diene monomer ( EPDM ) rubber under high-rate uniaxial compression using an SHPB (5). Additionally, Song and Chen used a strain energy-based function to...describe a one-dimensional constitutive relation to describe the high strain rate behavior of the EPDM rubber , which agreed with the experimental...intermediate rate to about 6 MPa at 500 s -1 . This behavior and rate dependence was similar to the EPDM rubber studied by Chen and Zhang (2), which
Wettability of naturally aged silicone and EPDM composite insulators
DOE Office of Scientific and Technical Information (OSTI.GOV)
Gubanski, S.M.; Vlastos, A.E.
1990-07-01
This paper reports the wettability of aged surfaces and of the bulk of naturally aged silicone and EPDM insulator housings and of silicone elastomer insulator coatings studied. The samples were taken either directly from the insulators or treated by exposing them to corona discharges and/or to saline pollution. The results show that the contact angles of the silicone rubber insulator surfaces are larger than the contact angles of the RTV silicone rubber coating and of the EPDM rubber insulator surfaces, especially when the surfaces are aged. When the insulators were exposed to corona discharges, the contact angles of the siliconemore » rubber insulators are reduced but after the exposure they recover with time. The contact angles of the EPDM rubber insulators, however, after the exposure, continue to reduce. When exposed to artificial saline pollution, the silicone rubber insulators show a limited recovery of their contact angles with time, while, when exposed to corona discharge, they show a recovery of the contact angle after the exposure. The time for recovery is dependent on the exposure time to the corona discharges.« less
1992-08-01
Cleaning Aged EPDM Rubber Roofing Membrane Material for Patching: Laboratory Investigations and Recommendations Walter J. Rossiter, Jr. T N n-’T ic...condition of the aged EPDM rubber before bonding. This study assessed the effectiveness of different cleaning methods for preparing aged EPDM membranes for...REPORT DATE 3. REPORT TYPE AND DATES COVERED August 1992 Final 4. TITLE AND SUBTITLE 5. FUNDING NUMBERS Cleaning Aged EPDM Rubber Roofing Membrane
Chlorinated rubbers with advanced properties for tire industry
NASA Astrophysics Data System (ADS)
Mikhaylov, I. A.; Sukhareva, K. V.; Andriasyan, Yu. O.; Popov, A. A.
2017-12-01
The paper investigates the production and processing of halide-modified chlorinated rubbers, such as isobutylene isoprene rubber and ethylene-propylene-diene-monomer rubber (IIR and EPDM), which are perspective in terms of application in rubber industry. Prospects for their production and application are determined by the specific properties of these rubbers (low gas permeability of IIR, high heat and ozone resistance of EPDM). These properties are governed by the structure of both initial IIR and EPDM and chlorinated rubbers (ChIIR and ChEPDM). A new alternative technology of obtaining chlorinated elastomers based on solid-phase mechanochemical halide modification is proposed. Novel chlorinated polyolefin rubbers obtained by the developed technology show good technological properties under industrial production conditions due to enhanced covulcanization.
The Shock and Vibration Digest. Volume 14, Number 10
1982-10-01
temperatures. An equation for predicting the temper- ature sensitivity of the elastic modulus is presented. Some dynamic data on EPDM rubbers have been...presented [23, 24]. The effects of oil type, carbon black level, and a cure system for an EPDM rubber were studied (23); six commercial EPDM rubbers ...Behavior of EPDM Rubbers ," J. Appl. Poly. Sei., 23 (6), p 1607 (Mar 15,1979). 25. Darlow, M.S., Smalley, A.J., and Cunningham, R.E., "Dynamic Properties
1987-03-01
Reinforced Black EPDM Rubber Sheets for Use in Roofing Applications ( Rubber Manufacturers Association [RMAJ, 1984). Minimum Requirements for Fabric-Reinforced...Black Polychloroprene Rubber Sheets for Use in Roofing Applications (RMA, 1984). Minimum Requirements for Non-Reinforced Black EPDM Rubber Sheets for...and materials. The Rubber Manufacturers Amoeiation (RMA) (USA) RMA is funding a study in conjunction with ASTM to evaluate three different EPDM
Surface improvement of EPDM rubber by plasma treatment
NASA Astrophysics Data System (ADS)
Moraes, J. H.; da Silva Sobrinho, A. S.; Maciel, H. S.; Dutra, J. C. N.; Massi, M.; Mello, S. A. C.; Schreiner, W. H.
2007-12-01
The surface of ethylene-propylene-diene monomer (EPDM) rubber was treated in N2/Ar and N2/H2/Ar RF plasmas in order to achieve similar or better adhesion properties than NBR (acrylonitrile-butadiene) rubber, nowadays used as thermal protection of rocket chambers. The surface properties were studied by contact angle measurements and by x-ray photoelectron spectroscopy (XPS). The treated surfaces of the EPDM samples show a significant reduction in the contact angle measurement, indicating an increase in the surface energy. XPS analyses show the incorporation of polar nitrogen- and oxygen-containing groups on the rubber surface. After plasma treatment the presence of oxygen is observed due to surface oxidation which occurs when the samples are exposed to the air. Atomic force microscopy and scanning electron microscopy analyses indicate a decrease in the EPDM rubber surface roughness, promoted by surface etching during the plasma treatment. Strength tests indicate improvement of about 30% and 110% in the adhesion strength for the plasma treated EPDM/polyurethane liner interface and for the EPDM/epoxy adhesive interface, respectively. The adhesion strength of the EPDM/liner is similar to that obtained for the NBR/liner, which indicates that EPDM rubber can safely be used as thermal protection of the solid propellant rocket chamber.
Ethylene-Propylene Terpolymer Rubber Processing by Electron Beam Irradiation
NASA Astrophysics Data System (ADS)
Manaila, Elena N.; Zuga, Maria Daniela T.; Martin, Diana I.; Craciun, Gabriela D.; Ighigeanu, Daniel I.; Matei, Constantin I.
2007-04-01
The investigations on the cross-linking by accelerated electrons of 6.23 MeV in lowly unsaturated elastomers of EPDM (ethylene-propylene terpolymer rubber) type are presented. Two rubber blends based EPDM were prepared and irradiated at different doses up to 250kGy: blend A - based on EPDM maleinized with polyethylene, zinc oxide, plasticizers, filler, and blend B - based on EPDM / PE (50 % EPDM and 50% polyethylene). Blends were prepared on a laboratory electrically heated rubber mill at temperatures of 150-160°C to enable the polyethylene (PE) melting to be reached. Plates of 150 × 150 × 2 mm were obtained in a laboratory electrical press at 170°C.
Landfill Liners and Covers: Properties and Application to Army Landfills.
1984-06-01
polymers, TPE can be seamed by heat techniques. Materials such as thermoplastic EPDM and nitrile rubber /PVC blends are still being tested to determine their...such as polyethylene (PE), polyvinyl chloride (PVC), butyl rubber , ethylene propylene diene monomer ( EPDM ), chlorinated polyethylene (CPE), and others...chlorosulfonated polyethy- lene (CSPE), chlorinated polyethylene (CPE), butyl rubber , ethylene propylene S rubber ( EPDM ), neoprene, high-density polyethylene
Reusable Material for Drop Tower
2011-08-01
R3 Buna-N Rubber ............................................................................................... 32 B-3. R5 EPDM Rubber ...Butyl Rubber . Figure B-2. R3 Buna-N Rubber . Figure B-3. R5 EPDM Rubber . Figure B-4. R6 Gel Rubber . UNCLASSIFIED 33...11 Current Drop Tower Material & Setup .......................................................... 11 Bowling Ball Rubber Material Sample Test
Construction of Experimental Roofing.
1981-11-01
buildings at Fort Benning, GA; Fort Knox, KY; and Fort Lewis, WA. Sheets of EPDM synthetic rubber were installed on buildings at Forts Benning and Lewis...Contract and Unit Costs 14 5 Polyurethane Foam Roofing -- Initial Physical Properties 28 6 EPDM Sheet Rubber Roofing -- Initial Physical Properties 30 7...the new system. The system selected for Area A was an EPDM synthetic rubber manufactured by Carlisle Tire and Rubber Company. The contract specified
Ultra-Low Permeability Polymeric Encapsulants for Acoustic Applications
2006-05-10
polyurethane, tend to exhibit greater water permeability than those that are vulcanizates, such as butyl rubber, EPDM (ethylene propylene diene monomer) rubber...water permeation is a critical concern, hydrophobic, non-polar polymers such as EPDM and butyl rubber are typically used. These materials are vulcanizates...Their non-polar nature makes it difficult to bond anything else strongly to them. Thus, most EPDM and butyl rubber boots are secured to the underlying
Development of a Cavitation Erosion Resistant Advanced Material System
2005-11-01
Sheet EPD M results .............................................................................. 47 Figure 5.11 - EPDM rubber samples, sheet (left...Testing The long test times of EPDM rubber and other durable elastomer samples created a need for overnight testing capability. In the original test setup...seals, adhesives and molded flexible parts. Common examples of elastomers include natural and synthetic rubber , silicone, neoprene, EPDM , polyurethane
Radiation graft modification of EPDM rubber
NASA Astrophysics Data System (ADS)
Katbab, A. A.; Burford, R. P.; Garnett, J. L.
N-Vinyl pyrrolidone (NVP), 2-hydroxyethylmethacrylate (HEMA) and acrylamide (AAm) have been grafted to the surface of rubber vulcanizates based on ethylene-propylene-terpolymer (EPDM) using the simultaneous radiation method to alter surface properties such as wettability and therefore biocompatibility. The effect of monomer concentration, solvent and EPDM structural factors on the grafting behavior have been investigated. The inhibitory effect upon homopolymerization of various salts has also been evaluated for the three monomers. NVP and HEMA could be grafted onto EPDM rubber in the presence of aqueous solutions of cupric nitrate at 0.005 M and 1.0 M concentrations respectively. Aqueous solutions of Mohr's salt (ammonium ferrous sulphate) at 0.05 M not only suppressed the homopolymerization of AAm but also increased grafting yield. The percentage grafting also increased with increasing AAm concentration. A mechanism has been proposed to explain the behaviour of these monomers. The inclusion of multifunctional acrylates in additive amounts (1.0 vol%) enhanced the graft degree. Modified samples were able to be efficiently stained, allowing the depth of the graft copolymerization to be determined by light microscopy. Water was found to have an accelerating effect on the polymerization of these monomers, but methanol prevented their polymerization completely. The effect of EPDM structural factors upon degree of grafting was found to vary, depending upon the monomer type.
Energy Optimization Audit at Humphreys Engineer Center
2008-09-01
EPDM (ethylene propylene diene M- class [ rubber ]). Doors There are three pairs of doors to the interior terrace (Figure 6) and exit with a high...System EISA Energy Independence and Security Act EPAct Energy Policy Act EPDM EPDM (ethylene propylene diene M-class [ rubber ]) ERDC Engineer
2009-09-30
combustion chamber. Kevlar®-filled ethylene-propylene-diene rubber ( EPDM ) is the baseline insulation material for solid rocket motor cases. A novel...filled EPDM is the industry standard for this application. Since the elastic modulus of rubbers is low, they also act as absorbers during...Santoprene® thermoplastic rubber is already demonstrating their performance capability to replace EPDM in automotive weather seal applications [18]. An
Plasma immersion ion implantation modification of surface properties of polymer material
DOE Office of Scientific and Technical Information (OSTI.GOV)
Husein, I.F.; Zhou, Y.; Qin, S.
1997-12-01
The use of plasma immersion ion implantation (PIII) as a novel method for the treatment of polymer surfaces is investigated. The effect of PIII treatment on the coefficient of friction, contact angle modification, and surface energy of silicone and EPDM (ethylene-propylene-diene monomer) rubber are investigated as a function of pulse voltage, treatment time, and gas species. Low energy (0--8 keV) and high dose ({approximately}10{sup 17}--10{sup 18} ions/cm{sup 2}) implantation of N{sub 2}, Ar, and CF{sub 4} is performed using an inductively coupled plasma source (ICP) at low pressure (0.2 mTorr). PIII treatment reduces the coefficient of friction ({micro}) of siliconemore » rubber from {mu} = 0.464 to the range {mu} = 0.176--0.274, and {mu} of EPDM rubber decreases from 0.9 to the range {mu} = 0.27--0.416 depending on processing conditions. The contact angle of water and diiodomethylene decreases after implantation and increases at higher doses for both silicone and EPDM rubber.« less
Distribution of Oil in a PP/EPDM Thermoplastic Elastomer
NASA Astrophysics Data System (ADS)
Kikuchi, Yutaka; Okada, Tetsuo; Inoue, Takashi
Distribution of oil in a commercial PP(polypropylene)/EPDM(ethylene-propyrene-diene rubber) thermoplastic elastomer was analyzed by light scattering. It was shown that the oil preferentially stays in EPDM particles at low temperatures and it migrates to PP matrix at high temperatures. That is, the oil is expected to play a dual role; softener at ambient temperature and plasticizer at processing temperature. The temperature dependence of oil distribution was nicely interpreted by a thermodynamic discussion.
Hardness and compression resistance of natural rubber and synthetic rubber mixtures
NASA Astrophysics Data System (ADS)
Arguello, J. M.; Santos, A.
2016-02-01
This project aims to mechanically characterize through compression resistance and shore hardness tests, the mixture of hevea brasiliensis natural rubber with butadiene synthetic rubber (BR), styrene-butadiene rubber (SBR) and ethylene-propylene-diene monomer rubber (EPDM). For each of the studied mixtures were performed 10 tests, each of which increased by 10% the content of synthetic rubber in the mixture; each test consisted of carrying out five tests of compression resistance and five tests of shore hardness. The specimens were vulcanized on a temperature of 160°C, during an approximate time of 15 minutes, and the equipment used in the performance of the mechanical tests were a Shimadzu universal machine and a digital durometer. The results show that the A shore hardness increases directly proportional, with a linear trend, with the content of synthetic BR, SBR or EPDM rubber present in the mixture, being the EPDM the most influential. With respect to the compression resistance is observed that the content of BR or SBR increase this property directly proportional through a linear trend; while the EPDM content also increases but with a polynomial trend.
2006-09-30
Nanophase, Thermoplastic Elastomer, EPDM Rubber , Surface Modified MMT Clay, Carbon Nanofibers 16. SECURITY CLASSIFICATION OF: a. REPORT u b. ABSTRACT U...diene rubber ( EPDM ) is the baseline insulation material for solid rocket motor cases. A novel class of insulation materials was developed by the Air...Figure 1. Upon analysis of the control sample, it was observed that the EPDM rubber was totally burned forming a small amount of char, which was easily
Morphological explanation of high tear resistance of EPDM/NR rubber blends.
Gögelein, Christoph; Beelen, Henri Jacob Hubert; van Duin, Martin
2017-06-14
The fatigue properties of cross-linked blends of ethylene propylene diene rubber (EPDM) with low natural rubber (NR) content and reinforced with carbon black (CB) are studied. It is found that such EPDM/NR compounds have superior crack growth resistance and fatigue lifetime. For low NR contents, transmission electron microscopy reveals that the NR phase forms small droplets of 20-50 nm. Remarkably, these droplets are even smaller than the primary CB particles. Atomic force microscopy shows that the the NR phase droplets have a higher loss factor and a smaller elastic modulus than the surrounding EPDM matrix. Rheometer measurements are used to study the effect of the phase morphology on the rubber mechanical properties. These rheological data are compared with the prediction of the Eshelby model describing the effect of elastic inclusions on solids. A complex interplay between the rubber phase morphology and the solubility of both the sulfur cross-linking system and CB is observed, which cannot be predicted theoretically. It is proposed that the soft NR droplets effectively inhibit the crack propagation in the EPDM matrix.
Park, Gayoung; Kim, Yun Hee; Kim, Dong Soo; Ko, Young Chun
2010-05-01
Morphology and vulcanizate properties of EPDM/SBR blends were investigated. AAHR (a mixture of aliphatic and aromatic hydrocarbon resins) was used as a compatibilizer and bis(3-triethoxysilylpropyl)tetrasulfide (TESPT) was used as a coupling agent. The vulcanizate properties and the morphological studies revealed that EPDM and SBR were incompatible, and the addition of AAHR was very effective to enhance the compatibility between EPDM and SBR. The weight percent of bound rubbers was increased with increasing SBR contents. The addition of an AAHR increased the amounts of bound rubbers, and hence the vulcanizate properties such as tear strength and fatigue resistance of the EPDM/SBR blends were improved. The dynamic mechanical analysis and the morphological studies revealed that the addition of TESPT increased the weight of bound rubbers and provided better dispersion of carbon black, resulting in good mechanical properties such as tear strength and fatigue resistance of the vulcanized EPDM/SBR blends. The smaller particle of zinc oxide (i.e., 50 nm > 100 nm > 1000 nm) yielded to the better blending properties of the polymer blend.
EPDM Rubber Modified by Nitrogen Plasma Immersion Ion Implantation.
Kondyurin, Alexey
2018-04-24
Ethylene-propylene diene monomer rubber (EPDM) was treated by plasma immersion ion implantation (PIII) with nitrogen ions of 20 keV energy and fluence from 10 13 to 10 16 ions/cm². The Fourier-transform infrared attenuated total reflection spectra, atomic force microscopy and optical microscopy showed significant structure changes of the surface. The analysis of an interface of PIII treated EPDM rubber with polyurethane binder showed a cohesive character of the adhesion joint fracture at the presence of solvent and interpreted as covalent bond network formation between the PIII treated rubber and the adhesive.
EPDM Rubber Modified by Nitrogen Plasma Immersion Ion Implantation
2018-01-01
Ethylene-propylene diene monomer rubber (EPDM) was treated by plasma immersion ion implantation (PIII) with nitrogen ions of 20 keV energy and fluence from 1013 to 1016 ions/cm2. The Fourier-transform infrared attenuated total reflection spectra, atomic force microscopy and optical microscopy showed significant structure changes of the surface. The analysis of an interface of PIII treated EPDM rubber with polyurethane binder showed a cohesive character of the adhesion joint fracture at the presence of solvent and interpreted as covalent bond network formation between the PIII treated rubber and the adhesive. PMID:29695109
Wu, Hanguang; Tian, Ming; Zhang, Liqun; Tian, Hongchi; Wu, Youping; Ning, Nanying
2014-03-21
The breakup of the rubber phase in an ethylene-propylene-diene monomer (EPDM)/polypropylene (PP) blend at the early stage of dynamic vulcanization is similar to that in an unvulcanized EPDM/PP blend because of the low crosslink density of the EPDM phase. In this work, the minimum size of the rubber phase in the unvulcanized EPDM/PP blend was first calculated by using the critical breakup law of viscoelastic droplets in a matrix. The calculated results showed that the minimum size of the rubber phase in the unvulcanized blend was in the nanometer scale (25-46 nm), not the micrometer scale as reported in many works. Meanwhile, the actual size of the rubber phase in the thermoplastic vulcanizate (TPV) at both the early stage and the final stage of dynamic vulcanization was observed by using peak force tapping atomic force microscopy (PF-AFM). The results indicated that the EPDM phase indeed broke up into nanoparticles at the early stage of dynamic vulcanization, in good agreement with the calculated results. More interestingly, we first revealed that the micrometer-sized rubber particles commonly observed in TPV were actually the agglomerates of rubber nanoparticles with diameters between 40 and 60 nm. The mechanism for the formation of rubber nanoparticles and their agglomerates during dynamic vulcanization was then discussed. Our work provides guidance to control the microstructure of the rubber phase in TPV to prepare high performance TPV products for a wide range of applications in the automobile and electronic industries.
Prediction of packaging seal life using thermoanalytical techniques
DOE Office of Scientific and Technical Information (OSTI.GOV)
Nigrey, P.J.
1997-11-01
In this study, Thermogravimetric Analysis (TGA) has been used to study silicone, Viton and Ethylene Propylene (EPDM) rubber. The studies have shown that TGA accurately predicts the relative order of thermo-oxidative stability of these three materials from the calculated activation energies. As expected, the greatest thermal stability was found in silicone rubber followed by Viton and EPDM rubber. The calculated lifetimes for these materials were in relatively close agreement with published values. The preliminary results also accurately reflect decreased thermal stability and lifetime for EPDM rubber exposed to radiation and chemicals. These results suggest TGA provides a rapid method tomore » evaluate material stability.« less
Waterproofing Underground Concrete Structures
1990-01-01
include Rubberized Asphalt with 42 Polyethylene Cover, Vulcanized Rubbers such as EPDM , Butyl, and Neoprene, Thermoplastics such as PVC, CPE, HDPE, and...welding. However., PVC sheets tend to shrink excessively and become brittle with increasing age . The rubber sheets that are used most often in...underground concrete structures are Butyl rubber and Ethylene. Propylene Diene Monomer ( EPDM ). The adhesives with which they must be sealed are not quite as
1982-03-01
plyethylene PVC landfill- HypalonM PE, CPE, neoprene, EPDM ,* bentqcnite ethylene propylene rubber elasticized polvoleiin 20. A94V C? (Coit" an 0*V" aid...materials include Hyralon®, butyl rubber , EPDM , CPE, neo- prene, polyethylene, polypropylene, PVC8 and elasticized polyolefin. With all of these...and animal and vegetable fats and oils (Geswein, 1975). EPDM , or etiylene propylene rubber , is a terpolymer of ethylene, propylene and a small amount
NASA Astrophysics Data System (ADS)
Özdemir, Tonguç
2008-06-01
In this study, the radiation degradation/modification of the vulcanized EPDM and the effects of dose rate, peroxide type/content in vulcanization system and ENB content of EPDM were studied to investigate the change in the extend of the modification/degradation of the mechanical properties of vulcanized EPDM via gamma irradiation. In addition, thermal, dynamic mechanical, ATR-FTIR, TGA, TGA-FTIR tests were carried out to understand the change of properties of vulcanized EPDM via irradiation. Samples were irradiated with two different dose rates of 1280 and 64.6 Gy/h. Total dose of irradiation was up to 184 kGy. The FTIR spectral analysis showed structural changes of EPDM via irradiation. It was observed that the dose rate changed the mechanical properties with different extends. The change of ENB content of EPDM and peroxide type and content in vulcanization system affect extend of the modification/degradation of the EPDM's properties.
Recommendations for tool-handle material choice based on finite element analysis.
Harih, Gregor; Dolšak, Bojan
2014-05-01
Huge areas of work are still done manually and require the usages of different powered and non-powered hand tools. In order to increase the user performance, satisfaction, and lower the risk of acute and cumulative trauma disorders, several researchers have investigated the sizes and shapes of tool-handles. However, only a few authors have investigated tool-handles' materials for further optimising them. Therefore, as presented in this paper, we have utilised a finite-element method for simulating human fingertip whilst grasping tool-handles. We modelled and simulated steel and ethylene propylene diene monomer (EPDM) rubber as homogeneous tool-handle materials and two composites consisting of EPDM rubber and EPDM foam, and also EPDM rubber and PU foam. The simulated finger force was set to obtain characteristic contact pressures of 20 kPa, 40 kPa, 80 kPa, and 100 kPa. Numerical tests have shown that EPDM rubber lowers the contact pressure just slightly. On the other hand, both composites showed significant reduction in contact pressure that could lower the risks of acute and cumulative trauma disorders which are pressure-dependent. Based on the results, it is also evident that a composite containing PU foam with a more evident and flat plateau deformed less at lower strain rates and deformed more when the plateau was reached, in comparison to the composite with EPDM foam. It was shown that hyper-elastic foam materials, which take into account the non-linear behaviour of fingertip soft tissue, can lower the contact pressure whilst maintaining low deformation rate of the tool-handle material for maintaining sufficient rate of stability of the hand tool in the hands. Lower contact pressure also lowers the risk of acute and cumulative trauma disorders, and increases comfort whilst maintaining performance. Copyright © 2013 Elsevier Ltd and The Ergonomics Society. All rights reserved.
Inertial Upper Stage Thermal Test Program
1989-04-12
EPDM , a tnermal insuiative rubber material covering the SRM ignitor housing, were made in both convective and radiative heater environments under...N2 to ensure an inert environment for these tests. 11 EPDM RUBBER FIBERGLAS PHENOLIC Fig. 2. IUS SRM-2 ignitor. 12 RADIA TOR EMI SHIELD-,," MOVABLE...testing. EPDM Grafoil seal, Viton Thermal-protection materials , IBSTRACT (Continue on reve4 if necessary and identify by block number) An extensive ther
NMR investigation of gaseous SF6 confinement into EPDM rubber.
Neutzler, Sven; Terekhov, Maxim; Hoepfel, Dieter; Oellrich, Lothar Rainer
2005-02-01
The confinement process of gaseous sulphurhexafluoride (SF6) in ethylene-propylene-diene (EPDM) rubber was investigated by spectroscopic and spatially resolved NMR techniques. A strong elongation of T1 relaxation time of SF6 and a decrease of the diffusion coefficient were found. A possible explanation may be the strong restriction of molecular mobility due to interactions between SF6 and active centers of the EPDM.
Thin Film Composite Materials, Phase 2
1987-01-01
were Kevlar coated with silicone, EPDM , or neoprene rubber , with the following results: 1. Tensile testing of coated Kevlar fabric is very difficult...Monte, CA, but the samples were not large enough for our testing program. e. EPDM . This is a rubber compound which consists of ;n ethylene propylene...materials. 2. A method was developed for measuring water vapor permeability. Neoprene and EPDM are promising as coatings with good water resistance; however
Finite Strain Behavior of Polyurea for a Wide Range of Strain Rates
2010-02-01
dimensional dynamic compressive behavior of EPDM rubber ," Journal of Engineering Materials and Technology, Transaction of the ASME, 125:294-301. [97] Song, B...and Chen, W. (2004) "Dynamic compressive behavior of EPDM rubber un- der nearly uniaxial strain conditions," Journal of Engineering Materials and... rubber elastic springs to describe the steep initial stiffness of virgin butadiene rubber under tensile and compressive loading at intermediate strain
Development of Improved Rubber Compounds for Use in Weapon Applications
1974-08-01
temperature properties, oil resistance or resistance to aging were noted for the Japanese elastomers. Rubber For Use In Liquid Propellants Results of a...gun systems. However. EPDM . Hydrln. Butyl EPRVxton an3 Nitroso rubbers were indicated as likely choices. Vulc.nlzates based on the last three of... rubber already in use. An EPDM vulcanizate, Nordel 1070, could be used in liquid propeliant gun systans in which hydrazine is used as an oxidizer
NASA Astrophysics Data System (ADS)
Ginil Mon, S.; Jaya Vinse Ruban, Y.; Vetha Roy, D.
2011-09-01
In the large field of nanotechnology, polymer matrix-based nanocomposites have become a prominent area of current research and development. Exfoliated clay-based nanocomposites have dominated the polymer world with excellent characteristics. EPDM rubber composites have been synthesized by solution-intercalation using the easily available kaolinite as filler. The composite structure has been elucidated by X-ray diffraction (XRD), Fourier transform IR, and scanning electron microscope studies. The molecular level dispersion of clay layers has been verified by the disappearance of basal XRD peak of kaolinite in the EPDM/kaolinite composites. The mechanical properties showed significant improvement of EPDM/kaolinite composites with respect to neat EPDM.
Natural ageing of EPDM composite insulators
DOE Office of Scientific and Technical Information (OSTI.GOV)
Vlastos, A.E.; Sherif, E.
1990-01-01
Long-rod composite insulators, with weather sheds (sheds) made of ethylene propylene rubbers (EPDM), were exposed for many years to HVAC and HVDC under realistic conditions and natural pollution. The change of their properties with time and their aging was studied. The results show that the insulator shed material undergoes a slow degradation process and loses successively its water repelling properties which initially make the EPDM composite insulators superior to inorganic glass and porcelain insulator. The outdoor degradation of the shed material depends on the electric stress, in the environmental factors (such as pollution, rain, salt-laden fog, and UV-radiation from sun)more » and on the materials and fillers used in the construction of the composite insulators. A thorough macro- and microscopic study of the EPDM composite insulator sheds illustrates the differences of the surface state of EPDM insulators of different makes in which different basic material compositions and fillers are used. The poor performance of aged EPDM composite insulators compared to inorganic insulators depends on the design and on environmental factors.« less
Hugoniot-based equations of state for two filled EPDM rubbers
NASA Astrophysics Data System (ADS)
Pacheco, A. H.; Dattelbaum, D. M.; Orler, E. B.; Bartram, B. D.; Gustavsen, R. L.
2014-05-01
Particle-filled elastomers are commonly used as engineering components due to their ability to provide structural support via their elastic mechanical response. Even small amounts of particle fillers are known to increase the mechanical strength of elastomers due to polymer-filler interactions. In this work, the shock response of two filled (SiO2 or silica and KevlarTMfillers) ethylene-propylene-diene (EPDM) rubbers were studied using single and two-stage gas gun-driven plate impact experiments. Hugoniot states were determined using standard plate impact methods. Both filled-EPDM elastomers exhibit high compressibility under shock loading and have a response similar to adiprene rubber.
Assessment of Alternatives for Upgrading Navy Solid Waste Disposal Sites. Volume 2.
1981-08-01
chloride (PVC), butyl rubber , Hypalon, ethylene propylene diene monomer ( EPDM ) , and chlorinated polyethylene (CPE). These materials have been used...September 1976): • Butyl rubber • Chlorinated polyethylene (CPE) • Chlorosulfonate polyethylene (hypalon) • Ethylene propylene rubber ( EPDM ...CLASSIFICATION OF THIS » AGE r*T>«n D«a Eni.r.a) V • 1 . i , ... »*l«. • • ,.,. • ’in EXECUTIVE SUMMARY ASSESSMENT OF
Combined effects of microwaves, electron beams and polyfunctional monomers on rubber vulcanization.
Manaila, Elena; Martin, Diana; Stelescu, Daniela Zuga; Craciun, Gabriela; Ighigeanu, Daniel; Matei, Constantin
2009-01-01
This paper presents comparative results obtained by conventional vulcanization with benzoyl peroxide (CV-BP), separate electron beam vulcanization (EB-V) and simultaneous electron beam and microwave vulcanization (EB+MW-V) applied to two kind of rubber samples: EVA (ethylene vinyl acetate) rubber-sample (EVA-sample) and EPDM (ethylene-propylene terpolymer) rubber-sample (EPDM-sample). The EVA-samples contain 61.54% EVA Elvax 260, 30.77% carbon black, 1.85% TAC (triallylcyanurate) polyfunctional monomer and 5.84% filler (zinc oxide, stearic acid, polyethylene glycol and antioxidant). The EPDM-samples contain 61.54% EPDM Nordel 4760, 30.77% carbon black, 1.85% TMPT (trimethylopropane trimethacrylate) polyfunctional monomer and 5.84% filler (zinc oxide, stearic acid, polyethylene glycol and antioxidant). The rubber samples designed for different vulcanization methods were obtained from raw rubber mixtures, as compressed sheets of 2 mm in the polyethylene foils to minimize oxidation. For EB and EB + MW treatments the sheets were cut in rectangular shape 0.15 x 0.15 m2. The physical properties of samples obtained by CV-BP EV-Vand EB + MW-V methods were evaluated by measuring the tearing strength, residual elongation, elongation at break, tensile strength, 300% modulus, 100% modulus, elasticity and hardness. The obtained results demonstrate an improvement of rubber several properties obtained by EB and EB + MW processing as compared to classical procedure using benzoyl peroxide.
Rubber contact mechanics: adhesion, friction and leakage of seals.
Tiwari, A; Dorogin, L; Tahir, M; Stöckelhuber, K W; Heinrich, G; Espallargas, N; Persson, B N J
2017-12-13
We study the adhesion, friction and leak rate of seals for four different elastomers: Acrylonitrile Butadiene Rubber (NBR), Ethylene Propylene Diene (EPDM), Polyepichlorohydrin (GECO) and Polydimethylsiloxane (PDMS). Adhesion between smooth clean glass balls and all the elastomers is studied both in the dry state and in water. In water, adhesion is observed for the NBR and PDMS elastomers, but not for the EPDM and GECO elastomers, which we attribute to the differences in surface energy and dewetting. The leakage of water is studied with rubber square-ring seals squeezed against sandblasted glass surfaces. Here we observe a strongly non-linear dependence of the leak rate on the water pressure ΔP for the elastomers exhibiting adhesion in water, while the leak rate depends nearly linearly on ΔP for the other elastomers. We attribute the non-linearity to some adhesion-related phenomena, such as dewetting or the (time-dependent) formation of gas bubbles, which blocks fluid flow channels. Finally, rubber friction is studied at low sliding speeds using smooth glass and sandblasted glass as substrates, both in the dry state and in water. The measured friction coefficients are compared to theory, and the origin of the frictional shear stress acting in the area of real contact is discussed. The NBR rubber, which exhibits the strongest adhesion both in the dry state and in water, also shows the highest friction both in the dry state and in water.
Development of a Two-Piece Mask and Lens and Mold for Same.
1980-05-01
Antioxidants in EPDM -6150C Heat - Ref. No. Antioxidant Composition of Antioxidant % gel aged Unaged QA0010-Q Control 98.16 1 3.5 -1 Agerite NA Polymeric...Uniroyal. With the exception of Royalene 100, which is an SPu, the types we examined are EPDM rubbers . Our trials with Royalene 100 were not successful...with aliphatic hydrocarbons is probably what explains the good compatibility of this resin with EPDM rubbers , one of our candidate polymers. Elvax resins
Wu, Chang Mou; Hsieh, Wen Yen; Cheng, Kuo Bin; Lai, Chiu-Chun; Lee, Kuei Chi
2018-05-09
The triacetin and nitroglycerin barrier properties of layered-silicate reinforced ethylenepropylenediene monomer/chloroprene rubber (EPDM/CR) nanorubbers were investigated as rocket-propellant inhibitors. EPDM/CR nanorubbers with intercalated structures were formulated and prepared by the melt-compounding method. The triacetin permeability and nitroglycerin absorption were observed to decrease with increasing layered-silicate content. The layered silicates also improved the flame retardancies of the nanorubbers by forming silicate reinforced carbonaceous chars. Layered-silicate reinforced EPDM/CR nanorubbers are potentially effective rocket propellant-inhibiting materials.
A green procedure using ozone for Cleaning-in-Place in the beverage industry.
Nishijima, Wataru; Okuda, Tetsuji; Nakai, Satoshi; Okada, Mitsumasa
2014-06-01
Cleaning-in-Place (CIP) in the beverage industry is typically carried out in production lines with alkaline and acidic solutions with detergents. This cleaning not only produces alkaline and acidic wastewater with detergents but also takes significant time. One of the important targets for CIP is adsorbed odorous compounds on gaskets, hence, we have tried to establish a rapid and green CIP process to remove traces of such compounds, especially d-limonene, an odorous component of orange juice, using two approaches; an ozone cleaning method and a change of gasket material from ethylene propylene diene monomer (EPDM) rubber to silicone rubber. By changing the gasket material from EPDM rubber to silicone rubber, the removability of d-limonene by typical alkaline and acidic cleanings with detergents was improved. However, complete removal of 4 mg g(-1) of d-limonene on both EPDM and silicone gaskets could not be achieved even using a series of conventional cleaning procedures that included alkaline and acidic cleaning for 220 min. Ozone treatment dramatically improved the removability of d-limonene, removing 87% from the EPDM gasket at 60 min and 100% from the silicone gasket at 30 min. The combination of the silicone gasket and ozone treatment resulted in the most effective cleaning. The main removal mechanism for ozone treatment was confirmed to be oxidation by molecular ozone. Effectiveness of changing the gasket material from EPDM rubber to silicone rubber in reducing residual amounts of odorous compounds adsorbed on the gaskets was also confirmed for furfural and 4-vinylguaiacol. Copyright © 2014 Elsevier Ltd. All rights reserved.
NASA Astrophysics Data System (ADS)
Indrajati, I. N.; Dewi, I. R.
2017-07-01
The objective of this study was to evaluate the performance of maleated castor oil (MACO) as plasticizer on natural rubber (NR), ethylene propylene diene monomer (EPDM), and nitrile butadiene rubber (NBR). The parameter studied were involving rheological, curing and swelling properties. The MACOs were prepared by an esterification reaction between castor oil (CO) and maleic anhydride (MAH) with the help of xylene as water entrainer to improve water removal. Resulting oils then applied as a plasticizer in each of those rubbers within a fixed loading of 5 phr. Comparison has been made to evaluate the performance of MACO and conventional plasticizer (paraffinic oil for NR and EPDM, DOP for NBR) on each rubber. Rheology, curing characteristic and swelling of each rubber were studied. The results showed that rubber (NR/EPDM/NBR) plasticized with MACO had given similar flow characteristic to conventional plasticizers. MACO exhibited slow curing, confirmed by higher t90, but the scorch safety was of the same magnitude. MAH loading tended to decrease the flow properties and curing rate, while scorch time (ts2) was independent.
NMR measurements of gaseous sulfur hexafluoride (SF6) to probe the cross-linking of EPDM rubber.
Terekhov, M; Neutzler, S; Aluas, M; Hoepfel, D; Oellrich, L R
2005-11-01
The effects of embedding gaseous SF6 into EPDM rubber were investigated using NMR methods. It was found that observed sorption and desorption processes follow the behavior of the dual mode sorption model. A strong correlation was found between EPDM cross-linking and transversal relaxation time of embedded SF6. EPDM samples with different cross-link densities, preliminarily determined by 1H transversal relaxation using the Gotlib model and Litvinov's method, were investigated using embedded SF6. The sensitivity of the 19F transversal relaxation rate of SF6 to the EPDM cross-link density variation was found to be at least 10 times higher than for 1H in the polymer chain. First experiments on probing the swelling effects in EPDM due to its contact with polar liquids have been performed. Copyright (c) 2005 John Wiley & Sons, Ltd.
Analytical Prediction of Lower Leg Injury in a Vehicular Mine Blast Event
2010-01-01
the spring constant of the tibia is nearly arbitrary; the spring constant of the boot assumes a hard ethylene propylene diene monomer ( EPDM ) rubber ...the sole of the boot. The significantly lower spring constant of the EPDM rubber in the sole compared to the bone structures greatly diminished the
On the radiation induced degradation of NBR-EPDM rubbers
NASA Astrophysics Data System (ADS)
Chipara, M. D.; Grecu, V. V.; Chipara, M. I.; Ponta, C.; Reyes Romero, J.
1999-05-01
The modification of the elongation at break for NBR-EPDM rubbers subjected to gamma irradiation at various integral doses ranging from 10 to 200 kGy, at different dose rates (0.14, 0.47, 1, 3, 4.7 kGy/h) are reported. The presence of the dose rate effect is noticed.
Flexible strain sensor based on carbon nanotube rubber composites
NASA Astrophysics Data System (ADS)
Kim, Jin-Ho; Kim, Young-Ju; Baek, Woon Kyung; Lim, Kwon Taek; Kang, Inpil
2010-04-01
Electrically conducting rubber composites (CRC) with carbon nanotubes (CNTs) filler have received much attention as potential materials for sensors. In this work, Ethylene propylene diene M-class rubber (EPDM)/CNT composites as a novel nano sensory material were prepared to develop flexible strain sensors that can measure large deformation of flexible structures. The EPDM/CNT composites were prepared by using a Brabender mixer with multi-walled CNTs and organo-clay. A strain sensor made of EPDM/CNT composite was attached to the surface of a flexible beam and change of resistance of the strain sensor was measured with respect to the beam deflection. Resistance of the sensor was change quite linearly under the bending and compressive large beam deflection. Upon external forces, CRC deformation takes place with the micro scale change of inter-electrical condition in rubber matrix due to the change of contact resistance, and CRC reveals macro scale piezoresistivity. It is anticipated that the CNT/EPDM fibrous strain sensor can be eligible to develop a biomimetic artificial neuron that can continuously sense deformation, pressure and shear force.
Riba Ruiz, Jordi-Roger; Canals, Trini; Cantero, Rosa
2017-01-01
Ethylene propylene diene monomer (EPDM) rubber is widely used in a diverse type of applications, such as the automotive, industrial and construction sectors among others. Due to its appealing features, the consumption of vulcanized EPDM rubber is growing significantly. However, environmental issues are forcing the application of devulcanization processes to facilitate recovery, which has led rubber manufacturers to implement strict quality controls. Consequently, it is important to develop methods for supervising the vulcanizing and recovery processes of such products. This paper deals with the supervision process of EPDM compounds by means of Fourier transform mid-infrared (FT-IR) spectroscopy and suitable multivariate statistical methods. An expedited and nondestructive classification approach was applied to a sufficient number of EPDM samples with different applied processes, that is, with and without application of vulcanizing agents, vulcanized samples, and microwave treated samples. First the FT-IR spectra of the samples is acquired and next it is processed by applying suitable feature extraction methods, i.e., principal component analysis and canonical variate analysis to obtain the latent variables to be used for classifying test EPDM samples. Finally, the k nearest neighbor algorithm was used in the classification stage. Experimental results prove the accuracy of the proposed method and the potential of FT-IR spectroscopy in this area, since the classification accuracy can be as high as 100%.
NASA Astrophysics Data System (ADS)
Razak, Jeefferie Abd; Ahmad, Sahrim Haji; Ratnam, Chantara Thevy; Mahamood, Mazlin Aida; Yaakub, Juliana; Mohamad, Noraiham
2014-09-01
Fractional 25 two-level factorial design of experiment (DOE) was applied to systematically prepare the NR/EPDM blend using Haake internal mixer set-up. The process model of rubber blend preparation that correlates the relationships between the mixer process input parameters and the output response of blend compatibility was developed. Model analysis of variance (ANOVA) and model fitting through curve evaluation finalized the R2 of 99.60% with proposed parametric combination of A = 30/70 NR/EPDM blend ratio; B = 70°C mixing temperature; C = 70 rpm of rotor speed; D = 5 minutes of mixing period and E = 1.30 phr EPDM-g-MAH compatibilizer addition, with overall 0.966 desirability. Model validation with small deviation at +2.09% confirmed the repeatability of the mixing strategy with valid maximum tensile strength output representing the blend miscibility. Theoretical calculation of NR/EPDM blend compatibility is also included and compared. In short, this study provides a brief insight on the utilization of DOE for experimental simplification and parameter inter-correlation studies, especially when dealing with multiple variables during elastomeric rubber blend preparation.
2002-09-01
bitumens, EPDM , and PVC. Most heat-driven aging tests for building materials use a temperature of 70 °C. Ultraviolet radiation exposure in the...of 0.85 mm/sec. These samples generated three types of load-strain curves. A relatively straight line was generated by each EPDM rubber sample...Mathey 1974) at -18 °C. Except for the EPDM rubber membranes and Sample H, all samples tested comply with this suggested requirement. Sample H is an
Hsieh, Wen Yen; Cheng, Kuo Bin; Lai, Chiu-Chun; Lee, Kuei Chi
2018-01-01
The triacetin and nitroglycerin barrier properties of layered-silicate reinforced ethylenepropylenediene monomer/chloroprene rubber (EPDM/CR) nanorubbers were investigated as rocket-propellant inhibitors. EPDM/CR nanorubbers with intercalated structures were formulated and prepared by the melt-compounding method. The triacetin permeability and nitroglycerin absorption were observed to decrease with increasing layered-silicate content. The layered silicates also improved the flame retardancies of the nanorubbers by forming silicate reinforced carbonaceous chars. Layered-silicate reinforced EPDM/CR nanorubbers are potentially effective rocket propellant-inhibiting materials. PMID:29747427
NASA Astrophysics Data System (ADS)
Özdemir, T.; Güngör, A.; Reyhancan, İ. A.
2017-02-01
In this study, EPDM and boron trioxide composite was produced and mechanical, thermal and neutron shielding tests were performed. EPDM rubber (Ethylene Propylene Diene Monomer) having a considerably high hydrogen content is an effective neutron shielding material. On the other hand, the materials containing boron components have effective thermal neutron absorption crossection. The composite of EPDM and boron trioxide would be an effective solution for both respects of flexibility and effectiveness for developing a neutron shielding material. Flexible nature of EPDM would be a great asset for the shielding purpose in case of intervention action to a radiation accident. The theoretical calculations and experimental neutron absorption tests have shown that the results were in parallel and an effective neutron shielding has been achieved with the use of the developed composite material.
Chen, Yukun; Xu, Chuanhui; Cao, Liming; Wang, Yanpeng; Fang, Liming
2013-06-27
Polypropylene (PP)/ethylene-propylene-diene monomer (EPDM)/zinc dimethacrylate (ZDMA) blend (EPDM/PP ratio of 30/70) with remarkable extensibility was successfully prepared via peroxide dynamic vulcanization. The uniaxial tensile properties, crystallization behavior, structure, and morphology during stretching were investigated. The tensile process study showed that the PP/EPDM/ZDMA blend exhibited the rubbery-like behavior with an elongation beyond 600%. The ZDMA graft-product domain increased the compatibility and interfacial adhesion between rubber and PP phases, while it reduced the crystallinity of the PP phase. On the basis of TEM and SEM analyses, we found that the cross-linked rubber particles could be elongated and oriented along the tensile direction, whereas the ZDMA graft-product domain "encapsulated" rubber phase together, acting as a "bridge" between elongated rubber phases and the PP phase during uniaxial stretching. The stress could be effectively transferred from the PP phase to the numerous elongated rubber phases due to the excellent compatibility and interfacial adhesion between rubber and PP phases, resulting in the rubbery-like behavior.
Synthetic-rubber extrusions form low cost roll-on solar collector
DOE Office of Scientific and Technical Information (OSTI.GOV)
Smay, V.E.
1979-06-01
Synthetic rubber extrusions composed of ethylene propylene diene monomer (EPDM) have been developed in 4.4-inch-wide mats as solar absorbers that are light weight and simple to install. The mats, which come in rolls up to 600 ft long, have 6 small tubes alternating with thin webbing. EPDM has a lifespan of 30-50 yrs and maintains its flexibility within a temperature range of -80 to 375/sup 0/F. The mats are laid over rigid insulation and covered with glazing, detailed assembly instructions are provided. EPDM is not subject to corrosion and is not damaged by freezing water, a second EPDM extrusion ismore » used for glazed solar collectors. The efficiency of the design is attributed to the greater surface-to-mass ratio, permitting more heat collection, and the smaller mass of the synthetic rubber, which allows faster heat-up. The total cost for a complete, installed solar heating system of this type, including pumps, tanks, and plumbing, is about $12/ft/sup 2/.« less
NASA Astrophysics Data System (ADS)
Ryzhikova, I. G.; Bauman, N. A.; Volkov, A. M.; Kazakov, Yu. M.; Volfson, S. I.
2014-05-01
The study concerned the effect of molecular-mass characteristics and Mooney viscosity of the initial EPDM rubber on the changes in the structure, impact strength and rheological properties of PP/EPDM blends as a result of their modification in a melt under the action of organic peroxide and peroxide-trimethylolpropane triacrylate (TMPTA) system.
Low-Level Analytical Methodology Updates to Support Decontaminant Performance Evaluations
2011-06-01
from EPDM and tire rubber coupon materials that were spiked with a known amount of the chemical agent VX, treated with bleach decontaminant, and...to evaluate the performance of bleach decontaminant on EPDM and tire rubber coupons. Dose-confirmation or Tool samples were collected by delivering...components • An aging or damaged analytical column • Dirty detector • Other factors related to general instrument and/or sample analysis performance
DOE Office of Scientific and Technical Information (OSTI.GOV)
Vroomen, G.L.M.; Visser, G.W.; Gehring, J.
1991-11-01
Normally EPDM rubbers are vulcanized by systems based on sulphur, resin or peroxide. The common feature of these systems is that they all require activator energy in the form of heat. The (extremely) high temperatures (approximately 180C) have the disadvantage that the final properties of the finished product may be affected in one way or another by a variety of uncontrolled side reactions which may occur. Radiation curing, on the other hand, is a process which differs from those mentioned above in that the final curing is carried out at about 20C under closely controlled conditions (such as radiation dose,more » penetration depth, etc.), and this form of curing ultimately results in a more well-defined end product. In the rubber industry, this technique is used by large rubber processors (for example, in roof sheeting and cable production). Its widespread use is, however, impeded by the high investment costs. One way of avoiding these high costs is to arrange for the products to be irradiated by contractors. The optimum radiation dose for EPDM is determined by the required pattern of properties. From this study it may be concluded that the network is primarily built up at a radiation dose of up to approximately 100 kGy. The degree to which it is built up depends partly on the coactivator used and the EPDM type used. In choosing the coactivator, allowance has to be made for its solubility in EPDM. The type of oil chosen and any stabilizer additions will affect the crosslinking efficiency. Contrary to studies published earlier, in this study it was found that when EDMA is used as a coactivator, no difference can be detected between a DCPD type (4%) and an ENB type (4%), provided both have an identical molecular weight distribution. Increasing the ENB content has less effect on the final crosslink density than using a type having a broader molecular weight distribution.« less
Hugoniot-based equations of state for two filled EPDM rubbers
NASA Astrophysics Data System (ADS)
Pacheco, Adam; Dattelbaum, Dana; Orler, E.; Gustavsen, R.
2013-06-01
The shock response of silica filled and Kevlar filled ethylene-propylene-diene (EPDM) rubbers was studied using gas gun-driven plate impact experiments. Both materials are proprietary formulations made by Kirkhill-TA, Brea CA USA, and are used for ablative internal rocket motor insulation. Two types of experiments were performed. In the first, the filled-EPDM sample was mounted on the front of the projectile and impacted a Lithium Fluoride (LiF) window. The Hugoniot state was determined from the measured projectile velocity, the EPDM/LiF interface velocity (measured using VISAR) and impedance matching to LiF. In the second type of experiment, electromagnetic particle velocity gauges were embedded between layers of filled-EPDM. These provided in situ particle velocity and shock velocity measurements. Experiments covered a pressure range of 0.34 - 14 GPa. Hugoniot-based equations of state were obtained for both materials, and will be compared to those of other filled elastomers such as silica-filled polydimethylsiloxane and adiprene. Work performed while at Los Alamos National Laboratory.
The heterogeneity of segmental dynamics of filled EPDM by (1)H transverse relaxation NMR.
Moldovan, D; Fechete, R; Demco, D E; Culea, E; Blümich, B; Herrmann, V; Heinz, M
2011-01-01
Residual second moment of dipolar interactions M(2) and correlation time segmental dynamics distributions were measured by Hahn-echo decays in combination with inverse Laplace transform for a series of unfilled and filled EPDM samples as functions of carbon-black N683 filler content. The fillers-polymer chain interactions which dramatically restrict the mobility of bound rubber modify the dynamics of mobile chains. These changes depend on the filler content and can be evaluated from distributions of M(2). A dipolar filter was applied to eliminate the contribution of bound rubber. In the first approach the Hahn-echo decays were fitted with a theoretical relationship to obtain the average values of the (1)H residual second moment
Gu, Zhen; Zhang, Xian; Ding, Xin; Bao, Chao; Fang, Fei; Li, Shiyuan; Zhou, Haifeng; Xue, Meng; Wang, Huan; Tian, Xingyou
2014-08-28
This article studied the influence of silica (SiO2) particles on the crosslinked network and the molecular mobility of ethylene-propylene-diene (EPDM) rubber chains by dynamic mechanical analysis (DMA). When SiO2 fraction is lower than 8 phr, the chain segments that participate in the glass-rubber transition (α transition) decrease with increasing the SiO2 content, while the whole crosslinked network is almost unaffected by the presence of SiO2. When the SiO2 fraction increases to about 20 phr, there appears a new tan δ peak (α' transition) above the α transition. This could be because the crosslinking reaction took place only on a small scale and the formed network became gradually incomplete when the content of the particles exceeded some critical value, and the α' transition is attributed primarily to the motion of non-elastic network chains loosely attached to the three-dimensional network. However, at SiO2 loadings higher than 40 phr, the crosslinking density was kept basically constant. The α' transition is hindered by a restriction of the chain mobility due to SiO2. The different changes of α' transition depended on the two coupled effects of SiO2, including restricting the chain mobility and decreasing the crosslinking density. Correspondingly, with increasing the mobility of EPDM chains and SiO2-induced strengthening, the mechanical properties of EPDM composite are dramatically improved. With the addition of 20 phr of SiO2 in the EPDM, a 113% increase in the elongation at break, a 510% increase in the fracture energy, and a 283% increase in the tensile strength are achieved.
The heterogeneity of segmental dynamics of filled EPDM by 1H transverse relaxation NMR
NASA Astrophysics Data System (ADS)
Moldovan, D.; Fechete, R.; Demco, D. E.; Culea, E.; Blümich, B.; Herrmann, V.; Heinz, M.
2011-01-01
Residual second moment of dipolar interactions M∼2 and correlation time segmental dynamics distributions were measured by Hahn-echo decays in combination with inverse Laplace transform for a series of unfilled and filled EPDM samples as functions of carbon-black N683 filler content. The fillers-polymer chain interactions which dramatically restrict the mobility of bound rubber modify the dynamics of mobile chains. These changes depend on the filler content and can be evaluated from distributions of M∼2. A dipolar filter was applied to eliminate the contribution of bound rubber. In the first approach the Hahn-echo decays were fitted with a theoretical relationship to obtain the average values of the 1H residual second moment
NASA Astrophysics Data System (ADS)
Mirzadeh, Amin
For this work, different grades of polypropylene-g-maleic anhydride polymers were chosen to elucidate the effect of compatibilizer on the nanoclay dispersion level in thermoplastic phase. X-ray diffraction (XRD) patterns along with transmission electron microscopy (TEM) and scanning electron microscope (SEM) micrographs confirmed that prepared PP nanocomposites ranged from intercalated structure to a coexistence of intercalated tactoids and exfoliated layers namely “partially exfoliated” nanocomposite. Among various factors affecting the compatibilizer performance, it is shown that only the relaxation behaviour of compatibilizer correlates directly with the nanocomposites characterization results; higher relaxation times of the compatibilizer are associated with better dispersion of nanoclay. To study the co-continuity development of the nonreactive blends, EPDM and the mentioned PP nanocomposites at various compositions were melt blended using an internal mixer. Based on continuity measurements of TPEs and TPE nanocomposites for both thermoplastic and rubber phase, it is shown that the presence of nanoclay decreases the co-continuity composition range and alters its symmetrical feature. However, this effect is more pronounced in the intercalated nanocomposites than in partially exfoliated nanocomposites. It seems that better nanoclay dispersion limits the reduction of the thermoplastic phase continuity in a manner that the continuity index of the thermoplastic phase for partially exfoliated TPE nanocomposite prepared at high EPDM content (i.e. at 70 wt%) is greater than that of corresponding TPE without nanoclay. According to these results, it is possible to shift to higher EPDM content using partially exfoliated system before formation of matrix-dispersed particle structure which limits thermoplastic vulcanizate production. This should be mentioned that gamma irradiation was carried out in order to fix the EPDM morphology to estimate the continuity of PP using the solvent extraction and gravimetry technique. Additionally, the effect of continuity on rheological behaviour of TPE nanocomposites was investigated. The ultimate goal in this field is to maximize the rubber like behaviour by controlling the blend morphology and the level of crosslinking. Therefore, this study also covers the effects of nanoclay presence and its dispersion level on the crosslinking reaction of thermoplastic vulcanizate nanocomposites prepared by reactive extrusion. Here, the rubber phase was dynamically vulcanized using dimethylol phenolic resin or octylphenol-formaldehyde resin along with stannous chloride dihydrate as the catalyst. In the present study, the dynamic vulcanization of the prepared TPVs and corresponding nanocomposites are characterized using different criteria, such as gel content, viscosity and normalized storage modulus in the time sweep tests, nuclear magnetic resonance (NMR) signal line width, bound curative content and residual diene concentration. The combination of the above parameters appears to be sufficient to provide a clear description of the systems. The last part of the present study is devoted to find how the dispersion level of nanoclay and consequently the extent of crosslinking change the rubber like behaviour and the morphology of the prepared TPVs. Therefore, recently developed method named temperature scanning stress relaxation (TSSR) was used to estimate the rubber indices of TPVs and TPV nanocomposites. The mentioned method also successfully provided information about the extent of crosslinking reaction. It is shown that the rubber like behaviour of the blends containing 50wt% and 60wt% of EPDM in which morphological studies suggest the presence of the rubber droplets in vicinity of irregular shape rubber particles with a low level of interconnectivity, correlates with the rubber droplet size. Therefore, the nanoclay presence affects the rubber index values mainly through its effect on the size of the rubber droplets that controls the number of retraction points in the proposed buckling mechanism during the TSSR test. It should be mentioned that by increasing the EPDM content, the number of the droplet like domains decreases and more irregular shape rubber particles is formed. On the other hand, the direct relation between rubber index values and the crosslink density is observed only for those series of TPVs showing the fully developed extensive network between irregular shape rubber domains (blends containing 70wt% of EPDM). Hence, the nanoclay dispersion level influences the rubber like behaviour through its effect on the crosslink density. (Abstract shortened by UMI.).
Surface structural changes of naturally aged silicone and EPDM composite insulators
DOE Office of Scientific and Technical Information (OSTI.GOV)
Vlastos, A.E.; Gubanski, S.M.
1991-04-01
In a long-term outdoor test with high direct and alternating voltages, silicone and EPDM rubber composite insulators have, at the beginning, shown a superior performance to that of glass and porcelain insulators. In the long-term test, however, the silicone rubber composite insulator has, in spite of the ageing of both insulator types, kept its good performance, while the performance of the EPDM rubber composite insulator was drastically deteriorated. In order to get a better insight into results obtained, the wettability and the surface structural changes of the insulators were studied by the drop deposition method (using a goniometer) and bymore » advanced techniques such as SEM, ESCA, FTIR and SIMS respectively. The results show that the differences in performance have to be found in the differences in the surface structural changes and in the dynamic ability of the surface to compensate the ageing.« less
Response of ethylene propylene diene monomer rubber (EPDM) to simulant Hanford tank waste
DOE Office of Scientific and Technical Information (OSTI.GOV)
NIGREY,PAUL J.
2000-02-01
This report presents the findings of the Chemical Compatibility Program developed to evaluate plastic packaging components that may be incorporated in packaging mixed-waste forms for transportation. Consistent with the methodology outlined in this report, the author performed the second phase of this experimental program to determine the effects of simulant Hanford tank mixed wastes on packaging seal materials. That effort involved the comprehensive testing of five plastic liner materials in an aqueous mixed-waste simulant. The testing protocol involved exposing the materials to {approximately}143, 286, 571, and 3,670 krad of gamma radiation and was followed by 7-, 14-, 28-, 180-day exposuresmore » to the waste simulant at 18, 50, and 60 C. Ethylene propylene diene monomer (EPDM) rubber samples subjected to the same protocol were then evaluated by measuring seven material properties: specific gravity, dimensional changes, mass changes, hardness, compression set, vapor transport rates, and tensile properties. The author has determined that EPDM rubber has excellent resistance to radiation, this simulant, and a combination of these factors. These results suggest that EPDM is an excellent seal material to withstand aqueous mixed wastes having similar composition to the one used in this study.« less
NASA Astrophysics Data System (ADS)
Kwak, Eung-Bum; Choi, Nak-Sam
The degradation behaviors of EPDM (ethylene-propylene diene monomer) rubbers used for automotive radiator hoses subjected to thermo-oxidative and electrochemical stresses were studied. As a result of the thermo-oxidative aging tests, the IRHD (international rubber hardness degrees) hardness of the rubber specimens increased, while their elongation at break decreased much. A slight increase in crosslink density indicated that changes in the properties were caused by the concentration of carbonyl groups in the skin layer. For the electrochemical degradation (ECD), the weight of rubber specimens increased whereas their elongation and hardness much decreased because water solution penetrated into the skin part. There was little change in crosslink density. Formation of many chain scissions and thus microvoid networks in the skin layer induced the swelling behavior leading to a linear reduction of hardness versus the weight increase.
New Polytetrahydrofuran Graft Copolymers.
1979-03-15
chioroprene) , chiorobutyl - ~~~~~ rubber , bromobutyl rubber , chlorinated EPDM , chlorinated poly(buta— diene) and chlorinated butadiene styrene copolymer...bromobutyl rubber , which after dehalogenation is unstable with respect to conjugated dienes, the yields of graft copolymer are low. With poly(chloroprerte
Demonstration of Corrosion-Resistant Fire Hydrant Retrofits for Military Installations
2013-10-01
diene M-class rubber ( EPDM )/powder coated steel sleeve inserted into the top of the hy- drant barrel at the traffic breakaway allowing the seat for...The insert seat of the valve shall be made of a ethylene propylene diene M-class rubber ( EPDM )/powder coated steel sleeve in- serted into the top of...intentional water-supply contamination. The technology was installed on 90 fire hy- drants of various makes, models, and ages at Fort Leonard Wood, MO. To
1980-02-01
propylene rubber) EPDM Brake valve parts and seals 80 EPDM (SAE, RM 69) Referee test slabs 70L VITON 0-rings 70 TN4 -i______ - -.- . .J....... TABLE 2...separated. The volume and hardness of two rubber test specimens was determined. One specimen was placed in the lower fluid layer (conventional fluid...and one specimen was suspended horizontally in the top fluid layer (silicone). The jar was stored on the laboratory shelf at ambient temperature. The
In vitro biocompatibility of EPM and EPDM rubbers.
Mast, F; Hoschtitzky, J A; Van Blitterswijk, C A; Huysmans, H A
1997-01-01
The in vitro toxicity of two EPDM rubbers (K 778 and K 4802) and one EPM rubber (K 740) was tested using human fibroblasts. The modulus of elasticity of each rubber was varied by exposure to different amounts of electron-beam radiation (0, 5 and 10 Mrad). The short-term in vitro toxicity was tested by culturing cells on polymer films. The long-term effect of ageing was simulated by growing fibroblasts in nutrient media prepared from extracts of heat-exposed materials. Cell cultures were studied both quantitatively and (ultra) structurally. Growth curves obtained in the toxicity test did not differ significantly from control values at any day of observation, and also showed that electron-beam radiation did not alter the biocompatibility. The same results were found for all but one material in the artificial ageing test. The number of cells in the K4802/10 Mrad extraction medium was decreased. Ultrastructurally no gross deviations from normal morphology were observed, either in the direct contact test or in the artificial ageing test. The most characteristic feature was a somewhat dilated endoplasmic reticulum. In summary, the in vitro biocompatibility of EPDM-rubbers as observed in this study is satisfactory and motivates further investigation of their biocompatibility in animal experiments.
Wang, Fang; Xu, Juan; Luo, Heyi; Wang, Jinggang; Wang, Qian
2009-10-12
Practical adhesion of rubber to aluminum is measured for various aluminum silanization treatments. In this study, 6-(3-triethoxysilylpropylamino)-1,3,5-triazine-2,4-dithiol (TES) was used as the coupling agent for preparing self-assembly monolayers (SAMs) on an aluminum surface. The structure and chemical composition of the SAMs were analyzed using Fourier transform infra-red spectroscopy (FT-IR) and X-ray photoelectron spectroscopy (XPS). The changes in the surface features of the aluminum surface due to TES treatment were investigated by atomic force microscopy (AFM). The adhesive properties of the silanized aluminum surface and EPDM rubber have been evaluated by a T-peel strength test. The results suggested that the Si-O-Al bonding at aluminum TES interface existed and a TES self-assembly monolayer was formed on the aluminum surface. More than 6.0 KN/m adhesion strength is obtained when the aluminum is silanized with 2.5 mmol/dm(3) TES, cured at 160 degrees C and vulcanized with EPDM rubber at 160 degrees C for 30 min. It is suggested that the TES self-assembly monolayer is bound to aluminum through its ethoxysilyl functional group, and the thiol function group is strongly crosslinked to EPDM rubber, respectively.
DOE Office of Scientific and Technical Information (OSTI.GOV)
Soerqvist, T.; Vlastos, A.E.
