and function of the photosynthetic apparatus. We also discuss the agronomic, plant breeding, and transgenic approaches that are used to remediate Fe deficiency of plants on calcareous soils, and suggest ways to increase the Fe content and bioavailability of the edible parts of crops to improve human diet. Copyright © 2014 Elsevier Ltd. All rights reserved.

  9. Investigating the Evolution of Progressive Die Wear on Uncoated Dp1180 Steel in Production Environment

    NASA Astrophysics Data System (ADS)

    Wu, W.; Zhou, D. J.; Adamski, D. J.; Young, D.; Wang, Y. W.

    2017-09-01

    A study of die wear was performed using an uncoated dual phase, 1,180 MPa ultimate tensile strength steel (DP1180) in a progressive die. The objectives of the current study are to evaluate the die durability of various tooling materials and coatings for forming operations on uncoated DP1180 steel and update OEM’s die standards based on the experimental results in the real production environment. In total, 100,800 hits were performed in manufacturing production conditions, where 33 die inserts with the combination of 10 die materials and 9 coatings were investigated. The die inserts were evaluated for surface wear using scanning electron microscopy and characterized in terms of die material and/or coating defects, failure mode, failure initiation and propagation. Surface roughness of the formed parts was characterized using a WYKO NT110 machine. The analytical analysis of the die inserts and formed parts, combined with the failure mode and service life, provide a basis for die material and coating selection for forming AHSS components. The conclusions of this study will guide the selection of die material and coatings for high-volume production of AHSS components.

  10. Influence of raw milk quality on processed dairy products: How do raw milk quality test results relate to product quality and yield?

    PubMed

    Murphy, Steven C; Martin, Nicole H; Barbano, David M; Wiedmann, Martin

    2016-12-01

    This article provides an overview of the influence of raw milk quality on the quality of processed dairy products and offers a perspective on the merits of investing in quality. Dairy farmers are frequently offered monetary premium incentives to provide high-quality milk to processors. These incentives are most often based on raw milk somatic cell and bacteria count levels well below the regulatory public health-based limits. Justification for these incentive payments can be based on improved processed product quality and manufacturing efficiencies that provide the processor with a return on their investment for high-quality raw milk. In some cases, this return on investment is difficult to measure. Raw milks with high levels of somatic cells and bacteria are associated with increased enzyme activity that can result in product defects. Use of raw milk with somatic cell counts >100,000cells/mL has been shown to reduce cheese yields, and higher levels, generally >400,000 cells/mL, have been associated with textural and flavor defects in cheese and other products. Although most research indicates that fairly high total bacteria counts (>1,000,000 cfu/mL) in raw milk are needed to cause defects in most processed dairy products, receiving high-quality milk from the farm allows some flexibility for handling raw milk, which can increase efficiencies and reduce the risk of raw milk reaching bacterial levels of concern. Monitoring total bacterial numbers in regard to raw milk quality is imperative, but determining levels of specific types of bacteria present has gained increasing importance. For example, spores of certain spore-forming bacteria present in raw milk at very low levels (e.g., <1/mL) can survive pasteurization and grow in milk and cheese products to levels that result in defects. With the exception of meeting product specifications often required for milk powders, testing for specific spore-forming groups is currently not used in quality incentive programs in

  11. Assessing product image quality for online shopping

    NASA Astrophysics Data System (ADS)

    Goswami, Anjan; Chung, Sung H.; Chittar, Naren; Islam, Atiq

    2012-01-01

    Assessing product-image quality is important in the context of online shopping. A high quality image that conveys more information about a product can boost the buyer's confidence and can get more attention. However, the notion of image quality for product-images is not the same as that in other domains. The perception of quality of product-images depends not only on various photographic quality features but also on various high level features such as clarity of the foreground or goodness of the background etc. In this paper, we define a notion of product-image quality based on various such features. We conduct a crowd-sourced experiment to collect user judgments on thousands of eBay's images. We formulate a multi-class classification problem for modeling image quality by classifying images into good, fair and poor quality based on the guided perceptual notions from the judges. We also conduct experiments with regression using average crowd-sourced human judgments as target. We compute a pseudo-regression score with expected average of predicted classes and also compute a score from the regression technique. We design many experiments with various sampling and voting schemes with crowd-sourced data and construct various experimental image quality models. Most of our models have reasonable accuracies (greater or equal to 70%) on test data set. We observe that our computed image quality score has a high (0.66) rank correlation with average votes from the crowd sourced human judgments.

  12. 78 FR 16832 - Corrosion-Resistant Carbon Steel Flat Products From Germany and the Republic of Korea: Revocation...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-03-19

    .... Excluded from the scope of the orders are flat-rolled steel products either plated or coated with tin, lead, chromium, chromium oxides, both tin and lead (``terne plate''), or both chromium and chromium oxides (``tin...

  13. Mineral resource of the month: Iron and steel

    USGS Publications Warehouse

    Fenton, Michael D.

    2014-01-01

    Since 2008, steelmaking capacity has greatly exceeded apparent steel consumption, primarily as a result of China’s rapid economic expansion and rapidly increasing capacity. This has resulted in an influx of steel products into the United States and other steelmaking countries that already have excess capacity. Demand by China’s steelmakers has also driven unprecedented increases in the prices of iron ore and metallurgical coal. In the short term, steelmaking capacity, globally and especially in China, is expected to continue to exceed steel consumption, with steel prices and production costs remaining stable.

  14. 77 FR 54891 - Certain Corrosion-Resistant Carbon Steel Flat Products from the Republic of Korea: Preliminary...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-09-06

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Certain Corrosion-Resistant...) is conducting the 18th administrative review of the antidumping order on corrosion-resistant carbon steel flat products (CORE) from the Republic of Korea \\1\\ (Korea). This review covers seven...

  15. An improved segmentation method for defects inspection on steel roller surface

    NASA Astrophysics Data System (ADS)

    Xu, Jirui; Li, Xuekun; Cao, Yuzhong; Shi, Depeng; Yang, Jun; Jiang, Sheng; Rong, Yiming

    2018-05-01

    In the field of metal rolling, the quality of the steel roller's surface is significant for the final rolling products, e.g. metal sheets or foils. Besides the dimensional accuracy and surface roughness, the optical uniformity of the roller surface is also required for high quality rolling application. The typical optical defects of rollers after finish grinding include speckles, chatter marks, feed traces, and combination of all above. Unlike surface roughness, the optical defects can hardly be characterized by the topography or scanning electrical microscope measurement. Only the inspection by bared eyes of experienced engineers appears to be the effective manner for surface optical defects examination for large steel rollers. In this paper, an on-site machine vision system is designed to add on to the roller grinding machine to capture the surface image, and then an improved optical defects segmentation algorithm is developed based on the active contour model. Finally, experiments are carried out to verify the efficacy of the improved model.

  16. 75 FR 2107 - Certain Cut-to-Length Carbon-Quality Steel Plate from the Republic of Korea: Extension of the...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-01-14

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-836] Certain Cut-to-Length Carbon... preliminary results of the administrative review of the antidumping duty order on certain cut-to-length carbon.... See Certain Cut-to-Length Carbon-Quality Steel Plate From the Republic of Korea: Preliminary Results...

  17. Production, microstructure and mechanical properties of two different austenitic ODS steels

    NASA Astrophysics Data System (ADS)

    Gräning, T.; Rieth, M.; Hoffmann, J.; Möslang, A.

    2017-04-01

    This article is to summarize and examine processing parameters of novel developed austenitic oxide dispersed strengthened (ODS) steels. Comparing hot-rolled and extruded conditions after the same degree of deformation after and before annealing, are just some examples to give insights into the complex processing of austenitic ODS steels. One of the major drawbacks of the material is the more sophisticated production process. Due to a ductile matrix material with an increased stickiness during milling, a two-step milling procedure with the use of ZrO2 milling balls was applied to raise the production yield and to use the abrasion of the ZrO2 as an additional element to facilitate the formation of nano-sized precipitates. To get a better understanding how the different powder particle sizes after milling affect final properties, sieving was applied and revealed a serious effect in terms of precipitate size, distribution and mechanical properties. Grain sizes in relation to the precipitate size, annealing time and processing parameters were determined and compared to the mechanical properties. Hardness and tensile test have pointed out, that the precipitate size and number are more important in respect to the ultimate tensile strength than the grain size and that in this study hot-rolled material exhibited the better properties. The investigation of the microstructure illustrated the stability of precipitates during annealing at 1100 °C for 40 h. These heat treatments also led to a consistent grain size, due to the pinning effect of the grain boundaries, caused by precipitates.

  18. A real-time surface inspection system for precision steel balls based on machine vision

    NASA Astrophysics Data System (ADS)

    Chen, Yi-Ji; Tsai, Jhy-Cherng; Hsu, Ya-Chen

    2016-07-01

    Precision steel balls are one of the most fundament components for motion and power transmission parts and they are widely used in industrial machinery and the automotive industry. As precision balls are crucial for the quality of these products, there is an urgent need to develop a fast and robust system for inspecting defects of precision steel balls. In this paper, a real-time system for inspecting surface defects of precision steel balls is developed based on machine vision. The developed system integrates a dual-lighting system, an unfolding mechanism and inspection algorithms for real-time signal processing and defect detection. The developed system is tested under feeding speeds of 4 pcs s-1 with a detection rate of 99.94% and an error rate of 0.10%. The minimum detectable surface flaw area is 0.01 mm2, which meets the requirement for inspecting ISO grade 100 precision steel balls.

  19. Enhanced corrosion resistance of stainless steel type 316 in sulphuric acid solution using eco-friendly waste product

    NASA Astrophysics Data System (ADS)

    Sanni, O.; Popoola, A. P. I.; Fayomi, O. S. I.

    2018-06-01

    Literature has shown that different organic compounds are effective corrosion inhibitors for metal in acidic environments. Such compounds usually contain oxygen, nitrogen or sulphur and function through adsorption on the metal surface, thereby creating a barrier for corrosion attack. Unfortunately, these organic compounds are toxic, scarce and expensive. Therefore, plants, natural product and natural oils have been posed as cheap, environmentally acceptable, abundant, readily available and effective molecules having low environmental impact. The corrosion resistance of austenitic stainless steel Type 316 in the presence of eco-friendly waste product was studied using weight loss and potentiodynamic polarization techniques in 0.5 M H2SO4. The corrosion rate and corrosion potential of the steel was significantly altered by the studied inhibitor. Results show that increase in concentration of the inhibitor hinders the formation of the passive film. Experimental observation shows that its pitting potential depends on the concentration of the inhibitor in the acid solution due to adsorption of anions at the metal film interface. The presence of egg shell powder had a strong influence on the corrosion resistance of stainless steel Type 316 with highest inhibition efficiency of 94.74% from weight loss analysis, this is as a result of electrochemical action and inhibition of the steel by the ionized molecules of the inhibiting compound which influenced the mechanism of the redox reactions responsible for corrosion and surface deterioration. Inhibitor adsorption fits the Langmuir isotherm model. The two methods employed for the corrosion assessment were in good agreement.

  20. Magnetoelastic Effect-Based Transmissive Stress Detection for Steel Strips: Theory and Experiment

    PubMed Central

    Zhang, Qingdong; Su, Yuanxiao; Zhang, Liyuan; Bi, Jia; Luo, Jiang

    2016-01-01

    For the deficiencies of traditional stress detection methods for steel strips in industrial production, this paper proposes a non-contact stress detection scheme based on the magnetoelastic effect. The theoretical model of the transmission-type stress detection is established, in which the output voltage and the tested stress obey a linear relation. Then, a stress detection device is built for the experiment, and Q235 steel under uniaxial tension is tested as an example. The result shows that the output voltage rises linearly with the increase of the tensile stress, consistent with the theoretical prediction. To ensure the accuracy of the stress detection method in actual application, the temperature compensation, magnetic shielding and some other key technologies are investigated to reduce the interference of the external factors, such as environment temperature and surrounding magnetic field. The present research develops the theoretical and experimental foundations for the magnetic stress detection system, which can be used for online non-contact monitoring of strip flatness-related stress (tension distribution or longitudinal residual stress) in the steel strip rolling process, the quality evaluation of strip flatness after rolling, the life and safety assessment of metal construction and other industrial production links. PMID:27589742

  1. Quality plan for a product line.

    PubMed

    Lanza, M L; Binus, G K; McMillan, F J

    1997-12-01

    Continuous Quality improvement (CQI) has undergone radical change as health care facilities merge, expand, and modify their existing services. CQI has shifted from a centralized position in health care organizations, to unit based, to product lines. This paper describes one product line's endeavors to develop a Quality Plan to direct CQI activities. One particular strength of our innovation is that the Quality Plan was developed with attention to the important balance of interdisciplinary cooperation and maintenance of appropriate discipline boundaries.

  2. Occupational Heat Stress Impacts on Health and Productivity in a Steel Industry in Southern India.

    PubMed

    Krishnamurthy, Manikandan; Ramalingam, Paramesh; Perumal, Kumaravel; Kamalakannan, Latha Perumal; Chinnadurai, Jeremiah; Shanmugam, Rekha; Srinivasan, Krishnan; Venugopal, Vidhya

    2017-03-01

    Workers laboring in steel industries in tropical settings with high ambient temperatures are subjected to thermally stressful environments that can create well-known risks of heat-related illnesses and limit workers' productivity. A cross-sectional study undertaken in a steel industry in a city nicknamed "Steel City" in Southern India assessed thermal stress by wet bulb globe temperature (WBGT) and level of dehydration from urine color and urine specific gravity. A structured questionnaire captured self-reported heat-related health symptoms of workers. Some 90% WBGT measurements were higher than recommended threshold limit values (27.2-41.7°C) for heavy and moderate workloads and radiational heat from processes were very high in blooming-mill/coke-oven (67.6°C globe temperature). Widespread heat-related health concerns were prevalent among workers, including excessive sweating, fatigue, and tiredness reported by 50% workers. Productivity loss was significantly reported high in workers with direct heat exposures compared to those with indirect heat exposures (χ 2  = 26.1258, degrees of freedom = 1, p  < 0.001). Change in urine color was 7.4 times higher among workers exposed to WBGTs above threshold limit values (TLVs). Preliminary evidence shows that high heat exposures and heavy workload adversely affect the workers' health and reduce their work capacities. Health and productivity risks in developing tropical country work settings can be further aggravated by the predicted temperature rise due to climate change, without appropriate interventions. Apart from industries enhancing welfare facilities and designing control interventions, further physiological studies with a seasonal approach and interventional studies are needed to strengthen evidence for developing comprehensive policies to protect workers employed in high heat industries.

  3. 78 FR 19734 - Diffusion-Annealed, Nickel-Plated Steel Flat-Rolled Products From Japan; Institution of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-04-02

    ..., by reason of imports from Japan of diffusion-annealed, nickel-plated steel flat-rolled products... 45 days, or in this case by May 13, 2013. The Commission's views are due at Commerce within five.... Lisa R. Barton, Acting Secretary to the Commission. [FR Doc. 2013-07584 Filed 4-1-13; 8:45 am] BILLING...

  4. Visualization of turbulent combustion of TNT detonation products in a steel vessel

    NASA Astrophysics Data System (ADS)

    Wolański, P.; Gut, Z.; Trzciński, W. A.; Szymańczyk, L.; Paszula, J.

    Mixing and afterburning of TNT detonation products in a steel vessel are recorded by the use of the Schlieren visualization system and high speed photography. The vessel is filled with air or 50% oxygen enriched air. Overpressure histories at the vessel wall are also recorded by using pressure transducers. In these experiments nitrogen, air or 50% oxygen enriched air are used as vessel fillers. The Oppenheim-Kuhl theory of thermodynamics of closed systems is applied to estimate the released energy on the basis of pressure histories.

  5. Air Quality Co-benefits of Energy Policy in China: Evidence from Iron & Steel and Cement Industries

    NASA Astrophysics Data System (ADS)

    Qiu, M.; Weng, Y.; Selin, N. E.; Karplus, V. J.; Cao, J.

    2017-12-01

    Previous literature has calculated large air quality co-benefits from policies that reduce CO2 emissions and increase energy efficiency. These (often prospective) studies rely on assumptions about how air pollutant emissions respond to energy use changes. Using a unique firm-level data set from China, we examine how a real-world energy efficiency policy affected SO2 emissions, estimate its actual effects on atmospheric PM2.5, and compare to ex ante theoretical estimates. During the 11th Five-year plan (2006-2010), the Chinese government implemented policies directing large energy-consuming firms to reduce their energy consumption per unit of economic output. The Top 1000 Enterprises Program (T1000P) set binding energy intensity targets for China's 1000 highest energy-consuming firms. This program is widely considered a policy success, as 92% of firms met their energy intensity target. Focusing on the cement and iron and steel industry, we examine how T1000P (and related provincial policies) affected firms' SO2 emissions and coal consumption from 2005 to 2008. By comparing T1000P firms with similar firms not subject to the policy, we find that T1000P had a very limited incremental effect on energy use or on air quality co-benefits. Compared to firms not subject to the policy, T1000P firms had 14.7% (cement) and 24.0% (iron & steel) lower reductions in SO2 emission per unit energy use. We also observe large, heterogeneous changes in emission factors (defined as SO2 emissions per unit of coal consumption) among all firms during this period. In comparison to co-benefits estimates that assume constant emission factors, SO2 emissions from T1000P firms in the post-policy period are 23.2% (iron and steel) and 40.2% (cement) lower, but spatially heterogeneous, with some regions experiencing increases. Using the GEOS-Chem model, we estimate the air quality co-benefits of the T1000P policy with realized SO2 emissions changes and compare them with two theoretical estimations

  6. Effective Process Design for the Production of HIC-Resistant Linepipe Steels

    NASA Astrophysics Data System (ADS)

    Nieto, J.; Elías, T.; López, G.; Campos, G.; López, F.; Garcia, R.; De, Amar K.

    2013-09-01

    Production of slabs for sour service applications requires stringent control in slab internal quality and secondary processing so as to guarantee resistance against hydrogen-induced cracking (HIC). ArcelorMittal Steelmaking facility at Lazaro Cardenas, Mexico had recently implemented key steelmaking and casting processing technologies for production of sound, centerline free slabs for catering to the growing API Linepipe and off-shore market for sour service applications. State-of-the-art steelmaking with use of residual-free Direct-reduced Iron and continuous casting facilities with dynamic soft reduction were introduced for the production of slabs with ultra clean centerline. Introduction of controlled cooling of slabs for atomic hydrogen control well below 2 ppm has enabled production of slabs suitable for excellent HIC-resistant plate processing. Substantial tonnages of slabs were produced for production of API X52-X65 grade plates and pipes for sour service. Stringent quality control at each stage of steelmaking, casting, and slab inspection ensured slabs with excellent internal quality suitable for HIC resistance to be guaranteed in final product (Plates & Pipes). Details of production steps which resulted in successful HIC-resistant slab production have been described in this article.

  7. 77 FR 14501 - Certain Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Notice of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-03-12

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Certain Corrosion-Resistant... the preliminary results of the antidumping duty administrative review for certain corrosion-resistant carbon steel flat products (CORE) from the Republic of Korea (Korea).\\1\\ This review covers eight...

  8. Pyrolysis-catalysis of waste plastic using a nickel-stainless-steel mesh catalyst for high-value carbon products.

    PubMed

    Zhang, Yeshui; Nahil, Mohamad A; Wu, Chunfei; Williams, Paul T

    2017-11-01

    A stainless-steel mesh loaded with nickel catalyst was produced and used for the pyrolysis-catalysis of waste high-density polyethylene with the aim of producing high-value carbon products, including carbon nanotubes (CNTs). The catalysis temperature and plastic-to-catalyst ratio were investigated to determine the influence on the formation of different types of carbon deposited on the nickel-stainless-steel mesh catalyst. Increasing temperature from 700 to 900°C resulted in an increase in the carbon deposited on the nickel-loaded stainless-steel mesh catalyst from 32.5 to 38.0 wt%. The increase in sample-to-catalyst ratio reduced the amount of carbon deposited on the mesh catalyst in terms of g carbon g -1 plastic. The carbons were found to be largely composed of filamentous carbons, with negligible disordered (amorphous) carbons. Transmission electron microscopy analysis of the filamentous carbons revealed them to be composed of a large proportion (estimated at ∼40%) multi-walled carbon nanotubes (MWCNTs). The optimum process conditions for CNT production, in terms of yield and graphitic nature, determined by Raman spectroscopy, was catalysis temperature of 800°C and plastic-to-catalyst ratio of 1:2, where a mass of 334 mg of filamentous/MWCNTs g -1 plastic was produced.

  9. Optimal Recycling of Steel Scrap and Alloying Elements: Input-Output based Linear Programming Method with Its Application to End-of-Life Vehicles in Japan.

    PubMed

    Ohno, Hajime; Matsubae, Kazuyo; Nakajima, Kenichi; Kondo, Yasushi; Nakamura, Shinichiro; Fukushima, Yasuhiro; Nagasaka, Tetsuya

    2017-11-21

    Importance of end-of-life vehicles (ELVs) as an urban mine is expected to grow, as more people in developing countries are experiencing increased standards of living, while the automobiles are increasingly made using high-quality materials to meet stricter environmental and safety requirements. While most materials in ELVs, particularly steel, have been recycled at high rates, quality issues have not been adequately addressed due to the complex use of automobile materials, leading to considerable losses of valuable alloying elements. This study highlights the maximal potential of quality-oriented recycling of ELV steel, by exploring the utilization methods of scrap, sorted by parts, to produce electric-arc-furnace-based crude alloy steel with minimal losses of alloying elements. Using linear programming on the case of Japanese economy in 2005, we found that adoption of parts-based scrap sorting could result in the recovery of around 94-98% of the alloying elements occurring in parts scrap (manganese, chromium, nickel, and molybdenum), which may replace 10% of the virgin sources in electric arc furnace-based crude alloy steel production.

  10. Enhancing steel properties through in situ formation of ultrahard ceramic surface

    PubMed Central

    Pahlevani, Farshid; Kumar, Rahul; Gorjizadeh, Narjes; Hossain, Rumana; Cholake, Sagar T; Privat, Karen; Sahajwalla, Veena

    2016-01-01

    Abrasion and corrosion resistant steel has attracted considerable interest for industrial application as a means of minimising the costs associated with product/component failures and/or short replacement cycles. These classes of steels contain alloying elements that increase their resistance to abrasion and corrosion. Their benefits, however, currently come at a potentially prohibitive cost; such high performance steel products are both more technically challenging and more expensive to produce. Although these methods have proven effective in improving the performance of more expensive, high-grade steel components, they are not economically viable for relatively low cost steel products. New options are needed. In this study, a complex industrial waste stream has been transformed in situ via precisely controlled high temperature reactions to produce an ultrahard ceramic surface on steel. This innovative ultrahard ceramic surface increases both the hardness and compressive strength of the steel. Furthermore, by modifying the composition of the waste input and the processing parameters, the ceramic surface can be effectively customised to match the intended application of the steel. This economical new approach marries industry demands for more cost-effective, durable steel products with global imperatives to address resource depletion and environmental degradation through the recovery of resources from waste. PMID:27929096

  11. Enhancing steel properties through in situ formation of ultrahard ceramic surface.

    PubMed

    Pahlevani, Farshid; Kumar, Rahul; Gorjizadeh, Narjes; Hossain, Rumana; Cholake, Sagar T; Privat, Karen; Sahajwalla, Veena

    2016-12-08

    Abrasion and corrosion resistant steel has attracted considerable interest for industrial application as a means of minimising the costs associated with product/component failures and/or short replacement cycles. These classes of steels contain alloying elements that increase their resistance to abrasion and corrosion. Their benefits, however, currently come at a potentially prohibitive cost; such high performance steel products are both more technically challenging and more expensive to produce. Although these methods have proven effective in improving the performance of more expensive, high-grade steel components, they are not economically viable for relatively low cost steel products. New options are needed. In this study, a complex industrial waste stream has been transformed in situ via precisely controlled high temperature reactions to produce an ultrahard ceramic surface on steel. This innovative ultrahard ceramic surface increases both the hardness and compressive strength of the steel. Furthermore, by modifying the composition of the waste input and the processing parameters, the ceramic surface can be effectively customised to match the intended application of the steel. This economical new approach marries industry demands for more cost-effective, durable steel products with global imperatives to address resource depletion and environmental degradation through the recovery of resources from waste.

  12. Accumulation of radioactive corrosion products on steel surfaces of VVER-type nuclear reactors. II. 60Co

    NASA Astrophysics Data System (ADS)

    Varga, Kálmán; Hirschberg, Gábor; Németh, Zoltán; Myburg, Gerrit; Schunk, János; Tilky, Péter

    2001-10-01

    In the case of intact fuel claddings, the predominant source of radioactivity in the primary circuits of water-cooled nuclear reactors is the activation of corrosion products in the core. The most important corrosion product radionuclides in the primary coolant of pressurized water reactors (PWRs) are 60Co, 58Co, 51Cr, 54Mn, 59Fe (as well as 110mAg in some Soviet-made VVER-type reactor). The second part of this series is focused on the complex studies of the formation and build-up of 60Co-containing species on an austenitic stainless steel type 08X18H10T (GOST 5632-61) and magnetite-covered carbon steel often to be used in Soviet-planned VVERs. The kinetics and mechanism of the cobalt accumulation were studied by a combination (coupling) of an in situ radiotracer method and voltammetry in a model solution of the primary circuit coolant. In addition, independent techniques such as X-ray photoelectron spectroscopic (XPS) and ICP-OES are also used to analyze the chemical state of Co species in the passive layer formed on stainless steel as well as the chemical composition of model solution. The experimental results have revealed that: (i) The passive behavior of the austenitic stainless steel at open-circuit conditions, the slightly alkaline pH and the reducing water chemistry can be considered to be optimal to minimize the 60Co contamination. (ii) The highly potential dependent deposition of various Co-oxides at E>1.10 V (vs. RHE) offers a unique possibility to elaborate a novel electrochemical method for the decrease or removal of cobalt traces from borate-containing coolants contaminated with 60Co and/or 58Co radionuclides.

  13. Application of RNAMlet to surface defect identification of steels

    NASA Astrophysics Data System (ADS)

    Xu, Ke; Xu, Yang; Zhou, Peng; Wang, Lei

    2018-06-01

    As three main production lines of steels, continuous casting slabs, hot rolled steel plates and cold rolled steel strips have different surface appearances and are produced at different speeds of their production lines. Therefore, the algorithms for the surface defect identifications of the three steel products have different requirements for real-time and anti-interference. The existing algorithms cannot be adaptively applied to surface defect identification of the three steel products. A new method of adaptive multi-scale geometric analysis named RNAMlet was proposed. The idea of RNAMlet came from the non-symmetry anti-packing pattern representation model (NAM). The image is decomposed into a set of rectangular blocks asymmetrically according to gray value changes of image pixels. Then two-dimensional Haar wavelet transform is applied to all blocks. If the image background is complex, the number of blocks is large, and more details of the image are utilized. If the image background is simple, the number of blocks is small, and less computation time is needed. RNAMlet was tested with image samples of the three steel products, and compared with three classical methods of multi-scale geometric analysis, including Contourlet, Shearlet and Tetrolet. For the image samples with complicated backgrounds, such as continuous casting slabs and hot rolled steel plates, the defect identification rate obtained by RNAMlet was 1% higher than other three methods. For the image samples with simple backgrounds, such as cold rolled steel strips, the computation time of RNAMlet was one-tenth of the other three MGA methods, while the defect identification rates obtained by RNAMlet were higher than the other three methods.

  14. 76 FR 4291 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Partial Rescission of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-01-25

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-580-818] Corrosion-Resistant Carbon... Commerce (the Department) initiated an administrative review of the countervailing duty order on corrosion- resistant carbon steel flat products from the Republic of Korea covering the period January 1, 2009, through...

  15. 78 FR 55057 - Corrosion-Resistant Carbon Steel Flat Products from the Republic of Korea: Preliminary Results of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-09-09

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Corrosion-Resistant Carbon... Department) is conducting an administrative review of the antidumping duty order on corrosion-resistant carbon steel flat products (CORE) from the Republic of Korea (Korea), covering the period [[Page 55058...

  16. 78 FR 16247 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea; Final Results of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-03-14

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Corrosion-Resistant Carbon... preliminary results of the administrative review of the antidumping duty order on corrosion-resistant carbon steel flat products (CORE) from the Republic of Korea (Korea).\\1\\ This review covers seven manufacturers...

  17. 76 FR 48143 - Certain Hot-Rolled Carbon Steel Flat Products From the People's Republic of China: Preliminary...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-08-08

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-570-865] Certain Hot-Rolled Carbon... on certain hot- rolled carbon steel flat products (``hot-rolled'') from the People's Republic of... INFORMATION: Background On November 29, 2001, the Department published the antidumping duty order on hot...

  18. 76 FR 66901 - Certain Hot-Rolled Carbon Steel Flat Products From the People's Republic of China: Final...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-10-28

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-570-865] Certain Hot-Rolled Carbon... of the administrative review of the antidumping duty order on certain hot-rolled carbon steel flat products (``hot-rolled'') from the People's Republic of China (``PRC'').\\1\\ This administrative review...

  19. [Measurement of chemical agents in metallurgy field: electric steel plant].

    PubMed

    Cottica, D; Grignani, E; Ghitti, R; Festa, D; Apostoli, P

    2012-01-01

    The steel industry maintains its important position in the context of the Italian production involving thousands of workers. The iron and steel processes are divided into primary steel industry, production of intermediate minerals, and secondary steel, scrap from the production of semi-finished industrial and consumer sector (metal inserted into components and metal used for dissipative uses, primarily coatings) and industrial waste. The paper presents the results of environmental monitoring carried out in some electric steel plant for the measurement of airborne chemicals that characterize the occupational exposure of workers employed in particular area like electric oven, to treatment outside the furnace, continuous casting area. For the sampling of the pollutants were used both personal and in fixed positions samplers. The pollutants measured are those typical of steel processes inhalable dust, metals, respirable dust, crystalline silica, but also Polycyclic Aromatic Hydrocarbons (PAH), polychlorinated dioxins (PCDDs) and polychlorinated dibenzofurans (PCDFs).

  20. A Comparative Study on Formability of the Third-Generation Automotive Medium-Mn Steel and 22MnB5 Steel

    NASA Astrophysics Data System (ADS)

    Zheng, Guojun; Li, Xiaodong; Chang, Ying; Wang, Cunyu; Dong, Han

    2018-02-01

    Third-generation advanced automotive medium-Mn steel, which can replace 22MnB5 steel, was newly developed to improve the lightweight and crashworthiness of automobile. Studies on the formability and simulation method of medium-Mn steel have just been initiated. In this study, finite element simulation models of square-cup deep drawing were established based on various material property experiments and validated by experiments. The effects of blank holder force (BHF), fillet radii of tools (die and punch) on the maximum drawing depth (MDD), thickness distribution of the formed products, and the microstructure before and after forming were investigated and compared with those on 22MnB5 steel. Results show that the MDD of the two steels decreased with increased BHF but increased with the fillet radius of punch; however, the fillet radius of die showed no significant effect on the MDD for both steels. Compared with hot-formed 22MnB5 steel, the martensitic transformation of the hot-formed medium-Mn steel is rarely influenced by the process parameters; thus, it holds the complete, fine-grained, and uniform martensitic microstructure. Moreover, the medium-Mn has better formability, lower initial blank temperature, and smaller impact of BHF and fillet radius of tools on the hot-formed product. Thus, a theoretical basis for the replacement of 22MnB5 steel by medium-Mn steel in hot forming process is provided.

  1. Updated atmospheric speciated mercury emissions from iron and steel production in China during 2000-2015

    NASA Astrophysics Data System (ADS)

    Wu, Qingru; Gao, Wei; Wang, Shuxiao; Hao, Jiming

    2017-09-01

    Iron and steel production (ISP) is one of the significant atmospheric Hg emission sources in China. Atmospheric mercury (Hg) emissions from ISP during 2000-2015 were estimated by using a technology-based emission factor method. To support the application of this method, databases of Hg concentrations in raw materials, technology development trends, and Hg removal efficiencies of air pollution control devices (APCDs) were constructed through national sampling and literature review. Hg input to ISP increased from 21.6 t in 2000 to 94.5 t in 2015. In the various types of raw materials, coking coal and iron concentrates contributed 35-46 and 25-32 % of the total Hg input. Atmospheric Hg emissions from ISP increased from 11.5 t in 2000 to 32.7 t in 2015 with a peak of 35.6 t in 2013. Pollution control promoted the increase in average Hg removal efficiency, from 47 % in 2000 to 65 % in 2015. During the study period, sinter/pellet plants and blast furnaces were the largest two emission processes. However, emissions from roasting plants and coke ovens cannot be ignored, which accounted for 22-34 % of ISP's emissions. Overall, Hg speciation shifted from 50/44/6 (gaseous elemental Hg (Hg0)/gaseous oxidized Hg (HgII)/particulate-bound Hg (Hgp)) in 2000 to 40/59/1 in 2015, which indicated a higher proportion of Hg deposition around the emission points. Future emissions of ISP were expected to decrease based on the comprehensive consideration crude-steel production, steel scrap utilization, energy saving, and pollution control measures.

  2. 7 CFR 58.142 - Product quality and stability.

    Code of Federal Regulations, 2012 CFR

    2012-01-01

    ... Procedures § 58.142 Product quality and stability. The receiving, holding and processing of milk and cream... accordance with clean and sanitary methods, consistent with good commercial practices to promote the production of the highest quality of finished product and improve product stability. Milk should not be more...

  3. 7 CFR 58.142 - Product quality and stability.

    Code of Federal Regulations, 2011 CFR

    2011-01-01

    ... Procedures § 58.142 Product quality and stability. The receiving, holding and processing of milk and cream... accordance with clean and sanitary methods, consistent with good commercial practices to promote the production of the highest quality of finished product and improve product stability. Milk should not be more...

  4. 7 CFR 58.142 - Product quality and stability.

    Code of Federal Regulations, 2013 CFR

    2013-01-01

    ... Procedures § 58.142 Product quality and stability. The receiving, holding and processing of milk and cream... accordance with clean and sanitary methods, consistent with good commercial practices to promote the production of the highest quality of finished product and improve product stability. Milk should not be more...

  5. 7 CFR 58.142 - Product quality and stability.

    Code of Federal Regulations, 2014 CFR

    2014-01-01

    ... Procedures § 58.142 Product quality and stability. The receiving, holding and processing of milk and cream... accordance with clean and sanitary methods, consistent with good commercial practices to promote the production of the highest quality of finished product and improve product stability. Milk should not be more...

  6. Evaluation of Safety, Quality and Productivity in Construction

    NASA Astrophysics Data System (ADS)

    Usmen, M. A.; Vilnitis, M.