1996-12-31
The hydrophobicity of polymeric insulators is crucial for their performance. This paper reports the hydrophobicity and the peak leakage current statistics of one porcelain, two ethylene-propylene-diene monomer (EPDM) and four silicone rubber (SIR) commercially available insulators. The insulators have been energized with 130 kV rms phase-to-ground AC voltage under identical outdoor conditions for more than seven years. The results presented show that under wet and polluted conditions the hydrophilic EPDM rubber insulators develop high leakage currents and substantial arcing. During a typical salt-storm the arcing amplitude of the EPDM rubber insulators is at least twice as high as that ofmore » the porcelain insulator. The SIR insulators, on the other hand, preserve a high degree of hydrophobicity after more than seven years in service and maintain very low leakage currents. However, the results show that during heavy salt contaminated conditions a highly stressed SIR insulator can temporarily lose its hydrophobicity and thereby develop considerable surface arcing.« less
Thermal Insulation Chemical Composition and Method of Manufacture.
conditions in high temperature solid propellant gas generators can be formed of an ethylene propylene, diene monomer ( EPDM )-neoprene rubber binders containing...silica powder filler and aramid fibers. The specific chemical constituents include EPDM elastomer, 2 Chlorobutadiene 1,3 elastomer, Silica hydrate
Surface characterisation of ethylene propylene diene rubber upon exposure to aqueous acidic solution
NASA Astrophysics Data System (ADS)
Mitra, Susanta; Ghanbari-Siahkali, Afshin; Kingshott, Peter; Hvilsted, Søren; Almdal, Kristoffer
2006-07-01
Two types of pure ethylene propylene diene rubbers were exposed to two different acids for varying period of time. Surface characterisation was carried out using X-ray photoelectron spectroscopy (XPS). Two EPDM rubbers selected for this study were comparable in co-monomer compositions but significantly different with respect to molar mass and the presence of long chain branching. Both rubbers contained 5-ethylidene-2-norbornene (ENB) as diene. Solution cast films of pure EPDM samples were exposed in two different acidic solutions, viz. chromosulphuric (Cr (VI)/H 2SO 4) and sulphuric acid (H 2SO 4) (20%, v/v) at ambient temperature from 1 to 12 weeks. XPS analysis indicated that several oxygenated species were formed on the surface of both rubbers after exposure. It was postulated from the XPS analyses that both aqueous acidic solutions attacked the olefinic double bonds (C dbnd C) of ENB. Furthermore, 20% Cr (VI)/H 2SO 4 also attacked the allylic carbon-hydrogen (C sbnd H) bonds of ENB resulting in more oxygenated species on the surface compared to 20% H 2SO 4 under identical conditions. Cr (VI) in the 20% Cr (VI)/H 2SO 4 was found to play an important role in alteration of surface chemistry. Studies using a model system consisting of EPDM mixed with Cr (VI) and Cr (III) salts revealed that the change of oxidation state from Cr (VI) to Cr (III) as a consequence of direct involvement of Cr (VI) in the chemical alteration of EPDM surfaces. Interestingly, the presence of long chain branching and molar mass did not significantly influence the chemical processes owing to the acid treatment.
Silva, Lorena M A; Alves Filho, Elenilson G; Simpson, André J; Monteiro, Marcos R; Cabral, Elaine; Ifa, Demian; Venâncio, Tiago
2017-10-01
Biodiesel has been introduced as an energetic matrix in several countries around the world. However, the affinity of biodiesel with the components of petrodiesel engines is a growing concern. In order to obtain information regarding the effect of biodiesel on the rubber structure, nuclear magnetic resonance technics under a new technology named as comprehensive multiphase (CMP NMR) and the imaging through desorption electrospray ionization mass spectrometry (DESI-MS imaging) were used. The 1 H CMP-DOSY NMR showed the entrapped fuel into the rubber cavities, which the higher constraint caused by the rubber structure is related to the smaller diffusion coefficient. The less affected type of rubber by biodiesel was ethylene-propylene-diene monomer (EPDM), and the most affected was synthetic rubber nitrile (NBR). The 13 C CMP MAS-SPE experiments also confirmed that the internal region of EPDM was less accessible to the biodiesel molecules (no fuels detected) while other rubbers were more susceptible to the penetration of the fuel. DESI-MS imaging revealed for the first time the topography of the rubbers exposed to fuels. The biodiesel molecules entrapped at the EPDM and NBR pores were in oxidized form, which might degrade the rubber structure at long exposure time. The employed technics enabled the study of dynamic and molecular structure of the mixing complex multiphase. The DOSY under CMP used in this study could prove helpful in assessing the interactions throughout all physical phases (liquid, solid, and gel or semi-solid) by observing swellability caused by the fuel in the rubber. In addition, the DESI-MS was especially valuable to detect the degradation products of biodiesel entangled at the rubber structure. In our knowledge, this was the first report in which chemical changes of commercial rubbers induced by biodiesel and petrodiesel were investigated by means of DESI-MS and DOSY NMR. Copyright © 2017 Elsevier B.V. All rights reserved.
NASA Astrophysics Data System (ADS)
Patermann, S.; Altstädt, V.
2014-05-01
Thermoplastic vulcanizates (TPVs) combine the elastic properties of thermoset cross-linked rubbers with the melt processability of thermoplastics. The most representative examples of this class are the TPVs based on polypropylene (PP) and ethylene-propylenediene terpolymer rubber (EPDM). The PP/EPDM blends were produced by dynamic vulcanization in a continuous extrusion process. The influence of different peroxide concentrations was studied with regard to cross-link density, compression set, tensile strength/elongation at break and morphology. With increasing peroxide concentration, the cross-link density increases, leading to a reduction of the compression set by 50 %. The cross-linked blends show smaller dispersed EPDM particles than the uncured one. With a peroxide concentration between 0.2 and 0.6 % a maximum in tensile strength and elongation at break was found and with increasing peroxide concentration, the complex viscosity of the TPVs decreases. Compared to batch processes, the results show nearly the same trends.
Processing and Properties of Fire Resistant EPDM Rubber-Based Ceramifiable Composites
NASA Astrophysics Data System (ADS)
Anyszka, Rafał; Bieliński, Dariusz M.; Pędzich, Zbigniew; Zarzecka-Napierała, Magdalena; Imiela, Mateusz; Rybiński, Przemysław
2017-10-01
Low softening point temperature glassy frit, reinforcing silica, wollastonite and dicumyl peroxide were incorporated into ethylene-propylene-diene (EPDM) rubber matrix in different amounts in order to obtain ceramifiable composites. Kinetics of vulcanization of the mixes was measured. Mechanical properties, micromorphology, thermal properties and combustibility of the vulcanizates were studied as well as compression strength of the ceramic residue obtained after heat treatment. Studies show that optimal amount of glassy frit from the point of view of ceramification effectiveness in dispersed mineral phase is 40 % wt.
Sulfur Mustard Penetration of Thermoplastic Elastomers
2008-10-01
blend of polypropylene and finely dispersed, highly vulcanised EPDM rubber [4]. However its exact composition is a trade secret. The Santoprene grade... rubber or silicone rubber . Compared to thermoplastic elastomers, these thermosetting elastomers are expensive and difficult to process. Therefore a...the last few decades, CBR respirators have generally been manufactured from either butyl rubber (as in the British and Australian S10), or silicone
DOE Office of Scientific and Technical Information (OSTI.GOV)
Gorur, R.S.; Cherney, E.A.; Hackam, R.
1988-07-01
A comparative study of the ac (60 Hz) surface aging in a fog chamber is reported on cylindrical rod samples of high temperature vulcanized (HTV) silicone rubber and ethylene propylene diene monomer (EPDM) rubber containing various amounts of alumina trihydrate (ATH) and/or silica fillers. In low conductivity (250 ..mu..S/cm) fog, silicone rubber performed better than EPDM samples whereas in high conductivity (1000 ..mu..S/cm) fog, the order of performance was reversed. The mechanisms by which fillers impart tracking and erosion resistance to materials is discussed as influenced by the experimental conditions of the accelerated aging tests. Surface studies by ESCA (Electronmore » Spectroscopy for Chemical Analysis) demonstrate that the hydrophobicity of silicone rubber, despite the accumulation of surface contamination, can be attributed to migration of low molecular weight polymer chains and/or mobile fluids, such as silicone oil.« less
FTIR spectra and mechanical strength analysis of some selected rubber derivatives.
Gunasekaran, S; Natarajan, R K; Kala, A
2007-10-01
Rubber materials have wide range of commercial applications such as, infant diapers, famine hygiene products, drug delivery devices and incontinency products such as rubber tubes, tyres, etc. In the present work, studies on mechanical properties of some selected rubber materials viz., natural rubber (NR), styrene butadiene rubber (SBR), nitrile butadiene rubber (NBR) and ethylene propylene diene monomer (EPDM) have been carried out in three states viz., raw, vulcanized and reinforced. To enhance the quality of rubber elastomers, an attempt is made to prepare new elastomers called polyblends. In the present study an attempt is made to blend NR with NBR and with EPDM. We here report, a novel approach for the evaluation of various physico-mechanical properties such as mechanical strength, tensile strength, elongation and hardness. The method is simple, direct and fast and involves infrared spectral measurements for the evaluation of these properties. With the applications of modern infrared spectroscopy, the mechanical strength of these rubber materials have been analyzed by calculating the internal standards among the methyl and methylene group vibrational frequencies obtained from FTIR spectroscopy. Also the tensile strength measurements carried out by universal testing machine. The results pertaining physico-mechanical properties of the rubber derivatives undertaken in the present study obtained by IR-based method are in good agreement with data resulted from the standard methods.
FTIR spectra and mechanical strength analysis of some selected rubber derivatives
NASA Astrophysics Data System (ADS)
Gunasekaran, S.; Natarajan, R. K.; Kala, A.
2007-10-01
Rubber materials have wide range of commercial applications such as, infant diapers, famine hygiene products, drug delivery devices and incontinency products such as rubber tubes, tyres, etc. In the present work, studies on mechanical properties of some selected rubber materials viz., natural rubber (NR), styrene butadiene rubber (SBR), nitrile butadiene rubber (NBR) and ethylene propylene diene monomer (EPDM) have been carried out in three states viz., raw, vulcanized and reinforced. To enhance the quality of rubber elastomers, an attempt is made to prepare new elastomers called polyblends. In the present study an attempt is made to blend NR with NBR and with EPDM. We here report, a novel approach for the evaluation of various physico-mechanical properties such as mechanical strength, tensile strength, elongation and hardness. The method is simple, direct and fast and involves infrared spectral measurements for the evaluation of these properties. With the applications of modern infrared spectroscopy, the mechanical strength of these rubber materials have been analyzed by calculating the internal standards among the methyl and methylene group vibrational frequencies obtained from FTIR spectroscopy. Also the tensile strength measurements carried out by universal testing machine. The results pertaining physico-mechanical properties of the rubber derivatives undertaken in the present study obtained by IR-based method are in good agreement with data resulted from the standard methods.
Effects of simulant mixed waste on EPDM and butyl rubber
DOE Office of Scientific and Technical Information (OSTI.GOV)
Nigrey, P.J.; Dickens, T.G.
1997-11-01
The authors have developed a Chemical Compatibility Testing Program for the evaluation of plastic packaging components which may be used in transporting mixed waste forms. In this program, they have screened 10 plastic materials in four liquid mixed waste simulants. These plastics were butadiene-acrylonitrile copolymer (Nitrile) rubber, cross-linked polyethylene, epichlorohydrin rubber, ethylene-propylene (EPDM) rubber, fluorocarbons (Viton and Kel-F{trademark}), polytetrafluoro-ethylene (Teflon), high-density polyethylene, isobutylene-isoprene copolymer (Butyl) rubber, polypropylene, and styrene-butadiene (SBR) rubber. The selected simulant mixed wastes were (1) an aqueous alkaline mixture of sodium nitrate and sodium nitrite; (2) a chlorinated hydrocarbon mixture; (3) a simulant liquid scintillation fluid; andmore » (4) a mixture of ketones. The screening testing protocol involved exposing the respective materials to approximately 3 kGy of gamma radiation followed by 14-day exposures to the waste simulants at 60 C. The rubber materials or elastomers were tested using Vapor Transport Rate measurements while the liner materials were tested using specific gravity as a metric. The authors have developed a chemical compatibility program for the evaluation of plastic packaging components which may be incorporated in packaging for transporting mixed waste forms. From the data analyses performed to date, they have identified the thermoplastic, polychlorotrifluoroethylene, as having the greatest chemical compatibility after having been exposed to gamma radiation followed by exposure to the Hanford Tank simulant mixed waste. The most striking observation from this study was the poor performance of polytetrafluoroethylene under these conditions. In the evaluation of the two elastomeric materials they have concluded that while both materials exhibit remarkable resistance to these environmental conditions, EPDM has a greater resistance to this corrosive simulant mixed waste.« less
Phase Inversion of EPDM/PP Blends: Effect of Viscosity Ratio
NASA Astrophysics Data System (ADS)
Machado, Ana Vera; Antunes, Carla Filipa; van Duin, Martin
2011-07-01
EPDM/PP blends and TPVs with and without crosslinking, respectively, were prepared, in a batch mixer, using three different EPDM rubbers. EPDM/PP based TPVs were dynamic vulcanised using the resol/SnCl2 system. Samples were collected along the time in order to get information on the morphology evolution and crosslinking density during dynamic vulcanisation. The morphology was studied by SEM and the crosslink density by gel content. In the case of low viscosity EPDMs, crosslinking of the EPDM phase was retarded due to its low crosslinking efficiency. This delay on crosslinking reaction enables the observation of the various stages of the morphological mechanism that takes place during dynamic vulcanisation. It could be observed that phase inversion takes place via lamellar mechanism. More detailed insight on phase inversion mechanism during dynamic vulcanisation was accomplished.
Service Lifetime Estimation of EPDM Rubber Based on Accelerated Aging Tests
NASA Astrophysics Data System (ADS)
Liu, Jie; Li, Xiangbo; Xu, Likun; He, Tao
2017-04-01
Service lifetime of ethylene propylene diene monomer (EPDM) rubber at room temperature (25 °C) was estimated based on accelerated aging tests. The study followed sealing stress loss on compressed cylinder samples by compression stress relaxation methods. The results showed that the cylinder samples of EPDM can quickly reach the physical relaxation equilibrium by using the over-compression method. The non-Arrhenius behavior occurred at the lowest aging temperature. A significant linear relationship was observed between compression set values and normalized stress decay results, and the relationship was not related to the ambient temperature of aging. It was estimated that the sealing stress loss in view of practical application would occur after around 86.8 years at 25 °C. The estimations at 25 °C based on the non-Arrhenius behavior were in agreement with compression set data from storage aging tests in natural environment.
NASA Astrophysics Data System (ADS)
Schwyzer, Olivier; Saenger, Nicole
2016-11-01
The Hydraulic Pressure Machine (HPM) is an energy converter to exploit head differences between 0.5 and 2.5 m in small streams and irrigation canals. Previous investigations show that efficiencies above 60% are possible. Several case studies indicate good continuity for aquatic life (e.g. fish) and bed load for the technology. The technology is described as an economically and ecologically viable option for small scale hydropower generation. Primary goal of this research is to improve the HPM blade design regarding its continuity properties by maintaining good efficiency rates. This is done by modifying the blade tip and testing within a large physical model under laboratory condition. Blade tips from steel (conventional - reference case) and a combination of EPDM rubber and steel as sandwich construction (rubber, steel, rubber - adhesive layered) are tested and compared. Both materials reach similar values for hydraulic efficiency (approx. 58%) and mechanical power output (approx. 220 W). The variation of different gap sizes pointed out the importance of small clearance gaps to reach high efficiencies. For assessing the two blade tip materials regarding continuity for aquatic life, fish dummies were led through the wheel. Analysis of slow motion video of dummies hit by the blade show significant advantages for the EPDM blade tip. The EPDM rubber allows to bend and thus reduces the shock and the probability for cuts on the fish dummy. It was shown that blade tips from EPDM have certain advantages regarding continuity compared to standard blade tips from steel. No compromise regarding energy production had to be made. These results from the HPM can be transferred to breast shot water wheel and may be applied for new and retrofitting projects.
1995-07-01
and a ductile, rubber compound ( EPDM ) utilized in applications requiring flexible insulation. These tests were typically performed in a vacuum or... EPDM ) rt7l materials, as indicated by the "x". In addition to the more common groups, data is included for a relatively new dielectric film (PBO
JPRS Report. Science & Technology: Japan
1987-07-29
for NBR, CR, and EPDM which have been in use, the adoption of fluoric rubber , acrylic rubber , and hydrin rubber attracts attention. Adhesives have... Propeller Analysis, by Shigeru Saito 56 Null-Collision Technique, by Katsuhisa Koura 59 Laminated Carbon Fiber Composite, by Ryuji Ishikawa 60 Flutter...tendency will last in the future. On the contrary, there is a slight decrease in the amount of paint and rubber . The application of ceramics for not
Toxicity of Pyrolysis Gases from Elastomers
NASA Technical Reports Server (NTRS)
Hilado, Carlos J.; Kosola, Kay L.; Solis, Alida N.; Kourtides, Demetrius A.; Parker, John A.
1977-01-01
The toxicity of the pyrolysis gases from six elastomers was investigated. The elastomers were polyisoprene (natural rubber), styrene-butadiene rubber (SBR), ethylene propylene diene terpolymer (EPDM), acrylonitrile rubber, chlorosulfonated polyethylene rubber, and polychloroprene. The rising temperature and fixed temperature programs produced exactly the same rank order of materials based on time to death. Acryltonitrile rubber exhibited the greatest toxicity under these test conditions; carbon monoxide was not found in sufficient concentrations to be the primary cause of death.
A potential utilization of end-of-life tyres as recycled carbon black in EPDM rubber.
Sagar, M; Nibedita, K; Manohar, N; Kumar, K Raj; Suchismita, S; Pradnyesh, A; Reddy, A Babul; Sadiku, E Rotimi; Gupta, U N; Lachit, P; Jayaramudu, J
2018-04-01
End-of-life (EOL) tyres and their decomposition present severe environmental concern due to their resistance to moisture, oxygen, natural degradation, etc. Pyrolysis is considered to be the most effective and sustainable process for recycling, due to its eco-friendly process. The current work studied the effect of recycled carbon black (rCB), obtained from the pyrolysis of EOL tyres, on the properties of ethylene propylene diene rubber (EPDM). The rCB was characterized by scanning electron microscopy (SEM), thermogravimetric analysis (TGA) and chemical methods. rCB was incorporated solely, into a conventional EPDM formulation and also in combination with N550 carbon black. The physico-mechanical properties of the EPDM vulcanizates, before and after aging, were succinctly studied by SEM, TGA, Differential Scanning Calorimetry (DSC), tensile tests and cross-link density. The average particle size of rCB was observed to be 8 µm and the ash content was observed to be higher when compared to the conventional N550 carbon black, which was evident, by the TGA and SEM-EDX analyses. The reinforcing effect and the cross-link density of the rCB-filled vulcanizates were found to be marginally inferior in comparison to the conventional carbon black (N550). The morphology of the tensile- and tear-fractured surfaces were studied by SEM and it was observed that the breaking mechanism follows the rubber chain detachment from the surface mode. Copyright © 2018 Elsevier Ltd. All rights reserved.
NASA Astrophysics Data System (ADS)
Arshad Bashir, M.; Shahid, M.; Ahmed, Riaz; Yahya, A. G.
2014-06-01
In this research paper the effect of blending ratio of natural rubber (NR) with Ethylene Propylene Diene Monomer (EPDM) were investigated. Different samples of EPDM/NR ratio were prepared to study the variation of NR in EPDM on rheology, curing characteristics, tangent δ, and viscosity variation during vulcanization of sponge nano composites.The main aim of present research is to develop elastomeric based sponge composites with the blending ratio of base elastomers along with the carbon nano particles for high energy absorbing and damping applications. The curing characteristics, rheology and viscoelastic nature of the composite is remarkably influenced with the progressive blending ratio of the base elastomeric matrix.
Method for Improving Acoustic Impedance of Epoxy Resins
2010-06-11
neoprene, ethylene propylene diene monomer ( EPDM ) and polyurethane rubbers . Typical applications of these materials encapsulate and protect acoustic...different material (e.g., rubber ) cannot be used. Thus, a hard, strong and acoustically transparent material is needed. Suitable high modulus...epoxy resin. In this method, an epoxy resin component is mixed with a rubber component. The epoxy resin component is preferably a bisphenol A
Air-Inflated Fabric Structures
2006-11-05
environmental exposure to ultraviolet rays, moisture, fire, chemicals, etc. Coating such as urethane, PVC (polyvinyl chloride), neoprene, EPDM (ethylene...tests on rubber -coated, plain-woven fabrics and established that the initial shear response was dominated by the coating and with increased shearing...Farboodmanesh, S., Chen, J., Mead, J. L., White, K., "Effect of Construction on Mechanical Behavior of Fabric Reinforced Rubber ," Rubber Division
Effect of electron beam irradiation on the properties of crosslinked rubbers
NASA Astrophysics Data System (ADS)
Banik, Indranil; Bhowmick, Anil K.
2000-05-01
Influence of electron beam (EB) irradiation on the mechanical and dynamic mechanical properties of crosslinked fluorocarbon (FKM) rubber, natural rubber (NR), ethylene propylene diene monomer (EPDM) rubber and nitrile rubber (NBR) has been investigated. The modulus, gel fraction, glass transition temperature ( Tg) and storage modulus increased, while the elongation at the break and the loss tangent (tan δ) Tg decreased. FKM and NBR vulcanizates have been shown to have EB radiation resistance up to 1500 kGy.
Fabrication of T142 Tank Track Pads for Evaluation of a Rubber-Kevlar Composite Compound
1982-06-01
fully developed with highly saturated rubbers such as butyl or ROYALENE® ( EPDM ) A-3 ...PERIOD COVERED Fabrication of T142 Tank Track Pads for Evaluation of a Rubber -Kevlar Composite FINAL Compound S. PERFORMING ORG. REPORT NUMBER 7. AUTHOR...developed for evaluation in T142 tank track pads. Bonding of the rubber to the fiber was achieved by addition of bonding agents to the compound. 175, T142
Method for Improving Acoustic Impedance of Epoxy Resins
2010-06-21
include neoprene, ethylene propylene diene monomer ( EPDM ) and polyurethane rubbers . Typical applications of these materials encapsulate and protect...a different material (e.g., rubber ) cannot be used. Thus, a hard, strong and acoustically transparent material is needed. Suitable high modulus...an epoxy resin. In this method, an epoxy resin component is mixed with a rubber component. The epoxy resin component is preferably a bisphenol A
Evaluation of some antioxidants in radiation vulcanized ethylene-propylene diene (EPDM) rubber
NASA Astrophysics Data System (ADS)
Abdel-Aziz, M. M.; Basfar, A. A.
2001-12-01
Thermogravimetric analysis (TGA) and differential scanning calorimetry (DSC) have been used to study the oxidation of γ-ray vulcanized ethylene-propylene diene rubber (EPDM) stabilized with various types of antioxidants. The antioxidants used were pentaerythrityl tetrakis(3,5-di-tert-butyl(-4-hydroxyphenyl))propionate (Irganox 1010), Irganox 1035, Irganox 1520D, as primary antioxidants; Irganox B561 and Irganox B900, as synergistic blends; hindered amine light stabilizer (HALS), i.e. Tinuvin 622 LD; N-isopropyl- N-phenyl- p-phenylene diamine (IPPD) and trimethyl quinoline (TMQ) and their mixtures. The measurements were carried out under atmospheric conditions. The effects of antioxidant type and its selected concentration were determined and mechanism of reaction proposed.
Accelerated aging and stabilization of radiation-vulcanized EPDM rubber
NASA Astrophysics Data System (ADS)
Basfar, A. A.; Abdel-Aziz, M. M.; Mofti, S.
2000-03-01
The effect of different antioxidants and their mixtures on the thermal aging and accelerated weathering of γ-radiation vulcanized EPDM rubber in presence of crosslinking coagent, was investigated. The compounds used were either a synergistic blend of phenolic and phosphite antioxidants, i.e. 1:4 Irganox 1076: Irgafos 168 or a blend of arylamine and quinoline type antioxidants, i.e. 1:1 IPPD: TMQ, at fixed concentration. Tinuvin 622 LD hindered amine light stabilized (HALS) was also used. The response was evaluated by the tensile strength and elongation at break for irradiated samples after thermal aging at 100°C for 28 days and accelerated weathering (Xenon test) up to 200 h.
Butyl rubber O-ring seals: Revision of test procedures for stockpile materials
DOE Office of Scientific and Technical Information (OSTI.GOV)
Domeier, L.A.; Wagter, K.R.
1996-12-01
Extensive testing showed little correlation between test slab and O-ring performance. New procedures, comparable to those used with the traditional test slabs, were defined for hardness, compression set, and tensile property testing on sacrificial O-ring specimens. Changes in target performance values were made as needed and were, in one case, tightened to reflect the O-ring performance data. An additional study was carried out on O-ring and slab performance vs cure cycle and showed little sensitivity of material performance to large changes in curing time. Aging and spectra of certain materials indicated that two sets of test slabs from current vendormore » were accidently made from EPDM rather than butyl rubber. Random testing found no O-rings made from EPDM. As a result, and additional spectroscope test will be added to the product acceptance procedures to verify the type of rubber compound used.« less
Synthesis of ethylene-propylene rubber graft copolymers by borane approach
DOE Office of Scientific and Technical Information (OSTI.GOV)
Chung, T.C.; Janvikul, W.; Bernard, R.
1994-01-01
This paper describes a new method to prepare graft copolymers which have an EP rubber backbone and several free radical polymerized polymers grafted thereto. The process involves hydroboration of commercial EPDM rubbers, such as poly(ethylene-co-propylene-co-1,4-hexadiene) and poly(ethylene-co-propylene-co-5-ethylidene-2-norbornene), with 9-borabicyclononane (9-BBN). The resulting secondary alkyl-9-BBN moieties in the EPDM copolymer were then exposed to oxygen in the presence of free radical polymerizable monomers. Under certain conditions, the selective autoxidation reaction of secondary alkyl-9-BBN took place to create desirable polymeric radicals which can in situ initiate free radical polymerization. High graft efficiency was observed with controllable copolymer compositions. The graft copolymer ofmore » EP-g-PMMA is used to show the chemistry as well as some of the physical properties.« less
2012-02-21
Testing and Materials °C Celsius DiEGME Diethylene Glycol Monomethyl Ether EPDM Ethylene Propylene Diene Monomer FARE Forward Area Refueling...urethane class AU, polyether urethane class EU, EPDM , Viton®, fluorosilicone class FQ, polytetrafluoroethylene (PTFE), polyolefin and polyester...sleeve Material not provided AAFARS 4720-00-540-1368 Hose, nonmetallic Material not provided AAFARS 4720-01-218-6958 Hose, preformed Rubber
Development of a Cold Sterilant for Field Medical Use.
1996-11-01
Dental Devices Using STERIS 20C at Use Dilution and Manual Soak Technique .............. 1086 Akron Rubber Development Laboratory Report 32918...simulated reuse protocol with lot P-2 of 25 months of age , a number of positives (i.e. sterilization failures) were noted, in particular for the...Ethylene propylene ELASTOMERS Brass Ethylene propylene diene Ethylene propylene diene ( EPDM ) ( EPDM ) Brass 360 Polyamide RTV 133 Nickel-plated Cooper
Stabilization effects of naringenin and caffeic acid on γ-irradiatedEPDM
NASA Astrophysics Data System (ADS)
Zaharescu, T.; Jipa, S.; Mantsch, A.; Henderson, D.
2013-03-01
The stabilization of ethylene-propylene diene rubber (EPDM) with naringenin and caffeic acid is studied. The selected concentrations were 0.25, 0.50 and 1 phr. The degradation was performed by γ-irradiation. The protective effect of these antioxidants was investigated by isothermal chemiluminescence at 170 °C and FTIR spectroscopy. The synergetic action of these compounds and metallic selenium was also revealed. The exceptional contribution provided by these phenolic stabilizers is characterized by three kinetic parameters: initial CL intensity, oxidation induction time and maximum period of degradation. The radiation stability of stabilized EPDM is efficiently depicted by induction periods which are the minimum 6times longer for unirradiated samples and 2-50 times longer for 50 kGy-irradiated specimens than pristineEPDM.
Ghanbari-Siahkali, Afshin; Almdal, Kristoffer; Kingshott, Peter
2003-12-01
The effects of laser irradiation on changes to the surface chemistry and structure of a commercially available ethylene propylene diene monomer (EPDM) rubber sample after Raman microscopy analysis was investigated. The Raman measurements were carried out with different levels of laser power on the sample, ranging from 4.55 mW to 0.09 mW. The surface of the EPDM was analyzed before and after laser exposure using X-ray photoelectron spectroscopy (XPS) and attenuated total reflectance Fourier transform infrared (ATR-FTIR) spectroscopy. The techniques have surface probe depths of approximately < or = 10 nm and 1 microm, respectively. Both sets of analysis show that ingredients of the blended EPDM rubber "bloom" to the surface as a result of local heating that takes place due to the absorption of laser by carbon black during the Raman analysis. Scanning electron microscopy (SEM) analysis was also performed on the Raman analyzed areas to visually illustrate the effects created due to laser light exposure (i.e., burning marks). The change in surface chemistry also occurs in regions a few millimeters from the exposed sites, indicating that the effect is quite long range. However, this phenomenon has no major influence, as far as XPS or ATR-FTIR results disclose, on the backbone structure of the rubber sample. The results indicate that precautions should be taken when analyzing complex blended polymer samples using Raman spectroscopy.
Surface modification of EPDM rubber by plasma treatment.
Grythe, Kai Frode; Hansen, Finn Knut
2006-07-04
The effect of argon, oxygen, and nitrogen plasma treatment of solvent cast EPDM rubber films has been investigated by means of atomic force microscopy (AFM), X-ray photoelectron spectroscopy (XPS), and surface energy measurements. Plasma treatment leads to changes in the surface energy from 25 to 70 mN/m. Treatment conditions influenced both the changes in surface energy and the stability, and it became more difficult to obtain good contact angle measurements after longer (> ca. 4 min) treatment times, probably because of an increasingly uneven surface structure. XPS analyses revealed that up to 20 at. % oxygen can be easily incorporated and that variations of approximately 5% can be controlled by the plasma conditions. Oxygen was mainly found in hydroxyl groups, but also as carbonyl and carboxyl. XPS analyses showed more stable surfaces than expected from contact angles, probably because XPS analysis is less surface sensitive than contact angle measurements. AFM measurements revealed different surface structures with the three gases. The surface roughness increased generally with treatment time, and dramatic changes could be observed at longer times. At short times, surface energy changes were much faster than the changes in surface structure, showing that plasma treatment conditions can be utilized to tailor both surface energies and surface structure of EPDM rubber.
Effect of heating rate on toxicity of pyrolysis gases from some elastomers
NASA Technical Reports Server (NTRS)
Hilado, C. J.; Kosola, K. L.; Solis, A. N.
1977-01-01
The effect of heating rate on the toxicity of the pyrolysis gases from six elastomers was investigated, using a screening test method. The elastomers were polyisoprene (natural rubber), styrene-butadiene rubber (SBR), ethylene propylene diene terpolymer (EPDM), acrylonitrile rubber, chlorosulfonated polyethylene rubber, and polychloroprene. The rising temperature and fixed temperature programs produced exactly the same rank order of materials based on time to death. Acrylonitrile rubber exhibited the greatest toxicity under these test conditions, and carbon monoxide was not found in sufficient concentrations to be the primary cause of death.
DOE Office of Scientific and Technical Information (OSTI.GOV)
Smith, F. G.; Daniels, E. J.
This report summarizes an assessment conducted by Environmental Technologies Alternatives, Inc., under a subcontract to Argonne National Laboratory. The project was conducted in two phases. An assessment of alternative technologies for recycling of prompt non-tire rubber was conducted in the first phase, and an experimental program focusing on a new technology called the catalytic Regeneration Process offered the greatest opportunity for recovery of high-value recyclable rubber material. An experimental and large-scale test program was undertaken to further delineate the economic potential as an essential step leading to commercial deployment and to determine the course of continued development of the technologymore » by the private sector. The experimental program defined process-operating conditions for the technology and verified the degree of devulcanisation achievable for two rubber compounds: ethylene-propylene-nonconjugated-diene monomer (EPDM) and neoprene. To determine product acceptance, samples of devulcanized EPDM and neoprene were prepared and used in factory trials for the production of automotive moldings (EPDM) and fiber-filled belting (neoprene). The factory trials indicated that the physical properties of the products were acceptable in both cases. The appearance of molded and calendared surface finishes was acceptable, while that of extruded finishes was unsatisfactory. The fiber-filled neoprene belting application offers the greatest economic potential. Process costs were estimated at $0.34/lb for neoprene waste rubber relative to a value of $0.57/lb. The results of the experimental program led to the decision to continue development of this technology is being planned, subject to the availability of about $3 million in financing from private-sector investors. The ability to recycle non-tire rubber scrap could conserve as much as 90,000 Btu/lb, thus yielding an estimated energy savings potential of about 0.25 quad/yr.« less
Constitutive Modeling, Nonlinear Behavior, and the Stress-Optic Law
2011-01-01
estimates of D̂ from dynamic mechanical measurements. Some results are shown in Figure 58 for a filled EPDM rubber [116]. There is rough agreement with...elastomers and filler-reinforced rubber . 5.1 Linearity and the superposition principle The problem of analyzing viscoelastic mechanical behavior is greatly...deformation such as shear. For crosslinked rubber the strain can be defined in terms of the strain function suggested by the statistical theories of
Completely open-foldable domes remaining cool in sunshine
NASA Astrophysics Data System (ADS)
Hammerschlag, Robert H.; Deelen, Sander; Hoogendoorn, Pieter W.; Kommers, Johannes N. M.; Sonner, Thomas; Simoes, Roberto; Grassin, Olivier; Fischer, Andreas; Visser, Simon; Thewissen, Kristof
2016-07-01
These open-foldable very light-weight domes, based on very strong textile membranes highly tensioned between steel bows, are designed for bad-weather protection and maintenance of instruments for astronomical, meteorological and civil-engineering measurements and have extremely high wind stability. The domes of the GREGOR telescope and the Dutch Open Telescope are the two existing prototypes. Improvements were developed with all parts light-colored to remain cool in solar light. The new specially made connection parts (eyes) between the textile parts are made from white-colored PETP, a very strong and UV-stable synthetic, and have a better geometrical shape giving higher stability. The rubber seal tubes on top of the dome were of black-colored chloride rubber CR (neoprene), strong and UV stable, but very warm in sunlight. New UV-stable EPDM rubber tubes were produced in natural light color. To get this rubber stiff enough to give good sealing, a black-colored stiff EPDM rubber is put inside the light-colored one. Tests were performed and the forces necessary for compression of the rubber tubes were measured. An inside black tube with a circa 1.3 times larger compression force than the original black tubes was applied. The assembling of the black tubes into the light-colored tubes was successfully applied at the DOT and GREGOR domes.
Wear Resistant Rubber Tank Track Pads
1975-10-01
began to de- crease significantly during the winter months of 1973-1974. The December 1973 issie of Rubber Age carried the statement that the ready...to tear or abrasion. Because EPDM vulcanizates are inherently ozone resistant and have excellent age resistance, even at temperatures as high as...attempts to improve the tear resistance of this blend would be worthwhile. In an article1--’ appearing in the May 1973 issue of Rubber Age , the intro
Molecular dynamics modelling of mechanical properties of polymers for adaptive aerospace structures
NASA Astrophysics Data System (ADS)
Papanikolaou, Michail; Drikakis, Dimitris; Asproulis, Nikolaos
2015-02-01
The features of adaptive structures depend on the properties of the supporting materials. For example, morphing wing structures require wing skin materials, such as rubbers that can withstand the forces imposed by the internal mechanism while maintaining the required aerodynamic properties of the aircraft. In this study, Molecular Dynamics and Minimization simulations are being used to establish well-equilibrated models of Ethylene-Propylene-Diene Monomer (EPDM) elastomer systems and investigate their mechanical properties.
Peters, R; van Duin, M; Tonoli, D; Kwakkenbos, G; Mengerink, Y; van Benthem, R A T M; de Koster, C G; Schoenmakers, P J; van der Wal, Sj
2008-08-08
The dicumyl-peroxide-initiated addition and combination reactions of mixtures of alkanes (n-octane, n-decane) and alkenes [5,6-dihydrodicyclopentadiene (DCPDH), 5-ethylidene-2-norbornane (ENBH) and 5-vinylidene-2-norbornane (VNBH)] were studied to mimic the peroxide cross-linking reactions of terpolymerised ethylene, propylene and a diene monomer (EPDM). The reaction products of the mixtures were separated by both gas chromatography (GC) and comprehensive two-dimensional gas chromatography (GCxGC). The separated compounds were identified from their mass spectra and their GC and GCxGC elution pattern. Quantification of the various alkyl/alkyl, alkyl/allyl and allyl/allyl combination products shows that allylic-radicals comprise approximately 60% of the substrate radicals formed. The total concentration of the products formed by combination is found to be independent of the concentration and the type of alkene. The total concentration of the products formed by addition to the alkene increases with increasing concentration of alkene. In addition, the total concentration of the formed addition products depends strongly on the type of the alkene used, viz. VNBH>ENBH approximately DCPDH, which is a consequence of differences in steric hindrance of the unsaturation. The peroxide curing efficiency, defined as the number of moles of cross-linked products formed per mol of peroxide, is 173% using 9% (w/w) 5-vinylidene-2-norbornane (VNBH). This indicates that the addition reaction is recurrent. All these findings are consistent with experimental studies on peroxide curing of EPDM rubber. In addition, the present results provide more-detailed structural information, increasing the understanding of the mechanism of peroxide curing of EPDM. The described approach to use low-molecular-weight model compounds followed by GC-mass spectrometry (MS) and GCxGC-MS analysis is proven to be a very powerful tool to study the cross-linking of EPDM.
DOE Office of Scientific and Technical Information (OSTI.GOV)
Morita, Y.; Hagiwara, M.; Kasai, N.
1982-09-01
As a continuation of a series of the studies on the flame and ..gamma..-radiation resistant modification of ethylene-propylene-diene rubber (EPDM), condensed bromoacenaphthylene (con-BACN) as a newly developed flame retardant was synthesized and its effects on the radiation resistance of EPDM were investigated. The radiation resistance evaluated by measuring tensile properties of irradiated sheets of 2 mm thick was found improved greatly by adding con-BACN together with ordinary rubber ingredients but decreased by decabromodiphenylether (DBDPE) that has bromins in aromatic rings as con-BACN. When EPDM sheets of 1 mm thick were irradiated in oxygen at a dose rate of 1 Xmore » 10/sup 5/ rad/h, the weight swelling ratio increased with increasing dose, indicating that oxidative main chain scission is predominant under the irradiation conditions. On the other hand, crosslinking was shown to be predominant in nitrogen. From the results of the swelling experiments with different additives, it was concluded that DBDPE accelerates both the main chain scission in oxygen and the crosslinking in nitrogen. In contrast to this, con-BACN reduced the chain scission in oxygen. This observation was accounted by the assumption that the influence of the oxidative chain scission is partly compensated by the concurrent crosslinking which takes place through additions of con-BACN to substrate polymers even in the presence of oxygen.« less
Greenland Inland Traverse (GrIT): 2010 Mobility Performance and Implications
2011-10-01
solar irradiance were also measured. The right-hand bladder sled (Fig. 5), designated Sled2, had black- rubber covers ( EPDM roofing material) wrapped...CRREL TR-11-16 ix tion only). Sled2 had thin, black- rubber covers over the bladders to in- crease solar gain. Some performance improvement...Pole Station from McMurdo Station, a distance of 1030 miles, using large, rubber -track tractors to haul fuel and cargo over the snow on flexible
Material morphology and electrical resistivity differences in EPDM rubbers.
DOE Office of Scientific and Technical Information (OSTI.GOV)
Yang, Nancy Y. C.; Domeier, Linda A.
2008-03-01
Electrical resistance anomalies noted in EPDM gaskets have been attributed to zinc-enriched surface sublayers, about 10-{micro}m thick, in the sulfur cured rubber material. Gasket over-compression provided the necessary connector pin contact and was also found to cause surprising morphological changes on the gasket surfaces. These included distributions of zinc oxide whiskers in high pressure gasket areas and cone-shaped features rich in zinc, oxygen, and sulfur primarily in low pressure protruding gasket areas. Such whiskers and cones were only found on the pin side of the gaskets in contact with a molded plastic surface and not on the back side inmore » contact with an aluminum surface. The mechanisms by which such features are formed have not yet been defined.« less
NASA Astrophysics Data System (ADS)
Favre, Audrey
Rubber composites are widely used in several engineering fields, such as automotive, and more recently for inflatable dams and other innovative underwater applications. These rubber materials are composed by an elastomeric matrix while the reinforcing phase is a synthetic fabric. Since these components are expected to operate several years in water environment, their durability must be guaranteed. The use of rubber materials immersed in water is not new, in fact, these materials have been studied for almost one century. However, the knowledge on reinforced rubber composites immersed several years in water is still limited. In this work, investigations on reinforced rubbers were carried out in the framework of a research project in partnership with Alstom and Hydro-Quebec. The objective of this study was to identify rubber composites that could be used under water for long periods. Various rubber composites with ethylene-propylene-diene monomer (EPDM), silicone, EPDM/silicone and polychloroprene (Neoprene) matrices reinforced with E-glass fabric were studied. Thus, these materials were exposed to an accelerated ageing at 85 °C underwater for periods varying from 14 to 365 days. For comparison purposes, they were also immersed and aged one year at room temperature (21 °C). The impact of accelerated aging was estimated through three different characterization methods. Scanning electron microscopy (SEM) was first used to assess the quality of fiber-matrix interface. Then, water absorption tests were performed to quantify the rate of water absorption during immersion. Finally the evolution of the mechanical properties was followed by the determination of Young's modulus (E) and ultimate stress (sigmau) using a dedicated traction test. This analysis allowed to point out that the quality of the fiber-matrix interface was the main factor influencing the drop of the mechanical properties and their durability. Moreover, it was noticed that this interface could be improved by using appropriate coupling agent as confirmed by the silicone composite with treated fabric. It was also observed that fiber-matrix interface could be a place where high stresses were localized because of differential swelling leading to an important loss of mechanical properties. The results revealed very different behaviors from one composite to another. The accelerated aging of EPDM/silicone and Neoprene composites led to a rapid diminution of mechanical properties in only 14 days. Conversely, silicone composites showed a 20 % increase of mechanical properties after 75 days of immersion. EPDM composites exhibited an important variability from one sample to another. It can be concluded from this study that composites made from silicone matrix with treated E-glass result in a better durability underwater. Keywords: composite elastomer, accelerated ageing, immersion in the water
2015-06-01
methylphosphonothiolate (VX) through natural latex rubber and neoprene resulting from LVAP tests. 2. The permeation model is used to study the sensitivity of...Styrene–Butadiene– Rubber , Ethylene–Propylene–Diene Terpolymer, and Natural Rubber Versus Hydrocarbons (C8–C16). Macromolecules 1991, 24 (9), 2598–2605...22 14. Harogoppad, S.B.; Aminabhavi, T.M. Diffusion and Sorption of Organic Liquids through Polymer Membranes 2. Neoprene, SBR, EPDM , NBR, and
2007-06-01
Joint At the exit of the expansion tank, a polymeric composition of ethylene-propylene- diene terpolymer ( EPDM ) rubber was used to mate the flange of...The final connection of the detonator was cumbersome for an operator wearing thick butyl rubber gloves. The detonator wire connection was made to a...operators were required to wear PPE, including rubber gloves. The decision was made to transfer the PLC components to outside the VCS. In Phase I, the
Large strain dynamic compression for soft materials using a direct impact experiment
NASA Astrophysics Data System (ADS)
Meenken, T.; Hiermaier, S.
2006-08-01
Measurement of strain rate dependent material data of low density low strength materials like polymeric foams and rubbers still poses challenges of a different kind to the experimental set up. For instance, in conventional Split Hopkinson Pressure Bar tests the impedance mismatch between the bars and the specimen makes strain measurement almost impossible. Application of viscoelastic bars poses new problems with wave dispersion. Also, maximum achievable strains and strain rates depend directly on the bar lengths, resulting in large experimental set ups in order to measure relevant data for automobile crash applications. In this paper a modified SHPB will be presented for testing low impedance materials. High strains can be achieved with nearly constant strain rate. A thin film stress measurement has been applied to the specimen/bar interfaces to investigate the initial sample ring up process. The process of stress homogeneity within the sample was investigated on EPDM and PU rubber.
NASA Astrophysics Data System (ADS)
da Maia, J. V.; Pereira, F. P.; Dutra, J. C. N.; Mello, S. A. C.; Becerra, E. A. O.; Massi, M.; Sobrinho, A. S. da Silva
2013-11-01
The ethylene propylene diene monomer (EPDM) rubber possesses excellent physical/chemical bulk properties, is cost-effective, and has been used in the mechanical and aerospace industry. However, it has an inert surface and needs a surface treatment in order to improve its adhesion properties. Plasma modification is the most accepted technique for surface modification of polymers without affecting the properties of the bulk. In this study, an afterglow microwave plasma reactor was used to generate the plasma species responsible for the EPDM surface modification. The plasma modified surfaces were analyzed by means of contact angle measurement, adhesion tests, attenuated total reflection-infrared spectroscopy, X-ray photoelectron spectroscopy and scanning electron microscopy. Two experimental variables were analyzed: type of the plasma gases and exposure time were considered. The predominant failure mode was adhesive, for long treatment times a mixture of adhesive and cohesive failure can be observed and the best conditions tested there was an increase of the rupture strength of about 27%, that can be associated mainly with the creation of oxygen containing functional groups on the rubber surface (CO, COC and CO) identified by spectroscopic methods. The predominant failure mode was adhesive, for long treatment times a mixture of adhesive and cohesive failure can be observed. In various conditions tested the contact angles easily decreased more than 500%. What can be concluded that high wettability is a necessary condition to obtain good adhesion, but this is not a sufficient condition.
O-Ring Installation for Underwater Components and Applications
1982-04-15
cure is effected and the heat source removed. AGING -- To undergo changes in physical properties with age or lapse of time. AIR CHECKS -- Surface...the use of heat and pressure, resulting in greatly increased strength and elasticity of rubber -like materials. VULCANIZING AGENT -- A material that...Cross Section Dia -- Diameter EP, EPM, EPDM -- Ethylene-Propylene Rubber F or ’F -- Degrees Fahrenheit FED -- Federal Specification FPM -- Fluorocarbon
Sonar Transducer Reliability Improvement Program FY 80.
1980-04-01
transducers has shown that tricresvl Dhosvhate has 2 promise for use where a careful selection of rubber is possible. See Section 2.3. * Information...impedance and are frequently incompatible with the various plastics and rubbers in the transducer. Further research is necessary to find and qualify fill...have excellent or good compatibility with Viton, butyl, chlorobutyl, silicone, and EPDM elastomers. TCP shows marginal compatibility with natural
NASA Astrophysics Data System (ADS)
Patermann, Simone; Altstädt, Volker
2015-05-01
Thermoplastic vulcanizates (TPVs) combine the elastic properties of thermoset cross-linked rubbers with the melt processability of thermoplastics. The most representative examples of this class are the TPVs based on polypropylene (PP) and ethylene-propylene-diene terpolymer rubber (EPDM). The PP/EPDM blends were produced by dynamic vulcanization in a continuous extrusion process. The influence of different crosslinking systems was studied with regard to cross-link density, compression set, tensile strength/elongation at break and morphology. With increasing peroxide concentration, the cross-link density increases, leading to a reduction of the compression set by 50 %. The same improvement is only reachable with twice the concentration of phenolic resin. Only the peroxide cross-linked blends show smaller dispersed EPDM particles with increasing peroxide concentration. With a peroxide concentration between 0.2 and 0.5 wt. %, a maximum in tensile strength and elongation at break was found. For the phenolic resin cross-linked blends, the tensile strength stays almost constant with increasing phenolic resin concentration and the elongation at break shows best results at 0.5 wt. % phenolic resin. Compared to batch processes, the results show different values, but comparable trends.
The ac and dc performance of polymeric insulating materials under accelerated aging in a fog chamber
DOE Office of Scientific and Technical Information (OSTI.GOV)
Gorur, R.S.; Cherney, E.A.; Hackam, R.
1988-10-01
The paper presents the results of the dc performance of polymeric insulating materials in a fog chamber. The materials evaluated in fog produced from low (250 ..mu..S/cm) and high (1000 ..mu..S/cm) conductivity water include cylindrical rod samples of high temperature vulcanized (HTV) silicone rubber and ethylene propylene diene monomer (EPDM) rubber containing various amounts of either alumina trihydrate (ATH) or silica fillers, or both. Comparison is made of material performance obtained with ac which was reported in an earlier study. In both low and high conductivity fog, the time to failure with ac and +dc was very similar, but amore » reduction by a factor of about four was observed in the time to failure with -dc. For both ac and dc, silicone rubber performed better than EPDM samples in low conductivity fog, while the order of performance was reversed in high conductivity fog. A theoretical model to determine the effect of dry band discharges on material is presented. Good agreement of the predicted behavior of materials with the experimental findings is shown.« less
NASA Astrophysics Data System (ADS)
Shoushtari Zadeh Naseri, Aida; Jalali-Arani, Azam
2015-10-01
Rubber blends based on (styrene-butadiene rubber (SBR)/ethylene-propylene-diene monomer (EPDM)) with and without organoclay (OC) were prepared through a melt mixing process. The concentration ratio of the rubber phases (EPDM/SBR; 50/50 wt%) and the amount of the OC were kept constant. The samples were then vulcanized by means of gamma radiation using a Co-60 gamma source as well as sulfur cure system. The effect of absorbed dose on the formation of the crosslinks was confirmed by the Fourier transform infrared spectroscopy (FTIR). The effects of absorbed dose, sulfur cure system and OC on the gel content, and crosslink density were evaluated by the chemical tests. Applying the Charlesby-Pinner equation to estimate the radiation chemical yield, revealed that the use of OC in the blend caused 20% reduction in the degradation/crosslinking ratio. Employing the swelling test data, some thermodynamic parameters were determined. Using field emission scanning electron microscopy (FE-SEM) to investigate microstructure of the samples revealed a more homogeneous structure and also an increase in compatibility of the blend components in the sample cured by the irradiation in comparison to that cured by the sulfur curing system.
2007-08-28
enables high yield integration onto wafers, glass plates, plastic sheets, rubber slabs or other surfaces. As one application example, bottom gate thin... EPDMS 1m2Si ESi 1m2PDMS 23 is the critical strain for buck- ling, epre is the degree of prestrain, k0 and A0 are...Young’s modulus of Si and PDMS. The following values were used to yield the calcualted value of it (i.e., 84 lm): ESi = 160 GPa, EPDMS = 2 MPa, mPDMS
ODC-Free Solvent Implementation Issues for Vulcanized Rubber and Bond Systems
NASA Technical Reports Server (NTRS)
Hodgson, James R.; McCool, Alex (Technical Monitor)
2001-01-01
Thiokol Propulsion has worked extensively to replace 1,1,1-trichloroethane (TCA) with ozone depleting chemicals (ODC)-free solvents for use in the manufacture of the Reusable Solid Rocket Motor (RSRM) for the Space Shuttle Program. As Thiokol has transitioned from sub-scale to full-scale testing and implementation of these new solvents, issues have been discovered which have required special attention. The original intent of Thiokol's solvent replacement strategy was to replace TCA with a single drop-in solvent for all equivalent applications. We have learned that a single candidate does not exist for replacing TCA. Solvent incompatibility with process materials has caused us to seek for niche solvents and/or processing changes that provide an ODC-free solution for special applications. This paper addresses some of the solvent incompatibilities, which have lead to processes changes and possible niche solvent usage. These incompatibilities were discovered during full-scale testing of ODC-free solvents and relate to vulcanized rubber and bond systems in the RSRM. Specifically, the following items are presented: (1) Cure effects of d-limonene based solvents on Silica Filled Ethylene Propylene Diene Monomer (SF-EPDM) rubber. During full-scale test operations, Thiokol discovered that d-limonene (terpene) based solvents inhibit the cure of EPDM rubber. Subsequent testing showed the same issue with Nitrile Butadiene Rubber (NBR). Also discussed are efforts to minimize uncured rubber exposure to solvents; and (2) Cured bond system sensitivity to ODC-free solvents. During full scale testing it was discovered that a natural rubber to steel vulcanized bond could degrade after prolonged exposure to ODC-free solvents. Follow on testing showed that low vapor pressure and residence time seemed to be most likely cause for failure.
Causes and Control of Corrosion in Buried-Conduit Heat Distribution Systems
1991-07-01
rubber , and foamed plastics such as polyurethanic anld phenolic) nominally contain 10 to 500 ppmn soluble chloide.’ Further, insulation can also become...pressure ratings. A maximum P X T limitation exists for all gasket materials. For example, the maximum temperature and pressure ratings for an EPDM ...ethylene propylene diene monomer) rubber material are, respectively, 3() ’F and 150 psi. The material, however, cannot be expected to perform
DOE Office of Scientific and Technical Information (OSTI.GOV)
Vroomen, G.L.M.; Lievens, S.S.; Maes, J.P.
1999-08-01
EPDM (ethylene-propylene rubber) has been used for more than 25 years as the main elastomer in radiator hoses because it offers a well-balanced price/performance ratio in this field of application. Some years ago the automotive and rubber industry became aware of a problem called electrochemical degradation and cracking. Cooling systems broke down due to a typical cracking failure of some radiator hoses. Different test methods were developed to simulate and solve the problem on laboratory scale. The influence of different variables with respect to the electrochemical degradation and cracking. Cooling systems broke down due to a typical cracking failure ofmore » some radiator hoses. Different test methods were developed to simulate and solve the problem on laboratory scale. The influence of different variables with respect to the electrochemical degradation process has been investigated, but until recently the influence of the engine coolant was ignored. Using a test method developed by DSM elastomers, the influence of the composition of the engine coolant as well as of the EPDM composition has now been evaluated. This paper gives an overview of test results with different coolant technologies and offers a plausible explanation of the degradation mechanisms as a function of the elastomer composition.« less
ERIC Educational Resources Information Center
Betker, Edward
1998-01-01
Looks at Ethylene Propylene Diene Terpolymer rubber roof membranes and the potential problems associated with this material's shrinkage. Discusses how long such a roof should perform and issues affecting repair or replacement. Recommends that a building's function be considered in any roofing decision. (RJM)
Investigation of Materials for Ship-to-Shore Low Pressure Steam Hoses.
1977-07-01
t aging results in either softening or hardening of rubber prod u c ts used for tite tube , cover , and adhesion layers of steam l iose~ • In the...preliniinarv evaluation will be available after in-servile use . EPDM rubber is a l s o suitable for the cover of a steam hose ex c e p t where contact... rubber -lined Steam hoses were invi s t ig i ted At t he present si, itc 01 the art , the average lift for a steam hose is about (t mont hs to one
Hot air vulcanization of rubber profiles
DOE Office of Scientific and Technical Information (OSTI.GOV)
Gerlach, J.
1995-07-01
Elastomer profiles are deployed in quantity by the automobile industry as seals and wateproofing in coachwork. The high standards demanded by the industry; improvement in weather prediction, noise reduction, restriction of tolerances, together with powerful demand for EPDM force the rubber processing industry into development, particularly of elastomers. Complex proofing systems must also be achieved with extremely complicated profile forms. All too often such profiles have an extremely large surface together with a low cross-section density. They frequently consist of two or three rubber compounds and are steel reinforced. Sometimes they are flocked and coated with a low friction finish.more » Such high-tech seals require an adjustment of the vulcanization method. The consistent trend in the nineties towards lower quantities of elastomer per sealing unit and the dielectric factor, especially with EPDM, has brought an old fashioned vulcanization method once more to the fore, a method developed over the past years to an extremely high standard, namely the hot-air method. This paper describes various vulcanization and curing methods and their relative merits and disadvantages, the Gerlach hot-air concept, the hot air installation concept, and energy saving and efficiency afforded by this technique. 4 figs.« less
NASA Astrophysics Data System (ADS)
Feng, Wenlai
This is a study of the continuous ultrasound aided extrusion process for the in-situ compatibilization of isotactic polypropylene (iPP)/ethylene-propylene diene rubber (EPDM) thermoplastic elastomer (TPE) using a newly developed ultrasonic treatment reactor. The rheological, mechanical properties and morphology of the TPE with and without ultrasonic treatment were studied. In-situ compatibilization in the ultrasonically treated blends was observed as evident by their more stable morphology after annealing, improved mechanical properties and IR spectra. The obtained results indicated that ultrasonic treatment induced the thermo-mechanical degradations and led to the possibility of enhanced molecular transport and chemical reactions at the interfaces. Processing conditions were established for enhanced in situ compatibilization of the PP/EPDM TPE. The ultrasonic treatments of butyl rubber gum and ultrasonic devulcanization of butyl rubber, tire-curing bladder during extrusion using a grooved barrel ultrasonic reactor were carried out. The ultrasonic treatment of gum caused degradation of the polymer main chain leading to lower molecular weight, broader molecular weight distribution, less unsaturation and changes in physical properties. The devulcanization of butyl rubber was successfully accomplished only at severe conditions of ultrasonic treatment. The mechanical properties of vulcanizates prepared from devulcanized butyl rubber are comparable to that of the virgin vulcanizate. The molecular characterization of sol fraction of devulcanized butyl rubber showed the devulcanization and degradation of butyl rubber occurred simultaneously. 1H NMR transverse relaxation was also used to study butyl rubber gum before and after ultrasonic treatment, and ultrasonically devulcanized unfilled butyl rubber. The T2 relaxation decays were successfully described using a two-component model. The recyclability of tire-curing bladder was also investigated. Gel fraction, crosslink density, cure behavior, dynamic properties and mechanical properties were measured. Good mechanical properties of revulcanized rubber were achieved by blending devulcanized rubber with the carbon black filled virgin butyl rubber. The structural characteristics of devulcanized butyl rubber were simulated using the Dobson-Gordon theory of rubber network statistics. A fairly good agreement between experimental data and theoretical prediction on normalized gel fraction vs. normalized crosslink density was achieved. The simulation of devulcanized butyl rubber indicated that the rate of crosslink rupture is much higher than that of the main chain.
Chen, Yukun; Xu, Chuanhui; Liang, Xingquan; Cao, Liming
2013-09-12
This work demonstrates an approach of in situ reactive compatibilization between polypropylene (PP) and ethylene-propylene-diene monomer (EPDM) by using zinc dimethacrylate (ZDMA) as a compatibilizer and, simultaneously, as a very strong reinforcing agent. With the incorporation of 7phr ZDMA in the PP/EPDM (30/70, w/w) thermoplastic vulcanizate (TPV), the tensile strength, tear strength, elongation at break, and hardness of PP/EPDM/ZDMA TPV were increased from 5.3 MPa, 31.3 kN/m, 222%, and 78 up to 11.2 MPa, 64.2 kN/m, 396%, and 83, respectively. This tremendous reinforcing as well as the compatibilization effect of the ZDMA was understood by polymerization of ZDMA and ZDMA reacted with EPDM and PP during peroxide-induced dynamic vulcanization. A peculiar phase structure that rubber particles were surrounded and "bonded" by a thick transition zone that contained numerous of nanoparticles with dimensions of about 20-30 nm was observed from transmission electron microscopy. Scanning electron microscopy results confirmed that incorporation of ZDMA reduced the size of the cross-linked EPDM particles. Moreover, we found that the compatibilized TPV showed a higher tan δ peak temperature for EPDM phase and a lower tan δ peak temperature for PP phase. The suggested method for in situ reactive compatibilization of PP and EPDM offers routes to the design of new TPV-based technical products for diversified applications.
2016-09-30
4 of 42 Figure 9. Left: Schematic representation of the gas -gun experiment and a typical speckle pattern the specimen surface, the 12...12 correlation window used in subsequent analysis is also indicated (red rectangle). Right: a photograph of the gas -gun system...20 Figure 11. Left: Averaged acceleration and strain rate and history of μ and α prediction from gas -gun experiment on an EPDM specimen
Effect of polyfunctional monomers on properties of radiation crosslinked EPDM/waste tire dust blend
NASA Astrophysics Data System (ADS)
Yasin, Tariq; Khan, Sajid; Nho, Young-Chang; Ahmad, Rashid
2012-04-01
In this study, waste tire dust is recycled as filler and blended with ethylene-propylene diene monomer (EPDM) rubber. Three different polyfuntional monomers (PFMs) are incorporated into the standard formulation and irradiated under electron beam at different doses up to maximum of 100 kGy. The combined effects of PFMs and absorbed dose on the physical properties of EPDM/WTD blend are measured and compared with sulfur crosslinked formulation. Thermogravimetric analysis showed that radiation developed better crosslinked network with higher thermal stability than sulfur crosslinked structure. The physical properties of radiation crosslinked blend are similar to the sulfur crosslinked blend. The absence of toxic chemicals/additives in radiation crosslinked blends made them an ideal candidate for many applications such as roof sealing sheets, water retention pond, playground mat, sealing profile for windows etc.
A low-cost efficient and durable low-temperature solar collector
NASA Astrophysics Data System (ADS)
Odonnell, T. P.
The considered collector utilizes a material made of ethylene-propylene-diene-monomer (EPDM). This material has been used in solar systems to heat domestic water, pools, spas, and homes by radiant energy. EPDM or ethylene propylene rubber compounds are synthetic elastomers. EPDM elastomers combine superior ozone, good heat and oxygen resistance, and very good low temperature properties to produce a compound with excellent overall age resistance. The material is extruded into 4.4 inch wide mats. Each mat has six small tubes alternating with thin webbing. The absorber mat will adhere to any clean building surface with the use of thermosetting construction-grade mastic adhesive. Carbon black contained in the mat material acts to increase the solar absorptivity. Their low cost makes the elastomers commercially very attractive. The efficiency and durability of the material are discussed.
2016-06-01
Membranes .2. Neoprene, SBR, EPDM , NBR, and Natural- Rubber Versus Normal-Alkanes. J. Appl. Polym. Sci. 1991, 42 (8), 2329–2336. 24. Harogoppad, S.B...highly absorptive (e.g., tire rubber ). Absorptive materials are often more challenging to decontaminate because of the reduced accessibility of the...then aged for 60 min. During the aging period, agent mass was absorbed by a flux-based process.7 The agent-contaminated area of the panel may affect
Effect of gamma irradiation on ethylene propylene diene terpolymer rubber composites
NASA Astrophysics Data System (ADS)
Abou Zeid, M. M.; Rabie, S. T.; Nada, A. A.; Khalil, A. M.; Hilal, R. H.
2008-01-01
Composites of ethylene propylene dine terpolymer rubber (EPDM), high density polyethylene (HDPE) and ground tire rubber powder (GTR) at different ratios were subjected to gamma irradiation at various doses up to 250 kGy. The physical, mechanical and thermal properties were investigated as a function of irradiation dose and blend composition. Gamma irradiation led to a significant improvement in the properties for all blend compositions. The results indicate that the improvement in properties is inversely proportional to the substituted ratio of GTR, attributed to the development of an interfacial adhesion between GTR and blend components. The results were confirmed by examining the fracture surfaces by scanning electron microscopy.
An Integrated Inherent Optical Property Sensor for AUVs
2007-09-30
handling and installation into compact platforms. Previous hard plastic shields were replaced with an EPDM foam rubber tube that slips over the laser...Schofield, O., J. Kohut, J. Kerfoot, L. Creed, C. Mugdal, S. Glenn, M. Twardowski, C. Jones, and D. Webb. 2004. Dawn in the age of ocean robots: what
Mayele, M; Oellrich, L R
2004-03-01
In order to evaluate the suitability of a polymer as a sealing material for certain working fluids used in process plants, information about the fluid diffusivity into the polymer or the polymer permeability to the fluid is a prerequisite. The fluid of interest in the present work is 1,1,1,2-tetrafluorethane, CH(2)FCF(3), a partly fluorinated hydrocarbon (HFC) commonly known as refrigerant R134a. HFCs are increasingly used in refrigeration, air conditioning, and heat pump applications as substitutes for the chlorofluorocarbons (CFCs) or hydrochlorofluorocarbons (HCFCs) that are believed to be responsible for ozone depletion in the stratosphere. The polymers studied were FPM, a perfluoroelastomer, and EPDM, an ethylene-propylene-diene rubber. The study was carried out using magnetic resonance imaging (MRI). The contact time dependence of diffusion of the fluid into the polymer, as well as the spatial distributions of spin-lattice, T(1), and spin-spin, T(2), relaxation times, were used as indicators of the influence of the EPDM matrix on the mobility of R134a molecules.