    2015-11-01

    This paper examines the success indicators of construction projects, safety, quality and productivity, in terms of their implications and impacts during and after construction. First safety is considered during construction with a focus on hazard identification and the prevention of occupational accidents and injuries on worksites. The legislation mandating safety programs, training and compliance with safety standards is presented and discussed. Consideration of safety at the design stage is emphasized. Building safety and the roles of building codes in prevention of structural failures are also covered in the paper together with factors affecting building failures and methods for their prevention. Quality is introduced in the paper from the perspective of modern total quality management. Concepts of quality management, quality control, quality assurance and Six Sigma and how they relate to building quality and structural integrity are discussed with examples. Finally, productivity concepts are presented with emphasis on effective project management to minimize loss of productivity, complimented by lean construction and lean Six Sigma principles. The paper concludes by synthesizing the relationships between safety, quality and productivity.

  7. 76 FR 77775 - Corrosion-Resistant Carbon Steel Flat Products from the Republic of Korea: Extension of Time...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-12-14

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-580-818] Corrosion-Resistant Carbon... results of the administrative review of the countervailing duty order on corrosion-resistant carbon steel flat products from the Republic of Korea covering the period January 1, 2009, through December 31, 2009...

  8. 78 FR 59651 - Certain Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Notice of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-09-27

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Certain Corrosion-Resistant... duty order on certain corrosion-resistant carbon steel flat products (``CORE'') from the Republic of... covering the period of review (``POR'') of August 1, 2006 through July 31, 2007, with respect to the...

  9. 78 FR 59652 - Certain Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Notice of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2013-09-27

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Certain Corrosion-Resistant... corrosion-resistant carbon steel flat products (``CORE'') from the Republic of Korea (``Korea''), pursuant... administrative review of the antidumping duty order on CORE from Korea covering the period of review (``POR'') of...

  10. Finite element simulation and experimental verification of steel cord extraction of steel cord conveyor belt splice

    NASA Astrophysics Data System (ADS)

    Li, X. G.; Long, X. Y.; Jiang, H. Q.; Long, H. B.

    2018-05-01

    The splice is the weakest part of the entire steel cord conveyor belt. And it occurs steel cord twitch fault frequently. If this fault cannot be dealt with timely and accurately, broken belt accidents would be occurred that affecting the safety of production seriously. In this paper, we investigate the steel cord pullout of the steel cord conveyor belt splice by using ABAQUS software. We selected the strength of steel cord conveyor belt ST630, the same as experiment sample in type specification. The finite element model consists of rubber, steel cord and failure unit. And the failure unit is used to simulate the bonding relationship between the steel cord and the rubber. Mooney-Rivlin hyper-elastic model for rubber was employed in the numerical simulations. The pullout force of length 50.0 mm single steel cord, on both sides of a single steel cord and on both sides of the double steel cords each impacted at steel cord conveyor belt splice were numerically computer and typical results obtained have been validated by experimental result. It shows that the relative error between simulation results and experimental results is within 10% and can be considered that the simulation model is reliable. A new method is provided for studying the steel cord twitch fault of the steel cord conveyor belt splice.

  11. Exploiting Process-Related Advantages of Selective Laser Melting for the Production of High-Manganese Steel.

    PubMed

    Haase, Christian; Bültmann, Jan; Hof, Jan; Ziegler, Stephan; Bremen, Sebastian; Hinke, Christian; Schwedt, Alexander; Prahl, Ulrich; Bleck, Wolfgang

    2017-01-11

    Metal additive manufacturing has strongly gained scientific and industrial importance during the last decades due to the geometrical flexibility and increased reliability of parts, as well as reduced equipment costs. Within the field of metal additive manufacturing methods, selective laser melting (SLM) is an eligible technique for the production of fully dense bulk material with complex geometry. In the current study, we addressed the application of SLM for processing a high-manganese TRansformation-/TWinning-Induced Plasticity (TRIP/TWIP) steel. The solidification behavior was analyzed by careful characterization of the as-built microstructure and element distribution using optical and scanning electron microscopy (SEM). In addition, the deformation behavior was studied using uniaxial tensile testing and SEM. Comparison with conventionally produced TRIP/TWIP steel revealed that elemental segregation, which is normally very pronounced in high-manganese steels and requires energy-intensive post processing, is reduced due to the high cooling rates during SLM. Also, the very fast cooling promoted ε- and α'-martensite formation prior to deformation. The superior strength and pronounced anisotropy of the SLM-produced material was correlated with the microstructure based on the process-specific characteristics.

  12. Exploiting Process-Related Advantages of Selective Laser Melting for the Production of High-Manganese Steel

    PubMed Central

    Haase, Christian; Bültmann, Jan; Hof, Jan; Ziegler, Stephan; Bremen, Sebastian; Hinke, Christian; Schwedt, Alexander; Prahl, Ulrich; Bleck, Wolfgang

    2017-01-01

    Metal additive manufacturing has strongly gained scientific and industrial importance during the last decades due to the geometrical flexibility and increased reliability of parts, as well as reduced equipment costs. Within the field of metal additive manufacturing methods, selective laser melting (SLM) is an eligible technique for the production of fully dense bulk material with complex geometry. In the current study, we addressed the application of SLM for processing a high-manganese TRansformation-/TWinning-Induced Plasticity (TRIP/TWIP) steel. The solidification behavior was analyzed by careful characterization of the as-built microstructure and element distribution using optical and scanning electron microscopy (SEM). In addition, the deformation behavior was studied using uniaxial tensile testing and SEM. Comparison with conventionally produced TRIP/TWIP steel revealed that elemental segregation, which is normally very pronounced in high-manganese steels and requires energy-intensive post processing, is reduced due to the high cooling rates during SLM. Also, the very fast cooling promoted ε- and α’-martensite formation prior to deformation. The superior strength and pronounced anisotropy of the SLM-produced material was correlated with the microstructure based on the process-specific characteristics. PMID:28772416

  13. Effect of Total Quality Management on the Quality and Productivity of Human Resources

    NASA Astrophysics Data System (ADS)

    Siregar, I.; Nasution, A. A.; Sari, R. M.

    2017-03-01

    Human resources is the main factor in improving company performance not only in industrial products but also services. Therefore, all of the organization performers involved must work together to achieve product quality services expected by consumers. Educational institutions are the service industries which are educators and instructor involved in it. Quality of product and services produced depends on the education organization performers. This study did a survey of instructors in public and private universities in North Sumatra to obtain the factors that affect quality of human resources and productivity of human resources. Human resources quality is viewed by the elements of TQM. TQM elements that are discussed in this study are leadership, communication, training and education, support structure, measurement and reward and recognition. The results of this study showed a correlation numbers across the exogenous variables on endogenous variables relationships tend to be strong and be positive. In addition, elements of TQM are discussed except the support structure which has a direct influence on the quality of human resources. Variable leadership, reward and recognition and quality of human resources have a significant effect on productivity.

  14. Selection of Compositions in Ti-Cr-C-Steel, Ti-B, Ti-B-Me Systems and Establishing Synthesis Parameters for Obtaining Product by “SHS-Electrical Rolling”

    NASA Astrophysics Data System (ADS)

    Aslamazashvili, Zurab; Tavadze, Giorgi; Chikhradze, Mikheil; Namicheishvili, Teimuraz; Melashvili, Zaqaria

    2017-12-01

    For the production materials by the proposed Self-propagating High-Temperature Synthesis (SHS) - Electric Rolling method, there are no limitations in the length of the material and the width only depends on the length of rolls. The innovation method enables to carry out the process in nonstop regime, which is possible by merging energy consuming SHS method and Electrical Rolling. For realizing the process it is mandatory and sufficient, that initial components, after initiation by thermal pulse, could interaction with the heat emission, which itself ensures the self-propagation of synthesis front in lieu of heat transfer in the whole sample. Just after that process, the rolls instantly start rotation with the set speed to ensure the motion of material. This speed should be equal to the speed of propagation of synthesis front. The synthesized product in hot plastic condition is delivered to the rolls in nonstop regime, simultaneously, providing the current in deformation zone in order to compensate the energy loses. As a result by using the innovation SHS -Electrical Rolling technology we obtain long dimensional metal-ceramic product. In the presented paper optimal compositions of SHS chasms were selected in Ti-Cr-C-Steel, Ti-B and Ti-B-Me systems. For the selection of the compounds the thermodynamic analysis has been carried out which enabled to determine adiabatic temperature of synthesis theoretically and to determine balanced concentrations of synthesized product at synthesis temperature. Thermodynamic analysis also gave possibility to determine optimal compositions of chasms and define the conditions, which are important for correct realization of synthesis process. For obtaining non porous materials and product by SHS-Electrical Rolling, it is necessary to select synthesis and compacting parameters correctly. These parameters are the pressure and the time. In Ti-Cr-C-Steel, Ti-B and Ti-B-Me systems the high quality (nonporous or low porosity <2%) of materials

  15. Vacuum brazing of 316L stainless steel based on additively manufactured and conventional material grades

    NASA Astrophysics Data System (ADS)

    Tillmann, W.; Henning, T.; Wojarski, L.

    2018-06-01

    Many industrial applications require components with an increasing geometric complexity and specific material properties. Furthermore, the production costs and the affordable production time have to be minimized in order to ensure competitiveness. These divergent objectives are difficult to achieve with a single manufacturing technology. Therefore, joining of selective laser melted (SLM) complex shaped parts to conventionally produced high-volume components provides a high potential. The current investigation focuses on vacuum brazing conventionally manufactured to non-hipped SLM generated AISI 316L stainless steel. Cylindrical samples (Ø 14 mm) were brazed using a B-Ni2 foil (50 µm) at 1050 °C for 30 minutes in vacuum (< 4.5·10-5 mbar) and directly cooled down to room temperature with 4 bar overpressure to prevent the formation of chromium carbides within the base material. It could be proven that the brazing quality is extremely sensitive to even marginal porosities (< 0.2 %) and/or oxide inclusions of the SLM microstructure. Therefore, the fracture mirror in SLM/conventional steel brazements was at the joint braze/SLM steel interface, leading to a joint strength of 317.4 MPa. This corresponds to only 67.4 % of the joint strength obtained with conventional steel, where the fracture propagated through the diffusion area.

  16. 46 CFR 164.019-13 - Production quality control requirements.

    Code of Federal Regulations, 2011 CFR

    2011-10-01

    ... 46 Shipping 6 2011-10-01 2011-10-01 false Production quality control requirements. 164.019-13....019-13 Production quality control requirements. (a) General. Each component manufacturer shall establish procedures for maintaining quality control of the materials used in production, manufacturing...

  17. 46 CFR 164.019-13 - Production quality control requirements.

    Code of Federal Regulations, 2012 CFR

    2012-10-01

    ... 46 Shipping 6 2012-10-01 2012-10-01 false Production quality control requirements. 164.019-13....019-13 Production quality control requirements. (a) General. Each component manufacturer shall establish procedures for maintaining quality control of the materials used in production, manufacturing...

  18. 46 CFR 164.019-13 - Production quality control requirements.

    Code of Federal Regulations, 2010 CFR

    2010-10-01

    ... 46 Shipping 6 2010-10-01 2010-10-01 false Production quality control requirements. 164.019-13....019-13 Production quality control requirements. (a) General. Each component manufacturer shall establish procedures for maintaining quality control of the materials used in production, manufacturing...

  19. 46 CFR 164.019-13 - Production quality control requirements.

    Code of Federal Regulations, 2014 CFR

    2014-10-01

    ... 46 Shipping 6 2014-10-01 2014-10-01 false Production quality control requirements. 164.019-13....019-13 Production quality control requirements. (a) General. Each component manufacturer shall establish procedures for maintaining quality control of the materials used in production, manufacturing...

  20. 46 CFR 164.019-13 - Production quality control requirements.

    Code of Federal Regulations, 2013 CFR

    2013-10-01

    ... 46 Shipping 6 2013-10-01 2013-10-01 false Production quality control requirements. 164.019-13....019-13 Production quality control requirements. (a) General. Each component manufacturer shall establish procedures for maintaining quality control of the materials used in production, manufacturing...

  1. Process Hood Stand Support Steel

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    VAN KATWIJK, C.

    2000-04-03

    This package is written to comply with EN-6-035-00 for upgrade dedication of commercial grade items (CGI). The SNF-5953 CGI package provides the Technical evaluation to identify the critical characteristics and the acceptance criteria associated with the safety function of the Hood Stand Support Steel. Completion of the technical and quality requirements identified in the dedication package will provide enough data to be reasonably assured that CGI Hood Stand Support Steel will perform its SC function.

  2. "Product on Stopper" in a Lyophilized Drug Product: Cosmetic Defect or a Product Quality Concern?

    PubMed

    Mehta, Shyam B; Roy, Shouvik; Yang, Han-Chang Cathy

    2018-06-01

    During manufacturing of a lyophilized drug product, operator errors in product handling during loading of product filled vials onto the lyophilizer can lead to a seemingly cosmetic defect which can impact certain critical quality attributes of finished product. In this study, filling of a formulated monoclonal antibody in vials was performed using a peristaltic pump filling unit, and subsequently, the product was lyophilized. After lyophilization, upon visual inspection, around 40% of vials had cosmetic defect with residual product around stopper of the vial and were categorized as "product on stopper" vials, whereas remaining 60% vials with no cosmetic defect were called "acceptable vials." Both groups of vials from 1 single batch were tested for critical quality attributes including protein concentration (ultraviolet absorbance at 280), residual moisture (Karl Fischer), sterility (membrane filtration), and container closure integrity (CCI) (blue dye ingress). Analysis of protein quality attributes such as aggregation, protein concentration, residual moisture showed no significant difference between vials with "product on stopper" and "acceptable vials." However, CCI of the "product on stopper" vials was compromised due to the presence of product around stopper of the vial. The results from this case study demonstrate the following 2 important findings: (1) that a seemingly cosmetic defect may impact product quality, compromising the integrity of the product and (2) that CCI test method can be used as an orthogonal method to sterility testing to evaluate sterility assurance of the product. The corrective action proposed to mitigate this defect is use of a larger sized vial that can potentially minimize this defect that arises because of product handling errors. Copyright © 2018 American Pharmacists Association®. Published by Elsevier Inc. All rights reserved.

  3. 75 FR 80455 - Certain Hot-Rolled Carbon Steel Flat Products From India: Amended Final Results of Countervailing...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-12-22

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-533-821] Certain Hot-Rolled Carbon...-rolled carbon steel flat products (HRCS) from India covering the 2006 POR, to reflect the CIT's order in... INFORMATION: Background On July 14, 2008, the Department published its final results in the countervailing...

  4. Production system with process quality control: modelling and application

    NASA Astrophysics Data System (ADS)

    Tsou, Jia-Chi

    2010-07-01

    Over the past decade, there has been a great deal of research dedicated to the study of quality and the economics of production. In this article, we develop a dynamic model which is based on the hypothesis of a traditional economic production quantity model. Taguchi's cost of poor quality is used to evaluate the cost of poor quality in the dynamic production system. A practical case from the automotive industry, which uses the Six-sigma DMAIC methodology, is discussed to verify the proposed model. This study shows that there is an optimal value of quality investment to make the production system reach a reasonable quality level and minimise the production cost. Based on our model, the management can adjust its investment in quality improvement to generate considerable financial return.

  5. An investigation of laser cutting quality of 22MnB5 ultra high strength steel using response surface methodology

    NASA Astrophysics Data System (ADS)

    Tahir, Abdul Fattah Mohd; Aqida, Syarifah Nur

    2017-07-01

    In hot press forming, changes of mechanical properties in boron steel blanks have been a setback in trimming the final shape components. This paper presents investigation of kerf width and heat affected zone (HAZ) of ultra high strength 22MnB5 steel cutting. Sample cutting was conducted using a 4 kW Carbon Dioxide (CO2) laser machine with 10.6 μm wavelength with the laser spot size of 0.2 mm. A response surface methodology (RSM) using three level Box-Behnken design of experiment was developed with three factors of peak power, cutting speed and duty cycle. The parameters were optimised for minimum kerf width and HAZ formation. Optical evaluation using MITUTOYO TM 505 were conducted to measure the kerf width and HAZ region. From the findings, laser duty cycle was crucial to determine cutting quality of ultra-high strength steel; followed by cutting speed and laser power. Meanwhile, low power intensity with continuous wave contributes the narrowest kerf width formation and least HAZ region.

  6. [Pharmaceutical product quality control and good manufacturing practices].

    PubMed

    Hiyama, Yukio

    2010-01-01

    This report describes the roles of Good Manufacturing Practices (GMP) in pharmaceutical product quality control. There are three keys to pharmaceutical product quality control. They are specifications, thorough product characterization during development, and adherence to GMP as the ICH Q6A guideline on specifications provides the most important principles in its background section. Impacts of the revised Pharmaceutical Affairs Law (rPAL) which became effective in 2005 on product quality control are discussed. Progress of ICH discussion for Pharmaceutical Development (Q8), Quality Risk Management (Q9) and Pharmaceutical Quality System (Q10) are reviewed. In order to reconstruct GMP guidelines and GMP inspection system in the regulatory agencies under the new paradigm by rPAL and the ICH, a series of Health Science studies were conducted. For GMP guidelines, product GMP guideline, technology transfer guideline, laboratory control guideline and change control system guideline were written. For the GMP inspection system, inspection check list, inspection memo and inspection scenario were proposed also by the Health Science study groups. Because pharmaceutical products and their raw materials are manufactured and distributed internationally, collaborations with other national authorities are highly desired. In order to enhance the international collaborations, consistent establishment of GMP inspection quality system throughout Japan will be essential.

  7. The use of steel slag in concrete

    NASA Astrophysics Data System (ADS)

    Martauz, P.; Vaclavik, V.; Cvopa, B.

    2017-10-01

    This paper presents the results of a research dealing with the use of unstable steel slag as a 100% substitute for natural aggregate in the production of concrete. Portland cement CEM I 42.5N and alkali activated hybrid cement H-CEMENT were used as the binder. The test results confirm the possibility to use steel slag as the filler in the production of concrete.

  8. Steel industry energy consumption: Sensitivity to technology choice, fuel prices, and carbon prices

    EIA Publications

    2016-01-01

    Steel industry energy consumption in 2010 totaled 1,158 trillion British thermal units (Btu), representing 8% of total manufacturing energy consumption. Energy consumption in the steel industry is largely for crude steel production using basic oxygen furnace (BOF) and electric arc furnace (EAF) technologies. Overall energy intensity in EAF, used primarily to melt scrap steel, is significantly lower than in BOF which is used to create virgin steel from iron ore. Over the past two decades, a shift from BOF to EAF has contributed to a substantial reduction in the energy intensity of the U.S. steel industry. From 1991 to 2010, the EAF share of total U.S. steel production in physical units increased from 38% to 61%, and the overall energy intensity of crude steel production in Btu per metric ton decreased by 37%.

  9. Impacts of Marcellus Shale Natural Gas Production on Regional Air Quality

    NASA Astrophysics Data System (ADS)

    Swarthout, R.; Russo, R. S.; Zhou, Y.; Mitchell, B.; Miller, B.; Lipsky, E. M.; Sive, B. C.

    2012-12-01

    Natural gas is a clean burning alternative to other fossil fuels, producing lower carbon dioxide (CO2) emissions during combustion. Gas deposits located within shale rock or tight sand formations are difficult to access using conventional drilling techniques. However, horizontal drilling coupled with hydraulic fracturing is now widely used to enhance natural gas extraction. Potential environmental impacts of these practices are currently being assessed because of the rapid expansion of natural gas production in the U.S. Natural gas production has contributed to the deterioration of air quality in several regions, such as in Wyoming and Utah, that were near or downwind of natural gas basins. We conducted a field campaign in southwestern Pennsylvania on 16-18 June 2012 to investigate the impact of gas production operations in the Marcellus Shale on regional air quality. A total of 235 whole air samples were collected in 2-liter electropolished stainless- steel canisters throughout southwestern Pennsylvania in a regular grid pattern that covered an area of approximately 8500 square km. Day and night samples were collected at each grid point and additional samples were collected near active wells, flaring wells, fluid retention reservoirs, transmission pipelines, and a processing plant to assess the influence of different stages of the gas production operation on emissions. The samples were analyzed at Appalachian State University for methane (CH4), CO2, C2-C10 nonmethane hydrocarbons (NMHCs), C1-C2 halocarbons, C1-C5 alkyl nitrates and selected reduced sulfur compounds. In-situ measurements of ozone (O3), CH4, CO2, nitric oxide (NO), total reactive nitrogen (NOy), formaldehyde (HCHO), and a range of volatile organic compounds (VOCs) were carried out at an upwind site and a site near active gas wells using a mobile lab. Emissions associated with gas production were observed throughout the study region. Elevated mixing ratios of CH4 and CO2 were observed in the

  10. Steels with controlled hardenability for induction hardening

    NASA Astrophysics Data System (ADS)

    Shepelyakovskii, K. Z.

    1980-07-01

    Steels of the CH and LH type developed in the Soviet Union permit the use of a new method of induction hardening — bulk-surface hardening — and efficient utilization of the high-strength conditions (σb = 230-250 kgf/mm2). These steels make it possible to improve the structural strength, operating characteristics, service life, and reliability of critical heavily loaded machine parts. At the same time, CH steels make it possible to reduce by a factor of 2-3 the quantity of alloying elements, reduce the electrical energy for heat treatment, and completely exclude the cost of quenching oil for heat treatment in automatic equipment with high labor productivity, while retaining good working conditions. All this leads to substantial savings in production and operation. For example, when transmission gears (cylindrical and conical) are manufactured from LH steels the annual savings amount to more than 700,000 rubles at two automobile plants. Machine parts of CH steels — half axles and bearings in railway cars —have saved respectively six and four million rubles annually. The introduction of controlled-hardenability steels for induction hardening is a necessary condition for technological progress in machine construction and metallurgy.

  11. Engineering study for a melting, casting, rolling and fabrication facility for recycled contaminated stainless steel

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    NONE

    This Preliminary Report is prepared to study the facilities required for recycling contaminated stainless steel scrap into plate which will be fabricated into boxes suitable for the storage of contaminated wastes and rubble. The study is based upon the underlying premise that the most cost effective way to produce stainless steel is to use the same processes employed by companies now in production of high quality stainless steel. Therefore, the method selected for this study for the production of stainless steel plate from scrap is conventional process using an Electric Arc Furnace for meltdown to hot metal, a Continuous Castermore » for production of cast slabs, and a Reversing Hot Mill for rolling the slabs into plate. The fabrication of boxes from the plate utilizes standard Shears, Punch Presses and welding equipment with Robotic Manipulators. This Study presumes that all process fumes, building dusts and vapors will be cycled through a baghouse and a nuclear grade HEPA filter facility prior to discharge. Also, all process waste water will be evaporated into the hot flue gas stream from the furnace utilizing a quench tank; so there will be no liquid discharges from the facility and all vapors will be processed through a HEPA filter. Even though HEPA filters are used today in controlling radioactive contamination from nuclear facilities there is a sparsity of data concerning radioactivity levels and composition of waste that may be collected from contaminated scrap steel processing. This report suggests some solutions to these problems but it is recommended that additional study must be given to these environmental problems.« less

  12. How product trial changes quality perception of four new processed beef products.

    PubMed

    Saeed, Faiza; Grunert, Klaus G; Therkildsen, Margrethe

    2013-01-01

    The purpose of this paper is the quantitative analysis of the change in quality perception of four new processed beef products from pre to post trial phases. Based on the Total Food Quality Model, differences in pre and post-trial phases were measured using repeated measures technique for cue evaluation, quality evaluation and purchase motive fulfillment. For two of the tested products, trial resulted in a decline of the evaluation of cues, quality and purchase motive fulfillment compared to pre-trial expectations. For these products, positive expectations were created by giving information about ingredients and ways of processing, which were not confirmed during trial. For the other two products, evaluations on key sensory dimensions based on trial exceeded expectations, whereas the other evaluations remained unchanged. Several demographic factors influenced the pattern of results, notably age and gender, which may be due to underlying differences in previous experience. The study gives useful insights for testing of new processed meat products before market introduction. Copyright © 2012 Elsevier Ltd. All rights reserved.

  13. Transitions to material efficiency in the UK steel economy.

    PubMed

    Allwood, Julian M

    2013-03-13

    Steel production is energy intensive so already has achieved impressive levels of energy efficiency. If the emissions associated with steel must be reduced in line with the requirements of the UK Climate Change Act, demand for new steel must be reduced. The strategies of 'material efficiency' aim to achieve such a reduction, while delivering the same final services. To meet the emissions targets set into UK law, UK consumption of steel must be reduced to 30 per cent of present levels by 2050. Previous work has revealed six strategies that could contribute to this target, and this paper presents an approximate analysis of the required transition. A macro-economic analysis of steel in the UK shows that while the steel industry is relatively small, the construction and manufacturing sectors are large, and it would be politically unacceptable to pursue options that lead to a major contraction in other sectors. Alternative business models are therefore required, and these are explored through four representative products--one for each final sector with particular emphasis given to options for reducing product weight, and extending product life. Preliminary evidence on the triggers that would lead to customers preferring these options is presented and organized in order to predict required policy measures. The estimated analysis of transitions explored in this paper is used to define target questions for future research in the area.

  14. Water requirements of the iron and steel industry

    USGS Publications Warehouse

    Walling, Faulkner B.; Otts, Louis Ethelbert

    1967-01-01

    concentrate. Water use in concentration plants is related to the physical state of the ore. The data in this report indicate that grain size of the ore is the most important factor; the very fine grained taconite and jasper required the greatest amount of water. Reuse was not widely practiced in the iron ore industry.Consumption of water by integrated steel plants ranged from 0 to 2,010 gallons per ton of ingot steel and by steel processing plants from 120 to 3,420 gallons per ton. Consumption by a typical integrated steel plant was 681 gallons per ton of ingot steel, about 1.8 percent of the intake and about 1 percent of the gross water use. Consumption by a typical steel processing plant was 646 gallons per ton, 18 percent of the intake, and 3.2 percent of the gross water use. The quality of available water was found not to be a critical factor in choosing the location of steel plants, although changes in equipment and in operating procedures are necessary when poor-quality water is used. The use of saline water having a concentration of dissolved solids as much as 10,400 ppm (parts per million) was reported. This very saline water was used for cooling furnaces and for quenching slag. In operations such as rolling steel in which the water comes into contact with the steel being processed, better quality water is used, although water containing as much as 3,410 ppm dissolved solids has been used for this purpose. Treatment of water for use in the iron and steel industry was not widely practiced. Disinfection and treatment for scale and corrosion control were the most frequently used treatment methods.

  15. Quality of original and biosimilar epoetin products.

    PubMed

    Brinks, Vera; Hawe, Andrea; Basmeleh, Abdul H H; Joachin-Rodriguez, Liliana; Haselberg, Rob; Somsen, Govert W; Jiskoot, Wim; Schellekens, Huub

    2011-02-01

    To compare the quality of therapeutic erythropoietin (EPO) products, including two biosimilars, with respect to content, aggregation, isoform profile and potency. Two original products, Eprex (epoetin alpha) and Dynepo (epoetin delta), and two biosimilar products, Binocrit (epoetin alpha) and Retacrit (epoetin zeta), were compared using (1) high performance size exclusion chromatography, (2) ELISA, (3) SDS-PAGE, (4) capillary zone electrophoresis and (5) in-vivo potency. Tested EPO products differed in content, isoform composition, and potency. Of the tested products, the biosimilars have the same or even better quality as the originals. Especially, the potency of originals may significantly differ from the value on the label.

  16. 75 FR 18152 - Certain Hot-Rolled Carbon Steel Flat Products from India: Extension of Time Limit for Final...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-04-09

    ... DEPARTMENT OF COMMERCE International Trade Administration [C-533-821] Certain Hot-Rolled Carbon Steel Flat Products from India: Extension of Time Limit for Final Results of Countervailing Duty Administrative Review AGENCY: Import Administration, International Trade Administration, Department of Commerce. FOR FURTHER INFORMATION CONTACT: Gayle...

  17. 75 FR 55742 - Certain Hot-Rolled Carbon Steel Flat Products from India: Extension of Time Limit for Preliminary...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-09-14

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-533-820] Certain Hot-Rolled Carbon Steel Flat Products from India: Extension of Time Limit for Preliminary Results of the Antidumping Duty Administrative Review AGENCY: Import Administration, International Trade Administration, Department of Commerce. EFFECTIVE DATE: September 14, 2010...

  18. 76 FR 69703 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Notice of Extension of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-11-09

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Corrosion-Resistant Carbon... administrative review of the antidumping duty order on corrosion-resistant carbon steel flat products from Korea, covering the period August 1, 2009, to July 31, 2010. See Initiation of Antidumping and Countervailing Duty...

  19. 75 FR 77615 - Corrosion-Resistant Carbon Steel Flat Products From the Republic of Korea: Notice of Extension of...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-12-13

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-580-816] Corrosion-Resistant Carbon... administrative review of the antidumping duty order on corrosion-resistant carbon steel flat products from Korea, covering the period August 1, 2008, to July 31, 2009. See Initiation of Antidumping and Countervailing Duty...

  20. Quality- and dilution losses in the recycling of ferrous materials from end-of-life passenger cars: input-output analysis under explicit consideration of scrap quality.

    PubMed

    Nakamura, Shinichiro; Kondo, Yasushi; Matsubae, Kazuyo; Nakajima, Kenichi; Tasaki, Tomohiro; Nagasaka, Tetsuya

    2012-09-04

    Metals can in theory be infinitely recycled in a closed-loop without any degradation in quality. In reality, however, open-loop recycling is more typical for metal scrap recovered from end-of-life (EoL) products because mixing of different metal species results in scrap quality that no longer matches the originals. Further losses occur when meeting the quality requirement of the target product requires dilution of the secondary material by adding high purity materials. Standard LCA usually does not address these losses. This paper presents a novel approach to quantifying quality- and dilution losses, by means of hybrid input-output analysis. We focus on the losses associated with the recycling of ferrous materials from end-of-life vehicle (ELV) due to the mixing of copper, a typical contaminant in steel recycling. Given the quality of scrap in terms of copper density, the model determines the ratio by which scrap needs to be diluted in an electric arc furnace (EAF), and the amount of demand for EAF steel including those quantities needed for dilution. Application to a high-resolution Japanese IO table supplemented with data on ferrous materials including different grades of scrap indicates that a nationwide avoidance of these losses could result in a significant reduction of CO(2) emissions.

  1. Effect of welding process on the microstructure and properties of dissimilar weld joints between low alloy steel and duplex stainless steel

    NASA Astrophysics Data System (ADS)

    Wang, Jing; Lu, Min-xu; Zhang, Lei; Chang, Wei; Xu, Li-ning; Hu, Li-hua

    2012-06-01

    To obtain high-quality dissimilar weld joints, the processes of metal inert gas (MIG) welding and tungsten inert gas (TIG) welding for duplex stainless steel (DSS) and low alloy steel were compared in this paper. The microstructure and corrosion morphology of dissimilar weld joints were observed by scanning electron microscopy (SEM); the chemical compositions in different zones were detected by energy-dispersive spectroscopy (EDS); the mechanical properties were measured by microhardness test, tensile test, and impact test; the corrosion behavior was evaluated by polarization curves. Obvious concentration gradients of Ni and Cr exist between the fusion boundary and the type II boundary, where the hardness is much higher. The impact toughness of weld metal by MIG welding is higher than that by TIG welding. The corrosion current density of TIG weld metal is higher than that of MIG weld metal in a 3.5wt% NaCl solution. Galvanic corrosion happens between low alloy steel and weld metal, revealing the weakness of low alloy steel in industrial service. The quality of joints produced by MIG welding is better than that by TIG welding in mechanical performance and corrosion resistance. MIG welding with the filler metal ER2009 is the suitable welding process for dissimilar metals jointing between UNS S31803 duplex stainless steel and low alloy steel in practical application.

  2. Effect of Heat Input on Geometry of Austenitic Stainless Steel Weld Bead on Low Carbon Steel

    NASA Astrophysics Data System (ADS)

    Saha, Manas Kumar; Hazra, Ritesh; Mondal, Ajit; Das, Santanu

    2018-05-01

    Among different weld cladding processes, gas metal arc welding (GMAW) cladding becomes a cost effective, user friendly, versatile method for protecting the surface of relatively lower grade structural steels from corrosion and/or erosion wear by depositing high grade stainless steels onto them. The quality of cladding largely depends upon the bead geometry of the weldment deposited. Weld bead geometry parameters, like bead width, reinforcement height, depth of penetration, and ratios like reinforcement form factor (RFF) and penetration shape factor (PSF) determine the quality of the weld bead geometry. Various process parameters of gas metal arc welding like heat input, current, voltage, arc travel speed, mode of metal transfer, etc. influence formation of bead geometry. In the current experimental investigation, austenite stainless steel (316) weld beads are formed on low alloy structural steel (E350) by GMAW using 100% CO2 as the shielding gas. Different combinations of current, voltage and arc travel speed are chosen so that heat input increases from 0.35 to 0.75 kJ/mm. Nine number of weld beads are deposited and replicated twice. The observations show that weld bead width increases linearly with increase in heat input, whereas reinforcement height and depth of penetration do not increase with increase in heat input. Regression analysis is done to establish the relationship between heat input and different geometrical parameters of weld bead. The regression models developed agrees well with the experimental data. Within the domain of the present experiment, it is observed that at higher heat input, the weld bead gets wider having little change in penetration and reinforcement; therefore, higher heat input may be recommended for austenitic stainless steel cladding on low alloy steel.

  3. Parametric Optimization Of Gas Metal Arc Welding Process By Using Grey Based Taguchi Method On Aisi 409 Ferritic Stainless Steel

    NASA Astrophysics Data System (ADS)

    Ghosh, Nabendu; Kumar, Pradip; Nandi, Goutam

    2016-10-01

    Welding input process parameters play a very significant role in determining the quality of the welded joint. Only by properly controlling every element of the process can product quality be controlled. For better quality of MIG welding of Ferritic stainless steel AISI 409, precise control of process parameters, parametric optimization of the process parameters, prediction and control of the desired responses (quality indices) etc., continued and elaborate experiments, analysis and modeling are needed. A data of knowledge - base may thus be generated which may be utilized by the practicing engineers and technicians to produce good quality weld more precisely, reliably and predictively. In the present work, X-ray radiographic test has been conducted in order to detect surface and sub-surface defects of weld specimens made of Ferritic stainless steel. The quality of the weld has been evaluated in terms of yield strength, ultimate tensile strength and percentage of elongation of the welded specimens. The observed data have been interpreted, discussed and analyzed by considering ultimate tensile strength ,yield strength and percentage elongation combined with use of Grey-Taguchi methodology.

  4. Nd:YAG laser welding of coated sheet steel

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Graham, M.P.; Kerr, H.W.; Weckman, D.C.