Chemical compatibility screening test results
DOE Office of Scientific and Technical Information (OSTI.GOV)
Nigrey, P.J.; Dickens, T.G.
1997-12-01
A program for evaluating packaging components that may be used in transporting mixed-waste forms has been developed and the first phase has been completed. This effort involved the screening of ten plastic materials in four simulant mixed-waste types. These plastics were butadiene-acrylonitrile copolymer rubber, cross-linked polyethylene (XLPE), epichlorohydrin rubber, ethylene-propylene rubber (EPDM), fluorocarbon (Viton or Kel-F), polytetrafluoroethylene, high-density polyethylene (HDPE), isobutylene-isoprene copolymer rubber (butyl), polypropylene, and styrene-butadiene rubber (SBR). The selected simulant mixed wastes were (1) an aqueous alkaline mixture of sodium nitrate and sodium nitrite; (2) a chlorinated hydrocarbon mixture; (3) a simulant liquid scintillation fluid; and (4) amore » mixture of ketones. The testing protocol involved exposing the respective materials to 286,000 rads of gamma radiation followed by 14-day exposures to the waste types at 60{degrees}C. The seal materials were tested using vapor transport rate (VTR) measurements while the liner materials were tested using specific gravity as a metric. For these tests, a screening criterion of 0.9 g/hr/m{sup 2} for VTR and a specific gravity change of 10% was used. Based on this work, it was concluded that while all seal materials passed exposure to the aqueous simulant mixed waste, EPDM and SBR had the lowest VTRs. In the chlorinated hydrocarbon simulant mixed waste, only Viton passed the screening tests. In both the simulant scintillation fluid mixed waste and the ketone mixture simulant mixed waste, none of the seal materials met the screening criteria. For specific gravity testing of liner materials, the data showed that while all materials with the exception of polypropylene passed the screening criteria, Kel-F, HDPE, and XLPE offered the greatest resistance to the combination of radiation and chemicals.« less
NASA Astrophysics Data System (ADS)
Arib Rejab, M. N.; Shukor, S. A. Abdul; Sofian, M. R. Mohd; Inayat-Hussain, J. I.; Nazirah, A.; Asyraf, I.
2017-10-01
This paper presents the results of an experimental work to determine the dynamic stiffness and loss factor of elastomeric mounts. It also presents the results of theoretical analysis to determine the transmissibility and vibration power flow of these mounts, which are associated with their contribution to structure-borne noise. Four types of elastomeric mounts were considered, where three of them were made from green natural rubber material (SMR CV60, Ekoprena and Pureprena) and one made from petroleum based synthetic rubber (EPDM). In order to determine the dynamic stiffness and loss factor of these elastomeric mounts, dynamic tests were conducted using MTS 830 Elastomer Test System. Dynamic stiffness and loss factor of these mounts were measured for a range of frequency between 5 Hz and 150 Hz, and with a dynamic amplitude of 0.2 mm (p-p). The transmissibility and vibration power flow were determined based on a simple 2-Degree-of-Freedom model representing a vibration isolation system with a flexible receiver. This model reprsents the three main parts of a vehicle, which are the powertrain and engine mounting, the flexible structure and the floor of the vehicle. The results revealed that synthetic rubber (EPDM) was only effective at high frequency region. Natural rubber (Ekoprena), on the other hand, was found to be effective at both low and high frequency regions due to its low transmissibility at resonant frequency and its ability to damp the resonance. The estimated structure-borne noise emission showed that Ekoprena has a lower contribution to structure-borne noise as compared to the other types of elastomeric mounts.
Aluas, Mihaela; Filip, Claudiu
2005-05-01
A novel approach for solid-state NMR characterization of cross-linking in polymer blends from the analysis of (1)H-(13)C polarization transfer dynamics is introduced. It extends the model of residual dipolar couplings under permanent cross-linking, typically used to describe (1)H transverse relaxation techniques, by considering a more realistic distribution of the order parameter along a polymer chain in rubbers. Based on a systematic numerical analysis, the extended model was shown to accurately reproduce all the characteristic features of the cross-polarization curves measured on such materials. This is particularly important for investigating blends of great technological potential, like thermoplastic elastomers, where (13)C high-resolution techniques, such as CP-MAS, are indispensable to selectively investigate structural and dynamical properties of the desired component. The validity of the new approach was demonstrated using the example of the CP build-up curves measured on a well resolved EPDM resonance line in a series of EPDM/PP blends.
NASA Astrophysics Data System (ADS)
Shokoohi, Shirin
2015-11-01
Polypropylene (PP)/polyamide6 (PA6)/ethylene propylene diene rubber (EPDM) (70/15/15) ternary polymer blends compatibilized with maleic anhydride-grafted EPDM (EPDM-g-MA) were prepared under various processing parameters (barrel temperature, screw speed, and blending sequence). Thermal studies on the prepared blend samples were carried out using differential scanning calorimetry and dynamic mechanical thermal analysis. According to the results, heterogeneous nucleation phenomenon was observed due to the solidification of the PA6 particles dispersed within the PP melt leading to a significant increase in the crystallinity degree and exotherm crystallization peak temperature of PP compared to the pure homopolymer. This was suppressed in the samples with core-shell morphology due to the reduced PP/PA6 interfacial contact. Fractionated crystallization was observed when PA6 droplets dispersed too fine within the matrix (in this case bar{d}_M˜ 0.3 \\upmu {m}). Scanning electron microscopy micrographs were consistent with the melting and crystallization behavior of the blend samples.
NASA Astrophysics Data System (ADS)
Rivaton, A.; Cambon, S.; Gardette, J.-L.
2005-01-01
This paper is devoted to the identification and quantification of the main chemical changes resulting from the radiochemical ageing under oxygen atmosphere of ethylene-propylene-diene monomer (EPDM) and ethylene-propylene rubber (EPR) films containing the same molar ratio of ethylene/propylene. IR and UV-Vis analysis showed that radiooxidation produces a complex mixture of different products and provokes the consumption of the diene double bond. The radiochemical yields of formation of ketones, carboxylic acids, hydroperoxides and alcohols were determined by combining IR analysis with derivatisation reactions and chemical titration. The contributions of secondary and tertiary structures of these two types of -OH groups were separated. Esters and γ-lactones were formed in low concentration. The oxidation products distribution in irradiated films was determined by micro-FTIR spectroscopy. Crosslinking was evaluated by gel fraction methods. In complement, the gas phase composition was analysed by mass spectrometry.
DOE Office of Scientific and Technical Information (OSTI.GOV)
Hay, M.G.; Baron, J.J.; Moffat, T.A.
1996-08-01
Types S31600 and S31254 stainless steel heat exchanger plates have suffered crevice corrosion and stress corrosion cracking under gaskets in rich amine service in a sour gas plant. The gasket material, ethylene-propylene-diene monomer (EPDM), has been used successfully for many years at other sour gas plants. Laboratory testing has duplicated the corrosion observed and shown that the mechanism is synergistic sulfide-halide attack. The use of a bromine plus chlorine-activated curing system for the EPDM rubber gaskets provided the necessary halides. Laboratory testing identified some nickel-based superalloys which were resistant to this corrosion and also demonstrated that essentially halogen-free, peroxide-cured EPDMmore » gaskets do not cause attack of S31600 or S31254. The heat exchanger packs were replaced with S31600 plates and peroxide-cured EPDM gaskets having a specified total halogen concentration of 200 ppm maximum. Field operating experience has been excellent.« less
An experimental study of the PTC properties of polymers with carbon black fillers
NASA Astrophysics Data System (ADS)
Lin, Jianlian
The Positive Temperature Coefficient (PTC) phenomenon, first discovered by Harman in 1957, is defined as the sharp increase of the electrical resistivity of the material with temperature, especially at the Curie transition temperature. Polymeric PTC materials have been widely used since 1975 as self-regulating components, over current or over heat protectors, sensors, etc. In this project a detailed study of polymeric PTC materials has been carried out. Polymeric PTC materials consist of a non-conducting polymeric phase in which conductive particles, such as CB's, are added. Previously most of the studies of the polymer matrices of PTC materials were limited to single component semi-crystalline polymers, such as HDPE, LDPE, EVA etc. In this work, the PTC effects of carbon black filled binary polymer blends, such as LDPE/EPDM, HDPD/EPDM, HDPE/EVA, etc. are mainly studied. For the LDPE/EPDM/CB system, it is found that the PTC intensity of the blends after gamma-ray irradiation increases by almost 5 orders of magnitude compared with that of irradiated LDPE/CB compound. This increase in PTC intensity is due to the greater thermal expansion coefficient of the rubber (EPDM) phase. In addition, a comparison of E-beam and gamma-ray irradiation is made and the resulting effect on the PTC properties of LDPE/EPDM/CB blends is studied in detail. It is found that with higher dose of gamma-ray, the material undergoes significant radiation damage, while irradiation with E-beam prevents radiation damage due to shorter exposure time. The influence of using treated carbon blacks on the PTC/NTC effects of the composites is also studied. The polymer blends filled with oxidized carbon black display higher PTC intensity followed by a weaker NTC effect, which is due to stronger interactions between oxidized CB's & polymer. It is concluded that strong interactions between polymers and fillers suppress the NTC effect. Finally ESR analysis is used to study the interactions between the polymer blends and fillers. It is found that relatively high structure CB's (CSF-III) have a strong interaction with the polymer blend. Based on all the work done, it is concluded that a blend of high polymer with a crystalline rubber filled with relatively high structure carbon blacks that is irradiated by E-beam will be a good polymer PTC material.
DOE Office of Scientific and Technical Information (OSTI.GOV)
Nigrey, P.J.; Dickens, T.G.; Dickman, P.T.
1997-08-01
Based on regulatory requirements for Type A and B radioactive material packaging, a Testing Program was developed to evaluate the effects of mixed wastes on plastic materials which could be used as liners and seals in transportation containers. The plastics evaluated in this program were butadiene-acrylonitrile copolymer (Nitrile rubber), cross-linked polyethylene, epichlorohydrin, ethylene-propylene rubber (EPDM), fluorocarbons, high-density polyethylene (HDPE), butyl rubber, polypropylene, polytetrafluoroethylene, and styrene-butadiene rubber (SBR). These plastics were first screened in four simulant mixed wastes. The liner materials were screened using specific gravity measurements and seal materials by vapor transport rate (VTR) measurements. For the screening of linermore » materials, Kel-F, HDPE, and XLPE were found to offer the greatest resistance to the combination of radiation and chemicals. The tests also indicated that while all seal materials passed exposure to the aqueous simulant mixed waste, EPDM and SBR had the lowest VTRs. In the chlorinated hydrocarbon simulant mixed waste, only Viton passed the screening tests. In both the simulant scintillation fluid mixed waste and the ketone mixture waste, none of the seal materials met the screening criteria. Those materials which passed the screening tests were subjected to further comprehensive testing in each of the simulant wastes. The materials were exposed to four different radiation doses followed by exposure to a simulant mixed waste at three temperatures and four different exposure times (7, 14, 28, 180 days). Materials were tested by measuring specific gravity, dimensional, hardness, stress cracking, VTR, compression set, and tensile properties. The second phase of this Testing Program involving the comprehensive testing of plastic liner has been completed and for seal materials is currently in progress.« less
CBR/TIC Filter Design and Evaluation
2006-12-29
CBR/TIC Filters Aged CK Filter Life Predicitions.................................................................. 29 Figure 30. CBR/TIC Filters...potting adhesive. Neoprene rubber face gaskets are adhered to each end of the particulate filter for airtight sealing. Figure 16. CBR/TIC HEPA...attached with adhesive to the bottom end cover and is spaced by the compression pads on the top end. EPDM foam compression pads are placed on top
NASA Astrophysics Data System (ADS)
Dubey, K. A.; Bhardwaj, Y. K.; Chaudhari, C. V.; Kumar, Virendra; Goel, N. K.; Sabharwal, S.
2009-03-01
Blends of polychloroprene rubber (PCR) and ethylene propylene diene terpolymer rubber (EPDM) of different compositions were made and exposed to different gamma radiation doses. The radiation sensitivity and radiation vulcanization efficiency of blends was estimated by gel-content analysis, Charlesby-Pinner parameter determination and crosslinking density measurements. Gamma radiation induced crosslinking was most efficient for EPDM ( p0/ q0 ˜ 0.08), whereas it was the lowest for blends containing 40% PCR ( p0/ q0 ˜ 0.34). The vulcanized blends were characterized for solvent diffusion characteristics by following the swelling dynamics. Blends with higher PCR content showed anomalous swelling. The sorption and permeability of the solvent were not strictly in accordance with each other and the extent of variation in two parameters was found to be a function of blend composition. The Δ G values for solvent diffusion were in the range -2.97 to -9.58 kJ/mol and indicated thermodynamically favorable sorption for all blends. These results were corroborated by dynamic swelling, experimental as well as simulated profiles and have been explained on the basis of correlation between crosslinking density, diffusion kinetics, thermodynamic parameters and polymer-polymer interaction parameter.
The surface modification of clay particles by RF plasma technique
NASA Astrophysics Data System (ADS)
Lee, Sang-Keol
In this study, the surface coatings of ball clay, organoclay and exfoliated clay prepared by sol-gel process were done by RF plasma polymerization to improve the surface activity of the clay filler. Characterization of the above plasma-treated clays has been carried out by various techniques. The effects of plasma-treated clays as substitute of carbon black in styrene-butadiene rubber (SBR) and ethylene-propylene-diene monomer (EPDM) on the curing and mechanical properties were investigated. After plasma treatment, the tensile properties of organo and exfoliated clay were not unsatisfactory to that of carbon black filler system. Moreover, only 10 phr filler loading of plasma-treated organoclay in EPDM vulcanizates showed better results than 40 phr filler loading of carbon black in EPDM vulcanizates. The main objective of this study was to verify the applicability of the plasma technique for modifying clay surfaces for their use in the tire manufacturing industry. Another purpose was to reveal the advantage of the plasma technique used to obtain modified-clay and improved properties that those materials can display.
Morphology and viscoelastic properties of sealing materials based on EPDM rubber.
Milić, J; Aroguz, A; Budinski-Simendić, J; Radicević, R; Prendzov, S
2008-12-01
In this applicative study, the ratio of active and inactive filler loadings was the prime factor for determining the dynamic-mechanical behaviour of ethylene-propylene-diene monomer rubbers. Scanning electron microscopy was used to study the structure of reinforced dense and microcellular elastomeric materials. The effects of filler and blowing agent content on the morphology of composites were investigated. Microcellular samples cured in salt bath show smaller cells and uniform cell size compared with samples cured in hot air. Dynamic-mechanical thermal analysis showed appreciable changes in the viscoelastic properties by increasing active filler content, which could enable tailoring the material properties to suit sealing applications.
Study of EPDM/PP polymeric blends: mechanical behavior and effects of compatibilization
NASA Astrophysics Data System (ADS)
Bouchart, Vanessa; Bhatnagar, N.; Brieu, Mathias; Ghosh, A. K.; Kondo, Djimedo
2008-09-01
A blend of Ethylene Propylene Diene Monomer (EPDM) rubber reinforced by polypropylene (PP) particles has been processed and its hyperelastic behavior has been characterized under cyclic uni-axial tensile tests. The experimental results show a significant effect of the fraction of polypropylene particles (10%, 25% and 30% by weight). Moreover, from another series of tests conducted on materials containing compatibilizers at different mass concentration, it is observed that the introduction of a compatibilizer increases the rigidity of the blends and affects notably their macroscopic behavior. These observations are interpreted as a consequence of the modification at microlevel of adherence between particles and matrix phases. The use of a nonlinear micromechanical model allows us to confirm this interpretation. To cite this article: V. Bouchart et al., C. R. Mecanique 336 (2008).
Containment penetration elastomer seal leak rate tests
DOE Office of Scientific and Technical Information (OSTI.GOV)
Bridges, T.L.
1987-07-01
Tests were performed on three elastomer seal designs commonly used for nuclear plant containment mechanical penetrations. The objective of this research project is to obtain an understanding of the integrity and leakage behavior of these seal designs under severe accident temperature and pressure conditions. The three designs tested and the seal materials used in the tests were: (1) double tongue-and-groove design with silicone rubber seals, (2) double-O-ring design with neoprene and ethylene-propylene (EPDM) seals, and (3) double gumdrop design with neoprene and EPDM seals. The effects of thermal aging and angular rotations of flange mating surfaces were determined. The testmore » results provide information required to characterize the leakage behavior of penetrations under severe accident conditions. 3 refs., 10 figs., 12 tabs.« less
Sonar Transducer Reliability Improvement Program (STRIP)
1981-01-01
Fair *[51] EPDM NORDOL 1370 - Poor *[511 NATURAL 1155- Poor *[51] NITRILE 6100 - Good *[51] VITON CTBN (BF635075) - Poor *[511 CORK- RUBBER ... aging problems have been found. A report entitled "Reliability and Service Life Concepts for Sonar Transducer Applications" has been completed. - A draft...or aging problems have been found. See Section 9. * A report entitled "Reliability and Service Life Concepts for Sonar Transducer Applications" has
1992-01-30
Chemical Agent Resistant Coating, retractable nylon handles, ethylene propylenediene monomer ( EPDM ) rubber securing straps, and a woven monofilament...Polypropylene Honeycomb 19 Saran Honeycomb 22 4. Mattress fabric: 5laobcbe 29!, 10.6 oz/sq yd, Source: Herculite Products, Inc., York, PA UI r Q r W&de k ( Ag
(Heat utilization at a commercial laundramat)
DOE Office of Scientific and Technical Information (OSTI.GOV)
Not Available
1985-01-01
An EPDM rubber tube mat (trade name - Sola Roll) was used as a heat exchanger to trap heat being vented through the dryer exhaust pipes at the Friendship St. Laundramat. Results of studies are presented. A savings of 54.4% on fuel oil usage was obtained during a full year's trial of the system. The waste heat was used to heat water for the washing machines. 5 figs., 1 tab. (DMC)
Wave Absorber with Fine Weatherability for Improving ETC Environment
NASA Astrophysics Data System (ADS)
Miura, Yu; Matsumoto, Kouta; Okada, Osamu; Hashimoto, Osamu
Wave absorber of rubber sheet containing natural rubber and EPDM is designed, fabricated and measured for improving ETC environment. As a result, proposed absorption material has fine weatherability and wave absorption satisfied with ETC standard can be realized theoretically before and after the weatherability test if the thickness of absorber is fabricated at the ranging from 2.26mm to 2.52mm. Moreover, absorber sheet sample based on theoretical values is fabricated and are measured. As a result, 20dB or more is also confirmed at the incident angle ranging from 5 to 55 degrees experimentally. Therefore, the wave absorber with fine weatherability being satisfied with ETC standard can be realized.
Deuterium permeation through EPDM rubber compounds
DOE Office of Scientific and Technical Information (OSTI.GOV)
Zapp, P.E.
1988-01-01
The permeation of deuterium through a specially formulated compound of ethylene propylene diene rubber was measured in the temperature range of 26/degree/C to 120/degree/C. The results were similar to permeation through two commercial compounds of this elastomer. Permeation was reduced after gamma irradiation (in the presence of hydrogen gas to simulate a tritium exposure). However the reduction was smaller than that experienced by the two commercial compounds. Radiation damage is apparently less severe in the special compound. It is possible that mechanical properties such as compression set may be influenced less by ionizing radiation in this compound as compared withmore » the commercial compounds. 4 figs., 1 tab.« less
The Preparation and Properties of Thermo-reversibly Cross-linked Rubber Via Diels-Alder Chemistry.
Polgar, Lorenzo Massimo; van Duin, Martin; Picchioni, Francesco
2016-08-25
A method for using Diels Alder thermo-reversible chemistry as cross-linking tool for rubber products is demonstrated. In this work, a commercial ethylene-propylene rubber, grafted with maleic anhydride, is thermo-reversibly cross-linked in two steps. The pending anhydride moieties are first modified with furfurylamine to graft furan groups to the rubber backbone. These pendant furan groups are then cross-linked with a bis-maleimide via a Diels-Alder coupling reaction. Both reactions can be performed under a broad range of experimental conditions and can easily be applied on a large scale. The material properties of the resulting Diels-Alder cross-linked rubbers are similar to a peroxide-cured ethylene/propylene/diene rubber (EPDM) reference. The cross-links break at elevated temperatures (> 150 °C) via the retro-Diels-Alder reaction and can be reformed by thermal annealing at lower temperatures (50-70 °C). Reversibility of the system was proven with infrared spectroscopy, solubility tests and mechanical properties. Recyclability of the material was also shown in a practical way, i.e., by cutting a cross-linked sample into small parts and compression molding them into new samples displaying comparable mechanical properties, which is not possible for conventionally cross-linked rubbers.
Surface-and bulk-properties of EPDM rubber modified by electron beam irradiation
NASA Astrophysics Data System (ADS)
Majumder, Papiya Sen; Bhowmick, Anil K.
1999-01-01
Electron beam initiated grafting of trimethylol propane triacrylate (TMPTA) onto ethylene propylene diene monomer (EPDM) has been carried out over a wide range of irradiation doses (0-200 kGy) using a fixed concentration (10%) of TMPTA. The samples have been both surface and bulk modified. Infrared (IR) studies indicate increased peak absorbances at 1730, 1260, 1120 and 1019 cm -1 upto 50 kGy and hence increased CO and C-O-C concentrations. The results are further supported by X-ray photoelectron spectroscopy (XPS) studies. The surface energy of EPDM increases from 46.5 to 60.7 mJ/m 2 on irradiation of the surface modified samples to 50 kGy dose, due to increased contribution of γSAB and γS(-). The results have been explained with the help of IR and XPS data. The values of tensile strength of the surface modified samples have not changed very significantly, while the moduli values have increased at the cost of the elongation at break. DMTA studies have shown changes in Tg and tan δmax on modification of the surface. The surface morphology of the modified and irradiated samples reveals acrylate flow marks at high magnification.
NASA Astrophysics Data System (ADS)
Basak, Ganesh C.; Bandyopadhyay, Abhijit; Neogi, Sudarsan; Bhowmick, Anil K.
2011-01-01
Vulcanized ethylene propylene diene polymethylene (EPDM) rubber surface was treated in a radio frequency capacitatively coupled low pressure argon/oxygen plasma to improve adhesion with compounded natural rubber (NR) during co-vulcanization. The plasma modified surfaces were analyzed by means of contact angle measurement, surface energy, attenuated total reflection-infrared spectroscopy, X-ray photoelectron spectroscopy, scanning electron microscopy, energy dispersive X-ray sulfur mapping and atomic force microscopy. Several experimental variables such as plasma power, length of exposure time and composition of the argon-oxygen gas mixture were considered. It was delineated that plasma treatment changed both surface composition and roughness, and consequently increased peel strength. The change in surface composition was mainly ascribed to the formation of C-O and -Cdbnd O functional groups on the vulcanized surfaces. A maximum of 98% improvement in peel strength was observed after plasma treatment.
1979-05-01
polyethylene (PE), polyvinyl chloride (PVC), butyl rubber , Hyalon (a registered trademark of Dupont), ethylene propylene diene monomer ( EPDM ), chlorinated...studies are explained in part by the following factors: age of the landfill and corresponding state of stabilization; composition of the solid waste, the...an active anaerobic population of methane formers. The removal of organics resulted in a more rapid stabilization or " aging " of the experimental
High voltage insulation of bushing for HTS power equipment
NASA Astrophysics Data System (ADS)
Kim, Woo-Jin; Choi, Jae-Hyeong; Kim, Sang-Hyun
2012-12-01
For the operation of high temperature superconducting (HTS) power equipments, it is necessary to develop insulating materials and high voltage (HV) insulation technology at cryogenic temperature of bushing. Liquid nitrogen (LN2) is an attractive dielectric liquid. Also, the polymer insulating materials are expected to be used as solid materials such as glass fiber reinforced plastic (GFRP), polytetra-fluoroethylene (PTFE, Teflon), Silicon (Si) rubber, aromatic polyamide (Nomex), EPDM/Silicon alloy compound (EPDM/Si). In this paper, the surface flashover characteristics of various insulating materials in LN2 are studied. These results are studied at both AC and impulse voltage under a non-uniform field. The use of GFRP and Teflon as insulation body for HTS bushing should be much desirable. Especially, GFRP is excellent material not only surface flashover characteristics but also mechanical characteristics at cryogenic temperature. The surface flashover is most serious problem for the shed design in LN2 and operation of superconducting equipments.
Failure life determination of oilfield elastomer seals in sour gas/dimethyl disulfide environments
DOE Office of Scientific and Technical Information (OSTI.GOV)
Kennelley, K.J.; Abrams, P.I.; Vicic, J.C.
1989-01-01
Previous screening tests of various oilfield elastomers in sour gas/dimethyl disulfide environments indicated that hydrogenated nitrile (HNBR), tetrafluoroethylene-propylene (TFE/P), ethylene-propylene-diene (EPDM), and perfluorinated rubber (FFKM) elastomers may perform satisfactorily in these environments. This paper describes subsequent failure life tests conducted with the subject elastomers in the sour gas/dimethyl disulfide test environment at several elevated temperatures (> 135{degrees}C). The materials were tested in the form of O-rings (size 214), which were used to seal an autoclave containing the test environment at 14 MPa gas pressure. The results were used to extrapolate time to failure at a common reference temperature of 135{degrees}C.more » The performance of EPDM and HNBR in the sour gas/dimethyl disulfide mixture substantially exceeded a projected 20-year service life at 135{degrees}C, while FFKM and TFE/P did not.« less
NASA Astrophysics Data System (ADS)
Zenoni, A.; Bignotti, F.; Donzella, A.; Donzella, G.; Ferrari, M.; Pandini, S.; Andrighetto, A.; Ballan, M.; Corradetti, S.; Manzolaro, M.; Monetti, A.; Rossignoli, M.; Scarpa, D.; Alloni, D.; Prata, M.; Salvini, A.; Zelaschi, F.
2017-11-01
Materials and components employed in the presence of intense neutron and gamma fields are expected to absorb high dose levels that may induce deep modifications of their physical and mechanical properties, possibly causing loss of their function. A protocol for irradiating elastomeric materials in reactor mixed neutron and gamma fields and for testing the evolution of their main mechanical and physical properties with absorbed dose has been developed. Four elastomeric compounds used for vacuum O-rings, one fluoroelastomer polymer (FPM) based and three ethylene propylene diene monomer rubber (EPDM) based, presently available on the market have been selected for the test. One EPDM is rated as radiation resistant in gamma fields, while the other elastomers are general purpose products. Particular care has been devoted to dosimetry calculations, since absorbed dose in neutron fields, unlike pure gamma fields, is strongly dependent on the material composition and, in particular, on the hydrogen content. The products have been tested up to about 2 MGy absorbed dose. The FPM based elastomer, in spite of its lower dose absorption in fast neutron fields, features the largest variations of properties, with a dramatic increase in stiffness and brittleness. Out of the three EPDM based compounds, one shows large and rapid changes in the main mechanical properties, whereas the other two feature more stable behaviors. The performance of the EPDM rated as radiation resistant in pure gamma fields does not appear significantly better than that of the standard product. The predictive capability of the accelerated irradiation tests performed as well as the applicable concepts of threshold of radiation damage is discussed in view of the use of the examined products in the selective production of exotic species facility, now under construction at the Legnaro National Laboratories of the Italian Istituto Nazionale di Fisica Nucleare. It results that a careful account of dose rate effects and oxygen penetration in the material, both during test irradiations and in operating conditions, is needed to obtain reliable predictions.
Zenoni, A; Bignotti, F; Donzella, A; Donzella, G; Ferrari, M; Pandini, S; Andrighetto, A; Ballan, M; Corradetti, S; Manzolaro, M; Monetti, A; Rossignoli, M; Scarpa, D; Alloni, D; Prata, M; Salvini, A; Zelaschi, F
2017-11-01
Materials and components employed in the presence of intense neutron and gamma fields are expected to absorb high dose levels that may induce deep modifications of their physical and mechanical properties, possibly causing loss of their function. A protocol for irradiating elastomeric materials in reactor mixed neutron and gamma fields and for testing the evolution of their main mechanical and physical properties with absorbed dose has been developed. Four elastomeric compounds used for vacuum O-rings, one fluoroelastomer polymer (FPM) based and three ethylene propylene diene monomer rubber (EPDM) based, presently available on the market have been selected for the test. One EPDM is rated as radiation resistant in gamma fields, while the other elastomers are general purpose products. Particular care has been devoted to dosimetry calculations, since absorbed dose in neutron fields, unlike pure gamma fields, is strongly dependent on the material composition and, in particular, on the hydrogen content. The products have been tested up to about 2 MGy absorbed dose. The FPM based elastomer, in spite of its lower dose absorption in fast neutron fields, features the largest variations of properties, with a dramatic increase in stiffness and brittleness. Out of the three EPDM based compounds, one shows large and rapid changes in the main mechanical properties, whereas the other two feature more stable behaviors. The performance of the EPDM rated as radiation resistant in pure gamma fields does not appear significantly better than that of the standard product. The predictive capability of the accelerated irradiation tests performed as well as the applicable concepts of threshold of radiation damage is discussed in view of the use of the examined products in the selective production of exotic species facility, now under construction at the Legnaro National Laboratories of the Italian Istituto Nazionale di Fisica Nucleare. It results that a careful account of dose rate effects and oxygen penetration in the material, both during test irradiations and in operating conditions, is needed to obtain reliable predictions.
Filtration System for Removal of Depleted Uranium from Water.
1988-02-01
PVC, 3-Way 65 1 1" Pressure Control Valve, Posacon #677, PVC Body, EPDM Diaphragm, Threaded Union Ends Valves with Actuators 29 2 1" PVC 3-Way Multi...Gaskets/Clamps 14 24 1/2" x 2 1/4" LG. Machine Bolts 15 32 1,2" Hex Nuts 16 64 1/2" Washer 17 8 1 1" Full Face Black Rubber Gasket 36 8 5/8" x 3" LG...Machine Bolts 37 8 5/8" Hex Nuts 38 16 5/8" Washers 39 6 3" Full Face Black Rubber Gasket 45 8 1/2" x 2 1/4" Machine Bolts 78 6 1 1/2" K40 Gasket 79 2 2
Pervaporative stripping of acetone, butanol and ethanol to improve ABE fermentation.
Jitesh, K; Pangarkar, V G; Niranjan, K
2000-01-01
Acetone-butanol-ethanol fermentation by anaerobic bacterium C. acetobutylicum is a potential source for feedstock chemicals. The problem of product induced inhibition makes this fermentation economically infeasible. Pervaporation is studied as an effective separation technique to remove the toxic inhibitory products. Various membranes like Styrene Butadiene Rubber (SBR), Ethylene Propylene Diene Rubber (EPDM), plain Poly Dimethyl Siloxane (PDMS) and silicalite filled PDMS were studied for the removal of acetone, butanol and ethanol, from binary aqueous mixtures and from a quaternary mixture. It was found that the overall performance of PDMS filled with 15% w/w of silicalite was the best for removal of butanol in binary mixture study. SBR performance was best for the quaternary mixture studied.
The dynamic Virtual Fields Method on rubbers at medium and high strain rates
NASA Astrophysics Data System (ADS)
Yoon, Sung-Ho; Siviour, Clive R.
2015-09-01
Elastomeric materials are widely used for energy absorption applications, often experiencing high strain rate deformations. The mechanical characterization of rubbers at high strain rates presents several experimental difficulties, especially associated with achieving adequate signal to noise ratio and static stress equilibrium, when using a conventional technique such as the split Hopkinson pressure bar. In the present study, these problems are avoided by using the dynamic Virtual Fields Method (VFM) in which acceleration fields, clearly generated by the non-equilibrium state, are utilized as a force measurement with in the frame work of the principle of virtual work equation. In this paper, two dynamic VFM based techniques are used to characterise an EPDM rubber. These are denoted as the linear and nonlinear VFM and are developed for (respectively) medium (drop-weight) and high (gas-gun) strain-rate experiments. The use of the two VFMs combined with high-speed imaging analysed by digital imaging correlation allows the identification of the parameters of a given rubber mechanical model; in this case the Ogden model is used.
Investigating Low Temperature Properties of Rubber Seals - 13020
DOE Office of Scientific and Technical Information (OSTI.GOV)
Jaunich, M.; Wolff, D.; Stark, W.
To achieve the required tightness levels of containers for low and intermediate level radioactive wastes rubbers are widely applied as main sealing materials. The save encapsulation of the radioactive container contents has to be guaranteed according to legislation and appropriate guidelines for long storage periods as well as down to temperatures of -40 deg. C during transportation. Therefore the understanding of failure mechanisms that lead to leakage at low temperatures is of high importance. It is known that the material properties of rubbers are strongly influenced by temperature. At low temperatures this is caused by the rubber-glass transition (abbr. glassmore » transition). During continuous cooling the material changes from rubber-like entropy-elastic to stiff energy-elastic behaviour, that allows nearly no strain or retraction. Therefore, rubbers are normally used above their glass transition but the minimum working temperature limit is not defined precisely, what can cause problems during application. The temperature range where full functionality is possible is strongly dependent on the application conditions and the material. For this investigation mainly ethylene propylene diene (EPDM) and fluorocarbon rubbers (FKM) were selected as they are often used for radioactive waste containers. Differential Scanning Calorimetry (DSC) and Dynamic Mechanical Analysis (DMA) are typically used for the determination of the temperature range of the glass transition process. The standardized compression set measurement according to ISO 815 is common for investigation of rubber sealing materials as the test simulates the seal behaviour after release. To reduce the test time of the standard tests a faster technique giving the same information was developed. Additionally, the breakdown temperature of the sealing function of complete O-ring seals is measured in a component test setup to compare it with the results of the other tests. The experimental setup is capable of measuring the leakage rate at low temperatures by the pressure rise method. A model was developed that allows calculating the minimum working temperature limit of a seal by combining the results of the applied methods. (authors)« less
Massively Parallel Simulations of Diffusion in Dense Polymeric Structures
DOE Office of Scientific and Technical Information (OSTI.GOV)
Faulon, Jean-Loup, Wilcox, R.T.
1997-11-01
An original computational technique to generate close-to-equilibrium dense polymeric structures is proposed. Diffusion of small gases are studied on the equilibrated structures using massively parallel molecular dynamics simulations running on the Intel Teraflops (9216 Pentium Pro processors) and Intel Paragon(1840 processors). Compared to the current state-of-the-art equilibration methods this new technique appears to be faster by some orders of magnitude.The main advantage of the technique is that one can circumvent the bottlenecks in configuration space that inhibit relaxation in molecular dynamics simulations. The technique is based on the fact that tetravalent atoms (such as carbon and silicon) fit in themore » center of a regular tetrahedron and that regular tetrahedrons can be used to mesh the three-dimensional space. Thus, the problem of polymer equilibration described by continuous equations in molecular dynamics is reduced to a discrete problem where solutions are approximated by simple algorithms. Practical modeling applications include the constructing of butyl rubber and ethylene-propylene-dimer-monomer (EPDM) models for oxygen and water diffusion calculations. Butyl and EPDM are used in O-ring systems and serve as sealing joints in many manufactured objects. Diffusion coefficients of small gases have been measured experimentally on both polymeric systems, and in general the diffusion coefficients in EPDM are an order of magnitude larger than in butyl. In order to better understand the diffusion phenomena, 10, 000 atoms models were generated and equilibrated for butyl and EPDM. The models were submitted to a massively parallel molecular dynamics simulation to monitor the trajectories of the diffusing species.« less
DOE Office of Scientific and Technical Information (OSTI.GOV)
Walker, I.S.; Gaines, A.
1987-11-01
The W.R. Grace Chemical Division plant in Lake Charles, LA had to stop producing catalysts for the oil refining industry whenever a piping system for 98% sulfuric acid developed a leak. Gaskets of a nonasbestos material were being used between the flanges of the steel pipe lined with TFE or polypropylene. The flange bolts were kept tight, but the gaskets usually failed to maintain a leaktight seal with the acid at 60 psi for more than a few weeks or months. The acid lines had to be drained before the faulty gasket could be replaced, and production downtime would rangemore » from one to three hours. In July 1986, the plant decided to try a chemical resistant gasket of Teflon molded and bonded to a core of Shore A 65-66 durometer EPDM rubber in the acid lines. The resilient gasket also has patented double convex rings on both faces for optimum sealing with only one-eighth the bolt tightening torque commonly required with flat-faced gaskets. The low sealing force requirement prolongs the life of the gasket, eliminates plastic cold flow at the flange of lined steel pipe, and avoids stresses that can damage thermoplastic and fiberglass piping systems. The gasket has a temperature range of {minus}4 to 210{degree}F and is available in 1/2 through 12 inch sizes that conform to ANSI B16.1 flange dimensions. Alternative gasket materials are Kynar PVDF-bonded EPDM and EPDM without a fluoropolymer laminate. The Teflon-bonded EPDM gaskets eliminated unscheduled catalyst production downtime due to leakage from the sulfuric acid piping system. The plant maintains an inventory of the low torque gasket, but has never had to replace any that have been in service since July 1986.« less
Mittan, Margaret Birmingham [Oakland, CA; Miros, Robert H. J. [Fairfax, CA; Brown, Malcolm P [San Francisco, CA; Stancel, Robert [Loss Altos Hills, CA
2012-06-05
A photovoltaic panel clamp includes an upper and lower section. The interface between the assembled clamp halves and the module edge is filled by a flexible gasket material, such as EPDM rubber. The gasket preferably has small, finger like protrusions that allow for easy insertion onto the module edge while being reversed makes it more difficult to remove them from the module once installed. The clamp includes mounting posts or an integral axle to engage a bracket. The clamp also may include a locking tongue to secure the clamp to a bracket.
Brown, Malcolm P.; Mittan, Margaret Birmingham; Miros, Robert H. J.; Stancel, Robert
2013-03-19
A photovoltaic panel clamp includes an upper and lower section. The interface between the assembled clamp halves and the module edge is filled by a flexible gasket material, such as EPDM rubber. The gasket preferably has small, finger like protrusions that allow for easy insertion onto the module edge while being reversed makes it more difficult to remove them from the module once installed. The clamp includes mounting posts or an integral axle to engage a bracket. The clamp also may include a locking tongue to secure the clamp to a bracket.
1992-01-30
Agent Resistant Coating, retractable nylon handles, ethylene propylenediene monomer ( EPDM ) rubber securing straps, and a woven monofilament polypropylene...without Z-folds: overlapping layers of fabric sewn as reinforcement in the cover opposite the spreader bars. These covers were made from fabrics that...problem is not isolated to the decon litter and mattress. Comparable slippage should be expected when the vinyl mattress is used with the new nylon
NASA Astrophysics Data System (ADS)
Milani, Gabriele; Milani, Federico
2012-12-01
The main problem in the industrial production process of thick EPM/EPDM elements is constituted by the different temperatures which undergo internal (cooler) and external regions. Indeed, while internal layers remain essentially under-vulcanized, external coating is always over-vulcanized, resulting in an overall average tensile strength insufficient to permit the utilization of the items in several applications where it is required a certain level of performance. Possible ways to improve rubber output mechanical properties include a careful calibration of exposition time and curing temperature in traditional heating or a vulcanization through innovative techniques, such as microwaves. In the present paper, a comprehensive numerical model able to give predictions on the optimized final mechanical properties of vulcanized 2D and 3D thick rubber items is presented and applied to a meaningful example of engineering interest. A detailed comparative numerical study is finally presented in order to establish pros and cons of traditional vulcanization vs microwaves curing.
Detectability of Delaminations in Solid Rocket Motors with Embedded Stress Sensors
2011-10-14
composite grain of hydroxyl-terminated polybutadiene/ammonium perchlorate (HTPB/AP). The insulation layer is ethylene propylene diene monomer ( EPDM ...The temperature-dependent mechanical properties of HTPB/AP and EPDM were obtained from in-house testing at AFRL/RZSM (Edwards AFB). The motor case is...temperature (DBST) sensors and Greg Yandek of AFRL/RZSM for the data collection of EPDM insulation material. Distribution A: Approved for public
Hydrophobic Characteristics of Composite Insulators in Simulated Inland Arid Desert Environment
NASA Astrophysics Data System (ADS)
Khan, Yasin; Al-Arainy, Abdulrehman Ali; Malik, Nazar Hussain; Qureshi, Muhammad Iqbal
2010-06-01
Presently along with traditional insulators i.e. glass and porcelain, etc., the polymeric insulators are also used world widely. These polymeric insulators are very sensitive to various environmental parameters e.g. UV radiations, heat, etc. The UV radiation level in the central region of Saudi Arabia is high as compared to the recommended IEC-61109 standard for the accelerated aging of the composite insulators. In this study, thermoplastic elastomer (TPE) and Ethylene Propylene Diene Monomer (EPDM) insulators were subjected to accelerated aging stress as per IEC standard as well as modified IEC standard simulating the inland arid desert's atmospheric conditions. The hydrophobic characteristics were studied by measuring the contact angle along the insulator surface before and after the accelerated aging of the samples. It was found that TPE loses its hydrophobic properties more as compared to EPDM insulator. This loss was proportional to the intensity of UV irradiation. The rate of recovery is also low for both the tested materials as compared to Silicone Rubber insulators.
HYDROPHOBIC CHARACTERISTICS OF COMPOSITE INSULATORS IN SIMULATED INLAND ARID DESERT ENVIRONMENT
DOE Office of Scientific and Technical Information (OSTI.GOV)
Khan, Yasin; Al-Arainy, Abdulrehman Ali; Malik, Nazar Hussain
2010-06-15
Presently along with traditional insulators i.e. glass and porcelain, etc., the polymeric insulators are also used world widely. These polymeric insulators are very sensitive to various environmental parameters e.g. UV radiations, heat, etc. The UV radiation level in the central region of Saudi Arabia is high as compared to the recommended IEC-61109 standard for the accelerated aging of the composite insulators. In this study, thermoplastic elastomer (TPE) and Ethylene Propylene Diene Monomer (EPDM) insulators were subjected to accelerated aging stress as per IEC standard as well as modified IEC standard simulating the inland arid desert's atmospheric conditions. The hydrophobic characteristicsmore » were studied by measuring the contact angle along the insulator surface before and after the accelerated aging of the samples. It was found that TPE loses its hydrophobic properties more as compared to EPDM insulator. This loss was proportional to the intensity of UV irradiation. The rate of recovery is also low for both the tested materials as compared to Silicone Rubber insulators.« less
Detectability of Delaminations in Solid Rocket Motors with Embedded Stress Sensors
2012-05-04
thick, respectively. The propellant is a typical HTPB/AP composite grain with an EPDM insulation layer. The temperature-dependent elastic mechanical...properties of HTPB/AP and EPDM were obtained from in-house testing at AFRL/RZSM (Edwards AFB). The motor case is assumed to be a filament-wound...collection of EPDM insulation material. REFERENCES 1 Ruderman, G. A., “Health Management Issues and Strategy for Air Force Missiles,” International
Moritz, Miriam M; Flemming, Hans-Curt; Wingender, Jost
2010-06-01
Drinking water biofilms were grown on coupons of plumbing materials, including ethylene-propylene-diene-monomer (EPDM) rubber, silane cross-linked polyethylene (PE-X b), electron-ray cross-linked PE (PE-X c) and copper under constant flow-through of cold tap water. After 14 days, the biofilms were spiked with Pseudomonas aeruginosa, Legionella pneumophila and Enterobacter nimipressuralis (10(6) cells/mL each). The test bacteria were environmental isolates from contamination events in drinking water systems. After static incubation for 24 h, water flow was resumed and continued for 4 weeks. Total cell count and heterotrophic plate count (HPC) of biofilms were monitored, and P. aeruginosa, L. pneumophila and E. nimipressuralis were quantified, using standard culture-based methods or culture-independent fluorescence in situ hybridization (FISH). After 14 days total cell counts and HPC values were highest on EPDM followed by the plastic materials and copper. P. aeruginosa and L. pneumophila became incorporated into drinking water biofilms and were capable to persist in biofilms on EPDM and PE-X materials for several weeks, while copper biofilms were colonized only by L. pneumophila in low culturable numbers. E. nimipressuralis was not detected in any of the biofilms. Application of the FISH method often yielded orders of magnitude higher levels of P. aeruginosa and L. pneumophila than culture methods. These observations indicate that drinking water biofilms grown under cold water conditions on domestic plumbing materials, especially EPDM and PE-X in the present study, can be a reservoir for P. aeruginosa and L. pneumophila that persist in these habitats mostly in a viable but non-culturable state.
Comparison of batch and column tests for the elution of artificial turf system components.
Krüger, O; Kalbe, U; Berger, W; Nordhauβ, K; Christoph, G; Walzel, H-P
2012-12-18
Synthetic athletic tracks and turf areas for outdoor sporting grounds may release contaminants due to the chemical composition of some components. A primary example is that of zinc from reused scrap tires (main constituent, styrene butadiene rubber, SBR), which might be harmful to the environment. Thus, methods for the risk assessment of those materials are required. Laboratory leaching methods like batch and column tests are widely used to examine the soil-groundwater pathway. We tested several components for artificial sporting grounds with batch tests at a liquid to solid (LS) ratio of 2 L/kg and column tests with an LS up to 26.5 L/kg. We found a higher zinc release in the batch test eluates for all granules, ranging from 15% higher to 687% higher versus data from column tests for SBR granules. Accompanying parameters, especially the very high turbidity of one ethylene propylene diene monomer rubber (EPDM) or thermoplastic elastomer (TPE) eluates, reflect the stronger mechanical stress of batch testing. This indicates that batch test procedures might not be suitable for the risk assessment of synthetic sporting ground components. Column tests, on the other hand, represent field conditions more closely and allow for determination of time-dependent contaminants release.
Air Force Geophysics Laboratory Aerodynamically Shaped Tethered Balloon. 45,000 Cubic Feet.
1980-12-01
21 ~i ag 1 -- - - - - ’U - .~ zw ’U - - .~ -- ~ - ~-4 a~ - ~ N. ’U 1 N. - - - ~ - - ~- >- - ~J-’~ - -4-4 ~4 Cf -4 N N~’ N -, N. N.-~N.N.- N. ~ ~ ~ N N...extent that the physical parafmters will change, thus requiring vendor formulation selection. The above polymers plus others such as Teflon, Saran and EPDM ...Lnating Between Plies L utYi1 rubber i,, recommended by ILC Dover, instead of neoprene, for the middle 1,1vor of two ply biased laminated
Understanding Trap Effects on Electrical Treeing Phenomena in EPDM/POSS Composites.
Du, Boxue; Su, Jingang; Tian, Meng; Han, Tao; Li, Jin
2018-05-31
POSS (polyhedral oligomeric silsesquioxane) provides an interesting alternative nano-silica and has the potential of superior dielectric properties to restrain electrical degradation. By incorporating POSS into EPDM to suppress electrical tree, one of precursors to dielectric failure, is promising to improve the lifetime of insulation materials. This paper focuses on the electrical treeing phenomena in EPDM/OVPOSS (ethylene propylene diene monomer/octavinyl-POSS) composites based on their physicochemical properties and trap distributions. ATR-IR and SEM characteristics are investigated to observe the chemical structure and physical dispersion of EPDM/OVPOSS composites. Electrical treeing characteristics are studied by the needle-plane electrode, and the trap level distributions are characterized by surface potential decay (SPD) tests. The results show that the 3 wt% EPDM/OVPOSS is more effective to restrain the electrical tree growth than the neat EPDM in this paper. It is indicated that the EPDM/OVPOSS with a filler content of 3 wt% introduces the largest energy level and trap density of deep trapped charges, which suppress the transportation of charge carriers injected from the needle tip and further prevent the degradation of polymer molecules. The polarity effects are obvious during the electrical treeing process, which is dependent on the trap level differences between positive and negative voltage.
Kumar, P V Anil; Anilkumar, S; Varughese, K T; Thomas, Sabu
2012-01-15
Polymer membranes were prepared by blending high density polyethylene (HDPE) with ethylene propylene diene terpolymer rubber (EPDM). These blend membranes were evaluated for the selective separation of n-hexane from acetone. The flux and selectivity of the membranes were determined both as a function of the blend composition and feed mixture composition. Results showed that polymer blending method could be very useful to develop new membranes with improved selectivity. Pervaporation properties could be optimized by adjusting the blend composition. The effects of blend ratio, feed composition, and penetrant size on the pervaporation process were analyzed. The permeation properties have been explained on the basis of interaction between the membrane and solvents and blend morphology. Flux increases with increasing alkane content in the feed composition. Copyright © 2011 Elsevier B.V. All rights reserved.
Towards ultraporous poly(L-lactide) scaffolds from quaternary immiscible polymer blends.
Virgilio, N; Sarazin, P; Favis, B D
2010-08-01
Ultraporous poly(l-lactide) (PLLA) scaffolds were prepared by melt-processing quaternary ethylene propylene diene rubber/poly(epsilon-caprolactone)/polystyrene/poly(l-lactide) (EPDM/PCL/PS/PLLA) 45/45/5/5 %vol. polymer blends modified with a PS-b-PLLA diblock copolymer. The morphology consists of a PS+PLLA+copolymer sub-blend layer forming at the interface of the EPDM and PCL phases. Quiescent annealing and interfacial modification using the block copolymer are used to control the blend microstructure. The ultraporous structure is subsequently obtained by selectively extracting the EPDM, PS and PCL phases. The PLLA scaffolds modified with the PS-b-PLLA copolymer present themselves as fully interconnected porous networks with asymmetric channel walls, one side being smooth while the other is covered with an array of submicron-sized PLLA droplets. They are prepared with a high degree of control over the pore size, with averages ranging from 5microm to over 100microm and a specific surface from 9.1 to 23.1m(2)/g of PLLA, as annealing is carried out from 0 to 60min. The void volume reaches values as high as 95% and in all cases the shape and dimensions of the scaffolds are maintained with a high level of integrity. The proposed method represents a comprehensive approach towards the design and generation of porous PLLA scaffolds based on complex morphologies from melt-processed multiphase polymer systems. Copyright 2010 Elsevier Ltd. All rights reserved.
NASA Astrophysics Data System (ADS)
Feng, Q. L.; Li, C.; Liao, Y. F.
2017-12-01
Short fiber reinforced EPDM is a new kind of composite material used in solid rocket motor winding and coating. It has relatively large deformation under the small stress condition, and the physical non-linear characteristic is obvious. Due to the addition of fiber in the specific direction of the rubber, the macroscopic mechanical properties are expressed as transversely isotropic properties. In order to describe the mechanical behavior under the impact and vibration, the transversely isotropic hyperelastic constitutive model based on tensor function is proposed. The symmetry of the transversely isotropic incompressible material limits the stress tensor ‘ K ’ to be characterized as a function of 5 tensor invariants and 4 scalar invariants. The third power constitutive equations of the model give 12 independent elastic constants of the transversely isotropic nonlinear elastic material. The experimental results show that the non-zero elastic constants are different in the fiber direction and at the different strain rate. Number and value of adiabatic layer and related products R & D has a reference value.
The correlation between elongation at break and thermal decomposition of aged EPDM cable polymer
NASA Astrophysics Data System (ADS)
Šarac, T.; Devaux, J.; Quiévy, N.; Gusarov, A.; Konstantinović, M. J.
2017-03-01
The effect of simultaneous thermal and gamma irradiation ageing on the mechanical and physicochemical properties of industrial EPDM was investigated. Accelerated ageing, covering a wide range of dose rates, doses and temperatures, was preformed in stagnant air on EPDM polymer samples extracted from the cables in use in the Belgian nuclear power plants. The mechanical properties, ultimate tensile stress and elongation at break, are found to exhibit the strong dependence on the dose, ageing temperature and dose rate. The thermal decomposition of aged polymer is observed to be the dose dependent when thermogravimetry test is performed under air atmosphere. No dose dependence is observed when thermal decomposition is performed under nitrogen atmosphere. The thermal decomposition rates are found to fully mimic the reduction of elongation at break for all dose rates and ageing temperatures. This effect is argued to be the result of thermal and radiation mediated oxidation degradation process.
1988-10-01
these types of waste are available, with only general descriptions such as "toxic pharmaceutical waste" or " rubber and plastic waste" provided. 30...liner materials (i.e., HDPE through EPDM (ethylene/propylene/diene terpolymer)) are one to two orders of magnitude better barriers to water (on a per... ages in areas where the liner had been worked on with earth-moving equipment during removal operations (Nelson, Haxo, and McGlew 1985). Natural Soil
New approach to the ecotoxicological risk assessment of artificial outdoor sporting grounds.
Krüger, O; Kalbe, U; Richter, E; Egeler, P; Römbke, J; Berger, W
2013-04-01
Artificial surfaces for outdoor sporting grounds may pose environmental and health hazards that are difficult to assess due to their complex chemical composition. Ecotoxicity tests can indicate general hazardous impacts. We conducted growth inhibition (Pseudokirchneriella subcapitata) and acute toxicity tests (Daphnia magna) with leachates obtained from batch tests of granular infill material and column tests of complete sporting ground assemblies. Ethylene propylene diene monomer rubber (EPDM) leachate showed the highest effect on Daphnia magna (EC(50) < 0.4% leachate) and the leachate of scrap tires made of styrene butadiene rubber (SBR) had the highest effect on P. subcapitata (EC(10) = 4.2% leachate; EC(50) = 15.6% leachate). We found no correlations between ecotoxicity potential of leachates and zinc and PAH concentrations. Leachates obtained from column tests revealed lower ecotoxicological potential. Leachates of column tests of complete assemblies may be used for a reliable risk assessment of artificial sporting grounds. Copyright © 2013 Elsevier Ltd. All rights reserved.
Polymer materials and component evaluation in acidic-radiation environments
NASA Astrophysics Data System (ADS)
Celina, M.; Gillen, K. T.; Malone, G. M.; Clough, R. L.; Nelson, W. H.
2001-07-01
Polymeric materials used for cable/wire insulation, electrical connectors, O-rings, seals, and in critical components such as motors, level switches and resistive thermo-devices were evaluated under accelerated degradation conditions in combined radiation-oxidative elevated-temperature acidic-vapor (nitric/oxalic) environments relevant to conditions in isotope processing facilities. Experiments included the assessment of individual materials such as PEEK, polyimides, polyolefin based cable insulation, EPDM rubbers, various epoxy systems, commercial caulking materials as well as some functional testing of components. We discuss how to conduct laboratory experiments to simulate such complex hostile environments, describe some degradation effects encountered, and evaluate the impact on appropriate material and component selection.
Structural adhesives for missile external protection material
NASA Astrophysics Data System (ADS)
Banta, F. L.; Garzolini, J. A.
1981-07-01
Two basic rubber materials are examined as possible external substrate protection materials (EPM) for missiles. The analysis provided a data base for selection of the optimum adhesives which are compatible with the substrate, loads applied and predicted bondline temperatures. Under the test conditions, EA934/NA was found to be the optimum adhesive to bond VAMAC 2273 and/or NBR/EPDM 9969A to aluminum substrate. The optimum adhesive for composite structures was EA956. Both of these adhesives are two-part epoxy systems with a pot life of approximately two hours. Further research is suggested on field repair criteria, nuclear hardness and survivability effects on bondline, and ageing effects.
Impact of Herbivory and Plant Competition on the Growth of Hydrilla in Small Ponds
2007-02-01
pond (6m x 6m with a depth of 1.3 m) was lined with 45-mil synthetic EPDM rubber (Ethylene propylene diene monomer, Firestone, Akron, OH...3000 4000 5000 6000 Competition No Competition % D am ag ed L ea ve s 0 10 20 30 40 50 60 Jul-01 Sep-01 Nov-01 Jan-02 Mar-02 May-02 Jul-02 Sept-02 Nox...02 Jan-03 Mar-03 May-03 % D am ag ed L ea ve s 0 10 20 30 40 50 60 No Competition Competition A B C D Figure 1. Number of immatures per kg in
Influence of different components in a TPV PP/EPDM based with low hardness
NASA Astrophysics Data System (ADS)
Gheller, J.; Jacobi, M. M.
2014-05-01
Thermoplastic vulcanizates (TPVs) are a class of polymeric material obtained by dynamic vulcanization of an elastomer in a melted thermoplastic matrix. This work intend to evaluate different variables in the production of low hardness TPVs made of polypropylene (PP) and ethylene propylene rubber (EPDM), as well the optimization of the variables looking for TPVs with improved performance. In the Study I the influence of PP crystallinity were evaluated, in the Study II the effects of different amounts of dicumyl peroxide (DCP) were evaluated and in the Study III the amount of the phenolic resin were evaluated. This extended abstract presents, in a more detailed way, the results considering the curative phenolic resin content (Study III). The others results and discussions are briefly described in the results and discussions section. The compounds were obtained in a closed mixing chamber and their processability properties, swelling, hardness and tensile strength were evaluated. With the results obtained were possible to evaluate the influence of different ingredients in the TPVs properties. The results were discussed and presented looking for a better understanding of the influence of this variable in the final product, as well the correlation between then.
EPDM Based Double Slope Triangular Enclosure Solar Collector: A Novel Approach
Qureshi, Shafiq R.; Khan, Waqar A.
2014-01-01
Solar heating is one of the important utilities of solar energy both in domestic and industrial sectors. Evacuated tube heaters are a commonly used technology for domestic water heating. However, increasing cost of copper and nickel has resulted in huge initial cost for these types of heaters. Utilizing solar energy more economically for domestic use requires new concept which has low initial and operating costs together with ease of maintainability. As domestic heating requires only nominal heating temperature to the range of 60–90°C, therefore replacing nickel coated copper pipes with any cheap alternate can drastically reduce the cost of solar heater. We have proposed a new concept which utilizes double slope triangular chamber with EPDM based synthetic rubber pipes. This has reduced the initial and operating costs substantially. A detailed analytical study was carried out to design a novel solar heater. On the basis of analytical design, a prototype was manufactured. Results obtained from the experiments were found to be in good agreement with the analytical study. A maximum error of 10% was recorded at noon. However, results show that error is less than 5% in early and late hours. PMID:24688407
EPDM based double slope triangular enclosure solar collector: a novel approach.
Qureshi, Shafiq R; Khan, Waqar A; Sarwar, Waqas
2014-01-01
Solar heating is one of the important utilities of solar energy both in domestic and industrial sectors. Evacuated tube heaters are a commonly used technology for domestic water heating. However, increasing cost of copper and nickel has resulted in huge initial cost for these types of heaters. Utilizing solar energy more economically for domestic use requires new concept which has low initial and operating costs together with ease of maintainability. As domestic heating requires only nominal heating temperature to the range of 60-90 °C, therefore replacing nickel coated copper pipes with any cheap alternate can drastically reduce the cost of solar heater. We have proposed a new concept which utilizes double slope triangular chamber with EPDM based synthetic rubber pipes. This has reduced the initial and operating costs substantially. A detailed analytical study was carried out to design a novel solar heater. On the basis of analytical design, a prototype was manufactured. Results obtained from the experiments were found to be in good agreement with the analytical study. A maximum error of 10% was recorded at noon. However, results show that error is less than 5% in early and late hours.
Quantitative confirmation of diffusion-limited oxidation theories
DOE Office of Scientific and Technical Information (OSTI.GOV)
Gillen, K.T.; Clough, R.L.
1990-01-01
Diffusion-limited (heterogeneous) oxidation effects are often important for studies of polymer degradation. Such effects are common in polymers subjected to ionizing radiation at relatively high dose rate. To better understand the underlying oxidation processes and to aid in the planning of accelerated aging studies, it would be desirable to be able to monitor and quantitatively understand these effects. In this paper, we briefly review a theoretical diffusion approach which derives model profiles for oxygen surrounded sheets of material by combining oxygen permeation rates with kinetically based oxygen consumption expressions. The theory leads to a simple governing expression involving the oxygenmore » consumption and permeation rates together with two model parameters {alpha} and {beta}. To test the theory, gamma-initiated oxidation of a sheet of commercially formulated EPDM rubber was performed under conditions which led to diffusion-limited oxidation. Profile shapes from the theoretical treatments are shown to accurately fit experimentally derived oxidation profiles. In addition, direct measurements on the same EPDM material of the oxygen consumption and permeation rates, together with values of {alpha} and {beta} derived from the fitting procedure, allow us to quantitatively confirm for the first time the governing theoretical relationship. 17 refs., 3 figs.« less
Deformational characteristics of thermoplastic elastomers
NASA Astrophysics Data System (ADS)
Indukuri, Kishore K.
This thesis focuses primarily on the structure-property relationships of poly (styrene-ethylene-butylene-styrene) triblock copolymer TPEs. First evidence for strain-induced crystallization occurring in certain SEBS block copolymers has been established using unique techniques like deformation calorimetry, combined in-situ small angle X-ray and wide angle X-ray diffraction (SAXD/WAXD). Also the ramifications of such strain-induced crystallization on the mechanical properties like cyclic hysteresis, stress relaxation/creep retention of these SEBS systems have been studied. In addition, the structural changes in the morphology of these systems on deformation have been investigated using combined SAXD/WAXD setup. Small angle X-ray diffraction probed the changes at the nano-scale of polystyrene (PS) cylinders, while wide angle X-ray diffraction probed the changes at molecular length scales of the amorphous/crystalline domains of the elastomeric mid-block in these systems. New structural features at both these length scales have been observed and incorporated into the overall deformation mechanisms of the material. Continuous processing techniques like extrusion have been used to obtain ultra long-range order and orientation in these SEBS systems. Thus well ordered crystal like hexagonal packing of cylinders, where in each element in this hexagonal lattice can be individually addressed without any grain boundaries can be realized using these robust techniques. The effect of long-range order/orientation on the mechanical properties has been studied. In addition, these well ordered systems serve as model systems for evaluating deformation mechanisms of these SEBS systems, where the relative contributions of each of the phases can be estimated. EPDM/i-PP thermoplastic vulcanizates (TPVs) have micron size scale phase separated morphologies of EPDM rubber dispersed in a semicrystalline i-PP matrix as a result of the dynamic vulcanization process. Confocal microscopy studies, along with scanning electron microscopy (SEM) studies show that the morphology of these EPDM/i-PP systems resembles a microcellular "filled" foam in which i-PP occupies the strut regions and EPDM the inner core. Based on this, an analytical model has been developed that takes into account composition information, molecular weight, cure state and morphology into account.
Silane cross-linkable ethylene-propylene elastomer compositions prepared by reactive processing
NASA Astrophysics Data System (ADS)
Kozawa, Eiji; Nakajima, Yasuo; Kim, Jae Kyung
2015-05-01
Thermoplastic Elastomers (TPEs) have received attention as the alternative materials of EPDM due to an advantage for mass production. In recent years, by the progress of polymerization technology, Ethylene-propylene Elastomer (EP), one of the TPEs, is beginning to be applied to many products because of its good properties as rubber. However, as much as a complete replacement for EPDM, it is not provided with sufficient properties. In such circumstance, we found that EP's performance properties can be further enhanced via chemical modification such as cross-linking. The advent of a newer technique, involving the grafting of organo-functional silane onto the polymer chain in the reaction extrusion process is more attractive due to various industrial advantages. Although the functionalization of the EP by silane grafting through reactive processing is very useful, the silane grafting process of EP has a difficulty. It is most likely a consequence of the nature of the PP chain scission (β-scission), which is the dominant reaction in PP when subjected to free radicals at elevated temperature during processing. Therefore, the objective of our current work is to investigate a reactive extrusion process for the silane cross-linkable EP while minimizing the degradation, as well as evaluate the properties of the modified polymer.
Accelerated aging of EPDM and butyl elastomers
DOE Office of Scientific and Technical Information (OSTI.GOV)
Wilson, M.H.
1996-06-01
This study was composed of three parts: a post cure study to optimize final properties of an ethylene-propylene-diene (EPDM) formulation, an accelerated aging study to compare the stress relaxation behavior of a butyl and an EPDM elastomer under compression, and a cursory evaluation of a new 70 Shore A EPDM. The optimum postcure for the EPDM was found to be 2 to 4 hours at 182{degrees}C in a vacuum. The EPDM was also shown to have superior aging characteristics compared to the butyl and is recommended for use instead of the butyl material. The physical properties for new 70 Shoremore » A EPDM are satisfactory, and the stress relaxation behavior was only slightly inferior to the other EPDM.« less
Saiwari, Sitisaiyidah; van Hoek, Johannes W; Dierkes, Wilma K; Reuvekamp, Louis E A M; Heideman, Geert; Blume, Anke; Noordermeer, Jacques W M
2016-08-24
As a means to decrease the amount of waste tires and to re-use tire rubber for new tires, devulcanization of ground passenger car tires is a promising process. Being an established process for NR and EPDM, earlier work has shown that for ground passenger car tire rubber with a relatively high amount of SBR, a devulcanization process can be formulated, as well. This was proven for a laboratory-scale batch process in an internal mixer, using diphenyl disulfide as the devulcanization aid and powder-sized material. In this paper, the devulcanization process for passenger car tire rubber is upscaled from 15 g per batch and transformed into a continuous process in a co-rotating twin screw extruder with a capacity of 2 kg/h. As SBR is rather sensitive to devulcanization process conditions, such as thermal and mechanical energy input, the screw design was based on a low shear concept. A granulate with particle sizes from 1-3.5 mm was chosen for purity, as well as economic reasons. The devulcanization process conditions were fine-tuned in terms of: devulcanization conditions (time/temperature profile, concentration of devulcanization aid), extruder parameters (screw configuration, screw speed, fill factor) and ancillary equipment (pre-treatment, extrudate handling). The influence of these parameters on the devulcanization efficiency and the quality of the final product will be discussed. The ratio of random to crosslink scission as determined by a Horikx plot was taken for the evaluation of the process and material. A best practice for continuous devulcanization will be given.
Saiwari, Sitisaiyidah; van Hoek, Johannes W.; Dierkes, Wilma K.; Reuvekamp, Louis E.A.M.; Heideman, Geert; Blume, Anke; Noordermeer, Jacques W.M.
2016-01-01
As a means to decrease the amount of waste tires and to re-use tire rubber for new tires, devulcanization of ground passenger car tires is a promising process. Being an established process for NR and EPDM, earlier work has shown that for ground passenger car tire rubber with a relatively high amount of SBR, a devulcanization process can be formulated, as well. This was proven for a laboratory-scale batch process in an internal mixer, using diphenyl disulfide as the devulcanization aid and powder-sized material. In this paper, the devulcanization process for passenger car tire rubber is upscaled from 15 g per batch and transformed into a continuous process in a co-rotating twin screw extruder with a capacity of 2 kg/h. As SBR is rather sensitive to devulcanization process conditions, such as thermal and mechanical energy input, the screw design was based on a low shear concept. A granulate with particle sizes from 1–3.5 mm was chosen for purity, as well as economic reasons. The devulcanization process conditions were fine-tuned in terms of: devulcanization conditions (time/temperature profile, concentration of devulcanization aid), extruder parameters (screw configuration, screw speed, fill factor) and ancillary equipment (pre-treatment, extrudate handling). The influence of these parameters on the devulcanization efficiency and the quality of the final product will be discussed. The ratio of random to crosslink scission as determined by a Horikx plot was taken for the evaluation of the process and material. A best practice for continuous devulcanization will be given. PMID:28773843
Zupančič, Jerneja; Raghupathi, Prem K; Houf, Kurt; Burmølle, Mette; Sørensen, Søren J; Gunde-Cimerman, Nina
2018-01-01
Biofilms formed on rubber seals in dishwashers harbor diverse microbiota. In this study, we focussed on the microbial composition of bacteria and fungi, isolated from a defined area of one square centimeter of rubber from four domestic dishwashers and assessed their abilities to in vitro multispecies biofilm formation. A total of 80 isolates (64 bacterial and 16 fungal) were analyzed. Multiple combinations of bacterial isolates from each dishwasher were screened for synergistic interactions. 32 out of 140 tested (23%) four-species bacterial combinations displayed consistent synergism leading to an overall increase in biomass, in all experimental trails. Bacterial isolates from two of the four dishwashers generated a high number of synergistically interacting four-species consortia. Network based correlation analyses also showed higher co-occurrence patterns observed between bacterial members in the same two dishwasher samples, indicating cooperative effects. Furthermore, two synergistic four-species bacterial consortia were tested for their abilities to incorporate an opportunistic fungal pathogen, Exophiala dermatitidis and their establishment as biofilms on sterile ethylene propylene diene monomer M-class (EPDM) rubber and polypropylene (PP) surfaces. When the bacterial consortia included E. dermatitidis , the overall cell numbers of both bacteria and fungi increased and a substantial increase in biofilm biomass was observed. These results indicate a novel phenomenon of cross kingdom synergy in biofilm formation and these observations could have potential implications for human health.
Zupančič, Jerneja; Raghupathi, Prem K.; Houf, Kurt; Burmølle, Mette; Sørensen, Søren J.; Gunde-Cimerman, Nina
2018-01-01
Biofilms formed on rubber seals in dishwashers harbor diverse microbiota. In this study, we focussed on the microbial composition of bacteria and fungi, isolated from a defined area of one square centimeter of rubber from four domestic dishwashers and assessed their abilities to in vitro multispecies biofilm formation. A total of 80 isolates (64 bacterial and 16 fungal) were analyzed. Multiple combinations of bacterial isolates from each dishwasher were screened for synergistic interactions. 32 out of 140 tested (23%) four-species bacterial combinations displayed consistent synergism leading to an overall increase in biomass, in all experimental trails. Bacterial isolates from two of the four dishwashers generated a high number of synergistically interacting four-species consortia. Network based correlation analyses also showed higher co-occurrence patterns observed between bacterial members in the same two dishwasher samples, indicating cooperative effects. Furthermore, two synergistic four-species bacterial consortia were tested for their abilities to incorporate an opportunistic fungal pathogen, Exophiala dermatitidis and their establishment as biofilms on sterile ethylene propylene diene monomer M-class (EPDM) rubber and polypropylene (PP) surfaces. When the bacterial consortia included E. dermatitidis, the overall cell numbers of both bacteria and fungi increased and a substantial increase in biofilm biomass was observed. These results indicate a novel phenomenon of cross kingdom synergy in biofilm formation and these observations could have potential implications for human health. PMID:29441043
Influence of melt mixer on injection molding of thermoset elastomers
NASA Astrophysics Data System (ADS)
Rochman, Arif; Zahra, Keith
2016-10-01
One of the drawbacks in injection molding is that the plasticizing screw is short such that polymers having high concentrations of additives, such as thermoset elastomers, might not mix homogeneously within the short period of time during the plasticizing stage. In this study, various melt mixers inside the nozzle chamber, together forming a mixing nozzle, were developed. Three different materials were investigated, namely nitrile butadiene rubber (NBR), ethylene propylene-diene monomer (EPDM) and fluorocarbon (FKM). The use of these melt mixers resulted in better homogeneity and properties of the molded parts despite a curing time reduction of 10 s. This was due to the increase in mixing and shearing introduced a higher rate of crosslinking formation in the molded parts.
NASA Technical Reports Server (NTRS)
Law, R. D.
1989-01-01
A contaminant is any material or substance which is potentially undesirable or which may adversely affect any part, component, or assembly. Contamination control of SRM hardware surfaces is a serious concern, for both Thiokol and NASA, with particular concern for contaminants which may adversely affect bonding surfaces. The purpose of this study is to develop laboratory analytical techniques which will make it possible to certify the cleanliness of any designated surface, with special focus on particulates (dust, dirt, lint, etc.), oils (hydrocarbons, silicones, plasticizers, etc.), and greases (HD-2, fluorocarbon grease, etc.). The hardware surfaces of concern will include D6AC steel, aluminum alloys, anodized aluminum alloys, glass/phenolic, carbon/phenolic, NBR/asbestos-silica, and EPDM rubber.
Flame-retardant EPDM compounds containing phenanthrene to enhance radiation resistance
NASA Astrophysics Data System (ADS)
Chen, Jian; Huang, Wei; Jiang, Shu-Bin; Li, Xiao-Yan; An, You; Li, Chuang; Gao, Xiao-Ling; Chen, Hong-Bing
2017-01-01
Ethylene propylene diene monomer (EPDM) compounds with good flame-retardant and γ-ray radiation resistant properties were prepared by adding complex flame retardants and phenathrene. The resultant EPDM formulations have a long time to ignition (TTI >46 s), a low peak heat release rate (PHRR 341 kW/m2) and a high limited oxygen index (LOI >30). Effects of γ-ray radiation on the resultant flame-retardant EPDM was investigated. The formulated EPDM is a crosslinking dominated polymer under γ-ray radiation. The γ-ray radiation resistant property of EPDM was enhanced by adding phenanthrene. Elongation at break of EPDM formulated with phenanthrene could retain 91% after being irradiated to 0.3 MGy and still retains 40% elongation even after being irradiated to 0.9 MGy, which is much better the control. It is expected that the formulated flame-retardant and radiation resistant EPDM materials could meet the requirements for use in radiation environments.
Szczotko, Maciej; Stankiewicz, Agnieszka; Jamsheer-Bratkowska, Małgorzata
Plumbing materials in water distribution networks and indoor installations are constantly evolving. The application of new, more economical solutions with plastic materials eliminates the corrosion problems, however, do not fully protect the consumer against secondary microbial contamination of water intended for human consumption caused by the presence of a biofilm on the inner surface of materials applied. National Institute of Public Health - National Institute of Hygiene conducts research aimed at a comprehensive assessment of this type of materials, resulting their further marketing authorization in Poland. Evaluation and comparison of polymer and rubber materials intended to contact with water for the susceptibility to biofilm formation. Plastic materials (polyethylene, polypropylene, polyvinyl chloride) and rubber compounds (EPDM, NBR), from different manufacturers were evaluated. The study was carried out on 37 samples, which were divided into groups according to the material of which they were made. The testing was conducted according to the method based on conditions of dynamic flow of tap water. The level of bioluminescence in swabs taken from the surface of the tested materials was investigated with a luminometer. Evaluation of plastic materials does not show major objections in terms of hygienic assessment. All materials met the evaluation criteria established for methodology used. In case of rubber compounds, a substantial part clearly exceeded the limit values, which resulted in their negative assessment and elimination of these materials from domestic market. High susceptibility to the formation of biofilm in the group of products made of rubber compounds has been demonstrated. Examined plastic materials, except for several cases, do not revealed susceptibility to biofilm formation, but application of plastics for distribution of water intended for human consumption does not fully protect water from secondary, microbiological contamination. Complete verification of plumbing materials including biofilm formation test before their introduction into the domestic market should be continued.
Schoberleitner, Christoph; Archodoulaki, Vasiliki-Maria; Koch, Thomas; Lüftl, Sigrid; Werderitsch, Markus; Kuschnig, Gerhard
2013-01-01
To develop a matched sealing material for socket rehabilitation of grey cast iron pipes, an epoxy resin is modified by the addition of different components to improve the flexibility. Three different modifications are made by adding ethylene-propylene diene monomer (EPDM) rubber powder, reactive liquid polymer (ATBN) and epoxidized modifier. In this paper the effect of the modification method as well as the influence of absorption of water on the mechanical and physical properties are analyzed in terms of: tensile strength, modulus of elasticity, adhesion performance, pressure resistance, glass transition temperature and water content. A comparison with neat epoxy shows for all materials that the modulus of elasticity and strength decrease. Unlike other tested modification methods, the modification with rubber powder did not enhance the flexibility. All materials absorb water and a plasticization effect arises with further changes of mechanical and physical properties. The application of the sealant on the grey cast iron leads to a reduction of the strain at break (in comparison to the common tensile test of the pure materials) and has to be evaluated. The main requirement of pressure resistance up to 1 MPa was tested on two chosen materials. Both materials fulfill this requirement. PMID:28788404
Schoberleitner, Christoph; Archodoulaki, Vasiliki-Maria; Koch, Thomas; Lüftl, Sigrid; Werderitsch, Markus; Kuschnig, Gerhard
2013-11-27
To develop a matched sealing material for socket rehabilitation of grey cast iron pipes, an epoxy resin is modified by the addition of different components to improve the flexibility. Three different modifications are made by adding ethylene-propylene diene monomer (EPDM) rubber powder, reactive liquid polymer (ATBN) and epoxidized modifier. In this paper the effect of the modification method as well as the influence of absorption of water on the mechanical and physical properties are analyzed in terms of: tensile strength, modulus of elasticity, adhesion performance, pressure resistance, glass transition temperature and water content. A comparison with neat epoxy shows for all materials that the modulus of elasticity and strength decrease. Unlike other tested modification methods, the modification with rubber powder did not enhance the flexibility. All materials absorb water and a plasticization effect arises with further changes of mechanical and physical properties. The application of the sealant on the grey cast iron leads to a reduction of the strain at break (in comparison to the common tensile test of the pure materials) and has to be evaluated. The main requirement of pressure resistance up to 1 MPa was tested on two chosen materials. Both materials fulfill this requirement.
Surface degradation of polymer insulators under accelerated climatic aging in weather-ometer
DOE Office of Scientific and Technical Information (OSTI.GOV)
Xu, G.; McGrath, P.B.; Burns, C.W.
1996-12-31
Climatic aging experiments were conducted on two types of outdoor polymer insulators by using a programmable weather-ometer. The housing materials for the insulators were silicone rubber (SR) and ethylene propylene diene monomer (EPDM). The accelerated aging stresses were comprised of ultraviolet radiation, elevated temperature, temperature cycling, thermal shock and high humidity. Their effects on the insulator surface conditions and electrical performance wee examined through visual inspection and SEM studies, contact angle measurements, thermogravimetric analysis (TGA), energy dispersive spectroscopy (EDS) analysis, and 50% impulse flashover voltage tests. The results showed a significant damage on the insulator surface caused by some ofmore » the imposed aging stresses. The EDS analysis suggested a photooxidation process that happened on the insulator surface during the aging period.« less
NASA Astrophysics Data System (ADS)
Matsunaga, G.; Okabayashi, M.; Aiba, N.; Boedo, J. A.; Ferron, J. R.; Hanson, J. M.; Hao, G. Z.; Heidbrink, W. W.; Holcomb, C. T.; In, Y.; Jackson, G. L.; Liu, Y. Q.; Luce, T. C.; McKee, G. R.; Osborne, T. H.; Pace, D. C.; Shinohara, K.; Snyder, P. B.; Solomon, W. M.; Strait, E. J.; Turnbull, A. D.; Van Zeeland, M. A.; Watkins, J. G.; Zeng, L.; the DIII-D Team; the JT-60 Team
2013-12-01
In the wall-stabilized high-β plasmas in JT-60U and DIII-D, interactions between energetic particle (EP) driven modes (EPdMs) and edge localized modes (ELMs) have been observed. The interaction between the EPdM and ELM are reproducibly observed. Many EP diagnostics indicate a strong correlation between the distorted waveform of the EPdM and the EP transport to the edge. The waveform distortion is composed of higher harmonics (n ⩾ 2) and looks like a density snake near the plasma edge. According to statistical analyses, ELM triggering by the EPdMs requires a finite level of waveform distortion and pedestal recovery. ELM pacing by the EPdMs occurs when the repetition frequency of the EPdMs is higher than the natural ELM frequency. EPs transported by EPdMs are thought to contribute to change the edge stability.
Effect of electron beam irradiation on thermal and crystallization behavior of PP/EPDM blend
NASA Astrophysics Data System (ADS)
Balaji, Anand Bellam; Ratnam, Chantara Thevy; Khalid, Mohammad; Walvekar, Rashmi
2017-12-01
The irradiation stability of ethylene-propylene diene terpolymer (EPDM)/ polypropylene (PP) blends is studied in an attempt to develop radiation compatible PP/EPDM blends suitable for medical applications. The PP/EPDM blends with mixing ratios of 80/20, 50/50/ 20/80 were prepared in an internal mixer at 165 °C and a rotor speed of 50 rpm followed by compression molding. The blends and the individual components were irradiated using 3.0 MeV electron beam (EB) accelerator at doses ranging from 0 to 100 kGy in air and room temperature. Later, the PP/EPDM blends were subjected to gel content, thermal stability, crystallization and dynamic mechanical properties before and after irradiation. Results revealed that the irradiation-induced crosslinking in the PP/EPDM blend increases with the increasing irradiation dose and the EPDM content in the blend. However, the thermal stability of the blends did not show any significant changes upon irradiation. The dynamic mechanical analysis shows that the EPDM rich blend has higher compatibility than PP dominant blends. A further improvement in the blend compatibility found to be achieved upon irradiation.
Novel percolation phenomena and mechanism of strengthening elastomers by nanofillers.
Wang, Zhenhua; Liu, Jun; Wu, Sizhu; Wang, Wenchuan; Zhang, Liqun
2010-03-28
Nano-strengthening by employing nanoparticles is necessary for high-efficiency strengthening of elastomers, which has already been validated by numerous researches and industrial applications, but the underlying mechanism is still an open challenge. In this work, we mainly focus our attention on studying the variation of the tensile strength of nanofilled elastomers by gradually increasing the filler content, within a low loading range. Interestingly, the percolation phenomenon is observed in the relationship between the tensile strength and the filler loading, which shares some similarities with the percolation phenomenon occurring in rubber toughened plastics. That is, as the loading of nanofillers (carbon black, zinc oxide) increases, the tensile strength of rubber nanocomposites (SBR, EPDM) increases slowly at first, then increases abruptly and finally levels off. Meanwhile, the bigger the particle size, the higher the filler content at the percolation point, and the lower the corresponding tensile strength of rubber nanocomposites. The concept of a critical particle-particle distance (CPD) is proposed to explain the observed percolation phenomenon. It is suggested that rubber strengthening through nanoparticles is attributed to the formation of stretched straight polymer chains between neighbor particles, induced by the slippage of adsorbed polymer chains on the filler surface during tension. Meanwhile, the factors to govern this CPD and the critical minimum particle size (CMPS) figured out in this work are both discussed and analyzed in detail. Within the framework of this percolation phenomenon, this paper also clearly answers two important and intriguing issues: (1) why is it necessary and essential to strengthen elastomers through nanofillers; (2) why does it need enough loading of nanofillers to effectively strengthen elastomers. Moreover, on the basis of the percolation phenomenon, we give out some guidance for reinforcement design of rubbery materials: the interfacial interactions between rubber and fillers cannot be complete chemical bonding, and partial physical absorption of macromolecular chains on the filler surface is necessary, otherwise the formation of stretched straight chains would be seriously hindered. There should exist such an optimum crosslinking density for a certain filler reinforced rubber system, and as well an optimum filler loading for rubber strengthening. Additionally, the different percolation behaviors of Young's modulus, the tensile strength and the electrical conductivity are compared and analyzed in our work. Lastly, molecular simulation indicates that it is not possible to strengthen glassy or hard polymer matrices by incorporating spherical nanoparticles. In general, by providing substantial experimental data and detailed analyses, this work is believed to promote the fundamental understanding of rubber reinforcement, as well provide better guidance for the design of high-performance and multi-functional rubber nanocomposites.
Palenzuela, D O; Benítez, J; Rivero, J; Serrano, R; Ganzó, O
1997-10-13
In the present work a concept proposed in 1992 by Dopotka and Giesendorf was applied to the quantitative analysis of antibodies to the p24 protein of HIV-1 in infected asymptomatic individuals and AIDS patients. Two approaches were analyzed, a linear model OD = b0 + b1.log(titer) and a nonlinear log(titer) = alpha.OD beta, similar to the Dopotka-Giesendorf's model. The above two proposed models adequately fit the dependence of the optical density values at a single point dilution, and titers achieved by the end point dilution method (EPDM). Nevertheless, the nonlinear model better fits the experimental data, according to residuals analysis. Classical EPDM was compared with the new single point dilution method (SPDM) using both models. The best correlation between titers calculated using both models and titers achieved by EPDM was obtained with the nonlinear model. The correlation coefficients for the nonlinear and linear models were r = 0.85 and r = 0.77, respectively. A new correction factor was introduced into the nonlinear model and this reduced the day-to-day variation of titer values. In general, SPDM saves time, reagents and is more precise and sensitive to changes in antibody levels, and therefore has a higher resolution than EPDM.
XPS analysis of Al/EPDM bondlines from IUS SRM-1 polar bosses
NASA Astrophysics Data System (ADS)
Hemminger, Carol S.; Marquez, Nicholas
1993-03-01
A temperature-stress rupture method using partial immersion in liquid nitrogen was developed for the aluminum/EPDM rubber insulation bondline of the IUS SRM-1 polar bosses in order to investigate a corrosion problem. Subsequent XPS analysis of the ruptured bondline followed changes in the locus of failure as corrosion progressed. Samples from the forward polar bosses had a predominantly noncorroded appearance on the ruptured surfaces. The locus of failure was predominantly through the primer layer, which is distinguished by a high concentration of chlorinated hydrocarbon. The aft polar boss segments analyzed were characterized by the presence of corrosion over the entire mid-section of the ruptured aluminum to insulation bondline. The predominant corrosion product detected was aluminum oxide/hydroxide. The corroded bondline sections had significantly higher concentrations of aluminum oxide/hydroxide than the noncorroded areas, and lower concentrations of primer material. The temperature-stress rupture appeared to progress most readily through areas of thickened aluminum oxide/hydroxide infiltrated into the primer layer. In general there was a very good correlation between the calculated Cl:Al atomic % ratio, and the visual characterization of the extent of corrosion. The Cl:Al ratio, which represents the primer to corrosion product ratio at the locus of failure, varied from 0.4 to 47. With only a few exceptions, surfaces with a predominantly noncorroded appearance had Cl:Al ratios greater than 2, and surfaces with a heavily corroded appearance had Cl:Al ratios less than 1.
Structural analysis of nanocomposites based on HDPE/EPDM blends.
Zitzumbo, Roberto; Alonso, Sergio; Avalos, Felipe; Ortiz, José C; López-Manchado, Miguel A; Arroyo, Miguel
2006-02-01
Intercalated and exfoliated nanocomposites based on HDPE and EPDM blends with an organoclay have been obtained through the addition of EPDM-g-MA as a compatibilizer. The combined effect of clay and EPDM-g-MA on the rheological behaviour is very noticeable with a sensible increase in viscosity which suggests the formation of a structural net of percolation induced by the presence of intercalated and exfoliated silicate layer. As deduced from rheological studies, a morphology based on nanostructured micro-domains dispersed in HDPE continuous phase is proposed for EPDM/HDPE blend nanocomposites. XRD and SEM analysis suggest that two different transport phenomena take simultaneously place during the intercalation process in the melt. One due to diffusion of HDPE chains into the tactoid and the other to diffusion of EPDM-g-MA into the silicate galleries.
Incorporation of High Energy Materials Into High Density Polymers
1987-09-21
and the pure graft copolymer was isolated by selective solvent extraction. 5 f. Isolation of pure Qraft copolymers. The isolation of pure EPDM -g-PS...characterized, such as EPDM -g-PST and EPDM -g-PMST. Two methods of synthesis were successful: a macromonomer (a polymer containing a polymerizab head group) was...copolymerized with ethylene and propylene to lead to the final product, and chlorination of a commercial EPDM allowed the chlorinated sites to serve as
Basuli, Utpal; Jose, Jobin; Lee, Ran Hee; Yoo, Yong Hwan; Jeong, Kwang-Un; Ahn, Jou-Hyeon; Nah, Changwoon
2012-10-01
Proton exchange membrane (PEM) fuel cell stack requires gaskets and seals in each cell to keep the reactant gases within their respective regions. Gasket performance is integral to the successful long-term operation of a fuel cell stack. This review focuses on properties, performance and degradation mechanisms of the different polymer gasket materials used in PEM fuel cell under normal operating conditions. The different degradation mechanisms and their corresponding representative mitigation strategies are also presented here. Summary of various properties of elastomers and their advantages and disadvantages in fuel cell'environment are presented. By considering the level of chemical degradation, mechanical properties and cost effectiveness, it can be proposed that EPDM is one of the best choices for gasket material in PEM fuel cell. Finally, the challenges that remain in using rubber component as in PEM fuel cell, as well as the prospects for exploiting them in the future are discussed.
Bright is the New Black - Multi-Year Performance of Generic High-Albedo Roofs in an Urban Climate
NASA Technical Reports Server (NTRS)
Gaffin, S. R.; Imhoff, M.; Rosenzweig, C.; Khanbilvardi, R.; Pasqualini, A.; Kong, A. Y. Y.; Grillo, D.; Freed, A.; Hillel, D.; Hartung, E.
2012-01-01
High-albedo white and cool roofing membranes are recognized as a fundamental strategy that dense urban areas can deploy on a large scale, at low cost, to mitigate the urban heat island effect. We are monitoring three generic white membranes within New York City that represent a cross-section of the dominant white membrane options for U.S. flat roofs: (1) an ethylene propylene diene monomer (EPDM) rubber membrane; (2) a thermoplastic polyolefin (TPO) membrane and; (3) an asphaltic multi-ply built-up membrane coated with white elastomeric acrylic paint. The paint product is being used by New York City s government for the first major urban albedo enhancement program in its history. We report on the temperature and related albedo performance of these three membranes at three different sites over a multi-year period. The results indicate that the professionally installed white membranes are maintaining their temperature control effectively and are meeting the Energy Star Cool Roofing performance standards requiring a three-year aged albedo above 0.50. The EPDM membrane however shows evidence of low emissivity. The painted asphaltic surface shows high emissivity but lost about half of its initial albedo within two years after installation. Given that the acrylic approach is an important "do-it-yourself," low-cost, retrofit technique, and, as such, offers the most rapid technique for increasing urban albedo, further product performance research is recommended to identify conditions that optimize its long-term albedo control. Even so, its current multi-year performance still represents a significant albedo enhancement for urban heat island mitigation.
DOE Office of Scientific and Technical Information (OSTI.GOV)
Fondeur, F. F.
The Office of Waste Processing, within the Office of Technology Innovation and Development, funded the development of an enhanced Caustic-Side Solvent Extraction (CSSX) solvent for deployment at the Savannah River Site for removal of cesium from High Level Waste. This effort lead to the development of the Next Generation Solvent (NGS) with Tris (3,7-dimethyl octyl) guanidine (TiDG). The first deployment target for the NGS solvent is within the Modular CSSX Unit (MCU). Deployment of a new chemical within an existing facility requires verification that the new chemical components are compatible with the installed equipment. In the instance of a newmore » organic solvent, the primary focus is on compatibility of the solvent with organic polymers used in the affected facility. This report provides the calculated data from exposing these polymers to the Next Generation Solvent. An assessment of the dimensional stability of polymers known to be used or present in the MCU, Defense Waste Processing Facility (DWPF), and Saltstone facilities that will be exposed to the NGS showed that TiDG could selectively affect the elastomers and some thermoplastics to varying extents, but the typical use of these polymers in a confined geometry will likely prevent the NGS from impacting component performance. The polymers identified as of primary concern include Grafoil® (flexible graphite), Tefzel®, Isolast®, ethylene-propylene-diene monomer (EPDM) rubber, nitrile-butadiene rubber (NBR), styrene-butadiene rubber (SBR), ultra high molecular weight polyethylene (UHMWPE), and fluorocarbon rubber (FKM). Certain polymers like NBR and EPDM were found to interact mildly with NGS but their calculated swelling and the confined geometry will impede interaction with NGS. In addition, it was found that Vellumoid (cellulose fibers-reinforced glycerin and protein) may leach protein and Polyvinyl Chloride (PVC) may leach plasticizer (such as Bis-Ethylhexyl-Phthalates) into the NGS solvent. Either case will not impact decontamination or immobilization operations at Savannah River Site (SRS). Some applications have zero tolerance for dimensional changes such as the operation of valves while other applications a finite dimensional change improves the function of the application such as seals and gaskets. Additional considerations are required before using the conclusions from this work to judge outcomes in field applications. Decane, a component of Isopar L that is most likely to interact with the polymers, mildly interacted with the elastomers and the propylene based polymers but their degree of swelling is at most 10% and the confined geometry that they are typically placed in indicate this is not significant. In addition, it was found that Vellumoid may leach protein into the NGS solvent. Since Vellumoid is used at the mixer in Saltstone where it sees minimum quantities of solvent, this leaching has no effect on the extraction process at MCU or the immobilization process at saltstone. No significant interaction is expected between MaxCalix and the polymers and elastomers used at MCU, DWPF, and Saltstone. Overall, minimal and insignificant interactions are expected on extraction and immobilization operations when MCU switches from CSSX to NGS solvent. It is expected that contacting NGS will not accelerate the aging rate of polymers and elastomers under radiation and heat. This is due to the minimal interaction between NGS and the polymers and the confined geometries for these polymers. SRNL recommends the use of the HSP method (for screening) and some testing to evaluate the impact of other organic such as alcohols, glycolate, and their byproducts on the polymers used throughout the site.« less
Dependence of particle volume fraction on sound velocity and attenuation of EPDM composites.
Kim, K S; Lee, K I; Kim, H Y; Yoon, S W; Hong, S H
2007-05-01
The sound velocity and the attenuation coefficient of EPDM (Ethylene-propylene Diene Monomer) composites incorporated with Silicon Carbide particles (SiCp's) of various volume fractions (0-40%) were experimentally and theoretically investigated. For the experiment a through-transmission technique was used. For the theoretical prediction, some mechanical property models such as Reuss model and Coherent Potential Approximation (CPA) model etc. were employed. The experimental results showed that the sound velocity decreased with the increase of the SiCp volume fraction up to 30% and then increased with the 40 vol% specimen. The attenuation coefficient was increased with the increasing SiCp volume fractions. The modified Reuss model with a longitudinal elastic modulus predicted most well the experimental sound velocity and elastic modulus results.
Effect of EPDM-g-MAH on properties of HDPE/OBC blends
NASA Astrophysics Data System (ADS)
Li, M.; Yu, L. Y.; Li, P. F.; Bin, Y. H.; Zhang, H. J.
2017-04-01
In this paper, we take the HDPE as the matrix material, OBC as the toughening material, and EDPM-g-MAH as the compatibility agent, HDPE/OBC/EPDM-g-MAH blends were prepared by high speed mixing, melt extrusion, injection molding and so on. The effects of OBC and EPDM-g-MAH on mechanical properties, crystalline properties, fracture surface structure and rheological properties of HDPE were analyzed by universal tensile tester, melt mass flow rate test machine, DSC and SEM. Experimental results show that: with the addition of EPDM-g-MAH, the notched impact strength of the blends increased first and then decreased; HDPE/OBC blend containing 4% EPDM-g-MAH, OBC dispersion in the matrix is more uniform, particle size is significantly refined, melt flow has some improvement, Compared with HDPE/OBC blend materials, notched impact strength and elongation at break increased by 41.07% and 107.28% respectively, the toughness of the blend was greatly improved.
Bright is the new black—multi-year performance of high-albedo roofs in an urban climate
NASA Astrophysics Data System (ADS)
Gaffin, S. R.; Imhoff, M.; Rosenzweig, C.; Khanbilvardi, R.; Pasqualini, A.; Kong, A. Y. Y.; Grillo, D.; Freed, A.; Hillel, D.; Hartung, E.
2012-03-01
High-albedo white and cool roofing membranes are recognized as a fundamental strategy that dense urban areas can deploy on a large scale, at low cost, to mitigate the urban heat island effect. We are monitoring three generic white membranes within New York City that represent a cross section of the dominant white membrane options for US flat roofs: (1) an ethylene-propylene-diene monomer (EPDM) rubber membrane; (2) a thermoplastic polyolefin (TPO) membrane; and (3) an asphaltic multi-ply built-up membrane coated with white elastomeric acrylic paint. The paint product is being used by New York City’s government for the first major urban albedo enhancement program in its history. We report on the temperature and related albedo performance of these three membranes at three different sites over a multi-year period. The results indicate that the professionally installed white membranes are maintaining their temperature control effectively and are meeting the Energy Star Cool Roofing performance standards requiring a three-year aged albedo above 0.50. The EPDM membrane shows evidence of low emissivity; however this had the interesting effect of avoiding any ‘winter heat penalty’ for this building. The painted asphaltic surface shows high emissivity but lost about half of its initial albedo within two years of installation. Given that the acrylic approach is such an important ‘do-it-yourself’, low-cost, retrofit technique, and, as such, offers the most rapid technique for increasing urban albedo, further product performance research is recommended to identify conditions that optimize its long-term albedo control. Even so, its current multi-year performance still represents a significant albedo enhancement for urban heat island mitigation.
DOE Office of Scientific and Technical Information (OSTI.GOV)
Godail, M.J.
1983-08-01
The properties of paraffinic, naphthenic, and aromatic extender oils used as EPDM plasticizers are discussed in detail. Particular attention is given to viscosity, volatility, specific gravity, and aromatic content.
NASA Technical Reports Server (NTRS)
Guillot, David G. (Inventor); Harvey, Albert R. (Inventor)
2003-01-01
A novel and improved EPDM formulation for a solid propellant rocket motor is described wherein hexadiene EPDM monomer components are replaced by alkylidene norbornene components and with appropriate adjustment of curing and other additives functionally-required rheological and physical characteristics are achieved with the desired compatibility with any one of a plurality of solid filler materials, e.g. powder silica, carbon fibers or aramid fibers, and with appropriate adhesion and extended storage or shelf life characteristics.
NASA Technical Reports Server (NTRS)
Guillot, David G. (Inventor); Harvey, Albert R. (Inventor)
2008-01-01
A novel and improved EPDM formulation for a solid propellant rocket motor is described wherein hexadiene EPDM monomer components are replaced by alkylidene norbornene components, and, with appropriate adjustment of curing and other additives, functionally required rheological and physical characteristics are achieved with the desired compatibility with any one of a plurality of solid filler materials, e.g., powder silica, carbon fibers or aramid fibers, and with appropriate adhesion and extended storage or shelf-life characteristics.
NASA Technical Reports Server (NTRS)
Guillot, David G. (Inventor); Harvey, Albert R. (Inventor)
2004-01-01
A novel and improved EPDM formulation for a solid propellant rocket motor is described wherein hexadiene EPDM monomer components are replaced by alkylidene norbornene components, and, with appropriate adjustment of curing and other additives, functionally required rheological and physical characteristics are achieved with the desired compatibility with any one of a plurality of solid filler materials, e.g., powder silica, carbon fibers or aramid fibers, and with appropriate adhesion and extended storage or shelf-life characteristics.
Integrated residential photovoltaic array development
NASA Technical Reports Server (NTRS)
Royal, G. C., III
1981-01-01
Sixteen conceptual designs of residential photovoltaic arrays are described. Each design concept was evaluated by an industry advisory panel using a comprehensive set of technical, economic and institutional criteria. Key electrical and mechanical concerns that effect further array subsystem development are also discussed. Three integrated array design concepts were selected by the advisory panel for further optimization and development. From these concepts a single one will be selected for detailed analysis and prototype fabrication. The three concepts selected are: (1) An array of frameless panels/modules sealed in a T shaped zipper locking neoprene gasket grid pressure fitted into an extruded aluminum channel grid fastened across the rafters. (2) An array of frameless modules pressure fitted in a series of zipper locking EPDM rubber extrusions adhesively bonded to the roof. Series string voltage is developed using a set of integral tongue connectors and positioning blocks. (3) An array of frameless modules sealed by a silicone adhesive in a prefabricated grid of rigid tape and sheet metal attached to the roof.
Radiochemical ageing of EPDM elastomers. 3. Mechanism of radiooxidation
NASA Astrophysics Data System (ADS)
Rivaton, A.; Cambon, S.; Gardette, J.-L.
2005-01-01
The preceding paper of this series was devoted to the identification and quantification of the main chemical changes resulting from the radiochemical ageing of EPDM (77.9% ethylene, 21.4% propylene, 0.7% diene) and EPR (76.6% ethylene, 23.4% propylene) films irradiated under oxygen atmosphere using 60Co gamma rays. The double bond of the diene was observed to be consumed with a high radiochemical yield. The oxidation and reticulation rates were observed to be higher in the case of EPDM than in EPR. Accumulation of the major oxidation products in both polymers was shown to occur in the order of decreasing concentrations: hydroperoxides, ketones, carboxylic acids and alcohols, peroxides. On the basis of the analysis of the oxidation products formed in EPDM and EPR, and taking into account their relative concentrations, the mechanisms accounting for the EPDM γ-degradation under oxygen atmosphere are proposed in the present paper. Two main processes are involved in the EPDM radiooxidation. The random γ-radiolysis of the polymer provides a constant source of macroalkyl radicals mainly formed on ethylene units. The secondary radicals so formed are likely to initiate a selective oxidation of the polymer through free-radicals reactions involving the abstraction of labile hydrogen atoms. In particular, the hydroperoxides decomposition and the consumption of the ENB moieties, this latter being the most oxidisable site and the source of crosslinking, may result from hydrogen abstraction by radical species.
A proven elastomer compound for extremely hostile geothermal and oil field environments
DOE Office of Scientific and Technical Information (OSTI.GOV)
Hirasuna, A.R.; Friese, G.J.; Stephens, C.A.
1983-02-01
Since 1979 the Y267 EPDM elastomer has been independently tested by other organizations in a variety of field and laboratory applications. The following are some examples. The same Y267 EPDM O-rings worked with no leaks as logging tool seals for multiple trips to 4600M (15k ft.) at 320/sup 0/C (608F) BHST. A packer element performed flawlessly for five months in a 204/sup 0/C (400F) continuous steam injection well and was retrieved at the end of the test in an as-new condition. A high-pressure Y267 EPDM packer test was performed with complete success at 232/sup 0/C (450F) for a 7.5 daymore » test in sour crude with differential pressures to 138 MPa (20 ksi) and the seal condition was only very slightly changed by the test. Comprehensive compatibility testing of 34 compounds from 15 companies in geothermal brine, isobutane, and oil at 191C-266/sup 0/C (375-510F) showed that the Y267 EPDM was best of the 34 in all three fluids. Over 15 laboratory and over 20 field case histories of Y267 EPDM such as the above examples are reported. All strongly establish that Y267 EPDM is at the cutting edge of technology.« less
DOE Office of Scientific and Technical Information (OSTI.GOV)
Datta, S.; Cheremishinoff, N.P.; Kresge, E.N.
1993-12-31
Rapid extrusion of EPDM elastomers require low viscosity and thus low molecular weights for the polymer. Efficient vulcanization of these elastomers requires network perfection and thus high molecular weights for the polymer. The benefits of these apparently mutually exclusive goals is important in uses of EPDM elastomers which require extrusion of profiles which are later cured. This paper shows that by introducing simultaneously asymmetry in the distribution of molecular weights, crystallinity and vulcanizable sites these apparently contradictory goals can be resolved. While these polymers cannot be made from a single Ziegler polymerization catalyst, the authors show the synthesis of thesemore » model EPDM polymers by blending polymers with very different molecular weights, ethylene and ENB contents. These blends can be rapidly extruded without melt fracture and can be cured to vulcanizates which have excellent tensile properties.« less
Gabrielle, Brice; Lorthioir, Cédric; Lauprêtre, Françoise
2011-11-03
The possible influence of micrometric-size filler particles on the thermo-oxidative degradation behavior of the polymer chains at polymer/filler interfaces is still an open question. In this study, a cross-linked ethylene-propylene-diene (EPDM) terpolymer filled by aluminum trihydrate (ATH) particles is investigated using (1)H solid-state NMR. The time evolution of the EPDM network microstructure under thermal aging at 80 °C is monitored as a function of the exposure time and compared to that of an unfilled EPDM network displaying a similar initial structure. While nearly no variations of the topology are observed on the neat EPDM network over 5 days at 80 °C, a significant amount of chain scission phenomena are evidenced in EPDM/ATH. A specific surface effect induced by ATH on the thermodegradative properties of the polymer chains located in their vicinity is thus pointed out. Close to the filler particles, a higher amount of chain scissions are detected, and the characteristic length scale related to these interfacial regions displaying a significant thermo-oxidation process is determined as a function of the aging time.
Fricke, Julia; Hillebrand, Andrea; Twyman, Richard M; Prüfer, Dirk; Schulze Gronover, Christian
2013-04-01
Natural rubber is a high-molecular-mass biopolymer found in the latex of >2,500 plant species, including Hevea brasiliensis, Parthenium argentatum and Taraxacum spp. The active sites of rubber biosynthesis are rubber particles, which comprise a hydrophobic rubber core surrounded by a phospholipid monolayer membrane containing species-dependent lipids and associated proteins. Small rubber particle proteins are the most abundant rubber particle-associated proteins in Taraxacum brevicorniculatum (TbSRPPs) and may promote rubber biosynthesis by stabilizing the rubber particle architecture. We investigated the transcriptional regulation of genes encoding SRPPs and identified a bZIP transcription factor (TbbZIP.1) similar to the Arabidopsis thaliana ABI5-ABF-AREB subfamily, which is thought to include downstream targets of ABA and/or abiotic stress-inducible protein kinases. The TbbZIP.1 gene was predominantly expressed in laticifers and regulates the expression of TbSRPP genes in an ABA-dependent manner. The individual TbSRPP genes showed distinct induction profiles, suggesting diverse roles in rubber biosynthesis and stress adaptation. The potential involvement of TbSRPPs in the adaptation of T. brevicorniculatum plants to environmental stress is discussed based on our current knowledge of the stress-response roles of SRPPs and their homologs, and the protective function of latex and rubber against pathogens. Our data suggest that TbSRPPs contribute to stress tolerance in T. brevicorniculatum and that their effects are mediated by TbbZIP.1.
1983-06-01
NOTES 19. KEY WORDS (Continue on reveree side if necesaary and Identify by block number) Neoprene Synthetic Liners TCE, XR-5, EPDM Hypalon Compatibility...CPE, Hypalon , XR-5, HDPE, Neoprene, and EPDM ) were immersed in TNT, RDX, and TCE solutions for I week. Liner and test .*. method selection and data...Mean Weight Change Values - EPDM /Neoprene Group 57 Unexposed and in Distilled Water 7 Mean Weight Change Values - PVC Group in Distilled 58 Water and in
Aging Study Of EPDM O-Ring Material For The H1616 Shipping Package - Three Year Status
DOE Office of Scientific and Technical Information (OSTI.GOV)
Stefek, T.; Daugherty, W.; Skidmore, E.
This is a 3-year status report for tasks carried out per Task Technical Plan SRNL-STI-2011-00506. A series of tasks/experiments were performed at the Savannah River National Laboratory (SRNL) to monitor the aging performance of ethylene propylene diene monomer (EPDM) O-rings used in the H1616 shipping package. The test data provide a technical basis to extend the annual maintenance of the H1616 shipping package to three years and to predict the life of the EPDM O-rings at the bounding service conditions.
Effect of molecular weight on polymer processability
DOE Office of Scientific and Technical Information (OSTI.GOV)
Karg, R.F.
1983-01-01
Differences in rheological behavior due to the polymer molecular weight and molecular weight distribution have been shown with the MPT. SBR polymers having high molecular weight fractions develop higher stress relaxation time values due to the higher degree of polymer entanglements. Tests conducted at increasing temperatures show the diminishing influence of the polymer entanglements upon stress relaxation time. EPDM polymers show stress relaxation time and head pressure behavior which correlates with mill processability. As anticipated, compounded stock of EPDM have broad molecular weight distribution has higher stress relaxation time values than EPDM compounds with narrow molecular weight distribution.
Selvam, V; Senthil Kumar, P; Navaneetha Krishnan, G; Senthil Andavan, G T
2018-03-01
The original metal free graphitic carbon nitride/ethylene propylene diene monomer nanocomposite film (g-C 3 N 4 /EPDM NCF) was fabricated by facile solution cast method. g-C 3 N 4 /EPDM NCF with diameter (50mm) and thickness (4mm) was investigated towards the photocatalytic degradation of methylene blue (MB) and methyl orange (MO) dye solution under visible light irradiation. The as synthesized g-C 3 N 4 /EPDM NCF was exhibited high crystalline nature with the crystalline size of 21.53nm, the smooth surface nature and the particle size was observed from the TEM analysis is 20nm. Furthermore, the influence of operational parameters was carried out which demonstrated that 100mg photocatalyst and 25μM of dye concentration were obtained as an optimized condition for the best photocatalytic degradation results. As a result of scavenger experiment, it was concluded that the hydroxyl radical (OH) was actively involved in the photocatalytic degradation. The g-C 3 N 4 /EPDM NCF were recoverable from the photocatalytic reaction system and the present find findings may open up a new platform for the simple handpicked photocatalyst. Copyright © 2017 Elsevier B.V. All rights reserved.
Microstructure-based modelling of arbitrary deformation histories of filler-reinforced elastomers
NASA Astrophysics Data System (ADS)
Lorenz, H.; Klüppel, M.
2012-11-01
A physically motivated theory of rubber reinforcement based on filler cluster mechanics is presented considering the mechanical behaviour of quasi-statically loaded elastomeric materials subjected to arbitrary deformation histories. This represents an extension of a previously introduced model describing filler induced stress softening and hysteresis of highly strained elastomers. These effects are referred to the hydrodynamic reinforcement of rubber elasticity due to strain amplification by stiff filler clusters and cyclic breakdown and re-aggregation (healing) of softer, already damaged filler clusters. The theory is first developed for the special case of outer stress-strain cycles with successively increasing maximum strain. In this more simple case, all soft clusters are broken at the turning points of the cycle and the mechanical energy stored in the strained clusters is completely dissipated, i.e. only irreversible stress contributions result. Nevertheless, the description of outer cycles involves already all material parameters of the theory and hence they can be used for a fitting procedure. In the general case of an arbitrary deformation history, the cluster mechanics of the material is complicated due to the fact that not all soft clusters are broken at the turning points of a cycle. For that reason additional reversible stress contributions considering the relaxation of clusters upon retraction have to be taken into account for the description of inner cycles. A special recursive algorithm is developed constituting a frame of the mechanical response of encapsulated inner cycles. Simulation and measurement are found to be in fair agreement for CB and silica filled SBR/BR and EPDM samples, loaded in compression and tension along various deformation histories.
EFFECTS OF ONE WEEK TRITIUM EXPOSURE ON EPDM ELASTOMER
DOE Office of Scientific and Technical Information (OSTI.GOV)
Clark, E
This report documents test results for the exposure of four formulations of EPDM (ethylene-propylene diene monomer) elastomer to tritium gas at one atmosphere for approximately one week and characterization of material property changes and changes to the exposure gas during exposure. All EPDM samples were provided by Los Alamos National Laboratory (LANL). Material properties that were characterized include mass, sample dimensions, appearance, flexibility, and dynamic mechanical properties. The glass transition temperature was determined by analysis of the dynamic mechanical property data per ASTM standards. No change of glass transition temperature due to the short tritium gas exposure was observed. Filledmore » and unfilled formulations of Dupont{reg_sign} Nordel{trademark} 1440 had a slightly higher glass transition temperature than filled and unfilled formulations of Uniroyal{reg_sign} Royalene{reg_sign} 580H; filled formulations had the same glass transition as unfilled. The exposed samples appeared the same as before exposure--there was no evidence of discoloration, and no residue on stainless steel spacers contacting the samples during exposure was observed. The exposed samples remained flexible--all formulations passed a break test without failing. The unique properties of polymers make them ideal for certain components in gas handling systems. Specifically, the resiliency of elastomers is ideal for sealing surfaces, for example in valves. EPDM, initially developed in the 1960s, is a hydrocarbon polymer used extensively for sealing applications. EPDM is used for its excellent combination of properties including high/low-temperature resistance, radiation resistance, aging resistance, and good mechanical properties. This report summarizes initial work to characterize effects of tritium gas exposure on samples of four types of EPDM elastomer: graphite filled and unfilled formulations of Nordel{trademark} 1440 and Royalene{reg_sign} 580H.« less
NASA Astrophysics Data System (ADS)
Khattak, Abraiz; Amin, Muhammad; Iqbal, Muhammad; Abbas, Naveed
2018-02-01
Micro and nanocomposites of ethylene propylene diene monomer (EPDM) are recently studied for different characteristics. Study on life estimation and effects of multiple stresses on its dielectric strength and backbone scission and oxidation is also vital for endorsement of these composites for high voltage insulation and other outdoor applications. In order to achieve these goals, unfilled EPDM and its micro and nanocomposites are prepared at 23 phr micro silica and 6 phr nanosilica loadings respectively. Prepared samples are energized at 2.5 kV AC voltage and subjected for a long time to heat, ultraviolet radiation, acid rain, humidity and salt fog in accelerated manner in laboratory. Dielectric strength, leakage current and intensity of saturated backbone and carbonyl group are periodically measured. Loss in dielectric strength, increase in leakage current and backbone degradation and oxidation were observed in all samples. These effects were least in the case of EPDM nanocomposite. The nanocomposite sample also demonstrated longest shelf life.
Strain Sensing Characteristics of Rubbery Carbon Nanotube Composite for Flexible Sensors.
Choi, Gyong Rak; Park, Hyung-ki; Huh, Hoon; Kim, Young-Ju; Ham, Heon; Kim, Hyoun Woo; Lim, Kwon Taek; Kim, Sung Yong; Kang, Inpil
2016-02-01
In this study, the piezoresistive properties of CNT (Carbon Nanotube)/EPDM composite are characterized for the applications of a flexible sensor. The CNT/EPDM composites were prepared by using a Brabender mixer with MWCNT (Multi-walled Carbon Nanotube) and organoclay. The static and quasi-dynamic voltage output responses of the composite sensor were also experimentally studied and were compared with those of a conventional foil strain gage. The voltage output by using a signal processing system was fairly stable and it shows somehow linear responses at both of loading and unloading cases with hysteresis. The voltage output was distorted under a quasi-dynamic test due to its unsymmetrical piezoresistive characteristics. The CNT/EPDM sensor showed quite tardy response to its settling time test under static deflections and that would be a hurdle for its real time applications. Furthermore, since the CNT/EPDM sensor does not have directional voltage output to tension and compression, it only could be utilized as a mono-directional force sensor such as a compressive touch sensor.
Assessing the Strength Enhancement of Heterogeneous Networks of Miscible Polymer Blends
NASA Astrophysics Data System (ADS)
Giller, Carl; Roland, Mike
2013-03-01
At the typical crosslink densities of elastomers, the failure properties vary inversely with mechanical stiffness, so that compounding entails a compromise between stiffness and strength. Our approach to circumvent this conventional limitation is by forming networks of two polymers that: (i) are thermodynamically miscible, whereby the chemical composition is uniform on the segmental level; and (ii) have markedly different reactivities for network formation. The resulting elastomer consists of one highly crosslinked component and one that is lightly or uncrosslinked. This disparity in crosslinking causes their respective contributions to the network mechanical response to differ diametrically. Earlier results showed some success with this approach for thermally crosslinked blends of 1,2-polybutadiene (PVE) and polyisoprene (PI), as well as ethylene-propylene copolymer (EPM) and ethylene-propylene-diene random terpolymer (EPDM), taking advantage of their differing reactivities to sulfur. In this work we demonstrate the miscibility of polyisobutylene (PIB) with butyl rubber (BR) (a copolymer of PIB and polyisoprene) and show that networks in which only the BR is crosslinked possess greater tensile strengths than neat BR over the same range of moduli. Office of Naval Research
Roof system effects on in-situ thermal performance of HCFC polyisocyanurate insulation
DOE Office of Scientific and Technical Information (OSTI.GOV)
Christian, J.E.; Desjarlais, A.O.; Courville, G.
1992-10-01
Industry-produced, permeably-faced, experimental polyisocyanurate (PIR) laminated boardstock foamed with several different hydrochlorofluorcarbons (HCFCS) is undergoing in-situ testing at the Building Envelopes Research User Center at Oak Ridge National Laboratory (ORNL). The overall objective of this research is to determine the long term thermal performance differences between PIR foamed with CFC-11 and PIR foamed with HCFC-123, HCFC-14lb and blends of HCFCs. Boards from the same batch were installed in outdoor test facilities and instrumented in part to determine if the insulation thermal performance aging characteristics are dependent on how they are handled and installed in the field. One of the majormore » contributions of this research is the field validation of an accelerated thermal aging procedure. The laboratory measurements of the apparent thermal conductivity (k) of 10-mm-thick slices conducted over a period of less than a year are used to predict the k of 38-50-mm-thick PIR laminated board stock for 12--20 years after production. In situ thermal performance measurements of these well characterized three-year-old boards under white and under black ethylene propylene diene monomer (EPDM) membranes are compared with the accelerated aging procedure and with boards from the same batch in different roofing systems: mechanically attached EPDM, fully adhered EPDM, and built-up roof (BUR). The comparison indicates that this accelerated aging procedure should be seriously considered for providing in-service thermal performance information to building owners and roofing contractors.« less
DOE Office of Scientific and Technical Information (OSTI.GOV)
Christian, J.E.; Desjarlais, A.O.; Courville, G.
1992-01-01
Industry-produced, permeably-faced, experimental polyisocyanurate (PIR) laminated boardstock foamed with several different hydrochlorofluorcarbons (HCFCS) is undergoing in-situ testing at the Building Envelopes Research User Center at Oak Ridge National Laboratory (ORNL). The overall objective of this research is to determine the long term thermal performance differences between PIR foamed with CFC-11 and PIR foamed with HCFC-123, HCFC-14lb and blends of HCFCs. Boards from the same batch were installed in outdoor test facilities and instrumented in part to determine if the insulation thermal performance aging characteristics are dependent on how they are handled and installed in the field. One of the majormore » contributions of this research is the field validation of an accelerated thermal aging procedure. The laboratory measurements of the apparent thermal conductivity (k) of 10-mm-thick slices conducted over a period of less than a year are used to predict the k of 38-50-mm-thick PIR laminated board stock for 12--20 years after production. In situ thermal performance measurements of these well characterized three-year-old boards under white and under black ethylene propylene diene monomer (EPDM) membranes are compared with the accelerated aging procedure and with boards from the same batch in different roofing systems: mechanically attached EPDM, fully adhered EPDM, and built-up roof (BUR). The comparison indicates that this accelerated aging procedure should be seriously considered for providing in-service thermal performance information to building owners and roofing contractors.« less
Simulation and Design of Nanocomposite for Application in Ballistic Protection
2008-12-01
diene terpolymer ( EPDM ) nanocomposites with organo- montmorillonite (OMMT). It was found that the tensile modulus can be increased by 60% and...Y. D. and Li, W., 2005: Morphology and characterization of clay-reinforced EPDM nanocomposites, J. Comp. Mat., 39, 745- 754. [3] Avila, A. F
General theory of frictional heating with application to rubber friction
NASA Astrophysics Data System (ADS)
Fortunato, G.; Ciaravola, V.; Furno, A.; Lorenz, B.; Persson, B. N. J.
2015-05-01
The energy dissipation in the contact regions between solids in sliding contact can result in high local temperatures which may strongly effect friction and wear. This is the case for rubber sliding on road surfaces at speeds above 1 mm s-1. We derive equations which describe the frictional heating for solids with arbitrary thermal properties. The theory is applied to rubber friction on road surfaces and we take into account that the frictional energy is partly produced inside the rubber due to the internal friction of rubber and in a thin (nanometer) interfacial layer at the rubber-road contact region. The heat transfer between the rubber and the road surface is described by a heat transfer coefficient which depends on the sliding speed. Numerical results are presented and compared to experimental data. We find that frictional heating results in a kinetic friction force which depends on the orientation of the sliding block, thus violating one of the two basic Leonardo da Vinci ‘laws’ of friction.
General theory of frictional heating with application to rubber friction.
Fortunato, G; Ciaravola, V; Furno, A; Lorenz, B; Persson, B N J
2015-05-08
The energy dissipation in the contact regions between solids in sliding contact can result in high local temperatures which may strongly effect friction and wear. This is the case for rubber sliding on road surfaces at speeds above 1 mm s(-1). We derive equations which describe the frictional heating for solids with arbitrary thermal properties. The theory is applied to rubber friction on road surfaces and we take into account that the frictional energy is partly produced inside the rubber due to the internal friction of rubber and in a thin (nanometer) interfacial layer at the rubber-road contact region. The heat transfer between the rubber and the road surface is described by a heat transfer coefficient which depends on the sliding speed. Numerical results are presented and compared to experimental data. We find that frictional heating results in a kinetic friction force which depends on the orientation of the sliding block, thus violating one of the two basic Leonardo da Vinci 'laws' of friction.
High-temperature Y267 EPDM elastomer: field and laboratory experiences, August 1981
DOE Office of Scientific and Technical Information (OSTI.GOV)
Hirasuna, A.R.; Friese, G.J.; Stephens, C.A.
1982-03-01
Experiences which indicate the superiority of Y267 EPDM elastomer for high-temperature brines and other environments uses are summarized. Its good processing qualities, extremely good thermochemical stability, extremely good mechanical properties, its low-cost constituents, and its good performance in hydrocarbons are described in some case histories. (MCW)
Study on Thermal and Mechanical Properties of EPDM Insulation
NASA Astrophysics Data System (ADS)
Zhang, Zhong-Shui; Xu, Jin-Sheng; Chen, Xiong; Jiang, Jing
As the most common insulation material of solid rocket motors, thermal and mechanical properties of ethylene propylene diene monomer (EPDM) composite are inspected in the study. Referring to the results of thermogravimetric analysis (TGA), composition and morphology of EPDM composite in different thermal degradation degree are investigated by scanning electron microscope (SEM) to inspect the mechanism of thermal insulation. Mechanical properties of EPDM composite in the state of pyrolysis are investigated by uniaxial tensile tests. At the state of initial pyrolysis, composite belongs to the category of hyperelastic-viscoelastic material. The tendency of tensile strength increased and elongation decreased with increasing of heating temperature. Composite behaves as the linear rule at the state of late pyrolysis, which belongs to the category of bittle. The elasticity modulus of curves are almost the same while the heating temperature ranges from 200°C to 300°C, and then gradually go down. The tensile strength of pyrolytic material reach the highest at the heating temperature of 300°C, and the virgin material has the largest elongation.
Rubber friction: role of the flash temperature
NASA Astrophysics Data System (ADS)
Persson, B. N. J.
2006-08-01
When a rubber block is sliding on a hard rough substrate, the substrate asperities will exert time-dependent deformations of the rubber surface resulting in viscoelastic energy dissipation in the rubber, which gives a contribution to the sliding friction. Most surfaces of solids have roughness on many different length scales, and when calculating the friction force it is necessary to include the viscoelastic deformations on all length scales. The energy dissipation will result in local heating of the rubber. Since the viscoelastic properties of rubber-like materials are extremely strongly temperature dependent, it is necessary to include the local temperature increase in the analysis. At very low sliding velocity the temperature increase is negligible because of heat diffusion, but already for velocities of order 10-2 m s-1 the local heating may be very important. Here I study the influence of the local heating on the rubber friction, and I show that in a typical case the temperature increase results in a decrease in rubber friction with increasing sliding velocity for v>0.01 m s-1. This may result in stick-slip instabilities, and is of crucial importance in many practical applications, e.g. for tyre-road friction and in particular for ABS braking systems.
Biological coating of EPDM-membranes of fine bubble diffusers.
Wagner, M; von Hoessle, R
2004-01-01
Biological coatings on EPDM-membranes are a problem on many large wastewater treatment plants, as the oxygen supply of the micro-organisms is no longer guaranteed. Investigations prove that the pressure loss and the Shore A-hardness of the EPDM-membranes increase while on the other hand their softener content decreases accordingly. The detected coatings on the membrane surfaces and in the slits or holes of the membranes show extra-cellular organic substances (EPS), which, compared with fibrillar/filamented EPS usually found on surfaces in wastewater treatment plants, are viscous to a much greater extent. As, besides primary organic parts (carbon), the coatings on the membranes as well as in the slits or holes also consist of inorganic constituents (magnesium, silicon, and others), the authors assume that, the separating agent (and also inactive filler) talcum (magnesium silicate), used when producing the membranes, supports at least a first beginning of the coating. Superfine dust constituents and fibres, input via the compressed air, will build up inside the coating and consequently lead to a gradual clogging of the holes or slits. Besides chemical cleaning measures, the exchange of the EPDM-membranes against membranes of silicone would also be a possible measure to solve this problem. The market will decide, if, in the future, a cleaning or an exchange of the EPDM-membranes against membranes of silicone will be applied, but it has to be considered that the loss of softener is irreversible.
DOE Office of Scientific and Technical Information (OSTI.GOV)
Paroli, R.M.; Penn, J.
1994-09-01
Two ethylene-propylene-diene monomer (EPDM) roofing membranes were aged at 100 C for 7 and 28 days. The T{sub g} of these membranes was then determined by dynamic mechanical analysis (DMA), thermomechanical analysis (TMA), and differential scanning calorimetry (DSC) and the results compared. It was found that: (1) T{sub g} data can be obtained easily using the DMA and TMA techniques. The DSC method requires greater care due to the broad step change in the baseline which is associated with heavily plasticized materials. (2) The closest correspondence between techniques was for TMA and DSC (half-height). The latter, within experimental error, yieldedmore » the same glass transition temperature before and after heat-aging. (3) The peak maxima associated with tan{delta} and E{double_prime} measurements should be cited with T{sub g} values as significant differences can exist. (4) The T{sub g}(E{double_prime}) values were closer to the T{sub g}(TMA) and T{sub g}(DSC) data than were the T{sub g}(tan{delta}) values. Data obtained at 1 Hz (or possibly less) should be used when making comparisons based on various techniques. An assessment of T{sub g} values indicated that EPDM 112 roofing membrane is more stable than the EPDM 111 membrane. The T{sub g} for EPDM 112 did not change significantly with heat-aging for 28 days at 130 C.« less
Morphological studies of sulfonated polystyrene and sulfonated EPDM ionomers
DOE Office of Scientific and Technical Information (OSTI.GOV)
Jackson, D.A.
1992-12-31
Two ionomer systems have been investigated in this research. Sulfonated polystyrene (SPS) is a typical random ionomer and is a good material for studies into the nature of phase separation in ionomers. A series of narrow molecular weight distribution (MWD) zinc neutralized SPS samples of varying sulfonation levels were prepared and analyzed through small angle x-ray scattering (SAXS). Results indicated that the correlation distance varied with both molecular weight and sulfonation level. Increases in the position of the scattering maximum with sulfonation level is the result of a greater number of ionic groups. Increasing molecular weight led to the movementmore » of the scattering maximum to smaller scattering vectors, an indication of larger distances. It was also observed that ionomer peak occurred at smaller scattering vectors for the narrow MWD samples than in corresponding materials of greater dispersity. SAXS was also used to examine the morphology of zinc stearate (ZnSt) filled sulfonated EPDM (S-EPDM) ionomers and the nature of the interaction between the plasticizer and the ionomer. S-EPDM is a material that may find use as a thermoplastic elastomer, although its melt viscosity is too high to allow for convenient processing. The addition of of ZnSt as a plasticizer greatly reduces the melt viscosity of S-EPDM. ZnSt exists in this system as very small crystallites which are associated with ionic groups. As the temperature is increased, the crystallites anneal briefly into larger crystals before melting and diffusing into the S-EPDM matrix. Above the melting temperature of the ZnSt, it solvates the ionic groups of the ionomer, decreasing their self-association and the viscosity of the system. Increasing ZnSt loading is seen in the SAXS as an increase in scattering in the low angle region. However, this increase in intensity is not linear with concentration, showing that ZnSt exists in different environments at higher concentrations.« less
Rubber friction directional asymmetry
NASA Astrophysics Data System (ADS)
Tiwari, A.; Dorogin, L.; Steenwyk, B.; Warhadpande, A.; Motamedi, M.; Fortunato, G.; Ciaravola, V.; Persson, B. N. J.
2016-12-01
In rubber friction studies it is usually assumed that the friction force does not depend on the sliding direction, unless the substrate has anisotropic properties, like a steel surface grinded in one direction. Here we will present experimental results for rubber friction, where we observe a strong asymmetry between forward and backward sliding, where forward and backward refer to the run-in direction of the rubber block. The observed effect could be very important in tire applications, where directional properties of the rubber friction could be induced during braking.