    1994-12-31

    Coated sheet steels are used extensively in the automotive industry for the fabrication of automobile body components; however, their reduced weldability by the traditional welding processes has led to numerous studies into the use of alternate process such as laser welding. In this paper, we present a modified joint geometry which allows high quality lap welds of coated sheet steels to be made by laser welding processes. Hot-dipped galvanized sheet (16 gauge), with a 60 g/m zinc coating was used in this study. A groove was created in the top sheet of a specimen pair by pressing piano wires ofmore » various diameters into the sheet. The specimens were clamped together in a lag-joint configuration such that they were in contacted only along the grove projection. A parametric study was conducted using the variables of welding speed, laser mean power (685 W, 1000 W and 1350 W), and grove size. Weld quality and weld pool dimensions were assessed using metallurgical cross-sections and image analysis techniques. Acceptable quality seam welds were produced in the galvanized sheet steel with both grove sizes when using 1000 W and 1350 W laser mean powers and a range of welding speeds. Results of the shear-tensile tests showed that high loads to failure, with failure occurring in the parent material, were predominately found in welds produced at speeds over 1.2 m/min and when using the high mean laser powers: 1000 W and 1350 W. A modified lap joint geometry, in which a groove is pre-placed in the top sheet of the lap-joint configuration, has been developed which permits laser welding of coated sheet steels. Good quality seam welds have been produced in 16 gauge galvanized sheet steels at speeds up to 2.7 m/min using a 2 kW CW Nd:YAG laser operating at 1350 W laser mean power. Weld quality was not affected by changes in groove size.« less

  5. Ductile Tearing Resistance Indexing of Automotive Grade DP 590 Steel Sheets: EWF Testing Using DENT Specimens

    NASA Astrophysics Data System (ADS)

    Sahoo, Subhadra; Padmapriya, N.; De, Partha Sarathi; Chakraborti, P. C.; Ray, S. K.

    2018-03-01

    The essential work of fracture (EWF) method has been explored for indexing the ductile tearing resistance of DP 590 automotive grade dual-phase steel sheet both in longitudinal (L-T) and transverse (T-L) orientations. The simplest possible test and analysis procedures have been adopted. The EWF method is found to be eminently suitable for routine quality control and product development purposes for such materials. Areas for further research for improving the experimental strategy are highlighted. For the investigated steel sheet, the estimated tearing resistance is found to be distinctly higher for the L-T orientation compared to the T-L orientation; the reason thereof merits further investigation.

  6. Research of Influence Modification of Natural Concentrate on Quality Metal

    NASA Astrophysics Data System (ADS)

    Fedoseev, S. N.; Gizatulin, R. A.; Korotkova, E. A.

    2016-08-01

    Questions of increase of mechanical, technological and service properties of metal at minimum cost to produce it are relevant for the metallurgical enterprises. Modification of complex steel alloys containing reactive elements is one of the effective ways to improve the quality of steel. At the same time the direct costs for the use of modifiers are 0.2-0.3%, which little effect on the cost of production. The paper presents the results of the application of natural concentrates as a modifier steel. The effects on the metal quality changes due to the impact of the modification concentrates demonstrate the effectiveness of their application. As a result of modification decreased the content of nonmetallic inclusions and grain size. Reduction of impurity modified metal of was the cause more high plastic properties, especially, impact strength at ordinary and low temperatures of tests. Based on the experimental data evaluated hardening mechanisms that lead to a significant improvement of physic-mechanical properties of the metal workpiece after administration modifier.

  7. Experimental investigation of the effect of the laser beam polarization state on the quality of steel sheet cutting

    NASA Astrophysics Data System (ADS)

    Golyshev, A. A.; Orishich, A. M.; Shulyatyev, V. B.

    2017-10-01

    The paper presents the results of experimental investigation of the effect of the beam polarization on the quality of the oxygen-assisted laser cutting of steel by a CO2-laser. Under consideration is the effect of the laser cutting parameters by the beam with the linear polarization on the cut surface roughness. It is founded that the minimal roughness is reached when the electric field vector is perpendicular to the cutting speed vector. It is concluded that the absorbed power distribution imposes the essential influence on the surface quality, and that the radiation heating of side walls is important to have lower roughness. Obtained results enabled to present probable reasons of the worse surface quality of the metals cut by a fiber laser than the ones cut by a CO2-laser.

  8. Competition and product quality in the supermarket industry.

    PubMed

    Matsa, David A

    2011-01-01

    This article analyzes the effect of competition on a supermarket firm's incentive to provide product quality. In the supermarket industry, product availability is an important measure of quality. Using U.S. Consumer Price Index microdata to track inventory shortfalls, I find that stores facing more intense competition have fewer shortfalls. Competition from Walmart—the most significant shock to industry market structure in half a century—decreased shortfalls among large chains by about a third. The risk that customers will switch stores appears to provide competitors with a strong incentive to invest in product quality.

  9. Intelligent Systems Approaches to Product Sound Quality Analysis

    NASA Astrophysics Data System (ADS)

    Pietila, Glenn M.

    As a product market becomes more competitive, consumers become more discriminating in the way in which they differentiate between engineered products. The consumer often makes a purchasing decision based on the sound emitted from the product during operation by using the sound to judge quality or annoyance. Therefore, in recent years, many sound quality analysis tools have been developed to evaluate the consumer preference as it relates to a product sound and to quantify this preference based on objective measurements. This understanding can be used to direct a product design process in order to help differentiate the product from competitive products or to establish an impression on consumers regarding a product's quality or robustness. The sound quality process is typically a statistical tool that is used to model subjective preference, or merit score, based on objective measurements, or metrics. In this way, new product developments can be evaluated in an objective manner without the laborious process of gathering a sample population of consumers for subjective studies each time. The most common model used today is the Multiple Linear Regression (MLR), although recently non-linear Artificial Neural Network (ANN) approaches are gaining popularity. This dissertation will review publicly available published literature and present additional intelligent systems approaches that can be used to improve on the current sound quality process. The focus of this work is to address shortcomings in the current paired comparison approach to sound quality analysis. This research will propose a framework for an adaptive jury analysis approach as an alternative to the current Bradley-Terry model. The adaptive jury framework uses statistical hypothesis testing to focus on sound pairings that are most interesting and is expected to address some of the restrictions required by the Bradley-Terry model. It will also provide a more amicable framework for an intelligent systems approach

  10. 19 CFR 360.101 - Steel import licensing.

    Code of Federal Regulations, 2010 CFR

    2010-04-01

    ... Customs Duties INTERNATIONAL TRADE ADMINISTRATION, DEPARTMENT OF COMMERCE STEEL IMPORT MONITORING AND... timely completion of entry. (c) Foreign Trade Zone entries. All shipments of covered steel products into a foreign trade zones (FTZ), known as FTZ admissions, will require an import license prior to the...

  11. 19 CFR 360.101 - Steel import licensing.

    Code of Federal Regulations, 2014 CFR

    2014-04-01

    ... Customs Duties INTERNATIONAL TRADE ADMINISTRATION, DEPARTMENT OF COMMERCE STEEL IMPORT MONITORING AND... timely completion of entry. (c) Foreign Trade Zone entries. All shipments of covered steel products into a foreign trade zones (FTZ), known as FTZ admissions, will require an import license prior to the...

  12. 19 CFR 360.101 - Steel import licensing.

    Code of Federal Regulations, 2012 CFR

    2012-04-01

    ... Customs Duties INTERNATIONAL TRADE ADMINISTRATION, DEPARTMENT OF COMMERCE STEEL IMPORT MONITORING AND... timely completion of entry. (c) Foreign Trade Zone entries. All shipments of covered steel products into a foreign trade zones (FTZ), known as FTZ admissions, will require an import license prior to the...

  13. 19 CFR 360.101 - Steel import licensing.

    Code of Federal Regulations, 2011 CFR

    2011-04-01

    ... Customs Duties INTERNATIONAL TRADE ADMINISTRATION, DEPARTMENT OF COMMERCE STEEL IMPORT MONITORING AND... timely completion of entry. (c) Foreign Trade Zone entries. All shipments of covered steel products into a foreign trade zones (FTZ), known as FTZ admissions, will require an import license prior to the...

  14. 19 CFR 360.101 - Steel import licensing.

    Code of Federal Regulations, 2013 CFR

    2013-04-01

    ... Customs Duties INTERNATIONAL TRADE ADMINISTRATION, DEPARTMENT OF COMMERCE STEEL IMPORT MONITORING AND... timely completion of entry. (c) Foreign Trade Zone entries. All shipments of covered steel products into a foreign trade zones (FTZ), known as FTZ admissions, will require an import license prior to the...

  15. Experimental und numerical investigations on cooling efficiency of Air-Mist nozzles on steel during continuous casting

    NASA Astrophysics Data System (ADS)

    Arth, G.; Taferner, M.; Bernhard, C.; Michelic, S.

    2016-07-01

    Cooling strategies in continuous casting of steel can vary from rapid cooling to slow cooling, mainly controlled by adjusting the amount of water sprayed onto the surface of the product. Inadequate adjustment however can lead to local surface undercooling or reheating, leading to surface and inner defects. This paper focuses on cooling efficiency of Air-Mist nozzles on casted steel and the experimental and numerical prediction of surface temperature distributions over the product width. The first part explains the determination of heat transfer coefficients (HTC) on laboratory scale, using a so called nozzle measuring stand (NMS). Based on measured water distributions and determined HTC's for air-mist nozzles using the NMS, surface temperatures are calculated by a transient 2D-model on a simple steel plate, explained in the second part of this paper. Simulations are carried out varying water impact density and spray water distribution, consequently influencing the local HTC distribution over the plate width. Furthermore, these results will be interpreted with regard to their consequence for surface and internal quality of the cast product. The results reveal the difficulty of correct adjustment of the amount of sprayed water, concurrent influencing water distribution and thus changing HTC distribution and surface temperature.

  16. 77 FR 72827 - Corrosion-Resistant Carbon Steel Flat Products From Germany and the Republic of Korea: Final...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-12-06

    ... carbon steel flat products (``CORE'') from Germany and the Republic of Korea (``Korea'').\\1\\ We received... On January 3, 2012, the Department initiated the third sunset review of the AD orders on CORE from... respondent in either of the sunset reviews of the AD orders on CORE from Germany and Korea. As a result...

  17. Insight into the product film formed on Ni-advanced weathering steel in a tropical marine atmosphere

    NASA Astrophysics Data System (ADS)

    Wu, Wei; Cheng, Xuequn; Hou, Huaxing; Liu, Bo; Li, Xiaogang

    2018-04-01

    The product film formed on Ni-advanced weathering steel in a tropical marine environment was investigated in detail through outdoor exposure by using diverse surface analysis techniques combined with electrochemical impedance spectroscopy and scanning kelvin probe measurements. The results showed that the product film was mainly composed of nanophasic goethite in the inner layer and maghemite, akaganeite, and hematite in the outer layer. Moreover, the resistance to atmospheric corrosion gradually increased from the outermost product film to the innermost film. Ni was significantly enriched in the inner layer in the form of the spinel phase NiFe2O4, which transformed lepidocrocite to fine-grained goethite, withstood the invasion of chloridion, and improved the corrosion potential of the product film in a tropical marine atmosphere.

  18. On-line welding quality inspection system for steel pipe based on machine vision

    NASA Astrophysics Data System (ADS)

    Yang, Yang

    2017-05-01

    In recent years, high frequency welding has been widely used in production because of its advantages of simplicity, reliability and high quality. In the production process, how to effectively control the weld penetration welding, ensure full penetration, weld uniform, so as to ensure the welding quality is to solve the problem of the present stage, it is an important research field in the field of welding technology. In this paper, based on the study of some methods of welding inspection, a set of on-line welding quality inspection system based on machine vision is designed.

  19. Measuring Software Product Quality: The ISO 25000 Series and CMMI

    DTIC Science & Technology

    2004-06-14

    performance objectives” covers objectives and requirements for product quality, service quality , and process performance. Process performance objectives...such that product quality, service quality , and process performance attributes are measurable and controlled throughout the project (internal and

  20. How Will Copper Contamination Constrain Future Global Steel Recycling?

    PubMed

    Daehn, Katrin E; Cabrera Serrenho, André; Allwood, Julian M

    2017-06-06

    Copper in steel causes metallurgical problems, but is pervasive in end-of-life scrap and cannot currently be removed commercially once in the melt. Contamination can be managed to an extent by globally trading scrap for use in tolerant applications and dilution with primary iron sources. However, the viability of long-term strategies can only be evaluated with a complete characterization of copper in the global steel system and this is presented in this paper. The copper concentration of flows along the 2008 steel supply chain is estimated from a survey of literature data and compared with estimates of the maximum concentration that can be tolerated in steel products. Estimates of final steel demand and scrap supply by sector are taken from a global stock-saturation model to determine when the amount of copper in the steel cycle will exceed that which can be tolerated. Best estimates show that quantities of copper arising from conventional scrap preparation can be managed in the global steel system until 2050 assuming perfectly coordinated trade and extensive dilution, but this strategy will become increasingly impractical. Technical and policy interventions along the supply chain are presented to close product loops before this global constraint.

  1. Pharmaceutical quality by design: product and process development, understanding, and control.

    PubMed

    Yu, Lawrence X

    2008-04-01

    The purpose of this paper is to discuss the pharmaceutical Quality by Design (QbD) and describe how it can be used to ensure pharmaceutical quality. The QbD was described and some of its elements identified. Process parameters and quality attributes were identified for each unit operation during manufacture of solid oral dosage forms. The use of QbD was contrasted with the evaluation of product quality by testing alone. The QbD is a systemic approach to pharmaceutical development. It means designing and developing formulations and manufacturing processes to ensure predefined product quality. Some of the QbD elements include: Defining target product quality profile; Designing product and manufacturing processes; Identifying critical quality attributes, process parameters, and sources of variability; Controlling manufacturing processes to produce consistent quality over time. Using QbD, pharmaceutical quality is assured by understanding and controlling formulation and manufacturing variables. Product testing confirms the product quality. Implementation of QbD will enable transformation of the chemistry, manufacturing, and controls (CMC) review of abbreviated new drug applications (ANDAs) into a science-based pharmaceutical quality assessment.

  2. 46 CFR 164.120-11 - Production quality control requirements.

    Code of Federal Regulations, 2014 CFR

    2014-10-01

    ... 46 Shipping 6 2014-10-01 2014-10-01 false Production quality control requirements. 164.120-11... Rescue Boats § 164.120-11 Production quality control requirements. The resin manufacturer must institute a quality control procedure to ensure that all Coast Guard-accepted resin is produced to the same...

  3. 46 CFR 164.120-11 - Production quality control requirements.

    Code of Federal Regulations, 2012 CFR

    2012-10-01

    ... 46 Shipping 6 2012-10-01 2012-10-01 false Production quality control requirements. 164.120-11... Rescue Boats § 164.120-11 Production quality control requirements. The resin manufacturer must institute a quality control procedure to ensure that all Coast Guard-accepted resin is produced to the same...

  4. 46 CFR 164.120-11 - Production quality control requirements.

    Code of Federal Regulations, 2013 CFR

    2013-10-01

    ... 46 Shipping 6 2013-10-01 2013-10-01 false Production quality control requirements. 164.120-11... Rescue Boats § 164.120-11 Production quality control requirements. The resin manufacturer must institute a quality control procedure to ensure that all Coast Guard-accepted resin is produced to the same...

  5. MaTrace: tracing the fate of materials over time and across products in open-loop recycling.

    PubMed

    Nakamura, Shinichiro; Kondo, Yasushi; Kagawa, Shigemi; Matsubae, Kazuyo; Nakajima, Kenichi; Nagasaka, Tetsuya

    2014-07-01

    Even for metals, open-loop recycling is more common than closed-loop recycling due, among other factors, to the degradation of quality in the end-of-life (EoL) phase. Open-loop recycling is subject to loss of functionality of original materials, dissipation in forms that are difficult to recover, and recovered metals might need dilution with primary metals to meet quality requirements. Sustainable management of metal resources calls for the minimization of these losses. Imperative to this is quantitative tracking of the fate of materials across different stages, products, and losses. A new input-output analysis (IO) based model of dynamic material flow analysis (MFA) is presented that can trace the fate of materials over time and across products in open-loop recycling taking explicit consideration of losses and the quality of scrap into account. Application to car steel recovered from EoL vehicles (ELV) showed that after 50 years around 80% of the steel is used in products, mostly buildings and civil engineering (infrastructure), with the rest mostly resided in unrecovered obsolete infrastructure and refinery losses. Sensitivity analysis was conducted to evaluate the effects of changes in product lifespan, and the quality of scrap.

  6. Steel selection for UBC steel bridge

    NASA Astrophysics Data System (ADS)

    Liu, Haoyu

    2018-03-01

    This report conducts a material selection of different types of steel for UBC Steel Bridge Team. I am a third-year material engineering student, so the result from this material selection can only be taken into consideration but not fully adopted. As part of my academic journey, it is possible for technical mistakes in this material selection process. The mechanic properties are the most effective category of properties, making it necessary to be justified from the steel bridge design and chosen in accordance with the objective of the team. An introduction for currently-used steel properties and the expected steel properties is provided. The examination focus on how different alloy compositions of steel changes its properties. The properties of the steel are examined in three main aspects: hardness, strength, and toughness. The results suggest that more nickel, manganese, and chromium in the steel provide better steel for the team to use. Further research is needed if a more precise material selection is required.

  7. Bearing and gear steels for aerospace applications

    NASA Technical Reports Server (NTRS)

    Zaretsky, Erwin V.

    1990-01-01

    Research in metallurgy and processing for bearing and gear steels has resulted in improvements in rolling-element bearing and gear life for aerospace application by a factor of approximately 200 over that obtained in the early 1940's. The selection and specification of a bearing or gear steel is dependent on the integration of multiple metallurgical and physical variables. For most aerospace bearings, through-hardened VIM-VAR AISI M-50 steel is the material of preference. For gears, the preferential material is case-carburized VAR AISI 9310. However, the VAR processing for this material is being replaced by VIM-VAR processing. Since case-carburized VIM-VAR M-50NiL incorporates the desirable qualities of both the AISI M-50 and AISI 9310 materials, optimal life and reliability can be achieved in both bearings and gears with a single steel. Hence, this material offers the promise of a common steel for both bearings and gears for future aerospace applications.

  8. Assessment of recovery and recrystallisation behaviours of cold rolled IF steel through non-destructive electromagnetic characterisation

    NASA Astrophysics Data System (ADS)

    Roy, Rajat K.; Dutta, Siuli; Panda, Ashis K.; Rajinikanth, V.; Das, Swapan K.; Mitra, Amitava; Strangwood, M.; Davis, Claire L.

    2018-07-01

    The recovery and recrystallisation behaviours of cold rolled IF steel have been investigated by destructive (optical microscopy and hardness) and non-destructive electromagnetic sensor, (which allows direct measurement of strip samples with no surface preparation) techniques. The onset and completion of recrystallisation are clearly monitored through destructive techniques of optical microscopy and hardness measurements. The nucleation of new recrystallised grains is observed in the sample annealed at 600 °C/15 min, while completion of recrystallisation takes place at 700 °C/15 min. The destructive techniques are not very accurate in monitoring recovery, for example, changes in hardness of <20% are seen. In contrast, the magnetic properties of annealed steel show the onsets of both recovery and recrystallisation, with recovery accounting for ≈60% change in the coercivity value. Therefore, the measurement of magnetic softening through an electromagnetic sensor acts a crucial role for understanding recovery and recrystallisation behaviours of steels during industrial processing. The present investigation is aimed not only for controlling product quality but also saving characterisation time through off line monitoring during steel processing at industry.

  9. Steel bridge fabrication technologies in Europe and Japan

    DOT National Transportation Integrated Search

    2001-03-01

    The objective of this scanning tour was to conduct a broad overview of newly developed manufacturing techniques that are in use abroad for steel bridge fabrication and erection. The trip focused on the role of steel production, design, innovation, an...

  10. The optimization of CNT-PVA nanocomposite for mild steel coating: Effect of CNTs concentration on the corrosion rate of mild steel

    NASA Astrophysics Data System (ADS)

    Maryam, M.; Ibrahim, N. M. A. A.; Eswar, K. A.; Guliling, M.; Suhaimi, M. H. F.; Khusaimi, Z.; Abdullah, S.; Rusop, M.

    2018-05-01

    Carbon Nanotubes (CNTs) are molecular-scale tubes of graphitic carbon which have outstanding mechanical and magnetic properties with extraordinary strength. It can be said that CNTs can be used in coating application to prevent corrosion and lower the rate of corrosion on steel. However, CNT alone cannot be used for coating purposes. Therefore, by combining it with polymer to produce a nanocomposite thin film, it can be used for nanocoating on mild steel substrate. Polyvinyl alcohol (PVA) was chosen due to its high strength and high modulus polymer fibers and has the possibilities of improving the physicochemical properties of carbon nanotubes. Carbon nanotubes and polyvinyl alcohol (CNT-PVA) nanocomposite were prepared by using sol-gel method and coated as thin film on mild steel substrate by using spin coating. Sol-gel is a convenient technique used for the production of nanocomposite aqueous solution. Five samples were prepared at the different concentration of CNTs-PVA to verify the corrosion rate application. The samples were then characterized by Field Emission Scanning Electron Microscopy (FESEM) and Atomic Force Microscopy (AFM) obtaining the structural properties, surface morphology and topography of samples. Raman spectroscopy was used to determine the microraman spectra of CNTs which showed the quality and purity of samples. Finally, corrosion test was done to measure the corrosion rate of samples at the different concentration of CNTs/PVA nanocomposite.

  11. Capabilities of Unconventional Processing of Multiphase AHSS Steels

    NASA Astrophysics Data System (ADS)

    Jirkova, H.; Masek, B.; Stadler, C.; Jenicek, S.

    2016-03-01

    Today, new types of materials and procedures are sought continuously in order to achieve lower manufacturing costs, reduced energy consumption, shorter production times and other savings. In terms of the materials, TRIP steels are an attractive choice, as they provide an excellent combination of strength and ductility. They also offer good energy absorption in crash scenarios. Their main use is in the production of automotive body parts. One can expect that well-chosen processing parameters and unconventional forming routes would enable a wider range of thin-walled products to be made of these steels. Those could include thin-walled hollow products with excellent mechanical properties imparted by effective manufacturing routes at relatively low costs. If these materials are to be employed in real-world forming processes, an appropriate forming route must be chosen, integrated into an appropriate production chain and then optimized in terms of its parameters. This article describes a study of a rotary spin extrusion process. In the first stage, the impact of strain magnitude on microstructural evolution was studied in CMnSi steel using physical modelling of thermomechanical treatment. Subsequently, trials of a real-life technology chain, which efficiently combined incremental forming and heat treatment, were carried out on low-alloy CMnSi and CMnSiNb steels. The resulting products were stepped hollow parts of various diameters. Their strength was close to 1000 MPa and their elongation level exceeded 20%.

  12. Ensuring and Improving Information Quality for Earth Science Data and Products Role of the ESIP Information Quality Cluster

    NASA Technical Reports Server (NTRS)

    Ramapriyan, H. K. (Rama); Peng, Ge; Moroni, David; Shie, Chung-Lin

    2016-01-01

    Quality of products is always of concern to users regardless of the type of products. The focus of this paper is on the quality of Earth science data products. There are four different aspects of quality scientific, product, stewardship and service. All these aspects taken together constitute Information Quality. With increasing requirement on ensuring and improving information quality, there has been considerable work related to information quality during the last several years. Given this rich background of prior work, the Information Quality Cluster (IQC), established within the Federation of Earth Science Information Partners (ESIP) has been active with membership from multiple organizations. Its objectives and activities, aimed at ensuring and improving information quality for Earth science data and products, are discussed briefly.

  13. Ensuring and Improving Information Quality for Earth Science Data and Products: Role of the ESIP Information Quality Cluster

    NASA Technical Reports Server (NTRS)

    Ramapriyan, Hampapuram; Peng, Ge; Moroni, David; Shie, Chung-Lin

    2016-01-01

    Quality of products is always of concern to users regardless of the type of products. The focus of this paper is on the quality of Earth science data products. There are four different aspects of quality - scientific, product, stewardship and service. All these aspects taken together constitute Information Quality. With increasing requirement on ensuring and improving information quality, there has been considerable work related to information quality during the last several years. Given this rich background of prior work, the Information Quality Cluster (IQC), established within the Federation of Earth Science Information Partners (ESIP) has been active with membership from multiple organizations. Its objectives and activities, aimed at ensuring and improving information quality for Earth science data and products, are discussed briefly.

  14. Steel: Price and Policy Issues

    DTIC Science & Technology

    2006-08-31

    former North Star mills in Minnesota and Iowa, but operations have continued without a new replacement contract.28 World Steel Output Totals At the...supply contracts for the coming year, Nippon Steel agreed to an unprecedented 71.5% price increase with the large Brazilian iron mining company, CVRD...production, which is in the form of taconite that is subsequently pelletized, increased in 2004-05. After averaging less than 50 million MT in 2001-03

  15. Distribution of Stress in Deformation Zone of Niobium Microalloyed Steel

    NASA Astrophysics Data System (ADS)

    Jandrlić, Ivan; Rešković, Stoja; Brlić, Tin

    2018-03-01

    Microalloyed steels today represent a significant part of total world production and processing of steel. Although widely used, there are scarce data on the stress distribution in the deformation zone of these steels. Research was carried out on two steel grades, both low-carbon structural steels with the same basic chemical composition, with one of them additionally microalloyed with niobium. Differences in the stress distribution in the deformation zone between two tested steels were continuously observed and measured using the methods of digital image correlation and thermography. It has been found out that niobium microalloyed steel has significantly more complex material flow and stress distribution in the deformation zone when compared to the plain low carbon steel.

  16. Distribution of Stress in Deformation Zone of Niobium Microalloyed Steel

    NASA Astrophysics Data System (ADS)

    Jandrlić, Ivan; Rešković, Stoja; Brlić, Tin

    2018-07-01

    Microalloyed steels today represent a significant part of total world production and processing of steel. Although widely used, there are scarce data on the stress distribution in the deformation zone of these steels. Research was carried out on two steel grades, both low-carbon structural steels with the same basic chemical composition, with one of them additionally microalloyed with niobium. Differences in the stress distribution in the deformation zone between two tested steels were continuously observed and measured using the methods of digital image correlation and thermography. It has been found out that niobium microalloyed steel has significantly more complex material flow and stress distribution in the deformation zone when compared to the plain low carbon steel.

  17. Private Relations' Last Stand: U.S. Steel vs. the U.S.A..

    ERIC Educational Resources Information Center

    Olasky, Marvin N.

    1987-01-01

    Discusses how (1) the "private relations" that existed between U.S. Steel and the government between 1930 and 1960 ended in steel crisis of 1962 and (2) this policy was viewed as inadequate by both an angry public and the Kennedy Administration when the steel industry tried to match foreign competition on quality and prices by raising…

  18. Water quality assessment of bioenergy production

    Treesearch

    Rocio Diaz-Chavez; Goran Berndes; Dan Neary; Andre Elia Neto; Mamadou Fall

    2011-01-01

    Water quality is a measurement of the biological, chemical, and physical characteristics of water against certain standards set to ensure ecological and/or human health. Biomass production and conversion to fuels and electricity can impact water quality in lakes, rivers, and aquifers with consequences for aquatic ecosystem health and also human water uses. Depending on...

  19. New high-strength steels

    NASA Astrophysics Data System (ADS)

    Belyakov, L. N.; Petrakov, A. F.; Pokrovskaya, N. G.; Shal'kevich, A. B.

    1998-08-01

    Steels have found wide application in modern aircraft and are the profile materials in some structures. They are used when a high specific strength, rigidity, fatigue limit, and high-temperature strength are required, for example, in the production of wing bars, longerons, ribs, landing gear parts, and gear transmission mechanisms. Steels used in the aircraft industry should possess high parameters of fracture toughness, crack resistance under static and cyclic loads, and corrosion resistance (for the all-climatic variant) with preservation of a high adaptability to manufacturing (weldability, forgeability, processability).

  20. Advancement in modern approaches to mineral production quality control

    NASA Astrophysics Data System (ADS)

    Freidina, EV; Botvinnik, AA; Dvornikova, AN

    2017-02-01

    The natural resource potential of mineral deposits is represented by three categories: upside, attainable and investment. A modern methodology is proposed in this paper for production quality control, and its tools aimed at ensuring agreement between the product quality and the market requirements are described. The definitions of the costs of the product quality compliance and incompliance with the consumer requirements are introduced; the latter is suggested to use in evaluating resource potential of mineral deposits at a certain degree of probability.

  1. [Aquaculture in Italy. An integrated model of product quality control].

    PubMed

    De Giusti, Maria; Cocchieri, Renata Amodio; De Vito, Elisabetta; Grasso, Guido Maria; Ortaggi, Giancarlo; Reali, Daniela; Ricciardi, Gualtiero; Romano-Spica, Vincenzo; Boccia, Antonio

    2007-01-01

    Aquaculture is becoming increasingly diffuse even in Italy. The increased production introduces new problems such as product quality control and process safety. This article presents the results of a research project, funded by the Ministry of the Environment, whose aim was to evaluate and promote aquaculture product quality and safety in an environmentally responsible way. Four intensive land-based and offshore aquaculture sites were monitored to evaluate microbiological, biological and chemical (i.e. polychlorinated biphenyls and endocrine disruptors) quality of water, products and fish feed. In total 154 samples were analysed, of which 66 were water samples, 55 product samples and 33 feed samples. Salmonella and other enteric pathogens were absent in products and the aquatic environment, while other environmental pathogens of the Vibrio species were detected. Bacterial load and fecal indicators were found to be higher in off-shore products and in mussels from all aquaculture sites. PCBs were detected in all products in concentrations below 2 microg/g fresh product (Food and Drug Administration), but on average, higher concentrations were detected in off-shore products. No estrogen mimetic activity was detected in fish feed, in contrast it was detected in offshore products and water. Product quality was found to be strictly correlated with the quality of the environment. Genetically modified organisms were detected in fish feed but no integration of genetic material in products occurred.

  2. Water Quality in the Production of Containerized Longleaf Pine Seedlings

    Treesearch

    David J. Moorhead; John M. Ruter

    2002-01-01

    The consistent production of quality container grown seedlings requires that key production variables be identified and controlled; otherwise, quality and the percentage of marketable plants will be erratic (Garber and Ruter 1993a). Additionally, production times and costs may increase unless production variables are monitored and managed throughout the production...

  3. Process performance and product quality in an integrated continuous antibody production process.

    PubMed

    Karst, Daniel J; Steinebach, Fabian; Soos, Miroslav; Morbidelli, Massimo

    2017-02-01

    Continuous manufacturing is currently being seriously considered in the biopharmaceutical industry as the possible new paradigm for producing therapeutic proteins, due to production cost and product quality related benefits. In this study, a monoclonal antibody producing CHO cell line was cultured in perfusion mode and connected to a continuous affinity capture step. The reliable and stable integration of the two systems was enabled by suitable control loops, regulating the continuous volumetric flow and adapting the operating conditions of the capture process. For the latter, an at-line HPLC measurement of the harvest concentration subsequent to the bioreactor was combined with a mechanistic model of the capture chromatographic unit. Thereby, optimal buffer consumption and productivity throughout the process was realized while always maintaining a yield above the target value of 99%. Stable operation was achieved at three consecutive viable cell density set points (20, 60, and 40 × 10 6 cells/mL), together with consistent product quality in terms of aggregates, fragments, charge isoforms, and N-linked glycosylation. In addition, different values for these product quality attributes such as N-linked glycosylation, charge variants, and aggregate content were measured at the different steady states. As expected, the amount of released DNA and HCP was significantly reduced by the capture step for all considered upstream operating conditions. This study is exemplary for the potential of enhancing product quality control and modulation by integrated continuous manufacturing. Biotechnol. Bioeng. 2017;114: 298-307. © 2016 Wiley Periodicals, Inc. © 2016 Wiley Periodicals, Inc.

  4. Effect of Isothermal Bainitic Quenching on Rail Steel Impact Strength and Wear Resistance

    NASA Astrophysics Data System (ADS)

    Çakir, Fatih Hayati; Çelik, Osman Nuri

    2017-09-01

    The effect of heat treatment regimes on hardness, impact strength, and wear resistance of rail steel for high-speed tracks (rail quality category R350HT) is studied. Analysis of steel properties with a different structure is compared: pearlitic, and upper and lower bainite. It is shown that the steel with bainitic structure has the best impact strength, but wear resistance is better for steel with a lower bainite structure.

  5. A deterministic aggregate production planning model considering quality of products

    NASA Astrophysics Data System (ADS)

    Madadi, Najmeh; Yew Wong, Kuan

    2013-06-01

    Aggregate Production Planning (APP) is a medium-term planning which is concerned with the lowest-cost method of production planning to meet customers' requirements and to satisfy fluctuating demand over a planning time horizon. APP problem has been studied widely since it was introduced and formulated in 1950s. However, in several conducted studies in the APP area, most of the researchers have concentrated on some common objectives such as minimization of cost, fluctuation in the number of workers, and inventory level. Specifically, maintaining quality at the desirable level as an objective while minimizing cost has not been considered in previous studies. In this study, an attempt has been made to develop a multi-objective mixed integer linear programming model that serves those companies aiming to incur the minimum level of operational cost while maintaining quality at an acceptable level. In order to obtain the solution to the multi-objective model, the Fuzzy Goal Programming approach and max-min operator of Bellman-Zadeh were applied to the model. At the final step, IBM ILOG CPLEX Optimization Studio software was used to obtain the experimental results based on the data collected from an automotive parts manufacturing company. The results show that incorporating quality in the model imposes some costs, however a trade-off should be done between the cost resulting from producing products with higher quality and the cost that the firm may incur due to customer dissatisfaction and sale losses.

  6. Product quality considerations for mammalian cell culture process development and manufacturing.

    PubMed

    Gramer, Michael J

    2014-01-01

    The manufacturing of a biologic drug from mammalian cells results in not a single substance, but an array of product isoforms, also known as variants. These isoforms arise due to intracellular or extracellular events as a result of biological or chemical modification. The most common examples related to biomanufacturing include amino acid modifications (glycosylation, isomerization, oxidation, adduct formation, pyroglutamate formation, phosphorylation, sulfation, amidation), amino acid sequence variants (genetic mutations, amino acid misincorporation, N- and C-terminal heterogeneity, clipping), and higher-order structure modifications (misfolding, aggregation, disulfide pairing). Process-related impurities (HCP, DNA, media components, viral particles) are also important quality attributes related to product safety. The observed ranges associated with each quality attribute define the product quality profile. A biologic drug must have a correct and consistent quality profile throughout clinical development and scale-up to commercial production to ensure product safety and efficacy. In general, the upstream process (cell culture) defines the quality of product-related substances, whereas the downstream process (purification) defines the residual level of process- and product-related impurities. The purpose of this chapter is to review the impact of the cell culture process on product quality. Emphasis is placed on studies with industrial significance and where the direct mechanism of product quality impact was determined. Where possible, recommendations for maintaining consistent or improved quality are provided.