Acharya, H; Bhowmick, Anil K
2007-01-01
Ethylene propylene diene terpolymer (EPDM)/MgAl layered double hydroxide (LDH) nanocomposites have been synthesized by solution intercalation using organically modified LDH (DS-LDH). The molecular level dispersion of LDH nanolayers has been verified by the disappearance of basal XRD peak of DS-LDH in the composites. The internal structures, of the nanocomposite with the dispersion nature of LDH particles in EPDM matrix have been studied by TEM and AFM. Thermogravimetric analysis (TGA) shows thermal stability of nanocomposites improved by ≈40 °C when 10% weight loss was selected as point of comparison. The degradation for pure EPDM is faster above 380 °C while in case of its nanocomposites, it is much slower.
Effect of the surface roughness on interfacial breakdown between two dielectric surfaces
DOE Office of Scientific and Technical Information (OSTI.GOV)
Fournier, D.
1996-12-31
Cable splices and accessories are the weak link in an underground power distribution system. Investigations of problems related to cable splices and accessories becomes quite intricate once the simpler causes of failures are dismissed to allow more complex phenomena to be examined. The interfacial breakdown between two internal dielectric surfaces represents one of the major causes of failure for power cable joints. In order to better understand this phenomenon, breakdown experiments were performed at interfaces found in cable splices. An experimental jig was designed to induce breakdown between dielectric surfaces longitudinally along their interface. Effects of surface roughness at EPDM/XLPEmore » and EPDM/EPDM interfaces as well as the presence of silicone grease are taken into account.« less
NASA Astrophysics Data System (ADS)
Yang, Chun; Quarles, C. A.
2007-10-01
We have used positron Doppler Broadening Spectroscopy (DBS) to investigate the uniformity of rubber-carbon black composite samples. The amount of carbon black added to a rubber sample is characterized by phr, the number of grams of carbon black per hundred grams of rubber. Typical concentrations in rubber tires are 50 phr. It has been shown that the S parameter measured by DBS depends on the phr of the sample, so the variation in carbon black concentration can be easily measured to 0.5 phr. In doing the experiments we observed a dependence of the S parameter on small variation in the counting rate or deadtime. By carefully calibrating this deadtime correction we can significantly reduce the experimental run time and thus make faster determination of the uniformity of extended samples.
1982-08-01
Sliding Rubber and the Load Dependance of Road Tyre Friction," The Physics of Tire Tractio,’. Theory, and Experiment (Hays, D. F., and Brown, A. L...Saturation of Sliding Rubber and the Load Dependance of Road Tyre Friction," The Physics of Tire Traction, Theory, and Expe-iment (Hays, D. F., and...surfaces could be identified and evaluated before accidents happen or runway surfaces could be evaluated to determine if rubber or other contaminant
Rubber friction: role of the flash temperature.
Persson, B N J
2006-08-16
When a rubber block is sliding on a hard rough substrate, the substrate asperities will exert time-dependent deformations of the rubber surface resulting in viscoelastic energy dissipation in the rubber, which gives a contribution to the sliding friction. Most surfaces of solids have roughness on many different length scales, and when calculating the friction force it is necessary to include the viscoelastic deformations on all length scales. The energy dissipation will result in local heating of the rubber. Since the viscoelastic properties of rubber-like materials are extremely strongly temperature dependent, it is necessary to include the local temperature increase in the analysis. At very low sliding velocity the temperature increase is negligible because of heat diffusion, but already for velocities of order 10(-2) m s(-1) the local heating may be very important. Here I study the influence of the local heating on the rubber friction, and I show that in a typical case the temperature increase results in a decrease in rubber friction with increasing sliding velocity for v>0.01 m s(-1). This may result in stick-slip instabilities, and is of crucial importance in many practical applications, e.g. for tyre-road friction and in particular for ABS braking systems.
EFFECTS OF GAMMA IRRADIATION ON EPDM ELASTOMERS (REVISION 1)
DOE Office of Scientific and Technical Information (OSTI.GOV)
Clark, E.
Two formulations of EPDM elastomer, one substituting a UV stabilizer for the normal antioxidant in this polymer, and the other the normal formulation, were synthesized and samples of each were exposed to gamma irradiation in initially pure deuterium gas to compare their radiation stability. Stainless steel containers having rupture disks were designed for this task. After 130 MRad dose of cobalt-60 radiation in the SRNL Gamma Irradiation Facility, a significant amount of gas was created by radiolysis; however the composition indicated by mass spectroscopy indicated an unexpected increase in the total amount deuterium in both formulations. The irradiated samples retainedmore » their ductility in a bend test. No change of sample weight, dimensions, or density was observed. No change of the glass transition temperature as measured by dynamic mechanical analysis was observed, and most of the other dynamic mechanical properties remained unchanged. There appeared to be an increase in the storage modulus of the irradiated samples containing the UV stabilizer above the glass transition, which may indicate hardening of the material by radiation damage. Revision 1 adds a comparison with results of a study of tritium exposed EPDM. The amount of gas produced by the gamma irradiation was found to be equivalent to about 280 days exposure to initially pure tritium gas at one atmosphere. The glass transition temperature of the tritium exposed EPDM rose about 10°C. over 280 days, while no glass transition temperature change was observed for gamma irradiated EPDM. This means that gamma irradiation in deuterium cannot be used as a surrogate for tritium exposure.« less
A study of amino acid modifiers in guayule natural rubber
USDA-ARS?s Scientific Manuscript database
Natural rubber from the Hevea tree is a critical agricultural material vital to United States industry, medicine, and defense, yet the country is dependent on imports to meet domestic needs. Guayule, a desert shrub indigenous to the US, is under development as an alternative source of natural rubber...
A study of protein and amino acids in guayule natural rubber
USDA-ARS?s Scientific Manuscript database
Natural rubber (NR) from Hevea brasiliensis (the Hevea rubber tree) is a critical agricultural material vital to United States industry, medicine, and defense, yet the country is dependent on NR imports to meet domestic needs. Parthenium argentatum (guayule), a woody desert shrub indigenous to the U...
DOE Office of Scientific and Technical Information (OSTI.GOV)
Shurcliff, W.A.
1979-04-01
SolaRoll is a solar collector material composed of extruded strips of black ethylene propylene diene monomer (EPDM) that is suitable for water or air type collectors. SolaRoll is provided in rolls and consists of an absorber mat with tubes and fins and a framing strip comprising all the parts of the collector frame. The rolls are bent in a counterflow pattern to cover the entire collector area and the mat is fastened with a thermosetting mastic adhesive. The heat transfer fluid is plain water as freezing does not injure the EPDM. Installation of the glazing in the framing strip ismore » described. EPDM has the disadvantage of low thermal conductivity but its use does not require antifreeze or a heat exchanger. Design options and suitable applications of SolaRoll systems are discussed.« less
NASA Astrophysics Data System (ADS)
Hafiz Mohd Hazir, Mohd; Muda, Tuan Mohamad Tuan
2016-06-01
The Malaysian rubber industry, especially in the upstream sector, is much dependent on smallholders to produce latex or cup lumps. Identification and monitoring of rubber smallholders are essential tasks when it comes to the Malaysian rubber industry's sustainability. The authorised agencies who support the rubber smallholders can do better planning, arranging, and managing. This paper introduces a method of calculating the total number of smallholders as well as identifying the location of their planted rubber area. The scope of this study only focused on land owners as rubber smallholders in the selected study area of Negeri Sembilan. The land use map provided by the Department of Agriculture Malaysia gave information on distribution of rubber area in Malaysia, while the cadastral map from the Department of Survey and Mapping Malaysia was specifically used for identifying land owners of each rubber parcel or rubber lot. Both data were analyzed and processed with ArcGIS software to extract the information, and the results were then compared to the Malaysian Rubber Board smallholders database.
NASA Astrophysics Data System (ADS)
Schaumann, Ina; Malzer, Wolfgang; Mantouvalou, Ioanna; Lühl, Lars; Kanngießer, Birgit; Dargel, Rainer; Giese, Ulrich; Vogt, Carla
2009-04-01
For the validation of the quantification of the newly-developed method of 3D Micro X-ray fluorescence spectroscopy (3D Micro-XRF) samples with a low average Z matrix and minor high Z elements are best suited. In a light matrix the interferences by matrix effects are minimized so that organic polymers are appropriate as basis for analytes which are more easily detected by X-ray fluorescence spectroscopy. Polymer layer systems were assembled from single layers of ethylene-propylene-diene rubber (EPDM) filled with changing concentrations of silica and zinc oxide as inorganic additives. Layer thicknesses were in the range of 30-150 μm. Before the analysis with 3D Micro-XRF all layers have been characterized by scanning micro-XRF with regard to filler dispersion, by infrared microscopy and light microscopy in order to determine the layer thicknesses and by ICP-OES to verify the concentration of the X-ray sensitive elements in the layers. With the results obtained for stacked polymer systems the validity of the analytical quantification model for the determination of stratified materials by 3D Micro-XRF could be demonstrated.
IUS materials outgassing condensation effects on sensitive spacecraft surfaces
NASA Technical Reports Server (NTRS)
Mullen, C. R.; Shaw, C. G.; Crutcher, E. R.
1982-01-01
Four materials used on the inertial upper state (IUS) were subjected to vacuum conditions and heated to near-operational temperatures (93 to 316 C), releasing volatile materials. A fraction of the volatile materials were collected on 25 C solar cells, optical solar reflectors (OSR's) or aluminized Mylar. The contaminated surfaces were exposed to 26 equivalent sun hours of simulated solar ultraviolet (UV) radiation. Measurements of contamination deposit mass, structure, reflectance and effects on solar cell power output were made before and after UV irradiation. Standard total mass loss - volatile condensible materials (TML - VCM) tests were also performed. A 2500 A thick contaminant layer produced by EPDM rubber motor-case insulation outgassing increased the solar absorptance of the OSR's from 0.07 to 0.14, and to 0.18 after UV exposure. An 83,000 A layer caused an increase from 0.07 to 0.21, and then the 0.46 after UV exposure. The Kevlar-epoxy motor-case material outgassing condensation raised the absorptance from 0.07 to 0.13, but UV had no effect. Outgassing from multilayer insulation and carbon-carbon nozzle materials did not affect the solar absorptance of the OSR's.
Soft, comfortable polymer dry electrodes for high quality ECG and EEG recording.
Chen, Yun-Hsuan; Op de Beeck, Maaike; Vanderheyden, Luc; Carrette, Evelien; Mihajlović, Vojkan; Vanstreels, Kris; Grundlehner, Bernard; Gadeyne, Stefanie; Boon, Paul; Van Hoof, Chris
2014-12-10
Conventional gel electrodes are widely used for biopotential measurements, despite important drawbacks such as skin irritation, long set-up time and uncomfortable removal. Recently introduced dry electrodes with rigid metal pins overcome most of these problems; however, their rigidity causes discomfort and pain. This paper presents dry electrodes offering high user comfort, since they are fabricated from EPDM rubber containing various additives for optimum conductivity, flexibility and ease of fabrication. The electrode impedance is measured on phantoms and human skin. After optimization of the polymer composition, the skin-electrode impedance is only ~10 times larger than that of gel electrodes. Therefore, these electrodes are directly capable of recording strong biopotential signals such as ECG while for low-amplitude signals such as EEG, the electrodes need to be coupled with an active circuit. EEG recordings using active polymer electrodes connected to a clinical EEG system show very promising results: alpha waves can be clearly observed when subjects close their eyes, and correlation and coherence analyses reveal high similarity between dry and gel electrode signals. Moreover, all subjects reported that our polymer electrodes did not cause discomfort. Hence, the polymer-based dry electrodes are promising alternatives to either rigid dry electrodes or conventional gel electrodes.
Melt compounding with graphene to develop functional, high-performance elastomers
NASA Astrophysics Data System (ADS)
Araby, Sherif; Zaman, Izzuddin; Meng, Qingshi; Kawashima, Nobuyuki; Michelmore, Andrew; Kuan, Hsu-Chiang; Majewski, Peter; Ma, Jun; Zhang, Liqun
2013-04-01
Rather than using graphene oxide, which is limited by a high defect concentration and cost due to oxidation and reduction, we adopted cost-effective, 3.56 nm thick graphene platelets (GnPs) of high structural integrity to melt compound with an elastomer—ethylene-propylene-diene monomer rubber (EPDM)—using an industrial facility. An elastomer is an amorphous, chemically crosslinked polymer generally having rather low modulus and fracture strength but high fracture strain in comparison with other materials; and upon removal of loading, it is able to return to its original geometry, immediately and completely. It was found that most GnPs dispersed uniformly in the elastomer matrix, although some did form clusters. A percolation threshold of electrical conductivity at 18 vol% GnPs was observed and the elastomer thermal conductivity increased by 417% at 45 vol% GnPs. The modulus and tensile strength increased by 710% and 404% at 26.7 vol% GnPs, respectively. The modulus improvement agrees well with the Guth and Halpin-Tsai models. The reinforcing effect of GnPs was compared with silicate layers and carbon nanotube. Our simple fabrication would prolong the service life of elastomeric products used in dynamic loading, thus reducing thermosetting waste in the environment.
Time-Dependent Testing Evaluation and Modeling for Rubber Stopper Seal Performance.
Zeng, Qingyu; Zhao, Xia
2018-01-01
Sufficient rubber stopper sealing performance throughout the entire sealed product life cycle is essential for maintaining container closure integrity in the parenteral packaging industry. However, prior publications have lacked systematic considerations for the time-dependent influence on sealing performance that results from the viscoelastic characteristics of the rubber stoppers. In this paper, we report results of an effort to study these effects by applying both compression stress relaxation testing and residual seal force testing for time-dependent experimental data collection. These experiments were followed by modeling fit calculations based on the Maxwell-Wiechert theory modified with the Kohlrausch-Williams-Watts stretched exponential function, resulting in a nonlinear, time-dependent sealing force model. By employing both testing evaluations and modeling calculations, an in-depth understanding of the time-dependent effects on rubber stopper sealing force was developed. Both testing and modeling data show good consistency, demonstrating that the sealing force decays exponentially over time and eventually levels off because of the viscoelastic nature of the rubber stoppers. The nonlinearity of stress relaxation derives from the viscoelastic characteristics of the rubber stoppers coupled with the large stopper compression deformation into restrained geometry conditions. The modeling fit with capability to handle actual testing data can be employed as a tool to calculate the compression stress relaxation and residual seal force throughout the entire sealed product life cycle. In addition to being time-dependent, stress relaxation is also experimentally shown to be temperature-dependent. The present work provides a new, integrated methodology framework and some fresh insights to the parenteral packaging industry for practically and proactively considering, designing, setting up, controlling, and managing stopper sealing performance throughout the entire sealed product life cycle. LAY ABSTRACT: Historical publications in the parenteral packaging industry have lacked systematic considerations for the time-dependent influence on the sealing performance that results from effects of viscoelastic characteristic of the rubber stoppers. This study applied compression stress relaxation testing and residual seal force testing for time-dependent experimental data collection. These experiments were followed by modeling fit calculations based on the Maxwell-Wiechert theory modified with the Kohlrausch-Williams-Watts stretched exponential function, resulting in a nonlinear, time-dependent sealing force model. Experimental and modeling data show good consistency, demonstrating that sealing force decays exponentially over time and eventually levels off. The nonlinearity of stress relaxation derives from the viscoelastic characteristics of the rubber stoppers coupled with the large stopper compression deformation into restrained geometry conditions. In addition to being time-dependent stress relaxation, it is also experimentally shown to be temperature-dependent. The present work provides a new, integrated methodology framework and some fresh insights to the industry for practically and proactively considering, designing, setting up, controlling, and managing of the stopper sealing performance throughout the entire sealed product life cycle. © PDA, Inc. 2018.
NASA Astrophysics Data System (ADS)
Pecault, Isabelle Tovena
2017-11-01
High-power laser facilities, such as Laser MegaJoule, are currently being operated for inertial confinement fusion experiments. Emission of volatile organic compounds (VOC) and moreover semivolatile organic compounds (SVOCs) from seals in laser environment is of tremendous importance for the optics lifetime and laser performance. That is why all the seals were screening in the same conditions: 48 h at 30°C and three successive cycle of 1.5 h at 50°C. This paper focuses on the qualification test performed on three seals: two ethylene propylene diene monomer (EPDM) and one fluoropolymer (FPM). It is shown that the molded and the extruded EPDM do not outgas the same amount neither the same molecules whereas EPDM and FPM outgas nearly the same level of phthalates.
Studies of Contaminated Runways,
1980-01-01
slide friction we refer to the friction which is produced due to the relative motion between a rubber tyre and a hard runway. tThis type of friction is... rubber planing" and a tyre exposed to such a process shows damages in form of a local sticky surface or a locally worn-off layer. The steam, which...macrostructure causes when dry together with a rubber tyre brake numbers Prom 0.7 to 1.1 depending on the rubber mixture and inflation pressure. On this type of
Galiullina, E F; Valiev, A v; Kamilov, R F; Shakirov, D F; Buliakov, P T
2013-12-01
The article presents the results of studies concerning the effect of unfavorable factors of chemical nature on fluid of oral cavity among workers of the Ufa plant of elastomer materials, articles and structures. It is established that in persons contacting with chemical pollutants of manufacture of rubber and rubber technical production the indicators of chemiluminescence of saliva fluid are significantly expressed and depend on professional standing.
Chemistry of rubber processing and disposal.
Bebb, R L
1976-01-01
The major chemical changes during the processing of rubber occur with the breakdown in mastication and during vulcanization of the molded tire. There is little chemical change during the compounding, calendering, extrusion, and molding steps. Reclaiming is the process of converting scrap rubber into an unsaturated, processible product that can be vulcanized with sulfur. Pyrolysis of scrap rubber yields a complex mixture of liquids, gas, and residue in varying ratios dependent on the nature of the scrap and the conditions of pyrolysis. PMID:799964
Experimental Polyvinyl Chloride (PVC) Roofing: Field Test Results.
1987-02-01
construction. These were the single-ply membranes of the ethylene-propylene-diene monomer ( EPDM ) and polyvinyl chloride (PVC) types, and the sprayed-in-place...polyurethane foam (PUF) with an elastomeric coating. EPDM and PUF roofs were constructed in 19802 and the PVC roofs were completed during summer 1983...faced isocyanu- rate foam board in two layers . Roofing systems were installed loose-laid and ballasted. Specific membrane materials were Plymouth
RADIOLYTIC GAS PRODUCTION RATES OF POLYMERS EXPOSED TO TRITIUM GAS
DOE Office of Scientific and Technical Information (OSTI.GOV)
Clark, E.
Data from previous reports on studies of polymers exposed to tritium gas is further analyzed to estimate rates of radiolytic gas production. Also, graphs of gas release during tritium exposure from ultrahigh molecular weight polyethylene (UHMW-PE), polytetrafluoroethylene (PTFE, a trade name is Teflon®), and Vespel® polyimide are re-plotted as moles of gas as a function of time, which is consistent with a later study of tritium effects on various formulations of the elastomer ethylene-propylene-diene monomer (EPDM). These gas production rate estimates may be useful while considering using these polymers in tritium processing systems. These rates are valid at least formore » the longest exposure times for each material, two years for UHMW-PE, PTFE, and Vespel®, and fourteen months for filled and unfilled EPDM. Note that the production “rate” for Vespel® is a quantity of H{sub 2} produced during a single exposure to tritium, independent of length of time. The larger production rate per unit mass for unfilled EPDM results from the lack of filler- the carbon black in filled EPDM does not produce H{sub 2} or HT. This is one aspect of how inert fillers reduce the effects of ionizing radiation on polymers.« less
Rubber friction: The contribution from the area of real contact.
Tiwari, A; Miyashita, N; Espallargas, N; Persson, B N J
2018-06-14
There are two contributions to the friction force when a rubber block is sliding on a hard and rough substrate surface, namely, a contribution F ad = τ f A from the area of real contact A and a viscoelastic contribution F visc from the pulsating forces exerted by the substrate asperities on the rubber block. Here we present experimental results obtained at different sliding speeds and temperatures, and we show that the temperature dependency of the shear stress τ f , for temperatures above the rubber glass transition temperature T g , is weaker than that of the bulk viscoelastic modulus. The physical origin of τ f for T > T g is discussed, and we propose that its temperature dependency is determined by the rubber molecule segment mobility at the sliding interface, which is higher than in the bulk because of increased free-volume effect due to the short-wavelength surface roughness. This is consistent with the often observed reduction in the glass transition temperature in nanometer-thick surface layers of glassy polymers. For temperatures T < T g , the shear stress τ f is nearly velocity independent and of similar magnitude as observed for glassy polymers such as PMMA or polyethylene. In this case, the rubber undergoes plastic deformations in the asperity contact regions and the contact area is determined by the rubber penetration hardness. For this case, we propose that the frictional shear stress is due to slip at the interface between the rubber and a transfer film adsorbed on the concrete surface.
Rubber friction: The contribution from the area of real contact
NASA Astrophysics Data System (ADS)
Tiwari, A.; Miyashita, N.; Espallargas, N.; Persson, B. N. J.
2018-06-01
There are two contributions to the friction force when a rubber block is sliding on a hard and rough substrate surface, namely, a contribution Fad = τf A from the area of real contact A and a viscoelastic contribution Fvisc from the pulsating forces exerted by the substrate asperities on the rubber block. Here we present experimental results obtained at different sliding speeds and temperatures, and we show that the temperature dependency of the shear stress τf, for temperatures above the rubber glass transition temperature Tg, is weaker than that of the bulk viscoelastic modulus. The physical origin of τf for T > Tg is discussed, and we propose that its temperature dependency is determined by the rubber molecule segment mobility at the sliding interface, which is higher than in the bulk because of increased free-volume effect due to the short-wavelength surface roughness. This is consistent with the often observed reduction in the glass transition temperature in nanometer-thick surface layers of glassy polymers. For temperatures T < Tg, the shear stress τf is nearly velocity independent and of similar magnitude as observed for glassy polymers such as PMMA or polyethylene. In this case, the rubber undergoes plastic deformations in the asperity contact regions and the contact area is determined by the rubber penetration hardness. For this case, we propose that the frictional shear stress is due to slip at the interface between the rubber and a transfer film adsorbed on the concrete surface.
High-temperature Y267 epdm elastomer - field and laboratory experiences, August 1981
DOE Office of Scientific and Technical Information (OSTI.GOV)
Hirasuna, A.R.; Friese, G.J.; Stephens, G.A.
1982-01-01
During the period 1976 to 1979 L'Garde, Inc. developed geothermal elastomer compounds under a U.S. Department of Energy - Division of Geothermal Energy (DOE-DGE) contract. The resulting developments yielded compounds from 4 polymer systems which successfully exceeded the contract requirements. Since completion of the compound development, significant laboratory and down-hole experience occurred, primarily on the Y267 EPDM compound. This work summarizes those experiences. 11 references.
EPDM - Silicone blends - a high performance elastomeric composition for automotive applications
DOE Office of Scientific and Technical Information (OSTI.GOV)
Mitchell, J.M.
1987-01-01
Styling and design changes have dramatically altered performance requirements for elastomers. High performance engines with electronic fuel injection have increased temperatures under the hood. Therefore, high performance elastomers are required to meet today's service conditions. New technology has been developed to compatibilize EPDM and silicone into high performance elastomeric compositions. These blends have physical, electrical and mechanical properties, for 175/sup 0/C service. Formulations are discussed for applications which require heat and weather resistance.
REVIEW OF AGING DATA ON EPDM O-RINGS IN THE H1616 SHIPPING PACKAGE
DOE Office of Scientific and Technical Information (OSTI.GOV)
Skidmore, E.
Currently, all H1616 shipping package containers undergo annual re-verification testing, including containment vessel leak testing to verify leak-tightness (<1 x 10{sup -7} ref cc/sec air) as per ANSI N14.5. The purpose of this literature review is to supplement aging studies currently being performed by SRNL on the EPDM O-rings to provide the technical basis for extending annual re-verification testing for the H1616 shipping package and to predict the life of the seals at bounding service conditions. The available data suggest that the EPDM O-rings can retain significant mechanical properties and sealing force at or below bounding service temperatures (169 Fmore » or 76 C) beyond the 1 year maintenance period. Interpretation of available data suggests that a service life of at least 2 years and potentially 4-6 years may be possible at bounding temperatures. Seal lifetimes at lower, more realistic temperatures will likely be longer. Being a hydrocarbon elastomer, EPDM O-rings may exhibit an inhibition period due to the presence of antioxidants. Once antioxidants are consumed, mechanical properties and seal performance could decline at a faster rate. Testing is being performed to validate the assumptions outlined in this report and to assess the long-term performance of O-ring seals under actual service conditions.« less
A nonaffine network model for elastomers undergoing finite deformations
NASA Astrophysics Data System (ADS)
Davidson, Jacob D.; Goulbourne, N. C.
2013-08-01
In this work, we construct a new physics-based model of rubber elasticity to capture the strain softening, strain hardening, and deformation-state dependent response of rubber materials undergoing finite deformations. This model is unique in its ability to capture large-stretch mechanical behavior with parameters that are connected to the polymer chemistry and can also be easily identified with the important characteristics of the macroscopic stress-stretch response. The microscopic picture consists of two components: a crosslinked network of Langevin chains and an entangled network with chains confined to a nonaffine tube. These represent, respectively, changes in entropy due to thermally averaged chain conformations and changes in entropy due to the magnitude of these conformational fluctuations. A simple analytical form for the strain energy density is obtained using Rubinstein and Panyukov's single-chain description of network behavior. The model only depends on three parameters that together define the initial modulus, extent of strain softening, and the onset of strain hardening. Fits to large stretch data for natural rubber, silicone rubber, VHB 4905 (polyacrylate rubber), and b186 rubber (a carbon black-filled rubber) are presented, and a comparison is made with other similar constitutive models of large-stretch rubber elasticity. We demonstrate that the proposed model provides a complete description of elastomers undergoing large deformations for different applied loading configurations. Moreover, since the strain energy is obtained using a clear set of physical assumptions, this model may be tested and used to interpret the results of computer simulation and experiments on polymers of known microscopic structure.
Degradation of different elastomeric polymers in simulated geothermal environments at 300°C
DOE Office of Scientific and Technical Information (OSTI.GOV)
Sugama, Toshifumi; Pyatina, Tatiana; Redline, Erica Marie
This study evaluates the degradation of six different elastomeric polymers used for O-rings: EPDM, FEPM, type I- and II-FKM, FFKM, and FSR, in five different simulated geothermal environments at 300 °C: 1) non-aerated steam/cooling cycles, 2) aerated steam/cooling cycles, 3) water-based drilling fluid, 4) CO 2-rich geo-brine fluid, and, 5) heat–cool water quenching cycles. The factors assessed included the extent of oxidation, changes in thermal behavior, micro-defects, permeation of ionic species from the test environments into the O-rings, silicate-related scale-deposition, and changes in the O-rings' elastic modulus. The reliability of the O-rings to maintain their integrity depended on the elastomericmore » polymer composition and the exposure environment. FSR disintegrated while EPDM was oxidized only to some degree in all the environments, FKM withstood heat-water quenching but underwent chemical degradation, FEPM survived in all the environments with the exception of heat-water quenching where it underwent severe oxidation-induced degradation, and FFKM displayed outstanding compatibility with all the tested environments. This study discusses the degradation mechanisms of the polymers under the aforementioned conditions.« less
Degradation of different elastomeric polymers in simulated geothermal environments at 300°C
Sugama, Toshifumi; Pyatina, Tatiana; Redline, Erica Marie; ...
2015-07-17
This study evaluates the degradation of six different elastomeric polymers used for O-rings: EPDM, FEPM, type I- and II-FKM, FFKM, and FSR, in five different simulated geothermal environments at 300 °C: 1) non-aerated steam/cooling cycles, 2) aerated steam/cooling cycles, 3) water-based drilling fluid, 4) CO 2-rich geo-brine fluid, and, 5) heat–cool water quenching cycles. The factors assessed included the extent of oxidation, changes in thermal behavior, micro-defects, permeation of ionic species from the test environments into the O-rings, silicate-related scale-deposition, and changes in the O-rings' elastic modulus. The reliability of the O-rings to maintain their integrity depended on the elastomericmore » polymer composition and the exposure environment. FSR disintegrated while EPDM was oxidized only to some degree in all the environments, FKM withstood heat-water quenching but underwent chemical degradation, FEPM survived in all the environments with the exception of heat-water quenching where it underwent severe oxidation-induced degradation, and FFKM displayed outstanding compatibility with all the tested environments. This study discusses the degradation mechanisms of the polymers under the aforementioned conditions.« less
2011-03-25
mixing between two streams of different temperature/density. In addition, there are also regions of high density and high pressure in the braid region...acetone seeding in this work was as follows. A small pressure vessel was filled with liquid acetone and pressurized using a nitrogen tank. An EPDM hose ...through the EPDM hose , out of the pressure vessel, and ultimately through a wall fitting. This wall fitting was connected through the wall of the
High-temperature Y267 EPDM elastomer field and laboratory experiences, September 1982
DOE Office of Scientific and Technical Information (OSTI.GOV)
Hirasuna, Alan R.; Friese, Gilbert J.; Stephens, Clifford A.
1982-10-08
High performance elastomers were developed for hostile geothermal environments which clearly advance the state-of-the-art. The Y267 EPDM compound is eminently successful and has accumulated broad laboratory and field test experience. Over 15 separate tests are reviewed with about 95% performed independently by other organizations. The tests include a broad spectrum of environments with temperatures in excess of 320 C (608 F), differential pressures up to 138 MPa (20,000 psi) and in fluids including brine, oils, isobutane, and others.
Design Criteria Upgrade for U.S. Army Type II Air Traffic Control Towers.
1985-06-01
additional layer of EPDM adhered to the roofing membrane at the perimeter should protect the roof from foot traffic. However, if heavy use or any...chance of abuse is anticipated, precast payers can be laid on an adhered EPDM pad. 49 SINGLE LAYER GYPSUM ROARD(TYP.) RIGID INSULATION(TYP.) -’ STEEL...stairwell is not air-conditioned, and its ventilation is poor. At the Fort Huachuca tower, the fan is isolated from the stairwell by the cab door, and
Shimada, Kunio
2018-06-06
In the series of studies on new types of elastic and compressible artificial skins with hybrid sensing functions, photovoltaics, and battery, we have proposed a hybrid skin (H-Skin) by utilizing an electrolytically polymerized magnetic compound fluid (MCF) made of natural rubber latex (NR-latex). By using the experimental results in the first and second reports, we have clarified the feasibility of electric charge at irradiation, and that without illumination under compression and elongation. The former was explained in a wet-type MCF rubber solar cell by developing a tunneling theory together with an equivalent electric circuit model. The latter corresponds to the battery rather than to the solar cell. As for the MCF rubber battery, depending on the selected agent type, we can make the MCF rubber have higher electricity and lighter weight. Therefore, the MCF rubber has an electric charge and storage whether at irradiation or not.
Melt compounding with graphene to develop functional, high-performance elastomers.
Araby, Sherif; Zaman, Izzuddin; Meng, Qingshi; Kawashima, Nobuyuki; Michelmore, Andrew; Kuan, Hsu-Chiang; Majewski, Peter; Ma, Jun; Zhang, Liqun
2013-04-26
Rather than using graphene oxide, which is limited by a high defect concentration and cost due to oxidation and reduction, we adopted cost-effective, 3.56 nm thick graphene platelets (GnPs) of high structural integrity to melt compound with an elastomer-ethylene-propylene-diene monomer rubber (EPDM)-using an industrial facility. An elastomer is an amorphous, chemically crosslinked polymer generally having rather low modulus and fracture strength but high fracture strain in comparison with other materials; and upon removal of loading, it is able to return to its original geometry, immediately and completely. It was found that most GnPs dispersed uniformly in the elastomer matrix, although some did form clusters. A percolation threshold of electrical conductivity at 18 vol% GnPs was observed and the elastomer thermal conductivity increased by 417% at 45 vol% GnPs. The modulus and tensile strength increased by 710% and 404% at 26.7 vol% GnPs, respectively. The modulus improvement agrees well with the Guth and Halpin-Tsai models. The reinforcing effect of GnPs was compared with silicate layers and carbon nanotube. Our simple fabrication would prolong the service life of elastomeric products used in dynamic loading, thus reducing thermosetting waste in the environment.
Non-Asbestos Insulation Testing Using a Plasma Torch
NASA Technical Reports Server (NTRS)
Morgan, R. E.; Prince, A. S.; Selvidge, S. A.; Phelps, J.; Martin, C. L.; Lawrence, T. W.
2000-01-01
Insulation obsolescence issues are a major concern for the Reusable Solid Rocket Motor (RSRM). As old sources of raw materials disappear, new sources must be found and qualified. No simple, inexpensive test presently exists for predicting the erosion performance of a candidate insulation in the full-scale motor, Large motor tests cost million of dollars and therefore can only be used on a few very select candidates. There is a need for a simple, low cost method of screening insulation performance that can simulate some of the different erosion environments found in the RSRM. This paper describes a series of erosion tests on two different non-asbestos insulation formulations, a KEVLAR(registered) fiber-filled and a carbon fiber-filled insulation containing Ethylene-Propylene-Diene Monomer (EPDM) rubber as the binder. The test instrument was a plasma torch device. The two main variables investigated were heat flux and alumina particle impingement concentration. Statistical analysis revealed that the two different formulations had very different responses to the main variable. The results of this work indicate that there may be fundamental differences in how these insulation formulations perform in the motor operating environment. The plasma torch appears to offer a low-cost means of obtaining a fundamental understanding of insulation response to critical factors in a series of statistically designed experiments.
Soft, Comfortable Polymer Dry Electrodes for High Quality ECG and EEG Recording
Chen, Yun-Hsuan; de Beeck, Maaike Op; Vanderheyden, Luc; Carrette, Evelien; Mihajlović, Vojkan; Vanstreels, Kris; Grundlehner, Bernard; Gadeyne, Stefanie; Boon, Paul; Van Hoof, Chris
2014-01-01
Conventional gel electrodes are widely used for biopotential measurements, despite important drawbacks such as skin irritation, long set-up time and uncomfortable removal. Recently introduced dry electrodes with rigid metal pins overcome most of these problems; however, their rigidity causes discomfort and pain. This paper presents dry electrodes offering high user comfort, since they are fabricated from EPDM rubber containing various additives for optimum conductivity, flexibility and ease of fabrication. The electrode impedance is measured on phantoms and human skin. After optimization of the polymer composition, the skin-electrode impedance is only ∼10 times larger than that of gel electrodes. Therefore, these electrodes are directly capable of recording strong biopotential signals such as ECG while for low-amplitude signals such as EEG, the electrodes need to be coupled with an active circuit. EEG recordings using active polymer electrodes connected to a clinical EEG system show very promising results: alpha waves can be clearly observed when subjects close their eyes, and correlation and coherence analyses reveal high similarity between dry and gel electrode signals. Moreover, all subjects reported that our polymer electrodes did not cause discomfort. Hence, the polymer-based dry electrodes are promising alternatives to either rigid dry electrodes or conventional gel electrodes. PMID:25513825
EFFECTS OF GAMMA IRRADIATION ON EPDM ELASTOMERS
DOE Office of Scientific and Technical Information (OSTI.GOV)
Clark, E.
Two formulations of EPDM elastomer, one substituting a UV stabilizer for the normal antioxidant in this polymer, and the other the normal formulation, were synthesized and samples of each were exposed to gamma irradiation in initially pure deuterium gas to compare their radiation stability. Stainless steel containers having rupture disks were designed for this task. After 130 MRad dose of cobalt-60 radiation in the SRNL Gamma Irradiation Facility, a significant amount of gas was created by radiolysis; however the composition indicated by mass spectroscopy indicated an unexpected increase in the total amount deuterium in both formulations. The irradiated samples retainedmore » their ductility in a bend test. No change of sample weight, dimensions, or density was observed. No change of the glass transition temperature as measured by dynamic mechanical analysis was observed, and most of the other dynamic mechanical properties remained unchanged. There appeared to be an increase in the storage modulus of the irradiated samples containing the UV stabilizer above the glass transition, which may indicate hardening of the material by radiation damage. Polymeric materials become damaged by exposure over time to ionizing radiation. Despite the limited lifetime, polymers have unique engineering material properties and polymers continue to be used in tritium handling systems. In tritium handling systems, polymers are employed mainly in joining applications such as valve sealing surfaces (eg. Stem tips, valve packing, and O-rings). Because of the continued need to employ polymers in tritium systems, over the past several years, programs at the Savannah River National Laboratory have been studying the effect of tritium on various polymers of interest. In these studies, samples of materials of interest to the SRS Tritium Facilities (ultra-high molecular weight polyethylene (UHMW-PE), polytetrafluoroethylene (PTFE, Teflon{reg_sign}), Vespel{reg_sign} polyimide, and the elastomer ethylene propylene diene monomer (EPDM)) have been exposed in closed containers to tritium gas initially at 1 atmosphere pressure. These studies have demonstrated the degradation of properties when exposed to tritium gas. Also, the radiolytic production of significant amounts of hydrogen has been observed for UHMW-PE and EPDM. The study documented in this report exposes two similar formulations of EPDM elastomer to gamma irradiation in a closed container backfilled with deuterium. Deuterium is chemically identical to protium and tritium, but allows the identification of protium that is radiolytically produced from the samples. The goal of this program is to compare and contrast the response of EPDM exposure to two different types of ionizing radiation in a similar chemical environment.« less
Reduced Order Models for Dynamic Behavior of Elastomer Damping Devices
NASA Astrophysics Data System (ADS)
Morin, B.; Legay, A.; Deü, J.-F.
2016-09-01
In the context of passive damping, various mechanical systems from the space industry use elastomer components (shock absorbers, silent blocks, flexible joints...). The material of these devices has frequency, temperature and amplitude dependent characteristics. The associated numerical models, using viscoelastic and hyperelastic constitutive behaviour, may become computationally too expensive during a design process. The aim of this work is to propose efficient reduced viscoelastic models of rubber devices. The first step is to choose an accurate material model that represent the viscoelasticity. The second step is to reduce the rubber device finite element model to a super-element that keeps the frequency dependence. This reduced model is first built by taking into account the fact that the device's interfaces are much more rigid than the rubber core. To make use of this difference, kinematical constraints enforce the rigid body motion of these interfaces reducing the rubber device model to twelve dofs only on the interfaces (three rotations and three translations per face). Then, the superelement is built by using a component mode synthesis method. As an application, the dynamic behavior of a structure supported by four hourglass shaped rubber devices under harmonic loads is analysed to show the efficiency of the proposed approach.
An innovative approach for rubber dam isolation of root end tip: A case report.
Mittal, Sunandan; Kumar, Tarun; Mittal, Shifali; Sharma, Jyotika
2015-01-01
The success of an apicoectomy with a retrofilling is dependent upon obtaining an acceptable apical seal. The placement of the variously approved retrograde materials requires adequate access, visibility, lighting, and a sterile dry environment. There are instances, however, in which it is difficult to use the rubber dam. One such instance is during retrograde filling. This case report highlights an innovative technique for rubber dam isolation of root end retrograde filling.
DOE Office of Scientific and Technical Information (OSTI.GOV)
Towry, Amanda; Quarles, C. A.
Previous research has demonstrated a correlation between the Doppler broadening S parameter and the intensity of the ortho-positronium lifetime component in polymers that depends on the composition of the polymer. On the other hand, rubber polymers do not show this correlation and behave more like liquids for which the S parameter is essentially independent of the ortho-positronium intensity. The bubble model has been suggested as an explanation of the lack of correlation in analogy with liquids, but the bubble model applied to rubber is controversial. There are two important differences between the rubber and the polymers samples: first, the rubbermore » samples at room temperature were all above the glass transition temperature (T{sub G}). Second, the rubber samples all contained sulfur and were vulcanized. These differences were investigated by first measuring the S parameter for six rubber samples below T{sub G} where the bubble model would not be expected to work. Second, raw rubber samples that did not contain any sulfur and were unvulcanized were studied at room temperature. The results show that the lack of correlation between the S parameter and the ortho-positronium intensity previously observed for vulcanized rubber is due to the inhibition of positronium formation by the sulfur in the vulcanized rubber samples rather than to the rubber being above T{sub G}.« less
Image Classification of Ribbed Smoked Sheet using Learning Vector Quantization
NASA Astrophysics Data System (ADS)
Rahmat, R. F.; Pulungan, A. F.; Faza, S.; Budiarto, R.
2017-01-01
Natural rubber is an important export commodity in Indonesia, which can be a major contributor to national economic development. One type of rubber used as rubber material exports is Ribbed Smoked Sheet (RSS). The quantity of RSS exports depends on the quality of RSS. RSS rubber quality has been assigned in SNI 06-001-1987 and the International Standards of Quality and Packing for Natural Rubber Grades (The Green Book). The determination of RSS quality is also known as the sorting process. In the rubber factones, the sorting process is still done manually by looking and detecting at the levels of air bubbles on the surface of the rubber sheet by naked eyes so that the result is subjective and not so good. Therefore, a method is required to classify RSS rubber automatically and precisely. We propose some image processing techniques for the pre-processing, zoning method for feature extraction and Learning Vector Quantization (LVQ) method for classifying RSS rubber into two grades, namely RSS1 and RSS3. We used 120 RSS images as training dataset and 60 RSS images as testing dataset. The result shows that our proposed method can give 89% of accuracy and the best perform epoch is in the fifteenth epoch.
Respiratory and skin effects of exposure to wood dust from the rubber tree Hevea brasiliensis.
Sripaiboonkij, P; Phanprasit, W; Jaakkola, M S
2009-07-01
Potential health effects related to wood dust from the rubber tree, which produces natural rubber latex, have not been previously investigated. The main aim of this study was to investigate the relations of rubber tree dust exposure to respiratory and skin symptoms, asthma and lung function. A cross-sectional study was conducted among 103 workers (response rate 89%) in a rubber tree furniture factory and 76 office workers (73%) in four factories in Thailand. All participants answered a questionnaire and performed spirometry. Inhalable dust levels were measured in different work areas. Factory workers showed increased risk of wheezing, nasal symptoms and asthma compared to office workers. There was a dose-dependent increase in wheeze and skin symptoms in relation to dust level. Significantly increased risks of nasal symptoms (adj OR 3.67, 95% CI 1.45 to 9.28) and asthma (8.41, 1.06 to 66.60) were detected in the low exposure category. Workers exposed to ethyl cyanoacrylate glue had significantly increased risk of cough, breathlessness and nasal symptoms. There was dose-dependent reduction in spirometric lung function with wood dust level. This study provides new evidence that workers exposed to wood dust from the rubber tree experience increased risk of nasal symptoms, wheeze, asthma and skin symptoms and have reduced spirometric lung function. Exposure to cyanoacrylate is related to significantly increased respiratory symptoms. Results suggest that the furniture industry using rubber tree wood should implement appropriate exposure control measures to reduce wood dust exposure and cyanoacrylate glue exposure to protect their employees.
NASA Astrophysics Data System (ADS)
Jia, Shaojin; Zhang, Zhicheng; Du, Zhiwen; Teng, Renrui; Wang, Zhengzhou
2003-04-01
A dynamic flammability study of flame-retardant compound consisting of HDPE, EPDM and silicon elastomer blended with additives, as wire and cable insulation was made before and after irradiation. The data of RHR, EHC, SEC and the concentration of CO and CO 2 from cone colorimeter shown in the burning process were accessed. By blending silicon elastomer, CO release rate was reduced and the thermal endurance was improved. Oxygen index, mechanical property, morphology of the char formed in dynamical flame and thermal stability were also investigated.
Mathematical Modelling of Optimization of Structures of Monolithic Coverings Based on Liquid Rubbers
NASA Astrophysics Data System (ADS)
Turgumbayeva, R. Kh; Abdikarimov, M. N.; Mussabekov, R.; Sartayev, D. T.
2018-05-01
The paper considers optimization of monolithic coatings compositions using a computer and MPE methods. The goal of the paper was to construct a mathematical model of the complete factorial experiment taking into account its plan and conditions. Several regression equations were received. Dependence between content components and parameters of rubber, as well as the quantity of a rubber crumb, was considered. An optimal composition for manufacturing the material of monolithic coatings compositions was recommended based on experimental data.
Investigations into the mechanical and physical behavior of thermoplastic elastomers
NASA Astrophysics Data System (ADS)
Wright, Kathryn Janelle
This thesis describes investigations into the physical and mechanical characteristics of two commercial thermoplastic elastomer (TPE) systems. Both systems studied exhibit elastomeric behavior similar to more traditional crosslinked elastomers; however, in these TPEs non-conventional polymer architectures and morphologies are used to produce their elastomeric behavior. The two TPEs of interest are ethylene-propylene random copolymers and dynamically vulcanized blends of ethylene-propylene-diene monomer (EPDM) and isotactic polypropylene (iPP). Very few studies have examined the mechanical behavior of these materials in terms of their composition and morphology. As such, the primary goal of this research is to both qualitatively and quantitatively understand the influence of composition and morphology on mechanical behavior. In additional very little information is available that compares their performance with that of crosslinked elastomers. As a result, the secondary goal is to qualitatively compare the mechanical responses of these TPEs with that of their more traditional counterparts. The ethylene-propylene copolymers studied have very high comonomer contents and exhibit slow crystallization kinetics. Their morphology consists of nanoscale crystallites embedded in an amorphous rubbery matrix. These crystallites act as physical crosslinks that allow for elasticity. Slow crystallization causes subsequent changes in mechanical behavior that take place over days and even weeks. Physical responses (e.g., density, crystallization kinetics, and crystal structure) of five copolymer compositions are investigated. Mechanical responses (e.g., stiffness, ductility, yielding, and reversibility) are also examined. Finally, the influence of morphology on deformation is studied using in situ analytical techniques. The EPDM/iPP blends are dynamically vulcanized which produces a complex morphology consisting of chemically crosslinked EPDM domains embedded within a semicrystalline iPP matrix. Six compositions are investigated as a function of three parameters: major volume fraction, iPP molecular weight, and EPDM cure state. The influence of these parameters on morphology and resulting mechanical behavior is examined. This work culminates in the development of a morphological model to describe the steady-state reversibility of these EPDM/iPP blends. The model is then evaluated in terms of composition and cure state.
Effect of organo-clay on the dielectric relaxation response of silicone rubber
NASA Astrophysics Data System (ADS)
Gharavi, N.; Razzaghi-Kashani, M.; Golshan-Ebrahimi, N.
2010-02-01
Dielectric elastomers are light weight, low-cost, highly deformable and fast response smart materials capable of converting electrical energy into mechanical work or vice versa. Silicone rubber is a well-known dielectric elastomer which is used as actuator, and in order to enhance the efficiency of this smart material, compounding of silicone rubber with various fillers can be carried out. The effect of organically modified montmorillonite (OMMT) nano-clay on improvement of dielectric properties, actuation stress and its relaxation response was considered in this study. OMMT was dispersed in room temperature vulcanized (RTV) silicone rubber, and a composite film was cast. Using an in-house actuation set-up, it was shown that the actuation stress for a given electric field intensity is higher for composites than that for pristine silicone rubber. Also, the time-dependent actuation response of the samples was evaluated, and it was shown that the characteristic relaxation time of the actuation stress for composites is less than for the pristine rubber as a result of OMMT addition.
Mao, Guannan; Wang, Yingying; Hammes, Frederik
2018-02-01
Polymeric materials are widely used in drinking water distribution systems. These materials could release organic carbon that supports bacterial growth. To date, the available migration assays for polymeric materials have not included the potential influence of chlorination on organic carbon migration behavior. Hence, we established a migration and growth potential protocol specifically for analysis of carbon migration from materials in contact with chlorinated drinking water. Four different materials were tested, including ethylene propylene dienemethylene (EPDM), poly-ethylene (PEX b and PEX c) and poly-butylene (PB). Chlorine consumption rates decreased gradually over time for EPDM, PEXc and PB. In contrast, no free chlorine was detected for PEXb at any time during the 7 migration cycles. Total organic carbon (TOC) and assimilable organic carbon (AOC) was evaluated in both chlorinated and non-chlorinated migrations. TOC concentrations for EPDM and PEXb in chlorinated migrations were significantly higher than non-chlorinated migrations. The AOC results showed pronounced differences among tested materials. AOC concentrations from chlorinated migration waters of EPDM and PB were higher compared to non-chlorinated migrations, whereas the opposite trend was observed for PEXb and PEXc. There was also a considerable difference between tested materials with regards to bacterial growth potential. The results revealed that the materials exposed to chlorine-influenced migration still exhibited a strong biofilm formation potential. The overall results suggested that the choice in material would make a considerable difference in chlorine consumption and carbon migration behavior in drinking water distribution systems. Copyright © 2017 Elsevier B.V. All rights reserved.
Elastomer liners for geothermal tubulars Y267 EPDM Liner Program:
DOE Office of Scientific and Technical Information (OSTI.GOV)
Hirasuna, A.R.; Davis, D.L.; Flickinger, J.E.
1987-12-01
The elastomer, Y267 EPDM, has been identified as a hydrothermally stable material which can operate at temperatures in excess of 320/sup 0/C. The goal of the Y267 Liner Program was to demonstrate the feasibility of using this material as a liner for mild steel tubulars to prevent or mitigate corrosion. If successful, the usage of EPDM lined pipe by the geothermal community may have a significant impact on operating costs and serve as a viable alternative to the use of alloyed tubulars. Tooling procedures were developed under this program to mold a 0.64 cm (0.25'') thick Y267 EPDM liner intomore » a tubular test section 61 cm (2') in length and 19.1 cm (7.5'') in diameter (ID). A successful effort was made to identify a potential coupling agent to be used to bond the elastomer to the steel tubular wall. This agent was found to withstand the processing conditions associated with curing the elastomer at 288/sup 0/C and to retain a significant level of adhesive strength following hydrothermal testing in a synthetic brine at 260/sup 0/C for a period of 166 hours. Bonding tests were conducted on specimens of mild carbon steel and several alloys including Hastelloy C-276. An objective of the program was to field test the lined section of pipe mentioned above at a geothermal facility in the Imperial Valley. Though a test was conducted, problems encountered during the lining operation precluded an encouraging outcome. The results of the field demonstration were inconclusive. 6 refs., 13 figs., 13 tabs« less
Anomalous aging of EPDM and FEPM under combined thermo-oxidative and hydrolytic conditions
DOE Office of Scientific and Technical Information (OSTI.GOV)
Redline, Erica M.; Celina, Mathias C.; Harris, Charles E.
Previous observation of EPDM and FEPM materials aged in thermo-oxidative and thermo-oxidative plus hydrolytic environments revealed an unusual trend: the degradation and disintegration of these polymers in the former case but the ability to maintain mechanical performance and shape in the latter. No abnormalities were observed in the chemical (oxidation rates, FTIR spectra, solvent uptake, gel content, and weight loss vs. temperature) or physical (modulus profile) measurements that could explain these empirically observed aging differences. A second controlled aging test was conducted to verify this trend using only EPDM. Once again it was shown that thermo-oxidative conditions appear to causemore » more degradative damage (enhanced embrittlement) than observed for the combined thermo-oxidative plus hydrolytic environments. From these data we conclude that water may favorably interfere with normal thermo-oxidative degradation processes. This interference may occur via some combination of chemical and physical property changes in the presence of steam such as: oxidation rate and O 2 permeability changes, additional sensitivity to hydrolytic damage, and/or mechanistic changes in relation to pH and hydroperoxide formation.« less
Anomalous aging of EPDM and FEPM under combined thermo-oxidative and hydrolytic conditions
Redline, Erica M.; Celina, Mathias C.; Harris, Charles E.; ...
2017-09-15
Previous observation of EPDM and FEPM materials aged in thermo-oxidative and thermo-oxidative plus hydrolytic environments revealed an unusual trend: the degradation and disintegration of these polymers in the former case but the ability to maintain mechanical performance and shape in the latter. No abnormalities were observed in the chemical (oxidation rates, FTIR spectra, solvent uptake, gel content, and weight loss vs. temperature) or physical (modulus profile) measurements that could explain these empirically observed aging differences. A second controlled aging test was conducted to verify this trend using only EPDM. Once again it was shown that thermo-oxidative conditions appear to causemore » more degradative damage (enhanced embrittlement) than observed for the combined thermo-oxidative plus hydrolytic environments. From these data we conclude that water may favorably interfere with normal thermo-oxidative degradation processes. This interference may occur via some combination of chemical and physical property changes in the presence of steam such as: oxidation rate and O 2 permeability changes, additional sensitivity to hydrolytic damage, and/or mechanistic changes in relation to pH and hydroperoxide formation.« less
DOE Office of Scientific and Technical Information (OSTI.GOV)
Clark, E; Marie Kane, M
2008-12-12
Four formulations of EPDM (ethylene-propylene diene monomer) elastomer were exposed to tritium gas initially at one atmosphere and ambient temperature for between three and four months in closed containers. Material properties that were characterized include density, volume, mass, appearance, flexibility, and dynamic mechanical properties. The glass transition temperature was determined by analysis of the dynamic mechanical property data per ASTM standards. EPDM samples released significant amounts of gas when exposed to tritium, and the glass transition temperature increased by about 3 C. during the exposure. Effects of ultraviolet and gamma irradiation on the surface electrical conductivity of two types ofmore » polyaniline films are also documented as complementary results to planned tritium exposures. Future work will determine the effects of tritium gas exposure on the electrical conductivity of polyaniline films, to demonstrate whether such films can be used as a sensor to detect tritium. Surface conductivity was significantly reduced by irradiation with both gamma rays and ultraviolet light. The results of the gamma and UV experiments will be correlated with the tritium exposure results.« less
The effect of material choice on biofilm formation in a model warm water distribution system.
Waines, Paul L; Moate, Roy; Moody, A John; Allen, Mike; Bradley, Graham
2011-11-01
Water distribution systems (WDS) are composed of a variety of materials and may harbour potential pathogens within surface-attached microbial biofilms. Biofilm formation on four plumbing materials, viz. copper, stainless steel 316 (SS316), ethylene propylene diene monomer (EPDM) and cross-linked polyethylene (PEX), was investigated using scanning electron microscope (SEM)/confocal microscopy, ATP-/culture-based analysis, and molecular analysis. Material 'inserts' were incorporated into a mains water fed, model WDS. All materials supported biofilm growth to various degrees. After 84 days, copper and SS316 showed no significant overall differences in terms of the level of biofilm formation observed, whilst PEX supported a significantly higher level of biofilm. EPDM exhibited gross contamination by a complex, multispecies biofilm, at a level significantly higher than was observed on the other materials, regardless of the analytical method used. PCR-DGGE analysis showed clear differences in the composition of the biofilm community on all materials after 84 days. The primary conclusion of this study has been to identify EPDM as a potentially unsuitable material for use as a major component in WDS.
RUBBER BEARINGS FOR DOWN-HOLE PUMPS
DOE Office of Scientific and Technical Information (OSTI.GOV)
Bob Sullivan Mammoth Pacific, L.P.
2005-09-07
Synopsis of project activity: 1998--Awarded cost share grant from DOE. 1st Qtr 1999--Developed fail safe lubricating system. 2nd Qtr 1999--Performed first large scale test with nitrile based bearings. It failed due to material swelling. Failure was blamed on improper tolerance. 3rd Qtr 1999--Material tests were performed with autoclaves and exposure tests to Casa Diablo fluids. Testing of Viton materials began. Alternate bearing designs were developed to limit risk of improper tolerances. 4th Qtr 1999--Site testing indicated a chemical attack on the bearing material caused the test failure and not improper bearing tolerance. 1st Qtr 2000--The assistance of Brookhaven National Laboratorymore » was obtained in evaluating the chemical attack. The National Laboratory also began more elaborate laboratory testing on bearing materials. 2nd Qtr 2000--Testing indicated Viton was an inappropriate material due to degradation in Casa Diablo fluid. Testing of EPDM began. 3rd Qtr 2001--EPDM bearings were installed for another large scale test. Bearings failed again due to swelling. Further testing indicated that larger then expected oil concentrations existed in lubricating water geothermal fluid causing bearing failure. 2002-2003--Searched for and tested several materials that would survive in hot salt and oil solutions. Kalrez{reg_sign}, Viton{reg_sign}ETP 500 and Viton{reg_sign}GF were identified as possible candidates. 2003-2005--Kalrez{reg_sign}has shown superior resistance to downhole conditions at Casa Diablo from among the various materials tested. Viton ETP-500 indicated a life expectancy of 13 years and because it is significantly less expensive then Kalrez{reg_sign}, it was selected as the bearing material for future testing. Unfortunately during the laboratory testing period Dupont Chemical chose to stop manufacturing this specific formulation and replaced it with Viton ETP 600S. The material is available with six different fillers; three based on zinc oxide and three based on silicon oxide. Samples of all six materials have been obtained and are being tested at the National Laboratory in Brookhaven, New York. This new material's properties as a bearing material and its ability to adhere to a bearings shell must be reviewed, but cost information deemed the material to be too expensive to be economical.« less
Temperature dependence of the dielectric properties of rubber wood
Mohammed Firoz Kabir; Wan M. Daud; Kaida B. Khalid; Haji A.A. Sidek
2001-01-01
The effect of temperature on the dielectric properties of rubber wood was investigated in three anisotropic directionsâlongitudinal, radial, and tangential, and at different measurement frequencies. Low frequency measurements were conducted with a dielectric spectrometer, and high frequencies used microwave applied with open-ended coaxial probe sensors. Dielectric...
NASA Astrophysics Data System (ADS)
Quarles, C. A.; Sheffield, Thomas; Stacy, Scott; Yang, Chun
2009-03-01
The uniformity of rubber-carbon black composite materials has been investigated with positron Doppler Broadening Spectroscopy (DBS). The number of grams of carbon black (CB) mixed into one hundred grams of rubber, phr, is used to characterize a sample. A typical concentration for rubber in tires is 50 phr. The S parameter measured by DBS has been found to depend on the phr of the sample as well as the type of rubber and carbon black. The variation in carbon black concentration within a surface area of about 5 mm diameter can be measured by moving a standard Na-22 or Ge-68 positron source over an extended sample. The precision of the concentration measurement depends on the dwell time at a point on the sample. The time required to determine uniformity over an extended sample can be reduced by running with much higher counting rate than is typical in DBS and correcting for the systematic variation of S parameter with counting rate. Variation in CB concentration with mixing time at the level of about 0.5% has been observed.
DOE Office of Scientific and Technical Information (OSTI.GOV)
Toki,S.; Minouchi, N.; Sics, I.
2008-01-01
The tensile strength of rubber depends on a combination of contributions, in particular on the finite extensibility of chain segments between network points and on strain-induced crystallization. In order to achieve high tensile strength at high strain at break, we optimized the composition and processing parameters to gain high molecular flexibility by the cure conditions, to acquire high flexibility of sulfur bridges by the accelerator, and to increase the modulus level without losing rubber molecule flexibility by carbon black. As a result, our formula performed a tensile strength of 42.5 MPa at 25 C under ISO-37, as officially measured bymore » the Society of Rubber Industry, Japan, in 2004.« less
Strategies to improve the adhesion of rubbers to adhesives by means of plasma surface modification
NASA Astrophysics Data System (ADS)
Martín-Martínez, J. M.; Romero-Sánchez, M. D.
2006-05-01
The surface modifications produced by treatment of a synthetic sulfur vulcanized styrene-butadiene rubber with oxidizing (oxygen, air, carbon dioxide) and non oxidizing (nitrogen, argon) RF low pressure plasmas, and by treatment with atmospheric plasma torch have been assessed by ATR-IR and XPS spectroscopy, SEM, and contact angle measurements. The effectiveness of the low pressure plasma treatment depended on the gas atmosphere used to generate the plasma. A lack of relationship between surface polarity and wettability, and peel strength values was obtained, likely due to the cohesive failure in the rubber obtained in the adhesive joints. In general, acceptable adhesion values of plasma treated rubber were obtained for all plasmas, except for nitrogen plasma treatment during 15 minutes due to the creation of low molecular weight moieties on the outermost rubber layer. A toluene wiping of the N{2 } plasma treated rubber surface for 15 min removed those moieties and increased adhesion was obtained. On the other hand, the treatment of the rubber with atmospheric pressure by means of a plasma torch was proposed. The wettability of the rubber was improved by decreasing the rubber-plasma torch distance and by increasing the duration because a partial removal of paraffin wax from the rubber surface was produced. The rubber surface was oxidized by the plasma torch treatment, and the longer the duration of the plasma torch treatment, the higher the degree of surface oxidation (mainly creation of C O moieties). However, although the rubber surface was effectively modified by the plasma torch treatment, the adhesion was not greatly improved, due to the migration of paraffin wax to the treated rubber-polyurethane adhesive interface once the adhesive joint was produced. On the other hand, the extended treatment with plasma torch facilitated the migration of zinc stearate to the rubber-adhesive interface, also contributing to deteriorate the adhesion in greater extent. Finally, it has been found that cleaning of SBS rubber in an ultrasonic bath prior to plasma torch treatment produced a partial removal of paraffin waxes from the surface, and thus improved adhesion was obtained.
Gartiser, Stefan; Heisterkamp, Ines; Schoknecht, Ute; Burkhardt, Michael; Ratte, Monika; Ilvonen, Outi; Brauer, Frank; Brückmann, Jan; Dabrunz, André; Egeler, Philipp; Eisl, Andrea-Maria; Feiler, Ute; Fritz, Ines; König, Sabina; Lebertz, Herbert; Pandard, Pascal; Pötschke, Gabriele; Scheerbaum, Dirk; Schreiber, Frank; Soldán, Přemysl; Weiß, Roland; Weltens, Reinhilde
2017-05-01
A European round robin test according to ISO 5725-2 was conceptually prepared, realised, and evaluated. The aim was to determine the inter-laboratory variability of the overall process for the ecotoxicological characterization of construction products in eluates and bioassays. To this end, two construction products BAM-G1 (granulate) and HSR-2 (roof sealing sheet), both made of EPDM polymers (rubber), were selected. The granular construction product was eluted in a one stage batch test, the planar product in the Dynamic Surface Leaching test (DSLT). A total of 17 laboratories from 5 countries participated in the round robin test: Germany (12), Austria (2), Belgium (1), Czech Republic (1) and France (1). A test battery of four standardised ecotoxicity tests with algae, daphnia, luminescent bacteria and zebrafish eggs was used. As toxicity measures, EC50 and LID values were calculated. All tests, except the fish egg test, were basically able to demonstrate toxic effects and the level of toxicity. The reproducibility of test results depended on the test specimens and the test organisms. Generally, the variability of the EC50 or LID values increased with the overall level of toxicity. For the very toxic BAM-G1 eluate a relative high variability of CV = 73%-110% was observed for EC50 in all biotests, while for the less toxic HSR-2 eluate the reproducibility of EC50 varied with sensitivity: it was very good (CV = 9.3%) for the daphnia test with the lowest sensitivity, followed by the algae test (CV = 36.4%). The luminescent bacteria test, being the most sensitive bioassay for HSR-2 Eluate, showed the highest variability (CV = 74.8%). When considering the complex overall process the reproducibility of bioassays with eluates from construction products was acceptable. Copyright © 2017. Published by Elsevier Ltd.
Steinhauser, Dagmar; Möwes, Markus; Klüppel, Manfred
2016-12-14
The rheo-dielectric response of carbon black filled elastomer melts is investigated by dielectric relaxation spectroscopy in the frequency range from 0.1 Hz up to 10 MHz during oszillatory shearing in a plate-plate rheometer. Various concentrations and types of carbon blacks dispersed in a non-crosslinked EPDM melt are considered. It is demonstrated that during heat treatment at low strain amplitude a pronounced flocculation of filler particles takes place leading to a successive increase of the shear modulus and conductivity. Followed up by a strain sweep, the filler network breaks up and both quantities decrease simultaneously with increasing strain amplitude. Two relaxation times, obtained from a Cole-Cole fit of the dielectric spectra, are identified, which both decrease strongly with increasing flocculation time. This behaviour is analyzed in the frame of fractal network models, describing the effect of structural disorder of the conducting carbon black network on the diffusive charge transport. Significant deviations from the predictions of percolation theory are observed, which are traced back to a superimposed cluster-cluster aggregation process (CCA). During flocculation, a universal scaling behaviour holds between the conductivity and the corresponding high frequency relaxation time, which fits all the measured data. The scaling exponent agrees fairly well with the prediction obtained from CCA. It is demonstrated that the underlying basic mechanism is a change of the correlation length of the filler network, i.e. the size of the fractal heterogeneities. This decreases during flocculation due to the formation of additional conductive paths, making the system more homogeneous. An addition less pronounced effect is found from nanoscopic gaps between adjacent filler particles, which decrease during flocculation. The same universal scaling behaviour, as obtained for flocculation, is found for temperature-dependent dielectric measurements of the cured crosslinked systems, which are heated from room temperature up to 200 °C. Thereby, the conductivity decreases significantly and the relaxation time increases, indicating that the filler network breaks up randomly due to the thermal expansion of the rubber matrix.