  7. 49 CFR 178.45 - Specification 3T seamless steel cylinder.

    Code of Federal Regulations, 2012 CFR

    2012-10-01

    ..., or electric furnace process steel of uniform quality is authorized. The steel analysis must conform... inches in diameter. (4) All openings must be circular. (5) All openings must be threaded. Threads must be in compliance with the following: (i) Each thread must be clean cut, even, without any checks, and to...

  8. 49 CFR 178.45 - Specification 3T seamless steel cylinder.

    Code of Federal Regulations, 2014 CFR

    2014-10-01

    ..., or electric furnace process steel of uniform quality is authorized. The steel analysis must conform... inches in diameter. (4) All openings must be circular. (5) All openings must be threaded. Threads must be in compliance with the following: (i) Each thread must be clean cut, even, without any checks, and to...

  9. 49 CFR 178.45 - Specification 3T seamless steel cylinder.

    Code of Federal Regulations, 2013 CFR

    2013-10-01

    ..., or electric furnace process steel of uniform quality is authorized. The steel analysis must conform... inches in diameter. (4) All openings must be circular. (5) All openings must be threaded. Threads must be in compliance with the following: (i) Each thread must be clean cut, even, without any checks, and to...

  10. Review of Manganese Processing for Production of TRIP/TWIP Steels, Part 2: Reduction Studies

    NASA Astrophysics Data System (ADS)

    Elliott, R.; Coley, K.; Mostaghel, S.; Barati, M.

    2018-02-01

    Production of ultrahigh-manganese steels is expected to result in significant increase in demand for low-carbon (LC) ferromanganese (FeMn) and silicomanganese (SiMn). Current manganese processing techniques are energy intensive and typically yield a high-carbon product. The present work therefore reviews available literature regarding carbothermic reduction of Mn oxides and ores, with the objective of identifying opportunities for future process development to mitigate the cost of LC FeMn and SiMn. In general, there is consensus that carbothermic reduction of Mn oxides and ores is limited by gasification of carbon. Conditions which enhance or bypass this step (e.g., by application of CH4) show higher rates of reduction at lower temperatures. This phenomenon has potential application in solid-state reduction of Mn ore. Other avenues for process development include optimization of the prereduction step in conventional FeMn production and metallothermic reduction as a secondary reduction step.

  11. Analysis of Power Supply Heating Effect during High Temperature Experiments Based on the Electromagnetic Steel Teeming Technology

    NASA Astrophysics Data System (ADS)

    He, Ming; Wang, Qiang; Liu, Xin'an; Shi, Chunyang; Liu, Tie; He, Jicheng

    2017-04-01

    For further lowering inclusions and improving the quality of steel, a new electromagnetic steel-teeming technology based on electromagnetic induction heating was proposed. To assess the proposed technology, an experimental platform that imitates the actual production condition of steelmakers was established. High temperature experiments were performed to investigate the melting length of Fe-C alloy under different power and frequency conditions. The heating effect was analyzed, and the method of magnetic shielding to reduce the power loss of power supply was put forward. The results show that when the power is 40 kW and frequency is 25 kHz, the melting length of the Fe-C alloy is 89.2 mm in 120 s, which meets the requirements of steel teeming. In addition, when magnetic shielding material is installed under the induction coil, the power loss is reduced by about 64 %, effectively improving the heating effect of power supply.

  12. 76 FR 28419 - Certain Hot-Rolled Carbon Steel Flat Products From India: Notice of Extension of Time Limit for...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2011-05-17

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-533-820] Certain Hot-Rolled Carbon...-rolled carbon steel flat products from India for the period December 1, 2008, through November 30, 2009... September 14, 2010, in accordance with section 751(a)(3)(A) of the Tariff Act of 1930, as amended (the Act...

  13. Chromium-Makes stainless steel stainless

    USGS Publications Warehouse

    Kropschot, S.J.; Doebrich, Jeff

    2010-01-01

    Chromium, a steely-gray, lustrous, hard metal that takes a high polish and has a high melting point, is a silvery white, hard, and bright metal plating on steel and other material. Commonly known as chrome, it is one of the most important and indispensable industrial metals because of its hardness and resistance to corrosion. But it is used for more than the production of stainless steel and nonferrous alloys; it is also used to create pigments and chemicals used to process leather.

  14. Corrosion behavior of 2205 duplex stainless steel.

    PubMed

    Platt, J A; Guzman, A; Zuccari, A; Thornburg, D W; Rhodes, B F; Oshida, Y; Moore, B K

    1997-07-01

    The corrosion of 2205 duplex stainless steel was compared with that of AISI type 316L stainless steel. The 2205 stainless steel is a potential orthodontic bracket material with low nickel content (4 to 6 wt%), whereas the 316L stainless steel (nickel content: 10 to 14 wt%) is a currently used bracket material. Both stainless steels were subjected to electrochemical and immersion (crevice) corrosion tests in 37 degrees C, 0.9 wt% sodium chloride solution. Electrochemical testing indicates that 2205 has a longer passivation range than 316L. The corrosion rate of 2205 was 0.416 MPY (milli-inch per year), whereas 316L exhibited 0.647 MPY. When 2205 was coupled to 316L with equal surface area ratio, the corrosion rate of 2205 reduced to 0.260 MPY, indicating that 316L stainless steel behaved like a sacrificial anode. When 316L is coupled with NiTi, TMA, or stainless steel arch wire and was subjected to the immersion corrosion test, it was found that 316L suffered from crevice corrosion. On the other hand, 2205 stainless steel did not show any localized crevice corrosion, although the surface of 2205 was covered with corrosion products, formed when coupled to NiTi and stainless steel wires. This study indicates that considering corrosion resistance, 2205 duplex stainless steel is an improved alternative to 316L for orthodontic bracket fabrication when used in conjunction with titanium, its alloys, or stainless steel arch wires.

  15. Numerical simulation and experimental investigation of laser dissimilar welding of carbon steel and austenitic stainless steel

    NASA Astrophysics Data System (ADS)

    Nekouie Esfahani, M. R.; Coupland, J.; Marimuthu, S.

    2015-07-01

    This study reports an experimental and numerical investigation on controlling the microstructure and brittle phase formation during laser dissimilar welding of carbon steel to austenitic stainless steel. The significance of alloying composition and cooling rate were experimentally investigated. The investigation revealed that above a certain specific point energy the material within the melt pool is well mixed and the laser beam position can be used to control the mechanical properties of the joint. The heat-affected zone within the high-carbon steel has significantly higher hardness than the weld area, which severely undermines the weld quality. A sequentially coupled thermo-metallurgical model was developed to investigate various heat-treatment methodology and subsequently control the microstructure of the HAZ. Strategies to control the composition leading to dramatic changes in hardness, microstructure and service performance of the dissimilar laser welded fusion zone are discussed.

  16. Pharmaceutical product development: A quality by design approach

    PubMed Central

    Pramod, Kannissery; Tahir, M. Abu; Charoo, Naseem A.; Ansari, Shahid H.; Ali, Javed

    2016-01-01

    The application of quality by design (QbD) in pharmaceutical product development is now a thrust area for the regulatory authorities and the pharmaceutical industry. International Conference on Harmonization and United States Food and Drug Administration (USFDA) emphasized the principles and applications of QbD in pharmaceutical development in their guidance for the industry. QbD attributes are addressed in question-based review, developed by USFDA for chemistry, manufacturing, and controls section of abbreviated new drug applications. QbD principles, when implemented, lead to a successful product development, subsequent prompt regulatory approval, reduce exhaustive validation burden, and significantly reduce post-approval changes. The key elements of QbD viz., target product quality profile, critical quality attributes, risk assessments, design space, control strategy, product lifecycle management, and continual improvement are discussed to understand the performance of dosage forms within design space. Design of experiments, risk assessment tools, and process analytical technology are also discussed for their role in QbD. This review underlines the importance of QbD in inculcating science-based approach in pharmaceutical product development. PMID:27606256

  17. Pharmaceutical product development: A quality by design approach.

    PubMed

    Pramod, Kannissery; Tahir, M Abu; Charoo, Naseem A; Ansari, Shahid H; Ali, Javed

    2016-01-01

    The application of quality by design (QbD) in pharmaceutical product development is now a thrust area for the regulatory authorities and the pharmaceutical industry. International Conference on Harmonization and United States Food and Drug Administration (USFDA) emphasized the principles and applications of QbD in pharmaceutical development in their guidance for the industry. QbD attributes are addressed in question-based review, developed by USFDA for chemistry, manufacturing, and controls section of abbreviated new drug applications. QbD principles, when implemented, lead to a successful product development, subsequent prompt regulatory approval, reduce exhaustive validation burden, and significantly reduce post-approval changes. The key elements of QbD viz., target product quality profile, critical quality attributes, risk assessments, design space, control strategy, product lifecycle management, and continual improvement are discussed to understand the performance of dosage forms within design space. Design of experiments, risk assessment tools, and process analytical technology are also discussed for their role in QbD. This review underlines the importance of QbD in inculcating science-based approach in pharmaceutical product development.

  18. Quality and Safety Aspects of Cereals (Wheat) and Their Products.

    PubMed

    Varzakas, Theo

    2016-11-17

    Cereals and, most specifically, wheat are described in this chapter highlighting on their safety and quality aspects. Moreover, wheat quality aspects are adequately addressed since they are used to characterize dough properties and baking quality. Determination of dough properties is also mentioned and pasta quality is also described in this chapter. Chemometrics-multivariate analysis is one of the analyses carried out. Regarding production weighing/mixing of flours, kneading, extruded wheat flours, and sodium chloride are important processing steps/raw materials used in the manufacturing of pastry products. Staling of cereal-based products is also taken into account. Finally, safety aspects of cereal-based products are well documented with special emphasis on mycotoxins, acrylamide, and near infrared methodology.

  19. Perfusion seed cultures improve biopharmaceutical fed-batch production capacity and product quality.

    PubMed

    Yang, William C; Lu, Jiuyi; Kwiatkowski, Chris; Yuan, Hang; Kshirsagar, Rashmi; Ryll, Thomas; Huang, Yao-Ming

    2014-01-01

    Volumetric productivity and product quality are two key performance indicators for any biopharmaceutical cell culture process. In this work, we showed proof-of-concept for improving both through the use of alternating tangential flow perfusion seed cultures coupled with high-seed fed-batch production cultures. First, we optimized the perfusion N-1 stage, the seed train bioreactor stage immediately prior to the production bioreactor stage, to minimize the consumption of perfusion media for one CHO cell line and then successfully applied the optimized perfusion process to a different CHO cell line. Exponential growth was observed throughout the N-1 duration, reaching >40 × 10(6) vc/mL at the end of the perfusion N-1 stage. The cultures were subsequently split into high-seed (10 × 10(6) vc/mL) fed-batch production cultures. This strategy significantly shortened the culture duration. The high-seed fed-batch production processes for cell lines A and B reached 5 g/L titer in 12 days, while their respective low-seed processes reached the same titer in 17 days. The shortened production culture duration potentially generates a 30% increase in manufacturing capacity while yielding comparable product quality. When perfusion N-1 and high-seed fed-batch production were applied to cell line C, higher levels of the active protein were obtained, compared to the low-seed process. This, combined with correspondingly lower levels of the inactive species, can enhance the overall process yield for the active species. Using three different CHO cell lines, we showed that perfusion seed cultures can optimize capacity utilization and improve process efficiency by increasing volumetric productivity while maintaining or improving product quality. © 2014 American Institute of Chemical Engineers.

  20. Productivity, Quality, and Patient Satisfaction

    PubMed Central

    Fairchild, David G; McLoughlin, Karen Sax; Gharib, Soheyla; Horsky, Jan; Portnow, Michelle; Richter, James; Gagliano, Nancy; Bates, David W

    2001-01-01

    CONTEXT Although few data are available, many believe that part-time primary care physicians (PCPs) are less productive and provide lower quality care than full-time PCPs. Some insurers exclude part-time PCPs from their provider networks. OBJECTIVE To compare productivity, qualtiy of preventive care, patient satisfaction, and risk-adjusted resource utilization of part-time and full-time PCPs. DESIGN Retrospective cohort study. SETTING Boston. PARTICIPANTS PCPs affiliated with 2 academic outpatient primary care networks. MEASUREMENTS PCP productivity, patient satisfaction, resource utilization, and compliance with screening guidelines. RESULTS Part-time PCP productivity was greater than that of full-time PCPs (2.1 work relative value units (RVUs)/bookable clinical hour versus 1.3 work RVUs/bookable clinical hour, P < .01). A similar proportion of part-time PCPs (80%) and full-time PCPs (75%) met targets for mammography, Pap smears, and cholesterol screening (P = .67). After adjusting for clinical case mix, practice location, gender, board certification status, and years in practice, resource utilization of part-time PCPs ($138 [95% confidence interval (CI), $108 to $167]) was similar to that of full-time PCPs ($139 [95% CI, $108 to $170], P = .92). Patient satisfation was similar for part-time and full-time PCPs. CONCLUSIONS In these academic primary care practices, rates of patient satisfaction, compliance with screenig guidelines, and resource utilization were similar for part-time PCPs compared to full-time PCPs. Productivity per clinical hour was markedly higher for part-time PCPs are atleast as efficient as full-time PCPs and that the quality of their work is similar. PMID:11679033

  1. Effectiveness of creative and productive instructional method towards students' learning achievement in steel structure course

    NASA Astrophysics Data System (ADS)

    Sugiyanto, Pribadi, Supriyanto, Bambang

    2017-09-01

    The purpose of this study was to investigate the effectiveness of Creative & Productive instructional method compared with conventional method. This research was a quasi-experimental study involving all Civil Engineering students at Universitas Negeri Malang who were taking a course of Steel Structure. The students were randomly assigned to two different treatment groups, 30 students in experimental group and 37 students in the control group. It was assumed that these groups were equal in all relevant aspects; they differed only in the treatment administered. We used the t-test to test the hypothesis. The results of this research suggest that: (l) the use of Creative & Productive instructional method can significantly improve students' learning achievement, (2) the use of Creative & Productive instructional method can significantly improve students' retention, (3) students' motivation has a significant effect on their learning achievement, and (4) students' motivation has a significant effect on their retention.

  2. Improved wastewater treatment at Wheeling-Pittsburgh Steel Corporations`s Steubenville East Coke Plant

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Goshe, A.J.; Nodianos, M.J.

    1995-12-01

    Wheeling-Pittsburgh Steel Corporation recently improved its wastewater treatment at it`s by-products coke plant. This has led to greatly improved effluent quality. Excess ammonia liquor, along with wastewater from the light oil recovery plant, desulfurization facility, and coal pile runoff, must be treated prior to being discharged into the Ohio River. This is accomplished using a biological wastewater treatment plant to remove 99.99% of the organic contaminants and ammonia. Biologically treated, clarified wastewater is now polished in the newly constructed tertiary treatment plant.

  3. Impacts of iron and steelmaking facilities on soil quality.

    PubMed

    Strezov, Vladimir; Chaudhary, Chandrakant

    2017-12-01

    Iron and steel are highly important materials used in a wide range of products with important contribution to the economic development. The processes for making iron and steel are energy intensive and known to contribute to local pollution. Deposition of the metals may also have adverse impacts on soil quality, which requires detailed assessment. The aim of this study was to investigate the impacts of iron and steelmaking facilities on the local soil quality. Soil samples were collected in the vicinity of two steelmaking sites in Australia, one based on blast furnace steelmaking operation, while the second site was based on electric arc furnace steel recycling. The soil samples were compared to a background site where no industrial impact is expected. The soil collected near industrial facilities contained larger toxic metal contents, however this concentration for all priority metals was within the Australian National Environmental Protection Measure guidelines for the acceptable recreational soil quality. When compared to the international soil quality guidelines, some of the soils collected near the industrial sites, particularly near the blast furnace operated steelmaking, exceeded the arsenic, iron and manganese (according to United States Environmental Protection Agency guidelines) and chromium, copper and nickel concentrations (according to the Canadian guidelines). The work further provided a novel environmental assessment model taking into consideration the environmental and health impacts of each element. The environmental assessment revealed most significant contribution of manganese, followed by titanium, zinc, chromium and lead. Titanium was the second most important contributor to the soil quality, however this metal is currently not included in any of the international soil quality guidelines. Copyright © 2017 Elsevier Ltd. All rights reserved.

  4. Properties of Galvanized and Galvannealed Advanced High Strength Hot Rolled Steels

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    V.Y. Guertsman; E. Essadiqi; S. Dionne

    2008-04-01

    The objectives of the project were (i) to develop the coating process information to achieve good quality coatings on 3 advanced high strength hot rolled steels while retaining target mechanical properties, (ii) to obtain precise knowledge of the behavior of these steels in the various forming operations and (iii) to establish accurate user property data in the coated conditions. Three steel substrates (HSLA, DP, TRIP) with compositions providing yield strengths in the range of 400-620 MPa were selected. Only HSLA steel was found to be suitable for galnaizing and galvannealing in the hot rolled condition.

  5. The influence of farmland pollution on the quality and safety of agricultural products

    NASA Astrophysics Data System (ADS)

    Ma, Z. L.; Li, L. Y.; Ye, C.; Lin, X. Y.; B, C.; Wei

    2018-02-01

    The quality and safety of agricultural products is not only a major livelihood issues for people’s health, but also the main barriers to international trade of agricultural products nowadays. The soil is the foundation to the production of agricultural products and the guarantee of agricultural development. The farmland soil quality is directly related to the quality and safety of agricultural products. Our country’s soil has been polluted by a series of pollution, Such as the excessive discharge of industrial wastes, the encroachment of household waste, and the unreasonable use of pesticides and fertilizers. Soil degradation is a serious threat to the quality and safety of agricultural products, so eliminating soil degradation is the fundamental way out for quality and safety of agricultural products. By analyzing problems of the quality and safety of agricultural products in our country, and exploring the farmland soil influence on the quality and safety of agricultural products. This article provides a reference for improving the control level of quality and safety of agricultural products and the farmland soil quality.

  6. Comparative study on the processing of armour steels with various unconventional technologies

    NASA Astrophysics Data System (ADS)

    Herghelegiu, E.; Schnakovszky, C.; Radu, M. C.; Tampu, N. C.; Zichil, V.

    2017-08-01

    The aim of the current paper is to analyse the suitability of three unconventional technologies - abrasive water jet (AWJ), plasma and laser - to process armour steels. In view of this, two materials (Ramor 400 and Ramor 550) were selected to carry out the experimental tests and the quality of cuts was quantified by considering the following characteristics: width of the processed surface at the jet inlet (Li), width of the processed surface at the jet outlet (Lo), inclination angle (a), deviation from perpendicularity (u), surface roughness (Ra) and surface hardness. It was fond that in terms of cut quality and environmental impact, the best results are offered by abrasive water jet technology. However, it has the lowest productivity comparing to the other two technologies.

  7. 21 CFR 178.3300 - Corrosion inhibitors used for steel or tinplate.

    Code of Federal Regulations, 2014 CFR

    2014-04-01

    ... 21 Food and Drugs 3 2014-04-01 2014-04-01 false Corrosion inhibitors used for steel or tinplate... and Production Aids § 178.3300 Corrosion inhibitors used for steel or tinplate. Corrosion inhibitors may be safely used for steel or tinplate intended for use in, or to be fabricated as, food containers...

  8. Removal of copper ions from aqueous solutions by a steel-making by-product.

    PubMed

    López, F A; Martín, M I; Pérez, C; López-Delgado, A; Alguacil, F J

    2003-09-01

    A study is made of the use of a steel-making by-product (rolling mill scale) as a material for removing Cu(2+) ions from aqueous solutions. The influence of contact time, initial copper ion concentration and temperature on removal capability is considered. The removal of Cu(2+) ions from an aqueous solution involves two processes: on the one hand, the adsorption of Cu(2+) ions on the surface of mill scale due to the iron oxides present in the latter; and on the other hand, the cementation of Cu(2+) onto metallic iron contained in the mill scale. Rolling mill scale is seen to be an effective material for the removal of copper ions from aqueous solutions.

  9. The Effects of Development Team Skill on Software Product Quality

    NASA Technical Reports Server (NTRS)

    Beaver, Justin M.; Schiavone, Guy A.

    2006-01-01

    This paper provides an analysis of the effect of the skill/experience of the software development team on the quality of the final software product. A method for the assessment of software development team skill and experience is proposed, and was derived from a workforce management tool currently in use by the National Aeronautics and Space Administration. Using data from 26 smallscale software development projects, the team skill measures are correlated to 5 software product quality metrics from the ISO/IEC 9126 Software Engineering Product Quality standard. in the analysis of the results, development team skill is found to be a significant factor in the adequacy of the design and implementation. In addition, the results imply that inexperienced software developers are tasked with responsibilities ill-suited to their skill level, and thus have a significant adverse effect on the quality of the software product. Keywords: software quality, development skill, software metrics

  10. Additive manufacturing for steels: a review

    NASA Astrophysics Data System (ADS)

    Zadi-Maad, A.; Rohib, R.; Irawan, A.

    2018-01-01

    Additive manufacturing (AM) of steels involves the layer by layer consolidation of powder or wire feedstock using a heating beam to form near net shape products. For the past decades, the AM technique reaches the maturation of both research grade and commercial production due to significant research work from academic, government and industrial research organization worldwide. AM process has been implemented to replace the conventional process of steel fabrication due to its potentially lower cost and flexibility manufacturing. This paper provides a review of previous research related to the AM methods followed by current challenges issues. The relationship between microstructure, mechanical properties, and process parameters will be discussed. Future trends and recommendation for further works are also provided.

  11. Work Hardening Behavior of 1020 Steel During Cold-Beating Simulation

    NASA Astrophysics Data System (ADS)

    CUI, Fengkui; LING, Yuanfei; XUE, Jinxue; LIU, Jia; LIU, Yuhui; LI, Yan

    2017-03-01

    The present research of cold-beating formation mainly focused on roller design and manufacture, kinematics, constitutive relation, metal flow law, thermo-mechanical coupling, surface micro-topography and microstructure evolution. However, the research on surface quality and performance of workpieces in the process of cold-beating is rare. Cold-beating simulation experiment of 1020 steel is conducted at room temperature and strain rates ranging from 2000 to 4000 s-1 base on the law of plastic forming. According to the experimental data, the model of strain hardening of 1020 steel is established, Scanning Electron Microscopy(SEM) is conducted, the mechanism of the work hardening of 1020 steel is clarified by analyzing microstructure variation of 1020 steel. It is found that the strain rate hardening effect of 1020 steel is stronger than the softening effect induced by increasing temperatures, the process of simulation cold-beating cause the grain shape of 1020 steel significant change and microstructure elongate significantly to form a fibrous tissue parallel to the direction of deformation, the higher strain rate, the more obvious grain refinement and the more hardening effect. Additionally, the change law of the work hardening rate is investigated, the relationship between dislocation density and strain, the relationship between work hardening rate and dislocation density is obtained. Results show that the change trend of the work hardening rate of 1020 steel is divided into two stages, the work hardening rate decreases dramatically in the first stage and slowly decreases in the second stage, finally tending toward zero. Dislocation density increases with increasing strain and strain rate, work hardening rate decreases with increasing dislocation density. The research results provide the basis for solving the problem of improving the surface quality and performance of workpieces under cold-beating formation of 1020 steel.

  12. The effects of a common stainless steel orthodontic bracket on the diagnostic quality of cranial and cervical 3T- MR images: a prospective, case-control study.

    PubMed

    Cassetta, Michele; Pranno, Nicola; Stasolla, Alessandro; Orsogna, Nicola; Fierro, Davide; Cavallini, Costanza; Cantisani, Vito

    2017-08-01

    To evaluate the effect of orthodontic stainless steel brackets and two different types of archwires on the diagnostic quality of 3-T MR images. This prospective, case-control study was conducted following Strengthening the Reporting of Observational Studies in Epidemiology guidelines. The recruitment was conducted among orthodontic patients. 80 subjects, requiring MRI for the presence of temporomandibular disorders, were enrolled and divided into four groups: 20 patients using aligners (control group); 20 patients with stainless steel brackets without archwires; 20 patients with stainless steel brackets and nickel-titanium archwires; and 20 patients with stainless steel brackets and stainless steel archwires. Two experts in neuroradiology evaluated the images to determine the amount of distortion in 6 regions and 48 districts. A score was subjectively assigned according to a modified receiver operating characteristic method of distortion classification. Any disagreement was resolved through consensus seeking; when this was not possible, a third neuroradiologist was consulted. The following statistical methods were used: descriptive statistics, Cohen's kappa coefficient (k), Kruskal-Wallis test, pairwise comparisons using the Dunn-Bonferroni approach. The significance was set at p ≤ 0.05. The presence of stainless steel brackets with or without archwires negatively influenced MRI of the cervical region, paranasal sinuses, head and neck region, and cervical vertebrae but did not influence MRI of brain and temporomandibular joint regions. Patients with a stainless steel multibracket orthodontic appliance should remove it before cervical vertebrae, cervical region, paranasal sinuses, and head and neck MRI scans. The brain and temporomandibular joint region MRI should not require the removal of such appliances.

  13. Laser Surface Modification of H13 Die Steel using Different Laser Spot Sizes

    NASA Astrophysics Data System (ADS)

    Aqida, S. N.; Naher, S.; Brabazon, D.

    2011-05-01

    This paper presents a laser surface modification process of AISI H13 tool steel using three sizes of laser spot with an aim to achieve reduced grain size and surface roughness. A Rofin DC-015 diffusion-cooled CO2 slab laser was used to process AISI H13 tool steel samples. Samples of 10 mm diameter were sectioned to 100 mm length in order to process a predefined circumferential area. The parameters selected for examination were laser peak power, overlap percentage and pulse repetition frequency (PRF). Metallographic study and image analysis were done to measure the grain size and the modified surface roughness was measured using two-dimensional surface profilometer. From metallographic study, the smallest grain sizes measured by laser modified surface were between 0.51 μm and 2.54 μm. The minimum surface roughness, Ra, recorded was 3.0 μm. This surface roughness of the modified die steel is similar to the surface quality of cast products. The grain size correlation with hardness followed the findings correlate with Hall-Petch relationship. The potential found for increase in surface hardness represents an important method to sustain tooling life.

  14. Influence of manufacturing practices on quality of pharmaceutical products manufactured in Kenya.

    PubMed

    Orwa, J A; Keter, L K; Ouko, S P A; Kibwage, I O; Rukunga, G M

    2004-06-01

    To establish the quality of pharmaceutical products manufactured by the respective industries in Kenya and determine the effect of manufacturing practices on the quality of these products. Cross-sectional study. Industries examined are in Nairobi, Kenya. Laboratory analysis was carried out using available facilities at Kenya Medical Research Institute and University of Nairobi, Faculty of Pharmacy. Structured Questionnaires were administered to examine how the code of good manufacturing practices has been used in the production of each pharmaceutical product by respective companies. Questionnaires designed to evaluate the distribution and carry out limited post-market surveillance study were administered to community pharmacy outlets. Drugs were sampled and analyzed for their quality according to the respective monographs. The questionnaires administered to the industry included the source of raw materials, quarantine procedure before and after manufacture, manufacturing procedure, quality audit, quality assurance procedure, equipment, and staff. That administered to the pharmacy outlet included availability, affordability and acceptability of locally manufactured pharmaceutical products. Quality analysis of products involved the establishment of the chemical content, dissolution profile, friability, uniformity of weight and identity. For antibiotic suspensions the stability after reconstitution was also determined. There were 15 respondents and two non-respondents from the industry and six out of nine respondents from the pharmacy outlets. The ratio of qualified staff to product range produced seemed to influence product quality. Industries producing several products with only limited number of pharmaceutical staff had more products failing to comply with pharmacopoeia specifications compared to those producing only few products. Nevertheless, all companies are well equipped with quality control equipment, in accordance with type of product manufactured. Private

  15. Semisolid forming of S48C steel grade

    NASA Astrophysics Data System (ADS)

    Plata, Gorka; Lozares, Jokin; Azpilgain, Zigor; Hurtado, Iñaki; Loizaga, Iñigo; Idoyaga, Zuriñe

    2017-10-01

    Steel production and component manufacturing industries have to face the challenge of globalization, trying to overcome the economic pressure to remain competitive. Moreover, the lightweighting trend of the latter years implies an even higher challenge to maintain the steel use. Therefore, advanced manufacturing processes will be the cornerstone. In this field, Semisolid forming (SSF) has demonstrated the capability of obtaining complex geometries and saving raw material and energy. Despite it is complicated the SSF of sound components, in Mondragon Unibertsitatea it has been successfully demonstrated the capability of producing strong enough automotive components with 42CrMo4 steel grade. In this work, we demonstrate the capability of SSF S48C steel grade with great mechanical properties.

  16. A Bottom-up Energy Efficiency Improvement Roadmap for China’s Iron and Steel Industry up to 2050

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Zhang, Qi; Hasanbeigi, Ali; Price, Lynn

    Iron and steel manufacturing is energy intensive in China and in the world. China is the world largest steel producer accounting for around half of the world steel production. In this study, we use a bottom-up energy consumption model to analyze four steel-production and energy-efficiency scenarios and evaluate the potential for energy savings from energy-efficient technologies in China’s iron and steel industry between 2010 and 2050. The results show that China’s steel production will rise and peak in the year 2020 at 860 million tons (Mt) per year for the base-case scenario and 680 Mt for the advanced energy-efficiency scenario.more » From 2020 on, production will gradually decrease to about 510 Mt and 400 Mt in 2050, for the base-case and advanced scenarios, respectively. Energy intensity will decrease from 21.2 gigajoules per ton (G/t) in 2010 to 12.2 GJ/t and 9.9 GJ/t in 2050 for the base-case and advanced scenarios, respectively. In the near term, decreases in iron and steel industry energy intensity will come from adoption of energy-efficient technologies. In the long term, a shift in the production structure of China’s iron and steel industry, reducing the share of blast furnace/basic oxygen furnace production and increasing the share of electric-arc furnace production while reducing the use of pig iron as a feedstock to electric-arc furnaces will continue to reduce the sector’s energy consumption. We discuss barriers to achieving these energy-efficiency gains and make policy recommendations to support improved energy efficiency and a shift in the nature of iron and steel production in China.« less

  17. Optimum profit model considering production, quality and sale problem

    NASA Astrophysics Data System (ADS)

    Chen, Chung-Ho; Lu, Chih-Lun

    2011-12-01

    Chen and Liu ['Procurement Strategies in the Presence of the Spot Market-an Analytical Framework', Production Planning and Control, 18, 297-309] presented the optimum profit model between the producers and the purchasers for the supply chain system with a pure procurement policy. However, their model with a simple manufacturing cost did not consider the used cost of the customer. In this study, the modified Chen and Liu's model will be addressed for determining the optimum product and process parameters. The authors propose a modified Chen and Liu's model under the two-stage screening procedure. The surrogate variable having a high correlation with the measurable quality characteristic will be directly measured in the first stage. The measurable quality characteristic will be directly measured in the second stage when the product decision cannot be determined in the first stage. The used cost of the customer will be measured by adopting Taguchi's quadratic quality loss function. The optimum purchaser's order quantity, the producer's product price and the process quality level will be jointly determined by maximising the expected profit between them.

  18. Wood Products by Species and Quality in Upland Forests

    Treesearch

    David W. Patterson

    2004-01-01

    Products that can be produced from an upland forest depend on the species and quality of the trees present. Quality depends on growth rate and tree form. These variables are discussed as well as the products that can be produced such as veneer and plywood, grade lumber, handle stock, pallet stock, cross ties, and industrial lumber.

  19. Galvanizability of Advanced High-Strength Steels 1180TRIP and 1180CP

    NASA Astrophysics Data System (ADS)

    Kim, M. S.; Kwak, J. H.; Kim, J. S.; Liu, Y. H.; Gao, N.; Tang, N.-Y.

    2009-08-01

    In general, Si-bearing advanced high-strength steels (AHSS) possess excellent mechanical properties but poor galvanizability. The galvanizability of a transformation-induced plasticity (TRIP) steel 1180TRIP containing 2.2 pct Mn and 1.7 pct Si and a complex phase steel 1180CP containing 2.7 pct Mn and 0.2 pct Si was extensively studied using a galvanizing simulator. The steel coupons were annealed at fixed dew points in the simulator. The surface features of the as-annealed steel coupons, together with galvanized and galvannealed coatings, were carefully examined using a variety of advanced analysis techniques. It was found that various oxides formed on the surface of these steels, depending on the steel composition and on the dew point control. Coating quality was good at 0 °C dew point but deteriorated as the dew point decreased to -35 °C and -65 °C. Based on the findings, guidance was provided for improving galvanizability by adjusting the Mn:Si ratio in steel compositions according to the dew point.

  20. Protein Aggregation and Its Impact on Product Quality

    PubMed Central

    Roberts, Christopher J.

    2014-01-01

    Protein pharmaceutical products are typically active as folded monomers that are composed of one or more protein chains, such as the heavy and light chains in monoclonal antibodies that are a mainstay of current drug pipelines. There are numerous possible aggregated states for a given protein, some of which are potentially useful, while most of which are considered deleterious from the perspective of pharmaceutical product quality and performance. This review provides an overview of how and why different aggregated states of proteins occur, how this potentially impacts product quality and performance, fundamental approaches to control aggregate formation, and the practical approaches that are currently used in the pharmaceutical industry. PMID:25173826

  1. Association between sleep quality and nurse productivity among Korean clinical nurses.

    PubMed

    Park, Eunok; Lee, Hyo Young; Park, Claire Su-Yeon

    2018-06-01

    To determine the association between sleep quality and nurse productivity. Although poor sleep quality may decrease nurses' productivity, the association between the two has not yet been evaluated in the literature. A cross-sectional survey was completed in May 2014 by 188 nurses working in acute hospitals in South Korea using the Pittsburgh Sleep Quality Index. Descriptive statistics, t tests, ANOVA, Pearson's correlation, and stepwise multiple regression were conducted for data analysis. The prevalence of poor sleep quality was high (79.8%). Among the components of sleep quality, sleep disturbances (β = -0.19) and subjective sleep quality (β = -0.16) were determined to be statistically significant predictive factors of nurse productivity, in addition to shift work (β = -0.20) and age (β = 0.32). Poor sleep quality may lead to lower nurse productivity. Nurse leaders and executives should consider measures to improve nurses' sleep quality and enhance nurse productivity. Steps that need to be considered include longer intervals between shift-work cycles, clockwise scheduling order, a longer break time after night shift work, allowing nurses to nap before / during a night shift, and providing a worksite healthy sleep programme. © 2018 John Wiley & Sons Ltd.