NASA Astrophysics Data System (ADS)
Steinhauser, Dagmar; Möwes, Markus; Klüppel, Manfred
2016-12-01
The rheo-dielectric response of carbon black filled elastomer melts is investigated by dielectric relaxation spectroscopy in the frequency range from 0.1 Hz up to 10 MHz during oszillatory shearing in a plate-plate rheometer. Various concentrations and types of carbon blacks dispersed in a non-crosslinked EPDM melt are considered. It is demonstrated that during heat treatment at low strain amplitude a pronounced flocculation of filler particles takes place leading to a successive increase of the shear modulus and conductivity. Followed up by a strain sweep, the filler network breaks up and both quantities decrease simultaneously with increasing strain amplitude. Two relaxation times, obtained from a Cole-Cole fit of the dielectric spectra, are identified, which both decrease strongly with increasing flocculation time. This behaviour is analyzed in the frame of fractal network models, describing the effect of structural disorder of the conducting carbon black network on the diffusive charge transport. Significant deviations from the predictions of percolation theory are observed, which are traced back to a superimposed cluster-cluster aggregation process (CCA). During flocculation, a universal scaling behaviour holds between the conductivity and the corresponding high frequency relaxation time, which fits all the measured data. The scaling exponent agrees fairly well with the prediction obtained from CCA. It is demonstrated that the underlying basic mechanism is a change of the correlation length of the filler network, i.e. the size of the fractal heterogeneities. This decreases during flocculation due to the formation of additional conductive paths, making the system more homogeneous. An addition less pronounced effect is found from nanoscopic gaps between adjacent filler particles, which decrease during flocculation. The same universal scaling behaviour, as obtained for flocculation, is found for temperature-dependent dielectric measurements of the cured crosslinked systems, which are heated from room temperature up to 200 °C. Thereby, the conductivity decreases significantly and the relaxation time increases, indicating that the filler network breaks up randomly due to the thermal expansion of the rubber matrix.
Lyophilization closures for protein based drugs.
DeGrazio, F; Flynn, K
1992-01-01
Rubber stopper formulations which are currently used as lyophilization stoppers vary widely in their capacities to absorb and release moisture. Release of moisture from the stopper over the shelf life of the product may result in drug degradation for extremely low cake weight products. The degree to which rubber formulations absorb water is dependent upon the components of these formulations. Independently, polymers and fillers absorb water during autoclave cycles to varying levels depending upon such factors as the solubility, structure, possibility of chemical reactions and impurity levels of these materials. Once combined into a stopper formulation, the raw materials can react to form species which further promote absorption. Data is presented comparing the absorption characteristics of low versus high absorbent rubber formulations. The release of moisture from these formulas when stoppered on vials containing dry product is also discussed.
NASA Astrophysics Data System (ADS)
Zlobina, I. V.; Bekrenev, N. V.; Muldasheva, G. K.
2017-10-01
The change in the performance characteristics of sealing and anti friction materials of pipeline armature exposed to a microwave electromagnetic field of low specific power 4-5 W/cm3 was studied. The dimensional and mass fluoroplastics and the change in the compliance of the sealing rubber were evaluated. It was established that the treatment in a microwave electromagnetic field with a frequency of 2,450 MHz with a specific power of 4-5 W/cm3 for 4 minutes ensures a reduction in the size and mass wear upon contact. Besides, the compliance of the rubber increases by 20-64 %, depending on the degree of deformation of the counter-body — by 55 and 25 %. After microwave treatment in a similar mode, the malleability of the rubber increases by 20-64 %, depending on the degree of deformation.
Jonsson, Ulf; Lindahl, Olof; Andersson, Britt
2014-12-01
To gain an understanding of the high-frequency elastic properties of silicone rubber, a finite element model of a cylindrical piezoelectric element, in contact with a silicone rubber disk, was constructed. The frequency-dependent elastic modulus of the silicone rubber was modeled by a fourparameter fractional derivative viscoelastic model in the 100 to 250 kHz frequency range. The calculations were carried out in the range of the first radial resonance frequency of the sensor. At the resonance, the hyperelastic effect of the silicone rubber was modeled by a hyperelastic compensating function. The calculated response was matched to the measured response by using the transitional peaks in the impedance spectrum that originates from the switching of standing Lamb wave modes in the silicone rubber. To validate the results, the impedance responses of three 5-mm-thick silicone rubber disks, with different radial lengths, were measured. The calculated and measured transitional frequencies have been compared in detail. The comparison showed very good agreement, with average relative differences of 0.7%, 0.6%, and 0.7% for the silicone rubber samples with radial lengths of 38.0, 21.4, and 11.0 mm, respectively. The average complex elastic moduli of the samples were (0.97 + 0.009i) GPa at 100 kHz and (0.97 + 0.005i) GPa at 250 kHz.
Temperature dependence of the elastocaloric effect in natural rubber
NASA Astrophysics Data System (ADS)
Xie, Zhongjian; Sebald, Gael; Guyomar, Daniel
2017-07-01
The temperature dependence of the elastocaloric (eC) effect in natural rubber (NR) has been studied. This material exhibits a large eC effect over a broad temperature range from 0 °C to 49 °C. The maximum adiabatic temperature change (ΔT) occurred at 10 °C and the behavior could be predicted by the temperature dependence of the strain-induced crystallization (SIC) and the temperature-induced crystallization (TIC). The eC performance of NR was then compared with that of shape memory alloys (SMAs). This study contributes to the SIC research of NR and also broadens the application of elastomers.
Viscoelastic Properties of Rubber Composites Reinforced by Wheat Gluten and Wheat Starch Co-filler
USDA-ARS?s Scientific Manuscript database
Due to different abilities of wheat gluten (WG) and wheat starch (WS) to increase the modulus of rubber composites, the composite properties can be adjusted by varying the ratio of WG to WS as a co-filler. This study shows that the co-filler composites became more temperature dependent as the WG co...
Viscoelastic Properties of Rubber Composites Reinforced by Wheat Gluten and Starch Co-filler
USDA-ARS?s Scientific Manuscript database
Due to different abilities of wheat gluten (WG) and wheat starch (WS) to increase the modulus of rubber composites, the composite properties can be adjusted by varying the ratio of WG to WS as a co-filler. This study shows that the co-filler composites became more temperature dependent as the WG co...
Vilmin, Franck; Dussap, Claude; Coste, Nathalie
2006-06-01
In the tire industry, synthetic styrene-butadiene rubber (SBR), butadiene rubber (BR), and isoprene rubber (IR) elastomers are essential for conferring to the product its properties of grip and rolling resistance. Their physical properties depend on their chemical composition, i. e., their microstructure and styrene content, which must be accurately controlled. This paper describes a fast, robust, and highly reproducible near-infrared analytical method for the quantitative determination of the microstructure and styrene content. The quantitative models are calculated with the help of pure spectral profiles estimated from a partial least squares (PLS) regression, using (13)C nuclear magnetic resonance (NMR) as the reference method. This versatile approach allows the models to be applied over a large range of compositions, from a single BR to an SBR-IR blend. The resulting quantitative predictions are independent of the sample path length. As a consequence, the sample preparation is solvent free and simplified with a very fast (five minutes) hot filming step of a bulk polymer piece. No precise thickness control is required. Thus, the operator effect becomes negligible and the method is easily transferable. The root mean square error of prediction, depending on the rubber composition, is between 0.7% and 1.3%. The reproducibility standard error is less than 0.2% in every case.
DOE Office of Scientific and Technical Information (OSTI.GOV)
Gillen, K.T.; Wise, J.; Celina, M.
1997-09-01
Because of the need to significantly extend the lifetimes of weapons, and because of potential implications of environmental O-ring failure on degradation of critical internal weapon components, the authors have been working on improved methods of predicting and verifying O-ring lifetimes. In this report, they highlight the successful testing of a new predictive method for deriving more confident lifetime extrapolations. This method involves ultrasensitive oxygen consumption measurements. The material studied is an EPDM formulation use for the environmental O-ring the W88. Conventional oven aging (155 C to 111 C) was done on compression molded sheet material; periodically, samples were removedmore » from the ovens and subjected to various measurements, including ultimate tensile elongation, density and modulus profiles. Compression stress relaxation (CSR) measurements were made at 125 C and 111 C on disc shaped samples (12.7 mm diameter by 6 mm thick) using a Shawbury Wallace Compression Stress Relaxometer MK 2. Oxygen consumption measurements were made versus time, at temperatures ranging from 160 C to 52 C, using chromatographic quantification of the change in oxygen content caused by reaction with the EPDM material in sealed containers.« less
Ultrasonic Method for Measuring Internal Temperature Profile in Heated Materials
NASA Astrophysics Data System (ADS)
Ihara, I.; Takahashi, M.
2008-02-01
A new ultrasonic method for internal temperature measurement is presented. The principle of the method is based on temperature dependence of the velocity of the ultrasonic wave propagating through the material. An inverse analysis to determine the temperature profile in a heated material is developed and an experiment is carried out to verify the validity of the developed method. A single side of a silicone rubber plate of 30 mm thickness is heated and ultrasonic pulse-echo measurements are then performed during heating. A change in transit time of ultrasonic wave in the heated rubber plate is monitored and used to determine the transient variation in internal temperature distribution of the rubber. The internal temperature distribution determined ultrasonically agrees well with both obtained using commercial thermocouples installed in the rubber and estimated theoretically.
The role of oxide structure on copper wire to the rubber adhesion
NASA Astrophysics Data System (ADS)
Su, Yea-Yang; Shemenski, Robert M.
2000-07-01
Most metals have an oxide layer on the surface. However, the structure of the oxide varies with the matrix composition, and depends upon the environmental conditions. A bronze coating, nominal composition of 98.5% Cu and balance of Sn, is applied to steel wire for reinforcing pneumatic tire beads and to provide adhesion to rubber. This work studied the influence of copper oxides on the bronze coating on adhesion during vulcanization. To emphasize the oxide structures, electrolytic tough pitch (ETP) copper wire was used instead of the traditional bronze-coated tire bead wire. Experimental results confirmed the hypothesis that cuprous oxide (Cu 2O) could significantly improve bonding between copper wire and rubber, and demonstrated that the interaction between rubber and oxide layer on wire is an electrochemical reaction.
Identification of an exposure risk to heavy metals from pharmaceutical-grade rubber stoppers.
Li, Xianghui; Qian, Pingping
2017-07-01
Exposure to low concentrations of heavy metals and metalloids represents a well-documented risk to animal and human health. However, current standards (European Pharmacopeia [EP], United States Pharmacopoeia [USP], International Organization for Standardization [ISO], YBB concerned with rubber closures) only require testing for Zn in pharmaceutical-grade rubber stoppers and then using only pure water as a solvent. We extracted and quantified heavy metals and trace elements from pharmaceutical-grade rubber stoppers under conditions that might occur during the preparation of drugs. Pure water, saline, 10% glucose, 3% acetic acid (w/v), 0.1 mol/L hydrochloric acid, and diethylenetriaminepentaacetic acid (4 mg/mL, 0.4 mg/mL, and 0.04 mg/mL) were used as extraction agents. We quantified the extracted arsenic, lead, antimony, iron, magnesium, aluminum, and zinc using inductively coupled plasma mass spectrometry. The concentration of extracted metals varied depending on the different extraction solutions used and between the different rubber stopper manufacturers. Rubber stoppers are ubiquitously used in the pharmaceutical industry for the storage and preparation of drugs. Extraction of heavy metals during the manufacturing and preparation of drugs represents a significant risk, suggesting a need for industry standards to focus on heavy metal migration from rubber stoppers. Copyright © 2016. Published by Elsevier B.V.
The water-food nexus of natural rubber production
NASA Astrophysics Data System (ADS)
Chiarelli, D. D.; Rosa, L.; Rulli, M. C.; D'Odorico, P.
2017-12-01
The increasing global demand for natural rubber (100% increase in the last 15 years) is for most part met by Malaysia and Indonesia, and - to a lesser extent - other countries in south-east Asia and Africa. The consequent expansion of rubber plantation has often occurred at the expenses of agricultural land for staple food, particularly in southeast Asia, where most of the land suitable for agriculture is already harvested for food crops or other uses. Here we investigate the extent to which the ongoing increase in rubber production is competing with the food system and affecting the livelihoods of rural communities in the areas of production and their appropriation of natural resources, such as water. We also investigate to what extent the expansion of rubber plantations is taking place through large scale land acquisitions (LSLAs) and evaluate the impacts on rural communities. Our results show how rubber production has strong environmental, social and economic impacts. Despite their ability to bring employment and increase the average income of economically disadvantaged areas, rubber plantations may threaten the local water and food security and induce a loss of rural livelihoods, particularly when the new plantations result from LSLAs that displace semi-subsistence forms of production thereby forcing the local populations to depend on global markets.
Occupational nitrosamine exposure. 1. Rubber and tyre industry.
Spiegelhalder, B; Preussmann, R
1983-09-01
To determine the role of N-nitrosamines in the known increased cancer risk of rubber workers, air concentrations of such carcinogens were measured by area sampling or personal monitoring in 19 factories. N-Nitrosodimethylamine (NDMA) and N-nitrosomorpholine (NMOR) were found regularly, the air concentrations varying between 0.1 and 380 micrograms/m3 personal monitoring. The mean concentration was usually in the range of 1-10 micrograms/m3. Several other nitrosamines could be detected in certain production branches. In retail shops and storage rooms of tyres NDMA and NMOR were found. Most rubber chemicals based on amines are contaminated with N-nitrosamines, but this contamination cannot explain the air concentrations of nitrosamines found. The occurrence of nitrosamines mainly depends upon their formation during production of rubber and rubber products from used vulcanisation accelerators based on amines and the presence of nitrosating agents, such as diphenylnitrosamine (retarder A) and of nitrous gases, in products or production areas. Elimination of one or both precursors for nitrosamine formation resulted in significant reduction of airial contamination of nitrosamines. The results are discussed in regard to the mechanisms of nitrosamine formation during rubber production, as basis for future epidemiological studies and their potential for exposure prevention.
Faivre, Nathan; Dönz, Jonathan; Scandola, Michele; Dhanis, Herberto; Bello Ruiz, Javier; Bernasconi, Fosco; Salomon, Roy; Blanke, Olaf
2017-01-04
Vision is known to be shaped by context, defined by environmental and bodily signals. In the Taylor illusion, the size of an afterimage projected on one's hand changes according to proprioceptive signals conveying hand position. Here, we assessed whether the Taylor illusion does not just depend on the physical hand position, but also on bodily self-consciousness as quantified through illusory hand ownership. Relying on the somatic rubber hand illusion, we manipulated hand ownership, such that participants embodied a rubber hand placed next to their own hand. We found that an afterimage projected on the participant's hand drifted depending on illusory ownership between the participants' two hands, showing an implication of self-representation during the Taylor illusion. Oscillatory power analysis of electroencephalographic signals showed that illusory hand ownership was stronger in participants with stronger α suppression over left sensorimotor cortex, whereas the Taylor illusion correlated with higher β/γ power over frontotemporal regions. Higher γ connectivity between left sensorimotor and inferior parietal cortex was also found during illusory hand ownership. These data show that afterimage drifts in the Taylor illusion do not only depend on the physical hand position but also on subjective ownership, which itself is based on the synchrony of somatosensory signals from the two hands. The effect of ownership on afterimage drifts is associated with β/γ power and γ connectivity between frontoparietal regions and the visual cortex. Together, our results suggest that visual percepts are not only influenced by bodily context but are self-grounded, mapped on a self-referential frame. Vision is influenced by the body: in the Taylor illusion, the size of an afterimage projected on one's hand changes according to tactile and proprioceptive signals conveying hand position. Here, we report a new phenomenon revealing that the perception of afterimages depends not only on bodily signals, but also on the sense of self. Relying on the rubber hand illusion, we manipulated hand ownership, so that participants embodied a rubber hand placed next to their own hand. We found that visual afterimages projected on the participant's hand drifted laterally, only when the rubber hand was embodied. Electroencephalography revealed spectral dissociations between somatic and visual effects, and higher γ connectivity along the dorsal visual pathways when the rubber hand was embodied. Copyright © 2017 the authors 0270-6474/17/370011-12$15.00/0.
Effect of Ambient Temperature on Hydrophobic Recovery Behavior of Silicone Rubber Composites
NASA Astrophysics Data System (ADS)
Peng, Xiangyang; Li, Zijian; Zheng, Feng; Zhang, Ni; Huang, Zhen; Fang, Pengfei
A series of silicone rubber samples with different cyclosiloxanes contents have been successfully prepared, and their hydrophobic recovery behaviors and mechanism were investigated in detail. The gas chromatography-mass spectroscopy technique after Soxhlet extraction was utilized to examine the low molecular weight siloxanes in the sample, SEM was used to observe the surface morphology of the silicone rubber influenced by plasma treatment, and contact angle measurement was applied to probe the hydrophobic recovery of the sample surface after plasma treatment at different storage temperatures. The storage time-dependent contact angle of water can be well fitted by the diffusion model calculated from Fick’s second law. The results imply that the hydrophobic recovery of silicone rubber is related to the diffusion of low molecular weight siloxanes, while larger content or higher temperature can induce faster hydrophobic recovery.
DOE Office of Scientific and Technical Information (OSTI.GOV)
Teixeira, M.D.R. Jr.
This paper describes the development of new wet design MV power cables, up to 35 kV, using EPDM compound as insulation and longitudinal water tightness. The combination of the cable design and the type of insulation compound allow for reduction of the insulation thickness in such a way, as to have an electrical stress at the conductor of 4 kV/mm which is significantly greater than used in MV distribution cables. Following a methodology established, at the author's company, the reliability of this design, cable and EPDM's formulation, in wet location, without metallic water barriers, was well demonstrated. Mini-installation of modelmore » cables in service-like conditions, to estimate the ageing rate, are presented and discussed.« less
RHETT2/EPDM Hall Thruster Propulsion System Electromagnetic Compatibility Evaluation
NASA Technical Reports Server (NTRS)
Sarmiento, Charles J.; Sankovic, John M.; Freitas, Joseph; Lynn, Peter R.
1997-01-01
Electromagnetic compatibility measurements were obtained as part of the Electric Propulsion Demonstration Module (EPDM) flight qualification program. Tests were conducted on a Hall thruster system operating at a nominal 66O W discharge power. Measurements of conducted and radiated susceptibility and emissions were obtained and referenced to MEL-STD-461 C. The power processor showed some conducted susceptibility below 4 kHz for the magnet current and discharge voltage. Radiated susceptibility testing yielded a null result. Conducted emissions showed slight violations of the specified limit for MIL-461C CE03. Radiated emissions exceeded the RE02 standard at low frequencies, below 300 MHz, by up to 40 dB RV/m/MHz.
Stability of an arch type shock absorber made of a rubber-like material
NASA Astrophysics Data System (ADS)
Kabrits, Sergey A.; Kolpak, Eugeny P.
2018-05-01
The paper considers the stability problem of an arch shock absorber made of a rubber-like material. As a model, the nonlinear theory of thin shells from elastomers K.F. Chernykh is used. The case of symmetrical and asymmetrical deformation of an arch shock absorber under symmetrical compression is investigated. The possibility of asymmetric bifurcation is evaluated depending on the boundary conditions.
Study on mechanical and ablative properties of EPDM/OMMT thermal insulating nanocomposites.
Gao, Guoxin; Zhang, Zhicheng; Li, Xuefei; Meng, Qingjie; Zheng, Yuansuo; Jin, Zhihao
2010-11-01
In order to enhance the elongation at break, the ablation resistant properties as well as the tensile strength of the thermal insulating materials, organo-montmorillonite (OMMT) was introduced into the short aramid fibers reinforced Ethylene-Propylene-Diene Monomer (EPDM) based nanocomposites. The effects of OMMT content on the mechanical and ablative properties of the nanocomposites were investigated systematically. X-ray diffraction (XRD) and transmission electron microscopy (TEM) confirm that EPDM-matrix has been intercalated into OMMT interlayers after a mixing process on a two-roll mill. The brittle fracture of nanocomposites also indicates that OMMT can lubricate aramid fiber to weaken the interfacial adhesive strength between the fibers and the matrix. As a result, the tensile strength and elongation at break are both improved sharply with OMMT content increasing from 1 phr to 7 phr. However, thanks to the inevitable agglomeration of OMMT with high loading inside the nanocomposites, the tensile strength and elongation at break reduce gently once OMMT is over 7 phr. Furthermore, the ablation resistant properties are improved greatly by increasing OMMT from 1 phr to 11 phr. Therefore, the optimal content of OMMT is 7-11 phr for the thermal insulating nanocomposites with big elongation and excellent ablation resistant properties.
Argon gas analysis to predict water leakage into the W88
DOE Office of Scientific and Technical Information (OSTI.GOV)
Gillen, K.T.
1990-08-01
Analyses of the internal argon gas concentrations monitored on surveillance units of the W84 indicates that field aging of this weapon for times up to {approximately}4 years does not lead to important increases in the rate at which water leaks into the interior of the weapon. This implies that the EPDM environmental seals used on the W84 do not age significantly over this time period. By comparing the percentages of oxygen and argon in the internal atmosphere, an estimate of the oxygen consumption rate is made for a typical W84 unit. The argon gas analysis approach is then applied tomore » the W88, which is sealed with a new EPDM material. Predictive expressions are derived which relate the anticipated argon gas concentrations of future, field-returned units to their water leakage rates. The predictions are summarized in convenient plots, which can be immediately and easily applied to surveillance data as reported. Since the argon approach is sensitive enough to be useful over the entire lifetime of the W88, it can be used to point out leaking units and to determine whether long-term aging has any significant effect on the new EPDM material. 11 refs., 10 figs., 3 tabs.« less
DOE Office of Scientific and Technical Information (OSTI.GOV)
Morita, Y.; Hagiwara, M.
1982-09-01
Bromoacenaphthylenes and their condensates as flame-retardant reagents were synthesized by bromination of acenaphthylene using ZnCl/sub 2/ - CF/sub 3/COOH or FeCl/sub 3/ as catalysts and subsequent dehydrobromination. The chief components were identified as bromoacenaphthylene monomers when ZnCl/sub 2/ - CF/sub 3/COOH were used, and as their condensates (mostly trimers) in the case of FeCl/sub 3/. Their performance as flame-retardant reagents for ethylene-propylene-diene terpolymer (EPDM) was evaluated by measuring the oxygen index of finished compounds, and flammability by a vertical flammability test based on UL-94-VO. Both the monomers and the condensates demonstrated high flame-retardant effectiveness. The high efficiency was attributed tomore » their excellent dispersity in the base polymer and their characteristic thermal decomposition behavior. In thermal gravimetric analysis (TGA), they decomposed in a very wide range of temperature (ca.200-560/sup 0/C), which covers the decomposition range of EPDM. This was attributed to the existence of bromines of different thermal stabilities in one molecule. This paper is a part of a series of studies to develop new flame retardants which can give high flame retardancy as well as stabilty against ionizing radiation to EPDM.« less
Waste handling: A study of tributyl phosphate compatibility with nonmetallic materials
DOE Office of Scientific and Technical Information (OSTI.GOV)
Jenkins, C.F.; Briedenbach, P.J.
1989-01-01
The need for numerous seals, plastic tubing, instrument components, and miles of plastic pipe for transferring process waste streams containing tributyl phosphate (TBP) and petroleum solvents led to an investigation of compatibility. TBP is a solvent for many plastics and elastomers and causes softening, crazing, or cracking of most nonmetallics tested. In this regard it may be considered an external plasticizer for some polymers. TBP also is a surfactant in aqueous solution. Dimension changes and property changes associated with softening will preclude the use of some materials as gaskets. Teflon/trademark/ and Kalrez/trademark/ gaskets appear to be compatible with TBP. Mixedmore » results were obtained with EPDM elastomers, but EPDM O-rings are less costly than Kalrez/trademark/ and are being applied in some areas. Exposure of CPVC rigid piping led to crazing and, ultimately, catastrophic stress cracking, thus precluding its use in the waste services described. High-density polyethylene and PVDF plastic piping were unaffected by the test exposures and are useable for process and process waste service. Applications include 25-30 miles of polyethylene pipe and a large number of EPDM gaskets in the filter assembly of an effluent treatment system at the Savannah River Plant. 3 refs., 7 figs., 3 tabs.« less
Stelescu, Maria-Daniela; Craciun, Gabriela; Dumitrascu, Maria
2014-01-01
A new polymeric composite based on natural rubber reinforced with hemp has been processed by electron beam irradiation and characterized by several methods. The mechanical characteristics: gel fraction, crosslink density, water uptake, swelling parameters, and FTIR of natural rubber/hemp fiber composites have been investigated as a function of the hemp content and absorbed dose. Physical and mechanical properties present a significant improvement as a result of adding hemp fibres in blends. Our experiments showed that the hemp fibers have a reinforcing effect on natural rubber similar to mineral fillers (chalk, carbon black, silica). The crosslinking rates of samples, measured using the Flory-Rehner equation, increase as a result of the amount of hemp in blends and the electron beam irradiation dose increasing. The swelling parameters of samples significantly depend on the amount of hemp in blends, because the latter have hydrophilic characteristics. PMID:24688419
Stelescu, Maria-Daniela; Manaila, Elena; Craciun, Gabriela; Dumitrascu, Maria
2014-01-01
A new polymeric composite based on natural rubber reinforced with hemp has been processed by electron beam irradiation and characterized by several methods. The mechanical characteristics: gel fraction, crosslink density, water uptake, swelling parameters, and FTIR of natural rubber/hemp fiber composites have been investigated as a function of the hemp content and absorbed dose. Physical and mechanical properties present a significant improvement as a result of adding hemp fibres in blends. Our experiments showed that the hemp fibers have a reinforcing effect on natural rubber similar to mineral fillers (chalk, carbon black, silica). The crosslinking rates of samples, measured using the Flory-Rehner equation, increase as a result of the amount of hemp in blends and the electron beam irradiation dose increasing. The swelling parameters of samples significantly depend on the amount of hemp in blends, because the latter have hydrophilic characteristics.
Detection of internal cracks in rubber composite structures using an impact acoustic modality
NASA Astrophysics Data System (ADS)
Shen, Q.; Kurfess, T. R.; Omar, M.; Gramling, F.
2014-01-01
The objective of this study is to investigate the use of impact acoustic signals to non-intrusively inspect rubber composite structures for the presence of internal cracks, such as those found in an automobile tyre. Theoretical contact dynamic models for both integral and defective rubber structures are developed based on Hertz's impact model, further modified for rubber composite materials. The model generates the prediction of major impact dynamic quantities, namely the maximum impact force, impact duration and contact deformation; such parameters are also theoretically proven to be correlated with the presence of internal cracks. The tyre structures are simplified into cubic rubber blocks, to mitigate complexity for analytical modelling. Both impact force and impact sound signals are measured experimentally, and extraction of useful features from both signals for defect identification is achieved. The impact force produces two direct measurements of theoretical impact dynamic quantities. A good correlation between these experimental discriminators and the theoretical dynamic quantities provide validation for the contact dynamics models. Defect discriminators extracted from the impact sound are dependent on both time- and frequency-domain analyses. All the discriminators are closely connected with the theoretical dynamic quantities and experimentally verified as good indicators of internal cracks in rubber composite structures.
Chevron cutting: Experiment with new runway mixtures
NASA Technical Reports Server (NTRS)
Tyran, K. (Compiler)
1978-01-01
Chevron cutting is shown to occur in different forms depending on the type of tire and the rubber on the running surface. Hardest wear is shown by the main tires of the B-747. Four defects occurred, in the form of two rip separation and two breakouts of the running surface. Tires capped by Thompson are more affected than any of the other rubber-capping fabrics. For Thompson tires, Chevron Cutting is greatly reduced with a fiberglass-rubber mixture. For Goodyear tires, it is eliminated with spiral wrap rubbercapping; resistance to damages through cuts seems to be more positive for Goodyear tires. For Mader tires, the extent of Chevron Cutting is generally smaller than for Thompson cappings.
Effects of tritium gas exposure on the dynamic mechanical properties of EPDM elastomer
DOE Office of Scientific and Technical Information (OSTI.GOV)
Clark, E. A.; Staack, G. C.
2008-07-15
Samples of ethylene propylene diene monomer (EPDM) elastomer were exposed to tritium gas in closed containers at 101 kPa (1 atmosphere) pressure and ambient temperature for about one week. Tritium exposure effects on the samples were characterized by dynamic mechanical analysis (DMA) and radiolysis products were characterized by measuring the total final pressure and composition in the exposure containers at the end of exposure period. There was no effect of one week tritium exposure on the glass transition temperature, Tg, of the samples tested. Impurity gases produced in the closed containers included HT and lesser amounts of H{sub 2}, DTO,more » and CT{sub 4}. The total pressure remained the same during exposure. (authors)« less
EFFECTS OF TRITIUM GAS EXPOSURE ON THE DYNAMIC MECHANICAL PROPERTIES OF EPDM ELASTOMER
DOE Office of Scientific and Technical Information (OSTI.GOV)
Clark, E; Gregory Staack, G
2007-08-13
Samples of ethylene propylene diene monomer (EPDM) elastomer were exposed to tritium gas in closed containers initially at 101 kPa (1 atmosphere) pressure and ambient temperature for about one week. Tritium exposure effects on the samples were characterized by dynamic mechanical analysis (DMA) and radiolysis products were characterized by measuring the total final pressure and composition in the exposure containers at the end of exposure period. There was no effect of one week tritium exposure on the glass transition temperature, Tg, of the samples tested. Impurity gases produced in the closed containers included HT and lesser amounts of H{sub 2},more » DTO, and CT{sub 4}. The total pressure remained the same during exposure.« less
NASA Astrophysics Data System (ADS)
Alzamil, M. A.; Alfaramawi, K.; Abboudy, S.; Abulnasr, L.
2018-02-01
Electrical properties of butyl rubber filled with General Purpose Furnace (GPF) carbon black were studied. The carbon black concentration ( X) in the compound was X = 40, 60, 70, 80, and 100 parts by weight per hundred parts by weight of rubber (phr). The corresponding volume fractions of GPF carbon black were 0.447 ± 0.022, 0.548 ± 0.027, 0.586 ± 0.029, 0.618 ± 0.031 and 0.669 ± 0.034, respectively. The concentration dependence of conductivity ( σ ) at constant temperature showed that σ follows a percolation theory; σ ∝ ( {X - Xo } )^{γ } , where X o is the concentration at percolation threshold. The exponent γ was found as 6.6 (at room temperature 30°C). This value agrees with other experimental values obtained by many authors for different rubber-carbon black systems. Electron tunneling between the aggregates, which are dispersed in the insulator rubber, was mainly the conduction process proposed at constant temperature in the butyl-GPF carbon black composites. Temperature dependence of conductivity was investigated in the temperature range from 30°C up to 120°C. All samples exhibit negative temperature coefficients of conductivity (NTCC). The values obtained are - 0.130°C-1, - 0.019°C-1, - 0.0082°C-1, - 0.0094°C-1, and - 0.072°C-1 for carbon black concentrations of 40 phr, 60 phr, 70 phr, 80 phr, and 100 phr, respectively. The samples of concentrations 40 phr and 60 phr have also positive temperature coefficients of conductivity (PTCC) of values + 0.031 and + 0.013, respectively. Electrical conduction at different temperatures showed various mechanisms depending on the carbon black concentration and/or the interval of temperature. The hopping conduction mechanism was noticed at the lower temperature region while carrier thermal activation mechanisms were recorded at the higher temperature range.
Thakkar, Katharine N; Nichols, Heathman S; McIntosh, Lindsey G; Park, Sohee
2011-01-01
A weakened sense of self may contribute to psychotic experiences. Body ownership, one component of self-awareness, can be studied with the rubber hand illusion (RHI). Watching a rubber hand being stroked while one's unseen hand is stroked synchronously can lead to a sense of ownership over the rubber hand, a shift in perceived position of the real hand, and a limb-specific drop in stimulated hand temperature. We aimed to assess the RHI in schizophrenia using quantifiable measures: proprioceptive drift and stimulation-dependent changes in hand temperature. The RHI was elicited in 24 schizophrenia patients and 21 matched controls by placing their unseen hand adjacent to a visible rubber hand and brushing real and rubber hands synchronously or asynchronously. Perceived finger location was measured before and after stimulation. Hand temperature was taken before and during stimulation. Subjective strength of the illusion was assessed by a questionnaire. Across groups, the RHI was stronger during synchronous stimulation, indicated by self-report and proprioceptive drift. Patients reported a stronger RHI than controls. Self-reported strength of RHI was associated with schizotypy in controls Proprioceptive drift was larger in patients, but only following synchronous stimulation. Further, we observed stimulation-dependent changes in skin temperature. During right hand stimulation, temperature dropped in the stimulated hand and rose in the unstimulated hand. Interestingly, induction of RHI led to an out-of-body experience in one patient, linking body disownership and psychotic experiences. The RHI is quantitatively and qualitatively stronger in schizophrenia. These findings suggest that patients have a more flexible body representation and weakened sense of self, and potentially indicate abnormalities in temporo-parietal networks implicated in body ownership. Further, results suggest that these body ownership disturbances might be at the heart of a subset of the pathognomonic delusions of passivity.
Thakkar, Katharine N.; Nichols, Heathman S.; McIntosh, Lindsey G.; Park, Sohee
2011-01-01
Background A weakened sense of self may contribute to psychotic experiences. Body ownership, one component of self-awareness, can be studied with the rubber hand illusion (RHI). Watching a rubber hand being stroked while one's unseen hand is stroked synchronously can lead to a sense of ownership over the rubber hand, a shift in perceived position of the real hand, and a limb-specific drop in stimulated hand temperature. We aimed to assess the RHI in schizophrenia using quantifiable measures: proprioceptive drift and stimulation-dependent changes in hand temperature. Methods The RHI was elicited in 24 schizophrenia patients and 21 matched controls by placing their unseen hand adjacent to a visible rubber hand and brushing real and rubber hands synchronously or asynchronously. Perceived finger location was measured before and after stimulation. Hand temperature was taken before and during stimulation. Subjective strength of the illusion was assessed by a questionnaire. Results Across groups, the RHI was stronger during synchronous stimulation, indicated by self-report and proprioceptive drift. Patients reported a stronger RHI than controls. Self-reported strength of RHI was associated with schizotypy in controls Proprioceptive drift was larger in patients, but only following synchronous stimulation. Further, we observed stimulation-dependent changes in skin temperature. During right hand stimulation, temperature dropped in the stimulated hand and rose in the unstimulated hand. Interestingly, induction of RHI led to an out-of-body experience in one patient, linking body disownership and psychotic experiences. Conclusions The RHI is quantitatively and qualitatively stronger in schizophrenia. These findings suggest that patients have a more flexible body representation and weakened sense of self, and potentially indicate abnormalities in temporo-parietal networks implicated in body ownership. Further, results suggest that these body ownership disturbances might be at the heart of a subset of the pathognomonic delusions of passivity. PMID:22073126
NASA Astrophysics Data System (ADS)
Rahman, R.; Nemmang, M. S.; Hazurina, Nor; Shahidan, S.; Khairul Tajuddin Jemain, Raden; Abdullah, M. E.; Hassan, M. F.
2017-11-01
The main issue related to this research was to examine the feasibility of natural rubber SMR 20 in the manufacturing of cement mortar for sub-base layer construction. Subbase layers have certain functions that need to be fulfilled in order to assure strong and adequate permeability of pavement performance. In a pavement structure, sub-base is below the base and serves as the foundation for the overall pavement structure, transmitting traffic loads to the sub-grade and providing drainage. Based on this research, the natural rubber, SMR 20 was with the percentages of 0%, 5%, 10% and 15% to mix with sand in the manufacture of the cement mortar. This research describes some of the properties and cost of the materials for the natural rubber and sand in cement mortar manufacturing by laboratory testing. Effects of the natural rubber replacement on mechanical properties of mortar were investigated by laboratory testing such as compressive strength test and density. This study obtained the 5% of natural rubber replaced in sand can achieved the strength of normal mortar after 7 days and 28 days. The strength of cement mortar depends on the density of cement mortar. According to the cost of both materials, sand shows the lower cost in material for the cement mortar manufacturing than the uses of natural rubber. Thus, the convectional cement mortar which used sand need lower cost than the modified rubber cement mortar and the most economical to apply in industrial. As conclusion, the percentage of 5% natural rubber in the cement mortar would have the same with normal cement mortar in terms of the strength. However, in terms of the cost of the construction, it will increase higher than cost of normal cement mortar production. So that, this modified cement mortar is not economical for the road sub-base construction.
NASA Astrophysics Data System (ADS)
Abdul Hamid, Siti Atkah; Abdullah, Mustaffa Hj.; Ahmad, Sahrim Hj.; Mansor, Abdul Aziz; Yusoff, Ahmad Nazlim
2002-09-01
A microwave (Li0.5Fe0.5)0.4Ni0.3Zn0.3Fe2O4 (LNZ) ferrite was prepared by a conventional sintering method in air. Thermoplastic natural rubber (TPNR) was prepared from polypropylene (PP) and natural rubber (NR) in the ratios of 80:20, 70:30, 60:40, 50:50 and 40:60 with liquid natural rubber as a compatibilizer by a melt blending technique. LNZ ferrite-TPNR composites with 20 wt% ferrite filler were prepared using a Brabender plasticorder internal mixer. The microwave electromagnetic properties of the composites were studied in the frequency range of 0.3-13.5 GHz using a microwave vector network analyzer (MVNA). The real and imaginary components of the relative complex dielectric permittivity (\\varepsilonr*=\\varepsilonr\\prime-j\\varepsilonr\\prime\\prime) and magnetic permeability (μr*=μr\\prime-jμr\\prime\\prime) were calculated from the measured complex scattering parameters (S11* and S12*) using the Nicolson-Ross model. The dielectric and magnetic properties were found to depend on the NR and PP content in the composites. The minimum reflection loss (RL) under the matching conditions increases with increasing NR content.
[Blue rubber bleb naevus syndrome].
Akutko, Katarzyna; Krzesiek, Elzbieta; Iwańczak, Barbara
2012-10-01
Blue rubber bleb nevus syndrome (Bean syndrome) is a rare disease characterized by the presence of multiple vascular malformation of rubber-like consistence. This disease is of a genetic origin and most often is caused by sporadic mutation, however, exist reports on autosomal dominant type of heritance. Nevi are most frequently met in the skin and alimentary tract but may be present in all organs and tissues. The most frequent symptom of Bean syndrome is anaemia due to ferrum deficiency, which is a result of chronic hemorrhagia from vascular malformations in the alimentary tract. Vascular anomalies on the skin are usually asymptomatic. Other symptoms are less frequent and depend on the localisation of vascular changes and therefore patients with Bean syndrome require meticulous analysis of reported multiple - specialistic medical care.
Soft matter dynamics: Accelerated fluid squeeze-out during slip
NASA Astrophysics Data System (ADS)
Hutt, W.; Persson, B. N. J.
2016-03-01
Using a Leonardo da Vinci experimental setup (constant driving force), we study the dependency of lubricated rubber friction on the time of stationary contact and on the sliding distance. We slide rectangular rubber blocks on smooth polymer surfaces lubricated by glycerol or by a grease. We observe a remarkable effect: during stationary contact the lubricant is only very slowly removed from the rubber-polymer interface, while during slip it is very rapidly removed resulting (for the grease lubricated surface) in complete stop of motion after a short time period, corresponding to a slip distance typically of order only a few times the length of the rubber block in the sliding direction. For an elastically stiff material, poly(methyl methacrylate), we observe the opposite effect: the sliding speed increases with time (acceleration), and the lubricant film thickness appears to increase. We propose an explanation for the observed effect based on transient elastohydrodynamics, which may be relevant also for other soft contacts.
Reinforcement of dynamically vulcanized EPDM/PP elastomers using organoclay fillers
Tsai, Yuhsin; Wu, Jyh-Horng; Wu, Yao-Tsu; Li, Chia-Hao; Leu, Ming-Tsong
2008-01-01
Dynamically vulcanized EPDM/PP (ethylene-propylene-diene/polypropylene) elastomers reinforced with various amounts of organoclay were prepared using octylphenol-formaldehyde resin and stannous chloride dehydrate as vulcanizing agents. The effects of organoclay on vulcanization characteristics, rheological behavior, morphology, thermal stability and thermomechanical properties were studied. Experimental results showed that organoclay affected neither the vulcanization process nor the degree of vulcanization chemically. X-ray analysis revealed that these organoclay-filled thermoplastic vulcanizates (TPVs) were intercalated. With respect to the mechanical properties, organoclay increased both the strength and degree of elongation of TPVs. The morphological observation of fractured surfaces suggested that organoclay acted as a nucleating agent in TPVs, improving their mechanical properties. However, adding organoclay reduced the thermal stability of TPVs by decomposing the swelling agents in the organoclay. PMID:27878033
TRITIUM EFFECTS ON DYNAMIC MECHANICAL PROPERTIES OF POLYMERIC MATERIALS
DOE Office of Scientific and Technical Information (OSTI.GOV)
Clark, E
2008-11-12
Dynamic mechanical analysis has been used to characterize the effects of tritium gas (initially 1 atm. pressure, ambient temperature) exposure over times up to 2.3 years on several thermoplastics-ultrahigh molecular weight polyethylene (UHMW-PE), polytetrafluoroethylene (PTFE), and Vespel{reg_sign} polyimide, and on several formulations of elastomers based on ethylene propylene diene monomer (EPDM). Tritium exposure stiffened the elastic modulus of UHMW-PE up to about 1 year and then softened it, and reduced the viscous response monotonically with time. PTFE initially stiffened, however the samples became too weak to handle after nine months exposure. The dynamic properties of Vespel{reg_sign} were not affected. Themore » glass transition temperature of the EPDM formulations increased approximately 4 C. following three months tritium exposure.« less
Reinforcement of dynamically vulcanized EPDM/PP elastomers using organoclay fillers.
Tsai, Yuhsin; Wu, Jyh-Horng; Wu, Yao-Tsu; Li, Chia-Hao; Leu, Ming-Tsong
2008-12-01
Dynamically vulcanized EPDM/PP (ethylene-propylene-diene/polypropylene) elastomers reinforced with various amounts of organoclay were prepared using octylphenol-formaldehyde resin and stannous chloride dehydrate as vulcanizing agents. The effects of organoclay on vulcanization characteristics, rheological behavior, morphology, thermal stability and thermomechanical properties were studied. Experimental results showed that organoclay affected neither the vulcanization process nor the degree of vulcanization chemically. X-ray analysis revealed that these organoclay-filled thermoplastic vulcanizates (TPVs) were intercalated. With respect to the mechanical properties, organoclay increased both the strength and degree of elongation of TPVs. The morphological observation of fractured surfaces suggested that organoclay acted as a nucleating agent in TPVs, improving their mechanical properties. However, adding organoclay reduced the thermal stability of TPVs by decomposing the swelling agents in the organoclay.
DOE Office of Scientific and Technical Information (OSTI.GOV)
Francis, R.; Irwin, J.; Byrne, G.
1995-10-01
There is an increasing use of CRAs (corrosion resistant alloys) for subsea flowlines. These pipes carry corrosive fluids at high temperatures and pressures, and insulation is usually, applied to prevent excessive cooling of the process fluids. The present tests were undertaken to investigate the effect of insulation defects on the susceptibility to localized corrosion of a super duplex stainless steel at different internal temperatures. Four different commercial coating systems were tested, Neoprene, EPDM, Polyurethane and Polyurethane foam. The results show that pitting occurred at an average temperature of 55 C for neoprene and EPDM, and at lower temperatures for themore » other two coatings. The reasons for this are discussed, and the implications for service applications.« less
NASA Astrophysics Data System (ADS)
Kari, Leif
2017-09-01
The dynamic stiffness of a chemically and physically ageing rubber vibration isolator in the audible frequency range is modelled as a function of ageing temperature, ageing time, actual temperature, time, frequency and isolator dimension. In particular, the dynamic stiffness for an axially symmetric, homogeneously aged rubber vibration isolator is derived by waveguides where the eigenmodes given by the dispersion relation for an infinite cylinder satisfying traction free radial surface boundary condition are matched to satisfy the displacement boundary conditions at the lateral surface ends of the finite rubber cylinder. The constitutive equations are derived in a companion paper (Part 1). The dynamic stiffness is calculated over the whole audible frequency range 20-20,000 Hz at several physical ageing times for a temperature history starting at thermodynamic equilibrium at +25°C and exposed by a sudden temperature step down to -60°C and at several chemical ageing times at temperature +25°C with simultaneous molecular network scission and reformation. The dynamic stiffness results are displaying a strong frequency dependence at a short physical ageing time, showing stiffness magnitude peaks and troughs, and a strong physical ageing time dependence, showing a large stiffness magnitude increase with the increased physical ageing time, while the peaks and troughs are smoothed out. Likewise, stiffness magnitude peaks and troughs are frequency-shifted with increased chemical ageing time. The developed model is possible to apply for dynamic stiffness prediction of rubber vibration isolator over a broad audible frequency range under realistic environmental condition of chemical ageing, mainly attributed to oxygen exposure from outside and of physical ageing, primarily perceived at low-temperature steps.
NASA Technical Reports Server (NTRS)
Stanley, Stephanie D.
2008-01-01
Silicone is a contaminant that can cause catastrophic failure of a bond system depending on the materials and processes used to fabricate the bond system, Unfortunately, more and more materials are fabricated using silicone. The purpose of this testing was to evaluate which bond systems are sensitive to silicone contamination and whether or not a cleaning process could be utilized to remove the silicone to bring the bond system performance back to baseline. Due to the extensive nature of the testing attempts will be made to generalize the understanding within classes of substrates, bond systems, and surface preparation and cleaning methods. This study was done by contaminating various meta! (steel, inconel, and aluminum), phenolic (carbon cloth phenolic and glass cloth phenolic), and rubber (natural rubber, asbestos-silicone dioxide filled natural butyldiene rubber, silica-filled ethylene propylenediene monomer, and carbon-filled ethylene propylenediene monomer) substrates which were then bonded using various adhesives and coatings (epoxy-based adhesives, paints, ablative compounds, and Chemlok adhesives) to determine the effect silicone contamination has on a given bond system's performance. The test configurations depended on the bond system being evaluated. The study also evaluated the feasibility of removing the silicone contamination by cleaning the contaminated substrate prior to bonding. The cleaning processes also varied depending on bond system.
Contamination of injectable solutions with 2-mercaptobenzothiazole leached from rubber closures.
Reepmeyer, J C; Juhl, Y H
1983-11-01
An impurity, discovered in a sample of digoxin injectable solution commercially packaged in a syringe for single-dose delivery, was found to originate from the rubber closure of the syringe and was identified as 2-mercaptobenzothiazole, a common accelerator for rubber vulcanization. Several similarly packaged injectable solutions of a variety of drugs from various manufacturers were examined and over half contained 2-mercaptobenzothiazole. The compound was identified by UV spectrophotometry (including a pH-dependent shift in its absorbance maximum), by mass spectrometry, and by comparison with standard 2-mercaptobenzothiazole using silica gel and reverse-phase high-performance liquid chromatography (HPLC). The presence of this impurity in injectable solutions may have implications with regard to toxicity and may interfere with the assay of digoxin injectable solution by HPLC.
NASA Astrophysics Data System (ADS)
Bonicelli, Alessandra; Fuentes, Luis G.; Khalil Dawd Bermejo, Ibrahim
2017-10-01
Pervious concrete pavement is a recognized sustainable solution for urban roads. To enhance mechanical properties of pervious concrete material, in order to allow wider use of this technology, a lot of studies are going on all over the world. The use of a little percentage of fine aggregates is proven to increase the material resistance without an excessive reduction of permeability. This study aimed to evaluate the effect of replacing the fine virgin aggregates with r cycled tire rubber. 14 different mixes were analysed in terms of indirect tensile strength resistance, void content and density. Two different dimensions of crumb rubber were studied, as well as two different dosages, which were applied to different no-fine control mixes. All results were compared with the same control mixes containing natural fine aggregate. The mixes had a fixed granulometric curve but varied in water/cement ratio; this in order to evaluate the effect of recycled rubber depending to w/c ratio of the mix. An image analysis was also conducted to verify the rubber distribution in the mixture and the cracking surfaces. The experimental analysis showed that a correct proportioning of fine sand significantly increased the strength of the material. Moreover, the use of recycled waste tire rubber, gave interesting improvements respect to the no-fine control mixes, even though the developed resistance was lower respect to mixes containing mineral sand. This result was expected because of the cementing property of mineral sand. Although, the important result was that it was possible to use waste tire rubber in pervious concrete, with an appropriate dosage and granular dimension, for increasing the performance of traditional mix design, in order to achieve pavement materials more and more sustainable.
RHETT/EPDM Performance Characterization
NASA Technical Reports Server (NTRS)
Haag, T.; Osborn, M.
1998-01-01
The 0.6 kW Electric Propulsion Demonstration Module (EPDM) flight thruster system was tested in a large vacuum facility for performance measurements and functional checkout. The thruster was operated at a xenon flow rate of 3.01 mg/s, which was supplied through a self-contained propellant system. All power was provided through a flight-packaged power processing unit, which was mounted in vacuum on a cold plate. The thruster was cycled through 34 individual startup and shutdown sequences. Operating periods ranged from 3 to 3600 seconds. The system responded promptly to each command sequence and there were no involuntary shutdowns. Direct thrust measurements indicated that steady state thrust was temperature sensitive, and varied from a high of 41.7 mN at 16 C, to a low of 34.8 mN at 110 C. Short duration thruster firings showed rapid response and good repeatability.
Tritium, deuterium, and helium permeation through EPDM O-rings
DOE Office of Scientific and Technical Information (OSTI.GOV)
Swansiger, W.A.
1992-03-01
This paper discusses tritium permeabilities determined at room temperature, 1.0 MPa (150 psia) tritium for three 23.4 cm diameter EPDM (ethylene-propylene-diene monomer) O-rings using a full-scale mock-up of the Al-SX shipping container seal geometry. The AL-SX container is being developed by Sandia National Laboratories for shipping tritium reservoirs. To determine the tritium permeation rate as a function of temperature, a 50.8 mm diameter EPDM O-ring was tested from room temperature to 150{degrees}C at a pressure of 1.0 MPa. Additional permeation measurements were made under the following test conditions: deuterium and helium-4 at room temperature and a pressure of 1.0 MPamore » using the full-scale AL-SX fixture, tritium from 0.1 MPa to 1.0 MPa at 142{degrees}C using the 50.8 mm fixture, and deuterium form room temperature to 150{degrees}C at a pressure of 1.0 MPa using the three full-scale O-rings showed the average room temperature, 1.0 MPa steady state tritium permeation rate to be about 1 {times} 10{sup {minus}2} Pa-liter/sec (7.6 {times} 10{sup {minus}5} torr-liter/sec or 1 {times} 10{sup {minus}4} std cc/sec), well within the allowable limit of 7.1 {times} 10{sup {minus}2} Pa-liter/sec for tritium release form the AL-SX container.« less
NASA Astrophysics Data System (ADS)
El Labban, A.; Mousseau, P.; Bailleul, J. L.; Deterre, R.
2007-04-01
Although numerical simulation has proved to be a useful tool to predict the rubber vulcanization process, few applications in the process control have been reported. Because the end-use rubber properties depend on the state of cure distribution in the parts thickness, the prediction of the optimal distribution remains a challenge for the rubber industry. The analysis of the vulcanization process requires the determination of the thermal behavior of the material and the cure kinetics. A nonisothermal vulcanization model with nonisothermal induction time is used in this numerical study. Numerical results are obtained for natural rubber (NR) thick-section part curing. A controlled gradient of the state of cure in the part thickness is obtained by a curing process that consists not only in mold heating phase, but also a forced convection mold cooling phase in order to stop the vulcanization process and to control the vulcanization distribution. The mold design that allows this control is described. In the heating phase, the state of cure is mainly controlled by the chemical kinetics (the induction time), but in the cooling phase, it is the heat diffusion that controls the state of cure distribution. A comparison among different cooling conditions is shown and a good state of cure gradient control is obtained.
[Rubber band ligation in treatment of hemorrhoids: our experience].
Gaj, F; Biviano, I; Sportelli, G; Candeloro, L
2015-01-01
Hemorrhoids are a very common condition. The treatment depends upon persistence and severity of symptoms. For hemorrhoids of II and III grade the rubber band ligation may be therapeutic. Our aim is to report the outcomes of rubber band ligation of hemorrhoids, with a follow up of 6 months. A total of 50 patients underwent rubber band ligation for symptomatic hemorrhoids (grade II and III) without prolapse, between June 2012 and June 2014. All patients underwent plug test to rule out presence of rectal mucosal prolapse and were classified according to PATE classification (1). Each hemorrhoid was ligated with one rubber band through a ligator. All patients were evaluated immediately at the end of the procedure, after ten days and six months after the treatment. Patient's demographic and operative data were collected and analyzed. The mean patients age was 47.6±12.3 years (range 24-72). All procedures were performed without complications. Before rubber band ligation, 42 patients had rectal bleeding, 38 had perineal discomfort and 27 had itching. Ten days after the treatment, 12 patients presented self-limited rectal bleeding, but 10 of these had more hemorrhoids and underwent a second rubber band ligation. No patients complained perineal discomfort, and 8 patients had itching; 78% and 16% of patients respectively, experienced feeling of a foreign body inside the canal anal and anal pain. After 6 months, only 13 patients were occasionally symptomatic: 4 patients had rectal bleeding, 2 had perineal discomfort and 4 had itching. Three more patients presented both perineal discomfort and hitching. None had the feeling of a foreign body in anal canal or anal pain. Rubber band ligation is an efficacious, cost-effective and simple treatment for the second and third degree hemorrhoids without rectal mucosal prolapsed. In our hands, no severe complications developed and minor complications could be handled with ease.
Chemical compatibility screening results of plastic packaging to mixed waste simulants
DOE Office of Scientific and Technical Information (OSTI.GOV)
Nigrey, P.J.; Dickens, T.G.
1995-12-01
We have developed a chemical compatibility program for evaluating transportation packaging components for transporting mixed waste forms. We have performed the first phase of this experimental program to determine the effects of simulant mixed wastes on packaging materials. This effort involved the screening of 10 plastic materials in four liquid mixed waste simulants. The testing protocol involved exposing the respective materials to {approximately}3 kGy of gamma radiation followed by 14 day exposures to the waste simulants of 60 C. The seal materials or rubbers were tested using VTR (vapor transport rate) measurements while the liner materials were tested using specificmore » gravity as a metric. For these tests, a screening criteria of {approximately}1 g/m{sup 2}/hr for VTR and a specific gravity change of 10% was used. It was concluded that while all seal materials passed exposure to the aqueous simulant mixed waste, EPDM and SBR had the lowest VTRs. In the chlorinated hydrocarbon simulant mixed waste, only VITON passed the screening tests. In both the simulant scintillation fluid mixed waste and the ketone mixture simulant mixed waste, none of the seal materials met the screening criteria. It is anticipated that those materials with the lowest VTRs will be evaluated in the comprehensive phase of the program. For specific gravity testing of liner materials the data showed that while all materials with the exception of polypropylene passed the screening criteria, Kel-F, HDPE, and XLPE were found to offer the greatest resistance to the combination of radiation and chemicals.« less
NASA Astrophysics Data System (ADS)
Kimel'blat, V. I.; Volfson, S. I.; Chebotareva, I. G.; Malysheva, T. V.
1998-09-01
Pressure relaxation was examined in the cylinder of an MPT Monsanto processability tester after stopping the piston. The experimental function of the pressure drop F(t) was smoothed over and approximated by cubic splines. The spectra of pressure relaxation times (SPRT) were obtained according to the method of Schwarzl-Staverman. The SPRT method served well for estimating the spectra of the molecular-mass distribution (MMD) of polymers close in their physical sense to the SPRT. The correlation of the characteristic relaxation times and average molecular mass of ethylene-propylene rubbers and polyethylenes obtained by gel permeation chromatography was approximated by optimum models used for calculating the the molecular mass of rubbers according to the measurement results of the relaxation pressure of melts. The SPRT and characteristic relaxation times were used to analyze the significant technical properties of compositions based on polyethylene and rubber. The SPRT method was used to examine the failure of the cure network of butyl rubber and the dependence of the mechanical properties of thermoplastic elastomers on the molecular features of the decomposite.
Characterization of linear viscoelastic anti-vibration rubber mounts
DOE Office of Scientific and Technical Information (OSTI.GOV)
Lodhia, B.B.; Esat, I.I.
1996-11-01
The aim of this paper is to identify the dynamic characteristics that are evident in linear viscoelastic rubber mountings. The characteristics under consideration included the static and dynamic stiffnesses with the variation of amplitude and frequency of the sinusoidal excitation. Test samples of various rubber mix were tested and compared to reflect magnitude of dependency on composition. In the light of the results, the validity and effectiveness of a mathematical model was investigated and a suitable technique based on the Tschoegl and Emri Algorithm, was utilized to fit the model to the experimental data. The model which was chosen, wasmore » an extension of the basic Maxwell model, which is based on linear spring and dashpot elements in series and parallel called the Wiechert model. It was found that the extent to which the filler and vulcanisate was present in the rubber sample, did have a great effect on the static stiffness characteristics, and the storage and loss moduli. The Tschoegl and Emri Algorithm was successfully utilized in modelling the frequency response of the samples.« less
NASA Technical Reports Server (NTRS)
Stanley, Stephanie D.
2008-01-01
Silicone is a contaminant that can cause catastrophic failure of a bond system depending on the materials and processes used to fabricate the bond system. Unfortunately, more and more materials are fabricated using silicone. The purpose of this testing was to evaluate which bond systems are sensitive to silicone contamination and whether or not a cleaning process could be utilized to remove the silicone to bring the bond system performance back to baseline. Due to the extensive nature of the testing, attempts will be made to generalize the understanding within classes of substrates, bond systems, and surface preparation and cleaning methods. This study was done by contaminating various metal (steel, Inconel, and aluminum), phenolic (carbon-cloth phenolic [CCP] and glass-cloth phenolic [GCP]), and rubber (natural rubber, asbestos-silicone dioxide filled natural butyldiene rubber [ASNBR]; silica-filled ethylene propylenediene monomer [SFEPDM], and carbon-filled ethylene propylenediene monomer [CFEPDM]) substrates which were then bonded using various adhesives and coatings (epoxy-based adhesives, paints, ablative compounds, and Chemlok adhesives) to determine the effect silicone contamination has on a given bond system's performance. The test configurations depended on the bond system being evaluated. The study also evaluated the feasibility of removing the silicone contamination by cleaning the contaminated substrate prior to bonding. The cleaning processes also varied depending on bond system.
Rodrigues, L R; Banat, I M; van der Mei, H C; Teixeira, J A; Oliveira, R
2006-03-01
The effects and extent of adhesion of four different bacterial and two yeast strains isolated from explanted voice prostheses to silicone rubber with and without an adsorbed rhamnolipid biosurfactant layer obtained from Pseudomonasaeruginosa DS10-129 was studied. The ability of rhamnolipid biosurfactant to inhibit adhesion of micro-organisms to silicone rubber was investigated in a parallel-plate flow chamber. The anti-adhesive activity of the biosurfactant at different concentrations was significant against all the strains and depended on the micro-organism tested. The results showed an effective reduction in the initial deposition rates, and the number of bacterial cells adhering after 4 h, for all micro-organisms tested at the 4 g l(-1) undiluted rhamnolipid solution. Maximum initial reduction of adhesion rate (an average of 66%) occurred for Streptococcus salivarius GB 24/9 and Candida tropicalis GB 9/9. The number of cells adhering after 4 h on silicone rubber conditioned with biosurfactant was reduced to 48% for Staphylococcus epidermidis GB 9/6, Strep. salivarius GB 24/9, Staphylococcus aureus GB 2/1 and C. tropicalis GB 9/9 in comparison to controls. Perfusing the flow chamber with biosurfactant containing solution followed by the passage of a liquid-air interface, to investigate detachment of micro-organisms adhering to silicone rubber, produced high detachment (96%) of adhered cells for all micro-organisms studied, except for Staph. aureus GB 2/1 (67%). It is concluded that biosurfactant represent suitable compounds that should be considered in developing future strategies to prevent the microbial colonization of silicone rubber voice prostheses.
Hydrazine-Compatible Elastomer
NASA Technical Reports Server (NTRS)
Markles, O., F.; Dye, T. G.
1982-01-01
Hydrazine hardly reacts with ethylene propylene diene monomer, even at high temperatures. According to report to tests, EPDM is most hydrazine-compatible material among elastomers. Has strong potential as valve-seat and O-ring seal with hydrazine, especially at high temperatures.
DOE Office of Scientific and Technical Information (OSTI.GOV)
Skena, C.C.; Keiser, J.R.
1986-08-01
Previous laboratory tests of elastomer O-rings in coal liquefaction solvents conducted at L'Garde, Inc., indicated that certain ethylenepropylenediene monomer (EPDM) compounds provided the best performance when a backup ring was used to limit swelling. Before service testing in a pump at the Wilsonville, Alabama, Advanced Coal Liquefaction Research and Development Facility, tests of six selected elastomers in the appropriate Wilsonville-produced solvent were conducted at Oak Ridge National Laboratory (ORNL). The ORNL tests measured the elastomers' changes in cross section, weight, density, and relative flexibility. Although two perfluoroelastomers showed less degradation of most properties during these tests, it was decided tomore » proceed with service testing of two EPDM elastomers because of their much lower cost. 5 refs., 14 figs., 7 tabs.« less
DOE Office of Scientific and Technical Information (OSTI.GOV)
Willis, P. B.; Baum, B.; Schnitzer, H. S.
1979-12-01
Springborn Laboratories is engaged in a study of evaluating potentially useful encapsulating materials for Task 3 of the Low-Cost Silicon Solar Array project (LSA) funded by DOE. The goal of this program is to identify, evaluate, and recommend encapsulant materials and processes for the production of cost-effective, long-life solar cell modules. This report presents the results of a cost analysis of candidate potting compounds for long life solar module encapsulation. Additionally, the two major encapsulation processes, sheet lamination and liquid casting, are costed on the basis of a large scale production facility. Potting compounds studied include EVA, sheet, clear; EVA,more » sheet, pigmented; EPDM, sheet, clear; Aliphatic urethane, syrup; PVC Plastisol; Butyl acrylate, syrup; and Butyl acrylate, sheet.« less
DOE Office of Scientific and Technical Information (OSTI.GOV)
Perry, D.D.; Bolcar, J.P.
1990-04-01
A study has been conducted to determine the effects of commercial degreasing solvents on the conductivity of an EPDM separable connector shield and two types of cable shields based on EPR and XLPE, respectively. Solvents tested included a chlorinated solvent based on 1,1,1-trichloroethane and several so-called citrus solvents consisting of the natural terpene, limonene, or blends of limonene with other hydrocarbons. All the solvents significantly degraded the conductivity of the EPR and EPDM materials, but had little effect on the XLPE cable shield. The solvents differed, however, in the extent of their effects, the rate of recovery of conductivity aftermore » removal of the solvent, and the degree to which the original conductivity of the material was restored. The consequences of these results in terms of appropriate field use of these types of solvents by utility personnel are discussed.« less
A rubber tube in the bladder as a complication of autoerotic stimulation of the urethra.