  2. Localized corrosion of 316L stainless steel in tritiated water containing aggressive radiolytic and decomposition products at different temperatures

    NASA Astrophysics Data System (ADS)

    Bellanger, G.

    2008-02-01

    Tritium is one of the more important radionuclides used in nuclear industry as plutonium and uranium. The tritium in tritiated water always causes difficulties in nuclear installations, including equipment corrosion. Moreover, with tritiated water there are, in addition, the radiolytic and decomposition products such as hydrogen peroxide formed during decay, chloride ions produced by degradation of organic seals and oils used for tightness and pumping, and acid pH produced by excitation of nitrogen in air by the β - particle. Highly concentrated tritiated water releases energy and its temperature is about 80 °C, moreover heating is necessary in the tritium processes. These conditions highly facilitate the corrosion of stainless steels by pitting and crevice attack. Corrosion tests were performed by electrochemical analysis methods and by visual inspection of the surface of stainless steel.

  3. Quality Assessment of Collection 6 MODIS Atmospheric Science Products

    NASA Astrophysics Data System (ADS)

    Manoharan, V. S.; Ridgway, B.; Platnick, S. E.; Devadiga, S.; Mauoka, E.

    2015-12-01

    Since the launch of the NASA Terra and Aqua satellites in December 1999 and May 2002, respectively, atmosphere and land data acquired by the MODIS (Moderate Resolution Imaging Spectroradiometer) sensor on-board these satellites have been reprocessed five times at the MODAPS (MODIS Adaptive Processing System) located at NASA GSFC. The global land and atmosphere products use science algorithms developed by the NASA MODIS science team investigators. MODAPS completed Collection 6 reprocessing of MODIS Atmosphere science data products in April 2015 and is currently generating the Collection 6 products using the latest version of the science algorithms. This reprocessing has generated one of the longest time series of consistent data records for understanding cloud, aerosol, and other constituents in the earth's atmosphere. It is important to carefully evaluate and assess the quality of this data and remove any artifacts to maintain a useful climate data record. Quality Assessment (QA) is an integral part of the processing chain at MODAPS. This presentation will describe the QA approaches and tools adopted by the MODIS Land/Atmosphere Operational Product Evaluation (LDOPE) team to assess the quality of MODIS operational Atmospheric products produced at MODAPS. Some of the tools include global high resolution images, time series analysis and statistical QA metrics. The new high resolution global browse images with pan and zoom have provided the ability to perform QA of products in real time through synoptic QA on the web. This global browse generation has been useful in identifying production error, data loss, and data quality issues from calibration error, geolocation error and algorithm performance. A time series analysis for various science datasets in the Level-3 monthly product was recently developed for assessing any long term drifts in the data arising from instrument errors or other artifacts. This presentation will describe and discuss some test cases from the

  4. 7th Annual NASA/Contractors Conference on Quality and Productivity: "Total Quality Leadership"

    NASA Technical Reports Server (NTRS)

    1991-01-01

    More than 750 NASA, government, contractor, and academic representatives attended the Seventh Annual NASA/Contractors Conference on Quality and Productivity on October 12-13, 1990, in Grenelefe, Florida. The panel presentations and keynote speeches revolving around the theme of 'Total Quality Leadership' provided a solid base of understanding of the importance, benefits, and principles of total quality management. The implementation of these strategies is critical if we are to effectively pursue our mission of continuous quality improvement and reliability in our products, processess, and services. The annual NASA/contractors conferences serve as catalysts for achieving success in this mission. The conference was highlighted by the announcement of the first recipients of the George M. Low Trophy: NASA's Quality and Excellence Award. My congratulations go out to all nine finalist organizations and to the two recipients of this prestigious honor: Rockwell Space Systems Division and Marotta Scientific Controls, Inc. (the first small business to achieve this honor). These organizations have demonstrated a commitment to quality that is unsurpassed in the aerospace industry. This report summarizes the presentations and is not intended to be a verbatim proceedings document. You are encouraged to contact the speakers with any requests for further information.

  5. Lightweight Steel Solutions for Automotive Industry

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Lee, Hong Woo; Kim, Gyosung; Park, Sung Ho

    2010-06-15

    Recently, improvement in fuel efficiency and safety has become the biggest issue in worldwide automotive industry. Although the regulation of environment and safety has been tightened up more and more, the majority of vehicle bodies are still manufactured from stamped steel components. This means that the optimized steel solutions enable to demonstrate its ability to reduce body weight with high crashworthiness performance instead of expensive light weight materials such as Al, Mg and composites. To provide the innovative steel solutions for automotive industry, POSCO has developed AHSS and its application technologies, which is directly connected to EVI activities. EVI ismore » a technical cooperation program with customer covering all stages of new car project from design to mass production. Integrated light weight solutions through new forming technologies such as TWB, hydroforming and HPF are continuously developed and provided for EVI activities. This paper will discuss the detailed status of these technologies especially light weight steel solutions based on innovative technologies.« less

  6. Lightweight Steel Solutions for Automotive Industry

    NASA Astrophysics Data System (ADS)

    Lee, Hong Woo; Kim, Gyosung; Park, Sung Ho

    2010-06-01

    Recently, improvement in fuel efficiency and safety has become the biggest issue in worldwide automotive industry. Although the regulation of environment and safety has been tightened up more and more, the majority of vehicle bodies are still manufactured from stamped steel components. This means that the optimized steel solutions enable to demonstrate its ability to reduce body weight with high crashworthiness performance instead of expensive light weight materials such as Al, Mg and composites. To provide the innovative steel solutions for automotive industry, POSCO has developed AHSS and its application technologies, which is directly connected to EVI activities. EVI is a technical cooperation program with customer covering all stages of new car project from design to mass production. Integrated light weight solutions through new forming technologies such as TWB, hydroforming and HPF are continuously developed and provided for EVI activities. This paper will discuss the detailed status of these technologies especially light weight steel solutions based on innovative technologies.

  7. Hot Corrosion Behavior of Stainless Steel with Al-Si/Al-Si-Cr Coating

    NASA Astrophysics Data System (ADS)

    Fu, Guangyan; Wu, Yongzhao; Liu, Qun; Li, Rongguang; Su, Yong

    2017-03-01

    The 1Cr18Ni9Ti stainless steel with Al-Si/Al-Si-Cr coatings is prepared by slurry process and vacuum diffusion, and the hot corrosion behavior of the stainless steel with/without the coatings is studied under the condition of Na2SO4 film at 950 °C in air. Results show that the corrosion kinetics of stainless steel, the stainless steel with Al-Si coating and the stainless steel with Al-Si-Cr coating follow parabolic laws in several segments. After 24 h corrosion, the sequence of the mass gain for the three alloys is the stainless steel with Al-Si-Cr coating < the stainless steel with Al-Si coating < the stainless steel without any coating. The corrosion products of the three alloys are layered. Thereinto, the corrosion products of stainless steel without coating are divided into two layers, where the outside layer contains a composite of Fe2O3 and FeO, and the inner layer is Cr2O3. The corrosion products of the stainless steel with Al-Si coating are also divided into two layers, of which the outside layer mainly consists of Cr2O3, and the inner layer is mainly SiO2. The corrosion film of the stainless steel with Al-Si-Cr coating is thin and dense, which combines well with substrate. Thereinto, the outside layer is mainly Cr2O3, and the inside layer is Al2O3. In the matrix of all of the three alloys, there exist small amount of sulfides. Continuous and protective films of Cr2O3, SiO2 and Al2O3 form on the surface of the stainless steel with Al-Si and Al-Si-Cr coatings, which prevent further oxidation or sulfide corrosion of matrix metals, and this is the main reason for the much smaller mass gain of the two alloys than that of the stainless steel without any coatings in the 24 h hot corrosion process.

  8. Process stability during fiber laser-arc hybrid welding of thick steel plates

    NASA Astrophysics Data System (ADS)

    Bunaziv, Ivan; Frostevarg, Jan; Akselsen, Odd M.; Kaplan, Alexander F. H.

    2018-03-01

    Thick steel plates are frequently used in shipbuilding, pipelines and other related heavy industries, and are usually joined by arc welding. Deep penetration laser-arc hybrid welding could increase productivity but has not been thoroughly investigated, and is therefore usually limited to applications with medium thickness (5-15 mm) sections. A major concern is process stability, especially when using modern welding consumables such as metal-cored wire and advanced welding equipment. High speed imaging allows direct observation of the process so that process behavior and phenomena can be studied. In this paper, 45 mm thick high strength steel was welded (butt joint double-sided) using the fiber laser-MAG hybrid process utilizing a metal-cored wire without pre-heating. Process stability was monitored under a wide range of welding parameters. It was found that the technique can be used successfully to weld thick sections with appropriate quality when the parameters are optimized. When comparing conventional pulsed and the more advanced cold metal transfer pulse (CMT+P) arc modes, it was found that both can provide high quality welds. CMT+P arc mode can provide more stable droplet transfer over a limited range of travel speeds. At higher travel speeds, an unstable metal transfer mechanism was observed. Comparing leading arc and trailing arc arrangements, the leading arc configuration can provide higher quality welds and more stable processing at longer inter-distances between the heat sources.

  9. Productivity improvement and quality enhancement at NASA

    NASA Technical Reports Server (NTRS)

    Braunstein, D. R.

    1985-01-01

    NASA's Productivity Improvement and Quality Enhancement (PIQE) effort has as its objectives the encouragement of greater employee participation in management decision-making and the identification of impediments as well as opportunities for high productivity. Attempts are also made to try out novel management practices, and to evolve productivity trend analysis techniques. Every effort is made to note, reward, and diffuse successfully instituted PIQE approaches throughout the NASA-contractor organization.

  10. Realization of high quality production schedules: Structuring quality factors via iteration of user specification processes

    NASA Technical Reports Server (NTRS)

    Hamazaki, Takashi

    1992-01-01

    This paper describes an architecture for realizing high quality production schedules. Although quality is one of the most important aspects of production scheduling, it is difficult, even for a user, to specify precisely. However, it is also true that the decision as to whether a scheduler is good or bad can only be made by the user. This paper proposes the following: (1) the quality of a schedule can be represented in the form of quality factors, i.e. constraints and objectives of the domain, and their structure; (2) quality factors and their structure can be used for decision making at local decision points during the scheduling process; and (3) that they can be defined via iteration of user specification processes.

  11. The analysis of critical cooling rate for high-rise building steel S460

    NASA Astrophysics Data System (ADS)

    Lu, Shiping; Chen, Xia; Li, Qun; Wang, Haibao; Gu, Linhao

    2017-09-01

    High-rise building steel S460 is an important structure steel.The product process of the steel is Quenching&Tempering. The critical cooling rate of steel is very important in heavy plate quenching process, and it is also the basis of the cooling process[1].The critical cooling rate of HSLA steel S460 is obtained from the Thermal simulation method,and the differences about the microstructure and properties of different cooling rate is also analyzed.In this article, the angle of the grain boundary and the average grain size are analyzed by EBSD under different cooling rate. The relationship between grain boundary angle and grain size with the cooling rate is obtained. According to the experiment,it provides the basis for the formulation of the quenching process of the industrial production.

  12. Metafrontier frameworks for studying hospital productivity growth and quality changes.

    PubMed

    Chen, Kuan-Chen; Chien, Li-Nien; Hsu, Yi-Hsin; Yu, Ming-Miin

    2016-12-01

    The objective of this study was to evaluate productivity growth and quality changes among different levels of accredited hospitals. This study used an attribute-incorporating Malmquist productivity index (MPI) under the metafrontier framework. This is the first attempt to compare productivity changes among hospitals operating under different production frontiers. The data consisted of 20 academic medical centers (AMCs), 61 metropolitan hospitals (MPs) and 112 local community hospitals (LCs) in Taiwan during the period 2007-2010. This study measured productivity growth and further identified technological gaps and catch-ups in different groups of hospitals with respect to the metafrontier. At the same time, comparisons of changes in quality among different levels of hospitals were also examined. We found that the sample hospitals of AMCs and MPs experienced productivity improvements mainly due to technological progress, but their efficiency and technology gap ratio (TGR) deteriorated. As for LCs, progress in technology along with improvements in their efficiency and TGR led to the highest productivity upgrade among the three groups of hospitals. We also found that the sample hospitals among the three groups showed improvements in quality. Moreover, hospitals in the local community group exhibited greater quality progress than the AMCs and MPs over the sample period. This paper presents a number of useful decompositions of the metafrontier MPI, which can provide useful insights into changes that are due to efficiency, quality improvements and/or technological changes in the healthcare sector. © The Author 2016. Published by Oxford University Press in association with the International Society for Quality in Health Care. All rights reserved. For permissions, please e-mail: journals.permissions@oup.com

  13. 77 FR 30589 - SteelRiver Infrastructure Partners LP, SteelRiver Infrastructure Associates LLC, SteelRiver...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-05-23

    ... DEPARTMENT OF TRANSPORTATION Surface Transportation Board [Docket No. FD 35622] SteelRiver Infrastructure Partners LP, SteelRiver Infrastructure Associates LLC, SteelRiver Infrastructure Fund North America LP, and Patriot Funding LLC--Control Exemption--Patriot Rail Corp., et al. SteelRiver...

  14. 49 CFR 178.50 - Specification 4B welded or brazed steel cylinders.

    Code of Federal Regulations, 2014 CFR

    2014-10-01

    ... service pressure of at least 150 but not over 500 psig. Cylinders closed in by spinning process are not authorized. (b) Steel. Open-hearth, electric or basic oxygen process steel of uniform quality must be used... using equipment and processes adequate to ensure that each cylinder produced conforms to the...

  15. 49 CFR 178.50 - Specification 4B welded or brazed steel cylinders.

    Code of Federal Regulations, 2012 CFR

    2012-10-01

    ... service pressure of at least 150 but not over 500 psig. Cylinders closed in by spinning process are not authorized. (b) Steel. Open-hearth, electric or basic oxygen process steel of uniform quality must be used... using equipment and processes adequate to ensure that each cylinder produced conforms to the...

  16. 49 CFR 178.50 - Specification 4B welded or brazed steel cylinders.

    Code of Federal Regulations, 2013 CFR

    2013-10-01

    ... service pressure of at least 150 but not over 500 psig. Cylinders closed in by spinning process are not authorized. (b) Steel. Open-hearth, electric or basic oxygen process steel of uniform quality must be used... using equipment and processes adequate to ensure that each cylinder produced conforms to the...

  17. The Fifth Annual NASA/Contractors Conference on Quality and Productivity. Quality: A Commitment to the Future

    NASA Technical Reports Server (NTRS)

    1989-01-01

    The report is a summary of the 5th NASA/Contractors Conference on Quality and Productivity. The theme was 'Quality - A Commitment to the Future'. The summary report highlights the key points: commitment to quality, strategic and long-range planning, quality commitment, risk management, teaming, quality measurement, creating a quality environment, contract incentives, software quality and reliability.

  18. 77 FR 64483 - Circular Welded Carbon-Quality Steel Pipe from the Socialist Republic of Vietnam: Notice of Final...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-10-22

    ... Pipe from the Socialist Republic of Vietnam;'' ``Verification of the Sales Response of Midwest Air... Steel Joint Stock Company.... Sun Steel Joint Stock 4.57 Company. Huu Lien Asia Corporation........ Huu Lien Asia 4.57 Corporation. Hoa Phat Steel Pipe Co Hoa Phat Steel Pipe Co.. 4.57 Vietnam-Wide Rate \\13...

  19. Introduction to NASA Symposium on Productivity and Quality

    NASA Technical Reports Server (NTRS)

    Braunstein, David

    1984-01-01

    The discussions will concentrate on white-collar organizational issues common to large organizations. The program will address a number of management issues for improving our nation's productivity and quality, and therefore its competitive position. executives have contributed their time to share /their experience with you. In addition, the American Institute of Astronautics & Aeronautics corporate members have helped to organize the sessions. I am most grateful for this support. The NASA Administrator has set the goal for NASA to become a leader in productivity and quality.

  20. In Situ Observations of Agglomeration of Non-metallic Inclusions at Steel/Ar and Steel/Slag Interfaces by High-Temperature Confocal Laser Scanning Microscope: A Review

    NASA Astrophysics Data System (ADS)

    Mu, Wangzhong; Dogan, Neslihan; Coley, Kenneth S.

    2018-05-01

    The agglomeration behavior of non-metallic inclusions in the steelmaking process is important for controlling the cleanliness of the steel. In this work, the observation of agglomeration behaviors of inclusions at steel/Ar and steel/slag interfaces using a high-temperature confocal laser scanning microscope (HT-CLSM) is summarized. This HT-CLSM technique has been applied to observe phase transformation during solidification and heat treatment and the engulfment and pushing behavior of inclusions in front of the solidified interface. In the current work, the inclusion agglomeration behavior at steel/Ar and steel/slag interfaces is summarized and discussed. Subsequently, the development of the theoretical work investigating inclusion agglomeration at steel/Ar and steel/slag interfaces including the initial capillary force model and Kralchevsky-Paunov model is described. Finally, the Kralchevsky-Paunov model is applied to investigating nitride inclusion agglomeration at high-manganese steel/Ar interfaces. This work aims to give a critical review of the application of HT-CLSM in secondary refining as well as a better control of inclusion elimination for clean steel production.

  1. 7 CFR 58.149 - Alternate quality control programs for dairy products.

    Code of Federal Regulations, 2011 CFR

    2011-01-01

    ... 7 Agriculture 3 2011-01-01 2011-01-01 false Alternate quality control programs for dairy products... and Grading Service 1 Operations and Operating Procedures § 58.149 Alternate quality control programs for dairy products. (a) When a plant has in operation an acceptable quality control program which is...

  2. High-performance thin layer chromatography to assess pharmaceutical product quality.

    PubMed

    Kaale, Eliangiringa; Manyanga, Vicky; Makori, Narsis; Jenkins, David; Michael Hope, Samuel; Layloff, Thomas

    2014-06-01

    To assess the sustainability, robustness and economic advantages of high-performance thin layer chromatography (HPTLC) for quality control of pharmaceutical products. We compared three laboratories where three lots of cotrimoxazole tablets were assessed using different techniques for quantifying the active ingredient. The average assay relative standard deviation for the three lots was 1.2 with a range of 0.65-2.0. High-performance thin layer chromatography assessments are yielding valid results suitable for assessing product quality. The local pharmaceutical manufacturer had evolved the capacity to produce very high quality products. © 2014 John Wiley & Sons Ltd.

  3. Product Quality Assurance for Off-Grid Lighting in Africa

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    World Bank; Mills, Evan; Mills, Evan

    Although the emergence of markets for high efficiency off-grid lighting technologies holds promise, realizing the potential of this opportunity on a long-term, sustainable basis requires careful attention to issues of product quality, consumer protection, and the potential for significant 'market spoiling', in anticipation of increases of sales of low cost, low performance off-grid lighting products. The goal of the Lighting Africa quality assurance workshop was to articulate strategies to mitigate the dangers of market spoiling and to explore ways to protect consumers from misleading advertising for sales of inferior, off-grid lighting products in the context of Lighting Africa's overarching objectivemore » to support the industry in developing a robust off-grid lighting market in Africa. The workshop resulted in the identification of two strategic approaches for meeting Lighting Africa quality assurance programmatic needs. The first strategy is intended to meet a short-term programmatic need for quality associated with requests for lighting products by bulk procurement agents, such as in a World Bank-financed project. The development of procurement specifications and test procedures that could be used in a quality/usability screening method in order to provide guidance for forthcoming large volume purchases emerged as the best solution to meet this need. Such approaches are used in World Bank-financed solar home systems (SHSs) projects in Bangladesh, Sri Lanka, and China, among others. However, unlike the SHSs which have multiple balance-of-system (BOS) components warranting the need for an array of specifications for individual components, stand alone lighting systems require specifications that are amenable to individual light points. To test this approach, Lighting Africa elected to use the technical specifications issued by the Photovoltaic Global Approval Program for solar lanterns that use CFL bulbs (PVRS11A) as the basis of qualifying such products. A

  4. 24 CFR 200.949 - Building product standards and certification program for exterior insulated steel door systems.

    Code of Federal Regulations, 2012 CFR

    2012-04-01

    ... certification program for exterior insulated steel door systems. 200.949 Section 200.949 Housing and Urban... program for exterior insulated steel door systems. (a) Applicable standards. (1) All Exterior Insulated Steel Door Systems shall be designed, manufactured, and tested in compliance with the following...

  5. 24 CFR 200.949 - Building product standards and certification program for exterior insulated steel door systems.

    Code of Federal Regulations, 2013 CFR

    2013-04-01

    ... certification program for exterior insulated steel door systems. 200.949 Section 200.949 Housing and Urban... program for exterior insulated steel door systems. (a) Applicable standards. (1) All Exterior Insulated Steel Door Systems shall be designed, manufactured, and tested in compliance with the following...

  6. Moving toward the circular economy: the role of stocks in the Chinese steel cycle.

    PubMed

    Pauliuk, Stefan; Wang, Tao; Müller, Daniel B

    2012-01-03

    As the world's largest CO(2) emitter and steel producer, China has set the ambitious goal of establishing a circular economy which aims at reconciling economic development with environmental protection and sustainable resource use. This work applies dynamic material flow analysis to forecast production, recycling, and iron ore consumption in the Chinese steel cycle until 2100 by using steel services in terms of in-use stock per capita as driver of future development. The whole cycle is modeled to determine possible responses of the steel industry in light of the circular economy concept. If per-capita stock saturates at 8-12 tons as evidence from industrialized countries suggests, consumption may peak between 2015 and 2020, whereupon it is likely to drop by up to 40% until 2050. A slower growing in-use stock could mitigate this peak and hence reduce overcapacity in primary production. Old scrap supply will increase substantially and it could replace up to 80% of iron ore as resource for steel making by 2050. This would require advanced recycling technologies as manufacturers of machinery and transportation equipment would have to shift to secondary steel as well as new capacities in secondary production which could, however, make redundant already existing integrated steel plants.

  7. Ultrahigh Ductility, High-Carbon Martensitic Steel

    NASA Astrophysics Data System (ADS)

    Qin, Shengwei; Liu, Yu; Hao, Qingguo; Zuo, Xunwei; Rong, Yonghua; Chen, Nailu

    2016-10-01

    Based on the proposed design idea of the anti-transformation-induced plasticity effect, both the additions of the Nb element and pretreatment of the normalization process as a novel quenching-partitioning-tempering (Q-P-T) were designed for Fe-0.63C-1.52Mn-1.49Si-0.62Cr-0.036Nb hot-rolled steel. This high-carbon Q-P-T martensitic steel exhibits a tensile strength of 1890 MPa and elongation of 29 pct accompanied by the excellent product of tensile and elongation of 55 GPa pct. The origin of ultrahigh ductility for high-carbon Q-P-T martensitic steel is revealed from two aspects: one is the softening of martensitic matrix due to both the depletion of carbon in the matensitic matrix during the Q-P-T process by partitioning of carbon from supersaturated martensite to retained austenite and the reduction of the dislocation density in a martensitic matrix by dislocation absorption by retained austenite effect during deformation, which significantly enhances the deformation ability of martensitic matrix; another is the high mechanical stability of considerable carbon-enriched retained austenite, which effectively reduces the formation of brittle twin-type martensite. This work verifies the correctness of the design idea of the anti-TRIP effect and makes the third-generation advanced high-strength steels extend to the field of high-carbon steels from low- and medium-carbon steels.

  8. Nano-yttria dispersed stainless steel composites composed by the 3 dimensional fiber deposition technique

    NASA Astrophysics Data System (ADS)

    Verhiest, K.; Mullens, S.; De Wispelaere, N.; Claessens, S.; DeBremaecker, A.; Verbeken, K.

    2012-09-01

    In this study, oxide dispersion strengthened (ODS) 316L steel samples were manufactured by the 3 dimensional fiber deposition (3DFD) technique. The performance of 3DFD as colloidal consolidation technique to obtain porous green bodies based on yttria (Y2O3) nano-slurries or paste, is discussed within this experimental work. The influence of the sintering temperature and time on sample densification and grain growth was investigated in this study. Hot consolidation was performed to obtain final product quality in terms of residual porosity reduction and final dispersion homogeneity.

  9. Microbial-Influenced Corrosion of Corten Steel Compared with Carbon Steel and Stainless Steel in Oily Wastewater by Pseudomonas aeruginosa

    NASA Astrophysics Data System (ADS)

    Mansouri, Hamidreza; Alavi, Seyed Abolhasan; Fotovat, Meysam

    2015-07-01

    The microbial corrosion behavior of three important steels (carbon steel, stainless steel, and Corten steel) was investigated in semi petroleum medium. This work was done in modified nutrient broth (2 g nutrient broth in 1 L oily wastewater) in the presence of Pseudomonas aeruginosa and mixed culture (as a biotic media) and an abiotic medium for 2 weeks. The behavior of corrosion was analyzed by spectrophotometric and electrochemical methods and at the end was confirmed by scanning electron microscopy. The results show that the degree of corrosion of Corten steel in mixed culture, unlike carbon steel and stainless steel, is less than P. aeruginosa inoculated medium because some bacteria affect Corten steel less than other steels. According to the experiments, carbon steel had less resistance than Corten steel and stainless steel. Furthermore, biofilm inhibits separated particles of those steels to spread to the medium; in other words, particles get trapped between biofilm and steel.

  10. State Policies and Planning to Increase Attainment, Quality, and Productivity

    ERIC Educational Resources Information Center

    Lingenfelter, Paul E.

    2007-01-01

    This article examines why state planning and policy for higher education are increasingly focused on increasing educational attainment, quality, and the productivity of the system. It presents four "stories" which illustrate initiatives to improve attainment, quality, and productivity, but fall far short of exhausting the available material.

  11. 24 CFR 200.949 - Building product standards and certification program for exterior insulated steel door systems.

    Code of Federal Regulations, 2011 CFR

    2011-04-01

    ... Doors and Frames; (viii) ISDSI-107-80—Thermal Performance Standard for Insulated Steel Door Systems; (ix... certification program for exterior insulated steel door systems. 200.949 Section 200.949 Housing and Urban... program for exterior insulated steel door systems. (a) Applicable standards. (1) All Exterior Insulated...

  12. Monitoring Quality of Biotherapeutic Products Using Multivariate Data Analysis.

    PubMed

    Rathore, Anurag S; Pathak, Mili; Jain, Renu; Jadaun, Gaurav Pratap Singh

    2016-07-01

    Monitoring the quality of pharmaceutical products is a global challenge, heightened by the implications of letting subquality drugs come to the market on public safety. Regulatory agencies do their due diligence at the time of approval as per their prescribed regulations. However, product quality needs to be monitored post-approval as well to ensure patient safety throughout the product life cycle. This is particularly complicated for biotechnology-based therapeutics where seemingly minor changes in process and/or raw material attributes have been shown to have a significant effect on clinical safety and efficacy of the product. This article provides a perspective on the topic of monitoring the quality of biotech therapeutics. In the backdrop of challenges faced by the regulatory agencies, the potential use of multivariate data analysis as a tool for effective monitoring has been proposed. Case studies using data from several insulin biosimilars have been used to illustrate the key concepts.

  13. Energy conditions of high quality laser-oxygen cutting of mild steel

    NASA Astrophysics Data System (ADS)

    Shulyatyev, V. B.; Orishich, A. M.; Malikov, A. G.

    2011-02-01

    In our previous work we found experimentally the scaling laws for the oxygen-assisted laser cutting of low-carbon steel of 5 - 25 mm. No dross and minimal roughness of the cut surface were chosen as criteria of quality. Formulas were obtained to determine the optimum values of the laser power and cutting speed for the given sheet thickness. In the present paper, the energy balance of the oxygen-assisted laser cutting is studied experimentally at these optimum parameters. The absorbed laser energy and heat conduction losses and cut width were measured experimentally, and then the energy of exothermic reaction of oxidation was found from the balance equation. To define the integral coefficient of absorption, the laser power was measured on the cutting channel exit during the cutting. The heat conduction losses were measured by the calorimetric method. It has been established that the absorbed laser energy, oxidation energy, thermal losses and melting enthalpy related to a sheet thickness unit, do not depend on the sheet thickness at the cutting with the minimal roughness. The results enable to determine the fraction of the oxidized iron in the melt and thermal efficiency at the cutting with the minimal roughness. The share of the oxidation reaction energy is 50 - 60% in the total contributed energy.

  14. Acute changes in lung function associated with proximity to a steel plant: a randomized study.

    PubMed

    Dales, Robert; Kauri, Lisa Marie; Cakmak, Sabit; Mahmud, Mamun; Weichenthal, Scott A; Van Ryswyk, Keith; Kumarathasan, Premkumari; Thomson, Errol; Vincent, Renaud; Broad, Gayle; Liu, Ling

    2013-05-01

    Steel production is a major industry worldwide yet there is relatively little information on the pulmonary effects of air quality near steel manufacturing plants. The aim of this study was to examine how lung function changes acutely when healthy subjects are situated near a steel plant which is adjacent to a residential area. Sixty-one subjects were randomly assigned to spend 5 consecutive, 8-hour days in a residential neighborhood approximately 0.9km from a steel plant, or approximately 4.5km away at a college campus. Subjects crossed-over between sites after a nine-day washout period. Lung function was measured daily at both sites along with air pollutants including SO2, NO2, O3, PM2.5, and ultrafine particles. Diffusion capacity and pulse oximetry were also examined. Compared with the college site, the forced expiratory volume in 1-second/forced vital capacity, forced expiratory flow between 25% and 75% of the FVC, total lung capacity, functional residual capacity, and residual volume were lower near the steel plant by 0.67% (95% CI: 0.28, 1.06),1.62% (95% CI: 0.50, 2.75), 1.54% (95% CI: 0.68, 2.39), 3.54% (95% CI: 1.95, 5.13) and 11.3% (95% CI: 4.92, 17.75), respectively. Diffusion capacity, forced expiratory volume in 1s, and pulse oximetry were also lower near the plant but these effects were not statistically significant. Sulfur dioxide, ultrafine particulates, and oxides of nitrogen were greater near the steel plant site compared to the college site. Spending short periods of time near a steel plant is associated with a decrease in lung function. Crown Copyright © 2013. Published by Elsevier Ltd. All rights reserved.

  15. Quality challenges associated with microbial-based cleaning products from the Industry Perspective.

    PubMed

    Teasdale, Steve M; Kademi, Ali

    2018-06-01

    Microbial-based cleaning products (MBCPs) continue to gain popularity in the market as environmentally friendly cleaners. The majority of these products contain spores of various Bacillus species. Although the microorganisms used in MBCPs are subject to regulation in Canada under the Canadian Environmental Protection Act, the products themselves are not. Unlike other types of microbial products such as probiotics and biopesticides, the use, manufacture and quality parameters of MBCPs in Canada and other countries are poorly defined and not specifically subject to any required standards. Due to their complexity and nature, these products feature unique quality challenges. We noted the existing MBCPs we analyzed vary vastly in quality; external microbial contaminants, viability of the spores and the biocompatibility of the ingredients are issues that greatly affect product quality. A proper taxonomic identification of the bacterial species used also seems to be a major challenge for a number of manufacturers. A good understanding of the mechanisms governing these quality challenges and the adoption of good practices for the cultivation, harvesting, formulation, and manufacture of these types of products are essential for achieving high-quality performance standards. Copyright © 2017 Elsevier Ltd. All rights reserved.

  16. Summary Report of the Seventh Annual NASA/Contractors Conference on Quality and Productivity: "Total Quality Leadership"

    NASA Technical Reports Server (NTRS)

    1991-01-01

    More than 750 NASA, government, contractor, and academic representatives attended the Seventh Annual NASA/Contractors Conference on Quality and Productivity on October 12-13, 1990, in Grenelefe, Florida. The panel presentations and keynote speeches revolving around the theme of 'Total Quality Leadership" provided a solid base of understanding of the importance, benefits, and principles of total quality management. The implementation of these strategies is critical if we are to effectively pursue our mission of continuous quality improvement and reliability in our products, processes, and services. The annual NASA/contractors conferences serve as catalysts for achieving success in this mission.

  17. Aircraft Steels

    DTIC Science & Technology

    2009-02-19

    component usage. PH 13-8Mo is a precipitation-hardenable martensitic stainless steel combining excellent corrosion resistance with strength. Custom 465 is...a martensitic , age-hardenable stainless steel capable of about 1,724 MPa (250 ksi) UTS when peak-aged (H900 condition). Especially, this steel can...NOTES 14. ABSTRACT Five high strength steels (4340, 300M, AerMet 100, Ferrium S53, and Hy-Tuf) and four stainless steels (High Nitrogen, 13

  18. Steel slag carbonation in a flow-through reactor system: the role of fluid-flux.

    PubMed

    Berryman, Eleanor J; Williams-Jones, Anthony E; Migdisov, Artashes A

    2015-01-01

    Steel production is currently the largest industrial source of atmospheric CO2. As annual steel production continues to grow, the need for effective methods of reducing its carbon footprint increases correspondingly. The carbonation of the calcium-bearing phases in steel slag generated during basic oxygen furnace (BOF) steel production, in particular its major constituent, larnite {Ca2SiO4}, which is a structural analogue of olivine {(MgFe)2SiO4}, the main mineral subjected to natural carbonation in peridotites, offers the potential to offset some of these emissions. However, the controls on the nature and efficiency of steel slag carbonation are yet to be completely understood. Experiments were conducted exposing steel slag grains to a CO2-H2O mixture in both batch and flow-through reactors to investigate the impact of temperature, fluid flux, and reaction gradient on the dissolution and carbonation of steel slag. The results of these experiments show that dissolution and carbonation of BOF steel slag are more efficient in a flow-through reactor than in the batch reactors used in most previous studies. Moreover, they show that fluid flux needs to be optimized in addition to grain size, pressure, and temperature, in order to maximize the efficiency of carbonation. Based on these results, a two-stage reactor consisting of a high and a low fluid-flux chamber is proposed for CO2 sequestration by steel slag carbonation, allowing dissolution of the slag and precipitation of calcium carbonate to occur within a single flow-through system. Copyright © 2014. Published by Elsevier B.V.

  19. Progress in thermomechanical control of steel plates and their commercialization

    NASA Astrophysics Data System (ADS)

    Nishioka, Kiyoshi; Ichikawa, Kazutoshi

    2012-04-01

    The water-cooled thermomechanical control process (TMCP) is a technology for improving the strength and toughness of water-cooled steel plates, while allowing control of the microstructure, phase transformation and rolling. This review describes metallurgical aspects of the microalloying of steel, such as niobium addition, and discusses advantages of TMCP, for example, in terms of weldability, which is reduced upon alloying. Other covered topics include the development of equipment, distortions in steel plates, peripheral technologies such as steel making and casting, and theoretical modeling, as well as the history of property control in steel plate production and some early TMCP technologies. We provide some of the latest examples of applications of TMCP steel in various industries such as shipbuilding, offshore structures, building construction, bridges, pipelines, penstocks and cryogenic tanks. This review also introduces high heat-affected-zone toughness technologies, wherein the microstructure of steel is improved by the addition of fine particles of magnesium-containing sulfides and magnesium- or calcium-containing oxides. We demonstrate that thanks to ongoing developments TMCP has the potential to meet the ever-increasing demands of steel plates.

  20. Mapping the global flow of steel: from steelmaking to end-use goods.

    PubMed

    Cullen, Jonathan M; Allwood, Julian M; Bambach, Margarita D

    2012-12-18

    Our society is addicted to steel. Global demand for steel has risen to 1.4 billion tonnes a year and is set to at least double by 2050, while the steel industry generates nearly a 10th of the world's energy related CO₂ emissions. Meeting our 2050 climate change targets would require a 75% reduction in CO₂ emissions for every tonne of steel produced and finding credible solutions is proving a challenge. The starting point for understanding the environmental impacts of steel production is to accurately map the global steel supply chain and identify the biggest steel flows where actions can be directed to deliver the largest impact. In this paper we present a map of global steel, which for the first time traces steel flows from steelmaking, through casting, forming, and rolling, to the fabrication of final goods. The diagram reveals the relative scale of steel flows and shows where efforts to improve energy and material efficiency should be focused.

  1. Microstructural Developments Leading to New Advanced High Strength Sheet Steels: A Historical Assessment of Critical Metallographic Observations

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Matlock, David K; Thomas, Larrin S; Taylor, Mark D

    In the past 30+ years significant advancements have been made in the development of higher strength sheet steels with improved combinations of strength and ductility that have enabled important product improvements leading to safer, lighter weight, and more fuel efficient automobiles and in other applications. Properties of the primarily low carbon, low alloy steels are derived through careful control of time-temperature processing histories designed to produce multiphase ferritic based microstructures that include martensite and other constituents including retained austenite. The basis for these developments stems from the early work on dual-phase steels which was the subject of much interest. Inmore » response to industry needs, dual-phase steels have evolved as a unique class of advanced high strength sheet steels (AHSS) in which the thermal and mechanical processing histories have been specifically designed to produce constituent combinations for the purpose of simultaneously controlling strength and deformation behavior, i.e. stress-strain curve shapes. Improvements continue as enhanced dual-phase steels have recently been produced with finer microstructures, higher strengths, and better overall formability. Today, dual phase steels are the primary AHSS products used in vehicle manufacture, and several companies have indicated that the steels will remain as important design materials well into the future. In this presentation, fundamental results from the early work on dual-phase steels will be reviewed and assessed in light of recent steel developments. Specific contributions from industry/university cooperative research leading to product improvements will be highlighted. The historical perspective provided in the evolution of dual-phase steels represents a case-study that provides important framework and lessons to be incorporated in next generation AHSS products.« less

  2. Evaluation of corrosion products formed by sulfidation as inhibitors of the naphthenic corrosion of AISI-316 steel

    NASA Astrophysics Data System (ADS)

    Sanabria-Cala, J. A.; Montañez, N. D.; Laverde Cataño, D.; Y Peña Ballesteros, D.; Mejía, C. A.

    2017-12-01

    Naphthenic acids present in oil from most regions worldwide currently stand as the main responsible for the naphthenic corrosion problems, affecting the oil-refining industry. The phenomenon of sulfidation, accompanying corrosion processes brought about by naphthenic acids in high-temperature refining plant applications, takes place when the combination of sulfidic acid (H2S) with Fe forms layers of iron sulphide (FeS) on the material surface, layers with the potential to protect the material from attack by other corrosive species like naphthenic acids. This work assessed corrosion products formed by sulfidation as inhibitors of naphthenic corrosion rate in AISI-316 steel exposed to processing conditions of simulated crude oil in a dynamic autoclave. Calculation of the sulfidation and naphthenic corrosion rates were determined by gravimetry. The surfaces of the AISI-316 gravimetric coupons exposed to acid systems; were characterized morphologically by X-Ray Diffraction (XRD) and X-ray Fluorescence by Energy Dispersive Spectroscopy (EDS) combined with Scanning Electron Microscopy (SEM). One of the results obtained was the determination of an inhibiting effect of corrosion products at 250 and 300°C, where lower corrosion rate levels were detected. For the temperature of 350°C, naphthenic corrosion rates increased due to deposition of naphthenic acids on the areas where corrosion products formed by sulfidation have lower homogeneity and stability on the surface, thus accelerating the destruction of AISI-316 steel. The above provides an initial contribution to oil industry in search of new alternatives to corrosion control by the attack of naphthenic acids, from the formation of FeS layers on exposed materials in the processing of heavy crude oils with high sulphur content.

  3. Corrosion Behavior and Durability of Low-Alloy Steel Rebars in Marine Environment

    NASA Astrophysics Data System (ADS)

    Liu, Ming; Cheng, Xuequn; Li, Xiaogang; Yue, Pan; Li, Jun

    2016-11-01

    The corrosion resistance of Cr-modified low-alloy steels and HRB400 carbon steel was estimated using the open-circuit potential, potentiodynamic polarization, electrochemical impedance spectroscopic, and weight loss methods in simulated concrete pore solution. Results show that Cr-modified steels exhibit a higher corrosion resistance with a higher critical chloride level (CTL), lower corrosion current density, and higher impedance than carbon steel. The CTL of the steels significantly reduces with increasing temperature. Weight loss measurement shows that the Cr-modified steels exhibit low corrosion rates and small corrosion pitting. The primary constituents of the corrosion scales are Fe2O3, Fe3O4, β-FeOOH, γ-FeOOH, and α-FeOOH. A large amount of α-FeOOH could be detected in the Cr-modified steel corrosion products. Moreover, the Cr-modified steels demonstrate a higher durability than HRB400 carbon steel.

  4. Redemption of asthma pharmaceuticals among stainless steel and mild steel welders: a nationwide follow-up study.

    PubMed

    Kristiansen, Pernille; Jørgensen, Kristian Tore; Hansen, Johnni; Bonde, Jens Peter

    2015-08-01

    The purpose was to examine bronchial asthma according to cumulative exposure to fume particulates conferred by stainless steel and mild steel welding through a proxy of redeemed prescribed asthma pharmaceuticals. A Danish national company-based historical cohort of 5,303 male ever-welders was followed from 1995 to 2011 in the Danish Medicinal Product Registry to identify the first-time redemption of asthma pharmaceuticals including beta-2-adrenoreceptor agonists, adrenergic drugs for obstructive airway diseases and inhalable glucocorticoids. Lifetime exposure to welding fume particulates was estimated by combining questionnaire data on welding work with a welding exposure matrix. The estimated exposure accounted for calendar time, welding intermittence, type of steel, welding methods, local exhaustion and welding in confined spaces. Hazard ratios (HRs) with 95% confidence intervals (CIs) were calculated using a Cox proportional hazards model adjusting for potential confounders and taking modifying effects of smoking into account. The average incidence of redemption of asthma pharmaceuticals in the cohort was 16 per 1,000 person year (95% CI 10-23 per 1,000 person year). A moderate nonsignificant increased rate of redemption of asthma medicine was observed among high-level exposed stainless steel welders in comparison with low-level exposed welders (HR 1.54, 95% CI 0.76-3.13). This risk increase was driven by an increase risk among non-smoking stainless steel welders (HR 1.46, 95% CI 1.06-2.02). Mild steel welding was not associated with increased risk of use asthma pharmaceuticals. The present study indicates that long-term exposure to stainless steel welding is related to increased risk of asthma in non-smokers.

  5. The Influence of Vanadium Microalloying on the Production of Thin Slab Casting and Direct Rolled Steel Strip

    NASA Astrophysics Data System (ADS)

    Li, Yu; Milbourn, David

    Vanadium microalloying is highly effective in high strength strip steels produced by thin slab casting and direct rolled process. Because of the high solubility of V(C,N) in austenite, vanadium is likely to remain in solution during casting, equalisation and rolling. Vanadium microalloyed steels have better hot ductility and are less prone to transverse cracking than niobium containing steels. Despite a coarse as-cast austenite grain size before rolling, significant grain refinement can be achieved in vanadium microalloyed steels by repeated recrystallization during rolling, resulting in a fine uniform ferrite microstructure in final strip. Almost all vanadium present in microalloyed steels is available to precipitate in ferrite as very fine particles, contributing to precipitation strengthening. Vanadium microalloyed steels show less sensitivity to rolling process variables and exhibit excellent combination of strength and toughness.

  6. 77 FR 19192 - Circular Welded Carbon-Quality Steel Pipe From India: Preliminary Affirmative Countervailing Duty...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-03-30

    .... See Memorandum to Susan H. Kuhbach, Director, Office 1 from David Layton, International Trade Analyst... Provision of Hot-Rolled Steel by the Steel Authority of India (``SAIL'') for Less Than Adequate Remuneration... the questions regarding land received at less than adequate remuneration, Zenith prevented us from...

  7. Burden of impaired sleep quality on work productivity in functional dyspepsia.

    PubMed

    Matsuzaki, Juntaro; Suzuki, Hidekazu; Togawa, Koji; Yamane, Tsuyoshi; Mori, Hideki; Komori, Takahiro; Masaoka, Tatsuhiro; Kanai, Takanori

    2018-04-01

    Impaired sleep quality is common, and can reduce work productivity in patients with functional dyspepsia (FD). The objective of this article is to evaluate whether there is a direct association between the presence of FD and the severity of impaired sleep quality, and to calculate the economic loss due to the decreased work productivity associated with sleep quality. In Study 1, using a web-based survey completed by workers with and without FD, we evaluated impaired sleep quality, work and daily productivity, and the severity of reflux and bowel symptoms. In Study 2, the association between the presence of FD and the severity of impaired sleep quality was validated in a hospital-based cohort. In both Study 1 and 2, although impaired sleep quality was more frequent in participants with FD than in those without FD, the independent association between the presence of FD and the severity of impaired sleep quality was not observed after adjustment for the severity of reflux and bowel symptoms. FD participants with impaired sleep quality reported additional economic loss of 53,500 Japanese yen/month. Although the association between impaired sleep quality and FD was indirect, concomitant impaired sleep quality could worsen economic loss.

  8. Evaluation of Environmental Quality Productive Ecosystem Guayas (Ecuador).

    NASA Astrophysics Data System (ADS)

    Pozo, Wilson; Pardo, Francisco; Sanfeliu, Teófilo; Carrera, Gloria; Jordan, Manuel; Bech, Jaume; Roca, Núria

    2015-04-01

    Natural resources are deteriorating very rapidly in the Gulf of Guayaquil and the area of influence in the Guayas Basin due to human activity. Specific problems are generated by the mismanagement of the aquaculture industry affecting the traditional agricultural sectors: rice, banana, sugarcane, cocoa, coffee, and soya also studied, and by human and industrial settlements. The development of industrial activities such as aquaculture (shrimp building for shrimp farming in ponds) and agriculture, have increasingly contributed to the generation of waste, degrading and potentially toxic elements in high concentrations, which can have adverse effects on organisms in the ecosystems, in the health of the population and damage the ecological and environmental balance. The productive Guayas ecosystem, consists of three interrelated ecosystems, the Gulf of Guayaquil, the Guayas River estuary and the Guayas Basin buffer. The objective of this study was to evaluate the environmental quality of the productive Guayas ecosystem (Ecuador), through operational and specific objectives: 1) Draw up the transition coastal zone in the Gulf of Guayaquil, 2) Set temporal spatial variability of soil salinity in wetlands rice, Lower Guayas Basin, 3) evaluate the heavy metals in wetland rice in the Lower Basin of Guayas. The physical and chemical parameters of the soils have been studied. These are indicators of environmental quality. The multivariate statistical method showed the relations of similarities and dissimilarities between variables and parameter studies as stable. Moreover, the boundaries of coastal transition areas, temporal spatial variability of soil salinity and heavy metals in rice cultivation in the Lower Basin of Guayas were researched. The sequential studies included and discussed represent a broad framework of fundamental issues that has been valued as a basic component of the productive Guayas ecosystem. They are determinants of the environmental quality of the Guayas

  9. Effluent Treatment Technologies in the Iron and Steel Industry - A State of the Art Review.

    PubMed

    Das, Pallabi; Mondal, Gautam C; Singh, Siddharth; Singh, Abhay K; Prasad, Bably; Singh, Krishna K

    2018-05-01

      Iron and steel industry is the principal driving force propelling economic and technological growth of a nation. However, since its inception this industry is associated with widespread environmental pollution and enormous water consumption. Different units of a steel plant discharge effluents loaded with toxic, hazardous pollutants, and unutilized components which necessitates mitigation. In this paper, pollutant removal efficiency, effluent volume product quality, and economic feasibility of existing treatments are studied vis-à-vis their merits, demerits, and innovations to access their shortcomings which can be overcome with new technology to identify future research directions. While conventional methods are inadequate for complete remediation and water reclamation, the potential of advanced treatments, like membrane separation, remains relatively untapped. It is concluded that integrated systems combining membrane separation with chemical treatments can guarantee a high degree of contaminant removal, reusability of effluents concurrently leading to process intensification ensuring ecofriendliness and commercial viability.

  10. Power Quality Improvement in Induction Furnace by Harmonic Reduction Using Dynamic Voltage Restorer

    NASA Astrophysics Data System (ADS)

    Saggu, Tejinder Singh; Singh, Lakhwinder

    2016-06-01

    Induction furnaces are used in wide quantity under different capacities for annual production of around 25 million tons of iron and steel in India. It plays a vital role in various manufacturing processes around the world for melting different types of metal scraps i. e. Copper, Cast Iron, Aluminium, Steel, Brass, Bronze, Silicon, Gold, Silver etc. which are further used in many other industrial applications. The induction furnace causes a huge disturbance to the utility and nearby consumers during its operation due to its non-linear characteristics. This is a serious phenomenon responsible for power quality degradation in the power system. This paper presents methodology to improve the power quality degradation caused by induction furnace using Dynamic Voltage Restorer (DVR) which is a type of custom power device. The real time data has been taken from an industry employing induction furnace for production of ingots from scrap material. The experimental readings are measured using power quality analyser equipment. The simulation of whole plant is done by analysing this same data and the simulation results are compared with actual onsite results. Then, solution methodology using DVR is presented which revealed that the implementation of DVR is an effective solution for voltage sag mitigation and harmonics improvement in induction furnace.

  11. Light quality and efficiency of consumer grade solid state lighting products

    NASA Astrophysics Data System (ADS)

    Dam-Hansen, Carsten; Corell, Dennis Dan; Thorseth, Anders; Poulsen, Peter Behrensdorff

    2013-03-01

    The rapid development in flux and efficiency of Light Emitting Diodes (LED) has resulted in a flooding of the lighting market with Solid State Lighting (SSL) products. Many traditional light sources can advantageously be replaced by SSL products. There are, however, large variations in the quality of these products, and some are not better than the ones they are supposed to replace. A lack of quality demands and standards makes it difficult for consumers to get an overview of the SSL products. Here the results of a two year study investigating SSL products on the Danish market are presented. Focus has been on SSL products for replacement of incandescent lamps and halogen spotlights. The warm white light and good color rendering properties of these traditional light sources are a must for lighting in Denmark and the Nordic countries. 266 SSL replacement lamps have been tested for efficiency and light quality with respect to correlated color temperature and color rendering properties. This shows a trade-off between high color rendering warm white light and energy efficiency. The lumen and color maintenance over time has been investigated and results for products running over 11000 h will be presented. A new internet based SSL product selection tool will be shown. Here the products can be compared on efficiency, light quality parameters, thus providing a better basis for the selection of SSL products for consumers.

  12. Deducing material quality in cast and hot-forged steels by new bending test

    NASA Astrophysics Data System (ADS)

    Valberg, Henry; Langøy, Morten; Nedreberg, Mette; Helvig, Torgeir

    2017-10-01

    A special bend test has been developed and applied for the purpose of characterization and comparison of the material ductility in crankpin steel discs manufactured by casting, or casting subsequently followed by hot open-die forging (ODF) or closed-die forging (CDF). The bending test specimen consists of a small rectangular plate of material with a round hole cut out in the middle. The "eye-shape" specimens were cut out from various positions either near to the surface of, or from the interior of the discs. The test method revealed differences in ductility for the investigated materials, and for different depth positions inside the discs. The roughening of the specimen surface on the top-side of the specimen bend also varied dependent on the processing method for the material. Current results show that this test method is useful for evaluation of material quality in differently processed material. Experimental bend test results are presented for differently processed variants of the same material, i.e., crankpin discs either made by solely casting or casting subsequently followed by hot working either by ODF or CDF.

  13. Air Pollutant Emissions Projections for the Cement and Steel Industry in China and the Impact of Emissions Control Technologies

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Hasanbeigi, Ali; Khanna, Nina; Price, Lynn

    significantly lower PM emissions for the cement industry, reaching to 1.7 million tons of PM in 2050, which is less than half of that in the other two scenarios. The Advanced EOP scenario also has the lowest SO2 emissions for the cement industry in China, reaching to 212,000 tons of SO2 in 2050, which is equal to 40 percent of the SO2 emissions in the Advanced scenario and 30 percent of the emissions in the Base Case scenario. The SO2 emission is mainly caused by fuel (coal) burning in cement kiln or steel processes. For the steel industry, the SO2 emissions of the Advanced EOP scenario are significantly lower than the other scenarios, with emissions declining to 323,000 tons in 2050, which is equal to 21 percent and 17 percent of the emissions of Advanced and Base Case scenarios in 2050, respectively. Results of the economic analysis show that for the Chinese cement industry, end-of-pipe PM control technologies have the lowest abatement cost per ton of PM reduced, followed by product change measures and energy efficiency measures, respectively. In summary, in order to meet Chinese national and regional air quality standards, best practice end-of-pipe emissions control technologies must be installed in both cement and steel industry and it must be supplemented by implementation of energy efficiency technologies and reduction of cement and steel production through structural change in industry.« less

  14. Characterization and prediction of carbon steel corrosion in diluted seawater containing pentaborate

    NASA Astrophysics Data System (ADS)

    Fukaya, Yuichi; Watanabe, Yutaka

    2018-01-01

    This study addresses the influence of Na2B10O16, which may be used for criticality control of fuel debris in the Fukushima Daiichi Nuclear Power Station, on the corrosion behavior of carbon steel in diluted artificial seawater. The corrosion forms of carbon steel were categorized as uniform corrosion, localized corrosion, and passivity based on the balance between the dilution ratio of artificial seawater and the concentration of Na2B10O16. The changes in corrosion forms were arranged on a water quality region map. Passivity was maintained by adding 3.7 × 10-2 M or more of Na2B10O16 to artificial seawater with a dilution ratio of 100-fold or more. The criticality control of the fuel debris and corrosion mitigation of the carbon steel components may be achieved simultaneously in the water quality. The prediction of the corrosion form of carbon steel was attempted by the extended Larson-Skold Index (LSI) = ([Cl-] + 2[SO42-])/([HCO3-] + 2[B10O162-]). However, because the passivating action of B10O162- was remarkably stronger than that of HCO3-, the prediction was difficult under the simple addition of equivalent concentrations. The localized corrosion of carbon steel under the addition of Na2B10O16 preferentially occurred from the crevices of the test specimens, as was the case in stainless steel.

  15. Respiratory health of workers exposed to low levels of chromium in stainless steel production.

    PubMed Central

    Huvinen, M; Uitti, J; Zitting, A; Roto, P; Virkola, K; Kuikka, P; Laippala, P; Aitio, A

    1996-01-01

    OBJECTIVES: To determine whether occupational exposure to chromite, trivalent chromium, or hexavalent chromium causes respiratory diseases, an excess of respiratory symptoms, a decrease in pulmonary function, or signs of pneumoconiosis among workers in an integrated chain of stainless steel production. METHODS: This cross sectional study was carried out in 1993 and the inclusion criterion was a minimum of eight years of employment in the same production department. A self administered questionnaire was collected, and spirometry, measurement of diffusing capacity, chest radiography, and laboratory tests were carried out by a mobile research unit. RESULTS: There were 221 workers in the exposure groups and 95 in the control group. The average duration of employment was 18 years. No significant differences in the odds ratios (ORs) of the symptoms were found between the exposure and the control groups. In a logistic regression analysis age and smoking significantly explained the occurrence of most of the respiratory symptoms. The smokers in the chromite group had significantly lower forced vital capacity (FVC), forced expiratory volume in one second (FEV1), and diffusing capacity than the corresponding values of the control group. The analysis of variance between study groups, smoking, and exposure time, without modelling for interactions, showed that the chromite group had lower values for FVC, FEV1, and diffusing capacity than the other groups. The occurrence of small opacities was more frequent on the chest radiographs of the workers in the chromite group. CONCLUSIONS: An average exposure time of 18 years in ferrochromium and stainless steel production and exposure to dusts containing low concentrations of hexavalent or trivalent chromium do not lead to any respiratory changes detectable by lung function tests or radiography nor to any increase in symptoms of respiratory diseases. The lung function values were lower and the occurrence of radiological findings was

  16. Certification of production-quality gLite Job Management components

    NASA Astrophysics Data System (ADS)

    Andreetto, P.; Bertocco, S.; Capannini, F.; Cecchi, M.; Dorigo, A.; Frizziero, E.; Giacomini, F.; Gianelle, A.; Mezzadri, M.; Molinari, E.; Monforte, S.; Prelz, F.; Rebatto, D.; Sgaravatto, M.; Zangrando, L.

    2011-12-01

    With the advent of the recent European Union (EU) funded projects aimed at achieving an open, coordinated and proactive collaboration among the European communities that provide distributed computing services, more strict requirements and quality standards will be asked to middleware providers. Such a highly competitive and dynamic environment, organized to comply a business-oriented model, has already started pursuing quality criteria, thus requiring to formally define rigorous procedures, interfaces and roles for each step of the software life-cycle. This will ensure quality-certified releases and updates of the Grid middleware. In the European Middleware Initiative (EMI), the release management for one or more components will be organized into Product Team (PT) units, fully responsible for delivering production ready, quality-certified software and for coordinating each other to contribute to the EMI release as a whole. This paper presents the certification process, with respect to integration, installation, configuration and testing, adopted at INFN by the Product Team responsible for the gLite Web-Service based Computing Element (CREAM CE) and for the Workload Management System (WMS). The used resources, the testbeds layout, the integration and deployment methods, the certification steps to provide feedback to developers and to grant quality results are described.

  17. 75 FR 5146 - Tempel Steel Company Including On-Site Leased Workers From Aerotek Staffing Chicago, IL; Tempel...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-02-01

    ... the production of lamination sheet steel for electric motors and transformers. New findings show that... affected by a shift in production of lamination sheet steel for electric motors and transformers to Mexico...

  18. Highlights of contractor initiatives in quality enhancement and productivity improvement

    NASA Technical Reports Server (NTRS)

    1986-01-01

    The NASA/Contractor Team efforts are presented as part of NASA's continuing effort to facilitate the sharing of quality and productivity improvement ideas among its contractors. This complilation is not meant to be a comprehensive review of contractor initiative nor does it necessarily express NASA's views. The submissions represent samples from a general survey, and were not edited by NASA. The efforts are examples of quality and productivity programs in private industry, and as such, highlight company efforts in individual areas. Topics range from modernization of equipment, hardware, and technology to management of human resources. Of particular interest are contractor initiatives which deal with measurement and evaluation data pertaining to quality and productivity performance.

  19. The influence of the structure of the metal load removal from liquid steel in electric arc furnaces

    NASA Astrophysics Data System (ADS)

    Pǎcurar, Cristina; Hepuť, Teodor; Crisan, Eugen

    2016-06-01

    One of the main technical and economic indicators in the steel industry and steel respectively the development it is the removal of liquid steel. This indicator depends on several factors, namely technology: the structure and the quality metal load, the degree of preparedness of it, and the content of non-metallic material accompanying the unit of drawing up, the technology for the elaboration, etc. research has been taken into account in drawing up steel electric arc furnace type spring EBT (Electric Bottom taping), seeking to load and removing components of liquid steel. Metal load has been composed of eight metal grades, in some cases with great differences in terms of quality. Data obtained were processed in the EXCEL spreadsheet programs and MATLAB, the results obtained being presented both graphically and analytically. On the basis of the results obtained may opt for a load optimal structure metal.

  20. Production of Near-Mirror Surface Quality by Precision Grinding

    NASA Technical Reports Server (NTRS)

    Dimofte, Florin; Krantz, Timothy

    2003-01-01

    Mechanical components such as gears and bearings operate with the working surfaces in intimate contact with a mating part. The performance of such components will be influenced by the quality of the working surface. In general, a smoother surface will perform better than a rougher surface since the lubrication conditions are improved. For example, surfaces with a special near-mirror quality finish of low roughness performed better than ground surfaces when tested using a block-on-ring arrangement. Bearings with near-mirror quality have been tested and analyzed; lower running torques were measured and improved fatigue life was anticipated. Experiments have been done to evaluate the performance of gears with improved, low roughness surface finishing. The measured performance improvements include an increased scuffing (scoring) load capacity by a factor of 1.6, a 30-percent reduction of gear tooth running friction, and longer fatigue lives by a factor of about four. One can also anticipate that near-mirror quality surface finishing could improve the performance of other mechanical components such as mechanical seals and heavily loaded journal bearings. Given these demonstrated benefits, capable and economical methods for the production of mechanical components with near-mirror quality surfaces are desired. One could propose the production of near-mirror quality surfaces by several methods such as abrasive polishing, chemical assisted polishing, or grinding. Production of the surfaces by grinding offers the possibility to control the macro-geometry (form), waviness, and surface texture with one process. The present study was carried out to investigate the possibility of producing near-mirror quality surfaces by grinding. The present study makes use of a specially designed grinding machine spindle to improve the surface quality relative to the quality produced when using a spindle of conventional design.

  1. The role of food quality assurance and product certification systems on marketing aspects

    NASA Astrophysics Data System (ADS)

    Petrović, Z.; Milićević, D.; Nastasijević, I.; Đorđević, V.; Trbović, D.; Velebit, B.

    2017-09-01

    The level of quality that a product offers to consumers is a fundamental aspect of competition in many markets. Consumers’ confidence in the safety and quality of foods they buy and consume is a significant support to the economic development of production organizations of this type, and therefore the overall economic development. Consumer concerns about food safety as well as the globalization of food production have also led to the existence of a global internationally linked food production and distribution system. The necessity demanded by the consumer population to provide safe food with consistent quality at an attractive price imposes a choice of an appropriate quality assurance model in accordance with the specific properties of the product and the production processes. Modern trends, especially for the last ten years in quality assurance within specific production, such as the food industry, have marked the trend of hyperproduction and a number of production and safety standards, as well as a change of approach in the certification process of organizations according to one or more standards. This can be an additional source of costs for organizations, and can burden the food business operator`s budget in order to ensure their consistent application and maintenance. Quality assurance (QA) standards are considered to be a proven mechanism for delivering quality of product.

  2. Getting started on metrics - Jet Propulsion Laboratory productivity and quality

    NASA Technical Reports Server (NTRS)

    Bush, M. W.

    1990-01-01

    A review is presented to describe the effort and difficulties of reconstructing fifteen years of JPL software history. In 1987 the collection and analysis of project data were started with the objective of creating laboratory-wide measures of quality and productivity for software development. As a result of this two-year Software Product Assurance metrics study, a rough measurement foundation for software productivity and software quality, and an order-of-magnitude quantitative baseline for software systems and subsystems are now available.

  3. Summary of strategies for planning Productivity Improvement and Quality Enhancement (PIQE)

    NASA Technical Reports Server (NTRS)

    1986-01-01

    The Summary of NASA Strategies for Productivity Improvement and Quality Enhancement respond to NASA's eighth top goal: Establish NASA as a leader in the development and application of advanced technology and management practices which contribute to significant increases in both Agency and national productivity. The Strategies provide the framework for development of the agency-wide Productivity Improvement and Quality Enhancement (PIQE) Plans.

  4. A quality-based cost model for new electronic systems and products

    NASA Astrophysics Data System (ADS)

    Shina, Sammy G.; Saigal, Anil

    1998-04-01

    This article outlines a method for developing a quality-based cost model for the design of new electronic systems and products. The model incorporates a methodology for determining a cost-effective design margin allocation for electronic products and systems and its impact on manufacturing quality and cost. A spreadsheet-based cost estimating tool was developed to help implement this methodology in order for the system design engineers to quickly estimate the effect of design decisions and tradeoffs on the quality and cost of new products. The tool was developed with automatic spreadsheet connectivity to current process capability and with provisions to consider the impact of capital equipment and tooling purchases to reduce the product cost.

  5. Aggregation of a Monoclonal Antibody Induced by Adsorption to Stainless Steel

    PubMed Central

    Bee, Jared S.; Davis, Michele; Freund, Erwin; Carpenter, John F.; Randolph, Theodore W.

    2014-01-01

    Stainless steel is a ubiquitous surface in therapeutic protein production equipment and is also present as the needle in some pre-filled syringe biopharmaceutical products. Stainless steel microparticles can cause of aggregation of a monoclonal antibody (mAb). The initial rate of mAb aggregation was second-order in steel surface area and zero-order in mAb concentration, generally consistent with a bimolecular surface aggregation being the rate-limiting step. Polysorbate 20 (PS20) suppressed the aggregation yet was unable to desorb the firmly bound first layer of protein that adsorbs to the stainless steel surface. Also, there was no exchange of mAb from the first adsorbed layer to the bulk phase, suggesting that the aggregation process actually occurs on subsequent adsorption layers. No oxidized Met residues were detected in the mass spectrum of a digest of a highly aggregated mAb, although there was five-fold increase in carbonyl groups due to protein oxidation. PMID:19725039

  6. Post driver for steel guardrail posts : final report.

    DOT National Transportation Integrated Search

    2003-01-01

    The objective of this research project was to locate an existing product, or if necessary, design and develop a product for use as a driver for steel guardrail posts. The post driver would also be able to minimize the bending and twisting of the stee...

  7. Mechanical Properties of Heat Affected Zone of High Strength Steels

    NASA Astrophysics Data System (ADS)

    Sefcikova, K.; Brtnik, T.; Dolejs, J.; Keltamaki, K.; Topilla, R.

    2015-11-01

    High Strength Steels became more popular as a construction material during last decade because of their increased availability and affordability. On the other hand, even though general use of Advanced High Strength Steels (AHSS) is expanding, the wide utilization is limited because of insufficient information about their behaviour in structures. The most widely used technique for joining steels is fusion welding. The welding process has an influence not only on the welded connection but on the area near this connection, the so-called heat affected zone, as well. For that reason it is very important to be able to determine the properties in the heat affected zone (HAZ). This area of investigation is being continuously developed in dependence on significant progress in material production, especially regarding new types of steels available. There are currently several types of AHSS on the world market. Two most widely used processes for AHSS production are Thermo-Mechanically Controlled Processing (TMCP) and Quenching in connection with Tempering. In the presented study, TMCP and QC steels grade S960 were investigated. The study is focused on the changes of strength, ductility, hardness and impact strength in heat affected zone based on the used amount of heat input.

  8. New alloys to conserve critical elements. [replacing chromium in steels

    NASA Technical Reports Server (NTRS)

    Stephens, J. R.

    1978-01-01

    Previous studies and surveys on availability of domestic reserves have shown that chromium is a most critical element within the U.S. metal industry. More precisely, the bulk of chromium is consumed in the production of stainless steels, specifically Type 304 stainless steel (304SS) which contains 18% Cr. The present paper deals with means of reducing chromium in commercial stainless steels by substituting more abundant or less expensive elements with the intent of maintaining the properties of 304SS. The discussion focuses on some of the oxidation and corrosion properties of new substitute stainless steels with only 12% Cr, which represents a potential saving of 33% of the chromium consumed in the production of 304SS. The alloying elements substituted for Cr in 304SS are selected according to their potential for protective oxide formation during high-temperature oxidation; these are Al, Si, Ti, Y, and misch metal which is 99.7% rare-earth metals containing 50 to 55% cerium. Other alloying elements to impart corrosion resistance are Mn, Mo, and V.

  9. Novel sintered ceramic materials incorporated with EAF carbon steel slag

    NASA Astrophysics Data System (ADS)

    Karayannis, V.; Ntampegliotis, K.; Lamprakopoulos, S.; Papapolymerou, G.; Spiliotis, X.

    2017-01-01

    In the present research, novel sintered clay-based ceramic materials containing electric arc furnace carbon steel slag (EAFC) as a useful admixture were developed and characterized. The environmentally safe management of steel industry waste by-products and their valorization as secondary resources into value-added materials towards circular economy have attracted much attention in the last years. EAF Carbon steel slag in particular, is generated during the manufacture of carbon steel. It is a solid residue mainly composed of rich-in- Fe, Ca and Si compounds. The experimental results show that the beneficial incorporation of lower percentages of EAFC up to 6%wt. into ceramics sintered at 950 °C is attained without significant variations in sintering behavior and physico-mechanical properties. Further heating up to 1100 °C strongly enhances the densification of the ceramic microstructures, thus reducing the porosity and strengthening their mechanical performance. On the other side, in terms of thermal insulation behavior as well as energy consumption savings and production cost alleviation, the optimum sintering temperature appears to be 950 °C.

  10. Progress in thermomechanical control of steel plates and their commercialization

    PubMed Central

    Nishioka, Kiyoshi; Ichikawa, Kazutoshi

    2012-01-01

    The water-cooled thermomechanical control process (TMCP) is a technology for improving the strength and toughness of water-cooled steel plates, while allowing control of the microstructure, phase transformation and rolling. This review describes metallurgical aspects of the microalloying of steel, such as niobium addition, and discusses advantages of TMCP, for example, in terms of weldability, which is reduced upon alloying. Other covered topics include the development of equipment, distortions in steel plates, peripheral technologies such as steel making and casting, and theoretical modeling, as well as the history of property control in steel plate production and some early TMCP technologies. We provide some of the latest examples of applications of TMCP steel in various industries such as shipbuilding, offshore structures, building construction, bridges, pipelines, penstocks and cryogenic tanks. This review also introduces high heat-affected-zone toughness technologies, wherein the microstructure of steel is improved by the addition of fine particles of magnesium-containing sulfides and magnesium- or calcium-containing oxides. We demonstrate that thanks to ongoing developments TMCP has the potential to meet the ever-increasing demands of steel plates. PMID:27877477

  11. Occult exposure to asbestos in steel workers revealed by bronchoalveolar lavage

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Corhay, J.-L.; Delavignette, J.-P.; Bury, T.