Stamatiou, Konstantinos; Moschouris, Hippocrates
2016-10-05
Self-insertion of foreign bodies in the urethra is most commonly associated with sexual or erotic arousal of adolescents with mental health disorders. Rarely it may practiced by healthy adults for masturbation. Migration of foreign bodies used for the abovementioned purpose from the urethra to adjacent organs is a relatively uncommon urologic problem that may cause serious complications which arose tardive. Presentation includes a variety of acute or chronic symptoms that depend of the underlying complications. The method of extraction depends on the shape, size and nature of the object and should be tailored according to the condition of the patient. In the present article we present a case of a rubber tube inserted to the urethra for erotic arousal purposes which migrated to the bladder during masturbation.
Reduced adherence of Candida to silane-treated silicone rubber.
Price, C L; Williams, D W; Waters, M G J; Coulthwaite, L; Verran, J; Taylor, R L; Stickler, D; Lewis, M A O
2005-07-01
Silicone rubber is widely used in the construction of medical devices that can provide an essential role in the treatment of human illness. However, subsequent microbial colonization of silicone rubber can result in clinical infection or device failure. The objective of this study was to determine the effectiveness of a novel silane-treated silicone rubber in inhibiting microbial adherence and material penetration. Test material was prepared by a combination of argon plasma discharge treatment and fluorinated silane coupling. Chemicophysical changes were then confirmed by X-ray photoelectron spectroscopy, contact-angle measurement, and atomic force microscopy. Two separate adherence assays and a material penetration assay assessed the performance of the new material against four strains of Candida species. Results showed a significant reduction (p < 0.01) of Candida albicans GDH 2346 adherence to silane-treated silicone compared with untreated controls. This reduction was still evident after the incorporation of saliva into the assay. Adherence inhibition also occurred with Candida tropicalis MMU and Candida krusei NCYC, although this was assay dependent. Reduced penetration of silane-treated silicone by Candida was evident when compared to untreated controls, plaster-processed silicone, and acrylic-processed silicone. To summarize, a novel silicone rubber material is described that inhibits both candidal adherence and material penetration. The clinical benefit and performance of this material remains to be determined. Copyright 2005 Wiley Periodicals, Inc.
Asbestos Free Insulation Development for the Space Shuttle Solid Propellant Rocket Motor (RSRM)
NASA Technical Reports Server (NTRS)
Allred, Larry D.; Eddy, Norman F.; McCool, A. A. (Technical Monitor)
2000-01-01
Asbestos has been used for many years as an ablation inhibitor in insulating materials. It has been a constituent of the AS/NBR insulation used to protect the steel case of the RSRM (Reusable Solid Rocket Motor) since its inception. This paper discusses the development of a potential replacement RSRM insulation design, several of the numerous design issues that were worked and processing problems that were resolved. The earlier design demonstration on FSM-5 (Flight Support Motor) of the selected 7% and 11% Kevlar(registered) filled EPDM (KF/EPDM) candidate materials was expanded. Full-scale process simulation articles were built and FSM-8 was manufactured using multiple Asbestos Free (AF) components and materials. Two major problems had to be overcome in developing the AF design. First, bondline corrosion, which occurred in the double-cured region of the aft dome, had to be eliminated. Second, KF/EPDM creates high levels of electrostatic energy (ESE), which does not readily dissipate from the insulation surface. An uncontrolled electrostatic discharge (ESD) of this surface energy during many phases of production could create serious safety hazards. Numerous processing changes were implemented and a conductive paint was developed to prevent exposed external insulation surfaces from generating ESE/ESD. Additionally, special internal instrumentation was incorporated into FSM-8 to record real-time internal motor environment data. These data included inhibitor insulation erosion rates and internal thermal environments. The FSM-8 static test was successfully conducted in February 2000 and much valuable data were obtained to characterize the AF insulation design.
Balaji, Ananad Bellam; Ratnam, Chantara Thevy; Khalid, Mohammad; Walvekar, Rashmi
2018-03-01
The effect of electron beam radiation on ethylene-propylene diene terpolymer/polypropylene blends is studied as an attempt to develop radiation sterilizable polypropylene/ethylene-propylene diene terpolymer blends suitable for medical devices. The polypropylene/ethylene-propylene diene terpolymer blends with mixing ratios of 80/20, 50/50, 20/80 were prepared in an internal mixer at 165°C and a rotor speed of 50 rpm/min followed by compression molding. The blends and the individual components were radiated using 3.0 MeV electron beam accelerator at doses ranging from 0 to 100 kGy in air and room temperature. All the samples were tested for tensile strength, elongation at break, hardness, impact strength, and morphological properties. After exposing to 25 and 100 kGy radiation doses, 50% PP blend was selected for in vivo studies. Results revealed that radiation-induced crosslinking is dominating in EPDM dominant blends, while radiation-induced degradation is prevailing in PP dominant blends. The 20% PP blend was found to be most compatible for 20-60 kGy radiation sterilization. The retention in impact strength with enhanced tensile strength of 20% PP blend at 20-60 kGy believed to be associated with increased compatibility between PP and EPDM along with the radiation-induced crosslinking. The scanning electron micrographs of the fracture surfaces of the PP/EPDM blends showed evidences consistent with the above contentation. The in vivo studies provide an instinct that the radiated blends are safe to be used for healthcare devices.
Geothermal packers and packer elastomers
DOE Office of Scientific and Technical Information (OSTI.GOV)
Hirasuna, A.R.; Stephens, C.A.
1981-10-01
Reliability of thermal packers has been an eternal problem at temperatures beyond the 149 to 177/sup 0/C (300 to 350/sup 0/F) level. High temperature packer elastomer compounds were developed for 260/sup 0/C (500/sup 0/F) environments. Compounds based on four polymer systems were developed which exceed the contract requirements. The Y267 EPDM compound, particularly, has generated interest because of its good performance, economic pricing of constituents and good processability. Several successful downhole and laboratory trials of Y267 EPDM have occurred at moderate and extremely high temperatures. Otis Engineering tested a Y267 packer seal at 302/sup 0/C (575/sup 0/F) for five days.more » The Y267 seal in an Otis packer was subsequently run in a Bakersfield continuous steam injection well at about 204/sup 0/C (400/sup 0/F) for 5 months. The same model packers and elements were run in Union Geothermal wells at the Baca, NM where hydraulic stimulation and diagnostics occurred at 160 to 171/sup 0/C (320 to 340/sup 0/F). Los Alamos National Laboratory tested the Y267 EPDM O-rings for a cablehead. Tests were first run in an autoclave with water and Mobil One oil to temperatures in excess of 340/sup 0/C (644/sup 0/F). The Y267 equipped cablehead was subsequently run at Fenton Hill at 317/sup 0/C (603/sup 0/F). A new casing packer concept for 371/sup 0/C (700/sup 0/F) production service is now undergoing full-scale prototype development.« less
ERIC Educational Resources Information Center
American School & University, 1998
1998-01-01
Provides guidelines for school administrators to aid in the selection of school-roofing systems, and information required to make specification and purchasing decisions. Low-slope roofing systems are examined, as are multiply systems such as modified bitumen, EPDM, thermoplastic, metal, and foam. (GR)
Study on Impact Acoustic—Visual Sensor-Based Sorting of ELV Plastic Materials
Huang, Jiu; Tian, Chuyuan; Ren, Jingwei; Bian, Zhengfu
2017-01-01
This paper concentrates on a study of a novel multi-sensor aided method by using acoustic and visual sensors for detection, recognition and separation of End-of Life vehicles’ (ELVs) plastic materials, in order to optimize the recycling rate of automotive shredder residues (ASRs). Sensor-based sorting technologies have been utilized for material recycling for the last two decades. One of the problems still remaining results from black and dark dyed plastics which are very difficult to recognize using visual sensors. In this paper a new multi-sensor technology for black plastic recognition and sorting by using impact resonant acoustic emissions (AEs) and laser triangulation scanning was introduced. A pilot sorting system which consists of a 3-dimensional visual sensor and an acoustic sensor was also established; two kinds commonly used vehicle plastics, polypropylene (PP) and acrylonitrile-butadiene-styrene (ABS) and two kinds of modified vehicle plastics, polypropylene/ethylene-propylene-diene-monomer (PP-EPDM) and acrylonitrile-butadiene-styrene/polycarbonate (ABS-PC) were tested. In this study the geometrical features of tested plastic scraps were measured by the visual sensor, and their corresponding impact acoustic emission (AE) signals were acquired by the acoustic sensor. The signal processing and feature extraction of visual data as well as acoustic signals were realized by virtual instruments. Impact acoustic features were recognized by using FFT based power spectral density analysis. The results shows that the characteristics of the tested PP and ABS plastics were totally different, but similar to their respective modified materials. The probability of scrap material recognition rate, i.e., the theoretical sorting efficiency between PP and PP-EPDM, could reach about 50%, and between ABS and ABS-PC it could reach about 75% with diameters ranging from 14 mm to 23 mm, and with exclusion of abnormal impacts, the actual separation rates were 39.2% for PP, 41.4% for PP/EPDM scraps as well as 62.4% for ABS, and 70.8% for ABS/PC scraps. Within the diameter range of 8-13 mm, only 25% of PP and 27% of PP/EPDM scraps, as well as 43% of ABS, and 47% of ABS/PC scraps were finally separated. This research proposes a new approach for sensor-aided automatic recognition and sorting of black plastic materials, it is an effective method for ASR reduction and recycling. PMID:28594341
Study on Impact Acoustic-Visual Sensor-Based Sorting of ELV Plastic Materials.
Huang, Jiu; Tian, Chuyuan; Ren, Jingwei; Bian, Zhengfu
2017-06-08
This paper concentrates on a study of a novel multi-sensor aided method by using acoustic and visual sensors for detection, recognition and separation of End-of Life vehicles' (ELVs) plastic materials, in order to optimize the recycling rate of automotive shredder residues (ASRs). Sensor-based sorting technologies have been utilized for material recycling for the last two decades. One of the problems still remaining results from black and dark dyed plastics which are very difficult to recognize using visual sensors. In this paper a new multi-sensor technology for black plastic recognition and sorting by using impact resonant acoustic emissions (AEs) and laser triangulation scanning was introduced. A pilot sorting system which consists of a 3-dimensional visual sensor and an acoustic sensor was also established; two kinds commonly used vehicle plastics, polypropylene (PP) and acrylonitrile-butadiene-styrene (ABS) and two kinds of modified vehicle plastics, polypropylene/ethylene-propylene-diene-monomer (PP-EPDM) and acrylonitrile-butadiene-styrene/polycarbonate (ABS-PC) were tested. In this study the geometrical features of tested plastic scraps were measured by the visual sensor, and their corresponding impact acoustic emission (AE) signals were acquired by the acoustic sensor. The signal processing and feature extraction of visual data as well as acoustic signals were realized by virtual instruments. Impact acoustic features were recognized by using FFT based power spectral density analysis. The results shows that the characteristics of the tested PP and ABS plastics were totally different, but similar to their respective modified materials. The probability of scrap material recognition rate, i.e., the theoretical sorting efficiency between PP and PP-EPDM, could reach about 50%, and between ABS and ABS-PC it could reach about 75% with diameters ranging from 14 mm to 23 mm, and with exclusion of abnormal impacts, the actual separation rates were 39.2% for PP, 41.4% for PP/EPDM scraps as well as 62.4% for ABS, and 70.8% for ABS/PC scraps. Within the diameter range of 8-13 mm, only 25% of PP and 27% of PP/EPDM scraps, as well as 43% of ABS, and 47% of ABS/PC scraps were finally separated. This research proposes a new approach for sensor-aided automatic recognition and sorting of black plastic materials, it is an effective method for ASR reduction and recycling.
Noble, Peter A; Park, Hee-Deung; Olson, Betty H; Asvapathanagul, Pitiporn; Hunter, M Colby; Garrido-Baserba, Manel; Lee, Sang-Hoon; Rosso, Diego
2016-07-01
Aeration diffusers in wastewater treatment plants generate air bubbles that promote mixing, distribution of dissolved oxygen, and microbial processing of dissolved and suspended matter in bulk solution. Biofouling of diffusers represents a significant problem to wastewater treatment plants because biofilms decrease oxygen transfer efficiency and increase backpressure on the blower. To better understand biofouling, we conducted a pilot study to survey the bacterial community composition and function of biofilms on different diffuser substrates and compare them to those in the bulk solution. DNA was extracted from the surface of ethylene-propylene-diene monomer (EPDM), polyurethane, and silicone diffusers operated for 15 months in a municipal treatment plant and sampled at 3 and 9 months. The bacterial community composition and function of the biofilms and bulk solution were determined by amplifying the 16S rRNA genes and pyrosequencing the amplicons and raw metagenomic DNA. The ordination plots and dendrograms of the 16S rRNA and functional genes showed that while the bacterial community composition and function of the bulk solution was independent of sampling time, the composition and function of the biofilms differed by diffuser type and testing time. For the EPDM and silicone diffusers, the biofilm communities were more similar in composition to the bulk solution at 3 months than 9 months. In contrast, the bacteria on the polyurethane diffusers were more dissimilar to the bulk solution at 3 months than 9 months. Taken together, the survey showed that the community composition and function of bacterial biofilms depend on the diffuser substrate and testing time, which warrants further elucidation.
Tjoa, Aiyen; Veldkamp, Edzo
2015-01-01
Rapid deforestation in Sumatra, Indonesia is presently occurring due to the expansion of palm oil and rubber production, fueled by an increasing global demand. Our study aimed to assess changes in soil-N cycling rates with conversion of forest to oil palm (Elaeis guineensis) and rubber (Hevea brasiliensis) plantations. In Jambi Province, Sumatra, Indonesia, we selected two soil landscapes – loam and clay Acrisol soils – each with four land-use types: lowland forest and forest with regenerating rubber (hereafter, “jungle rubber”) as reference land uses, and rubber and oil palm as converted land uses. Gross soil-N cycling rates were measured using the 15N pool dilution technique with in-situ incubation of soil cores. In the loam Acrisol soil, where fertility was low, microbial biomass, gross N mineralization and NH4 + immobilization were also low and no significant changes were detected with land-use conversion. The clay Acrisol soil which had higher initial fertility based on the reference land uses (i.e. higher pH, organic C, total N, effective cation exchange capacity (ECEC) and base saturation) (P≤0.05–0.09) had larger microbial biomass and NH4 + transformation rates (P≤0.05) compared to the loam Acrisol soil. Conversion of forest and jungle rubber to rubber and oil palm in the clay Acrisol soil decreased soil fertility which, in turn, reduced microbial biomass and consequently decreased NH4 + transformation rates (P≤0.05–0.09). This was further attested by the correlation of gross N mineralization and microbial biomass N with ECEC, organic C, total N (R=0.51–0. 76; P≤0.05) and C:N ratio (R=-0.71 – -0.75, P≤0.05). Our findings suggest that the larger the initial soil fertility and N availability, the larger the reductions upon land-use conversion. Because soil N availability was dependent on microbial biomass, management practices in converted oil palm and rubber plantations should focus on enriching microbial biomass. PMID:26222690
NASA Astrophysics Data System (ADS)
Amrina, E.; Yulianto, A.
2018-03-01
Sustainable maintenance is a new challenge for manufacturing companies to realize sustainable development. In this paper, an interpretive structural model is developed to evaluate sustainable maintenance in the rubber industry. The initial key performance indicators (KPIs) is identified and derived from literature and then validated by academic and industry experts. As a result, three factors of economic, social, and environmental dividing into a total of thirteen indicators are proposed as the KPIs for sustainable maintenance evaluation in rubber industry. Interpretive structural modeling (ISM) methodology is applied to develop a network structure model of the KPIs consisting of three levels. The results show the economic factor is regarded as the basic factor, the social factor as the intermediate factor, while the environmental factor indicated to be the leading factor. Two indicators of social factor i.e. labor relationship, and training and education have both high driver and dependence power, thus categorized as the unstable indicators which need further attention. All the indicators of environmental factor and one indicator of social factor are indicated as the most influencing indicator. The interpretive structural model hoped can aid the rubber companies in evaluating sustainable maintenance performance.
Yeang, Hoong-Yeet
2007-01-01
How tropical trees flower synchronously near the equator in the absence of significant day length variation or other meteorological cues has long been a puzzle. The rubber tree (Hevea brasiliensis) is used as a model to investigate this phenomenon. The annual cycle of solar radiation intensity is shown to correspond closely with the flowering of the rubber tree planted near the equator and in the subtropics. Unlike in temperate regions, where incoming solar radiation (insolation) is dependent on both day length and radiation intensity, insolation at the equator is due entirely to the latter. Insolation at the upper atmosphere peaks twice a year during the spring and autumn equinoxes, but the actual solar radiation that reaches the ground is attenuated to varying extents in different localities. The rubber tree shows one or two flowering seasons a year (with major and minor seasons in the latter) in accordance with the solar radiation intensity received. High solar radiation intensity, and in particular bright sunshine (as distinct from prolonged diffuse radiation), induces synchronous anthesis and blooming in Hevea around the time of the equinoxes. The same mechanism may be operational in other tropical tree species.
Mechanical behaviour of cerclage material consisting of silicon rubber.
Hinrichsen, G; Eberhardt, A; Springer, H
1979-09-01
Silicon rubber specimens of circular or rectangular cross-section (cross-section area between ca. 2 and 7 mm2) are used as cerclage bands. A series of commercial cerclage elements was investigated for mechanical characteristics, such as stress-strain behaviour and modulus of elasticity, using a tensile-testing machine. Large differences in these properties exist among the various specimens. Moreover, time-dependent effects, such as stress-relaxation, retardation, and creep, were analysed by the present investigations. One has to take into consideration that the initial length and stress of the cerclage band vary significantly with time after the operation.
Lafont, U; van Zeijl, H; van der Zwaag, S
2012-11-01
Synthetic systems with intrinsic self-repairing or self-healing abilities have emerged during the past decade. In this work, the influence of the cross-linker and chain rigidity on the healing ability of thermoset rubbers containing disulfide bonds have been investigated. The produced materials exhibit adhesive and cohesive self-healing properties. The recovery of these two functionalities upon the thermally triggered healing events has shown to be highly dependent on the network cross-link density and chain rigidity. As a result, depending on the rubber thermoset intrinsic physical properties, the thermal mending leading to full cohesive recovery can be achieved in 20-300 min at a modest healing temperature of 65 °C. The adhesive strength ranges from 0.2 to 0.5 MPa and is fully recovered even after multiple failure events.
de Vocht, Frank; Sobala, Wojciech; Wilczynska, Urszula; Kromhout, Hans; Szeszenia-Dabrowska, Neonila; Peplonska, Beata
2009-08-01
Most data on carcinogenic risk in the rubber industry are based on data from Western countries. This study assessed cancer risks in a retrospective cohort in a Polish tire manufacturing plant, relying on quantified exposure to inhalable aerosols and aromatic amines instead of job titles or external comparisons. Cumulative exposure for all exposures was assigned to cohort members based on estimates from a company-specific JEM. Cancer risks associated with cumulative exposure adjusted for co-exposures, gender and year of birth were calculated. Exposure levels were higher for women than for men. Aromatic amine exposure was significantly associated with increased urinary bladder cancer risk (RR=7.32-8.27), depending on exposure level, and prostate cancer at low levels only (RR=5.86). In women, increased risks were found for all cancers (RR=2.50) and of the digestive organs and peritoneum (RR=4.54) at low level only, while an exposure-response association with breast cancer risk was found. Inhalable aerosol exposure was associated with cancers of the liver and intrahepatic bile ducts in a dose-dependent manner, while dose-dependent reduced risks were found for respiratory cancers (most notably the larynx) and cancer of the colon. Increased risks for specific cancer sites in this rubber plant were similar to Western Europe and the US. However, several cancer risks were gender-specific which could relate to higher exposure levels in women or to differences in exposures to chemicals not assessed in this study.
Rubber dam use less stressful for children and dentists.
Innes, Nicola
2012-06-01
Randomised controlled trial, single centre and operator. 72 patients (6-16 years) assessed as compliant, with no allergies, not on significant medication were divided into two groups by 'drawing sealed lots'. 234 fully erupted teeth were sealed. Molars and/or premolars were sealed dependant on age. Teeth were pre-cleaned with prophy paste. In the controls, teeth were isolated with buccal and lingual cotton rolls and salivary ejector in the intervention group a rubber dam was used. The same etching, rinsing and placement protocol was used in both arms. Outcomes were: patients' subjective measures of pain using a visual analogue scale; blood pressure (before and after treatment), breath rate, pulse rate and skin resistance at five time points. The operator's pulse rate was measured and they completed a questionnaire on subjective mental and physical stress following treatment. Treatment times were recorded. The breath rate was significantly (P < 0.05) lower and the skin resistance level was significantly higher during treatment with rubber dam compared to the control group. Subjective pain perception was significantly lower for the test group. The treatment time needed for the fissure sealing procedure was 12.4% less in the test group. The authors state; '... in the hands of an experienced dentist, isolation with rubber dam is less stressful for children and adolescents than isolation with cotton rolls, and can save valuable treatment time.' The operator's stress measures were lower with rubber dam and treatment time was reduced.
Low Cost, Single Layer Replacement for the Back-Sheet and Encapsulant Layers
DOE Office of Scientific and Technical Information (OSTI.GOV)
Kempe, M. D.; Thapa, P.
2008-01-01
Ethylene propylene diene monomer (EPDM) based polymers have been formulated for specific use in photovoltaic modules to produce better performance and longer term stability at a lower cost than standard materials. EPDM formulations are advantageous over ethylene vinyl-acetate (EVA) because they can use the same lamination/cure cycle as EVA, they do not need a second back-sheet protective material (e.g. PET/Tedlar), they have a lower glass transition temperature, no melting transition, more constant mechanical moduli as a function of temperature, they are less polar than EVA (provides better corrosion protection), and they have excellent damp heat (85 C/85% relative humidity) resistancemore » against delamination. Module designs typically use EVA on the back side of cells despite the fact that transparency is not advantageous. We have developed a single encapsulant layer that will replace standard module back-sheet constructions consisting of EVA/PET/Tedlar. Because a single low-cost material layer is used, it will provide a significant materials cost savings of about $6 to $8/m{sup 2} as compared to traditional back-sheets. Electrical insulation tests were conducted using 0.85 mm thick stainless steel sheets as a model for a cell. It was found that a polymer layer thickness of about 0.33mm provided better high voltage electrical insulation than a combined film of Tedla (0.038 mm)/PET (0.051 mm)/EVA (0.55 mm). When formulated with a white pigment, reflectivity was comparable to Tedlar{trademark}. Upon accelerated exposure to light at 60C and 60% RH it was found that an EVA layer in front of these materials would decompose before significant yellowing and delamination of the back EPDM layer occurs.« less
Influence of Rubber Size on Properties of Crumb Rubber Mortars
Yu, Yong; Zhu, Han
2016-01-01
Studies on the properties and applications of rubber cement-based materials are well documented. The sizes of rubbers used in these materials varied. However, information about the effects of rubber size on the properties of rubber cement-based materials, especially pore structure, mechanical strengths, and drying shrinkage properties, remains limited. Three groups of rubber with major particle sizes of 2–4 mm, 1–3 mm, and 0–2 mm were selected in this study. This paper presents experimental studies on the effects of rubber size on the consistency, fresh density, pore structure, mechanical properties, and drying shrinkage properties of crumb rubber mortars (CRMs). Results demonstrated that the consistency and fresh density of CRMs decreased with the rubber size. As to the pore structure, the total pore volume increased with the decrease of the rubber size. By contrast, the influence of the rubber size on the mesopore (<50 nm) volume is not as significant as that of the rubber content. The mechanical properties of CRMs decreased with the rubber size. Low rubber stiffness and large pore volumes, especially those of small sized rubbers, contribute to the reduction of CRMs strength. The drying shrinkage of CRM increases as the rubber size decreases. The influences of rubber size on capillary tension are not significant. Thus, the shrinkage increases with the decrease of rubber size mainly because of its function in the deformation modulus reduction of CRMs. PMID:28773649
Hillebrand, Andrea; Post, Janina J.; Wurbs, David; Wahler, Daniela; Lenders, Malte; Krzyzanek, Vladislav; Prüfer, Dirk; Gronover, Christian Schulze
2012-01-01
The biosynthesis of rubber is thought to take place on the surface of rubber particles in laticifers, highly specialized cells that are present in more than 40 plant families. The small rubber particle protein (SRPP) has been supposed to be involved in rubber biosynthesis, and recently five SRPPs (TbSRPP1–5) were identified in the rubber-producing dandelion species Taraxacum brevicorniculatum. Here, we demonstrate by immunogold labeling that TbSRPPs are localized to rubber particles, and that rubber particles mainly consist of TbSRPP3, 4 and 5 as shown by high-resolution two-dimensional gel electrophoresis and mass spectrometric analysis. We also carried out an RNA-interference approach in transgenic plants to address the function of TbSRPPs in rubber biosynthesis as well as rubber particle morphology and stability. TbSRPP-RNAi transgenic T. brevicorniculatum plants showed a 40–50% reduction in the dry rubber content, but neither the rubber weight average molecular mass nor the polydispersity of the rubber were affected. Although no phenotypical differences to wild-type particles could be observed in vivo, rubber particles from the TbSRPP-RNAi transgenic lines were less stable and tend to rapidly aggregate in expelling latex after wounding of laticifers. Our results prove that TbSRPPs are very crucial for rubber production in T. brevicorniculatum, probably by contributing to a most favourable and stable rubber particle architecture for efficient rubber biosynthesis and eventually storage. PMID:22911861
Equilibrium swelling of elastomeric materials in solvent environments
DOE Office of Scientific and Technical Information (OSTI.GOV)
Green, P.F.
1990-03-01
The equilibrium swelling of silicones, fluorosilicones, VITON and ethylene-propylene-diene (EPDM) elastomers in an environment of the jet fuel JP4 was investigated. The volume of silicone and DPDM elastomers increased by approximately 100% when they were placed in a saturated environment of JP4. Conversely, the volume of the fluorosilicone elastomer increased by approximately 15% and that of VITON less than 1%. In acetone, a commonly used solvent, the equilibrium swelling of VITON and the fluorosilicone elastomer was excessive, on the order of 100%, wheras the silicone and EPDM elastomers exhibited small changes in dimensions. Reasons for these observations are discussed inmore » detail. We also present a simple scheme by which one may, qualitatively, determine the dimensional stability of these elastomers in different solvents if the cohesive energy density of the solvent, which is readily available in a number of handbooks, is known. We also evaluated the vulnerability of some commonly used engineering thermoplastics to JP4. The results are tabulated. 13 refs., 6 figs., 3 tab.« less
Fjeldaas, T; Sogstad, A M; Osterås, O
2011-03-01
This study was part of a cross-sectional project on freestall housing, and the aim was to compare locomotion and claw disorders in freestall dairy cattle herds with slatted concrete, solid concrete, or solid rubber flooring in the alleys. The final population for studying claw disorders consisted of 66 dairy herds with 2,709 dry or lactating cows, whereas the population for studying locomotion consisted of 54 herds with 2,216 cows. All herds used Norwegian Red as the main breed. The herds were visited by 15 trained claw trimmers one time during the period from the beginning of February to summer let-out onto pasture in 2008. The trimmers assessed locomotion scores (LocS) of all cows before trimming. At trimming, claw disorders were diagnosed and recorded in the Norwegian Claw Health Card. Estimates describing locomotion and claw disorders in the hind feet were identified by use of multivariable models fit with LocS and each claw disorder as dependent variables, respectively. Herd nested within claw trimmer was included in the model as random effects. The odds ratio (OR) of having LocS >2 and LocS >3 was 1.9 and 2.1, respectively, on slatted concrete compared with solid concrete. Fewer cases of dermatitis were found on slatted than solid concrete (OR=0.70) and a tendency was observed for fewer heel horn erosions on slatted concrete than solid rubber (OR=0.47). Hemorrhages of the white line and sole were more prevalent in herds housed on slatted and solid concrete than in those housed on solid rubber (OR=2.6 and OR=2.1, respectively). White line fissures were also more prevalent in herds housed on slatted and solid concrete than in those housed on solid rubber (OR=2.1 and OR=2.0, respectively). Double soles were more prevalent on solid concrete than solid rubber (OR=4.4). However, sole ulcers were less prevalent in herds with slatted and solid concrete than solid rubber (OR=0.39 and OR=0.53, respectively). Fewer corkscrewed claws were found on slatted concrete than both solid rubber and solid concrete (OR=0.60 and OR=0.44, respectively). More white line crossing fissures were recorded on slatted and solid concrete than solid rubber (OR=3.6 and OR=3.1, respectively). This shows that solid rubber flooring was favorable when most laminitis-related lesions were considered, whereas slatted concrete was favorable for infectious claw lesions and corkscrewed claws but not for locomotion. Copyright © 2011 American Dairy Science Association. Published by Elsevier Inc. All rights reserved.
Water requirements of the styrene, butadiene and synthetic-rubber industries
Durfor, Charles N.
1963-01-01
About 710 million gallons of makeup water is withdrawn daily by the styrene, butadiene, styrene-butadiene rubber (SBR), and specialty-rubber industries; 88 percent of this water is used only for once-through cooling. About 429 million gallons of water daily (mgd) is withdrawn by the butadiene industry; 158 ragd is withdrawn by the styrene industry; 94 mgd is used to make special-purpose synthetic rubber; and 29 mgd is used in the direct manufacture of SBR. The amount of makeup water withdrawn to produce SBR ranges from 11,400 to 418,000 gallons per long ton of finished rubber. The amount of makeup water withdrawn depends upon the type of rubber, the processes used to make SBR and its intermediates (styrene and butadiene), and the availability of water at the styrene, butadiene, and SBR plants. The amount of makeup water used to make styrene ranged from 2.19 to 123 gallons per pound; to make butadiene, ranged from 5.38 to 22.0 gallons per pound; and in the direct manufacture of SBR, ranged from 0.883 to 10.2 gallons per pound of finished rubber. The amount of makeup water withdrawn for use in the manufacture of special-purpose synthetic rubber ranged from 8.45 to 104 gallons per pound. About 64 percent of the makeup water was obtained from salty water sources. These waters, which were used only in once-through cooling, contained as much as 35,000 ppm of dissolved solids. About 26 percent of the makeup water was obtained from fresh-water streams and lakes, and most of the other makeup waters were obtained from ground water. Less than 1 percent of the makeup water was obtained from reprocessed municipal sewage. Most makeup water from fresh-water streams, lakes, and wells contained less than 1,000 ppm of dissolved solids, and most makeup water used in the manufacture of SBR contained less than 500 ppm of dissolved solids. The maximum hardness of the untreated fresh makeup waters; used in the manufacture of SBR was less than 500 ppm. About 97 percent of the makeup water withdrawn was discharged to surface waters; the warmed salty waters were returned to their source. The remaining 3 percent, or about 23.6 mgd, of makeup water was used consumptively. The styrene industry consumptively used about 2.0 percent of its intake; the butadiene industry, about 4.5 percent; the specialty-rubber industry, about 9.1 percent; and the SBR industry, about 11 percent. The water shipped in the synthetic-rubber products increased the consumptive use of water by these industries.
In-depth proteome analysis of the rubber particle of Hevea brasiliensis (para rubber tree).
Dai, Longjun; Kang, Guijuan; Li, Yu; Nie, Zhiyi; Duan, Cuifang; Zeng, Rizhong
2013-05-01
The rubber particle is a special organelle in which natural rubber is synthesised and stored in the laticifers of Hevea brasiliensis. To better understand the biological functions of rubber particles and to identify the candidate rubber biosynthesis-related proteins, a comprehensive proteome analysis was performed on H. brasiliensis rubber particles using shotgun tandem mass spectrometry profiling approaches-resulting in a thorough report on the rubber particle proteins. A total of 186 rubber particle proteins were identified, with a range in relative molecular mass of 3.9-194.2 kDa and in isoelectric point values of 4.0-11.2. The rubber particle proteins were analysed for gene ontology and could be categorised into eight major groups according to their functions: including rubber biosynthesis, stress- or defence-related responses, protein processing and folding, signal transduction and cellular transport. In addition to well-known rubber biosynthesis-related proteins such as rubber elongation factor (REF), small rubber particle protein (SRPP) and cis-prenyl transferase (CPT), many proteins were firstly identified to be on the rubber particles, including cyclophilin, phospholipase D, cytochrome P450, small GTP-binding protein, clathrin, eukaryotic translation initiation factor, annexin, ABC transporter, translationally controlled tumour protein, ubiquitin-conjugating enzymes, and several homologues of REF, SRPP and CPT. A procedure of multiple reaction monitoring was established for further protein validation. This comprehensive proteome data of rubber particles would facilitate investigation into molecular mechanisms of biogenesis, self-homeostasis and rubber biosynthesis of the rubber particle, and might serve as valuable biomarkers in molecular breeding studies of H. brasiliensis and other alternative rubber-producing species.
NASA Astrophysics Data System (ADS)
Saputra, A. H.; Juneva, S.; Sari, T. I.; Cifriadi, A.
2018-04-01
Dimethyl ether can cause degradation of the rubber material seal in some applications. In order to use of natural rubber in industry, research about a blending of natural rubber (NR) and nitrile rubber (NBR) to produce rubber to meet the standard seal material application were conducted. This study will observe the degradation mechanisms that occur in the blending natural rubber and nitrile rubber (NR/NBR) by dimethyl ether. Nitrile rubber types used in this study is medium quality nitrile rubber with 33% of acrylonitrile content (NBR33). The observed parameters are percent change in mass, mechanical properties and surface morphology. This study is limited to see the effect of variation vulcanized blending ratio (NR/NBR33) against to swelling. The increase of nitrile rubber (NBR33) ratio of blending rubber vulcanized can reduce the tensile strength and elongation. The best elastomer variation was obtained after comparing with the standard feasibility material of seal is rubber vulcanized blending (NR/NBR33) with ratio 40:60 NR: NBR.
NASA Technical Reports Server (NTRS)
Hare, David A.; Moore, Thomas C., Sr.
2000-01-01
The Langley Research Center uses strain gages in a wide variety of demanding test environments. Strain gage installations, depending on the testing scenario, may see high temperatures, cryogenic temperature, moisture accumulation, mechanical abuse, or any combination of these conditions. At Langley, there is often a need to provide protection for strain gages against moisture and mechanical abuse, especially when large-scale, harsh environment testing is to be encountered. This technical memorandum discusses the evaluation of a room temperature curing silicone rubber sealant manufactured by the General Electric Company for consideration as a moisture-barrier for certain strain gage installations.
A novel application of ADC/K-foaming agent-loaded NBR rubber composites as pressure sensor
NASA Astrophysics Data System (ADS)
Mahmoud, W. E.; El-Eraki, M. H. I.; El-Lawindy, A. M. Y.; Hassan, H. H.
2006-02-01
Nitrile butadiene rubber (NBR) structure foam of different apparent densities was obtained by using different concentrations of foaming agent, azodicarbonamide, ADC/K. The true stress-strain characteristics, in case of compression, of foamed samples were measured. It was found that the theoretical values predicted from the simple blending model are in more agreement with the experimental results than those from the square-relationship model. The effect of cyclic loading-unloading and dissipation energy of rubber foams was studied. The results also indicated that foams with low density exhibited a small hysteresis. The electrical properties were found dependent on the foaming agent concentration. This study was assisted by Mott and Gurney equation. The effect of compressive strain on the electrical conductivity of rubber foams was studied. The free current carrier mobility and the equilibrium concentration of charge carrier in the conduction band were produced as functions of compressive strain. The results also indicate that there is a linear variation between pressure and conductivity for all samples, which means that these samples can be used as a pressure sensor. At a certain concentration of foaming agent (5 phr) a change of electrical conductivity by more than three orders is observed at 20% compression strain.
NASA Astrophysics Data System (ADS)
Staszak, Maciej
2018-03-01
Following chapter presents short introductory description of rubber and rubber industry. The main problem of rubber industry is the way of the usage of spent tires. Furthermore very important group of problems arise considering the metal and nonmetal additives which are significant component of the vulcanized rubber. The key attention is dedicated to typical ways of rubber usage in utilization and recovery of metals from spent rubber materials concentrating specifically on used tires processing. The method of recovery of rare metals from rubber tires was described. The rubber debris finds widest use in the field of waste metal solutions processing. The environmental pollution caused by metals poses serious threat to humans. Several applications of the use of waste rubber debris to remove metals from environmental waters were described. Moreover, the agriculture usage of waste tire rubber debris is described, presenting systems where the rubber material can be useful as a soil replacement.
Rubber-like materials derived from biosourced phenolic resins
NASA Astrophysics Data System (ADS)
Amaral-Labat, G.; Grishechko, L. I.; Silva, G. F. B. Lenz e.; Kuznetsov, B. N.; Fierro, V.; Pizzi, A.; Celzard, A.
2017-07-01
The present work describes new gels derived from cheap, abundant and non-toxic wood bark extracts of phenolic nature, behaving like elastomers. Especially, we show that these materials might be used as rubber springs. Such amazing properties were obtained by a quite simple synthesis based on the autocondensation of flavonoid tannins in water at low pH in the presence of a plasticizer. After gelation and drying, the materials presented elastic properties that could be tuned from hard and brittle to quite soft and deformable, depending on the amount of plasticizer in the starting formulation. Not only the materials containing the relevant amount of plasticizer had stress-strain characteristics in quasi-static and cyclic compression similar to most commercial rubber springs, but they presented outstanding fire retardance, surviving 5 min in a flame at 1000°C in air. Neither flame propagation nor drips were noticed during the fire test, and the materials were auto-extinguishable. These excellent features make these materials potential substitutes to usual organic elastomers.
DOE Office of Scientific and Technical Information (OSTI.GOV)
Bandyopadhyay, S.
The deformation and failure processes involved in the fracture of unmodified epoxies are discussed in this chapter. A review of the fracture behavior of the carboxyl-terminated butadiene-acrylonitrile copolymer (CTBN) rubber-modified diglycidyl ether of bisphenol. A (DGEBA) polymers with or without a rigid particulate - fiber phase is presented in relation to the microscopic aspects of localized deformation and their relationship to microscopic fracture behavior are illustrated. The degree of improvement in fracture properties in modified materials depends to a great extent on the unmodified epoxy. If the latter is capable of even small-scale deformation at the crack tip, this inducesmore » in the modified system a number of additional microscopic failure mechanisms such as cavitation of rubber particles; enhanced shear deformation of the matrix, debonding and tearing of rubber, crack pinning, and debonding and pull-out of fibers. The recent research trend in toughening of high-temperature-grade TGMDA (tetraglycidyl 4,4{prime}-methylenedianiline) resin is also outlined. 73 refs., 23 figs., 2 tabs.« less
NASA Astrophysics Data System (ADS)
Indriani Dalimunthe, Cici; Tistama, Radite; Wahyuni, Sri
2017-12-01
The Conventional detection of White Root Disease (Rigidoporus microporus, WRD) still uses the visual method based on an abnormal color of leaf or mycelium growth on the tap root neck. The method was less effective and less efficient. The serological technique uses yolk chicken antibodies induced by immunization with mycelium extract. The purpose of this research was to examine the consistency of selected antibodies in detecting root fungi at various soil types in the rubber plantations. This research used a Completely Randomized Design non-factorial with twelve (12) treatments and two (2) replications. The results showed that the antibodies could detect WRD in various soils types. The serological detection was higher precisely than visual observation. The development of WRD mycelium varies depending on the soil types and it was different in the each estate area. In addition, this research is expected to get a serology kit to detect early symptoms of WRD in the rubber plants.
NASA Astrophysics Data System (ADS)
Ubaidillah; Imaduddin, Fitrian; Li, Yancheng; Amri Mazlan, Saiful; Sutrisno, Joko; Koga, Tsuyoshi; Yahya, Iwan; Choi, Seung-Bok
2016-11-01
This paper proposes a new type of magnetorheological elastomer (MRE) using rubber from waste tires and describes its performance characteristics. In this work, scrap tires were utilized as a primary matrix for the MRE without incorporation of virgin elastomers. The synthesis of the scrap tire based MRE adopted a high-temperature high-pressure sintering technique to achieve the reclaiming of vulcanized rubber. The material properties of the MRE samples were investigated through physical and viscoelastic examinations. The physical tests confirmed several material characteristics—microstructure, magnetic, and thermal properties-while the viscoelastic examination was conducted with a laboratory-made dynamic compression apparatus. It was observed from the viscoelastic examination that the proposed MRE has magnetic-field-dependent properties of the storage modulus, loss modulus, and loss tangent at different excitation frequencies and strain amplitudes. Specifically, the synthesized MRE showed a high zero field modulus, a reasonable MR effect under maximum applied current, and remarkable damping properties.
Laibach, Natalie; Hillebrand, Andrea; Twyman, Richard M; Prüfer, Dirk; Schulze Gronover, Christian
2015-05-01
Two protein families required for rubber biosynthesis in Taraxacum brevicorniculatum have recently been characterized, namely the cis-prenyltransferases (TbCPTs) and the small rubber particle proteins (TbSRPPs). The latter were shown to be the most abundant proteins on rubber particles, where rubber biosynthesis takes place. Here we identified a protein designated T. brevicorniculatum rubber elongation factor (TbREF) by using mass spectrometry to analyze rubber particle proteins. TbREF is homologous to the TbSRPPs but has a molecular mass that is atypical for the family. The promoter was shown to be active in laticifers, and the protein itself was localized on the rubber particle surface. In TbREF-silenced plants generated by RNA interference, the rubber content was significantly reduced, correlating with lower TbCPT protein levels and less TbCPT activity in the latex. However, the molecular mass of the rubber was not affected by TbREF silencing. The colloidal stability of rubber particles isolated from TbREF-silenced plants was also unchanged. This was not surprising because TbREF depletion did not affect the abundance of TbSRPPs, which are required for rubber particle stability. Our findings suggest that TbREF is an important component of the rubber biosynthesis machinery in T. brevicorniculatum, and may play a role in rubber particle biogenesis and influence rubber production. © 2015 The Authors The Plant Journal © 2015 John Wiley & Sons Ltd.
A non-affine micro-macro approach to strain-crystallizing rubber-like materials
NASA Astrophysics Data System (ADS)
Rastak, Reza; Linder, Christian
2018-02-01
Crystallization can occur in rubber materials at large strains due to a phenomenon called strain-induced crystallization. We propose a multi-scale polymer network model to capture this process in rubber-like materials. At the microscopic scale, we present a chain formulation by studying the thermodynamic behavior of a polymer chain and its crystallization mechanism inside a stretching polymer network. The chain model accounts for the thermodynamics of crystallization and presents a rate-dependent evolution law for crystallization based on the gradient of the free energy with respect to the crystallinity variables to ensures the dissipation is always non-negative. The multiscale framework allows the anisotropic crystallization of rubber which has been observed experimentally. Two different approaches for formulating the orientational distribution of crystallinity are studied. In the first approach, the algorithm tracks the crystallization at a finite number of orientations. In contrast, the continuous distribution describes the crystallization for all polymer chain orientations and describes its evolution with only a few distribution parameters. To connect the deformation of the micro with that of the macro scale, our model combines the recently developed maximal advance path constraint with the principal of minimum average free energy, resulting in a non-affine deformation model for polymer chains. Various aspects of the proposed model are validated by existing experimental results, including the stress response, crystallinity evolution during loading and unloading, crystallinity distribution, and the rotation of the principal crystallization direction. As a case study, we simulate the formation of crystalline regions around a pre-existing notch in a 3D rubber block and we compare the results with experimental data.
Identification of natural rubber and characterization of rubber biosynthetic activity in fig tree.
Kang, H; Kang, M Y; Han, K H
2000-07-01
Natural rubber was extracted from the fig tree (Ficus carica) cultivated in Korea as part of a survey of rubber producing plants. Fourier transform infrared and (13)C nuclear magnetic resonance analysis of samples prepared by successive extraction with acetone and benzene confirmed that the benzene-soluble residues are natural rubber, cis-1,4-polyisoprene. The rubber content in the latex of fig tree was about 4%, whereas the rubber content in the bark, leaf, and fruit was 0.3%, 0.1%, and 0.1%, respectively. Gel-permeation chromatography revealed that the molecular size of the natural rubber from fig tree is about 190 kD. Similar to rubber tree (Hevea brasiliensis) and guayule (Parthenium argentatum Gray), rubber biosynthesis in fig tree is tightly associated with rubber particles. The rubber transferase in rubber particles exhibited a higher affinity for farnesyl pyrophosphate than for isopentenyl pyrophosphate, with apparent K(m) values of 2.8 and 228 microM, respectively. Examination of latex serum from fig tree by sodium dodecyl sulfate-polyacrylamide gel electrophoresis revealed major proteins of 25 and 48 kD in size, and several proteins with molecular mass below 20 and above 100 kD. Partial N-terminal amino acid sequencing and immunochemical analyses revealed that the 25- and 48-kD proteins were novel and not related to any other suggested rubber transferases. The effect of EDTA and Mg(2+) ion on in vitro rubber biosynthesis in fig tree and rubber tree suggested that divalent metal ion present in the latex serum is an important factor in determining the different rubber biosynthetic activities in fig tree and rubber tree.
Identification of Natural Rubber and Characterization of Rubber Biosynthetic Activity in Fig Tree1
Kang, Hunseung; Kang, Min Young; Han, Kyung-Hwan
2000-01-01
Natural rubber was extracted from the fig tree (Ficus carica) cultivated in Korea as part of a survey of rubber producing plants. Fourier transform infrared and 13C nuclear magnetic resonance analysis of samples prepared by successive extraction with acetone and benzene confirmed that the benzene-soluble residues are natural rubber, cis-1,4-polyisoprene. The rubber content in the latex of fig tree was about 4%, whereas the rubber content in the bark, leaf, and fruit was 0.3%, 0.1%, and 0.1%, respectively. Gel-permeation chromatography revealed that the molecular size of the natural rubber from fig tree is about 190 kD. Similar to rubber tree (Hevea brasiliensis) and guayule (Parthenium argentatum Gray), rubber biosynthesis in fig tree is tightly associated with rubber particles. The rubber transferase in rubber particles exhibited a higher affinity for farnesyl pyrophosphate than for isopentenyl pyrophosphate, with apparent Km values of 2.8 and 228 μm, respectively. Examination of latex serum from fig tree by sodium dodecyl sulfate-polyacrylamide gel electrophoresis revealed major proteins of 25 and 48 kD in size, and several proteins with molecular mass below 20 and above 100 kD. Partial N-terminal amino acid sequencing and immunochemical analyses revealed that the 25- and 48-kD proteins were novel and not related to any other suggested rubber transferases. The effect of EDTA and Mg2+ ion on in vitro rubber biosynthesis in fig tree and rubber tree suggested that divalent metal ion present in the latex serum is an important factor in determining the different rubber biosynthetic activities in fig tree and rubber tree. PMID:10889262
NASA Astrophysics Data System (ADS)
Ismail, R.; Ibrahim, A.; Rusop, M.; Adnan, A.
2018-05-01
The present article compares the mechanical properties of natural rubber (NR) and carbon nanotubes (CNTs) filled natural rubber composites. Four types of nanocomposite specimens are fabricated with different MWCNT loadings: 0 wt% (pure natural rubber), 1 wt%, 3 wt%, and 5 wt%. The specimens are tested for their mechanical properties. It is observed that the tensile strength, hardness and elongation break of CNTs filled rubber composites are remarkably higher than that of raw rubber indicating the inherent reinforcing potential of CNTs. Percentage of the elongation at break of rubber CNTs composites is lower than that of raw rubber.
Mechanical Performance Test of Rubber-Powder Modified Concrete
NASA Astrophysics Data System (ADS)
Zhang, Yan Cong; Gao, Ling Ling
2018-06-01
A number of rubber cement concrete specimens that rubber powder dosage different were obtained using same cement, water and fine aggregates, by adjusting the dosage of rubber powder. Then it was used to research the influence of rubber powder dosage on performance of cement concrete by measuring its liquidity, strength and toughness. The results show that: when water-cement ratio was equal and rubber powder replacing the same volume sand, the fluidity of cement concrete almost linear increased with rubber powder dosage increasing. With dosage of rubber powder increasing, compressive strength and flexural strength reduced, but toughness linear growth trend when dosage of rubber powder less 30%.
40 CFR 428.20 - Applicability; description of the emulsion crumb rubber subcategory.
Code of Federal Regulations, 2013 CFR
2013-07-01
... emulsion crumb rubber subcategory. 428.20 Section 428.20 Protection of Environment ENVIRONMENTAL PROTECTION... CATEGORY Emulsion Crumb Rubber Subcategory § 428.20 Applicability; description of the emulsion crumb rubber... manufacture of emulsion crumb rubber, other than acrylonitrilebutadiene rubber. [40 FR 18173, Apr. 25, 1975] ...
40 CFR 428.20 - Applicability; description of the emulsion crumb rubber subcategory.
Code of Federal Regulations, 2012 CFR
2012-07-01
... emulsion crumb rubber subcategory. 428.20 Section 428.20 Protection of Environment ENVIRONMENTAL PROTECTION... CATEGORY Emulsion Crumb Rubber Subcategory § 428.20 Applicability; description of the emulsion crumb rubber... manufacture of emulsion crumb rubber, other than acrylonitrilebutadiene rubber. [40 FR 18173, Apr. 25, 1975] ...
40 CFR 428.20 - Applicability; description of the emulsion crumb rubber subcategory.
Code of Federal Regulations, 2014 CFR
2014-07-01
... emulsion crumb rubber subcategory. 428.20 Section 428.20 Protection of Environment ENVIRONMENTAL PROTECTION... CATEGORY Emulsion Crumb Rubber Subcategory § 428.20 Applicability; description of the emulsion crumb rubber... manufacture of emulsion crumb rubber, other than acrylonitrilebutadiene rubber. [40 FR 18173, Apr. 25, 1975] ...
Zhang, Tao; Cai, Guojun; Duan, Weihong
2018-02-01
The disposal of scrap rubber tires has induced critical environmental issue worldwide due to the rapid increase in the number of vehicles. Recycled scrap tires as a construction material in civil engineering have significant environmental benefits from a waste management perspective. A systematic study that deals with strength and microstructure characteristics of the rubber-sand mixtures is initiated, and mechanical response of the mixtures is discussed in this investigation. Experiments were conducted to evaluate the effects of rubber fraction on the basic properties including mass density (ρ), stress-strain characteristics, shear strength, and unconfined compression strength (q u ) of the rubber-sand mixtures. Additionally, scanning electron microscopy (SEM) was carried out to reveal the microstructure characteristics of the mixtures with various rubber fractions. A discussion on the micromechanics of the mixtures also was conducted. This study demonstrates that the ρ, friction angle, and q u decrease linearly with an increase in rubber fraction, whereas shear strain at peak increases. The stress-strain characteristics of the rubber-sand mixtures shift from brittle to ductile as the rubber fraction increase. These changes are attributed to remarkably lower stiffness and higher compressibility of the rubber particle compared with those of the conventional mineral aggregates. With an increase in the rubber fraction, the mechanical response of rubber-sand mixtures exhibits two types: sand-like material and rubber-like material. Rubber particle possesses the capacity to prevent the contacted sand particles from sliding at lower rubber fraction, whereas it transmits the applied loadings as the rubber fraction increased. This outcome reinforces the practicability of using recycled rubber tire-sand mixtures as a lightweight backfill in subbase/base applications.
Experimental Investigation of the Mechanical and Durability Properties of Crumb Rubber Concrete.
Liu, Hanbing; Wang, Xianqiang; Jiao, Yubo; Sha, Tao
2016-03-07
Recycling waste tire rubber by incorporating it into concrete has become the preferred solution to dispose of waste tires. In this study, the effect of the volume content of crumb rubber and pretreatment methods on the performances of concrete was evaluated. Firstly, the fine aggregate and mixture were partly replaced by crumb rubber to produce crumb rubber concrete. Secondly, the mechanical and durability properties of crumb rubber concrete with different replacement forms and volume contents had been investigated. Finally, the crumb rubber after pretreatment by six modifiers was introduced into the concrete mixture. Corresponding tests were conducted to verify the effectiveness of pretreatment methods as compared to the concrete containing untreated crumb rubber. It was observed that the mechanical strength of crumb rubber concrete was reduced, while durability was improved with the increasing of crumb rubber content. 20% replacement of fine aggregate and 5% replacement of the total mixture exhibited acceptable properties for practical applications. In addition, the results indicated that the modifiers had a positive impact on the mechanical and durability properties of crumb rubber concrete. It avoided the disadvantage of crumb rubber concrete having lower strength and provides a reference for the production of modified crumb rubber concrete.
Experimental Investigation of the Mechanical and Durability Properties of Crumb Rubber Concrete
Liu, Hanbing; Wang, Xianqiang; Jiao, Yubo; Sha, Tao
2016-01-01
Recycling waste tire rubber by incorporating it into concrete has become the preferred solution to dispose of waste tires. In this study, the effect of the volume content of crumb rubber and pretreatment methods on the performances of concrete was evaluated. Firstly, the fine aggregate and mixture were partly replaced by crumb rubber to produce crumb rubber concrete. Secondly, the mechanical and durability properties of crumb rubber concrete with different replacement forms and volume contents had been investigated. Finally, the crumb rubber after pretreatment by six modifiers was introduced into the concrete mixture. Corresponding tests were conducted to verify the effectiveness of pretreatment methods as compared to the concrete containing untreated crumb rubber. It was observed that the mechanical strength of crumb rubber concrete was reduced, while durability was improved with the increasing of crumb rubber content. 20% replacement of fine aggregate and 5% replacement of the total mixture exhibited acceptable properties for practical applications. In addition, the results indicated that the modifiers had a positive impact on the mechanical and durability properties of crumb rubber concrete. It avoided the disadvantage of crumb rubber concrete having lower strength and provides a reference for the production of modified crumb rubber concrete. PMID:28773298
Chakrabarty, Romit; Qu, Yang; Ro, Dae-Kyun
2015-05-01
Natural rubber, cis-1,4-polyisoprene, is an important raw material in chemical industries, but its biosynthetic mechanism remains elusive. Natural rubber is known to be synthesized in rubber particles suspended in laticifer cells in the Brazilian rubber tree (Hevea brasiliensis). In the rubber tree, rubber elongation factor (REF) and its homolog, small rubber particle protein (SRPP), were found to be the most abundant proteins in rubber particles, and they have been implicated in natural rubber biosynthesis. As lettuce (Lactuca sativa) can synthesize natural rubber, we utilized this annual, transformable plant to examine in planta roles of the lettuce REF/SRPP homologs by RNA interference. Among eight lettuce REF/SRPP homologs identified, transcripts of two genes (LsSRPP4 and LsSRPP8) accounted for more than 90% of total transcripts of REF/SRPP homologs in lettuce latex. LsSRPP4 displays a typical primary protein sequence as other REF/SRPP, while LsSRPP8 is twice as long as LsSRPP4. These two major LsSRPP transcripts were individually and simultaneously silenced by RNA interference, and relative abundance, polymer molecular weight, and polydispersity of natural rubber were analyzed from the LsSRPP4- and LsSRPP8-silenced transgenic lettuce. Despite previous data suggesting the implications of REF/SRPP in natural rubber biosynthesis, qualitative and quantitative alterations of natural rubber could not be observed in transgenic lettuce lines. It is concluded that lettuce REF/SRPP homologs are not critically important proteins in natural rubber biosynthesis in lettuce. Copyright © 2014 Elsevier Ltd. All rights reserved.
Code of Federal Regulations, 2010 CFR
2010-07-01
... RUBBER MANUFACTURING POINT SOURCE CATEGORY Small-Sized General Molded, Extruded, and Fabricated Rubber..., foam rubber backing, rubber cement-dipped goods, and retreaded tires by small-sized plants...
Code of Federal Regulations, 2010 CFR
2010-07-01
... RUBBER MANUFACTURING POINT SOURCE CATEGORY Large-Sized General Molded, Extruded, and Fabricated Rubber..., foam rubber backing, rubber cement-dipped goods, and retreaded tires by large-sized plants...
Characterization and Application of Passive Samplers for Monitoring of Pesticides in Water.
Ahrens, Lutz; Daneshvar, Atlasi; Lau, Anna E; Kreuger, Jenny
2016-08-03
Five different water passive samplers were calibrated under laboratory conditions for measurement of 124 legacy and current used pesticides. This study provides a protocol for the passive sampler preparation, calibration, extraction method and instrumental analysis. Sampling rates (RS) and passive sampler-water partition coefficients (KPW) were calculated for silicone rubber, polar organic chemical integrative sampler POCIS-A, POCIS-B, SDB-RPS and C18 disk. The uptake of the selected compounds depended on their physicochemical properties, i.e., silicone rubber showed a better uptake for more hydrophobic compounds (log octanol-water partition coefficient (KOW) > 5.3), whereas POCIS-A, POCIS-B and SDB-RPS disk were more suitable for hydrophilic compounds (log KOW < 0.70).
Criteria for asphalt-rubber concrete in civil airport pavements: Mixture design
NASA Astrophysics Data System (ADS)
Roberts, F. L.; Lytton, R. L.; Hoyt, D.
1986-07-01
A mixture design procedure is developed to allow the use of asphalt-rubber binders in concrete for flexible airport pavement. The asphalt-rubber is produced by reacting asphalt with ground, scrap tire rubber to produce the binder for the asphalt-rubber concrete. Procedures for laboratory preparation of alsphalt-rubber binders using an equipment setup that was found by researchers to produce laboratory binders with similar properties to field processes are included. The rubber-asphalt concrete mixture design procedure includes adjustments to the aggregate gradation to permit space for the rubber particles in the asphalt-rubber binder as well as suggested mixing and compaction temperatures, and compaction efforts. While the procedure was used in the laboratory to successfully produce asphalt-rubber concrete mixtures, it should be evaluated in the field to ensure that consistent results can be achieved in a production environment.
DOE Office of Scientific and Technical Information (OSTI.GOV)
Hossain, M.; Funk, L.P.; Sadeq, M.A.
1995-06-01
The major objective of this project was to formulate a Chunk Rubber Asphalt Concrete (CRAC) mix for use on low volume roads. CRAC is a rubber modified asphalt concrete product produced by the `dry process` where rubber chunks of 1/2 inch size are used as aggregate in a cold mix with a type C fly ash. The second objective of this project was to develop guidelines concerning the use of rubber modified asphalt concrete hot mix to include: (1) Design methods for use of asphalt-rubber mix for new construction and overlay, (2) Mix design method for asphalt-rubber, and (3) Testmore » method for determining the amount of rubber in an asphalt-rubber concrete for quality control purposes.« less
Microwave treatment of vulcanized rubber
Wicks, George G [Aiken, SC; Schulz, Rebecca L [Aiken, SC; Clark, David E [Gainesville, FL; Folz, Diane C [Gainesville, FL
2002-07-16
A process and resulting product is provided in which a vulcanized solid particulate, such as vulcanized crumb rubber, has select chemical bonds broken by microwave radiation. The direct application of microwaves in combination with uniform heating of the crumb rubber renders the treated crumb rubber more suitable for use in new rubber formulations. As a result, larger particle sizes and/or loading levels of the treated crumb rubber can be used in new rubber mixtures to produce recycled composite products with good properties.
Pochron, Sharon; Nikakis, Jacqueline; Illuzzi, Kyra; Baatz, Andrea; Demirciyan, Loriana; Dhillon, Amritjot; Gaylor, Thomas; Manganaro, Alexa; Maritato, Nicholas; Moawad, Michael; Singh, Rajwinder; Tucker, Clara; Vaughan, Daniel
2018-04-01
Solid waste management struggles with the sustainable disposal of used tires. One solution involves shredding used tires into crumb rubber and using the material as infill for artificial turf. However, crumb rubber contains hydrocarbons, organic compounds, and heavy metals, and it travels into the environment. Earthworms living in soil contaminated with virgin crumb rubber gained 14% less body weight than did earthworms living in uncontaminated soil, but the impact of aged crumb rubber on the earthworms is unknown. Since many athletic fields contain aged crumb rubber, we compared the body weight, survivorship, and longevity in heat and light stress for earthworms living in clean topsoil to those living in topsoil contaminated with aged crumb rubber. We also characterized levels of metals, nutrients, and micronutrients of both soil treatments and compared those to published values for soil contaminated with virgin crumb rubber. Consistent with earlier research, we found that contaminated soil did not inhibit microbial respiration rates. Aged crumb rubber, like new crumb rubber, had high levels of zinc. However, while exposure to aged crumb rubber did not reduce earthworm body weight as did exposure to new crumb rubber, exposure to aged crumb rubber reduced earthworm survival time during a stress test by a statistically significant 38 min (16.2%) relative to the survival time for worms that had lived in clean soil. Aged crumb rubber and new crumb rubber appear to pose similar toxic risks to earthworms. This study suggests an environmental cost associated with the current tire-recycling solution.
Nonaqueous ozonation of vulcanized rubber
Serkiz, Steven M.
1999-01-01
A process and resulting product is provided in which a solid particulate, such as vulcanized crumb rubber, has the surface functional groups oxidized by ozonation using a nonpolar solvent. The ozonation process renders the treated crumb rubber more suitable for use in new rubber formulations. As a result, larger loading levels of the treated crumb rubber can be used in new rubber mixtures.
Roy, Ram Vinod; Das, Mithu; Banerjee, Rintu; Bhowmick, Anil K
2006-12-01
A comparative study on biodegradation of di-cumyl peroxide (DCP) crosslinked and uncrosslinked natural rubber by Pseudomonas sp. was carried out. Decrease in organic carbon content along with the changes in tensile strength of the treated rubber, both DCP crosslinked and uncrosslinked natural rubber, indicated rubber hydrocarbon utilization by the Pseudomonas sp. A decrease in 60.88% MPa and 41.66% MPa was observed after five month's old treated uncrosslinked natural rubber and DCP crosslinked rubber, respectively. Biodegradation was more pronounced in natural uncrosslinked rubber, which was further confirmed by the formation of aldehydic compounds with decrease in CH2 stretching frequencies.
Effect of superhydrophobicity on surface damage of silicone rubber under AC voltage
NASA Astrophysics Data System (ADS)
Li, Yufeng; Jin, Haiyun; Nie, Shichao; Tong, Cheng; Gao, Naikui
2018-03-01
In this paper, the influence of superhydrophobicity on the surface damage of silicone rubber is studied. On a common silicone rubber surface, a droplet can become elongated, and arc discharge induced by the droplet can cause tracking on the silicone rubber surface. However, for a superhydrophobic silicone rubber surface, a droplet can leave the silicone rubber due to the low adhesion of the superhydrophobic surface. Accordingly, arc discharge caused by the droplet does not occur, and the surface of the silicone rubber is not affected. Results demonstrate that using a superhydrophobic surface has a significant effect on limiting the surface damage of silicone rubber.
Guterstam, Arvid; Zeberg, Hugo; Özçiftci, Vedat Menderes; Ehrsson, H Henrik
2016-10-01
To accurately localize our limbs and guide movements toward external objects, the brain must represent the body and its surrounding (peripersonal) visual space. Specific multisensory neurons encode peripersonal space in the monkey brain, and neurobehavioral studies have suggested the existence of a similar representation in humans. However, because peripersonal space lacks a distinct perceptual correlate, its involvement in spatial and bodily perception remains unclear. Here, we show that applying brushstrokes in mid-air at some distance above a rubber hand-without touching it-in synchrony with brushstrokes applied to a participant's hidden real hand results in the illusory sensation of a "magnetic force" between the brush and the rubber hand, which strongly correlates with the perception of the rubber hand as one's own. In eight experiments, we characterized this "magnetic touch illusion" by using quantitative subjective reports, motion tracking, and behavioral data consisting of pointing errors toward the rubber hand in an intermanual pointing task. We found that the illusion depends on visuo-tactile synchrony and exhibits similarities with the visuo-tactile receptive field properties of peripersonal space neurons, featuring a non-linear decay at 40cm that is independent of gaze direction and follows changes in the rubber hand position. Moreover, the "magnetic force" does not penetrate physical barriers, thus further linking this phenomenon to body-specific visuo-tactile integration processes. These findings provide strong support for the notion that multisensory integration within peripersonal space underlies bodily self-attribution. Furthermore, we propose that the magnetic touch illusion constitutes a perceptual correlate of visuo-tactile integration in peripersonal space. Copyright © 2016 The Author(s). Published by Elsevier B.V. All rights reserved.