    To investigate the asbestos burden in a steelplant environment, we counted asbestos bodies (ABs) in the bronchoalveolar lavage fluid (BALF) of 65 steel workers who had retired during the previous 5 y. They had worked for at least 15 y in the same area of the plant (coke oven or blast furnace) as maintenance or production workers. On the basis of occupational anamnesis, 28 had occasional past professional exposure to asbestos; the remaining 37 workers denied any contact with asbestos. A total of 54 white-collar workers who had no occupational exposure to asbestos were included in the study as controls.more » An increased prevalence and concentration of ABs was found in the BALF of steel workers. Electron microscopy and EDAX analysis of AB from steel workers revealed that the core fibers were mainly amphiboles. More ABs were found in the BALF of maintenance workers than in production workers. However, the BALF from steel workers who denied any contact with asbestos revealed an increased AB burden v. controls. This demonstrates that steel workers may be subject to an occult exposure to amphiboles in the steelplant environment.« less

  12. Innovative Use of Quality Management Methods for Product Improvement

    NASA Astrophysics Data System (ADS)

    Midor, Katarzyna; Žarnovský, Jozef

    2016-12-01

    Organisations constantly look for new, innovative solutions and methods which could be used to improve their efficiency and increase the quality of their products. Identifying the causes for returns is an important issue for modern companies, as returns are the cause for the increase in production costs and, most importantly, the loss of credibility in the eyes of the client. Therefore, for the company to be able to sustain or strengthen its position on the market, it has to follow the rules of quality management. Especially important is the rule of constant improvement. This rule is primarily connected with preventing errors and defects from occurring at all the stages of the production process. To achieve that, one must, among other things, use quality management tools. The article presents an analysis of causes for returns of a vibrating screen produced by a company which manufactures machinery and equipment for the extractive industry, using quality management tools such as the Ishikawa diagram and Pareto analysis. The analysis allowed for the identification of the causes of client returns which could not be previously identified, and proposing solutions for them.

  13. Atmospheric Corrosion Behavior and Mechanism of a Ni-Advanced Weathering Steel in Simulated Tropical Marine Environment

    NASA Astrophysics Data System (ADS)

    Wu, Wei; Zeng, Zhongping; Cheng, Xuequn; Li, Xiaogang; Liu, Bo

    2017-12-01

    Corrosion behavior of Ni-advanced weathering steel, as well as carbon steel and conventional weathering steel, in a simulated tropical marine atmosphere was studied by field exposure and indoor simulation tests. Meanwhile, morphology and composition of corrosion products formed on the exposed steels were surveyed through scanning electron microscopy, energy-dispersive x-ray spectroscopy and x-ray diffraction. Results indicated that the additive Ni in weathering steel played an important role during the corrosion process, which took part in the formation of corrosion products, enriched in the inner rust layer and promoted the transformation from loose γ-FeOOH to dense α-FeOOH. As a result, the main aggressive ion, i.e., Cl-, was effectively separated in the outer rust layer which leads to the lowest corrosion rate among these tested steels. Thus, the resistance of Ni-advanced weathering steel to atmospheric corrosion was significantly improved in a simulated tropical marine environment.

  14. Investigation of Cutting Quality of Remote DOE Laser Cutting in 0.5 mm Stainless Steel

    NASA Astrophysics Data System (ADS)

    Villumsen, Sigurd Lazic; Kristiansen, Morten

    It has previously been shown that the stability of the remote fusion cutting (RFC) process can be increased by modifying the intensity profile of the laser by means of a diffractive optical element (DOE). This paper investigates the quality of remote DOE cutting (RDC) conducted with a 3 kW single mode fiber laser in 0.5 mm stainless steel. An automatic measurement system is used to investigate how the travel speed, focus offset and angle of incidence effect the kerf width and kerf variance. The study shows that the RDC process has a very low kerf width variance, and that the kerf width decreases with cutting speed. Furthermore, selected etched samples show a significant increase in the perpendicularity of the cuts when compared to RFC. Also, on average, the depth of the layer of molten material for RFC is 83% deeper than for RDC.

  15. Joining dissimilar stainless steels for pressure vessel components

    NASA Astrophysics Data System (ADS)

    Sun, Zheng; Han, Huai-Yue

    1994-03-01

    A series of studies was carried out to examine the weldability and properties of dissimilar steel joints between martensitic and austenitic stainless steels - F6NM (OCr13Ni4Mo) and AISI 347, respectively. Such joints are important parts in, e.g. the primary circuit of a pressurized water reactor (PWR). This kind of joint requires both good mechanical properties, corrosion resistance and a stable magnetic permeability besides good weldability. The weldability tests included weld thermal simulation of the martensitic steel for investigating the influence of weld thermal cycles and post-weld heat treatment (PWHT) on the mechanical properties of the heat-affected zone (HAZ); implant testing for examining the tendency for cold cracking of martensitic steel; rigid restraint testing for determining hot crack susceptibility of the multi-pass dissimilar steel joints. The joints were subjected to various mechanical tests including a tensile test, bending test and impact test at various temperatures, as well as slow strain-rate test for examining the stress corrosion cracking tendency in the simulated environment of a primary circuit of a PWR. The results of various tests indicated that the quality of the tube/tube joints is satisfactory for meeting all the design requirements.

  16. Methods of steel manufacturing - The electric arc furnace

    NASA Astrophysics Data System (ADS)

    Dragna, E. C.; Ioana, A.; Constantin, N.

    2018-01-01

    Initially, the carbon content was reduced by mixing “the iron” with metallic ingots in ceramic crucibles/melting pots, with external heat input. As time went by the puddling procedure was developed, a procedure which also assumes a mixture with oxidized iron ore. In 1856 Bessemer invented the convertor, thus demonstrating that steel can be obtained following the transition of an air stream through the liquid pig iron. The invention of Thomas, a slightly modified basic-lined converter, fostered the desulphurization of the steel and the removal of the phosphate from it. During the same period, in 1865, in Sireuil, the Frenchman Martin applies Siemens’ heat regeneration invention and brings into service the furnace with a charge composed of iron pig, scrap iron and iron ore, that produces a high quality steel [1]. An act worthy of being highlighted within the scope of steelmaking is the start-up of the converter with oxygen injection at the upper side, as there are converters that can produce 400 tons of steel in approximately 50 minutes. Currently, the share of the steel produced in electric arc furnaces with a charge composed of scrap iron has increased. Due to this aspect, the electric arc furnace was able to impose itself on the market.

  17. Utilization of steel in industrialized highway bridge systems.

    DOT National Transportation Integrated Search

    1974-01-01

    The space frame concept presented in this report represents the results of an effort to minimize on-site construction time while utilizing steel to provide a high quality but competitive type of bridge structure. A necessary part of the effort was th...

  18. Laser Welding of Coated Press-hardened Steel 22MnB5

    NASA Astrophysics Data System (ADS)

    Siltanen, Jukka; Minkkinen, Ari; Järn, Sanna

    The press-hardening process is widely used for steels that are used in the automotive industry. Using ultra-high-strength steels enables car manufacturers to build lighter, stronger, and safer vehicles at a reduced cost and generating lower CO2 emissions. In the study, laser welding properties of the coated hot stamped steel 22BMn5 were studied. A constant 900 °C temperature was used to heat the steel plates, and two different furnace times were used in the press-hardening, being 300 and 740 seconds. Some of the plates were shot blasted to see the influence of the partly removed oxide layer on the laser welding and quality. The welding set-up, welding, and testing of the weld specimens complied with the automotive testing code SEP 1220.

  19. A comparative study on performance of CBN inserts when turning steel under dry and wet conditions

    NASA Astrophysics Data System (ADS)

    Abdullah Bagaber, Salem; Razlan Yusoff, Ahmad

    2017-10-01

    Cutting fluids is the most unsustainable components of machining processes, it is negatively impacting on the environmental and additional energy required. Due to its high strength and corrosion resistance, the machinability of stainless steel has attracted considerable interest. This study aims to evaluate performance of cubic boron nitride (CBN) inserts for the machining parameters includes the power consumption and surface roughness. Due to the high single cutting-edge cost of CBN, the performance of significant is importance for hard finish turning. The present work also deals with a comparative study on power consumption and surface roughness under dry and flood conditions. Turning process of the stainless steel 316 was performed. A response surface methodology based box-behnken design (BBD) was utilized for statistical analysis. The optimum process parameters are determined as the overall performance index. The comparison study has been done between dry and wet stainless-steel cut in terms of minimum value of energy and surface roughness. The result shows the stainless still can be machined under dry condition with 18.57% improvement of power consumption and acceptable quality compare to the wet cutting. The CBN tools under dry cutting stainless steel can be used to reduce the environment impacts in terms of no cutting fluid use and less energy required which is effected in machining productivity and profit.

  20. Quantifying Impact of Biofeedstock Production on Hydrology/Water Quality in Midwest USA

    NASA Astrophysics Data System (ADS)

    Chaubey, Indrajeet; Engel, Bernard; Thomas, Mark; Raj, Cibin; Saraswat, Dharmendra

    2010-05-01

    The production of biofeedstocks for biofuels is likely to impact the hydrology and water quality of watersheds. Communities potentially impacted are increasingly concerned, and at present, little is known regarding the magnitude of impacts of biofeedstock production on hydrology and water quality. We have initiated a national facilitation project to answer the following questions: What are the unintended environmental consequences of increased corn production to meet biofuel demands? What are the environmental impacts of various second generation biofeedstock production systems to meet cellulosic ethanol demands? Would the management of cropping systems involving corn silage meet cellulosic ethanol demands with minimal environmental impact? What are the broad-scale water quality implications of energy crops, such as switchgrass, grown for bioenergy production on highly erodible soils? This presentation will discuss development of multi-regional agricultural land management practices that can be implemented to mitigate potential negative environmental impacts associated with biofeedstock production while meeting the biofuel production demand. Specifically, we will discuss how watershed scale modeling can be utilized to evaluate the environmental impacts of various biofeedstock production strategies. We will also discuss regional differences in alternative biofeedstock production and associated hydrologic/water quality impacts.

  1. Process for making a martensitic steel alloy fuel cladding product

    DOEpatents

    Johnson, Gerald D.; Lobsinger, Ralph J.; Hamilton, Margaret L.; Gelles, David S.

    1990-01-01

    This is a very narrowly defined martensitic steel alloy fuel cladding material for liquid metal cooled reactors, and a process for making such a martensitic steel alloy material. The alloy contains about 10.6 wt. % chromium, about 1.5 wt. % molybdenum, about 0.85 wt. % manganese, about 0.2 wt. % niobium, about 0.37 wt. % silicon, about 0.2 wt. % carbon, about 0.2 wt. % vanadium, 0.05 maximum wt. % nickel, about 0.015 wt. % nitrogen, about 0.015 wt. % sulfur, about 0.05 wt. % copper, about 0.007 wt. % boron, about 0.007 wt. % phosphorous, and with the remainder being essentially iron. The process utilizes preparing such an alloy and homogenizing said alloy at about 1000.degree. C. for 16 hours; annealing said homogenized alloy at 1150.degree. C. for 15 minutes; and tempering said annealed alloy at 700.degree. C. for 2 hours. The material exhibits good high temperature strength (especially long stress rupture life) at elevated temperature (500.degree.-760.degree. C.).

  2. Contract Incentives for Product Quality

    DTIC Science & Technology

    1980-06-01

    incurred by the contractor, i.e., cost reimbursement contracts. It differs also in that the product may only be definable in general terms, thus...government employees. There are other fiscal motivations as well since if government quality personnel do not accept their system, reimbursement will not... reimbursement contracts in the DAR, Paragraph 3-808.1 as follows: 3-808 Profit, Including Fees Under Cost- Reimbursement Type Contracts 3-808.1 Policy (a

  3. Development and application of free pretreatment container steel

    NASA Astrophysics Data System (ADS)

    Yang, Y.; Liu, Y.; Han, B.; Wei, B.; Wang, S. Z.

    2017-12-01

    Due to economic and environmental advantages pre-treatment containers have good big development prospects, which can avoid shot blasting processes, and decrease the noise and dust pollution. By analyzing requirements of the container steel surface quality, target oxide scale structure of free pretreatment container steel has been determined. Trial process was carried out, and test results showed that the oxide scale achieved the desired objects, oxide scale with outer thin Fe3O4 layer and inner eutectoid α-Fe+Fe3O4. Salt spray test, second adhesion test, and modeling performance basically corroborated the container feasibility.

  4. Development of a Hot Working Steel Based on a Controlled Gas-Metal-Reaction

    NASA Astrophysics Data System (ADS)

    Ritzenhoff, Roman; Gharbi, Mohammad Malekipour

    As a result of cost sensitiveness, the demand on hot working steels with advanced characteristics and properties are ascending. We have used a controlled gas-metal-reaction in a P-ESR furnace to produce high quality hot working steel. These types of materials are also known as High Nitrogen Steels (HNS). An overview of the development in a pressurized induction furnace to the final industrial scale using P-ESR will be provided. Different heat treatment strategies are conducted and their effect on mechanical properties is investigated.

  5. Image processing system performance prediction and product quality evaluation

    NASA Technical Reports Server (NTRS)

    Stein, E. K.; Hammill, H. B. (Principal Investigator)

    1976-01-01

    The author has identified the following significant results. A new technique for image processing system performance prediction and product quality evaluation was developed. It was entirely objective, quantitative, and general, and should prove useful in system design and quality control. The technique and its application to determination of quality control procedures for the Earth Resources Technology Satellite NASA Data Processing Facility are described.

  6. Research and Process-Optimization on Mixed Crystal Caused Uneven-Performance of High-strength Structural Car Steel QStE500TM

    NASA Astrophysics Data System (ADS)

    Jian-wen, Li; Hong-yan, Liu

    Handan Iron and Steel production of high-strength structural car steel QStE500TM thin gauge products using Nb + Ti composite strengthening, with a small amount of Cr element to improve its hardenability, the process parameter control is inappropriate with Nb + Ti complex steel, it is easy to produce in the mixed crystal phenomenon, resulting in decreasing the toughness and uneven performance. In this paper, Gleeble 3500 thermal simulation testing machine for high-strength structural steel car QStE500TM product deformation austenite recrystallization behavior research, determined completely recrystallized, partial recrystallization and non-recrystallization region, provide theoretical basis and necessary data for reasonable controlled rolling process for production.

  7. Development and Technology of Large Thickness TMCP Steel Plate with 390MPA Grade Used for Engineering Machinery

    NASA Astrophysics Data System (ADS)

    Wang, Xiaoshu; Zhang, Zhijun; Zhang, Peng

    Recently, with the rapid upgrading of the equipment in the steel Corp, the rolling technology of TMCP has been rapidly developed and widely applied. A large amount of steel plate has been produced by using the TMCP technology. The TMCP processes have been used more and more widely and replaced the heat treatment technology of normalizing, quenching and tempering heat process. In this paper, low financial input is considered in steel plate production and the composition of the steel has been designed with low C component, a limited alloy element of the Nb, and certain amounts of Mn element. During the continuous casting process, the size of the continuous casting slab section is 300 mm × 2400 mm. The rolling technology of TMCP is controlled at a lower rolling and red temperature to control the transformation of the microstructure. Four different rolling treatments are chosen to test its effects on the 390MPa grade low carbon steel of bainitic microstructure and properties. This test manages to produce a proper steel plate fulfilling the standard mechanical properties. Specifically, low carbon bainite is observed in the microstructure of the steel plate and the maximum thickness of steel plate under this TMCP technology is up to 80mm. The mechanical property of the steel plate is excellent and the KV2 at -40 °C performs more than 200 J. Moreover, the production costs are greatly reduced when the steel plate is produced by this TMCP technology when replacing the current production process of quenching and tempering. The low cost steel plate could well meet the requirements of producing engineering machinery in the steel market.

  8. 75 FR 36678 - Prestressed Concrete Steel Wire Strand From China; Determinations

    Federal Register 2010, 2011, 2012, 2013, 2014

    2010-06-28

    ... Concrete Steel Wire Strand From China; Determinations On the basis of the record \\1\\ developed in the... prestressed concrete steel wire strand (PC strand), provided for in subheading 7312.10.30 of the Harmonized... Spring Wire Corp. (Bedford Heights, OH); Insteel Wire Products Co. (Mt. Airy, NC); and Sumiden Wire...

  9. Quality First in Education... Why Not? Using Quality and Productivity Methods To Improve Schools.

    ERIC Educational Resources Information Center

    Spanbauer, Stanley J.; Hillman, Jo Ann

    A description is provided of the implementation at Fox Valley Technical College (FVTC), Wisconsin, of the Quality First Process Model, which was adapted from a model commonly used in manufacturing and service industries. The model uses private sector quality and productivity procedures and new management styles to serve students more effectively,…

  10. Preparation and Characterization of Silanes Films to Protect Electrogalvanized Steel

    NASA Astrophysics Data System (ADS)

    Seré, Pablo R.; Egli, Walter; Di Sarli, Alejandro R.; Deyá, Cecilia

    2018-03-01

    Silanes are an interesting alternative to chromate-based surface treatments for temporary protection of electrogalvanized steel. In this work, the protective behavior of 3-mercaptopropyltrimethoxysilane (MTMO), 3-aminopropyltriethoxysilane (AMEO), or 3-glycidoxypropyltrimethoxysilane (GLYMO) films applied on electrogalvanized automotive quality steel sheets has been studied. The silane coating morphology, composition, and porosity were characterized by scanning electron microscopy (SEM), energy-dispersive x-ray spectroscopy (EDS), x-ray fluorescence, immersion in copper sulfate, and cyclic voltammetry. The corrosion protection was evaluated by polarization curves, electrochemical noise measurements, electrochemical impedance spectrometry, and accelerated humidity chamber tests. The results showed that the silanes protect temporarily electrogalvanized steel from corrosion. MTMO forms a relatively thick and cracked film. AMEO and GLYMO films were so thin that they could not be observed by SEM but silicon was detected by EDS. MTMO provided good temporary protection, being an alternative to replace Cr(VI) as protector of electrogalvanized steel.

  11. High Power Laser Welding. [of stainless steel and titanium alloy structures

    NASA Technical Reports Server (NTRS)

    Banas, C. M.

    1972-01-01

    A review of recent developments in high power, carbon dixoide laser welding is presented. Deep penetration welding in stainless steel to 0.5-in. thick, high speed welding in thin gage rimmed steel and gas shielded welding in Ti-6Al-4V alloy are described. The effects of laser power, power density, focusing optics, gas-shielding techniques, material properties and weld speed on weld quality and penetration are discussed. It is shown that laser welding performance in thin materials is comparable to that of electron beams. It is further shown that high quality welds, as evidenced by NDT, mechanical and metal-lographic tests, can be achieved. The potential of the laser for industrial welding applications is indicated.

  12. Application of fuzzy set theory for integral assessment of agricultural products quality

    NASA Astrophysics Data System (ADS)

    Derkanosova, N. M.; Ponomareva, I. N.; Shurshikova, G. V.; Vasilenko, O. A.

    2018-05-01

    The methodology of integrated assessment of quality and safety of agricultural products, approbated by the example of indicators of wheat grain in relation to the provision of consumer properties of bakery products, was developed. Determination of the level of quality of the raw ingredients will allow direct using of agricultural raw materials for food production, taking into account ongoing technology, types of products, and, respectively, rational use of resource potential of the agricultural sector. The mathematical tool of the proposed method is a fuzzy set theory. The fuzzy classifier to evaluate the properties of the grain is formed. The set of six indicators normalized by the national standard is determined; values are ordered and represented by linguistic variables with a trapeziform membership function; the rules for calculation of membership functions are presented. Specific criteria values for individual indicators in shaping the quality of the finished products are considered. For one of the samples of wheat grain values of membership; functions of the linguistic variable "level" for all indicators and the linguistic variable "level of quality" were calculated. It is established that the studied sample of grain obtains the 2 (average) level of quality. Accordingly, it can be recommended for the production of bakery products with higher requirements for the structural-mechanical properties bakery and puff pastry products hearth bread and flour confectionery products of the group of hard dough cookies and crackers

  13. Steel and biodiversity: a promising alliance

    NASA Astrophysics Data System (ADS)

    Peters, Klaus; Colla, Valentina; Moonen, Anna Camilla; Branca, Teresa Annunziata; Moretto, Deny Del; Ragaglini, Giorgio; Delmiro, Vanesa Maria Menendez; Romaniello, Lea; Carler, Sophie; Hodges, Jennifer; Bullock, Matthew; Malfa, Enrico

    2018-06-01

    The term "Biodiversity" derives from a contraction of "biological diversity" and commonly refers to a measure of the variety of organisms, which are present in different ecosystems, by considering genetic variation, ecosystem variation, or species variation within an area, biome, or planet. Biodiversity is receiving an ever-increasing attention at many levels of European society as well as from many industrial sectors, and a variety of actions are being put in place in order to protect, preserve and increase it. The present paper provides examples of the capabilities and potentials of the steel sector with respect to biodiversity. In effect, steel is a valuable and fundamental structural material in order to develop measures and systems for protection of biodiversity. On the other hand, biodiversity can represent for the steel industry not only a heritage to preserve, but, through its functional traits, it can become an opportunity, offering an ecosystem's perspective to all industrial companies. In the paper, steel relevant topics and applications are analyzed leading to the conclusion that biodiversity should be exploited and can play a role with potentially relevant benefits both for the company and for local communities. Sustainability and Ecodesign of processes, products and services

  14. Modernized Techniques for Dealing with Quality Data and Derived Products

    NASA Astrophysics Data System (ADS)

    Neiswender, C.; Miller, S. P.; Clark, D.

    2008-12-01

    "I just want a picture of the ocean floor in this area" is expressed all too often by researchers, educators, and students in the marine geosciences. As more sophisticated systems are developed to handle data collection and processing, the demand for quality data, and standardized products continues to grow. Data management is an invisible bridge between science and researchers/educators. The SIOExplorer digital library presents more than 50 years of ocean-going research. Prior to publication, all data is checked for quality using standardized criterion developed for each data stream. Despite the evolution of data formats and processing systems, SIOExplorer continues to present derived products in well- established formats. Standardized products are published for each cruise, and include a cruise report, MGD77 merged data, multi-beam flipbook, and underway profiles. Creation of these products is made possible by processing scripts, which continue to change with ever-evolving data formats. We continue to explore the potential of database-enabled creation of standardized products, such as the metadata-rich MGD77 header file. Database-enabled, automated processing produces standards-compliant metadata for each data and derived product. Metadata facilitates discovery and interpretation of published products. This descriptive information is stored both in an ASCII file, and a searchable digital library database. SIOExplorer's underlying technology allows focused search and retrieval of data and products. For example, users can initiate a search of only multi-beam data, which includes data-specific parameters. This customization is made possible with a synthesis of database, XML, and PHP technology. The combination of standardized products and digital library technology puts quality data and derived products in the hands of scientists. Interoperable systems enable distribution these published resources using technology such as web services. By developing modernized

  15. Vision-based surface defect inspection for thick steel plates

    NASA Astrophysics Data System (ADS)

    Yun, Jong Pil; Kim, Dongseob; Kim, KyuHwan; Lee, Sang Jun; Park, Chang Hyun; Kim, Sang Woo

    2017-05-01

    There are several types of steel products, such as wire rods, cold-rolled coils, hot-rolled coils, thick plates, and electrical sheets. Surface stains on cold-rolled coils are considered defects. However, surface stains on thick plates are not considered defects. A conventional optical structure is composed of a camera and lighting module. A defect inspection system that uses a dual lighting structure to distinguish uneven defects and color changes by surface noise is proposed. In addition, an image processing algorithm that can be used to detect defects is presented in this paper. The algorithm consists of a Gabor filter that detects the switching pattern and employs the binarization method to extract the shape of the defect. The optics module and detection algorithm optimized using a simulator were installed at a real plant, and the experimental results conducted on thick steel plate images obtained from the steel production line show the effectiveness of the proposed method.

  16. Molybdenum protective coatings adhesion to steel substrate

    NASA Astrophysics Data System (ADS)

    Blesman, A. I.; Postnikov, D. V.; Polonyankin, D. A.; Teplouhov, A. A.; Tyukin, A. V.; Tkachenko, E. A.

    2017-06-01

    Protection of the critical parts, components and assemblies from corrosion is an urgent engineering problem and many other industries. Protective coatings’ forming on surface of metal products is a promising way of corrosionprevention. The adhesion force is one of the main characteristics of coatings’ durability. The paper presents theoretical and experimental adhesion force assessment for coatings formed by molybdenum magnetron sputtering ontoa steel substrate. Validity and reliability of results obtained by simulation and sclerometry method allow applying the developed model for adhesion force evaluation in binary «steel-coating» systems.

  17. 77 FR 27421 - Certain Steel Nails From the United Arab Emirates: Amended Final Determination of Sales at Less...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-05-10

    ... limited to, nails made of round wire and nails that are cut. Certain steel nails may be of one piece construction or constructed of two or more pieces. Certain steel nails may be produced from any type of steel... following products: Non-collated (i.e., hand-drive or bulk), two-piece steel nails having plastic or steel...

  18. 46 CFR 59.20-1 - Carbon-steel or alloy-steel castings.

    Code of Federal Regulations, 2010 CFR

    2010-10-01

    ... BOILERS, PRESSURE VESSELS AND APPURTENANCES Welding Repairs to Castings § 59.20-1 Carbon-steel or alloy-steel castings. Defects in carbon-steel or alloy-steel castings may be repaired by welding. The repairs...

  19. 46 CFR 59.20-1 - Carbon-steel or alloy-steel castings.

    Code of Federal Regulations, 2011 CFR

    2011-10-01

    ... BOILERS, PRESSURE VESSELS AND APPURTENANCES Welding Repairs to Castings § 59.20-1 Carbon-steel or alloy-steel castings. Defects in carbon-steel or alloy-steel castings may be repaired by welding. The repairs...

  20. 46 CFR 59.20-1 - Carbon-steel or alloy-steel castings.

    Code of Federal Regulations, 2013 CFR

    2013-10-01

    ... BOILERS, PRESSURE VESSELS AND APPURTENANCES Welding Repairs to Castings § 59.20-1 Carbon-steel or alloy-steel castings. Defects in carbon-steel or alloy-steel castings may be repaired by welding. The repairs...

  1. 46 CFR 59.20-1 - Carbon-steel or alloy-steel castings.

    Code of Federal Regulations, 2012 CFR

    2012-10-01

    ... BOILERS, PRESSURE VESSELS AND APPURTENANCES Welding Repairs to Castings § 59.20-1 Carbon-steel or alloy-steel castings. Defects in carbon-steel or alloy-steel castings may be repaired by welding. The repairs...

  2. 46 CFR 59.20-1 - Carbon-steel or alloy-steel castings.

    Code of Federal Regulations, 2014 CFR

    2014-10-01

    ... BOILERS, PRESSURE VESSELS AND APPURTENANCES Welding Repairs to Castings § 59.20-1 Carbon-steel or alloy-steel castings. Defects in carbon-steel or alloy-steel castings may be repaired by welding. The repairs...

  3. Respiratory status of stainless steel and mild steel welders.

    PubMed

    Kalliomäki, P L; Kalliomäki, K; Korhonen, O; Nordman, H; Rahkonen, E; Vaaranen, V

    1982-01-01

    Eighty-three full-time stainless steel and 29 mild steel welders from one shipyard were examined clinically, and their lung function was measured. The stainless steel welders had used both tungsten inert-gas (low-fume concentration) and manual metal-arc (MMA) (high-fume concentration) welding methods. The individual exposure of the welders was estimated based on the time spent doing MMA welding, the amount of retained contaminants in the lungs (magnetopulmography), and urinary chromium excretion. The results suggest that there is a greater prevalence of small airway disease among shipyard mild steel MMA welders than among stainless steel welders. Among the stainless steel welders the impairment of lung function parameters was associated with the MMA welding method. The type of welding, then, is important when the health hazards of welders are studied, and welders cannot be regarded as a single, homogeneous group.

  4. Hybrid Laser-Arc Welding of the High-Strength Shipbuilding Steels: Equipment and Technology

    NASA Astrophysics Data System (ADS)

    Turichin, G.; Kuznetsov, M.; Tsibulskiy, I.; Firsova, A.

    Hybrid laser-arc welding (HLAW) allows getting weld joints with thickness up to 35 mm for one pass, provide good quality formation of joints, minimal thermal deformations, the productivity in 10 times more in comparison with arc welding. In addition, replacement arc welding to the HLAW allows economizing filler materials, shielding gas and consumable electricity more than 4 times. Therefore, HLAW is actually technology for basic engineering branches and especially for shipbuilding. The Institute of Laser and Welding Technologies (ILWT) developed laser and hybrid laser-arc welding technologies for different type of steels and alloys including high-strength shipbuilding steels. Also ILWT produced portal and robotic systems for HLAW process realization. Portal system for hybrid laser-arc welding of panels with dimensions 6x6 m using at the manufacturing of flat curvilinear sections in the shipbuilding is depicted in the article. Results of experimental researches of the hybrid laser-arc welding parameters influence on the formation and mechanical properties of weld joint are described at the publication also. Experimental part was made with using of the portal system.

  5. Characterization of Adipose Tissue Product Quality Using Measurements of Oxygen Consumption Rate.

    PubMed

    Suszynski, Thomas M; Sieber, David A; Mueller, Kathryn; Van Beek, Allen L; Cunningham, Bruce L; Kenkel, Jeffrey M

    2018-03-14

    Fat grafting is a common procedure in plastic surgery but associated with unpredictable graft retention. Adipose tissue (AT) "product" quality is affected by the methods used for harvest, processing and transfer, which vary widely amongst surgeons. Currently, there is no method available to accurately assess the quality of AT. In this study, we present a novel method for the assessment of AT product quality through direct measurements of oxygen consumption rate (OCR). OCR has exhibited potential in predicting outcomes following pancreatic islet transplant. Our study aim was to reapportion existing technology for its use with AT preparations and to confirm that these measurements are feasible. OCR was successfully measured for en bloc and postprocessed AT using a stirred microchamber system. OCR was then normalized to DNA content (OCR/DNA), which represents the AT product quality. Mean (±SE) OCR/DNA values for fresh en bloc and post-processed AT were 149.8 (± 9.1) and 61.1 (± 6.1) nmol/min/mg DNA, respectively. These preliminary data suggest that: (1) OCR and OCR/DNA measurements of AT harvested using conventional protocol are feasible; and (2) standard AT processing results in a decrease in overall AT product quality. OCR measurements of AT using existing technology can be done and enables accurate, real-time, quantitative assessment of the quality of AT product prior to transfer. The availability and further validation of this type of assay could enable optimization of fat grafting protocol by providing a tool for the more detailed study of procedural variables that affect AT product quality.

  6. Stability evaluation of quality parameters for palm oil products at low temperature storage.

    PubMed

    Ramli, Nur Aainaa Syahirah; Mohd Noor, Mohd Azmil; Musa, Hajar; Ghazali, Razmah

    2018-07-01

    Palm oil is one of the major oils and fats produced and traded worldwide. The value of palm oil products is mainly influenced by their quality. According to ISO 17025:2005, accredited laboratories require a quality control procedure with respect to monitoring the validity of tests for determination of quality parameters. This includes the regular use of internal quality control using secondary reference materials. Unfortunately, palm oil reference materials are not currently available. To establish internal quality control samples, the stability of quality parameters needs to be evaluated. In the present study, the stability of quality parameters for palm oil products was examined over 10 months at low temperature storage (6 ± 2 °C). The palm oil products tested included crude palm oil (CPO); refined, bleached and deodorized (RBD) palm oil (RBDPO); RBD palm olein (RBDPOo); and RBD palm stearin (RBDPS). The quality parameters of the oils [i.e. moisture content, free fatty acid content (FFA), iodine value (IV), fatty acids composition (FAC) and slip melting point (SMP)] were determined prior to and throughout the storage period. The moisture, FFA, IV, FAC and SMP for palm oil products changed significantly (P < 0.05), whereas the moisture content for CPO, IV for RBDPO and RBDPOo, stearic acid composition for CPO and linolenic acid composition for CPO, RBDPO, RBDPOo and RBDPS did not (P > 0.05). The stability study indicated that the quality of the palm oil products was stable within the specified limits throughout the storage period at low temperature. The storage conditions preserved the quality of palm oil products throughout the storage period. These findings qualify the use of the palm oil products CPO, RBDPO, RBDPOo and RBDPS as control samples in the validation of test results. © 2017 Society of Chemical Industry. © 2017 Society of Chemical Industry.

  7. Stainless Steel Permeability

    DOE Office of Scientific and Technical Information (OSTI.GOV)

    Buchenauer, Dean A.; Karnesky, Richard A.

    An understanding of the behavior of hydrogen isotopes in materials is critical to predicting tritium transport in structural metals (at high pressure), estimating tritium losses during production (fission environment), and predicting in-vessel inventory for future fusion devices (plasma driven permeation). Current models often assume equilibrium diffusivity and solubility for a class of materials (e.g. stainless steels or aluminum alloys), neglecting trapping effects or, at best, considering a single population of trapping sites. Permeation and trapping studies of the particular castings and forgings enable greater confidence and reduced margins in the models. For FY15, we have continued our investigation of themore » role of ferrite in permeation for steels of interest to GTS, through measurements of the duplex steel 2507. We also initiated an investigation of the permeability in work hardened materials, to follow up on earlier observations of unusual permeability in a particular region of 304L forgings. Samples were prepared and characterized for ferrite content and coated with palladium to prevent oxidation. Issues with the poor reproducibility of measurements at low permeability were overcome, although the techniques in use are tedious. Funding through TPBAR and GTS were secured for a research grade quadrupole mass spectrometer (QMS) and replacement turbo pumps, which should improve the fidelity and throughput of measurements in FY16.« less

  8. Co-extrusion of semi-finished aluminium-steel compounds

    NASA Astrophysics Data System (ADS)

    Thürer, S. E.; Uhe, J.; Golovko, O.; Bonk, C.; Bouguecha, A.; Klose, C.; Behrens, B.-A.; Maier, H. J.

    2017-10-01

    The combination of light metals and steels allows for new lightweight components with wear-resistant functional surfaces. Within the Collaborative Research Centre 1153 novel process chains are developed for the manufacture of such hybrid components. Here, the production process of a hybrid bearing bushing made of the aluminium alloy EN AW-6082 and the case-hardened steel 20MnCr5 is developed. Hybrid semi-finished products are an attractive alternative to conventional ones resulting from massive forming processes where the individual components are joined after the forming process. The actual hybrid semi-finished products were manufactured using a lateral angular co-extrusion (LACE) process. The bearing bushings are subsequently produced by die forging. In the present study, a tool concept for the LACE process is described, which renders the continuous joining of a steel rod with an aluminium tube possible. During the LACE process, the rod is fed into the extrusion die at an angle of approx. 90°. Metallographic analysis of the hybrid profile showed that the mechanical bonding between the different materials begins about 75 mm after the edge of the aluminium sheath. In order to improve the bonding strength, the steel rod is to be preheated during extrusion. Systematic investigations using a dilatometer, considering the maximum possible co-extrusion process parameters, were carried out. The variable parameters for the dilatometer experiments were determined by numerical simulation. In order to form a bond between the materials, the oxide layer needs to be disrupted during the co-extrusion process. In an attempt to better understand this effect, a modified sample geometry with chamfered steel was developed for the dilatometer experiments. The influence of the process parameters on the formation of the intermetallic phase at the interface was analysed by scanning electron microscopy and X-ray diffraction. This article, which was originally published online on 16

  9. Nitrogen-containing superlow-carbon austenitic steel 02Kh25N22AM2

    NASA Astrophysics Data System (ADS)

    Fe'ldgandler, É. G.; Svistunova, T. V.; Savkina, L. Ya.; Lapshina, O. B.

    1996-02-01

    At present the equipment for manufacturing carbamide mineral fertilizers is produced from domestic steel 03Kh17N14M3 having "carbamide quality." Imported equipment also used in the industry is produced from steel of the 25-22-2 (Cr -Ni-Mo) type shipped by various firms, namely, 2RE69 (Sandvik, Sweden), 254SFER (Avesta, Sweden), 2522LCN (VDM, Germany), DM 1.4466 (Germany), and X2CrNiMo 25-22-2 (Dalmine, Italy). The imported steels are used because in some units steel 03Khl7Nl4M3 does not provide the requisite corrosion resistance in an intensified process of carbamide manufacturing. We currently possess domestic high-alloyed steel for producing new and repairing imported equipment operating under the severe conditions of carbamide synthesis. The present paper concerns the structure, mechanical properties, and corrosion resistance of industrially produced steel 02Kh25N22AM2 (ChS-108) and the recommended range of its application.

  10. Mechanical characteristics of welded joints between different stainless steels grades

    NASA Astrophysics Data System (ADS)

    Topolska, S.; Łabanowski, J.

    2017-08-01

    Investigation of mechanical characteristics of welded joints is one of the most important tasks that allow determining their functional properties. Due to the very high, still rising, cost of some stainless steels it is justified, on economic grounds, welding austenitic stainless steel with steels that are corrosion-resistant like duplex ones. According to forecasts the price of corrosion resistant steels stil can increase by 26 ÷ 30%. For technical reasons welded joints require appropriate mechanical properties such as: tensile strength, bending, ductility, toughness, and resistance to aggressive media. Such joints are applied in the construction of chemical tankers, apparatus and chemical plants and power steam stations. Using the proper binder makes possible the welds directly between the elements of austenitic stainless steels and duplex ones. It causes that such joits behave satisfactorily in service in such areas like maritime constructions and steam and chemical plants. These steels have high mechanical properties such as: the yield strength, the tensile strength and the ductility as well as the resistance to general corrosion media. They are resistant to both pitting and stress corrosions. The relatively low cost of production of duplex steels, in comparison with standard austenitic steels, is inter alia, the result of a reduced amount of scarce and expensive Nickel, which is seen as a further advantage of these steels.

  11. A New Method to Produce Ni-Cr Ferroalloy Used for Stainless Steel Production

    NASA Astrophysics Data System (ADS)

    Chen, Pei-Xian; Chu, Shao-Jun; Zhang, Guo-Hua

    2016-08-01

    A new electrosilicothermic method has been proposed in the present paper to produce Ni-Cr ferroalloy, which can be used for the production of 300 series stainless steel. Based on this new process, the Ni-Si ferroalloy is first produced as the intermediate alloy, and then the desiliconization process of Ni-Si ferroalloy melt with chromium concentrate is carried out to generate Ni-Cr ferroalloy. The silicon content in the Ni-Si ferroalloy produced in the submerged arc furnace should be more than 15 mass% (for the propose of reducing dephosphorization), in order to make sure the phosphorus content in the subsequently produced Ni-Cr ferroalloy is less than 0.03 mass%. A high utilization ratio of Si and a high recovery ratio of Cr can be obtained after the desiliconization reaction between Ni-Si ferroalloy and chromium concentrate in the electric arc furnace (EAF)-shaking ladle (SL) process.

  12. Experimental investigation of various surface integrity aspects in hard turning of AISI 4340 alloy steel with coated and uncoated cermet

    NASA Astrophysics Data System (ADS)

    Das, Anshuman; Patel, S. K.; Sateesh Kumar, Ch.; Biswal, B. B.

    2018-03-01

    The newer technological developments are exerting immense pressure on domain of production. These fabrication industries are busy finding solutions to reduce the costs of cutting materials, enhance the machined parts quality and testing different materials, which can be made versatile for cutting materials, which are difficult for machining. High-speed machining has been the domain of paramount importance for mechanical engineering. In this study, the variation of surface integrity parameters of hardened AISI 4340 alloy steel was analyzed. The surface integrity parameters like surface roughness, micro hardness, machined surface morphology and white layer of hardened AISI 4340 alloy steel were compared using coated and uncoated cermet inserts under dry cutting condition. From the results, it was deduced that coated insert outperformed uncoated one in terms of different surface integrity characteristics.

  13. Numerical investigations on the lateral angular co-extrusion of aluminium and steel

    NASA Astrophysics Data System (ADS)

    Behrens, B.-A.; Klose, C.; Chugreev, A.; Thürer, S. E.; Uhe, J.

    2018-05-01

    In order to save weight and costs, different materials can be combined within one component. In the novel process chain being developed within the Collaborative Research Centre (CRC) 1153, joined semi-finished workpieces are used to produce hybrid solid components with locally adapted properties. Different materials are joined in an initial step before the forming process takes place. Hereby, the quality of the joining zone is improved by means of the thermo-mechanical treatment during the forming and machining processes. The lateral angular co-extrusion (LACE) approach is used to produce semi-finished workpieces because it allows for the production of coaxial semi-finished products consisting of aluminium and steel. In the further process chain, these semi-finished products are processed into hybrid bearing bushings with locally adapted properties by die forging. In the scope of this work, numerical investigations of the co-extrusion of aluminium-steel compounds were carried out using finite element (FE) simulation in order to examine the influence of the process parameters on the co-extrusion process. For this purpose, the relevant material properties of the aluminium alloy EN AW-6082 were determined experimentally and subsequently implemented in the numerical model. The obtained numerical model was used to study the impact of different ram speeds, press ratios and billet temperatures on the resulting extrusion forces and the material flow. The numerical results have been validated using force-time curves obtained from experimental extrusion tests carried out on a 2.5 MN laboratory extrusion press.

  14. Research progress on the effect of microwave sterilization on agricultural products quality

    NASA Astrophysics Data System (ADS)

    Zhu, Xiang-hao; Yang, Yu-xia; Duan, Zhen-hua

    2018-02-01

    Different sterilization methods have different effects on the quality of agricultural products, microwave sterilization inhibited or eliminated microorganism by the use of microwave thermal effects and non-thermal. In this paper, the effects of microwave sterilization on the quality of fruits and vegetables, dairy, meat, grain, aquatic products and other agricultural products were introduced, and the possible development trends of microwave sterilization in agricultural products processing application were put forward.

  15. Research on construction technology for orthotropic steel deck pavement of Haihe River Chunyi Bridge

    NASA Astrophysics Data System (ADS)

    Xue, Y. C.; Qian, Z. D.; Zhang, M.

    2017-01-01

    In order to ensure the good service quality of orthotropic steel deck pavement of Haihe River Chunyi Bridge in Tianjin, and to reduce the occurrence of pavement diseases like lateral and longitudinal cracks, the key working procedures such as steel deck cleaning, anticorrosive coating, bonding layer spraying, seam cutting, epoxy asphalt concrete’s mixing, transportation, paving and compaction were studied. The study was based on the main features of epoxy asphalt concrete which is the pavement materials of Haihe River Chunyi Bridge, and combined with the basic characteristics and construction conditions of Haihe River Chunyi Bridge. Furthermore, some processing measures like controlling time and temperature, continuous paving with two pavers, lateral feeding, and improving the compaction method were proposed. The project example shows that the processing measures can effectively solve the technical difficulties in the construction of orthotropic steel deck pavement of Haihe River Chunyi Bridge, can greatly improve the construction speed and quality, and can provide reference for the same kinds of orthotropic steel deck pavement construction.

  16. Respiratory health effects of long-term exposure to different chromium species in stainless steel production.

    PubMed

    Huvinen, M; Uitti, J; Oksa, P; Palmroos, P; Laippala, P

    2002-06-01

    The aim of this study was to determine whether occupational exposure to chromite, trivalent chromium (Cr(3+)) or hexavalent chromium (Cr(6+)) causes respiratory diseases, an excess of respiratory symptoms, a decrease in pulmonary function or signs of pneumoconiosis among workers in stainless steel production. Altogether, 203 exposed workers and 81 referents with an average employment of 23 years were investigated for indicators of respiratory health on two occasions, in 1993 and in 1998. Data collection with a self-administered questionnaire, flow volume spirometry, measurement of diffusing capacity, chest radiography and laboratory tests were carried out by a mobile research unit. Exposure to different chromium species and other metals was monitored regularly and studied separately. No adverse respiratory health effects were observed in the group exposed to Cr(6+), either in comparison with the control group in the first cross-sectional study or during the additional 5 year follow-up. Among the Cr (3+) exposed people, the production of phlegm, shortness of breath and breathlessness on exertion were significantly more frequent than in the control group, but the frequency of the symptoms did not increase during the follow-up; no differences were observed in the lung function tests and the radiographic findings did not progress. In the chromite group, the prevalence of breathlessness on exertion was higher than in the control group. However, in the follow-up, the occurrence of symptoms did not differ from 1993 to 1998. In the first study, most parameters of lung function were lower among the smokers in the chromite group than among the smoking controls, but in 1998 the difference was less marked. An average exposure time of 23 years in modern ferrochromium and stainless steel production and low exposure to dusts and fumes containing Cr(6+), Cr(3+), nickel and molybdenum do not lead to respiratory changes detectable by lung function tests or radiography. The workers

  17. 77 FR 32552 - Circular Welded Carbon-Quality Steel Pipe From the Socialist Republic of Vietnam: Preliminary...

    Federal Register 2010, 2011, 2012, 2013, 2014

    2012-06-01

    ... obtain separate-rate status in non-market economy (NME) investigations such as this investigation.\\3\\ \\2... Welded Non-Alloy Steel Pipe from Brazil, Mexico, the Republic of Korea, and Taiwan; and Certain Circular... Steel Pipe from the People's Republic of China, 73 FR 31970 (June 5, 2008), and accompanying Issues and...

  18. EAST ELEVATION, LTV STEEL (FORMERLY REPUBLIC STEEL), 8" BAR MILL, ...

    Library of Congress Historic Buildings Survey, Historic Engineering Record, Historic Landscapes Survey

    EAST ELEVATION, LTV STEEL (FORMERLY REPUBLIC STEEL), 8" BAR MILL, BUFFALO PLANT. VIEW LOOKING SOUTHWEST FROM ROLL SHOP. 8" BAR MILL DESIGNED AND BUILT BY DONNER STEEL CO. (PREDECESSOR OF REPUBLIC), 1919-1920. FOR DESCRIPTION OF ORIGINAL MILL SEE "IRON AGE", 116\\4 (23 JULY 1925): 201-204. - LTV Steel, 8-inch Bar Mill, Buffalo Plant, Buffalo, Erie County, NY

  19. Influence of cutting data on surface quality when machining 17-4 PH stainless steel

    NASA Astrophysics Data System (ADS)

    Popovici, T. D.; Dijmărescu, M. R.

    2017-08-01

    The aim of the research presented in this paper is to analyse the cutting data influence upon surface quality for 17-4 PH stainless steel milling machining. The cutting regime parameters considered for the experiments were established using cutting regimes from experimental researches or from industrial conditions as basis, within the recommended ranges. The experimental program structure was determined by taking into account compatibility and orthogonality conditions, minimal use of material and labour. The machined surface roughness was determined by measuring the Ra roughness parameter, followed by surface profile registration in the form of graphics which were saved on a computer with MarSurf PS1Explorer software. Based on Ra roughness parameter, maximum values were extracted from these graphics and the influence charts of the cutting regime parameters upon surface roughness were traced using Microsoft Excel software. After a thorough analysis of the resulting data, relevant conclusions were drawn, presenting the interdependence between the surface roughness of the machined 17-4 PH samples and the cutting data variation.

  20. Connections: Superplasticity, Damascus Steels, Laminated Steels, and Carbon Dating

    NASA Astrophysics Data System (ADS)

    Wadsworth, Jeffrey

    2016-12-01

    In this paper, a description is given of the connections that evolved from the initial development of a family of superplastic plain carbon steels that came to be known as Ultra-High Carbon Steels (UHCS). It was observed that their very high carbon contents were similar, if not identical, to those of Damascus steels. There followed a series of attempts to rediscover how the famous patterns found on Damascus steels blades were formed. At the same time, in order to improve the toughness at room temperature of the newly-developed UHCS, laminated composites were made of alternating layers of UHCS and mild steel (and subsequently other steels and other metals). This led to a study of ancient laminated composites, the motives for their manufacture, and the plausibility of some of the claims relating to the number of layers in the final blades. One apparently ancient laminated composite, recovered in 1837 from the great pyramid of Giza which was constructed in about 2750 B.C., stimulated a carbon dating study of ancient steels. The modern interest in "Bladesmithing" has connections back to many of these ancient weapons.

  1. Design of agricultural product quality safety retrospective supervision system of Jiangsu province

    NASA Astrophysics Data System (ADS)

    Wang, Kun

    2017-08-01

    In store and supermarkets to consumers can trace back agricultural products through the electronic province card to query their origin, planting, processing, packaging, testing and other important information and found that the problems. Quality and safety issues can identify the responsibility of the problem. This paper designs a retroactive supervision system for the quality and safety of agricultural products in Jiangsu Province. Based on the analysis of agricultural production and business process, the goal of Jiangsu agricultural product quality safety traceability system construction is established, and the specific functional requirements and non-functioning requirements of the retroactive system are analyzed, and the target is specified for the specific construction of the retroactive system. The design of the quality and safety traceability system in Jiangsu province contains the design of the overall design, the trace code design and the system function module.

  2. Glycoengineering of CHO Cells to Improve Product Quality.

    PubMed

    Wang, Qiong; Yin, Bojiao; Chung, Cheng-Yu; Betenbaugh, Michael J

    2017-01-01

    Chinese hamster ovary (CHO) cells represent the predominant platform in biopharmaceutical industry for the production of recombinant biotherapeutic proteins, especially glycoproteins. These glycoproteins include oligosaccharide or glycan attachments that represent one of the principal components dictating product quality. Especially important are the N-glycan attachments present on many recombinant glycoproteins of commercial interest. Furthermore, altering the glycan composition can be used to modulate the production quality of a recombinant biotherapeutic from CHO and other mammalian hosts. This review first describes the glycosylation network in mammalian cells and compares the glycosylation patterns between CHO and human cells. Next genetic strategies used in CHO cells to modulate the sialylation patterns through overexpression of sialyltransfereases and other glycosyltransferases are summarized. In addition, other approaches to alter sialylation including manipulation of sialic acid biosynthetic pathways and inhibition of sialidases are described. Finally, this review also covers other strategies such as the glycosylation site insertion and manipulation of glycan heterogeneity to produce desired glycoforms for diverse biotechnology applications.

  3. Effect of production phase on bottle-fermented sparkling wine quality.

    PubMed

    Kemp, Belinda; Alexandre, Hervé; Robillard, Bertrand; Marchal, Richard

    2015-01-14

    This review analyzes bottle-fermented sparkling wine research at each stage of production by evaluating existing knowledge to identify areas that require future investigation. With the growing importance of enological investigation being focused on the needs of the wine production industry, this review examines current research at each stage of bottle-fermented sparkling wine production. Production phases analyzed in this review include pressing, juice adjustments, malolactic fermentation (MLF), stabilization, clarification, tirage, lees aging, disgorging, and dosage. The aim of this review is to identify enological factors that affect bottle-fermented sparkling wine quality, predominantly aroma, flavor, and foaming quality. Future research topics identified include regional specific varieties, plant-based products from vines, grapes, and yeast that can be used in sparkling wine production, gushing at disgorging, and methods to increase the rate of yeast autolysis. An internationally accepted sensory analysis method specifically designed for sparkling wine is required.

  4. Automated X-ray quality control of catalytic converters

    NASA Astrophysics Data System (ADS)

    Shashishekhar, N.; Veselitza, D.

    2017-02-01

    Catalytic converters are devices attached to the exhaust system of automobile or other engines to eliminate or substantially reduce polluting emissions. They consist of coated substrates enclosed in a stainless steel housing. The substrate is typically made of ceramic honeycombs; however stainless steel foil honeycombs are also used. The coating is usually a slurry of alumina, silica, rare earth oxides and platinum group metals. The slurry also known as the wash coat is applied to the substrate in two doses, one on each end of the substrate; in some cases multiple layers of coating are applied. X-ray imaging is used to inspect the applied coating depth on a substrate to confirm compliance with quality requirements. Automated image analysis techniques are employed to measure the coating depth from the X-ray image. Coating depth is assessed by analysis of attenuation line profiles in the image. Edge detection algorithms with noise reduction and outlier rejection are used to calculate the coating depth at a specified point along an attenuation line profile. Quality control of the product is accomplished using several attenuation line profile regions for coating depth measurements, with individual pass or fail criteria specified for each region.

  5. Flexible optical metrology strategies for the control and quality assurance of small series production

    NASA Astrophysics Data System (ADS)

    Schmitt, R.; Pavim, A.

    2009-06-01

    The demand for achieving smaller and more flexible production series with a considerable diversity of products complicates the control of the manufacturing tasks, leading to big challenges for the quality assurance systems. The quality assurance strategy that is nowadays used for mass production is unable to cope with the inspection flexibility needed among automated small series production, because the measuring strategy is totally dependent on the fixed features of the few manufactured object variants and on process parameters that can be controlled/compensated during production time. The major challenge faced by a quality assurance system applied to small series production facilities is to guarantee the needed quality level already at the first run, and therefore, the quality assurance system has to adapt itself constantly to the new manufacturing conditions. The small series production culture requires a change of paradigms, because its strategies are totally different from mass production. This work discusses the tight inspection requirements of small series production and presents flexible metrology strategies based on optical sensor data fusion techniques, agent-based systems as well as cognitive and self-optimised systems for assuring the needed quality level of flexible small series. Examples of application scenarios are provided among the automated assembly of solid state lasers and the flexible inspection of automotive headlights.

  6. Design, Development and Application of New, High-Performance Gear Steels

    DTIC Science & Technology

    2010-02-01

    thesis work focused on design principles for advanced carburized bearing steels . He also received a Master of Product Development degree from...Design computational design technology to develop a new class of high-strength, secondary hardening gear steels that are optimized for high-temperature...high contact fatigue resistance, which makes it a candidate for applications such as camshafts and bearings , as well as gear sets. (Printed with

  7. Effect of Slag-Steel Reaction on the Initial Solidification of Molten Steel during Continuous Casting

    NASA Astrophysics Data System (ADS)

    Wang, Wanlin; Lou, Zhican; Zhang, Haihui

    2018-03-01

    With the mold simulator technique, the effect of slag-steel reaction on the initial shell solidification as well as the heat transfer and lubrication behavior of the infiltrated mold/shell slag film was studied in this article. The results showed that the Al2O3 content, the CaO/SiO2 ratio, and the viscosity of mold flux were increased with the progress of the slag-steel reaction during casting. The slag-steel reaction has two major effects on the initial shell solidification: one is increasing the mold heat flux and shell thickness by the decrease of slag film thickness. The other is the reduction of mold heat flux by the increase of crystal fraction in slag film. Mold flux with a lower basicity, viscosity, and crystallization temperature would result in a larger liquid slag consumption and the uneven infiltration of slag into the mold and shell gap that eventually leads to the irregular solidification of initial shell with a poor surface quality, such as slag entrapment and depressions as well as glaciation marks. Conversely, mold flux with a higher viscosity, basicity, and crystallization temperature would result in a smaller liquid slag consumption, which would cause the poor mold lubrication, the longitudinal shell surface defects, and drag marks.

  8. Effect of Slag-Steel Reaction on the Initial Solidification of Molten Steel during Continuous Casting

    NASA Astrophysics Data System (ADS)

    Wang, Wanlin; Lou, Zhican; Zhang, Haihui

    2018-06-01

    With the mold simulator technique, the effect of slag-steel reaction on the initial shell solidification as well as the heat transfer and lubrication behavior of the infiltrated mold/shell slag film was studied in this article. The results showed that the Al2O3 content, the CaO/SiO2 ratio, and the viscosity of mold flux were increased with the progress of the slag-steel reaction during casting. The slag-steel reaction has two major effects on the initial shell solidification: one is increasing the mold heat flux and shell thickness by the decrease of slag film thickness. The other is the reduction of mold heat flux by the increase of crystal fraction in slag film. Mold flux with a lower basicity, viscosity, and crystallization temperature would result in a larger liquid slag consumption and the uneven infiltration of slag into the mold and shell gap that eventually leads to the irregular solidification of initial shell with a poor surface quality, such as slag entrapment and depressions as well as glaciation marks. Conversely, mold flux with a higher viscosity, basicity, and crystallization temperature would result in a smaller liquid slag consumption, which would cause the poor mold lubrication, the longitudinal shell surface defects, and drag marks.

  9. [The industrial environment in the electric-furnace steel smelting, converter and open-hearth furnace methods of manufacturing manganese-alloyed steels].

    PubMed

    Karnaukh, N G; Petrov, G A; Gapon, V A; Poslednichenko, I P; Shmidt, S E

    1992-01-01

    Inspection of the environment in manganese-alloyed steel production showed inadequate hygienic conditions of the technological processes employed. Air was more polluted by manganese oxides during the oxygen-converter process though their highest concentrations, 38 times exceeding the MAS, appeared during the casting of steel. An electric furnace coated by dust-noise-proof material and gas cleaning is preferable from a hygienic point of view. The influence of unfavourable microclimate, intensive infrared irradiation and loud noise on workers necessitates automation and mechanization of the process in order to improve the working conditions.

  10. The Effect of Niobium Microalloying on Processing and Application Properties of Dual Phase Steel

    NASA Astrophysics Data System (ADS)

    Mohrbacher, Hardy

    Dual phase steel is widely used in today's car body manufacturing. Its characteristics of high n-value and good elongation (A80) are the basis of good press formability. However, practical experience has shown unexpected failure in forming operations where tight bending, stretch flanging or hole expansion are predominant. The inhomogeneous microstructure of soft ferrite and hard martensite in combination with highly localized straining is the origin of these problems. Furthermore, weldability and delayed cracking have been experienced to cause problems in ultra-high strength DP steel. Refinement and homogenization of the two-phase microstructure as well as lowering of the carbon content have been identified as remedies to the mentioned problems. However, mill processing of DP steel with reduced carbon content is more difficult especially for the higher strength levels. Niobium microalloying proved to be very effective in increasing the processing window of low-carbon DP steels besides of its natural effect of refining the microstructure. Meanwhile the production of niobium microalloyed DP steel has been established in several markets including China. The paper details the fundamentals, demonstrates respective production concepts and presents examples of application of Nb-microalloyed DP steels.

  11. Building quality into medical product software design.

    PubMed

    Mallory, S R

    1993-01-01

    The software engineering and quality assurance disciplines are a requisite to the design of safe and effective software-based medical devices. It is in the areas of software methodology and process that the most beneficial application of these disciplines to software development can be made. Software is a product of complex operations and methodologies and is not amenable to the traditional electromechanical quality assurance processes. Software quality must be built in by the developers, with the software verification and validation engineers acting as the independent instruments for ensuring compliance with performance objectives and with development and maintenance standards. The implementation of a software quality assurance program is a complex process involving management support, organizational changes, and new skill sets, but the benefits are profound. Its rewards provide safe, reliable, cost-effective, maintainable, and manageable software, which may significantly speed the regulatory review process and therefore potentially shorten the overall time to market. The use of a trial project can greatly facilitate the learning process associated with the first-time application of a software quality assurance program.

  12. Research on Ultrasonic Flaw Detection of Steel Weld in Spatial Grid Structure

    NASA Astrophysics Data System (ADS)

    Du, Tao; Sun, Jiandong; Fu, Shengguang; Zhang, Changquan; Gao, Qing

    2017-06-01

    The welding quality of spatial grid member is an important link in quality control of steel structure. The paper analyzed the reasons that the welding seam of small-bore pipe with thin wall grid structure is difficult to be detected by ultrasonic wave from the theoretical and practical aspects. A series of feasible detection methods was also proposed by improving probe and operation approaches in this paper, and the detection methods were verified by project cases. Over the years, the spatial grid structure is widely used the engineering by virtue of its several outstanding characteristics such as reasonable structure type, standard member, excellent space integrity and quick installation. The wide application of spatial grid structure brings higher requirements on nondestructive test of grid structure. The implementation of new Code for Construction Quality Acceptance of Steel Structure Work GB50205-2001 strengthens the site inspection of steel structure, especially the site inspection of ultrasonic flaw detection in steel weld. The detection for spatial grid member structured by small-bore and thin-walled pipes is difficult due to the irregular influence of sound pressure in near-field region of sound field, sound beam diffusion generated by small bore pipe and reduction of sensitivity. Therefore, it is quite significant to select correct detecting conditions. The spatial grid structure of welding ball and bolt ball is statically determinate structure with high-order axial force which is connected by member bars and joints. It is welded by shrouding or conehead of member bars and of member bar and bolt-node sphere. It is obvious that to ensure the quality of these welding positions is critical to the quality of overall grid structure. However, the complexity of weld structure and limitation of ultrasonic detection method cause many difficulties in detection. No satisfactory results will be obtained by the conventional detection technology, so some special

  13. Stainless steel welding and semen quality.

    PubMed

    Jelnes, J E; Knudsen, L E

    1988-01-01

    Questionnaire studies of patients from fertility clinics suggest that welders may have an increased risk of reduced semen quality. In this study, welders and nonwelders from the same plants were asked to provide blood, urine, and semen samples. Urine was analyzed for chromium and nickel, and for mutagenic activity and metal concentration; blood for metal concentrations, immunoglobulin G, total protein, and measures of genotoxicity in lymphocytes; and semen was evaluated by standard semen analysis. Results of the semen evaluation, presented here, showed no difference in semen quality between welders and nonwelders. Because the metal dust exposure of nonwelders in the plant may be higher than that in the general population, welders were also compared to referents not working in the metal industry. Again, no decrease in semen quality associated with welding was demonstrated.

  14. A real time quality control application for animal production by image processing.

    PubMed

    Sungur, Cemil; Özkan, Halil

    2015-11-01

    Standards of hygiene and health are of major importance in food production, and quality control has become obligatory in this field. Thanks to rapidly developing technologies, it is now possible for automatic and safe quality control of food production. For this purpose, image-processing-based quality control systems used in industrial applications are being employed to analyze the quality of food products. In this study, quality control of chicken (Gallus domesticus) eggs was achieved using a real time image-processing technique. In order to execute the quality control processes, a conveying mechanism was used. Eggs passing on a conveyor belt were continuously photographed in real time by cameras located above the belt. The images obtained were processed by various methods and techniques. Using digital instrumentation, the volume of the eggs was measured, broken/cracked eggs were separated and dirty eggs were determined. In accordance with international standards for classifying the quality of eggs, the class of separated eggs was determined through a fuzzy implication model. According to tests carried out on thousands of eggs, a quality control process with an accuracy of 98% was possible. © 2014 Society of Chemical Industry.

  15. Microbiological quality and safety assessment of lettuce production in Brazil.

    PubMed

    Ceuppens, Siele; Hessel, Claudia Titze; de Quadros Rodrigues, Rochele; Bartz, Sabrina; Tondo, Eduardo César; Uyttendaele, Mieke

    2014-07-02

    The microbiological quality and safety of lettuce during primary production in Brazil were determined by enumeration of hygiene indicators Escherichia coli, coliforms and enterococci and detection of enteric pathogens Salmonella and E. coli O157:H7 in organic fertilizers, soil, irrigation water, lettuce crops, harvest boxes and worker's hands taken from six different lettuce farms throughout the crop growth cycle. Generic E. coli was a suitable indicator for the presence of Salmonella and E. coli O157:H7, while coliforms and enterococci were not. Few pathogens were detected: 5 salmonellae and 2 E. coli O157:H7 from 260 samples, of which only one was lettuce and the others were manure, soil and water. Most (5/7) pathogens were isolated from the same farm and all were from organic production. Statistical analysis revealed the following environmental and agro-technical risk factors for increased microbial load and pathogen prevalence in lettuce production: high temperature, flooding of lettuce fields, application of contaminated organic fertilizer, irrigation with water of inferior quality and large distances between the field and toilets. Control of the composting process of organic fertilizers and the irrigation water quality appear most crucial to improve and/or maintain the microbiological quality and safety during the primary production of lettuce. Copyright © 2014 Elsevier B.V. All rights reserved.

  16. Liposomal Drug Product Development and Quality: Current US Experience and Perspective.

    PubMed

    Kapoor, Mamta; Lee, Sau L; Tyner, Katherine M

    2017-05-01

    Research in the area of liposomes has grown substantially in the past few decades. Liposomes are lipid bilayer structures that can incorporate drug substances to modify the drug's pharmacokinetic profile thereby improving drug delivery. The agency has received over 400 liposomal drug product submissions (excluding combination therapies), and there are currently eight approved liposomal drug products on the US market. In order to identify the pain points in development and manufacturing of liposomal drug products, a retrospective analysis was performed from a quality perspective on submissions for new and generic liposomal drug products. General analysis on liposomal drug product submissions was also performed. Results indicated that 96% of the submissions were Investigational New Drug (IND) applications, 3% were New Drug Applications (NDAs), and the remaining 1% was Abbreviated New Drug Applications (ANDAs). Doxorubicin hydrochloride was the most commonly used drug substance incorporated into the liposomes (31%). The majority of the liposomal products were administered via intravenous route (84%) with cancer (various types) being the most common indication (63%). From a quality perspective, major challenges during the development of liposomal drug products included identification and (appropriate) characterization of critical quality attributes of liposomal drug products and suitable control strategies during product development. By focusing on these areas, a faster and more efficient development of liposomal drug products may be achieved. Additionally, in this way, the drug review process for such products can be streamlined.

  17. Engineering Post-Graduate Programmes: A Quality and Productivity Analysis

    ERIC Educational Resources Information Center

    Soares de Mello, Joao Carlos C. B.; Gomes, Eliane Goncalves; Meza, Lidia Angulo; Soares de Mello, Maria Helena C.; Soares de Mello, Adelino Jose R.

    2006-01-01

    Post-graduate courses are periodically evaluated in accordance with not always very clear criteria by CAPES (Co-ordinating Committee for Teaching Staff Improvement). These criteria try to measure, among other things, academic productivity (including quantity and quality of scientific production), number of classes given by teachers, time to…

  18. The legal framework governing the quality of (traditional) herbal medicinal products in the European Union.

    PubMed

    Kroes, Burt H

    2014-12-02

    In the European Union a complex regulatory framework is in place for the regulation of (traditional) herbal medicinal products. It is based on the principle that a marketing authorisation granted by the competent authorities is required for placing medicinal products on the market. The requirements and procedures for acquiring such a marketing authorisation are laid down in regulations, directives and scientific guidelines. This paper gives an overview of the quality requirements for (traditional) herbal medicinal products that are contained in European pharmaceutical legislation. Pharmaceutical quality of medicinal product is the basis for ensuring safe and effective medicines. The basic principles governing the assurance of the quality of medicinal products in the European Union are primarily defined in the amended Directive 2001/83/EC and Directive 2003/63/EC. Quality requirements of herbal medicinal products are also laid down in scientific guidelines. Scientific guidelines provide a basis for practical harmonisation of how the competent authorities of EU Member States interpret and apply the detailed requirements for the demonstration of quality laid down in regulations and directives. Detailed quality requirements for herbal medicinal products on the European market are contained in European Union (EU) pharmaceutical legislation. They include a system of manufacturing authorisations which ensures that all herbal medicinal products on the European market are manufactured/imported only by authorised manufacturers, whose activities are regularly inspected by the competent authorities. Additionally, as starting materials only active substances are allowed which have been manufactured in accordance with the GMP for starting materials as adopted by the Community. The European regulatory framework encompasses specific requirements for herbal medicinal products. These requirements are independent from the legal status. Thus, the same quality standards equally apply

  19. Bond characteristics of steel fiber and deformed reinforcing steel bar embedded in steel fiber reinforced self-compacting concrete (SFRSCC)

    NASA Astrophysics Data System (ADS)

    Aslani, Farhad; Nejadi, Shami

    2012-09-01

    Steel fiber reinforced self-compacting concrete (SFRSCC) is a relatively new composite material which congregates the benefits of the self-compacting concrete (SCC) technology with the profits derived from the fiber addition to a brittle cementitious matrix. Steel fibers improve many of the properties of SCC elements including tensile strength, ductility, toughness, energy absorption capacity, fracture toughness and cracking. Although the available research regarding the influence of steel fibers on the properties of SFRSCC is limited, this paper investigates the bond characteristics between steel fiber and SCC firstly. Based on the available experimental results, the current analytical steel fiber pullout model (Dubey 1999) is modified by considering the different SCC properties and different fiber types (smooth, hooked) and inclination. In order to take into account the effect of fiber inclination in the pullout model, apparent shear strengths ( τ ( app)) and slip coefficient ( β) are incorporated to express the variation of pullout peak load and the augmentation of peak slip as the inclined angle increases. These variables are expressed as functions of the inclined angle ( ϕ). Furthurmore, steel-concrete composite floors, reinforced concrete floors supported by columns or walls and floors on an elastic foundations belong to the category of structural elements in which the conventional steel reinforcement can be partially replaced by the use of steel fibers. When discussing deformation capacity of structural elements or civil engineering structures manufactured using SFRSCC, one must be able to describe thoroughly both the behavior of the concrete matrix reinforced with steel fibers and the interaction between this composite matrix and discrete steel reinforcement of the conventional type. However, even though the knowledge on bond behavior is essential for evaluating the overall behavior of structural components containing reinforcement and steel fibers

  20. Pillars of Power: Silver and Steel of the Ottoman Empire.

    NASA Astrophysics Data System (ADS)

    Nerantzis, N.

    The Ottoman Empire was forged over disintegrating Byzantium, stretching across Anatolia and the Balkans and ruled for almost five centuries. One crucial parameter that allowed for its quick expansion has been a combination of economic wealth and superiority of armed forces. The Ottomans succeeded in both sectors by promoting innovative technology in the field of silver and steel production for supplying their monetary system and weapons industry. Rich mines and smelting workshops provided increased output in metals, allowing for quick expansion and economic growth. Some of the major centres for silver and steel production are being discussed in this paper in conjunction with analytical data from smelting residues.