Advances in rubber/halloysite nanotubes nanocomposites.
Jia, Zhixin; Guo, Baochun; Jia, Demin
2014-02-01
The research advances in rubber/halloysite nanotubes (rubber/HNTs) nanocomposites are reviewed. HNTs are environmentally-friendly natural nanomaterials, which could be used to prepare the rubber-based nanocomposites with high performance and low cost. Unmodified HNTs could be adopted to prepare the rubber/HNTs composites with improved mechanical properties, however, the rubber/HNTs nanocomposites with fine morphology and excellent properties were chiefly prepared with various modifiers by in situ mixing method. A series of rubber/HNTs nanocomposites containing several rubbers (SBR, NR, xSBR, NBR, PU) and different modifiers (ENR, RH, Si69, SA, MAA, ILs) have been investigated. The results showed that all the rubber/HNTs nanocomposites achieved strong interfacial interaction via interfacial covalent bonds, hydrogen bonds or multiple interactions, realized significantly improved dispersion of HNTs at nanoscale and exhibited excellent mechanical performances and other properties.
Roofing Materials Assessment: Investigation of Five Metals in Runoff from Roofing Materials.
Winters, Nancy; Granuke, Kyle; McCall, Melissa
2015-09-01
To assess the contribution of five toxic metals from new roofing materials to stormwater, runoff was collected from 14 types of roofing materials and controls during 20 rain events and analyzed for metals. Many of the new roofing materials evaluated did not show elevated metals concentrations in the runoff. Runoff from several other roofing materials was significantly higher than the controls for arsenic, copper, and zinc. Notably, treated wood shakes released arsenic and copper, copper roofing released copper, PVC roofing released arsenic, and Zincalume® and EPDM roofing released zinc. For the runoff from some of the roofing materials, metals concentrations decreased significantly over an approximately one-year period of aging. Metals concentrations in runoff were demonstrated to depend on a number of factors, such as roofing materials, age of the materials, and climatic conditions. Thus, application of runoff concentrations from roofing materials to estimate basin-wide releases should be undertaken cautiously.
Collins-Silva, Jillian; Nural, Aise Taban; Skaggs, Amanda; Scott, Deborah; Hathwaik, Upul; Woolsey, Rebekah; Schegg, Kathleen; McMahan, Colleen; Whalen, Maureen; Cornish, Katrina; Shintani, David
2012-07-01
Several proteins have been identified and implicated in natural rubber biosynthesis, one of which, the small rubber particle protein (SRPP), was originally identified in Hevea brasiliensis as an abundant protein associated with cytosolic vesicles known as rubber particles. While previous in vitro studies suggest that SRPP plays a role in rubber biosynthesis, in vivo evidence is lacking to support this hypothesis. To address this issue, a transgene approach was taken in Taraxacum kok-saghyz (Russian dandelion or Tk) to determine if altered SRPP levels would influence rubber biosynthesis. Three dandelion SRPPs were found to be highly abundant on dandelion rubber particles. The most abundant particle associated SRPP, TkSRPP3, showed temporal and spatial patterns of expression consistent with patterns of natural rubber accumulation in dandelion. To confirm its role in rubber biosynthesis, TkSRPP3 expression was altered in Russian dandelion using over-expression and RNAi methods. While TkSRPP3 over-expressing lines had slightly higher levels of rubber in their roots, relative to the control, TkSRPP3 RNAi lines showed significant decreases in root rubber content and produced dramatically lower molecular weight rubber than the control line. Not only do results here provide in vivo evidence of TkSRPP proteins affecting the amount of rubber in dandelion root, but they also suggest a function in regulating the molecular weight of the cis-1, 4-polyisoprene polymer. Copyright © 2012 Elsevier Ltd. All rights reserved.
Ionic charge accumulation at microscopic interfaces in filled composites
DOE Office of Scientific and Technical Information (OSTI.GOV)
Zhu Yutao; Wang Xinheng; Xie Hengkun
1996-12-31
In this paper the charge accumulation process at microscopic interfaces in insulating materials filled with inorganic fillers is analyzed by using a unit model. Dynamic equations of interfacial ionic charge accumulation are proposed by the authors. The charge accumulation and its regulations are proved by TSC test results obtained on silica filled EPDM samples.
Duranty, Edward R; Roosendaal, Timothy J; Pitman, Stan G; Tucker, Joseph C; Owsley, Stanley L; Suter, Jonathan D; Alvine, Kyle James
2018-03-31
High pressure hydrogen gas is known to adversely affect metallic components of compressors, valves, hoses, and actuators. However, relatively little is known about the effects of high pressure hydrogen on the polymer sealing and barrier materials also found within these components. More study is required in order to determine the compatibility of common polymer materials found in the components of the hydrogen fuel delivery infrastructure with high pressure hydrogen. As a result, it is important to consider the changes in physical properties such as friction and wear in situ while the polymer is exposed to high pressure hydrogen. In this protocol, we present a method for testing the friction and wear properties of ethylene propylene diene monomer (EPDM) elastomer samples in a 28 MPa high pressure hydrogen environment using a custom-built in situ pin-on-flat linear reciprocating tribometer. Representative results from this testing are presented which indicate that the coefficient of friction between the EPDM sample coupon and steel counter surface is increased in high pressure hydrogen as compared to the coefficient of friction similarly measured in ambient air.
Electrospinning of PVC with natural rubber
NASA Astrophysics Data System (ADS)
Othman, Muhammad Hariz; Mohamed, Mahathir; Abdullah, Ibrahim
2013-11-01
Polyvinyl chloride (PVC) was mixed with natural rubbers which are liquid natural rubber (LNR), liquid epoxidised natural rubber (LENR) and liquid epoxidised natural rubber acrylate (LENRA) for a preparation of a fine non-woven fiber's mat. PVC and each natural rubbers(PVC:LENR, PVC:LNR and PVC:LENRA) were mixed based on ratio of 70:30. Electrospinning method was used to prepare the fiber. The results show that the spinnable concentration of PVC/ natural rubber/THF solution is 16 wt%. The morphology, diameter, structure and degradation temperature of electrospun fibers were investigated by scanning electron microscopy (SEM) and thermogravimetric analysis (TGA). SEM photos showed that the morphology and diameter of the fibers were mainly affected by the addition of natural rubber. TGA results suggested that PVC electrospun fiber has higher degradation temperature than those electrospun fibers that contain natural rubber.
40 CFR 428.20 - Applicability; description of the emulsion crumb rubber subcategory.
Code of Federal Regulations, 2010 CFR
2010-07-01
... emulsion crumb rubber subcategory. 428.20 Section 428.20 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY (CONTINUED) EFFLUENT GUIDELINES AND STANDARDS RUBBER MANUFACTURING POINT SOURCE CATEGORY Emulsion Crumb Rubber Subcategory § 428.20 Applicability; description of the emulsion crumb rubber subcategory...
40 CFR 428.20 - Applicability; description of the emulsion crumb rubber subcategory.
Code of Federal Regulations, 2011 CFR
2011-07-01
... emulsion crumb rubber subcategory. 428.20 Section 428.20 Protection of Environment ENVIRONMENTAL PROTECTION AGENCY (CONTINUED) EFFLUENT GUIDELINES AND STANDARDS RUBBER MANUFACTURING POINT SOURCE CATEGORY Emulsion Crumb Rubber Subcategory § 428.20 Applicability; description of the emulsion crumb rubber subcategory...
21 CFR 177.1480 - Nitrile rubber modified acrylonitrile-methyl acrylate copolymers.
Code of Federal Regulations, 2010 CFR
2010-04-01
... 21 Food and Drugs 3 2010-04-01 2009-04-01 true Nitrile rubber modified acrylonitrile-methyl... Nitrile rubber modified acrylonitrile-methyl acrylate copolymers. Nitrile rubber modified acrylonitrile... rubber modified acrylonitrile-methyl acrylate copolymers consist of basic copolymers produced by the...
Effect of non-rubber constituents on Guayule and Hevea rubber intrinsic properties
USDA-ARS?s Scientific Manuscript database
To meet the increasing demand for natural rubber (NR), currently sourced from the tropical rubber tree Hevea brasiliensis, and address price volatility and steadily increasing labor costs, alternate rubber-producing species are in commercial development. One of these, guayule (Parthenium argentatum)...
NASA Astrophysics Data System (ADS)
Jin, Kailong; Li, Lingqiao; Torkelson, John
Rubber tires illustrate well the issues ranging from economic loss to environmental problems and sustainability issues that arise with spent, covalently crosslinked polymers. A nitroxide-mediated polymerization (NMP) strategy has been developed that allows for one-step synthesis of recyclable crosslinked polymers from monomers or polymers that contain carbon-carbon double bonds amenable to radical polymerization. Resulting materials possess dynamic alkoxyamine crosslinks that undergo reversible decrosslinking as a function of temperature. Using polybutadiene as starting material, and styrene, an appropriate nitroxide molecule and bifunctional initiator for initial crosslinking, a model for tire rubber can be produced by reaction at temperatures comparable to those employed in tire molding. Upon cooling, the crosslinks are made permanent due to the extraordinarily strong temperature dependence of the reverisible nitroxide capping and uncapping reaction. Based on thermomechanical property characterization, when the original crosslinked model rubber is chopped into bits and remolded in the melt state, a well-consolidated material is obtained which exhibits full recovery of properties reflecting crosslink density after multiple recycling steps.
Single Stage Silicone Border Molded Closed Mouth Impression Technique-Part II.
Solomon, E G R
2011-09-01
Functioning of a complete denture depends to a great extent on the impression technique. Several impression techniques have been described in the literature since the turn of this century when Greene [Clinical courses in dental prothesis, 1916] brothers introduced the first scientific system of recording dental impression. Advocates of each technique have their own claim of superiority over the other. The introduction of elastomeric impression materials [Skinner and Cooper, J Am Dent Assoc 51:523-536, 1955] has made possible new techniques of recording impression for complete denture construction. These rubber like materials are of two types; one has a polysulfide base and is popularily known as polysulfide rubber (Thiokol and Mercaptan). The other variety has a silicone base known as silicone rubber or silicone elastomer. Silicone elastomers are available in four different consistencies; a thin easy flowing light bodied material,a creamy medium bodied material, a highly viscous heavy bodied material and a kneadable putty material. This paper describes an active closed mouth impression technique with one stage border molding using putty silicone material as a substitute for low fusing compound.
Evaluation of peptides release using a natural rubber latex biomembrane as a carrier.
Miranda, M C R; Borges, F A; Barros, N R; Santos Filho, N A; Mendonça, R J; Herculano, R D; Cilli, E M
2018-05-01
The biomembrane natural (NRL-Natural Rubber Latex), manipulated from the latex obtained from the rubber tree Hevea brasiliensis, has shown great potential for application in biomedicine and biomaterials. Reflecting the biocompatibility and low bounce rate of this material, NRL has been used as a physical barrier to infectious agents and for the controlled release of drugs and extracts. The aim of the present study was to evaluate the incorporation and release of peptides using a latex biomembrane carrier. After incorporation, the release of material from the membrane was observed using spectrophotometry. Analyses using HPLC and mass spectroscopy did not confirm the release of the antimicrobial peptide [W 6 ]Hylin a1 after 24 h. In addition, analysis of the release solution showed new compounds, indicating the degradation of the peptide by enzymes contained in the latex. Additionally, the release of a peptide with a shorter sequence (Ac-WAAAA) was evaluated, and degradation was not observed. These results showed that the use of NRL as solid matrices as delivery systems of peptide are sequence dependent and could to be evaluated for each sequence.
Mechanical Behavior and Fatigue Studies of Rubber Components Used in Tracked Vehicles
2010-08-17
durability to this elastomers and polybutadiene is rubber , which gives rubber -like properties. SBR has good abrasion resistance and good aging ...SIMULATION, TESTING AND VALIDATION (MSTV) MINI-SYMPOSIUM AUGUST 17-19 DEARBORN, MICHIGAN MECHANICAL BEHAVIOR AND FATIGUE STUDIES OF RUBBER COMPONENTS USED...Analytics Group US Army TARDEC Warren, MI ABSTRACT In this study, a styrene butadiene rubber , which is similar to the rubber used in road wheel
Reinforcement effect of soy protein nanoparticles in amine-modified natural rubber latex
USDA-ARS?s Scientific Manuscript database
Mechanical properties of natural rubber reinforced with soy protein nanoparticles are useful for various rubber applications. However, the properties is further improved by improving interactions between soy protein and rubber. A novel method is used to modify particle surface of natural rubber late...
USDA-ARS?s Scientific Manuscript database
Blends of styrene-butadiene rubber and natural rubber that provide balanced properties were modified with acrylamide and reinforced with soy protein particles. The rubber composites show improved mechanical properties. Both modified rubber and composites showed a faster curing rate. The crosslinking...
Method for the addition of vulcanized waste rubber to virgin rubber products
Romine, Robert A.; Snowden-Swan, Lesley J.
1997-01-01
The invention is a method of using enzymes from thiophyllic microbes for selectively breaking the sulfur rubber cross-link bonds in vulcanized rubber. The process is halted at the sulfoxide or sulfone step so that a devulcanized layer is reactive with virgin rubber.
Rubber dam isolation for restorative treatment in dental patients.
Wang, Yan; Li, Chunjie; Yuan, He; Wong, May Cm; Zou, Jing; Shi, Zongdao; Zhou, Xuedong
2016-09-20
Successful restorations in dental patients depend largely on the effective control of moisture and microbes during the procedure. The rubber dam technique has been one of the most widely used isolation methods in dental restorative treatments. The evidence on the effects of rubber dam usage on the longevity of dental restorations is conflicting. Therefore, it is important to summarise the available evidence to determine the effects of this method. To assess the effects of rubber dam isolation compared with other types of isolation used for direct and indirect restorative treatments in dental patients. We searched the following electronic databases: Cochrane Oral Health's Trials Register (searched 17 August 2016), Cochrane Central Register of Controlled Trials (CENTRAL; 2016, Issue 7) in the Cochrane Library (searched 17 August 2016), MEDLINE Ovid (1946 to 17 August 2016), Embase Ovid (1980 to 17 August 2016), LILACS BIREME Virtual Health Library (Latin American and Caribbean Health Science Information database; 1982 to 17 August 2016), SciELO BIREME Virtual Health Library (1998 to 17 August 2016), Chinese BioMedical Literature Database (CBM, in Chinese) (1978 to 30 August 2016), VIP (in Chinese) (1989 to 30 August 2016), and China National Knowledge Infrastructure (CNKI, in Chinese) (1994 to 30 August 2016). We searched ClinicalTrials.gov and the World Health Organization International Clinical Trials Registry Platform, OpenGrey and Sciencepaper Online (in Chinese) for ongoing trials. There were no restrictions on the language or date of publication when searching the electronic databases. We included randomised controlled trials (including split-mouth trials) assessing the effects of rubber dam isolation for restorative treatments in dental patients. Two review authors independently screened the results of the electronic searches, extracted data and assessed the risk of bias of the included studies. We resolved disagreement by discussion. We included four studies that analysed 1270 participants (among which 233 participants were lost to follow-up). All the included studies were at high risk of bias. We excluded one trial from the analysis due to inconsistencies in the presented data.The results indicated that dental restorations had a significantly higher survival rate in the rubber dam isolation group compared to the cotton roll isolation group at six months in participants receiving composite restorative treatment of non-carious cervical lesions (risk ratio (RR) 1.19, 95% confidence interval (CI) 1.04 to 1.37, very low-quality evidence). It also showed that the rubber dam group had a lower risk of failure at two years in children undergoing proximal atraumatic restorative treatment in primary molars (hazard ratio (HR) 0.80, 95% CI 0.66 to 0.97, very low-quality evidence). One trial reported limited data showing that rubber dam usage during fissure sealing might shorten the treatment time. None of the included studies mentioned adverse effects or reported the direct cost of the treatment, or the level of patient acceptance/satisfaction. There was also no evidence evaluating the effects of rubber dam usage on the quality of the restorations. We found some very low-quality evidence, from single studies, suggesting that rubber dam usage in dental direct restorative treatments may lead to a lower failure rate of the restorations, compared with the failure rate for cotton roll usage. Further high quality research evaluating the effects of rubber dam usage on different types of restorative treatments is required.
Method for the addition of vulcanized waste rubber to virgin rubber products
Romine, R.A.; Snowden-Swan, L.J.
1997-01-28
The invention is a method of using enzymes from thiophyllic microbes for selectively breaking the sulfur rubber cross-link bonds in vulcanized rubber. The process is halted at the sulfoxide or sulfone step so that a devulcanized layer is reactive with virgin rubber. 8 figs.
USDA-ARS?s Scientific Manuscript database
Natural rubber (cis-1,4-polyisoprene) is an essential plant derived commodity required for the manufacture of numerous industrial, medical and household items. Rubber is synthesized and sequestered on cytsolic vesicles known as rubber particles. When provided with farnesyl pyrophosphate (FPP) and is...
Electrospinning of PVC with natural rubber
DOE Office of Scientific and Technical Information (OSTI.GOV)
Othman, Muhammad Hariz; Abdullah, Ibrahim; Mohamed, Mahathir
Polyvinyl chloride (PVC) was mixed with natural rubbers which are liquid natural rubber (LNR), liquid epoxidised natural rubber (LENR) and liquid epoxidised natural rubber acrylate (LENRA) for a preparation of a fine non-woven fiber’s mat. PVC and each natural rubbers(PVC:LENR, PVC:LNR and PVC:LENRA) were mixed based on ratio of 70:30. Electrospinning method was used to prepare the fiber. The results show that the spinnable concentration of PVC/ natural rubber/THF solution is 16 wt%. The morphology, diameter, structure and degradation temperature of electrospun fibers were investigated by scanning electron microscopy (SEM) and thermogravimetric analysis (TGA). SEM photos showed that the morphologymore » and diameter of the fibers were mainly affected by the addition of natural rubber. TGA results suggested that PVC electrospun fiber has higher degradation temperature than those electrospun fibers that contain natural rubber.« less
Microbial detoxification of waste rubber material by wood-rotting fungi.
Bredberg, Katarina; Andersson, B Erik; Landfors, Eva; Holst, Olle
2002-07-01
The extensive use of rubber products, mainly tires, and the difficulties to recycle those products, has resulted in world wide environmental problems. Microbial devulcanisation is a promising way to increase the recycling of rubber materials. One obstacle is that several microorganisms tested for devulcanisation are sensitive to rubber additives. A way to overcome this might be to detoxify the rubber material with fungi prior to the devulcanisation. In this study, 15 species of white-rot and brown-rot fungi have been screened with regard to their capacity to degrade an aromatic model compound in the presence of ground waste tire rubber. The most effective fungus, Resinicium bicolor, was used for detoxification of rubber material. Increase in growth of the desulfurising bacterium Thiobacillus ferrooxidans in presence of the rubber treated with Resinicium bicolor compared to untreated rubber demonstrated that detoxification with fungi is possible.
Effects of forests, roads and mistletoe on bird diversity in monoculture rubber plantations
NASA Astrophysics Data System (ADS)
Sreekar, Rachakonda; Huang, Guohualing; Yasuda, Mika; Quan, Rui-Chang; Goodale, Eben; Corlett, Richard T.; Tomlinson, Kyle W.
2016-02-01
Rising global demand for natural rubber is expanding monoculture rubber (Hevea brasilensis) at the expense of natural forests in the Old World tropics. Conversion of forests into rubber plantations has a devastating impact on biodiversity and we have yet to identify management strategies that can mitigate this. We determined the life-history traits that best predict bird species occurrence in rubber plantations in SW China and investigated the effects of surrounding forest cover and distance to roads on bird diversity. Mistletoes provide nectar and fruit resources in rubber so we examined mistletoe densities and the relationship with forest cover and rubber tree diameter. In rubber plantations, we recorded less than half of all bird species extant in the surrounding area. Birds with wider habitat breadths and low conservation value had a higher probability of occurrence. Species richness and diversity increased logarithmically with surrounding forest cover, but roads had little effect. Mistletoe density increased exponentially with rubber tree diameters, but was unrelated to forest cover. To maximize bird diversity in rubber-dominated landscapes it is therefore necessary to preserve as much forest as possible, construct roads through plantations and not forest, and retain some large rubber trees with mistletoes during crop rotations.
Effects of forests, roads and mistletoe on bird diversity in monoculture rubber plantations.
Sreekar, Rachakonda; Huang, Guohualing; Yasuda, Mika; Quan, Rui-Chang; Goodale, Eben; Corlett, Richard T; Tomlinson, Kyle W
2016-02-23
Rising global demand for natural rubber is expanding monoculture rubber (Hevea brasilensis) at the expense of natural forests in the Old World tropics. Conversion of forests into rubber plantations has a devastating impact on biodiversity and we have yet to identify management strategies that can mitigate this. We determined the life-history traits that best predict bird species occurrence in rubber plantations in SW China and investigated the effects of surrounding forest cover and distance to roads on bird diversity. Mistletoes provide nectar and fruit resources in rubber so we examined mistletoe densities and the relationship with forest cover and rubber tree diameter. In rubber plantations, we recorded less than half of all bird species extant in the surrounding area. Birds with wider habitat breadths and low conservation value had a higher probability of occurrence. Species richness and diversity increased logarithmically with surrounding forest cover, but roads had little effect. Mistletoe density increased exponentially with rubber tree diameters, but was unrelated to forest cover. To maximize bird diversity in rubber-dominated landscapes it is therefore necessary to preserve as much forest as possible, construct roads through plantations and not forest, and retain some large rubber trees with mistletoes during crop rotations.
Characterization of rubber particles and rubber chain elongation in Taraxacum koksaghyz
2010-01-01
Background Natural rubber is a biopolymer with exceptional qualities that cannot be completely replaced using synthetic alternatives. Although several key enzymes in the rubber biosynthetic pathway have been isolated, mainly from plants such as Hevea brasiliensis, Ficus spec. and the desert shrub Parthenium argentatum, there have been no in planta functional studies, e.g. by RNA interference, due to the absence of efficient and reproducible protocols for genetic engineering. In contrast, the Russian dandelion Taraxacum koksaghyz, which has long been considered as a potential alternative source of low-cost natural rubber, has a rapid life cycle and can be genetically transformed using a simple and reliable procedure. However, there is very little molecular data available for either the rubber polymer itself or its biosynthesis in T. koksaghyz. Results We established a method for the purification of rubber particles - the active sites of rubber biosynthesis - from T. koksaghyz latex. Photon correlation spectroscopy and transmission electron microscopy revealed an average particle size of 320 nm, and 13C nuclear magnetic resonance (NMR) spectroscopy confirmed that isolated rubber particles contain poly(cis-1,4-isoprene) with a purity >95%. Size exclusion chromatography indicated that the weight average molecular mass (w) of T. koksaghyz natural rubber is 4,000-5,000 kDa. Rubber particles showed rubber transferase activity of 0.2 pmol min-1 mg-1. Ex vivo rubber biosynthesis experiments resulted in a skewed unimodal distribution of [1-14C]isopentenyl pyrophosphate (IPP) incorporation at a w of 2,500 kDa. Characterization of recently isolated cis-prenyltransferases (CPTs) from T. koksaghyz revealed that these enzymes are associated with rubber particles and are able to produce long-chain polyprenols in yeast. Conclusions T. koksaghyz rubber particles are similar to those described for H. brasiliensis. They contain very pure, high molecular mass poly(cis-1,4-isoprene) and the chain elongation process can be studied ex vivo. Because of their localization on rubber particles and their activity in yeast, we propose that the recently described T. koksaghyz CPTs are the major rubber chain elongating enzymes in this species. T. koksaghyz is amenable to genetic analysis and modification, and therefore could be used as a model species for the investigation and comparison of rubber biosynthesis. PMID:20170509
Makita, Yuko; Kawashima, Mika; Lau, Nyok Sean; Othman, Ahmad Sofiman; Matsui, Minami
2018-01-19
Natural rubber is an economically important material. Currently the Pará rubber tree, Hevea brasiliensis is the main commercial source. Little is known about rubber biosynthesis at the molecular level. Next-generation sequencing (NGS) technologies brought draft genomes of three rubber cultivars and a variety of RNA sequencing (RNA-seq) data. However, no current genome or transcriptome databases (DB) are organized by gene. A gene-oriented database is a valuable support for rubber research. Based on our original draft genome sequence of H. brasiliensis RRIM600, we constructed a rubber tree genome and transcriptome DB. Our DB provides genome information including gene functional annotations and multi-transcriptome data of RNA-seq, full-length cDNAs including PacBio Isoform sequencing (Iso-Seq), ESTs and genome wide transcription start sites (TSSs) derived from CAGE technology. Using our original and publically available RNA-seq data, we calculated co-expressed genes for identifying functionally related gene sets and/or genes regulated by the same transcription factor (TF). Users can access multi-transcriptome data through both a gene-oriented web page and a genome browser. For the gene searching system, we provide keyword search, sequence homology search and gene expression search; users can also select their expression threshold easily. The rubber genome and transcriptome DB provides rubber tree genome sequence and multi-transcriptomics data. This DB is useful for comprehensive understanding of the rubber transcriptome. This will assist both industrial and academic researchers for rubber and economically important close relatives such as R. communis, M. esculenta and J. curcas. The Rubber Transcriptome DB release 2017.03 is accessible at http://matsui-lab.riken.jp/rubber/ .
NASA Astrophysics Data System (ADS)
Sreejith, M. P.; Balan, Aparna K.; Shaniba, V.; Jinitha, T. V.; Subair, N.; Purushothaman, E.
2017-06-01
Biodegradation behavior of styrene butadiene rubber composites reinforced with natural filler, coconut shell powder (CSP), with different filler loadings were carried out under soil burial conditions for three to six months. The extent of biodegradation of the composites was evaluated through weight loss, tensile strength and hardness measurements. It was observed that the permanence of the composites was remarkably dependent on filler modification, size of the filler particle and filler content. Composites containing silane modified filler were found to be more resistant to attack by the microbes present in the soil. Mechanical properties such as tensile strength, Young's modulus and hardness were decreased after soil burial testing due to the microbial attack onto the samples.
Chlorinolysis reclaims rubber of waste tires
NASA Technical Reports Server (NTRS)
Dufresne, E. R.; Tervet, J. H.; Hull, G. G.
1981-01-01
Process reclaims rubber and reduces sulfur content by using chlorine gas to oxidize sulfur bonds in preference to other bonds. Rubber does not have poor hysteresis and abrasion resistance like conventionally reclaimed rubber and is suitable for premium radial tires. Chlorinated rubber is less susceptible to swelling by oils and may be used as paint ingredient.
USDA-ARS?s Scientific Manuscript database
Several proteins have been identified and implicated in natural rubber biosynthesis, one of which, the small rubber particle protein (SRPP), was originally identified in Hevea brasiliensis as an abundant protein associated with cytosolic vesicles known as rubber particles. While previous in vitro s...
DOT National Transportation Integrated Search
2012-12-01
Crumb rubber, made from scrap tires, has been introduced into the production of different types of hot : mix asphalt (HMA) in either a wet or dry process. In the wet process, the crumb rubber and binder are : completely mixed to form asphalt rubber (...
21 CFR 872.6300 - Rubber dam and accessories.
Code of Federal Regulations, 2012 CFR
2012-04-01
... center intended to isolate a tooth from fluids in the mouth during dental procedures, such as filling a... center. The device includes the rubber dam, rubber dam clamp, rubber dam frame, and forceps for a rubber... sexually transmitted diseases through oral sex; those devices are classified as condoms in § 884.5300 of...
21 CFR 872.6300 - Rubber dam and accessories.
Code of Federal Regulations, 2011 CFR
2011-04-01
... center intended to isolate a tooth from fluids in the mouth during dental procedures, such as filling a... center. The device includes the rubber dam, rubber dam clamp, rubber dam frame, and forceps for a rubber... sexually transmitted diseases through oral sex; those devices are classified as condoms in § 884.5300 of...
21 CFR 872.6300 - Rubber dam and accessories.
Code of Federal Regulations, 2014 CFR
2014-04-01
... center intended to isolate a tooth from fluids in the mouth during dental procedures, such as filling a... center. The device includes the rubber dam, rubber dam clamp, rubber dam frame, and forceps for a rubber... sexually transmitted diseases through oral sex; those devices are classified as condoms in § 884.5300 of...
21 CFR 872.6300 - Rubber dam and accessories.
Code of Federal Regulations, 2010 CFR
2010-04-01
... center intended to isolate a tooth from fluids in the mouth during dental procedures, such as filling a... center. The device includes the rubber dam, rubber dam clamp, rubber dam frame, and forceps for a rubber... sexually transmitted diseases through oral sex; those devices are classified as condoms in § 884.5300 of...
21 CFR 872.6300 - Rubber dam and accessories.
Code of Federal Regulations, 2013 CFR
2013-04-01
... center intended to isolate a tooth from fluids in the mouth during dental procedures, such as filling a... center. The device includes the rubber dam, rubber dam clamp, rubber dam frame, and forceps for a rubber... sexually transmitted diseases through oral sex; those devices are classified as condoms in § 884.5300 of...
40 CFR 63.498 - Back-end process provisions-recordkeeping.
Code of Federal Regulations, 2011 CFR
2011-07-01
... be the crumb rubber dry weight of the rubber leaving the stripper. (iv) The organic HAP content of... be the crumb rubber dry weight of the crumb rubber leaving the stripper. (iii) The hourly average of... test runs. (1) The uncontrolled residual organic HAP content in the latex or dry crumb rubber, as...
40 CFR 63.498 - Back-end process provisions-recordkeeping.
Code of Federal Regulations, 2012 CFR
2012-07-01
... be the crumb rubber dry weight of the rubber leaving the stripper. (iv) The organic HAP content of... be the crumb rubber dry weight of the crumb rubber leaving the stripper. (iii) The hourly average of... test runs. (1) The uncontrolled residual organic HAP content in the latex or dry crumb rubber, as...
40 CFR 63.498 - Back-end process provisions-recordkeeping.
Code of Federal Regulations, 2014 CFR
2014-07-01
... be the crumb rubber dry weight of the rubber leaving the stripper. (iv) The organic HAP content of... be the crumb rubber dry weight of the crumb rubber leaving the stripper. (iii) The hourly average of... test runs. (1) The uncontrolled residual organic HAP content in the latex or dry crumb rubber, as...
40 CFR 63.498 - Back-end process provisions-recordkeeping.
Code of Federal Regulations, 2013 CFR
2013-07-01
... be the crumb rubber dry weight of the rubber leaving the stripper. (iv) The organic HAP content of... be the crumb rubber dry weight of the crumb rubber leaving the stripper. (iii) The hourly average of... test runs. (1) The uncontrolled residual organic HAP content in the latex or dry crumb rubber, as...
NASA Astrophysics Data System (ADS)
Royani, J. I.; Safarrida, A.; Rachmawati, I.; Khairiyah, H.; Mustika, I. P.; Suyono, A.; Rudiyana, Y.; Kubil; Nurjaya; Arianto, A.
2017-05-01
Rubber from Hevea brasiliensis is the only commercial natural rubber in the world. Propagation of rubber trees usually done by grafting and seed germination. BPPT had been producing rubber tree by in vitro technique with embryo somatic methods. Validation of mother plant for in vitro propagation is important to compare between mother plant and propagated plants. The aim for this research was to validation of PB 260 clone that planted at Cikumpay Plantation by SSR marker. Sampling of 10 rubber leaves were done at Cikumpay Plantation based on GPS position from the area of PB 260 clone. Rubber leaves were isolated with CTAB modification method to obtained DNA. Four of SSR primers from rubber, i.e.: hmac 4, hmac 5, hmct 1, and hmct 5, were used as primers to amplification of rubber DNA. The result showed that no band that different from 10 rubber of PB 260 clone at Cikumpay Plantation. This research will continue to compare genomic validation between mother plant and propagated plants that had been produced from BPPT.
Subcellular localization and interactions among rubber particle proteins from Hevea brasiliensis.
Brown, Daniel; Feeney, Mistianne; Ahmadi, Mathin; Lonoce, Chiara; Sajari, Roslinda; Di Cola, Alessandra; Frigerio, Lorenzo
2017-11-02
Natural rubber (polyisoprene) from the rubber tree Hevea brasiliensis is synthesized by specialized cells called laticifers. It is not clear how rubber particles arise, although one hypothesis is that they derive from the endoplasmic reticulum (ER) membrane. Here we cloned the genes encoding four key proteins found in association with rubber particles and studied their intracellular localization by transient expression in Nicotiana benthamiana leaves. We show that, while the cis-prenyltransferase (CPT), responsible for the synthesis of long polyisoprene chains, is a soluble, cytosolic protein, other rubber particle proteins such as rubber elongation factor (REF), small rubber particle protein (SRPP) and Hevea rubber transferase 1-REF bridging protein (HRBP) are associated with the endoplasmic reticulum (ER). We also show that SRPP can recruit CPT to the ER and that interaction of CPT with HRBP leads to both proteins relocating to the plasma membrane. We discuss these results in the context of the biogenesis of rubber particles. © The Author 2017. Published by Oxford University Press on behalf of the Society for Experimental Biology.
NASA Astrophysics Data System (ADS)
Russell, Bobby Glenn
Epoxy resins are thermosets with extraordinary adhesion; high strength; good resistance to creep, heat, and chemicals; and they have low shrinkage. Conversely, these polymers are brittle, they are sensitive to moisture, and they exhibit poor toughness. To improve their toughness, they are often modified by introducing dispersed rubber particles in the primary phase. In this study, the epoxy resin was modified with carboxyl-terminated butadiene acrylonitrile (CTBN), liquid-reactive rubbers. The initiator concentration, percent acrylonitrile in the CTBN rubber, and cure temperatures were altered to give varying materials properties. Statistical analysis of the morphology data showed that the percentage of rubber acrylonitrile had an effect on both the rubber particle size and volume fraction. The cure temperature had an effect on the rubber particle volume and modulus. Plots of the rubber particle size, volume fraction, and modulus versus bulk elastic storage modulus and fracture toughness revealed that rubber particle size had no effect on bulk properties, volume fraction and rubber particle modulus had an effect on both the bulk storage elastic modulus and fracture toughness.
Study on a Haptic Sensor Using MCF (Magnetic Compound Fluid) Electric Conductive Rubber
NASA Astrophysics Data System (ADS)
Zheng, Yaoyang; Shimada, Kunio
To provide a new composite material having a high degree of sensitivity regarding both electrical conduction and temperature for the field of robotics or sensing, we have developed magnetic rubber that contains a network-like magnetic cluster. We compared the temperature response of MCF rubber with others rubbers made under various experimental conditions, allowing us to find an optimum condition for making MCF rubber. The temperature response was obtained by an experimental equation. We also compared the electric conductivity of MCF rubber with that of ordinary electric conductive rubber and found that its electric sensitivity was lower at a small deformation, but increased at larger deformations. Therefore, MCF rubber has proven itself effective as a switching sensor when a small deformation is applied.
Combination biological and microwave treatments of used rubber products
Fliermans, Carl B.; Wicks, George G.
2002-01-01
A process and resulting product is provided in which a vulcanized solid particulate, such as vulcanized crumb rubber, has select chemical bonds altered by biotreatment with thermophillic microorganisms selected from natural isolates from hot sulfur springs. Following the biotreatment, microwave radiation is used to further treat the surface and to treat the bulk interior of the crumb rubber. The resulting combined treatments render the treated crumb rubber more suitable for use in new rubber formulations. As a result, larger loading levels and sizes of the treated crumb rubber can be used in new rubber mixtures and good properties obtained from the new recycled products.
Chrome-tanned leather shavings as a filler of butadiene-acrylonitrile rubber.
Przepiórkowska, A; Chrońska, K; Zaborski, M
2007-03-06
The noxious wastes from the tanning industry such as chrome-tanned leather shavings were used as the only filler of rubber mixes containing carboxylated butadiene-acrylonitrile rubber (XNBR) or butadiene-acrylonitrile rubber (NBR), and a dispersing agent Limanol PEV (Schill & Seilacher). The best form addition of leather powder to the rubber mixes is mixed the waste protein with zinc oxide. The leather powder added to the rubber mixes improves the mechanical properties: tensile strength (T(s)), elongation at break (epsilon(b)) and increase the cross-linking density of carboxylated XNBR and NBR rubber mixes. Satisfactory results of these studies are presented in this work.
Shear modulus and damping ratio of natural rubber containing carbon nanotubes
NASA Astrophysics Data System (ADS)
Ismail, R.; Ibrahim, A.; Rusop, M.; Adnan, A.
2018-05-01
This paper presents the results of an investigation into the potential application of Natural rubber (NR) containing Carbon Nanotubes (CNTs) by measuring its shear modulus and damping ratio. Four different types of rubber specimens which fabricated with different MWCNT loadings: 0 wt% (pure natural rubber), 1 wt%, 3 wt%, and 5 wt%. It is observed that the shear modulus and damping ratio of CNTs filled rubber composites are remarkably higher than that of raw rubber indicating the inherent reinforcing potential of CNTs.
Effects of forests, roads and mistletoe on bird diversity in monoculture rubber plantations
Sreekar, Rachakonda; Huang, Guohualing; Yasuda, Mika; Quan, Rui-Chang; Goodale, Eben; Corlett, Richard T.; Tomlinson, Kyle W.
2016-01-01
Rising global demand for natural rubber is expanding monoculture rubber (Hevea brasilensis) at the expense of natural forests in the Old World tropics. Conversion of forests into rubber plantations has a devastating impact on biodiversity and we have yet to identify management strategies that can mitigate this. We determined the life-history traits that best predict bird species occurrence in rubber plantations in SW China and investigated the effects of surrounding forest cover and distance to roads on bird diversity. Mistletoes provide nectar and fruit resources in rubber so we examined mistletoe densities and the relationship with forest cover and rubber tree diameter. In rubber plantations, we recorded less than half of all bird species extant in the surrounding area. Birds with wider habitat breadths and low conservation value had a higher probability of occurrence. Species richness and diversity increased logarithmically with surrounding forest cover, but roads had little effect. Mistletoe density increased exponentially with rubber tree diameters, but was unrelated to forest cover. To maximize bird diversity in rubber-dominated landscapes it is therefore necessary to preserve as much forest as possible, construct roads through plantations and not forest, and retain some large rubber trees with mistletoes during crop rotations. PMID:26903032
Shimada, Kunio; Mochizuki, Osamu; Kubota, Yoshihiro
2017-04-19
The aim of this study is to investigate the effect of particles as filler in soft rubber sensors installed in artificial skin. We examine sensors made of natural rubber (NR-latex) that include magnetic particles of Ni and Fe₃O₄ using magnetic compound fluid (MCF). The 1-mm thickness of the electrolytically polymerized MCF rubber makes production of comparatively thin rubber sensors feasible. We first investigate the effect of magnetic particles Ni and Fe₃O₄ on the curing of MCF rubber. Next, in order to adjust the electric properties of the MCF rubber, we adopt Al₂O₃ dielectric particles. We investigate the effect of Al₂O₃ particles on changes in electric current, voltage and temperature of electrolytically polymerized MCF rubber liquid, and on the electric properties under the application of normal and shear forces. By adjusting the ratio of Ni, Fe₃O₄, Al₂O₃ and water in MCF rubber with Al₂O₃, it is possible to change the electric properties.
Research on Extrusion of Rubber Composites Reinforced by Short Fibers Orientation Based on FEA
NASA Astrophysics Data System (ADS)
Zhang, Dewei; Wang, Chuansheng; Shen, Bo; Li, Shaoming; Bian, Huiguang
2018-06-01
In recent years, rubber composites reinforced by short fibers has been researched deeply, because of its good performances such as higher wear resistance, higher cut resistance and so on. Some research results indicated that if short fibers get orientation in rubber composites, the performances of rubber products could be promoted greatly. But how to make short fibers get orientation in rubber matrix during extrusion is still a real problem. And there are many parameters affect the short fibers orientation. So, in this paper, the effects of die structure including expansion-die and dam-expansion-die on extrusion flow field of short fiber and rubber composite material during extrusion process has been researched by Polyflow. And the FEA results about the pressure field, velocity field and the velocity vector of the rubber composites flow field indicate that, comparing with expansion-die and the dam-expansion-die, the latter one is better for the extrusion process of rubber composites and making short fibers get radial orientation in rubber matrix.
ERIC Educational Resources Information Center
Schmid, Sue
1994-01-01
Describes the benefits of using rubber floor coverings in a gym's free-weight and cardiovascular equipment areas. Tips on purchasing a rubber floor are highlighted as is an annotated list of suppliers and their rubber flooring products. (GR)
Natural rubber (NR) biosynthesis: perspectives from polymer chemistry
DOE Office of Scientific and Technical Information (OSTI.GOV)
Barkakaty, Balaka
Natural rubber is an important strategic raw material for manufacturing a wide variety of industrial products. There are at least 2,500 different latex-producing plant species; however, only Hevea brasiliensis (the Brazilian rubber tree) is a commercial source. The chemical structure of natural rubber is cis-1,4-polyisoprene, but the exact structure of the head and end groups remains unknown. Since synthetic cis-1,4-polyisoprenes cannot match the superior properties of natural rubber, understanding the chemistry behind the biosynthetic process is key to finding a possible replacement. T his chapter summarizes our current understandings from the perspective of a polymer scientist by comparing synthetic polyisoprenesmore » to natural rubber. The chapter also highlights biomimetic polymerization, research towards a synthetic match of natural rubber and the role of natural rubber in health care.« less
Higher modulus compositions incorporating particulate rubber
Bauman, B.D.; Williams, M.A.; Bagheri, R.
1997-12-02
Rubber particles, to be used as fillers or extenders for various composite polymer systems, are chlorinated by a gas-solid phase reaction with a chlorine-containing gas. A composite polymer containing the chlorinated rubber fillers or extenders exhibits a higher flexural modulus than if prepared using an unchlorinated rubber filler or extender. Chlorination of the rubber particles is carried out by contacting the finely divided rubber particles with a chlorine-containing gas comprising at least about 5 volume percent chlorine. Advantageously, the chlorine can be diluted with air, nitrogen or other essentially inert gases and may contain minor amounts of fluorine. Improved performance is obtained with nitrogen dilution of the chlorine gas over air dilution. Improved polymer composite systems having higher flexural modulus result from the use of the chlorinated rubber particles as fillers instead of unchlorinated rubber particles. 2 figs.
Higher modulus compositions incorporating particulate rubber
McInnis, E.L.; Scharff, R.P.; Bauman, B.D.; Williams, M.A.
1995-01-17
Rubber particles, to be used as fillers or extenders for various composite polymer systems, are chlorinated by a gas-solid phase reaction with a chlorine-containing gas. A composite polymer containing the chlorinated rubber fillers or extenders exhibits a higher flexural modulus than if prepared using an unchlorinated rubber filler or extender. Chlorination of the rubber particles is carried out by contacting the finely divided rubber particles with a chlorine-containing gas comprising at least about 5 volume percent chlorine. Advantageously, the chlorine can be diluted with air, nitrogen or other essentially inert gases and may contain minor amounts of fluorine. Improved performance is obtained with nitrogen dilution of the chlorine gas over air dilution. Improved polymer composite systems having higher flexural modulus result from the use of the chlorinated rubber particles as fillers instead of unchlorinated rubber particles. 2 figures.
Higher modulus compositions incorporating particulate rubber
McInnis, E.L.; Bauman, B.D.; Williams, M.A.
1996-04-09
Rubber particles, to be used as fillers or extenders for various composite polymer systems, are chlorinated by a gas-solid phase reaction with a chlorine-containing gas. A composite polymer containing the chlorinated rubber fillers or extenders exhibits a higher flexural modulus than if prepared using an unchlorinated rubber filler or extender. Chlorination of the rubber particles is carried out by contacting the finely divided rubber particles with a chlorine-containing gas comprising at least about 5 volume percent chlorine. Advantageously, the chlorine can be diluted with air, nitrogen or other essentially inert gases and may contain minor amounts of fluorine. Improved performance is obtained with nitrogen dilution of the chlorine gas over air dilution. Improved polymer composite systems having higher flexural modulus result from the use of the chlorinated rubber particles as fillers instead of unchlorinated rubber particles. 2 figs.
Optimizing particle size reduction of biochar using a planetary ball mill
USDA-ARS?s Scientific Manuscript database
With world demand for fossil fuels consistently growing, reducing our dependence on petroleum products is a necessary strategy. Our research group is currently studying the feasibility of biochar as rubber composite filler. If biochar can be used as a partial or complete substitute for carbon black ...
Biodiesel production methods of rubber seed oil: a review
NASA Astrophysics Data System (ADS)
Ulfah, M.; Mulyazmi; Burmawi; Praputri, E.; Sundari, E.; Firdaus
2018-03-01
The utilization of rubber seed as raw material of biodiesel production is seen highly potential in Indonesia. The availability of rubber seeds in Indonesia is estimated about 5 million tons per annum, which can yield rubber seed oil about 2 million tons per year. Due to the demand of edible oils as a food source is tremendous and the edible oil feedstock costs are far expensive to be used as fuel, production of biodiesel from non-edible oils such as rubber seed is an effective way to overcome all the associated problems with edible oils. Various methods for producing biodiesel from rubber seed oil have been reported. This paper introduces an optimum condition of biodiesel production methods from rubber seed oil. This article was written to be a reference in the selection of methods and the further development of biodiesel production from rubber seed oil. Biodiesel production methods for rubber seed oils has been developed by means of homogeneous catalysts, heterogeneous catalysts, supercritical method, ultrasound, in-situ and enzymatic processes. Production of biodiesel from rubber seed oil using clinker loaded sodium methoxide as catalyst is very interesting to be studied and developed further.
Crumb Rubber Recycling in Enhancing Damping Properties of Concrete
NASA Astrophysics Data System (ADS)
Sugapriya, P.; Ramkrishnan, R.
2018-02-01
Damping plays a major role in the design of roadside structures that gets affected due to vibrations transmitted from moving traffic. In this study, fine aggregates were partially replaced with crumb rubber in concrete, at varying percentages of 5, 10, 15 and 20% by weight. Three different sets of concrete, mixed with crumb rubber were prepared using raw rubber, treated rubber and treated rubber with partial replacement of cement. Cement was partially replaced with Ultra-Fine Ground Granulated Blast furnace Slag (UFGGBS) for this study. Samples were cast, cured and tested for various properties on the 7th and 28th day. The damping ratio and frequency of the peak value from a number of waves in rubber incorporated beams were found out using a FFT Analyser along with its Strength, Damping and Sorptivity characteristics. SEM analysis was conducted to analyse the micro structural bonding between rubber and concrete. The mode shapes of pavement slabs were modelled and analysed using a FEM tool, ANSYS. From the results, the behaviour of the three sets of rubberized concrete were compared and analysed, and an optimum percentage for crumb rubber and UFGGBS was proposed to achieve best possible damping without compromising the strength properties.
A review on the suitability of rubberized concrete for concrete bridge decks
NASA Astrophysics Data System (ADS)
Syamir Senin, Mohamad; Shahidan, Shahiron; Radziah Abdullah, Siti; Anting Guntor, Nickholas; Syazani Leman, Alif
2017-11-01
Road authorities manage a large population of ageing bridges, a substantial number of which fail to meet the current requirements either due to deterioration and other structural deficiencies or as a result of the escalating demands imposed by increased traffic. This problem is related to the dynamic load from vehicles. This problem can be solved by producing a type of concrete that can reduce the amplitude of oscillation or vibration such as rubberized concrete. Green construction has been a very important aspect in concrete production field in the last decade. One of the most problematic waste materials is scrap tires. The use of scrap tires in civil engineering is increasing by producing rubberized concrete. Rubberized concrete is a type of concrete that is mixed with rubber. The purpose of this review is to justify the suitability of rubberized concrete for concrete bridge decks. Several parameters named physical, chemical and mechanical properties were measured to ensure the suitability of rubberized concrete for concrete bridge decks. Rubberized concrete has similar workability to normal concrete. The rubber reduced the density and compressive strength of the concrete while increased the flexural strength, water absorption and damping ratio. The used of rubber in concrete beyond 20% is not recommended due to decreasing in compressive strength. Rubberized concrete recommended to be used in circumstances where vibration damping was required such as in bridge construction as shock-wave absorber.
Possibility of using waste tire rubber and fly ash with Portland cement as construction materials.
Yilmaz, Arin; Degirmenci, Nurhayat
2009-05-01
The growing amount of waste rubber produced from used tires has resulted in an environmental problem. Recycling waste tires has been widely studied for the last 20 years in applications such as asphalt pavement, waterproofing systems and membrane liners. The aim of this study is to evaluate the feasibility of utilizing fly ash and rubber waste with Portland cement as a composite material for masonry applications. Class C fly ash and waste automobile tires in three different sizes were used with Portland cement. Compressive and flexural strength, dry unit weight and water absorption tests were performed on the composite specimens containing waste tire rubber. The compressive strength decreased by increasing the rubber content while increased by increasing the fly ash content for all curing periods. This trend is slightly influenced by particle size. For flexural strength, the specimens with waste tire rubber showed higher values than the control mix probably due to the effect of rubber fibers. The dry unit weight of all specimens decreased with increasing rubber content, which can be explained by the low specific gravity of rubber particles. Water absorption decreased slightly with the increase in rubber particles size. These composite materials containing 10% Portland cement, 70% and 60% fly ash and 20% and 30% tire rubber particles have sufficient strength for masonry applications.
Mechanical properties of concrete containing a high volume of tire-rubber particles.
Khaloo, Ali R; Dehestani, M; Rahmatabadi, P
2008-12-01
Due to the increasingly serious environmental problems presented by waste tires, the feasibility of using elastic and flexible tire-rubber particles as aggregate in concrete is investigated in this study. Tire-rubber particles composed of tire chips, crumb rubber, and a combination of tire chips and crumb rubber, were used to replace mineral aggregates in concrete. These particles were used to replace 12.5%, 25%, 37.5%, and 50% of the total mineral aggregate's volume in concrete. Cylindrical shape concrete specimens 15 cm in diameter and 30 cm in height were fabricated and cured. The fresh rubberized concrete exhibited lower unit weight and acceptable workability compared to plain concrete. The results of a uniaxial compressive strain control test conducted on hardened concrete specimens indicate large reductions in the strength and tangential modulus of elasticity. A significant decrease in the brittle behavior of concrete with increasing rubber content is also demonstrated using nonlinearity indices. The maximum toughness index, indicating the post failure strength of concrete, occurs in concretes with 25% rubber content. Unlike plain concrete, the failure state in rubberized concrete occurs gently and uniformly, and does not cause any separation in the specimen. Crack width and its propagation velocity in rubberized concrete are lower than those of plain concrete. Ultrasonic analysis reveals large reductions in the ultrasonic modulus and high sound absorption for tire-rubber concrete.
The rubber tree genome reveals new insights into rubber production and species adaptation.
Tang, Chaorong; Yang, Meng; Fang, Yongjun; Luo, Yingfeng; Gao, Shenghan; Xiao, Xiaohu; An, Zewei; Zhou, Binhui; Zhang, Bing; Tan, Xinyu; Yeang, Hoong-Yeet; Qin, Yunxia; Yang, Jianghua; Lin, Qiang; Mei, Hailiang; Montoro, Pascal; Long, Xiangyu; Qi, Jiyan; Hua, Yuwei; He, Zilong; Sun, Min; Li, Wenjie; Zeng, Xia; Cheng, Han; Liu, Ying; Yang, Jin; Tian, Weimin; Zhuang, Nansheng; Zeng, Rizhong; Li, Dejun; He, Peng; Li, Zhe; Zou, Zhi; Li, Shuangli; Li, Chenji; Wang, Jixiang; Wei, Dong; Lai, Chao-Qiang; Luo, Wei; Yu, Jun; Hu, Songnian; Huang, Huasun
2016-05-23
The Para rubber tree (Hevea brasiliensis) is an economically important tropical tree species that produces natural rubber, an essential industrial raw material. Here we present a high-quality genome assembly of this species (1.37 Gb, scaffold N50 = 1.28 Mb) that covers 93.8% of the genome (1.47 Gb) and harbours 43,792 predicted protein-coding genes. A striking expansion of the REF/SRPP (rubber elongation factor/small rubber particle protein) gene family and its divergence into several laticifer-specific isoforms seem crucial for rubber biosynthesis. The REF/SRPP family has isoforms with sizes similar to or larger than SRPP1 (204 amino acids) in 17 other plants examined, but no isoforms with similar sizes to REF1 (138 amino acids), the predominant molecular variant. A pivotal point in Hevea evolution was the emergence of REF1, which is located on the surface of large rubber particles that account for 93% of rubber in the latex (despite constituting only 6% of total rubber particles, large and small). The stringent control of ethylene synthesis under active ethylene signalling and response in laticifers resolves a longstanding mystery of ethylene stimulation in rubber production. Our study, which includes the re-sequencing of five other Hevea cultivars and extensive RNA-seq data, provides a valuable resource for functional genomics and tools for breeding elite Hevea cultivars.
Performance of USDA guayule lines in the Northern Negev of Israel
DOE Office of Scientific and Technical Information (OSTI.GOV)
Mills, D.; Benzioni, A.; Forti, M.
The rubber yield of the guayule plant (Parthenium argentatum) is determined by its rubber concentration and biomass production, both of which are a function of genetic constituents and environmental conditions. With the aim of selecting best performing lines of guayule under the climatic conditions of the northern Negev of Israel, two-yr-old guayule plants from 13 USDA lines were evaluated for height, spread, canopy fresh and dry weight, branch and leaf dry weight, rubber and resin concentration, and rubber and resin yield per plant. Significant differences were found among the lines for all the characteristics tested. Lines 11600 and 11604 excelledmore » in rubber and biomass production and were taller and more uniform than the other lines; whereas line N593, conventionally used as a standard, performed poorly and was less uniform. The correlation between rubber yield per plant and rubber concentration was poor, rubber yield being related mainly to biomass production and to a lesser degree to height and spread of the plants. Taken together with fact that biomass production was more variable than rubber concentration, this finding suggests that breeding and selection of guayule and for high rubber yield should be directed primarily towards improvement of biomass production rather than rubber concentration. In the northern Negev of Israel, USDA lines 11600 and 11604 performed well.« less
Code of Federal Regulations, 2010 CFR
2010-07-01
...) ✔ Epichlorohydrin (106898) ✔ Ethylbenzene (100414) ✔ ✔ Ethylene Dichloride (107062) ✔ Ethylene Oxide (75218... Rubber. EPI = Epichlorohydrin Rubber. EPR = Ethylene Propylene Rubber. HBR = Halobutyl Rubber. HYP...
Rubber friction on road surfaces: Experiment and theory for low sliding speeds
DOE Office of Scientific and Technical Information (OSTI.GOV)
Lorenz, B.; Persson, B. N. J.; Oh, Y. R.
We study rubber friction for tire tread compounds on asphalt road surfaces. The road surface topographies are measured using a stylus instrument and atomic force microscopy, and the surface roughness power spectra are calculated. The rubber viscoelastic modulus mastercurves are obtained from dynamic mechanical analysis measurements and the large-strain effective modulus is obtained from strain sweep data. The rubber friction is measured at different temperatures and sliding velocities, and is compared to the calculated data obtained using the Persson contact mechanics theory. We conclude that in addition to the viscoelastic deformations of the rubber surface by the road asperities, theremore » is an important contribution to the rubber friction from shear processes in the area of contact. The analysis shows that the latter contribution may arise from rubber molecules (or patches of rubber) undergoing bonding-stretching-debonding cycles as discussed in a classic paper by Schallamach.« less
Structural characterization of rubber from jackfruit and euphorbia as a model of natural rubber.
Mekkriengkrai, Dararat; Ute, Koiichi; Swiezewska, Ewa; Chojnacki, Tadeusz; Tanaka, Yasuyuki; Sakdapipanich, Jitladda T
2004-01-01
A structural study of low molecular weight rubbers from Jackfruit (Artocarpus heterophyllus) and Painted spurge (Euphorbia heterophylla) was carried out as model compounds of natural rubber from Hevea brasiliensis. The rubber content of latex from Jackfruit was 0.4-0.7%, which is very low compared with that of 30-35% in the latex from Hevea tree. The rubber from Jackfruit latex was low molecular weight with narrow unimodal molecular weight distribution (MWD), whereas that obtained from E. heterophylla showed very broad MWD. The 1H and 13C NMR analyses showed that Jackfruit rubber consists of a dimethylallyl group and two trans-isoprene units connected to a long sequence of cis-isoprene units. The alpha-terminal group of Jackfruit rubber was presumed to be composed of a phosphate group based on the presence of 1H NMR signal at 4.08 ppm corresponding to the terminal =CH-CH2OP group.
USDA-ARS?s Scientific Manuscript database
Ground rubber contains 15-20 g Zn/kg but very low levels of Cd and could serve as an inexpensive byproduct Zn fertilizer. The aim of this investigation was to test the kinetics of Zn release in a soil treated with ground tire rubber and rubber ash compared with commercial Zn fertilizer and a labora...
Source Hierarchy List. Volume 2. E through N
1994-07-01
SEE CONTINENTAL AG HANNOVER (GERMANY F R) 421628 02 GENERAL TIRE AND RUBBER CO MARION IN 151750 02 GENERAL TIRE ANO RUBBER CO WABASH IN...151800 03 GENERAL TIRE AND RUBBER CO WABASH IN 151820 INDUSTRIAL PRODUCTS DIV...GENERAL TIRE AND RUBBER CO WABASH IN 151800 FOR HIGHEST ORGANIZATIONAL LEVEL SEE CONTINENTAL AG HANNOVER (GERMANY F R) G3 GENERAL TIRE AND RUBBER CO
Feng, Qian; Kong, Qingzhao; Jiang, Jian; Liang, Yabin; Song, Gangbing
2017-09-01
Rubber-steel-layered structures are used in many engineering applications. Laminated rubber-steel bearing, as a type of seismic isolation device, is one of the most important applications of the rubber-steel-layered structures. Interfacial debonding in rubber-steel-layered structures is a typical failure mode, which can severely reduce their load-bearing capacity. In this paper, the authors developed a simple but effective active sensing approach using embedded piezoceramic transducers to provide an in-situ detection of the interfacial debonding between the rubber layers and steel plates. A sandwiched rubber-steel-layered specimen, consisting of one rubber layer and two steel plates, was fabricated as the test specimen. A novel installation technique, which allows the piezoceramic transducers to be fully embedded into the steel plates without changing the geometry and the surface conditions of the plates, was also developed in this research. The active sensing approach, in which designed stress waves can propagate between a pair of the embedded piezoceramic transducers (one as an actuator and the other one as a sensor), was employed to detect the steel-rubber debonding. When the rubber-steel debonding occurs, the debonded interfaces will attenuate the propagating stress wave, so that the amplitude of the received signal will decrease. The rubber-steel debonding was generated by pulling the two steel plates in opposite directions in a material-testing machine. The changes of the received signal before and after the debonding were characterized in a time domain and further quantified by using a wavelet packet-based energy index. Experiments on the healthy rubber-steel-layered specimen reveal that the piezoceramic-induced stress wave can propagate through the rubber layer. The destructive test on the specimen demonstrates that the piezoceramic-based active sensing approach can effectively detect the rubber-steel debonding failure in real time. The active sensing approach is often used in structures with "hard" materials, such as steel, concrete, and carbon fiber composites. This research lays a foundation for extending the active sensing approach to damage detection of structures involving "soft" materials, such as rubber.
Research on the conductivity of a haptic sensor, especially with the sensor under extended condition
NASA Astrophysics Data System (ADS)
Zheng, Yaoyang; Shimada, Kunio
2008-11-01
The present paper describes the application of magnetic compound fluid (MCF) rubber as a haptic sensor for use as a material for robot sensors, artificial skin, and so on. MCF rubber is one of several new composite materials utilizing the MCF magnetic responsive fluid developed by Shimada. By applying MCF to silicon oil rubber, we can make MCF rubber highly sensitive to temperature and electric conduction. By mixing Cu and Ni particles in the silicon oil rubber and then applying a strong magnetic field, we can produce magnetic clusters at high density. The clusters form a network, as confirmed by optical observation. The MCF rubber with small deformations can act as an effective sensor. We report herein several experiments in which changes in the MCF rubber's resistance were observed when the rubber was compressed and a deformation was generated. We then made a trial haptic sensor using the MCF conductive rubber and performed many experiments to observe changes in the electrical resistance of the sensor. The experimental results showed that the proposed sensor made with MCF conductive rubber is useful for sensing small amounts of pressure or small deformations. Sometimes, however, the sensor rubber will be extended when we apply this sensor to the finger of the robot or an elbow. In these cases, it is necessary to understand the changes in sensor's conductivity. We therefore carried out some experiments to demonstrate how, under tensile conditions, the sensor's conductivity changes to a small value easier than the sensor in free condition. The results show that the sensors became more sensitive to the same pressure under extended conditions. In the present paper, we first describe the new type of functional fluid MCF rubber and a new composite material based on this MCF fluid. We then explain the production method for MCF conductive rubber and its conductive algorithm. Finally, we report our results regarding the MCF sensitivity when the MCF rubber was pulled. These experiments show an improvement in the sensitivity of the MCF rubber in the extended state.
Addition of Rubber to soil damages the functional diversity of soil.
Goswami, Madhurankhi; Bhattacharyya, Purnita; Tribedi, Prosun
2017-07-01
Rubber is a polymer of isoprene, consisting mainly of cis-1,4-polyisoprene units. The unmanageable production and its irresponsible disposal pose severe threats to environmental ecology. Therefore, the current study focuses extensively on the ill-effects of Rubber disposal on soil microbial functional diversity as it reflects the health of ecosystem by acting as a key component in ecosystem productivity. To investigate the effect of Rubber on soil microbial functional diversity, soil samples were collected from landfill sites and three different soil microcosms (Rubber treated, untreated, and sterile soil) were prepared. The soil enzymatic activity was determined by fluorescein diacetate hydrolysis followed by the determination of the microbial metabolic potential and functional diversity by average well color development and Shannon-Weaver index (H), respectively. BiOLOG ECO plates were used for determining the microbial functional diversity of the soil microcosms. Higher heterotrophic microbial count as well as higher soil microbial activity was observed in Rubber untreated soil than Rubber treated soil microcosm. The result indicated that the addition of Rubber to soil reduced soil heterotrophic microbial count and soil microbial activity considerably. Similarly, soil microbial metabolic potential as well as microbial functional diversity of soil had been decreased by the addition of Rubber gloves in it. Variation in soil microbial metabolic spectrum between Rubber treated and untreated microcosm was confirmed by multivariate analysis. Collectively, all the results demonstrated that the addition of Rubber to soil reduced the soil microbial functional diversity considerably. Therefore, it is necessary for the commission of serious steps regarding Rubber disposal and protection of the environment from serious environmental issues.
Research on a haptic sensor made using MCF conductive rubber
NASA Astrophysics Data System (ADS)
Zheng, Yaoyang; Shimada, Kunio
2008-05-01
To provide a new composite material having a high electrical sensitivity in the fields of robotics and sensing, a magnetic rubber having network-like magnetic clusters was developed by utilizing a magnetic compound fluid (MCF). MCF rubber with small deformations can provide an effective sensor. In this paper, we report many experiments in which changes of the MCF rubber's resistance were observed when the rubber was compressed and a deformation was generated; we then made a trial haptic sensor using the MCF conductive rubber and performed many experiments to observe changes of the electrical resistance of the sensor. The results of experiments showed that the proposed sensor made with MCF conductive rubber is useful for sensing small amounts of pressure or small deformations.
Research on a haptic sensor made using MCF conductive rubber.
Zheng, Yaoyang; Shimada, Kunio
2008-05-21
To provide a new composite material having a high electrical sensitivity in the fields of robotics and sensing, a magnetic rubber having network-like magnetic clusters was developed by utilizing a magnetic compound fluid (MCF). MCF rubber with small deformations can provide an effective sensor. In this paper, we report many experiments in which changes of the MCF rubber's resistance were observed when the rubber was compressed and a deformation was generated; we then made a trial haptic sensor using the MCF conductive rubber and performed many experiments to observe changes of the electrical resistance of the sensor. The results of experiments showed that the proposed sensor made with MCF conductive rubber is useful for sensing small amounts of pressure or small deformations.